TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf T1 - Sintering and foaming of bioactive glasses JF - Journal of American Ceramic Society N2 - Sintering, crystallization, and foaming of 44.8SiO2–2.5P2O3–36.5CaO–6.6Na2O–6.6K2O–3.0CaF2 (F3) and 54.6SiO2–1.7P2O3–22.1CaO–6.0Na2O–7.9K2O–7.7MgO (13–93) bioactive glass powders milled in isopropanol and CO2 were studied via heating microscopy, differential thermal analysis, vacuum hot extraction (VHE), Infrared spectroscopy, and time-of-flight secondary ion mass spectrometry. Full densification was reached in any case and followed by significant foaming. VHE studies show that foaming is driven by carbon gases and carbonates were detected by Infrared spectroscopy to provide the major foaming source. Carbonates could be detected even after heating to 750◦C, which hints on a thermally very stable species or mechanical trapping. Otherwise, dark gray compact colors for milling in isopropanol indicate the presence of residual carbon as well. Its significant contribution to foaming, however, could not be proved and might be limited by the diffusivity of oxygen needed for carbon oxidation to carbon gas. KW - Bioactive Glass KW - Crystallization KW - Foaming KW - Sintering PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-552454 DO - https://doi.org/10.1111/jace.18626 SN - 0002-7820 SP - 1 EP - 11 PB - Wiley online library AN - OPUS4-55245 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf A1 - Poologasundarampilai, G. A1 - Brauer, D. S. T1 - Sintering and concomitant crystallization of bioactive glasses JF - Journal of Applied Glass Science N2 - The sintering of bioactive glasses allows for the preparation of complex structures, such as three‐dimensional porous scaffolds. Such 3D constructs are particularly interesting for clinical applications of bioactive glasses in bone regeneration, as the scaffolds can act as a guide for in‐growing bone cells, allowing for good Integration with existing and newly formed tissue while the scaffold slowly degrades. Owing to the pronounced tendency of many bioactive glasses to crystallize upon heat treatment, 3D scaffolds have not been much exploited commercially. Here, we investigate the influence of crystallization on the sintering behavior of several bioactive glasses. In a series of mixed‐alkali glasses an increased CaO/alkali metal oxide Ratio improved sintering compared to Bioglass 45S5, where dense sintering was inhibited. Addition of small amounts of calcium fluoride helped to keep melting and sintering temperatures low. Unlike glass 13‐93, these new glasses crystallized during sintering but this did not prevent densification. Variation in bioactive glass particle size allowed for fine‐tuning the microporosity resulting from the sintering process. KW - Bioactive glass KW - Crystallization KW - Scaffolds KW - Sintering PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-485458 DO - https://doi.org/10.1111/ijag.13477 SN - 2041-1286 VL - 10 IS - 4 SP - 449 EP - 462 PB - Wiley AN - OPUS4-48545 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hmood, F. A1 - Schmidt, Franziska A1 - Görke, O. A1 - Günster, Jens T1 - Investigation of chemically modified ICIE16 bioactive glass, part II JF - Journal of Ceramic Science and Technology N2 - Chemically modified bioactive glasses based on ICIE16 were prepared with the melt-quenching method using water as a quenching medium. The sinterability of these bioactive glasses was investigated and is discussed in this article. The sintering experiments were conducted with different sintering temperatures, sintering times and heating rates. Those parameters are crucial for dense glass with an amorphous structure. The particle size (d50) of the starting glass powder was determined at 88 μm and kept constant. The pre-pressed glass pellets were cold-isostatically pressed at 300 MPa to a green density of around 63 %. Density development, phase identification, shrinkage behavior and the microstructure were investigated to determine the sinterability of the developed glasses. The glass powders were sintered at different temperatures inside the processing window while crystallization was monitored. The results have shown that the sinterability of the developed glasses strongly dependsonthe proposed chemical additions. The highest density reached was 96 %, which belongs to BP1 glass with sintering conditions of 20 K/min heating rate for 60 min at 750 °C. KW - Bioactive glass KW - Viscous sintering KW - Crystallization KW - Processing window KW - Grain boundary PY - 2019 DO - https://doi.org/10.4416/JCST2019-00031 VL - 11 IS - 1 SP - 1 EP - 9 PB - Göller Verlag AN - OPUS4-49913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Akatsuka, C. A1 - Honma, T. A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Tanaka, S. A1 - Komatsu, T. T1 - Surface crystallization and gas bubble formation during conventional heat treatment in Na2MnP2O7 glass JF - Journal of Non-Crystalline Solids N2 - The crystallization behavior of sodium ion conductive Na2MnP2O7 glass was examined to clarify the crystallization mechanism. The formation of thermodynamically metastable phase, layered Na2MnP2O7, at the surface of the glass occurred. Heat treatment at 430 °C for 3 h lead to surface crystals of Na2MnP2O7 oriented with the (101) direction perpendicular to the sample surface. As the heat treatment temperature increased, the glass-ceramic samples deformed, and the presence numerous micro bubbles due to dissolved water was detected. KW - Glass-ceramic KW - Crystallization KW - Sodium ion batteries KW - Bubble formation KW - Phosphate PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.01.030 VL - 510 SP - 36 EP - 41 PB - Elsevier B.V. AN - OPUS4-49618 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ivanov, V.V. A1 - Tielemann, Christopher A1 - Avramova, K. A1 - Reinsch, Stefan A1 - Tonchev, V. T1 - Modelling crystallization: When the normal growth velocity depends on the supersaturation JF - Journal of Physics and Chemistry of Solids N2 - The crystallization proceeds by the advance of the crystal faces into the disordered phase at the expense of the material excess, the supersaturation. Using a conservation constraint for the transformation ratio α∈[0,1] as complementing the rescaled supersaturation to 1 and a kinetic law for the normal growth velocity as function of the supersaturation raised to power g, the growth order, we derive an equation for the rate of transformation dα/dt. We integrate it for the six combinations of the three spatial dimensions D = 1, 2, 3 and the two canonical values of g = 1, 2 towards obtaining expressions for αDg. The same equation, with g = 1 and D = n (n is the so called Avrami exponent) is obtained when taking only the linear in α term from the Taylor’s expansion around α = 0 of the model equation of Johnson-Mehl-Avrami-Kolmogorov (JMAK). We verify our model by fitting datasets of α21 and α31 (from α = 0 to αupper = 0.999) with JMAK to obtain from the fit n = 1.725, 2.43, resp. We show further how the values of n depend on the value of αupper to which the fit is performed starting always from 0. Towards building a validation protocol, we start with validating α21 with published results. KW - Crystallization KW - Supersaturation KW - Growth kinetics KW - Growth rate KW - JMAK model PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581706 DO - https://doi.org/10.1016/j.jpcs.2023.111542 SN - 0022-3697 VL - 181 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-58170 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Paskin, A. A1 - Couasnon, T. A1 - Perez, J. P. H. A1 - Lobanov, S. S. A1 - Blukis, R. A1 - Reinsch, Stefan A1 - Benning, L. G. T1 - Nucleation and Crystallization of Ferrous Phosphate Hydrate via an Amorphous Intermediate JF - Journal of the American Chemical Society N2 - The fundamental processes of nucleation and crystallization are widely observed in systems relevant to material synthesis and biomineralization; yet most often, their mechanism remains unclear. In this study, we unravel the discrete stages of nucleation and crystallization of Fe3(PO4)2·8H2O (vivianite). We experimentally monitored the formation and transformation from ions to solid products by employing correlated, time-resolved in situ and ex situ approaches. We show that vivianite crystallization occurs in distinct stages via a transient amorphous precursor phase. The metastable amorphous ferrous phosphate (AFEP) intermediate could be isolated and stabilized. We resolved the differences in bonding environments, structure, and symmetric changes of the Fe site during the transformation of AFEP to crystalline vivianite through synchrotron X-ray absorption spectroscopy at the Fe K-edge. This intermediate AFEP phase has a lower water content and less distorted local symmetry, compared to the crystalline end product vivianite. Our combined results indicate that a nonclassical, hydration-induced nucleation and transformation driven by the incorporation and rearrangement of water molecules and ions (Fe2+ and PO4 3−) within the AFEP is the dominating mechanism of vivianite formation at moderately high to low vivianite supersaturations (saturation index ≤ 10.19). We offer fundamental insights into the aqueous, amorphous-to-crystalline transformations in the Fe2+−PO4 system and highlight the different attributes of the AFEP, compared to its crystalline counterpart. KW - Nucleation KW - Crystallization KW - Vivianite KW - Ferrous phosphate hydrate PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580696 DO - https://doi.org/10.1021/jacs.3c01494 SN - 0002-7863 VL - 145 IS - 28 SP - 15137 EP - 15151 PB - ACS Publications AN - OPUS4-58069 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf A1 - Boccaccini, A. R. T1 - Sintering and crystallization kinetics of bioactive glass 13-93 JF - Journal of Non-Crystalline Solids N2 - This study investigates the sintering and crystallization behavior and kinetic of the bioactive glass (BG) 13–93 with nominal composition (in mol%): 54.6 SiO2 - 1.7 P2O3 - 22.1 CaO - 6.0 Na2O - 7.9 K2O - 7.7 MgO. Sintering and crystallization were investigated non-isothermally for various particle size fractions smaller than 315 μm as well as for bulk samples. Densification was not hindered by the presence of crystalline phases across all particle size fractions. Afterwards, wollastonite was found as the dominant crystal phase at higher temperature which resorb primary surface precipitation-like quartz crystallites. The growth direction shifts into volume when the sample surface is nearly covered. The crystal growth rate of wollastonite was calculated from the crystalline surface layer thickness measured during heating. The findings of this study are relevant for the high temperature processing of BG 13–93. KW - Bioactive glass KW - Sintering KW - Crystallization PY - 2024 DO - https://doi.org/10.1016/j.jnoncrysol.2023.122790 SN - 0022-3093 VL - 627 SP - 1 EP - 7 PB - Elsevier AN - OPUS4-59337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nawaz, Q. A1 - Blaeß, Carsten A1 - Mueller, Ralf A1 - Boccaccini, A.R. T1 - Processing and cytocompatibility of Cu-doped and undoped fluoride-containing bioactive glasses JF - Open Ceramics N2 - Sintered or additive-manufactured bioactive glass (BG) scaffolds are highly interesting for bone replacement applications. However, crystallization often limits the high-temperature processability of bioactive glasses (BGs). Thus, the BG composition must combine high bioactivity and processability. In this study, three BGs with nominal molar (%) compositions 54.6SiO2-1.7P2O3-22.1CaO-6.0Na2O-7.9K2O-7.7MgO (13–93), 44.8SiO2-2.5P2O3-36.5CaO-6.6Na2O-6.6K2O-3.0CaF2 (F3) and 44.8SiO2-2.5P2O3-35.5CaO-6.6Na2O-6.6K2O-3.0CaF2-1.0CuO (F3–Cu) were investigated. The dissolution and ion release kinetics were investigated on milled glass powder and crystallized particles (500–600 μm). All glasses showed the precipitation of hydroxyapatite (HAp) crystals after 7 days of immersion in simulated body fluid. No significant differences in ion release from glass and crystalline samples were detected. The influence of surface roughness on cytocompatibility and growth of preosteoblast cells (MC3T3-E1) was investigated on sintered and polished BG pellets. Results showed that sintered BG pellets were cytocompatible, and cells were seen to be well attached and spread on the surface after 5 days of incubation. The results showed an inverse relation of cell viability with the surface roughness of pellets, and cells were seen to attach and spread along the direction of scratches. KW - Bioactive glass KW - Crystallization KW - Solubility KW - Cytocompatibility KW - Surface roughness PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-598257 DO - https://doi.org/10.1016/j.oceram.2024.100586 SN - 2666-5395 VL - 18 SP - 1 EP - 8 PB - Elsevier Ltd. AN - OPUS4-59825 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -