TY - GEN A1 - Schilling, Markus T1 - Full-Notch Creep Test Ontology (ontoFNCT) N2 - This is the stable version of the full-notch creep test ontology (OntoFNCT) that ontologically represents the full-notch creep test. OntoFNCT has been developed in accordance with the corresponding test standard ISO 16770:2019-09 Plastics - Determination of environmental stress cracking (ESC) of polyethylene - Full-notch creep test (FNCT). The OntoFNCT provides conceptualizations that are supposed to be valid for the description of full-notch creep tests and associated data in accordance with the corresponding test standard. By using OntoFNCT for storing full-notch creep test data, all data will be well structured and based on a common vocabulary agreed on by an expert group (generation of FAIR data) which is meant to lead to enhanced data interoperability. This comprises several data categories such as primary data, secondary data and metadata. Data will be human and machine readable. The usage of OntoFNCT facilitates data retrieval and downstream usage. Due to a close connection to the mid-level PMD core ontology (PMDco), the interoperability of full-notch creep test data is enhanced and querying in combination with other aspects and data within the broad field of materials science and engineering (MSE) is facilitated. The class structure of OntoFNCT forms a comprehensible and semantic layer for unified storage of data generated in a full-notch creep test including the possibility to record data from analysis and re-evaluation. Furthermore, extensive metadata allows to assess data quality and reliability. Following the open world assumption, object properties are deliberately low restrictive and sparse. KW - Ontology KW - Full-Notch Creep Test KW - FNCT KW - Knowledge Representation KW - Semantic Web Technologies KW - Data Structures KW - Data Management PY - 2024 UR - https://github.com/MarkusSchilling/ontoFNCT/blob/4abce82852190a5e444d302da077aa7404f433f0/ontoFNCT.ttl UR - https://raw.githubusercontent.com/MarkusSchilling/ontoFNCT/main/ontoFNCT.ttl PB - GitHub CY - San Francisco, CA, USA AN - OPUS4-59815 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Niebergall, Ute A1 - Marschall, Niklas A1 - Meinel, Dietmar A1 - Böhning, Martin T1 - Relation of craze to crack length during slow crack growth phenomena in high‐density polyethylene JF - Polymer Engineering & Science N2 - The craze‐crack mechanism occurring in high‐density polyethylene (HDPE) causing slow crack growth and environmental stress cracking is investigated in detail with respect to the relation of crack length and the related craze zone. This is essential for the understanding of the resulting features of the formed fracture surface and their interpretation in the context of the transition from crack propagation to ductile shear deformation. It turns out that an already formed craze zone does not inevitably result in formation of a propagating crack, but could also undergo ductile failure. For the examination, the full notch creep test (FNCT) was employed with a subsequent advanced fracture surface analysis that was performed using various imaging techniques: light microscopy, laser scanning microscopy, scanning electron microscopy, and X‐ray micro computed tomography scan. FNCT specimens were progressively damaged for increasing durations under standard test conditions applying Arkopal, the standard surfactant solution, and biodiesel as test media were used to analyze the stepwise growth of cracks and crazes. From considerations based on well‐established fracture mechanics approaches, a theoretical correlation between the length of the actual crack and the length of the preceding craze zone was established that could be evidenced and affirmed by FNCT fracture surface analysis. Moreover, the yield strength of a HDPE material exposed to a certain medium as detected by a classic tensile test was found to be the crucial value of true stress to induce the transition from crack propagation due to the craze‐crack mechanism to shear deformation during FNCT measurements. Highlights - Progress of crack formation in high‐density polyethylene is analyzed by different imaging techniques - Determined growth rates depend on distinction between craze zone and crack - The ratio of the present crack to the anteceding craze zone is validated theoretically - The transition from crack propagation to ductile shear deformation is identified - An already formed craze zone may still fail by ductile mechanisms KW - Craze-crack mechanism KW - Environmental stress cracking (ESC) KW - Full notch creep test (FNCT) KW - Laser scanning microscopy (LSM) KW - Slow crack growth (SCG) KW - X-ray computed tomography (CT) PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601831 DO - https://doi.org/10.1002/pen.26698 SN - 1548-2634 VL - 64 IS - 6 SP - 2387 EP - 2403 PB - Wiley AN - OPUS4-60183 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pavasarytė, Lina A1 - Azevedo do Nascimento, Allana A1 - Cysne Barbosa, Ana Paula A1 - Trappe, Volker A1 - Melo, Daniel T1 - Effects of particle size and particle concentration of poly (ethylene-co-methacrylic acid) on properties of epoxy resin JF - Journal of Applied Polymer Sciene N2 - Self-healing polymers have been developed to improve durability and reduce costs associated with maintenance during service. The addition of thermoplastics to thermosets to produce mendable polymers appears as a promising selfhealing technique. In this study, poly (ethylene-co-methacrylic acid) (EMAA) was added to epoxy resin and the effects of EMAA addition on epoxy properties were evaluated. Specimens with two different contents of thermoplastic and particles sizes were manufactured. A two-level full factorial experimental design was used to evaluate the effect of particle size and particle content on properties of epoxy modified with addition of EMAA. Tensile tests and dynamic mechanical analysis (DMA) were used and the evaluated responses were tensile strength, modulus of elasticity, and glass transition temperature (Tg). X-ray computed tomography (XCT) was used to investigate particle size and concentration after manufacturing. It was found that the particle concentration has greater effects on stress–strain behavior of epoxy while Tg was not significantly affected by neither of the analyzed entrance variables. KW - Fracture KW - Self-healing KW - Epoxy KW - Thermoplastic PY - 2024 DO - https://doi.org/10.1002/app.55677 SN - 0021-8995 SP - 1 EP - 14 PB - Wiley online library AN - OPUS4-60205 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Kalinka, Gerhard A1 - Loose, Florian T1 - Carbon fibre composites exemplarily research at BAM N2 - Lightweighting as a cross-cutting technology contributes significantly to achieve the European Green Deal goals. Based on, but not limited to, advanced materials and production technologies, the demand for natural resources and CO2 emmissions are reduced by lightweighting during production, as well as use phase. Therefore, lightweighting is a crucial transformation technology assisting in decoupling economic growth from resource consumption. In this manner, lightweighting contributes significantly as a key technology of relevance for many industrial sectors such as energy, mobility, and infrastructure, towards resource efficiency, climate action and economic strength, as well as a resilient Europe. To strengthen international partnerships, addressing global issues of today at the edge of science with high performance lightweight material based on carbon fibers, an overview about the BAM expertise in carbon fiber reinforced materials is given. T2 - Meeting KCarbon CY - Berlin, Germany DA - 15.06.2023 KW - Lightweighting KW - Carbon Fibers KW - Recycling KW - Push-out Test KW - multi scale testing PY - 2023 AN - OPUS4-58094 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Schilling, Markus A1 - Marschall, Niklas A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Dataset of comprehensive Full-notch creep tests (FNCT) of selected high-density polyethylene (PE-HD) materials N2 - The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770. The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature. KW - Polyethylene KW - Environmental Stress Cracking KW - Full-notch creep test KW - PE-HD KW - Crack growth PY - 2023 DO - https://doi.org/10.5281/zenodo.10143351 PB - Zenodo CY - Geneva AN - OPUS4-58835 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - Prolonging structural integrity—Fatigue of scarf repairs for wind turbine blade shell applications JF - Composites Part A N2 - The influence of scarf repair variables on the mechanical properties of glass fiber reinforced polymer sandwich structures is examined for the application of wind turbine blade shell repairs. Reference shell specimens are tested under fully-reversed cyclic loading to understand the fatigue behavior of the sub-component structure within a range of in-service loads, to which shell specimens with a scarf joint repair are compared. A fatiguesuperior repair material is shown to improve the fatigue behavior of the repaired structures compared to the reference specimens. In separating layup and geometry, damage development is examined on the subcomponent scale for a structural understanding of a scarf repair using in-situ digital image correlation-based strain field measurements as well as passive thermography. Within scarf repair variables, the geometry is shown to play a larger role than layup in the fatigue performance of the repaired structure. KW - Polymer–matrix composites KW - Fatigue KW - Joints/joining PY - 2023 DO - https://doi.org/10.1016/j.compositesa.2022.107419 SN - 1359-835X VL - 167 SP - 1 EP - 11 PB - Elsevier Ltd. AN - OPUS4-56942 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Ghafafian, Carineh T1 - Scarf-joint repairs under fatigue loading investigated for sandwich shell applications N2 - Wind turbine rotor blades are produced as aerodynamic, three-dimensionally formed sandwich shell structures using mainly glass fiber reinforced plastics (GFRP). The GFRP used today have the potential to withstand the harsh operating conditions of rotor blades over the projected service life of 20 years. Premature damages that occur can be traced primarily back to design and/or manufacturing imperfections, as well as unusually high load scenarios (for instance lightning strikes, or strong winds combined with system control errors). Therefore, rotor blades have to be repaired several times (on average 2-3 times) during their projected service life. Approximately 70% of these are repairs of small- to medium-sized sandwich shells, carried out by technicians directly accessing the blade by suspended roping at the wind turbine location. The goal is to execute repairs that will last over the remaining service life, i.e. be sustainable. Within the framework of a research project carried out at BAM, Division 5.3 Polymer Matrix Composites, Department 5 for Materials Engineering, not only was the geometric shape (round vs. square in relation to the top view) varied, but also the layup of the scarf repair structure, variables that have not been studied systematically to-date. Sub-component scale sandwich shell specimens with representative repairs were used in this work in addition to coupon-scale specimens that are more commonly seen in literature. These sub-component shell specimens were tested using a unique shell test bench under loading conditions representative of wind turbine blade shell operating conditions with respect to fatigue strength. Using non-destructive testing methods (field strain measurement and thermography), damage development and distribution was monitored and analyzed in-situ. As a result, a concept was developed in which the repaired areas showed at least equivalent if not higher fatigue strength than the reference shells that were not repaired. T2 - ICFC9 - The 9th International Conference on the Fatigue of Composites CY - Vicenza, Italy DA - 21.06.2023 KW - Repair of sandwich shell structures KW - Non-destructive testing KW - Wind turbine blades PY - 2023 AN - OPUS4-57929 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krauklis, A. E. A1 - Starovka, O. A1 - Gibhardt, D. A1 - Aouissi, H. A. A1 - Burlakovs, J. A1 - Sabalina, A. A1 - Fiedler, Bodo A1 - Kalinka, Gerhard T1 - Reversible and irreversible effects on the epoxy GFRP fiber-matrix interphase due to hydrothermal aging JF - Composites Part C N2 - Epoxy R-Glass Fiber-Reinforced Polymer (GFRP) composite plates were hydrothermally aged at 60 ◦C for 23, 75, and 133 days. The water content reached 0.97 wt%, 1.45 wt% and 1.63 wt%, respectively. The studied GFRP matrix was inert to hydrolysis or chain scission, allowing for investigation of irreversible changes in the fiber-matrix interphase due to hydrothermal aging upon re-drying. During each period, a subset of the specimens was removed from the water bath and dried in a chamber. The weight loss upon drying was explained with epoxy leaching (impurities), sizing-rich interphase hydrolysis, glass fiber surface hydrolysis, accumulated degradation products escaping, and water changing state from bound to free. The influence of hydrothermal aging on the fiber-matrix interfacial properties was investigated. Lower interfacial strength of hydrothermally aged (wet) samples was attributed to plasticization of the epoxy, plasticization and degradation of the sizing-rich interphase (including formation of hydrolytic flaws), and hydrolytic degradation of the glass fiber surface. The kinetics of epoxy-compatible epoxysilane W2020 sizing-rich interphase hydrolysis provided an estimate of ca. 1.49%, 4.80%, and 8.49% of the total composite interphase degraded after 23, 75, and 133 days, respectively. At these conditions, the interface lost 39%, 48%, and 51% of its strength. Upon re-drying the specimens, a significant part of the interfacial strength was regained. Furthermore, an upward trend was observed, being 13%, 10% and 3% strength, respectively; thus, indicating a possibility of partial recovery of properties. KW - GFRP KW - Hydrothermal Ageging KW - Interphase KW - Water Diffusion KW - Desorption KW - Interfacial Strength PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581554 DO - https://doi.org/10.1016/j.jcomc.2023.100395 SN - 2666-6820 VL - 12 SP - 1 EP - 9 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-58155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kalinka, Gerhard T1 - Testing the fibre matrix interface of short glass fibre reinforced PMCs with using the push out technique N2 - With this presentation, the push-out technique is explained. The focus of the experimental work is on the characterization of the fiber-matrix interface of short fiber reinforced composites. The reinforcing component was glass fibers and the matrix polymer was PA6.6 and PPA. It is demonstrated for the first time that the push-out technique ca be applied on injection molded short fiber PMC and is sensitive to the mechanical interface properties. Further studies are planned on the influence of multiple processing, the temperature and humidity. T2 - Composirtes United Workshop „Fiber Matrix Interphases“ CY - Online meeting DA - 09.11.2023 KW - Polymer Matrix Composite KW - Glass Fibres KW - PA6.6 KW - PPA KW - Push-out Test KW - Interface Strength PY - 2023 AN - OPUS4-59053 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rabe, T. A1 - Kalinka, Gerhard A1 - Mieller, Björn T1 - Manufacturing and deformation behavior of alumina and zirconia helical springs at room temperature JF - Journal of the American Ceramic Society N2 - Ceramic helical springs with identical dimensions were produced by hard machining from alumina, alumina toughened zirconia (ATZ), and tetragonal zirconia polycrystals (TZP) stabilized with different oxides. According to the results of the spring constant determination under deformation rates of 3 mm/min, the deformation behavior of all ceramic springs obeys to Hook’s law. However, variation of the deformation rate, tests under constant load, and spring recovery behavior revealed differences in the deformation behavior of alumina, TZP, and ATZ springs. Alumina springs exhibited time-independent deformation in all tests. In contrast, anelastic deformation at room temperature was demonstrated in all springs containing TZP. This deformation is completely reversible over a period of several days. Anelastic behavior is particularly pronounced in Y-TZP springs, whereas Ce-TZP springs exhibit comparatively very low but still reliably detectable anelasticity. Oxygen vacancies in the TZP ceramic are considered the most likely explanation for the anelastic behavior of TZP springs at room temperature. KW - Alumina KW - Creep KW - Elastic properties KW - Zirconia PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-571858 DO - https://doi.org/10.1111/jace.19085 SN - 0002-7820 SP - 1 EP - 14 PB - Wiley-Blackwell CY - Oxford [u.a.] AN - OPUS4-57185 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Böhning, Martin A1 - Schilling, Markus A1 - Thuy, Maximilian A1 - Niebergall, Ute T1 - Environmental Stress Cracking in PE-HD – Assessment of Crack Propagation and Mechanisms by Optical Methods N2 - Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules. A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth. For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography. T2 - 34th Polymer Degradation Disscussion Group (PDDG) Conference CY - Dubrovnik, Croatia DA - 12.06.2023 KW - Polyethylen KW - Full Notch Creep Test KW - Environmental Stress Cracking KW - Fracture Surface Analysis PY - 2023 AN - OPUS4-57711 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Rissentwicklung in CFK-Laminaten nachgewiesen durch in situ Röntgen-Refraktion N2 - In Leichtbauanwendungen sind Materialien mit geringen Dichten und hohen Festigkeiten gefragt. Insbesondere Faser-Kunststoff-Verbunde (FKV) erfüllen diese Anforderungen und werden zunehmend für Strukturbauteile eingesetzt. Die Oberflächen moderner Rotorblätter von Windkraftanlagen werden aus FKV gefertigt. Das Versagen dieser Materialien hat massiven Einfluss auf die Einsatzfähigkeit der gesamten Windkraftanlage. Daher ist die Kenntnis des Versagensverhaltens dieser Komponenten unter statischer und zyklischer Belastung von großem Interesse, um die Betriebsbeanspruchung abzuschätzen. Im Idealfall wird die Schadensentwicklung unter Betriebslast mit zerstörungsfreien in-situ-Prüfverfahren ermittelt. Hier berichten wir über die Beobachtung der Rissentwicklung in Carbon-Faserverstärkten Kunststoffen (CFK) unter kontinuierlicher Zugbelastung durch in-situ Synchrotron-Röntgenrefraktionsradiographie. Eine selbst entwickelte elektromechanische Zugprüfmaschine mit einem Kraftbereich bis zu 15 kN wurde in den Strahlengang an der BAMline (BESSY II) integriert. Da in herkömmlichen (Absorptions-) Radiographien Defekte wie Zwischenfaserbrüche oder Faser-Matrix-Enthaftung keinen ausreichenden Kontrast verursachen, wird zur Kontrastanhebung die Röntgenrefraktion benutzt. Hier wird das sogenannte Diffraction Enhanced Imaging (DEI) angewandt, um Primär- und gebrochene Strahlung mit Hilfe eines Analysatorkristalls zu trennen. Diese Technik ermöglicht schnelle Messungen mit einem Gesichtsfeld von einigen Quadratmillimetern (hier: 14 mm × 7.2 mm) und ist ideal für in-situ Untersuchungen. Die Bildgebung und der Zugversuch erfolgen mit einer Bildfrequenz von 0.7 / s und einer Dehnrate von 0.00055 / s . Bei 0°/90° Fasergelegen treten die ersten Zwischenfaserrisse bei 380 MPa (Dehnung 0.8 %) auf. Vor dem Versagen bei ca. 760 MPa (Dehnung 2.0 %) beobachten wir die Ausbildung eines nahezu äquidistanten Rissmusters (Risse in ca. 1 mm Abstand), das sich im geschädigten Zustand über die gesamte Probe erstreckt. T2 - DACH-Jahrestagung 2023 CY - Friedrichshafen, Germany DA - 15.05.2023 KW - Röntgen-Refraktion KW - Synchrotronstrahlung KW - CFK KW - Rissentwicklung PY - 2023 AN - OPUS4-57622 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Rissentwicklung in CFK-Laminaten nachgewiesen durch in situ Röntgen-Refraktion T2 - DGZfP-Berichtsband BB 180 N2 - In Leichtbauanwendungen sind Materialien mit geringen Dichten und hohen Festigkeiten gefragt. Insbesondere Faser-Kunststoff-Verbunde (FKV) erfüllen diese Anforderungen und werden zunehmend für Strukturbauteile eingesetzt. Die Oberflächen moderner Rotorblätter von Windkraftanlagen werden aus FKV gefertigt. Das Versagen dieser Materialien hat massiven Einfluss auf die Einsatzfähigkeit der gesamten Windkraftanlage. Daher ist die Kenntnis des Versagensverhaltens dieser Komponenten unter statischer und zyklischer Belastung von großem Interesse, um die Betriebsbeanspruchung abzuschätzen. Im Idealfall wird die Schadensentwicklung unter Betriebslast mit zerstörungsfreien in-situ-Prüfverfahren ermittelt. Hier berichten wir über die Beobachtung der Rissentwicklung in Carbon-Faserverstärkten Kunststoffen (CFK) unter kontinuierlicher Zugbelastung durch in-situ Synchrotron-Röntgenrefraktionsradiographie. Eine selbst entwickelte elektromechanische Zugprüfmaschine mit einem Kraftbereich bis zu 15 kN wurde in den Strahlengang an der BAMline (BESSY II) integriert. Da in herkömmlichen (Absorptions-) Radiographien Defekte wie Zwischenfaserbrüche oder Faser-Matrix-Enthaftung keinen ausreichenden Kontrast verursachen, wird zur Kontrastanhebung die Röntgenrefraktion benutzt. Hier wird das sogenannte Diffraction Enhanced Imaging (DEI) angewandt, um Primär- und gebrochene Strahlung mit Hilfe eines Analysatorkristalls zu trennen. Diese Technik ermöglicht schnelle Messungen mit einem Gesichtsfeld von einigen Quadratmillimetern (hier: 14 mm × 7.2 mm) und ist ideal für in-situ Untersuchungen. Die Bildgebung und der Zugversuch erfolgen mit einer Bildfrequenz von 0.7 / s und einer Dehnrate von 0.00055 / s . Bei 0°/90° Fasergelegen treten die ersten Zwischenfaserrisse bei 380 MPa (Dehnung 0.8 %) auf. Vor dem Versagen bei ca. 760 MPa (Dehnung 2.0 %) beobachten wir die Ausbildung eines nahezu äquidistanten Rissmusters (Risse in ca. 1 mm Abstand), das sich im geschädigten Zustand über die gesamte Probe erstreckt. T2 - DACH-Jahrestagung 2023 CY - Friedrichshafen, Germany DA - 15.05.2023 KW - Röntgen-Refraktion KW - Synchrotronstrahlung KW - CFK KW - Rissentwicklung PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576230 SN - 978-3-947971-29-9 VL - BB 180 SP - 1 EP - 8 AN - OPUS4-57623 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Thuy, Maximilian A1 - Brauch, N. A1 - Niebergall, Ute A1 - Alig, I. A1 - Oehler, H. A1 - Böhning, Martin T1 - Environmental Stress Cracking of PE-HD Induced by Liquid Test Media Representing Crop Protection Formulations T2 - Advances in Accelerated Testing and Predictive Methods in Creep, Fatigue, and Environmental Cracking N2 - Packaging containers for dangerous goods that include aggressive liquids require that any packaging material that is based on high-density polyethylene has a high degree of stability and durability. This work is focused on testing the environmental stress cracking of the high-density polyethylenes used for such containers in contact with crop protection formulations, in particular, two model liquids established in Germany as standardized test media representatives for crop protection formulations containing the various admixtures typical for such products. One of the liquids is water-based and contains mostly surface-active ingredients, while the other is solvent-based and includes some emulsifiers. Originally established for pin impression tests, these model liquids and their individual components were here used for the first time as environmental media in the Full Notch Creep Test, which addresses the resistance against environmental stress cracking. The Full Notch Creep Test was carried out on five high-density polyethylene types with both model liquids, and also on one selected material with its components. The evaluation was focused on the fracture surface structures, which were visualized by a scanning electron microscope and by optical in situ imaging of the notch opening. While the water-based model liquid and its surface-active individual components induced environmental stress cracking with the characteristic pattern for a craze-crack mechanism and so-called brittle fracture on the surface, the solvent-based model liquid and its soluble ingredients exhibited rather ductile failure behavior, caused by the plasticizing effect on the polymer that reduced the yield stress of the high-density polyethylene. For both cases, fracture surface analysis, together with side views of the crack opening, showed a clear relation between surface pattern, notch deformation (e.g., by blunting), or crack opening due to crack growth with time to failure and the solubility of the liquids in high-density polyethylene. KW - Environmental stress cracking KW - Fracture surface KW - Full Notch Creep Test KW - Crop protection formulations KW - High-density polyethylene PY - 2023 DO - https://doi.org/10.1520/STP164320210095 SP - 317 EP - 341 PB - ASTM International CY - West Conshohocken, PA (USA) AN - OPUS4-57459 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Altmann, Korinna A1 - Marzik, Julian T1 - Roving-Alterung und mechanische Eigenschaften N2 - Im statistischen Mittel steht eine Windkraftanlage (WKA) in Deutschland alle 6 Jahre wegen eines Schadens an den Rotorblättern und verursacht Kosten von 20k€-40k€ infolge Ertragsausfall und Reparaturkosten. Bei über 30.000 WKA in Deutschland verursacht dies jährlichen Kosten von 100-200 Mio. €. Zu 70% sind die Ursachen Fertigungsfehler. Diesem Themenkomplex widmet sich FB-5.3 in Kooperation mit FBs der Zerstörungsfreien Prüfung (Abt. 8) schon seit Jahren. Im aktuellen Projekt geht es um einen vorzeitigen Verschleiß der Rotorblätter infolge der Verwendung gealterter Glasfaser-Rovings. (GF). Die Entwicklung moderner Windkraftanlagen hatte in Europa seinen Ursprung in den 90er Jahren. OEMs und GF-Hersteller waren dicht beisammen. Die Globalisierung des Marktes führt heute zu einer weltweiten Verschiffung der GF in feucht-warmen Containern. Je nach Beschaffenheit (Chemie) der Schlichten (Oberflächenbehandlung) von GF können diese stark altern (Hydrolyse-Effekte) und die Festigkeit kann im Bauteil um bis zu 50% abgemindert sein. In einer Kooperation mit der Rotorblattallianz, einem Zusammenschluss der OEMs, Halbzeugherstellern und Forschungsinstituten, wurden schon vor 5 Jahren in einem Forschungsprojekt (FB-5.3; VH 5538) die chemischen Mechanismen der Alterung exemplarisch für eine Glasfaser-Roving-Type aufgeklärt. Im aktuellen Projekt (FB-5.3; VH 5304) wird ein beschleunigtes Alterungsverfahren (erhöhte Temperatur und Feuchte) am Roving im un-impregnierten Zustand entwickelt und die Festigkeit nachfolgend nach Einbettung in eine Epoxid-Harz-Matrix bestimmt. Je nach Alterungszustand zeigt sich eine Abnahme der Zwischenfaserbruchfestigkeit von bis zu 50%. Nicht alle Glasfaser-Roving-Typen zeigen diesen Effekt. Es ist gelungen für OEMs und Halbzeughersteller ein handhabbares Verfahren zur innerbetrieblichen Qualitätssicherung zu entwickeln, da die wenigsten Firmen über komplexe Analyseverfahren, wie an der BAM, verfügen. T2 - Composite United - AG Faserverbund in der Windenergie CY - Braunschweig, Germany DA - 09.05.2023 KW - Faserkunststoffverbunde KW - Windenergie KW - Alterung PY - 2023 AN - OPUS4-58409 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Sachs, Patrick T1 - Dynamic mechanical analysis of epoxy-matrix cross linking measured in-situ using an elastomer container N2 - A new patented dynamic mechanical analysis (DMA) is presented, where the tensile, bending- or torsional stiffness of a media can be characterized in-situ during the phase transition from liquid to solid. An epoxy system, e.g. Hexion L285/H287, is filled into an elastomer container, such as a silicone tube. This can be mounted into a conventional DMA and, based on a linear viscoelastic approach, the storage modulus (E’;G’), the loss modulus (E’’;G’’) and the loss angle tan(delta) can be measured at constant temperature as a function of time in order to investigate the liquid to sol-gel to solid transition. With this new method, the stiffness increase as a result of the cure process can be directly measured more precisely than with a rheometer in a shear plate set-up, because using an elastomer container gives a defined cross section for calculating the Young’s modulus. T2 - 20th European Conference on Composite Materials, ECCM20 CY - Lausanne, Switzerland DA - 26.06.2022 KW - Dynamic mechanical analysis (DMA) KW - Thermoset polymers KW - Cure process KW - Cross linking PY - 2022 AN - OPUS4-55213 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thuy, Maximilian A1 - Pedragosa-Rincon, M. A1 - Niebergall, Ute A1 - Oehler, H. A1 - Alig, I. A1 - Böhning, Martin T1 - Environmental Stress Cracking of High-Density Polyethylene Applying Linear Elastic Fracture Mechanics JF - Polymers N2 - The crack propagation rate of environmental stress cracking was studied on high-density polyethylene compact tension specimens under static loading. Selected environmental liquids are distilled water, 2 wt% aqueous Arkopal N100 solution, and two model liquid mixtures, one based on solvents and one on detergents, representing stress cracking test liquids for commercial crop protection products. The different surface tensions and solubilities, which affect the energetic facilitation of void nucleation and craze development, are studied. Crack growth in surface-active media is strongly accelerated as the solvents induce plasticization, followed by strong blunting significantly retarding both crack initiation and crack propagation. The crack propagation rate for static load as a function of the stress intensity factor within all environments is found to follow the Paris–Erdogan law. Scanning electron micrographs of the fracture surface highlight more pronounced structures with both extensive degrees of plasticization and reduced crack propagation rate, addressing the distinct creep behavior of fibrils. Additionally, the limitations of linear elastic fracture mechanisms for visco-elastic polymers exposed to environmental liquids are discussed. KW - Crack propagation KW - Environmental stress cracking KW - Fracture toughness KW - Crop protection products KW - High-density polyethylene KW - Craze–crack mechanism KW - Linear elastic fracture mechanics KW - Stress intensity factor PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550476 DO - https://doi.org/10.3390/polym14122415 SN - 2073-4360 VL - 14 IS - 12 SP - 1 EP - 21 PB - MDPI CY - Basel AN - OPUS4-55047 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lamoriniere, S. A1 - Mitchell, P. J. A1 - Ho, K. A1 - Kalinka, Gerhard A1 - Shaffer, M. S. P. A1 - Bismarck, A. T1 - Carbon nanotube enhanced carbon Fibre-Poly(ether ether ketone) interfaces in model hierarchical composites JF - Composites Science and Technology N2 - Poly (ether ether ketone) (PEEK) has a high continuous service temperature, excellent mechanical properties, and good solvent and abrasion resistance, which can be further improved through the addition of carbon nanotubes (CNTs). CNT-PEEK nanocomposites are promising matrices for continuous carbon fibre composites; powder processing can mitigate the high melt viscosities in these systems. In this study, model single fibre (hierarchical) composites were produced by embedding sized and desized carbon fibres in nanocomposite CNTPEEK powders followed by single fibre pull-out tests to assess interfacial characteristics. Carbon fibre-PEEK interfacial shear strength is typically 40–45 MPa. Increasing CNT loadings increased fibre-matrix interfacial shear strength linearly up to ~70 MPa at 5.0 wt%, which was attributed to the CNT-based mechanical modification of the PEEK matrix. Apparent interfacial shear strength was inversely correlated with the embedded fibre length irrespective of carbon fibre sizing or CNT loading, indicating brittle fracture of the fibre-matrix interface. Pulled out carbon fibres were still coated with the matrix, which indicated strong adhesion at the interface in all samples, likely related to a transcrystalline region. Adhesion was, however, negatively affected by the presence of epoxy sizings. Frictional shear strength was independent of embedded fibre length and CNT content for all samples. KW - Keywords: Poly(ether ether ketone) KW - Carbon fibres KW - Carbon nanotubes KW - Interfacial strength KW - Debonding PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550052 DO - https://doi.org/10.1016/j.compscitech.2022.109327 SN - 0266-3538 VL - 221 SP - 1 EP - 8 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-55005 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Guerra, E. S. S. A1 - Silva, B. L. A1 - Melo, J. D. D. A1 - Kalinka, Gerhard A1 - Barbosa, A. P. C. T1 - Microscale evaluation of epoxy matrix composites containing thermoplastic healing agent JF - Composites Science and Technology N2 - Among the strategies to produce healable thermosetting systems is their modification by the addition of thermoplastic particles. This work investigates the influence of poly(ethylene-co-methacrylic acid) (EMAA) on fibermatrix interfacial properties of a glass fiber reinforced epoxy matrix composite. Epoxy-EMAA interactions were evaluated using differential scanning calorimetry (DSC) and infrared spectroscopy. The effects of EMAA on the epoxy network formation were evidenced by changes in glass transition temperature, cure kinetics and alteration of chemical groups during cure. Interfacial shear strength (IFSS) measurements obtained by single fiber pull-out tests indicate similar interfacial properties for pure and EMAA modified epoxy. Additionally, the potential for self-healing ability of an EMAA modified epoxy was demonstrated. However, IFSS after a healing cycle for the EMAA modified epoxy was lower as compared to the pure epoxy, because of the lower fiber-EMAA interfacial shear strength. So, thermoplastic healing agents has not only to fill cracks in the matrix material, but also have to be optimized regarding its interface properties to the reinforcing fibers. KW - Interfacial strength KW - Fiber/matrix bond KW - Self-healing KW - Polymer-matrix composites (PMC) PY - 2022 DO - https://doi.org/10.1016/j.compscitech.2022.109843 SN - 0266-3538 VL - 232 SP - 1 EP - 9 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-56379 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Alig, I. A1 - Oehler, H. A1 - Brauch, Niels A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Charakterisierung von Behälterwerkstoffen aus Polyethylen N2 - Das langsame Risswachstum (slow crack growth, SCG) sowie der umgebungsbedingte Spannungsriss (environmental stress cracking, ESC) sind relevante Schädigungsmechanismen für teilkristalline Werkstoffe auf Basis von Polyethylen hoher Dichte (PE-HD). Der Vortrag gibt einerseits einen Überblick über die grundlegenden Struktur-Eigenschafts-Beziehungen in diesem Kontext, andererseits werden auch verschiedene praxisorientierte Prüfverfahren vorgestellt. Letztere wurden in gemeinsamen Forschungsprojekten von BAM und LBF mit dem Schwerpunkt Gefahrgutbehälter bzw. Pflanzenschutzmittel vergleichend untersucht und durch weitergehende Analytik ergänzt. T2 - 16. Tagung des Arbeitskreises Polymeranalytik Webkonferenz, Fraunhofer LBF und FGK CY - Online meeting DA - 22.03.2022 KW - Polyethylen KW - Full Notch Creep Test KW - Environmental Stress Cracking KW - Spannungsriss PY - 2022 AN - OPUS4-54547 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - THES A1 - Nielow, Dustin T1 - Einfluss fertigungsbedingter Imperfektionen auf die Schwingfestigkeit von FKV-Schalenstrukturen in Sandwichbauweise T2 - BAM-Dissertationsreihe N2 - Rotorblätter von Windenergieanlagen (WEA) weisen häufig nach wenigen Jahren, lange vor dem Erreichen der prognostizierten Lebensdauer von 20 bis 30 Jahren Risse in der Blattschale auf. Die Folge sind aufwendige Reparaturen am installierten und schwer zugänglichen Rotorblatt und der kostenintensive Nutzungsausfall durch den Stillstand der WEA. Als mögliche Initiatoren für die Schäden in der Blattschale der Rotorblätter gelten fertigungsbedingte Imperfektionen. Für die Untersuchung des Einflusses dieser Imperfektionen auf das Ermüdungsverhalten der Rotorblätter wurde an der BAM (Bundesanstalt für Mate-rialforschung und -prüfung) ein Prüfstand für statische und zyklische Versuche von Schalensegmenten im intermediate scale entwickelt und betrieben. Die untersuchten Schalensegmente in Sandwichbauweise sind der Rotorblattschale von WEA im Hinblick auf die Strukturmechanik, die eingesetzten Halbzeuge, den Laminataufbau und dem eingesetzten Fertigungsverfahren ähnlich. Als Imperfektionen wurden verschiedenen Variationen von Lagenstößen in die Hautlagen und Schaumstöße mit Breitenvariation in den Stützkern reproduzierbar eingebracht. Die Überwachung des Schädigungszustandes während der Schwingversuche unter realistischen Lastszenarien erfolgt über eine kombinierte in situ Schädigungsüberwachung mittels passiver Thermografie und Felddehnungsmessung. Mit den durchgeführten Schwingversuchen und der begleitenden Überwachung des Schädigungszustandes ließen sich die Schadensinitiation und die signifikante Herabsetzung der Lebensdauer durch die eingebrachten Imperfektionen zweifelsfrei nachweisen und entsprechende Konstruktionshinweise für die betriebssichere Auslegung von Sandwichstrukturen ableiten. N2 - Wind turbines often exhibit cracks in the blade shells after only a few years in service, significantly before their expected 20 to 30 year design lifespan. This leads to complicated repairs on difficult to reach rotor blades, and can cause a cost-intensive standstill of the turbine. A possible source of these defects in the rotor blade shells are the imperfections which occur during production. In order to investigate the effect of these imperfections on the fatigue behavior of rotor blades, a test rig was developed at the BAM (Bundesanstalt für Materialforschung und -prüfung) upon which intermediate scale static and cyclic-fatigue testing could be performed. The complementary sandwich shell specimens developed and investigated with the test rig are representative of the outer shell of wind turbine rotor blades in terms of materials and manufacturing processes, as well as structural mechanics. The specimens were built with reproducible imperfections, including laminate overlaps in the face sheets and gaps of varying size in the foam core. The damage condition was monitored during cyclic-fatigue testing under realistic load cases using a combination of in-situ passive thermography and strain field measurement. The cyclic testing and parallel non-destructive structural health monitoring of the shell specimens showed the imperfections to significantly influence the damage initiation and decrease the component service life. The results can be used accordingly as recommendations for operationally more reliable design of sandwich structures. T3 - BAM Dissertationsreihe - 170 KW - Erneuerbare Energien KW - Windenergie KW - Verbundwerkstoffe KW - Betriebsfestigkeit KW - Komponentenprüfung KW - Renewable ernergy KW - Wind energy KW - Intermediate scale KW - Composites KW - Fatigue PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-546701 SN - 1613-4249 VL - 170 SP - 1 EP - 178 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-54670 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Maximilian, Thuy A1 - Spyrantis, Alexander A1 - Böhning, Martin A1 - Niebergall, Ute A1 - Maaß, Robert T1 - Spatially resolved roughness exponent in polymer fracture JF - Physical review materials N2 - The fracture surface of slow and continuous crack propagation during environmental stress cracking of a semicrystalline polyethylene exhibits isotropic roughness exponents at the local scale but resolved across the macroscopic fracture surface a clear position dependence is found. The spatially resolved roughness exponent admits values in the range between 0.1 and 0.4, demonstrating nontrivial exponents in the small length-scale regime. Instead, they vary across the fracture surface according to the stress-state distribution, which suggests that the exponents are intimately linked to the locally dominating dissipation processes during craze cracking. KW - Plasticity KW - Fracture KW - Material failure KW - Mechanical deformation PY - 2022 DO - https://doi.org/10.1103/PhysRevMaterials.6.L090601 VL - 6 IS - 9 SP - 1 EP - 7 PB - American Physical Society CY - USA, Maryland AN - OPUS4-55797 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - Fully-reversed fatigue behavior of scarf joint repairs for wind turbine blade shell applications N2 - Due to manufacturing imperfections which can propagate to damage under in-service loads, wind turbine rotor blades, made primarily of glass fiber reinforced polymers (GFRP), often fail significantly before their design life. To enable a quick and cost-effective return to service, localized repairs can be executed by technicians in the field, directly accessing the blades by suspended roping. Scarf joint repairs, shown to be highly efficient with a smooth load transition across angled joint walls and a restored aerodynamic profile, are the focus of this study. The damage mechanisms of these structures were examined under fully-reversed mechanical cyclic loading with a load ratio R = -1, which was made possible on the coupon scale by a custom designed anti-buckling support. The number of cycles to failure were compared across load levels. While the scarf joint ratio was held constant at 1:50, known from industry and literature to be a good compromise between restored mechanical properties and repair size, the layup sequence was varied between small-to-large and large-to-small. Hereby the effect of the presence of resin pockets and fiber orientation mismatch between the parent and repair structure on the failure mechanism as well as fatigue strength of ±45° GFRP scarf joint repair structures was studied. Strain development across the joint length was measured to assess stiffness degradation in addition to the fatigue strength recovery of scarf joint structures with respect to pristine reference specimens. Grayscale analysis was used to monitor the damage state leading to fracture across the specimens. Post-mortem fractography analysis with light microscopy described the global failure mechanisms as well as local damage distribution within the structure, all of which provided insight to critical variables in scarf joint GFRP structures under fully-reversed mechanical cyclic loading, allowing for the tailoring of such repairs on wind turbine blade shells for maximum restoration of service life. T2 - 20th European Conference on Composite Materials (ECCM20) CY - Lausanne, Switzerland DA - 26.06.2022 KW - Glass fiber reinforced polymers KW - Scarf repairs KW - Fatigue PY - 2022 AN - OPUS4-55638 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Oehler, H. A1 - Alig, I. A1 - Böhning, Martin T1 - Damaging effect of admixtures used in crop protection products on high density polyethylene packaging material JF - Polymer Testing N2 - The phenomenon of environmental stress cracking is still a major issue in materials engineering as well as from a scientific perspective. Especially in the case of packaging materials made of high-density polyethylene, assessing the potential of premature damage due to environmental stress cracking is complex because of the large number of components in possible liquid filling goods. As a first guideline, the well-known effect of detergents and dispersants is usually considered, but the interplay with other components, such as organic solvents is often unknown. Particularly challenging in this respect are crop protection products, consisting of several different admixtures in addition to the biologically active ingredients. This study is based on two model liquids representing these admixtures that were established for testing in this context. The model liquids as well as their constituting components were used as liquid media in the Full Notch Creep Test to characterize the environmental stress cracking behavior of a typical high-density polyethylene. Complementary to the time-to failure of a notched specimen obtained from these tests, the crack opening was monitored optically, and the fracture surface was analyzed post-failure by laser scanning microscopy as well as scanning electron microscopy. Based on the results, the effect of various surfactants as well as the influence of organic solvents on environmental stress cracking are discussed. KW - Environmental stress cracking KW - High-density polyethylene KW - Crop protection products KW - Full notch creep test KW - Fracture surface analysis KW - Crack opening displacement PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-554631 DO - https://doi.org/10.1016/j.polymertesting.2022.107672 SN - 0142-9418 VL - 114 SP - 1 EP - 16 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-55463 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ghafafian, Carineh A1 - Trappe, Volker ED - Vassilopoulos, A. P. ED - Michaud, V. T1 - Fully-reversed fatigue behavior of scarf joint repairs for wind turbine blade shell applications T2 - Composites meet sustainability - Proceedings of the 20th European conference on composite materials, ECCM20, 26-30 June, 2022, Lausanne, Switzerland N2 - To enable a quick and cost-effective return to service for wind turbine blades, localized repairs can be executed by technicians in the field. Scarf repairs, shown to be highly efficient with a smooth load transition across angled joint walls and a restored aerodynamic profile, are the focus of this work. The failure mechanisms of these structures were examined under quasi-static tensile and fully-reversed cyclic loading. While the scarf ratio was held constant at 1:50, the repair layup was varied between large-to-small and small-to-large. The effect of the presence of resin pockets and the fiber orientation mismatch between parent and repair material on the restored strength of BIAX ±45° glass fiber reinforced polymer scarf joint structures was studied. T2 - 20th European Conference on Composite Materials CY - Lausanne, Switzerland DA - 26.06.2022 KW - Fatigue KW - Scarf repairs KW - Glass fiber reinforced polymers PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-569646 UR - https://infoscience.epfl.ch/record/298799 SN - 978-2-9701614-0-0 VL - Vol. 5 - Applications and structures SP - 195 EP - 201 PB - Composite Construction Laboratory (CCLab) CY - Lausanne AN - OPUS4-56964 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Sachs, Patrick ED - Vassilopoulos, A. P. ED - Michaud, V. T1 - Dynamic mechanical analysis of epoxy-matrix cross linking measured in-situ using an elastomer container T2 - Composites meet sustainability - Proceedings of the 20th European conference on composite materials, ECCM20, 26-30 June, 2022, Lausanne, Switzerland N2 - A new patented dynamic mechanical analysis (DMA) is presented, where the tensile, bending- or torsional stiffness of a media can be characterized in-situ during the phase transition from liquid to solid. An epoxy system, e.g. Hexion L285/H287, is filled into an elastomer container, such as a silicone tube. This can be mounted into a conventional OMA and, based on a linear viscoelastic approach, the storage modulus (E';G'), the loss modulus (E'';G'') and the loss angle tan(δ) can be measured at constant temperature as a function of time in order to investigate the liquid to sol-gel to solid transition. With this new method, the stiffness increase as a result of the cure process can be directly measured more precisely than with a rheometer in a shear plate set-up, because using an elastomer container gives a defined cross section for calculating the Young's modulus. T2 - 20th European Conference on Composite Materials CY - Lausanne, Switzerland DA - 26.06.2022 KW - Cross linking KW - Dynamic mechanical analysis (DMA) KW - Thermoset polymers KW - Cure process PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-569651 UR - https://infoscience.epfl.ch/record/298799 SN - 978-2-9701614-0-0 VL - Vol. 5 - Applications and structures SP - 181 EP - 186 PB - Composite Construction Laboratory (CCLab) CY - Lausanne AN - OPUS4-56965 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Azevedo do Nascimento, A. A1 - Trappe, Volker A1 - Diniz Melo, J. D. A1 - Cysne Barbosa, A. P. T1 - Fatigue behavior of self-healing glass fiber/epoxy composites with addition of poly (ethylene-co-methacrylic acid) (EMAA) JF - Polymer Testing N2 - The interest in repair technologies for polymer composites has increased significantly over the last decades, due to the growing use of these materials in structural applications. In this study, poly (ethylene-co-methacrylic acid) (EMAA) was used as self-healing agent to glass fiber/epoxy composite. Materials with EMAA contents of 2 wt% and 5 wt% were manufactured using Resin Transfer Molding (RTM) and the effects of the healing agent on the properties were investigated using tensile tests and Dynamic Mechanical Analysis (DMA). Results show slight variation of properties, which was more pronounced as the content of EMAA increased. In addition, the healing efficiency was investigated through fatigue tests and the addition of higher content of EMAA increased the number of cycles to failure after the healing activation cycle. KW - Fatigue KW - Glass fiber-epoxy composites KW - Self-healing KW - Smart materials PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-569661 DO - https://doi.org/10.1016/j.polymertesting.2022.107863 SN - 0142-9418 VL - 117 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-56966 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Cysne Barbosa, Ana Paula A1 - Azevedo do Nascimento, Allana A1 - Pavasarytė, Lina A1 - Trappe, Volker A1 - Melo, D. T1 - Effect of addition of thermoplastic self-healing agent on fracture toughness of epoxy T2 - Proceedings of 6th Brazilian Conference on Composite Materials N2 - Self-healing agents have the potential to restore mechanical properties and extend service life of composite materials. Thermoplastic healing agents have been extensively investigated for this purpose in epoxy matrix composites due to their strong adhesion to epoxy and their ability to fill in microcracks. One of the most investigated thermoplastic additives for this purpose is poly(ethylene-co-methacrylic acid) (EMAA). Despite the ability of thermoplastic healing agents to restore mechanical properties, it is important to assess how the addition of thermoplastic healing agents affect properties of the original epoxy material. In this work, EMAA was added to epoxy resin and the effect of the additive on fracture toughness of epoxy was evaluated. Results indicate that although added in low concentrations, EMAA can affect fracture toughness. T2 - 6th Brazilian Conference on Composite Materials CY - Tiradentes, Minas Gerais, Brazil DA - 14.08.2022 KW - Epoxy KW - Self-healing KW - Thermoplastic KW - Fracture PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-572707 SN - 978-65-00-49386-3 DO - https://doi.org/10.29327/566492 SN - 2316-1337 SP - 219 EP - 222 AN - OPUS4-57270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kalinka, Gerhard T1 - Optische Beobachtungen der Faser-Matrix-Trennung im Pull-out-Versuch N2 - Der Vortrag behandelt Rissentstehung und Ausbreitung an Faser-Matrix-Interfaces, untersucht mit dem optischen Mikroskop. T2 - Composites United, CU-Arbeitsgruppe/n Faser-Matrix-Haftung & Matrices CY - Online meeting DA - 02.12.2021 KW - Faser KW - Matrix KW - Pull-out KW - Interface PY - 2021 AN - OPUS4-53968 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker T1 - Current and future technological advancement in polymer matrix composites enabled through fundamental discoveries N2 - This presentation is a summary of the work from the past 20 years’ development of PMC-testing at the BAM-FB 5.3 with respect to safety-relevant design of advanced light weight structures in aircraft, wind turbine and automotive applications. The talk begins with wood as an example from nature, and emphasizes that load case, fiber architectural design and the production process and quality have to go hand in hand to generate an advanced light weight structure. Since PMC-relevant basic findings of mankind span across hundreds of years, high-performance composite applications today are based more on long term experiences than on breakthrough inventions of modern days. In the second part of the talk, future plans and projects of FB-5.3 are presented, specifically addressing H2-safety, circular economy, recycling by design and digitalization of PMC-technologies. T2 - Abteilungsseminar CY - Online meeting DA - 07.09.2021 KW - Polymer Matrix Composites KW - Thermo mechanical fatigue PY - 2021 AN - OPUS4-54150 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker T1 - Beschreibung des Ermüdungsverhaltens von Endlos-Faserverstärkten-Kunststoff-Verbunden mit Hilfe mikromechanischer Modelle N2 - Im Rahmen des Vortrags werden die neusten Ergebnisse aus dem Fachbereich 5.3 zur Beschreibung des Ermüdungsverhaltens von FKV mittels Mikromechanischer-Modelle präsentiert. Explizit wird der theoretische Ansatz am Beispiel von GFK unter thermomechanischer Beanspruchung hergeleitet und an Hand von Versuchsergebnissen verifiziert. T2 - Webkonferenz Composites United, Composite Fatigue CY - Online meeting DA - 30.09.2021 KW - Faser-Kunststoff-Verbunde KW - thermomechanische Beanspruchung KW - Materialmodell PY - 2021 AN - OPUS4-54151 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Umgebungsbedingter Spannungsriss: Gefahr für Kunststoffbauteile unter Medieneinfluss N2 - Polyethylen hoher Dichte (PE-HD) ist ein weit verbreitetes Material für Transportbehälter, die oft für eine längere Nutzungsdauer vorgesehen sind. Insbesondere in diesem Fall können mikroskopische Schäden im Material auch weit unterhalb der Streckgrenze auftreten, die durch eine Spannungskonzentration verursacht werden, deren Ursprung in intrinsischen Materialfehlern oder äußeren Kratzern liegt. Mit fortschreitender Schädigung bilden sich Rissstrukturen, die von verstreckten Fibrillen aufgespannt werden, bis es zum Versagen dieser Fibrillen kommt und sich der Riss ausbreitet. Dieser Schadensmechanismus des langsamen Risswachstums kann durch eine Vielzahl von Umgebungsmedien beschleunigt werden und wird dann als "environmental stress cracking" (ESC) bezeichnet. Eine international normierte Methode zur Validierung der Spannungsrissbeständigkeit von PE-HD Materialien ist der „Full Notch Creep Test“ (FNCT). Anhand von Bruchflächenauswertungen mittels Rasterelektronenmikroskopie und Laser-Scanning-Mikroskopie, werden die typischen Schädigungsstrukturen des ESC sichtbar. Die fibrillierten Strukturen des ESC auf der Bruchfläche von PE-HD ergeben sich besonders bei oberflächenaktiven wässrigen Umgebungsmedien. In Lösungsmittel-Umgebungsmedien, im Zusammenspiel mit PE-HD, kommt es aufgrund der plastifizierenden Wirkung zur Herabsetzung der Streckspannung und Bruchflächen aus dem FNCT veranschaulichen keine signifikanten Anzeichen des Schädigungsmechanismus ESC. T2 - 47. VDI-Jahrestagung Schadensanalyse 2021- Mediale und klimatische Beanspruchung von polymeren Produkten CY - Würzburg, Germany DA - 06.10.2021 KW - Umgebungsbedingter Spannungsriss KW - Polyethylen hoher Dichte KW - Full Notch Creep Test KW - Lösungsmittel KW - Oberflächenaktive wässrige Medien KW - Bruchflächenauswertung PY - 2021 AN - OPUS4-53665 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gebhardt, M. A1 - Malolakis, I. A1 - Kalinka, Gerhard A1 - Deubener, J. A1 - Chakraborty, S. A1 - Meiners, D. T1 - Re-use potential of carbon fibre fabric recovered from infusible thermoplastic CFRPs in 2nd generation thermosetting-matrix composites JF - Composites Communications N2 - The research presented here attempts to assess the potential for re-using carbon fibre (CF) fabrics recovered from recycling infusible acrylic thermoplastic carbon fibre reinforced polymer composites (CFRPs) in a universal manner, i.e. by combining with a wide variety of matrices to manufacture 2nd generation composite laminates by resin infusion. The 2nd generation composites have been compared in terms of bulk and interfacial properties against counteparts processed with virgin carbon fibre fabric infused with the same matrices. Generally, an increase in damping (tanδ) was observed in all 2nd generation composites, which can be attributed to a residual thin thermoplastic layer present on the recovered fibres. The interfacial adhesion of the 2nd generation Composites was investigated by shear tests and scanning electron micsoscopy, and also appears to be less influenced by the type of matrix. KW - Composite recycling KW - Thermoplastic matrix KW - Thermosetting resin KW - Fibre/matrix bonding PY - 2021 DO - https://doi.org/10.1016/j.coco.2021.100974 VL - 28 SP - 100974 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-53639 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Kraus, David T1 - Thermo-mechanical fatigue of glass fiber reinforced polymer N2 - Glass fiber reinforced polymer (GFRP) materials in practical applications have to endure cyclic mechanical loading in a wide temperature range (e.g. aircraft applications, automotive, wind turbine blades). In this study the static strength and fatigue behavior of GFRP was investigated in a temperature range from 213 K to 343 K. Therefor the coefficients of thermal expansion of the composite as well as the matrix are measured in this temperature interval. The inverse laminate theory was extended and used to calculate the inter fiber-failure effort for a virtual UD-layer according to the layer wise strength approach. The experimentally determined results are compared with the micro-mechanical model according to Krimmer, which has been enhanced to include the effect of temperature and fiber-perpendicular failure modes. A correlation between matrix effort, the dilatational strain energy of the matrix and the damage state of the specimen is demonstrated. It is shown that a fatigue life assessment can be performed with the aid of a temperature-independent master fatigue curve, as it was similar done for the fatigue behavior of CFRP and GFRP to very high load cycles at room temperature. T2 - ICFC8 - The 8th International Conference on the Fatigue of Composites CY - Online meeting DA - 23.06.2021 KW - Glass fibre reinforced plastics KW - Fatigue KW - Thermo-mechanical-loading PY - 2021 AN - OPUS4-52910 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Niebergall, Ute A1 - Marschall, Niklas A1 - Alig, I. A1 - Böhning, Martin T1 - A phenomenological criterion for an optical assessment of PE-HD fracture surfaces obtained from FNCT JF - Polymer Testing N2 - The full-notch creep test (FNCT) is a common test method to evaluate the environmental stress cracking (ESC) behavior of high-density polyethylene (PE-HD), e.g. for container materials. The test procedure as specified in ISO 16770 provides a comparative measure of the resistance against ESC using the time to failure of PE-HD specimens under constant mechanical load in a well-defined liquid test environment. Since the craze-crack damage mechanism underlying the ESC phenomenon is associated with brittle failure, the occurrence of a predominantly brittle fracture surface is a prerequisite to consider an FNCT measurement as representative for ESC, i.e. a time to failure dominated by craze-crack propagation. The craze-crack propagation continuously reduces the effective residual cross-sectional area of the specimen during the test, which results in a corresponding increase of the effective mechanical stress. Thus, a transition to ductile shear deformation is inevitable at later stages of the test, leading usually to a pronounced central ligament. Therefore, an optical evaluation of FNCT fracture surfaces concerning their brittleness is essential. An enhanced imaging analysis of FNCT fracture surfaces enables a detailed assessment of craze-crack Propagation during ESC. In this study, laser scanning microscopy (LSM) was employed to evaluate whether FNCT fracture surfaces are representative with respect to craze-crack propagation and ESC. Based on LSM height data, a phenomenological criterion is proposed to assess the validity of distinct FNCT measurements. This criterion is supposed to facilitate a quick evaluation of FNCT results in practical routine testing. Its applicability is verified on a sample basis for seven different commercial PE-HD container materials. KW - Environmental stress cracking (ESC) KW - Full notch creep test (FNCT) KW - Laser scanning microscopy (LSM) KW - Fracture surfaces KW - Optical criterion of brittleness PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-521012 DO - https://doi.org/10.1016/j.polymertesting.2020.107002 VL - 94 SP - 107002 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-52101 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - THES A1 - Kraus, David T1 - Ermüdungsverhalten von Glasfaser-Kunststoff-Verbunden unter thermomechanischer Beanspruchung T2 - BAM-Dissertationsreihe N2 - Die Werkstoffgruppe der Faser-Kunststoff-Verbunde (FKV) hat sich aufgrund ihrer hervorragenden Leichtbaueigenschaften unter anderem im Sportgerätebau, in der Luft- und Raumfahrt und in der Windenergieindustrie etabliert. Die so hergestellten Strukturen sind in der Regel nicht nur mechanischen Belastungen, sondern auch thermischen Lasten in einem breiten Temperaturspektrum ausgesetzt. Dennoch ist die Auswirkung des Temperatureinflusses bei einer Kombination von thermischer und mechanischer Last auf die Lebensdauer von Strukturen aus FKV bisher nur wenig untersucht. Im Rahmen dieser Arbeit wird der Einfluss von Temperaturen zwischen 213 K und 343 K auf einen Glasfaser-Epoxidharz-Verbund experimentell untersucht. Das Material wird in diesem Temperaturbereich eingehend charakterisiert: Es werden sowohl die thermomechanischen Eigenschaften von Faser- und Matrixwerkstoff als auch die des Verbundes ermittelt. In einem weiteren Schritt wird dann der Einfluss der Temperatur auf die Schädigungsentwicklung im quasi-statischen Lastfall sowie unter schwingender Ermüdungsbeanspruchung bei verschiedenen FKV-Mehrschichtverbunden analysiert. Basierend auf den experimentellen Daten wird ein Zusammenhang zwischen der Schädigung und der Anstrengung der Matrix innerhalb der Einzelschicht demonstriert. Die Matrixanstrengung wird mithilfe eines mikromechanischen Modells unter Berücksichtigung der thermomechanischen Eigenspannungen analytisch berechnet. Bei Querzugbeanspruchung kann gezeigt werden, dass eine Vorhersage der Schädigung in Abhängigkeit der Volumenänderungsenergie innerhalb der Matrix getroffen werden kann. Mithilfe des Konzepts der Matrixanstrengung ist eine Vorhersage der Lebensdauer des Werkstoffs unter schwingender Ermüdungsbeanspruchung in Abhängigkeit der Einsatztemperatur möglich. N2 - Due to their superior lightweight properties, fiber reinforced polymer (FRP) materials are well established in various fields, such as sports equipment, aerospace or wind energy structures. These structures are not only subjected to mechanical loads, but also to a broad spectrum of thermal environments. However, the impact of temperature on the fatigue life of thermomechanically loaded FRP structures is barely investigated to-date. In the scope of this work, the influence of temperatures in a range of 213 K to 343 K on a glass fiber reinforced epoxy polymer is experimentally examined. An extensive thermo-mechanical characterization of the static properties of the material is performed. The neat resin and Fiber material are investigated, as well as the composite. In addition, the impact of thermal loads on the damage evolution under quasi-static as well as cyclic fatigue loading is investigated for different multi-angle laminates. Based on the experimental data, a correlation is shown between damage and matrix effort of the unidirectional layer. The matrix effort is calculated according to a micromechanical model considering thermal residual stresses. Particularly under transverse loading, the damage Evolution can be predicted as a function of the dilatational strain energy of the matrix. Using the concept of the matrix effort presented in this work, a prediction of the fatigue life of the investigated material at different ambient temperature conditions can be performed. T3 - BAM Dissertationsreihe - 169 KW - Ermüdung KW - Faser-Kunststoff-Verbund KW - GFK KW - Schädigung KW - Thermomechanik KW - Fatigue KW - Composite KW - Glas fibre reinforced polymer KW - Damage KW - Thermomechanics PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-530253 SN - 1613-4249 VL - 169 SP - 1 EP - 164 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-53025 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Influence of molecular orientation on the environmental stress cracking resistance N2 - Molecular orientation has a significant effect on the material properties of polymers. Preferential orientation of the microstructure (polymer chains or crystallites) in a specific direction or plane often enhances the material properties, especially if the high-strength covalent bonds are primarily exposed to loads instead of the weaker van der Waals bonds. However, the orientation-dependent microstructure and its mechanical behavior is in general already well understood by many scientific studies [1-3]. Isotropic materials are frequently required for an intrinsic material characterization without prevailing processing-induced properties, as is the case for Full Notch Creep Test (FNCT) [4] addressing environmental stress cracking (ESC) in high-density polyethylene (PE-HD) [5, 6]. Since ESC is one of the major limiting issues for long-term performance of PE-HD pipes and containers [7], which in contrast have a production-related preferential orientated microstructure due to extrusion or extrusion blow molding, it is important to additionally investigate the ESC resistance of such anisotropic microstructure. Investigations of the slow crack growth (SCG) with respect to the molecular orientation generally obtain a factor of 1.2 up to 4.7 between crack growth perpendicular to the extrusion direction and crack growth parallel to the extrusion direction 8. Based on FNCT investigations with an aqueous detergent solution as environmental medium, hot pressed sheets with isotropic morphology are compared with extruded sheets from which specimens with different orientation angles are taken. However, the time to failure obtained by FNCT is also significantly influenced by the different cooling conditions under which the final morphology is formed. The tendency of the specimen to fail due to ESC is investigated as a function of environmental medium temperature. For a more detailed analysis of the affecting parameters in the manufacturing process, the ESC resistance is discussed considering the differences in crystallinity as revealed by thermal analysis. T2 - 36th International Conference of the Polymer Processing Society CY - Montreal, Canada DA - 26.09.2021 KW - Environmental stress cracking KW - Orientation-dependent microstructure KW - High-density polyethylene KW - Full Notch Creep Test PY - 2021 AN - OPUS4-53399 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Damage progression of environmental stress cracking affected by manufacturing process-induced microstructural orientation N2 - Currently, the Full Notch Creep Test (FNCT) [1] method is used by material suppliers and end users in industry for the approval of container and pipe materials based on high-density polyethylene (PE-HD). The resistance to environmental stress cracking (ESC) of the material is evaluated using the time to failure of the specimen in an aqueous solution of a detergent [2, 3]. Usually specimens made of sheets with isotropic material properties, manufactured by hot pressing, are employed in order to obtain intrinsic properties of the material in terms of ESC failure. In contrast, the processes used in manufacturing to form containers and pipes, such as extrusion blow molding or extrusion, impose anisotropic properties to the material. These are mostly due to a microstructural orientation (polymer chains or crystallites) [4]. Furthermore, the different cooling conditions significantly affect the size distribution of crystallites as well as the overall morphology. It is therefore essential to understand the influence of process-induced material characteristics on failure due to ESC. A large number of studies on material properties as a function of microstructural preferential orientation have already been conducted [5-7]. However, effects on ESC as the major failure mechanism of containers and pipes are still rather unexplored [8, 9]. The most important factor is whether primarily intramolecular high-strength covalent bonds or the substantially weaker intermolecular van der Waals forces are predominantly loaded. In addition to the widely established classification by time to failure, the strain or crack opening displacement (COD) provides valuable information about the evolution and progression of damage as a function of time [10, 11]. Optical strain measurement using digital image correlation allows the differences in COD for isotropic and different angles of orientation of anisotropic specimens to be discussed. Also, a post-fracture surface analysis provides clarification on the craze-crack mechanism of the ESC. These different ESC-related properties of extruded and hot-pressed specimens have been investigated at different environmental medium temperatures and different initial stresses to provide a broad characterization of the fracture behavior of PE-HD. T2 - 36th International Conference of the Polymer Processing Society CY - Montreal, Canada DA - 26.09.2021 KW - Environmental stress cracking KW - High-density polyethylene KW - Fracture behavior KW - Microstructural orientation PY - 2021 AN - OPUS4-53400 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gebhardt, M. A1 - Manolakis, I. A1 - Chatterjee, A. A1 - Kalinka, Gerhard A1 - Deubener, J. A1 - Pfnür, H. A1 - Chakraborty, S. A1 - Meiners, D. T1 - Reducing the raw material usage for room temperature infusible and polymerisable thermoplastic CFRPs through reuse of recycled waste matrix material JF - Composites Part B: Engineering N2 - In this work, a closed loop recycling process is investigated, which allows polymerised bulk thermoplastic matrix (Elium 150) from production waste (also referred to as recyclate) to be reused as additive in composite manufacturing by vacuum assisted resin infusion (VARI) of virgin Elium 150 monomer. It is shown that this process can save up to 7.5 wt% of virgin material usage in each processing cycle. At the same time, the thermal stability and stiffness of the composite increases with the proportion of recyclate introduced. Contemporarily, the shear and bending properties have also been observed to improve. Gel permeation chromatography (GPC) showed that the changes observed are due to an increase in molecular weight with the recyclate content. In particular, a correlation between the molecular weight and the shear properties of the composite was discovered using single fibre push-out tests. KW - Mechanical properties KW - Recycling KW - Carbon fibres KW - Fibre/matrix bond PY - 2021 DO - https://doi.org/10.1016/j.compositesb.2021.108877 SN - 1359-8368 VL - 216 SP - 108877 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-52711 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - The effect of fiber orientation mismatch on scarf joint damage mechanisms under fatigue load N2 - Wind turbine rotor blades commonly fail before their projected 20-year lifespan largely due to defects that originate during manufacturing and are propagated by operational fatigue and environmental conditions. The cost-intensive replacement outcomes lead to a high loss of earnings, and are one of the inhibitors of wind turbine production. A potential repair alternative to restoring the mechanical properties of such lightweight fiber reinforced polymer (FRP) structures is to locally patch these areas with scarf joints. This type of repair allows for a smoother load distribution across the joint, and is favored especially on structures where minor aerodynamic contour changes are key. The effects of such repairs on the structural integrity, however, is still largely unknown. Building upon an understanding of the static load failure mechanism of GFRP scarf joints, presented at the ICCS23 Joint Event in 2020, the influence of the fiber orientation mismatch between parent and repair materials of 1:50 scarf joints on the failure mechanism of monolithic glass FRP specimens under cyclic fatigue load were examined in this study. Specimens with various layups were produced with the vacuum-assisted resin infusion (VARI) process using biaxial E-glass non-crimp fabric (NCF). The patch layers were then joined directly to the parent structure with the VARI using biaxial E-glass NCF with half the areal weight of the parent side to allow for better drapability. This mimics the soft-to-hard patch style utilized in wind turbine blade shell field repairs. The specimens were tested under uniaxial fatigue load, during which they were periodically monitored for damage onset. A comparison of the +45/-45° and 0/90° layups allowed for an understanding of the role of a highly mismatching fiber orientation in the transition zone between parent and patch material on the failure mechanism of the scarf joint. In addition to the tensile strength and stiffness property recovery assessment, a grayscale analysis using in-situ camera images determined the damage state leading to failure in each region across the scarf joint, which varied in the parent material versus scarf joint region, providing insight to the critical regions in this composite structure under cyclic loading. T2 - ICCS24 - 24th International Conference on Composite Structures CY - Online meeting DA - 14.06.2021 KW - Glass fiber reinforced polymers KW - Scarf repairs KW - Damage mechanisms PY - 2021 AN - OPUS4-52817 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kraus, David A1 - Trappe, Volker T1 - Transverse damage in glass fiber reinforced polymer under thermo-mechanical loading JF - Composites Part C N2 - In this study, the thermomechanical damage behavior of a glass fiber reinforced polymer material is investigated. The coefficients of thermal expansion of the composite as well as the matrix are measured in a wide temperature range. Quasi-static experiments with neat resin, unidirectional and multidirectional laminates are performed as well as fatigue experiments in a temperature range from 213 K to 343 K. This study focusses on the matrix damage due to fiber-parallel loading. A correlation between matrix effort, the dilatational strain energy of the matrix and the damage state of the specimen is demonstrated. It is shown that a fatigue life assessment can be performed with the aid of a temperature-independent master fatigue curve. KW - Composite KW - Glass fiber reinforced polymer KW - Thermo-mechanics KW - Fatigue KW - Damage KW - Temperature PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-527462 DO - https://doi.org/10.1016/j.jcomc.2021.100147 SN - 2666-6820 VL - 5 SP - 100147 PB - Elsevier B.V. AN - OPUS4-52746 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Oehler, H. A1 - Alig, I. A1 - Böhning, Martin T1 - Evaluation of the damaging effect of crop protection formulations on high density polyethylene using the Full Notch Creep Test JF - Polymer N2 - Four typical high-density polyethylene container materials were used to investigate damage or stress cracking behavior in contact with model liquids for crop protection products. These model liquids are established in German regulations for the approval of dangerous goods containers and consist of typical admixtures used for crop protection products but without biological active ingredients. This study is performed with the standardized method of Full Notch Creep Test, adapting the media temperature to 40 °C according to the usual conditions where these test liquids are applied. The two model liquids differ into a water-based solution and a composition based on different organic solvents which are absorbed by the material up to significant levels. Therefore, extensive sorption measurements are performed. The fracture surfaces obtained are analyzed in detail not only by light microscopy, but also by laser scanning microscopy as well as scanning electron microscopy. Influence of pre-saturation and applied stress are addressed by respective systematic series of experiments. KW - Polyethylene KW - Full Notch Creep Test KW - Environmental Stress Cracking KW - Fracture PY - 2021 DO - https://doi.org/10.1016/j.polymer.2021.123853 SN - 0032-3861 VL - 228 SP - 123853 PB - Elsevier Ltd. AN - OPUS4-52686 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - Restoring lightweight strength - Effect of localized repairs on the mechanical properties of composites sandwich structures N2 - As a type of high-performance composite material, glass-fiber reinforced plastics (GFRP) are favored for the construction of wind turbine rotor blades due to their high specific strength and stiffness properties (Grasse et al, 2010). During the blade manufacturing process, however, imperfections are often introduced, then further propagated due to harsh environmental conditions and a variety of loads (Caminero et al, 2013; Trappe et al, 2018). This leads to failure significantly before their designed lifespan. Since replacement of entire blades can be a costly potential outcome, localized repairs of the damaged region to restore structural integrity and thus lengthen its lifespan can executed in the field by technicians accessing the blades directly by suspended roping. These methods involve replacing the lost load path with a new material that is joined to the parent structure. In recent years, considerable studies have been conducted to investigate the influence of different repair parameters on the stress distribution, ultimate strength, impact behavior, and residual stresses of bonded repaired structures [Caminero et al, 2013; Trappe et al, 2018; Shufeng et al, 2014; Harman and Rider, 2011; Ahn and Springer, 2000; Lekou and Vionis, 2002). However, there currently do not exist any standardized repair procedures for wind turbine rotor blades. Namely, there is a lack of understanding about the effects of the layup of various repair methods, especially on the damage mechanism and fatigue life of the shells of rotor blades (Caminero et al, 2013; Trappe et al, 2018). This work therefore aims to begin to enrich this knowledge gap by testing the influence of different variables among repair patches on the mechanical properties of sandwich composite structures. Manufactured with the vacuum-assisted resin infusion (VARI) process, the test specimens are produced as a GFRP structure to represent the outer shell portion of a wind turbine blade, then repaired with a scarf joint. Scarf repairs are favored as the most efficient of the common structural joints, as the removal of the damaged area with angled walls leads to a nearly uniform shear stress distribution along the bond surface and no eccentricity in the load distribution (Caminero et al, 2013; Lekou and Vionis, 2002; Siener, 1992). The performance of specific layup methods of repair patches, namely a large-to-small versus small-to-large scheme of repair layers, is studied with static and load-controlled fatigue testing, then compared to pristine test specimens as well as to each other in terms of mechanical property restoration. The transition layer between repair and parent material is especially of interest in the performance of the structure. Damage onset, crack development and eventual failure are monitored in-situ with non-destructive testing methods, including thermography with an infrared camera system and a 3D deformation analysis system, to develop a more robust understanding of the effects of these repair concept variables on wind turbine blade shell structures. T2 - Wind Energy Science Conference CY - Online Meeting DA - 25.05.2021 KW - Glass fiber reinforced polymers KW - Wind turbine blade shell structures KW - Scarf joint repair PY - 2021 AN - OPUS4-52687 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Plichta, T. A1 - Sirjovona, V. A1 - Zvonek, M. A1 - Kalinka, Gerhard A1 - Cech, V. T1 - The Adhesion of Plasma Nanocoatings Controls the Shear Properties of GF/Polyester Composite JF - Polymers N2 - High-performance fibre-reinforced polymer composites are important construction materials based not only on the specific properties of the reinforcing fibres and the flexible polymer Matrix but also on the compatible properties of the composite interphase. First, oxygen-free (a-CSi:H) and oxygen-binding (a-CSiO:H) plasma nanocoatings of different mechanical and tribological properties were deposited on planar silicon dioxide substrates that closely mimic E-glass. The nanoscratch test was used to characterize the nanocoating adhesion expressed in terms of critical normal load and work of adhesion. Next, the same nanocoatings were deposited on E-glass fibres, which were used as reinforcements in the polyester composite to affect its interphase properties. The shear properties of the polymer composite were characterized by macro- and micromechanical tests, namely a short beam shear test to determine the short-beam strength and a single fibre push-out test to determine the interfacial shear strength. The results of the polymer composites showed a strong correlation between the short-beam strength and the interfacial shear strength, proving that both tests are sensitive to changes in fibre-matrix adhesion due to different surface modifications of glass fibres (GF). Finally, a strong correlation between the shear properties of the GF/polyester composite and the adhesion of the plasma nanocoating expressed through the work of adhesion was demonstrated. Thus, increasing the work of adhesion of plasma nanocoatings from 0.8 to 1.5 mJ·m−2 increased the short-beam strength from 23.1 to 45.2 MPa. The results confirmed that the work of adhesion is a more suitable parameter in characterising the level of nanocoating adhesion in comparison with the critical normal load. KW - Mechanical properties KW - Plasma nanocoatings KW - Glass fibre KW - Polymer composite KW - Short-beam strength KW - Interfacial shear strength KW - Work of adhesion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-521844 DO - https://doi.org/10.3390/polym13040593 VL - 13 IS - 4 SP - 593 PB - MDPI CY - Basel,Schweiz AN - OPUS4-52184 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ghafafian, Carineh A1 - Popiela, Bartosz A1 - Trappe, Volker T1 - Failure Mechanisms of GFRP Scarf Joints under Tensile Load JF - Materials N2 - A potential repair alternative to restoring the mechanical properties of lightweight fiberreinforced polymer (FRP) structures is to locally patch these areas with scarf joints. The effects of such repair methods on the structural integrity, however, are still largely unknown. In this paper, the mechanical property restoration, failure mechanism, and influence of fiber orientation mismatch between parent and repair materials of 1:50 scarf joints are studied on monolithic glass fiber-reinforced polymer (GFRP) specimens under tensile load. Two different parent orientations of [-45/+45]2S and [0/90]2S are exemplarily examined, and control specimens are taken as a baseline for the tensile strength and stiffness property recovery assessment. Using a layer-wise stress analysis with finite element simulations conducted with ANSYS Composite PrepPost to support the experimental investigation, the fiber orientation with respect to load direction is shown to affect the critical regions and thereby failure mechanism of the scarf joint specimens. KW - Scarf joint KW - Glass fiber reinforced polymers KW - Failure mechanisms PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-523952 DO - https://doi.org/10.3390/ma14071806 VL - 14 IS - 7 SP - 1806 PB - MDPI CY - Basel, Switzerland AN - OPUS4-52395 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Taketa, I. A1 - Kalinka, Gerhard A1 - Gorbatikh, L. A1 - Lomov, S. A1 - Verpoest, I. T1 - Influence of cooling rate on the properties of carbon fiber unidirectional composites with polypropylene, polyamide 6, and polyphenylene sulfide matrices JF - Advanced composite materials N2 - The longitudinal and transverse strength of three unidirectional thermoplastic prepreg systems: carbon fiber/polypropylene (CF/PP), polyamide 6 (CF/PA6), and polyphenylene sulfide (CF/PPS) are studied and analytical formulas are proposed for the estimation of matrix and fiber/matrix interface properties from composites properties. Since the matrices are semi-crystalline thermoplastics, the influence of cooling rate on the strength is statistically evaluated. While the 0° tensile strength is found to be independent of the cooling rate, the 90° tensile strength is strongly influenced by the matrix type and cooling rate. The matrix modulus increases as the cooling rate is decreased; the degree of crystallinity also increases. The matrix residual stress, interfacial shear strength, and mode II interlaminar fracture toughness are also found to depend on the cooling rate, with the trends different for different matrices. KW - Matrix residual stress KW - Thermoplastic prepreg KW - Unidirectional composites KW - Cooling rate KW - Interfacial strength PY - 2020 DO - https://doi.org/10.1080/09243046.2019.1651083 SN - 0924-3046 SN - 1568-5519 N1 - Die originale japanische Version des Artikels erschien in: Journal of the Japan Society for Composite Materials, Jg. 44, Nr. 4 (2018), S. 123-128. - The original Japanese version of the article was published in: Journal of the Japan Society for Composite Materials, vol. 44, no. 4 (2018), pp. 123-128. VL - 29 IS - 1 SP - 101 EP - 113 PB - Taylor & Francis CY - London AN - OPUS4-45433 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Evolution of CFRP stress cracks observed by in situ X-ray refractive imaging N2 - Modern air-liners and rotor blades of wind turbines are basically made of fiber reinforced plastics (FRP). Their failure heavily impairs the serviceability and the operational safety. Consequently, knowledge of the failure behavior under static and cyclic loads is of great interest to estimate the operational strength and to compare the performance of different materials. Ideally, the damage evolution under operational load is determined with in-situ non-destructive testing techniques. Here, we report on in-situ synchrotron X-ray imaging of tensile stress induced cracks in carbon fiber reinforced plastics (CFRP) due to inter fiber failure. An in-house designed compact-tensile testing machine with a load range up to 15 kN was integrated into the beam path. Since conventional radiographs do not reveal sufficient contrast to distinct cracks due to inter fiber failure and micro cracking from fiber bundles, the Diffraction Enhanced Imaging technique (DEI) is applied in order to separate primary and scattered (refracted) radiation by means of an analyzer crystal. In the laboratory, scanning X-ray refraction topography of CFRP has been applied long before but it comes along with several disadvantages: the long total measuring time hampers real time (in-situ) measurements and the required small beam size hinders end-to-end imaging. The introduced technique overcomes both drawbacks. Imaging and tensile test rig are run unsynchronized at the greatest possible frame rate (0.7 s-1 at 28.8 µm pixel size) and smallest possible strain rate (5.5∙10-4 s-1). For 0°/90° non-crimped fabrics (ncf) the first inter fiber cracks occurred at 380 MPa (strain 0.7 %). Prior to failure at about 760 MPa (strain 2.0 %) we observe the evolution of a nearly equidistant 1 mm grid of cracks running across the entire sample in the fully damaged state before total failure. T2 - 41st Risø International Symposium on Materials Science - Materials and Design for Next Generation Wind Turbine Blades CY - Online meeting DA - 07.09.2020 KW - X-ray refraction KW - Diffraction Enhanced Imaging KW - Carbon Fiber Reinforced Plastics KW - In situ tensile test KW - Crack evolution PY - 2020 AN - OPUS4-51223 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - THES A1 - Schilling, Markus T1 - Environmental Stress Cracking (ESC) and Slow Crack Growth (SCG) of PE-HD induced by external fluids N2 - High-density polyethylene (PE-HD) is widely used as a packaging material. Typical applications are pipes and containers for storage and transport of dangerous goods. For these applications, the understanding of the craze-crack damage mechanisms slow crack growth (SCG) and environmental stress cracking (ESC) is of importance. Since these mechanisms are considered to be the major causes of failure, their understanding is essential for inspection and release of those materials. A well-established test method for the assessment of these damage mechanisms is the full-notch creep test (FNCT). It is used in this study for a detailed investigation of crack propagation phenomena in PE-HD container materials under the influence of different fluids such as air, water and aqueous detergent solutions (Arkopal N 100) as well as biodiesel and diesel. Based on the results of the FNCT, a classification scheme of different fluids is proposed, which allows for an assignment of the respective damage mechanisms. Hereby, it is differentiated between (i) inert, (ii) purely surface-active and (iii) additionally sorptive, bulk-active fluids with respect to SCG. If the test fluid changes the intrinsic properties (at the surface or in the bulk), the damage mechanism is addressed to ESC behavior. In FNCT investigations, stress, temperature and specimen geometry were varied systematically. In addition to the time to failure as common measure for the resistance of a PE-HD type against crack propagation, specimen elongation was considered in detail. Several imaging techniques were applied for fracture surface analysis of specimens tested in FNCT to gain novel information on SCG and ESC behavior. From height profiles obtained by laser scanning microscopy (LSM) and information on surface structures from scanning electron microscopy (SEM), indicators for the differentiation of the crack propagation mechanisms could be derived. Based on the LSM data, an algorithm for the distinction between ductile shear deformation and brittle crack growth as dominating failure mechanism was developed. Imaging techniques were also used for determination of crack propagation rates, which were related to time-resolved FNCT elongation data. From the time-resolved determination of crack lengths of partly damaged FNCT specimens, an increasing length of craze zone with a progressively propagating crack was revealed for the first time. This relation of crack and craze zones was specified by fracture mechanical considerations. N2 - Polyethylen hoher Dichte (PE-HD) wird als Werkstoff für Rohre und Behälter für den Transport und zur Lagerung von Gefahrgütern verwendet. Für die Beurteilung und technische Freigabe dieser Materialien ist das Verständnis der beiden Schädigungsmechanismen „langsames Risswachstum“ (engl.: „slow crack growth“, SCG) und „umgebungsbedingter Spannungsriss“ (engl.: „environmental stress cracking“, ESC) essentiell. Eine etablierte Prüfmethode zur Bewertung dieser Schädigungsmechanismen ist der Full-Notch Creep Test (FNCT), der in dieser Arbeit zur systematischen Untersuchung des Risswachstums in PE-HD Behältermaterialien unter Einwirkung von Luft, Wasser und wässrigen Netzmittellösungen (Arkopal N 100) sowie Biodiesel und Diesel verwendet wird. Aus den Ergebnissen des FNCT wird ein Klassifikationsschema für Fluide vorgeschlagen, welches ebenfalls eine Zuordnung zu den Schädigungsmechanismen erlaubt. Hierbei wird in (i) inerte, (ii) rein oberflächen-aktive und (iii) zusätzliche sorptive, volumen-aktive Fluide hinsichtlich des langsamen Risswachstums (SCG) unterschieden. Wenn ein Fluid lokal die intrinsischen Materialeigenschaften des Polymers verändert, wird der Schädigungsmechanismus dem umgebungsbedingten Spannungsriss (ESC) zugeordnet. Bei den FNCT-Untersuchungen wurden die mechanische Spannung, die Temperatur und die Prüfkörpergeometrie systematisch variiert. Zusätzlich zur Standzeit wurde die Prüfkörperdehnung zeitabhängig erfasst. Aus einer erweiterten Bruchflächenanalyse konnten neuartige Informationen über SCG und ESC erhalten werden. Hierzu wurden verschiedene Bildgebungsverfahren verwendet. Insbesondere wurden mit Laserscanningmikroskopie (LSM) Höhenprofile und mit Rasterelektronenmikroskopie (REM) Oberflächeninformationen zur Charakterisierung der Rissfortschrittsmechanismen erhalten. Auf Basis der LSM wurde unter Zuhilfenahme von Höhenprofildaten ein Algorithmus zur Unterscheidung zwischen duktiler Scherverformung und sprödem Risswachstum als dominierende Schädigungsmechanismen entwickelt. Die aus den bildgebenden Verfahren ermittelten Rissfortschrittsraten konnten mit den Daten der während des FNCT erfassten Dehnung der Prüfkörper in Beziehung gesetzt werden. Weiterhin wurde mithilfe von zeitaufgelösten Risslängendaten erstmals eine direkte Korrelation der Risslänge zu vorgeschädigten, fibrillierten Bereichen (Crazes) im PE-HD Prüfkörper während des FNCT nachgewiesen. Demnach vergrößert sich die Craze-Länge linear mit zunehmender Risslänge. Dieser Zusammenhang zwischen Riss- und Craze-Längen wurde auf mathematisch, bruchmechanischer Grundlage bestätigt. KW - High-density polyethylene (PE-HD) KW - Full-Notch Creep Test (FNCT) KW - Slow crack growth (SCG) KW - Environmental Stress Cracking (ESC) KW - Biodiesel KW - Diesel KW - Crack propagation analysis KW - Fracture Surface Analysis KW - Test Improvement KW - Imaging PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:tuda-tuprints-115443 DO - https://doi.org/10.25534/tuprints-00011544 SP - 1 EP - 212 CY - Darmstadt AN - OPUS4-50941 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ghafafian, Carineh A1 - Popiela, Bartosz A1 - Trappe, Volker T1 - Damage Mechanisms of Scarf Joint Repairs for Wind Turbine Rotor Blade Shell Applications N2 - Wind turbine rotor blades, made of fiber reinforced polymers (FRP), often fail before their projected 20-year lifespan, largely due to defects that originate during manufacturing and are propagated by operational fatigue and environmental conditions. The cost-intensive replacement outcomes lead to a high loss of earnings, and are one of the inhibitors of wind turbine production [1]. A potential repair alternative is to locally patch these areas of the blades with adhesively bonded structural repairs. However, the effects of such repair methods of the outer shell region on the structural integrity of the rotor blades are still largely unknown, and are thus investigated in this project. The shell components of rotor blades are made of FRP composite material sandwiching a lightweight core, often a rigid foam or Balsa wood. The repair methods involve replacing the lost load path with a new material that is joined to the parent structure [2]. Repairs in this project focus on the scarf method, which allow for a smoother load distribution across the joint, aiming to study the damage mechanism of glass FRP scarf repairs for wind turbine blade shell applications. Namely, the source and path of the damage initiation and propagation, role of the interface between parent and patch material, and the role of the fiber orientation mismatch at this interface are examined. Biaxial ±45° and 0/90° FRP specimens are produced with the vacuum-assisted resin infusion (VARI) process using E-glass non-crimp fabric. The patch layers are then joined using VARI with a scarf ratio of 1:50, using glass FRP fabric with half the areal weight of the parent side to allow for better drapability. The methods and practices in specimen production are based on common industry practice in rotor blade shell manufacturing and repairs. The specimens are tested under uniaxial tensile load, during which they are periodically monitored for damage onset. A comparison of the ±45° and 0/90° specimens allows for an understanding of the role of a highly mismatching fiber orientation in the transition zone between parent and patch material on the failure mechanism of the scarf joint. Although failure in both orientations begins as delamination at the joint edge, the difference in the mechanisms at play in the two different specimen types leads ultimately to different fracture paths. Namely, in the inter fiber failure mechanism of the ±45° specimens, the higher interlaminar strength compared to the intralaminar strength of the laminate leads to intralaminar failure of the ±45° scarf joint specimens. Alternatively, the competition in the 0/90° specimens lies between the interlaminar strength and fiber failure strength, and here we experience failure primarily across the scarf joint length. The scarf joint in the 0/90° specimens disrupts the continuity of the load-carrying 0° layers, directing the failure path to remain primarily along the scarf joint. Experimental results are compared to finite element analyses of scarf patch repairs on glass FRP sandwich specimens with the same respective layup orientations, where the damage initiation regions are identified and correlated to fiber orientation, serving as a bridge to future work which will experimentally examine the scarf repair patches on sandwich shell specimens. T2 - Joint Event: ICCS23 - 23rd International Conference on Composite Structures & MECHCOMP6 - 6th International Conference on Mechanics of Composites CY - Online meeting DA - 01.09.2020 KW - Wind turbine blade shells KW - Glass fiber reinforced polymers KW - Scarf repairs PY - 2020 AN - OPUS4-51175 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lüders, C. A1 - Kalinka, Gerhard A1 - Li, Wei A1 - Sinapius, M. A1 - Wille, T. T1 - Experimental and numerical multiscale approach to thermally cycled FRP JF - Composite Structures N2 - Due to the different thermal expansion of the constituent materials, cyclic thermal loading of FRP induces alternating stresses in the material at two scales: at the micro scale (level of fibre–matrix-interaction) and at the macro scale (level of the multidirectional laminate). Especially the micro scale effect is not comprehensively investigated yet. Additionally, computational investigations mostly neglect this effect due to the homogenous modelling of the composite material. As this effect is assumed to significantly contribute to the fatigue of FRP at thermal loads, the present paper suggests an experimental and numerical multiscale approach including Experiments at the different involved material scales to separately observe the effects acting at these scales. The approach also includes numerical modelling for each scale to complement the knowledge gained from the Experiments and to create a basis for the consideration of the micro effect even in macroscopic fatigue models treating homogeneous modelled composites. The main focus of the contribution is to bring the overall Approach up for discussion, rather than to present the multiscale modelling details. KW - Fatigue KW - Thermal cycling KW - Fibre reinforced plastic KW - Cryogenic KW - Carbon Fibre KW - Epoxy Resin PY - 2020 DO - https://doi.org/10.1016/j.compstruct.2020.112303 SN - 0263-8223 VL - 244 SP - 112303 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-50844 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -