TY - JOUR A1 - Fantin, Andrea A1 - Manzoni, Anna Maria A1 - Springer, H. A1 - Darvishi Kamachali, Reza A1 - Maaß, Robert T1 - Local lattice distortions and chemical short-range order in MoNbTaW N2 - Extended X-ray absorption fine structure (EXAFS) conducted on an equiatomic MoNbTaW bcc medium-entropy alloy that was annealed at 2273 K reveals unexpectedly small 1st and 2nd shell element-specific lattice distortions. An experimental size-mismatch parameter, δexp, is determined to be ca. 50% lower than the corresponding calculated value. Around W, short-range order (SRO) preferring 4d elements in the 1st and 2nd shells persists. A Nb-W ordering is found, which is reminiscent of ordering emerging at lower temperatures in the B2(Mo,W;Ta,Nb)- and B32(Nb,W)-phases. With high-temperature ordering preferences in fcc also foreshadowing low-temperature phase, these findings suggest a general feature of high-temperature SRO. KW - High Entropy Alloys KW - Short-range order KW - Lattice distortions KW - EXAFS PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-598164 DO - https://doi.org/10.1080/21663831.2024.2326014 SN - 2166-3831 VL - 12 IS - 5 SP - 346 EP - 354 PB - Taylor & Francis AN - OPUS4-59816 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bayerlein, Bernd A1 - Schilling, Markus A1 - von Hartrott, Philipp A1 - Waitelonis, Jörg T1 - Semantic integration of diverse data in materials science: Assessing Orowan strengthening N2 - AbstractThis study applies Semantic Web technologies to advance Materials Science and Engineering (MSE) through the integration of diverse datasets. Focusing on a 2000 series age-hardenable aluminum alloy, we correlate mechanical and microstructural properties derived from tensile tests and dark-field transmission electron microscopy across varied aging times. An expandable knowledge graph, constructed using the Tensile Test and Precipitate Geometry Ontologies aligned with the PMD Core Ontology, facilitates this integration. This approach adheres to FAIR principles and enables sophisticated analysis via SPARQL queries, revealing correlations consistent with the Orowan mechanism. The study highlights the potential of semantic data integration in MSE, offering a new approach for data-centric research and enhanced analytical capabilities. KW - Semantic Interoperability KW - Knowledge Graph KW - Orowan Mechanism KW - Aluminum Alloy Aging KW - Ontology KW - Semantic Data Integration PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599780 DO - https://doi.org/10.1038/s41597-024-03169-4 VL - 11 IS - 1 SP - 1 EP - 12 PB - Springer Science and Business Media LLC AN - OPUS4-59978 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jacobson, David A1 - Darvishi Kamachali, Reza A1 - Thompson, Gregory T1 - Coupling density phase field models with atomistic potentials N2 - A density-based phase field model is developed where the free energy functional is explicitly linked with molecular dynamics and is referred to as the Molecular Phase Field Method (MoPF). MoPF simulations involve expressing interatomic potentials in terms of density to form a density based free energy functional. Inputs to this functional are taken from atomistics such that the phase field density profile matches the corresponding density profile from atomistic simulations. We analyze our results by comparing the MoPF calculated excess interfacial energies with excess interfacial energies calculated using molecular dynamics associated with several nickel grain boundaries. Additionally, a comparison is made between our results and the interfacial energies of a \Sigma7 boundary across a variety of FCC systems simulated using density functional theory. The MoPF method is able to successfully predict grain boundary free energy trends between grain boundary and material types offering an atomistically informed mesoscale formulation for studying grain boundary physics. KW - Density-based Phase-Field Modelling KW - Atomistic Simulation KW - Grain Boundary PY - 2024 DO - https://doi.org/10.1016/j.commatsci.2023.112763 VL - 233 SP - 1 EP - 6 PB - Elsevier AN - OPUS4-59360 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Bayerlein, Bernd A1 - von Hartrott, Philipp A1 - Waitelonis, Jörg A1 - Birkholz, Henk A1 - Portella, Pedro Dolabella A1 - Skrotzki, Birgit T1 - FAIR and Structured Data: A Domain Ontology Aligned with Standard‐Compliant Tensile Testing N2 - The digitalization of materials science and engineering (MSE) is currently leading to remarkable advancements in materials research, design, and optimization, fueled by computer‐driven simulations, artificial intelligence, and machine learning. While these developments promise to accelerate materials innovation, challenges in quality assurance, data interoperability, and data management have to be addressed. In response, the adoption of semantic web technologies has emerged as a powerful solution in MSE. Ontologies provide structured and machine‐actionable knowledge representations that enable data integration, harmonization, and improved research collaboration. This study focuses on the tensile test ontology (TTO), which semantically represents the mechanical tensile test method and is developed within the project Plattform MaterialDigital (PMD) in connection with the PMD Core Ontology. Based on ISO 6892‐1, the test standard‐compliant TTO offers a structured vocabulary for tensile test data, ensuring data interoperability, transparency, and reproducibility. By categorizing measurement data and metadata, it facilitates comprehensive data analysis, interpretation, and systematic search in databases. The path from developing an ontology in accordance with an associated test standard, converting selected tensile test data into the interoperable resource description framework format, up to connecting the ontology and data is presented. Such a semantic connection using a data mapping procedure leads to an enhanced ability of querying. The TTO provides a valuable resource for materials researchers and engineers, promoting data and metadata standardization and sharing. Its usage ensures the generation of finable, accessible, interoperable, and reusable data while maintaining both human and machine actionability. KW - Data Interoperability KW - Domain Ontology Development KW - FAIR Data Management KW - Knowledge Representation KW - Tensile Test Ontology KW - Semantic Web Technologies PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-598142 DO - https://doi.org/10.1002/adem.202400138 SN - 1438-1656 SP - 1 EP - 19 PB - Wiley VHC-Verlag AN - OPUS4-59814 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hoffmann, Moritz A1 - Stawarczyk, Bogna A1 - Günster, Jens A1 - Zocca, Andrea T1 - Influence of additives and binder on the physical properties of dental silicate glass-ceramic feedstock for additive manufacturing N2 - Objectives The aim of the study was to investigate the impact of organic additives (binder, plasticizer, and the cross-linking ink) in the formulation of water-based feedstocks on the properties of a dental feldspathic glass-ceramic material developed for the slurry-based additive manufacturing technology “LSD-print.” Material and methods Three water-based feldspathic feedstocks were produced to study the effects of polyvinyl alcohol (AC1) and poly (sodium 4-styrenesulfonate) (AC2) as binder systems. A feedstock without organic additives was tested as the control group (CG). Disc-shaped (n = 15) and bar (n = 7) specimens were slip-cast and characterized in the green and fired states. In the green state, density and flexural strength were measured. In the fired state, density, shrinkage, flexural strength (FS), Weibull modulus, fracture toughness (KIC), Martens parameters, and microstructure were analyzed. Disc-shaped and bar specimens were also cut from commercially available CAD/CAM blocks and used as a target reference (TR) for the fired state. Results In the green state, CG showed the highest bulk density but the lowest FS, while the highest FS in the green state was achieved with the addition of a cross-linking ink. After firing, no significant differences in density and a similar microstructure were observed for all slip-cast groups, indicating that almost complete densification could be achieved. The CAD/CAM specimens showed the highest mean FS, Weibull modulus, and KIC, with significant differences between some of the slip-cast groups. Significance These results suggest that the investigated feedstocks are promising candidates for the slurry-based additive manufacturing of restorations meeting the class 1a requirements according to DIN EN ISO 6871:2019–01. KW - Firing KW - 3D-printing KW - Silicate glass-ceramics KW - Debinding PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600516 DO - https://doi.org/10.1016/j.jmbbm.2024.106563 SN - 1751-6161 VL - 155 SP - 1 EP - 12 PB - Elsevier B.V. AN - OPUS4-60051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kindrachuk, Vitaliy A1 - Darvishi Kamachali, Reza T1 - Mean-field modeling and phase-field simulation of grain growth under directional driving forces N2 - Directional grain growth is a common phenomenon in the synthetic and natural evolution of various polycrystals. It occurs in the presence of an external driving force, such as a temperature gradient, along which grains show a preferred, yet competitive, growth. Novel additive manufacturing processes, with intense, localized energy deposition, are prominent examples of when directional grain growth can occur, beneath the melting pool. In this work, we derive a phenomenological mean-field model and perform 3D phase-field simulations to investigate the directional grain growth and its underlying physical mechanisms. The effect of the intensity of driving force is simulated and systematically analyzed at the evolving growth front as well as various cross-sections perpendicular to the direction of the driving force. We found that although the directional growth significantly deviates from normal grain growth, it is still governed by a power law relation α tⁿ with an exponent n ~ 0.6–0.7. The exponent n exhibits a nontrivial dependence on the magnitude of the directional driving force, such that the lowest growth exponent is observed for intermediate driving forces. We elaborate that this can originate from the fact that the forces at grain boundary junctions evolve out of balance under the influence of the directional driving force. With increasing the driving forces, the growth exponent asymptotically approaches a value of n ≈ 0.63, imposed by the largest possible grain aspect ratio for given grain boundary energies. The current combined mean-field and phase-field framework pave the way for future exploration in broader contexts such as the evolution of complex additively manufactured microstructures. KW - Additive manufacturing KW - Phase-field simulation KW - Grain growth KW - Mean-field modelling KW - Directional grain growth PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593210 DO - https://doi.org/10.1016/j.mtla.2023.101989 SN - 2589-1529 VL - 33 SP - 1 EP - 10 PB - Elsevier AN - OPUS4-59321 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wang, Zengquan A1 - Riechers, Birte A1 - Derlet, Peter M. A1 - Maaß, Robert T1 - Atomic cluster dynamics causes intermittent aging of metallic glasses N2 - In the past two decades, numerous relaxation or physical aging experiments of metallic glasses have revealed signatures of intermittent atomic-scale processes. Revealed via intensity cross-correlations from coherent scattering using X-ray photon correlation spectroscopy (XPCS), the observed abrupt changes in the time-domain of atomic motion does not fit the picture of gradual slowing down of relaxation times and their origin continues to remain unclear. Using a binary Lennard-Jones model glass subjected to microsecond-long isotherms, we show here that temporally and spatially heterogeneous atomic-cluster activity at different length-scales drive the emergence of highly non-monotonous intensity cross-correlations. The simulated XPCS experiments reveal a variety of time-dependent intensity-cross correlations that, depending on both the structural evolution and the 𝑞-space sampling, give detailed insights into the possible structural origins of intermittent aging measured with XPCS. KW - Metallic glasses KW - Aging KW - Molecular dynamics KW - XPCS PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595415 DO - https://doi.org/10.1016/j.actamat.2024.119730 SN - 1359-6454 VL - 267 SP - 1 EP - 9 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-59541 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mrkwitschka, Paul A1 - Rühle, Bastian A1 - Kuchenbecker, Petra A1 - Löhmann, Oliver A1 - Lindemann, Franziska A1 - Hodoroaba, Vasile-Dan T1 - Embedding and cross-sectioning as a sample preparation procedure for accurate and representative size and shape measurement of nanopowders N2 - Reliable measurement of the size of polydisperse, complex-shaped commercial nanopowders is a difficult but necessary task, e.g., for regulatory requirements and toxicity risk assessment. Suitable methods exist for the accurate characterization of the size of non-aggregated, stabilized, spherical and monodisperse nanoparticles. In contrast, industrial nanoscale powders usually require dedicated sample preparation procedures developed for the analysis method of choice. These nano-powders tend to agglomerate and/or aggregate, a behavior which in combination with an innate broad particle size distribution and irregular shape often significantly alters the achievable accuracy of the measured size parameters. The present study systematically tests two commercially available nanoscale powders using different sample preparation methods for correlative analysis by scanning electron microscopy, dynamic light scattering, Brunauer–Emmet–Teller method and differential mobility analysis. One focus was set on the sample preparation by embedding nanoparticles in carbon-based hot-mounting resin. Literature on this topic is scarce and the accuracy of the data extracted from cross sections of these particles is unclearly stated. In this paper systematic simulations on the deviation of the size parameters of well-defined series of nanoparticles with different shapes from the nominal value were carried out and the contributing factors are discussed. KW - Nanopowder KW - Electron microscopy KW - Sample preparation KW - Cross-sectioning KW - Cerium oxide KW - Zinc oxide PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593289 DO - https://doi.org/10.1038/s41598-023-51094-0 SN - 2045-2322 VL - 14 SP - 1 EP - 10 PB - Springer Nature CY - London AN - OPUS4-59328 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zia, Ghezal Ahmad Jan A1 - Hanke, Thomas A1 - Skrotzki, Birgit A1 - Völker, Christoph A1 - Bayerlein, Bernd T1 - Enhancing Reproducibility in Precipitate Analysis: A FAIR Approach with Automated Dark-Field Transmission Electron Microscope Image Processing N2 - AbstractHigh-strength aluminum alloys used in aerospace and automotive applications obtain their strength through precipitation hardening. Achieving the desired mechanical properties requires precise control over the nanometer-sized precipitates. However, the microstructure of these alloys changes over time due to aging, leading to a deterioration in strength. Typically, the size, number, and distribution of precipitates for a quantitative assessment of microstructural changes are determined by manual analysis, which is subjective and time-consuming. In our work, we introduce a progressive and automatable approach that enables a more efficient, objective, and reproducible analysis of precipitates. The method involves several sequential steps using an image repository containing dark-field transmission electron microscopy (DF-TEM) images depicting various aging states of an aluminum alloy. During the process, precipitation contours are generated and quantitatively evaluated, and the results are comprehensibly transferred into semantic data structures. The use and deployment of Jupyter Notebooks, along with the beneficial implementation of Semantic Web technologies, significantly enhances the reproducibility and comparability of the findings. This work serves as an exemplar of FAIR image and research data management. KW - Industrial and Manufacturing Engineering KW - General Materials Science KW - Automated image analysis KW - FAIR research data management KW - Reproducibility KW - microstructural changes PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593905 DO - https://doi.org/10.1007/s40192-023-00331-5 SN - 2193-9772 SP - 1 EP - 15 PB - Springer Science and Business Media LLC CY - Heidelberg AN - OPUS4-59390 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bayerlein, Bernd A1 - Schilling, Markus A1 - Birkholz, Henk A1 - Jung, Matthias A1 - Waitelonis, Jörg A1 - Mädler, Lutz A1 - Sack, Harald T1 - PMD Core Ontology: Achieving semantic interoperability in materials science N2 - Knowledge representation in the Materials Science and Engineering (MSE) domain is a vast and multi-faceted challenge: Overlap, ambiguity, and inconsistency in terminology are common. Invariant (consistent) and variant (context-specific) knowledge are difficult to align cross-domain. Generic top-level semantic terminology often is too abstract, while MSE domain terminology often is too specific. In this paper, an approach how to maintain a comprehensive MSE-centric terminology composing a mid-level ontology–the Platform MaterialDigital Core Ontology (PMDco)–via MSE community-based curation procedures is presented. The illustrated findings show how the PMDco bridges semantic gaps between high-level, MSE-specific, and other science domain semantics. Additionally, it demonstrates how the PMDco lowers development and integration thresholds. Moreover, the research highlights how to fuel it with real-world data sources ranging from manually conducted experiments and simulations with continuously automated industrial applications. KW - Ontology KW - Materials science and engineering KW - Knowledge representation KW - Reproducibility KW - Semantic interoperability KW - Semantic data integration PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-592948 DO - https://doi.org/10.1016/j.matdes.2023.112603 SN - 0264-1275 VL - 237 SP - 1 EP - 12 PB - Elsevier CY - Amsterdam AN - OPUS4-59294 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf A1 - Boccaccini, A. R. T1 - Sintering and crystallization kinetics of bioactive glass 13-93 N2 - This study investigates the sintering and crystallization behavior and kinetic of the bioactive glass (BG) 13–93 with nominal composition (in mol%): 54.6 SiO2 - 1.7 P2O3 - 22.1 CaO - 6.0 Na2O - 7.9 K2O - 7.7 MgO. Sintering and crystallization were investigated non-isothermally for various particle size fractions smaller than 315 μm as well as for bulk samples. Densification was not hindered by the presence of crystalline phases across all particle size fractions. Afterwards, wollastonite was found as the dominant crystal phase at higher temperature which resorb primary surface precipitation-like quartz crystallites. The growth direction shifts into volume when the sample surface is nearly covered. The crystal growth rate of wollastonite was calculated from the crystalline surface layer thickness measured during heating. The findings of this study are relevant for the high temperature processing of BG 13–93. KW - Bioactive glass KW - Sintering KW - Crystallization PY - 2024 DO - https://doi.org/10.1016/j.jnoncrysol.2023.122790 SN - 0022-3093 VL - 627 SP - 1 EP - 7 PB - Elsevier AN - OPUS4-59337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Andreoli, A. F. A1 - Fantin, Andrea A1 - Kasatikov, S. A1 - Bacurau, V. P. A1 - Widom, M. A1 - Gargarella, P. A1 - Mazzer, E. M. A1 - Woodcock, T. G. A1 - Nielsch, K. A1 - Coury, F. G. T1 - The impact of chemical short-range order on the thermophysical properties of medium- and high-entropy alloys N2 - The unusual behavior observed in the coefficient of thermal expansion and specific heat capacity of CrFeNi, CoCrNi, and CoCrFeNi medium/high-entropy alloys is commonly referred to as the K-state effect. It is shown to be independent of the Curie temperature, as demonstrated by temperature-dependent magnetic moment measurements. CoCrFeNi alloy is chosen for detailed characterization; potential reasons for the K-state effect such as texture, recrystallization, and second-phase precipitation are ruled out. An examination of the electronic structure indicates the formation of a pseudo-gap in the Density of States, which suggests a specific chemical interaction between Ni and Cr atoms upon alloying. Hybrid Monte Carlo/Molecular Dynamic (MC/MD) simulations indicate the presence of non-negligible chemical short-range order (CSRO). Local lattice distortions are shown to be negligible, although deviations around Cr and Ni elements from those expected in a fully disordered structure are experimentally observed by X-ray absorption spectroscopy. The determined bonding distances are in good agreement with MC/MD calculations. A mechanism is proposed to explain the anomalies and calorimetric experiments and their results are used to validate the mechanism. KW - Mechanical Engineering KW - Mechanics of Materials KW - General Materials Science PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595869 DO - https://doi.org/10.1016/j.matdes.2024.112724 SN - 0264-1275 VL - 238 SP - 1 EP - 15 PB - Elsevier B.V. AN - OPUS4-59586 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Was, G.S. A1 - Bahn, C.-B. A1 - Busby, J. A1 - Cui, B. A1 - Farkas, D. A1 - Gussev, M. A1 - Rigen He, M. A1 - Hesterberg, J. A1 - Jiao, Z. A1 - Johnson, D. A1 - Kuang, W. A1 - McMurtrey, M. A1 - Robertson, I. A1 - Sinjlawi, A. A1 - Song, M. A1 - Stephenson, K. A1 - Sun, K. A1 - Swaminathan, Srinivasan A1 - Wang, M. A1 - West, E. T1 - How irradiation promotes intergranular stress corrosion crack initiation N2 - Irradiation assisted stress corrosion cracking (IASCC) is a form of intergranular stress corrosion cracking that occurs in irradiated austenitic alloys. It requires an irradiated microstructure along with high temperature water and stress. The process is ubiquitous in that it occurs in a wide range of austenitic alloys and water chemistries, but only when the alloy is irradiated. Despite evidence of this degradation mode that dates back to the 1960s, the mechanism by which it occurs has remained elusive. Here, using high resolution electron backscattering detection to analyze local stress-strain states, high resolution transmission electron microscopy to identify grain boundary phases at crack tips, and decoupling the roles of stress and grain boundary oxidation, we are able to unfold the complexities of the phenomenon to reveal the mechanism by which IASCC occurs. The significance of the findings impacts the mechanical integrity of core components of both current and advanced nuclear reactor designs worldwide. KW - Irradiation KW - Stress corrosion cracking KW - Grain boundaries KW - Oxidation KW - Austenitic alloys PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595748 DO - https://doi.org/10.1016/j.pmatsci.2024.101255 SN - 0079-6425 VL - 143 SP - 1 EP - 15 PB - Elsevier AN - OPUS4-59574 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Niebergall, Ute A1 - Marschall, Niklas A1 - Meinel, Dietmar A1 - Böhning, Martin T1 - Relation of craze to crack length during slow crack growth phenomena in high‐density polyethylene N2 - The craze‐crack mechanism occurring in high‐density polyethylene (HDPE) causing slow crack growth and environmental stress cracking is investigated in detail with respect to the relation of crack length and the related craze zone. This is essential for the understanding of the resulting features of the formed fracture surface and their interpretation in the context of the transition from crack propagation to ductile shear deformation. It turns out that an already formed craze zone does not inevitably result in formation of a propagating crack, but could also undergo ductile failure. For the examination, the full notch creep test (FNCT) was employed with a subsequent advanced fracture surface analysis that was performed using various imaging techniques: light microscopy, laser scanning microscopy, scanning electron microscopy, and X‐ray micro computed tomography scan. FNCT specimens were progressively damaged for increasing durations under standard test conditions applying Arkopal, the standard surfactant solution, and biodiesel as test media were used to analyze the stepwise growth of cracks and crazes. From considerations based on well‐established fracture mechanics approaches, a theoretical correlation between the length of the actual crack and the length of the preceding craze zone was established that could be evidenced and affirmed by FNCT fracture surface analysis. Moreover, the yield strength of a HDPE material exposed to a certain medium as detected by a classic tensile test was found to be the crucial value of true stress to induce the transition from crack propagation due to the craze‐crack mechanism to shear deformation during FNCT measurements. Highlights - Progress of crack formation in high‐density polyethylene is analyzed by different imaging techniques - Determined growth rates depend on distinction between craze zone and crack - The ratio of the present crack to the anteceding craze zone is validated theoretically - The transition from crack propagation to ductile shear deformation is identified - An already formed craze zone may still fail by ductile mechanisms KW - Craze-crack mechanism KW - Environmental stress cracking (ESC) KW - Full notch creep test (FNCT) KW - Laser scanning microscopy (LSM) KW - Slow crack growth (SCG) KW - X-ray computed tomography (CT) PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601831 DO - https://doi.org/10.1002/pen.26698 SN - 1548-2634 VL - 64 IS - 6 SP - 2387 EP - 2403 PB - Wiley AN - OPUS4-60183 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bordeenithikasem, Punnathat A1 - Carpenter, Kalind C. A1 - Hofmann, Douglas C. A1 - White, Victor E. A1 - Yee, Karl Y. A1 - Rizzardi, Quentin A1 - Maher, Jacob A1 - Maaß, Robert T1 - Miniaturized bulk metallic glass gripping structures for robotic mobility platforms N2 - Advancements in bulk metallic glass thermoplastic forming unleash the potential to fabricate microscale metallic features with unparalleled precision and durability, i.e. microspine gripping structures for mobility platforms on planetary or in-space robots. Four designs of grippers were fabricated and rigorously tested. Coefficient of friction on four test surfaces were measured and compared to SiC paper and Velcro. The hardness and elasticity of the bulk metallic glasses make them a game-changer in the field, offering a superior alternative to conventional nonmetallic grippers. KW - Bulk metallic glasses KW - Thermoplastic forming KW - Mobility KW - Microspine PY - 2024 DO - https://doi.org/10.1016/j.actaastro.2024.03.040 SN - 0094-5765 VL - 219 SP - 399 EP - 407 PB - Elsevier Ltd. CY - Amsterdam, Niederlande AN - OPUS4-60182 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dzugan, J. A1 - Lucon, E. A1 - Koukolikova, M. A1 - Li, Y. A1 - Rzepa, S. A1 - Yasin, M.S. A1 - Shao, S. A1 - Shamsaei, N. A1 - Seifi, M. A1 - Lodeiro, M. A1 - Lefebvre, F. A1 - Mayer, U. A1 - Olbricht, J. A1 - Houska, M. A1 - Mentl, V. A1 - You, Z. T1 - ASTM interlaboratory study on tensile testing of AM deposited and wrought steel using miniature specimens N2 - An interlaboratory study, involving eigth international laboratories and coordinated by COMTES FHT (Czech Republic), was conducted to validate tensile measurements obtained using miniature specimens on additively manufactured (AM) components and artifacts. In addition to AM 316L stainless steel (316L SS), a wrought highstrength steel (34CrNiMo6V, equivalent to AISI 4340) was also used. Based on the results, a precision statement in accordance with ASTM E691 standard practice was developed, intended for inclusion in a proposed annex to the ASTM E8/E8M tension testing method. The primary outcomes of the study highlighted the agreement between yield and tensile strength measured from miniature and standard-sized tensile specimens. Furthermore, most tensile properties exhibited similar standard deviations, offering users insight into the efficacy of miniature specimen applications. KW - 316L stainless steel KW - Additive manufacturing KW - High-strength steel KW - Miniature specimens KW - Tensile tests PY - 2024 DO - https://doi.org/10.1016/j.tafmec.2024.104410 SN - 0167-8442 VL - 131 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-60180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nawaz, Q. A1 - Blaeß, Carsten A1 - Mueller, Ralf A1 - Boccaccini, A.R. T1 - Processing and cytocompatibility of Cu-doped and undoped fluoride-containing bioactive glasses N2 - Sintered or additive-manufactured bioactive glass (BG) scaffolds are highly interesting for bone replacement applications. However, crystallization often limits the high-temperature processability of bioactive glasses (BGs). Thus, the BG composition must combine high bioactivity and processability. In this study, three BGs with nominal molar (%) compositions 54.6SiO2-1.7P2O3-22.1CaO-6.0Na2O-7.9K2O-7.7MgO (13–93), 44.8SiO2-2.5P2O3-36.5CaO-6.6Na2O-6.6K2O-3.0CaF2 (F3) and 44.8SiO2-2.5P2O3-35.5CaO-6.6Na2O-6.6K2O-3.0CaF2-1.0CuO (F3–Cu) were investigated. The dissolution and ion release kinetics were investigated on milled glass powder and crystallized particles (500–600 μm). All glasses showed the precipitation of hydroxyapatite (HAp) crystals after 7 days of immersion in simulated body fluid. No significant differences in ion release from glass and crystalline samples were detected. The influence of surface roughness on cytocompatibility and growth of preosteoblast cells (MC3T3-E1) was investigated on sintered and polished BG pellets. Results showed that sintered BG pellets were cytocompatible, and cells were seen to be well attached and spread on the surface after 5 days of incubation. The results showed an inverse relation of cell viability with the surface roughness of pellets, and cells were seen to attach and spread along the direction of scratches. KW - Bioactive glass KW - Crystallization KW - Solubility KW - Cytocompatibility KW - Surface roughness PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-598257 DO - https://doi.org/10.1016/j.oceram.2024.100586 SN - 2666-5395 VL - 18 SP - 1 EP - 8 PB - Elsevier Ltd. AN - OPUS4-59825 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pavasarytė, Lina A1 - Azevedo do Nascimento, Allana A1 - Cysne Barbosa, Ana Paula A1 - Trappe, Volker A1 - Melo, Daniel T1 - Effects of particle size and particle concentration of poly (ethylene-co-methacrylic acid) on properties of epoxy resin N2 - Self-healing polymers have been developed to improve durability and reduce costs associated with maintenance during service. The addition of thermoplastics to thermosets to produce mendable polymers appears as a promising selfhealing technique. In this study, poly (ethylene-co-methacrylic acid) (EMAA) was added to epoxy resin and the effects of EMAA addition on epoxy properties were evaluated. Specimens with two different contents of thermoplastic and particles sizes were manufactured. A two-level full factorial experimental design was used to evaluate the effect of particle size and particle content on properties of epoxy modified with addition of EMAA. Tensile tests and dynamic mechanical analysis (DMA) were used and the evaluated responses were tensile strength, modulus of elasticity, and glass transition temperature (Tg). X-ray computed tomography (XCT) was used to investigate particle size and concentration after manufacturing. It was found that the particle concentration has greater effects on stress–strain behavior of epoxy while Tg was not significantly affected by neither of the analyzed entrance variables. KW - Fracture KW - Self-healing KW - Epoxy KW - Thermoplastic PY - 2024 DO - https://doi.org/10.1002/app.55677 SN - 0021-8995 SP - 1 EP - 14 PB - Wiley online library AN - OPUS4-60205 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stargardt, Patrick A1 - Bresch, Sophie A1 - Falkenberg, Rainer A1 - Mieller, Björn T1 - Effect of Reaction Layers on Internal Stresses in Co‐Fired Multilayers of Calcium Manganate and Calcium Cobaltite N2 - A widespread recovery of waste heat requires a cost‐effective production of thermoelectric generators. Thermoelectric oxides are predestined for use at high temperatures. For manufacturing reasons, a multilayer generator design will be easily scalable and cost‐effective. To evaluate the potential of ceramic multilayer technology for that purpose, a multilayer of the promising thermoelectric oxides calcium cobaltite (Ca3Co4O9), calcium manganate (CMO, CaMnO3), and glass–ceramic insulation layers is fabricated. Cracks and reaction layers at the interfaces are observed in the microstructure. The compositions of these reaction layers are identified by energy‐dispersive X‐ray spectroscopy and X‐ray diffraction. Mechanical and thermal properties of all layers are compiled from literature or determined by purposeful sample preparation and testing. Based on this data set, the internal stresses in the multilayer after co‐firing are calculated numerically. It is shown that tensile stresses in the range of 50 MPa occur in the CMO layers. The reaction layers have only a minor influence on the level of these residual stresses. Herein, it is proven that the material system is basically suitable for multilayer generator production, but that the co‐firing process and the layer structure must be adapted to improve densification and reduce the tensile stresses in the CMO. KW - Ceramic multilayers KW - Co-firings KW - Internal stresses PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601626 DO - https://doi.org/10.1002/pssa.202300956 SP - 1 EP - 9 PB - Wiley VHC-Verlag AN - OPUS4-60162 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gadelmeier, C. A1 - Agudo Jácome, Leonardo A1 - Suárez Ocano, Patricia A1 - Glatzel, U. T1 - Effect of stacking fault energy (SFE) of single crystal, equiatomic CrCoNi and Cantor alloy on creep resistance N2 - Compared to mechanisms like solid solution strengthening, the stacking fault energy (SFE) should be considered as a further factor that influences the material properties. The effect of SFE of alloys or individual elements on strength and resistance can vary considerably. In the high-temperature regime above 700 ◦C, there are still significant gaps in the knowledge about the effect of the SFE on the mechanical properties of single-phase alloys. The effect of SFE on creep resistance of two face-entered cubic equiatomic medium and high entropy alloys, CrCoNi and CrMnFeCoNi, respectively, is evaluated to fill parts of these gaps. Using the Bridgman solidification process, the alloys were produced as single crystals and crept under vacuum at 700 ◦C up to 1100 ◦C. This work shows a significant impact of the lower SFE of CrCoNi on the creep behavior compared to the results of previous investigations of CrMnFeCoNi. The creep resistance of the former is higher over the complete temperature range. At very high temperatures, the strengthening effect of the stacking faults is significantly present. The formation of tetragonal stacking faults and extended dislocation nodes can be identified as the reason for this effect. KW - Medium entropy alloy KW - MEA KW - HEA KW - Single crystal KW - CrCoNi PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-602620 DO - https://doi.org/10.1016/j.msea.2024.146779 SN - 0921-5093 VL - A 908 SP - 1 EP - 9 PB - Elsevier B.V. AN - OPUS4-60262 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kingsbery, P. A1 - Manzoni, Anna M. A1 - Suárez Ocano, Patricia A1 - Többens, D. M. A1 - Stephan‐Scherb, C. T1 - High‐temperature KCl‐induced corrosion of high Cr and Ni alloys investigated by in‐situ diffraction N2 - High‐temperature KCl‐induced corrosion in laboratory air was observed in situ utilizing X‐ray diffraction. High Cr‐containing model alloys (Fe‐13Cr, Fe‐18Cr‐12Ni, and Fe‐25Cr‐20Ni) were coated with KCl and exposed to dry air at 560°C. KCl‐free alloys were studied in the equivalent atmosphere as a reference. After exposure to KCl‐free environments, all alloys showed the formation of very thin oxide layers, indicating good corrosion resistance. In contrast, KCl‐bearing alloys showed distinct damage after exposure. KW - Corrosion KW - In-situ diffraction KW - High-temperature corrosion PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600831 DO - https://doi.org/10.1002/maco.202314224 SN - 0947-5117 SP - 1 EP - 10 PB - Wiley VHC-Verlag AN - OPUS4-60083 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Beygi Nasrabadi, Hossein A1 - Bauer, Felix A1 - Uhlemann, Patrick A1 - Thärig, Steffen A1 - Rehmer, Birgit A1 - Skrotzki, Birgit T1 - Mechanical testing dataset of cast copper alloys for the purpose of digitalization N2 - This data article presents a set of primary, analyzed, and digitalized mechanical testing datasets for nine copper alloys. The mechanical testing methods including the Brinell and Vickers hardness, tensile, stress relaxation, and low-cycle fatigue (LCF) testing were performed according to the DIN/ISO standards. The obtained primary testing data (84 files) mainly contain the raw measured data along with the testing metadata of the processes, materials, and testing machines. Five secondary datasets were also provided for each testing method by collecting the main meta- and measurement data from the primary data and the outputs of data analyses. These datasets give materials scientists beneficial data for comparative material selection analyses by clarifying the wide range of mechanical properties of copper alloys, including Brinell and Vickers hardness, yield and tensile strengths, elongation, reduction of area, relaxed and residual stresses, and LCF fatigue life. Furthermore, both the primary and secondary datasets were digitalized by the approach introduced in the research article entitled “Toward a digital materials mechanical testing lab” [1]. The resulting open-linked data are the machine-processable semantic descriptions of data and their generation processes and can be easily queried by semantic searches to enable advanced data-driven materials research. KW - FAIR principles KW - Hardness KW - Low-Cycle Fatigue (LCF) KW - Tensile testing KW - Stress relaxation PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-605005 DO - https://doi.org/10.1016/j.dib.2024.110687 SN - 2352-3409 SP - 1 EP - 15 PB - Elsevier BV AN - OPUS4-60500 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zocca, Andrea A1 - Günster, Jens T1 - Towards a debinding-free additive manufacturing of ceramics: A development perspective of water-based LSD and LIS technologies N2 - Ceramic additive manufacturing (AM) requires a complex process chain with various post-processing steps that require expensive machines and special expertise. The key to further market penetration is AM that makes it possible to integrate into an already established ceramic process chain. Most successful AM technologies for ceramics are, however, based on processes that initially have been developed for polymeric materials. For ceramics AM, polymers or precursors are loaded with ceramic particles. This strategy facilitates the entry into AM, however the introduction of organic additives into the ceramic process chain represents a considerable technological challenge to ultimately obtain a ceramic component after additive shaping. In the present communication, two technologies based on ceramic suspensions will be introduced, the “layerwise slurry deposition” (LSD) and “laser induced slip casting” (LIS) technology. Both technologies take advantage of the high packing densities reached by conventional slip casting and moreover enable the processing of fines, even nanoparticles. KW - Additive Manufacturing KW - Ceramic KW - Water-based KW - Debinding KW - Slurry PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-605531 DO - https://doi.org/10.1016/j.oceram.2024.100632 SN - 2666-5395 VL - 19 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-60553 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Piesker, Benjamin A1 - Ávila Calderón, Luis Alexander A1 - Mohr, Gunther A1 - Rehmer, Birgit A1 - Agudo Jácome, Leonardo A1 - Hilgenberg, Kai A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Tensile and Low‐Cycle Fatigue Behavior of Laser Powder Bed Fused Inconel 718 at Room and High Temperature N2 - This study investigates the room‐ and high‐temperature (650 °C) tensile and low‐cycle‐fatigue behavior of Inconel 718 produced by laser powder bed fusion (PBF‐LB/M) with a four‐step heat treatment and compares the results to the conventional wrought material. The microstructure after heat treatment is characterized on different length scales. Compared to the wrought variant, the elastic and yield properties are comparable at both test temperatures while tensile strength, ductility, and strain hardening capacity are lower. The fatigue life of the PBF‐LB/M variant at room temperature is slightly lower than that of the wrought material, while at 650 °C, it is vice versa. The cyclic stress response for both material variants is characterized by cyclic softening, which is more pronounced at the higher test temperature. High strain amplitudes (≥0.7%) at room temperature and especially a high testing temperature result in the formation of multiple secondary cracks at the transitions of regions comprising predominantly elongated grain morphology and columns of stacked grains with ripple patterns in the PBF‐LB/M material. This observation and pronounced crack branching and deflection indicate that the cracks are controlled by sharp micromechanical gradients and local crystallite clusters. KW - Additive manufacturing KW - Fatigue damage KW - Heat treatment KW - Inconel 718 KW - Laser powder bed fusion KW - Low-cycle fatigue KW - Tensile strength PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599316 DO - https://doi.org/10.1002/adem.202302122 SN - 1527-2648 SP - 1 EP - 17 PB - Wiley AN - OPUS4-59931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Feng, W. A1 - Gemming, T. A1 - Giebeler, L. A1 - Qu, J. A1 - Weinel, Kristina A1 - Agudo Jácome, Leonardo A1 - Büchner, B. A1 - Gonzalez-Martinez, I. T1 - Influence of magnetic field on electron beam-induced Coulomb explosion of gold microparticles in transmission electron microscopy N2 - In this work we instigated the fragmentation of Au microparticles supported on a thin amorphous carbon film by irradiating them with a gradually convergent electron beam inside the Transmission Electron Microscope. This phenomenon has been generically labeled as ‘‘electron beam-induced fragmentation’’ or EBIF and its physical origin remains contested. On the one hand, EBIF has been primarily characterized as a consequence of beam-induced heating. On the other, EBIF has been attributed to beam-induced charging eventually leading to Coulomb explosion. To test the feasibility of the charging framework for EBIF, we instigated the fragmentation of Au particles under two different experimental conditions. First, with the magnetic objective lens of the microscope operating at full capacity, i.e. background magnetic field 𝐵 = 2 T, and with the magnetic objective lens switched off (Lorenz mode), i.e. 𝐵 = 0 T. We observe that the presence or absence of the magnetic field noticeably affects the critical current density at which EBIF occurs. This strongly suggests that magnetic field effects play a crucial role in instigating EBIF on the microparticles. The dependence of the value of the critical current density on the absence or presence of an ambient magnetic field cannot be accounted for by the beam-induced heating model. Consequently, this work presents robust experimental evidence suggesting that Coulomb explosion driven by electrostatic charging is the root cause of EBIF. KW - Electron beam-induced fragmentation KW - Coulomb explosion KW - X-ray diffraction KW - Lorenz transmission electron microscopy KW - Electron beam-induced charging PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600170 DO - https://doi.org/10.1016/j.ultramic.2024.113978 VL - 262 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-60017 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mieller, Björn A1 - Hassine, Sahar Ben A1 - Töpfer, Jörg A1 - Priese, Christoph A1 - Bochmann, Arne A1 - Capraro, Beate A1 - Stark, Sebastian A1 - Partsch, Uwe A1 - Fresemann, Carina T1 - Ontology‐based Data Acquisition, Refinement, and Utilization in the Development of a Multilayer Ferrite Inductor N2 - A key aspect in the development of multilayer inductors is the magnetic permeability of the ferrite layers. Here, the effects of different processing steps on the permeability of a NiCuZn ferrite is investigated. Dry pressed, tape cast, and co‐fired multilayer samples are analyzed. An automated data pipeline is applied to structure the acquired experimental data according to a domain ontology based on PMDco (Platform MaterialDigital core ontology). Example queries to the ontology show how the determined process‐property correlations are accessible to non‐experts and thus how suitable data for component design can be identified. It is demonstrated how the inductance of co‐fired multilayer inductors is reliably predicted by simulations if the appropriate input data corresponding to the manufacturing process is used.This article is protected by copyright. All rights reserved. KW - Ontology KW - Ceramic multilayer KW - Data pipeline PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-605483 DO - https://doi.org/10.1002/adem.202401042 SN - 1527-2648 SP - 1 EP - 11 PB - Wiley-VCH CY - Weinheim AN - OPUS4-60548 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sänger, Johanna C. A1 - Riechers, Birte A1 - Pauw, Brian Richard A1 - Maaß, Robert A1 - Günster, Jens T1 - Microplastic response of 2PP‐printed ceramics N2 - AbstractTwo‐photon polymerization (2PP) additive manufacturing (AM) utilizes feedstocks of ceramic nanoparticles of a few nanometers in diameter, enabling the fabrication of highly accurate technical ceramic design with structural details as small as 500 nm. The performance of these materials is expected to differ from conventional AM ceramics, as nanoparticles and three‐dimensional printing at high resolution introduce new microstructural aspects. This study applies 2PP‐AM of yttria‐stabilized zirconia to investigate the mechanical response behavior under compressive load, probing the influence of smallest structural units induced by the line packing during the printing process, design of sintered microblocks, and sintering temperature and thereby microstructure. We find a dissipative mechanical response enhanced by sintering at lower temperatures than conventional. The pursued 2PP‐AM approach yields a microstructured material with an increased number of grain boundaries that proposedly play a major role in facilitating energy dissipation within the here printed ceramic material. This microplastic response is further triggered by the filigree structures induced by hollow line packing at the order of the critical defect size of ceramics. Together, these unique aspects made accessible by the 2PP‐AM approach contribute to a heterogeneous nano‐ and microstructure, and hint toward opportunities for tailoring the mechanical response in future ceramic applications. KW - Manufacturing KW - Mechanical properties KW - Microstructure KW - Plasticity KW - Zirconia: yttria stabilized PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-605176 DO - https://doi.org/10.1111/jace.19849 SN - 1551-2916 SP - 1 EP - 10 PB - Wiley CY - Oxford AN - OPUS4-60517 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pereira, Raíssa Monteiro A1 - Lohbauer, Ulrich A1 - Schulbert, Christian A1 - Göken, Mathias A1 - Wurmshuber, Michael A1 - Campos, Tiago Bastos Moreira A1 - Thim, Gilmar Patrocínio A1 - Mieller, Björn A1 - Belli, Renan T1 - Instantiations of Multiscale Kinship in Pressing‐Defect Distributions in Yttria‐Stabilized Zirconias by Powder Partitioning N2 - Modern dry pressing of ceramic powders using spray‐dried granulates cannot avoid the occurrence of defects related to persisting inter‐ and intra‐granulate interstitial voids. These constitute the parent defect size population limiting the application of polycrystalline ceramics in high‐stress conditions. The mitigation of such defects could widen the range of application in technical and biomedical engineering, reduce the safety range for design, and extend the lifetime of components. Herein, the Weibull size‐effect on strength in size‐partitioned Yttria‐stabilized zirconias (YSZ) feedstocks is used to explore the viability of changing the density distribution of granulate sizes as an effective strategy to obtain a denser particle packing that could reduce the size distribution of strength‐limiting pressing defects. In a direct assessment of critical defect size using multiscale strength testing with a dataset of ≈1300 values, the success of such an approach in increasing the strength reliability for small volume components is demonstrated, along with its ultimate failure in altering the defect size distribution in sintered YSZ ceramics across several length scales. Finally, it is shown that granule morphology (spherical or dimpled) fails to affect the defect density and size distribution in YSZ ceramics. KW - Zirconia KW - Strength KW - Toughness KW - Weibull distribution KW - Defect population PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-602697 DO - https://doi.org/10.1002/adem.202400139 SN - 1438-1656 SP - 1 EP - 17 PB - Wiley VHC-Verlag AN - OPUS4-60269 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mieller, Björn A1 - Valavi, Masood A1 - Caldeira Rêgo, Celso Ricardo T1 - An Automatized Simulation Workflow for Powder Pressing Simulations Using SimStack N2 - Automated computational workflows are a powerful concept that can improve the usability and reproducibility of simulation and data processing approaches. Although used very successfully in bioinformatics, workflow environments in materials science are currently commonly applied in the field of atomistic simulations. This work showcases the integration of a discrete element method (DEM) simulation of powder pressing in the convenient SimStack workflow environment. For this purpose, a Workflow active Node (WaNo) was developed to generate input scripts for the DEM solver using LIGGGHTS Open Source Discrete Element Method Particle Simulation code. Combining different WaNos in the SimStack framework makes it possible to build workflows and loop over different simulation or evaluation conditions. The functionality of the workflows is explained, and the added user value is discussed. The procedure presented here is an example and template for many other simulation methods and issues in materials science and engineering. KW - Simulation workflow KW - Discrete element method PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-604791 DO - https://doi.org/10.1002/adem.202400872 SP - 1 EP - 7 PB - Wiley AN - OPUS4-60479 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Beygi Nasrabadi, Hossein A1 - Hanke, Thomas A1 - Skrotzki, Birgit T1 - Semantic Representation of Low‐Cycle‐Fatigue Testing Data Using a Fatigue Test Ontology and ckan.kupferdigital Data Management System N2 - Addressing a strategy for publishing open and digital research data, this article presents the approach for streamlining and automating the process of storage and conversion of research data to those of semantically queryable data on the web. As the use case for demonstrating and evaluating the digitalization process, the primary datasets from low‐cycle‐fatigue testing of several copper alloys are prepared. The fatigue test ontology (FTO) and ckan.kupferdigital data management system are developed as two main prerequisites of the data digitalization process. FTO has been modeled according to the content of the fatigue testing standard and by reusing the basic formal ontology, industrial ontology foundry core ontology, and material science and engineering ontology. The ckan.kupferdigital data management system is also constructed in such a way that enables the users to prepare the protocols for mapping the datasets into the knowledge graph and automatically convert all the primary datasets to those machine‐readable data which are represented by the web ontology language. The retrievability of the converted digital data is also evaluated by querying the example competency questions, confirming that ckan.kupferdigital enables publishing open data that can be highly reused in the semantic web. KW - Accessible KW - CKAN KW - Interoperable KW - Digitalizations KW - Ontologies KW - Reusable data KW - Fatigue testing PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-604991 UR - https://onlinelibrary.wiley.com/doi/10.1002/adem.202400675 DO - https://doi.org/10.1002/adem.202400675 SN - 1527-2648 SP - 1 EP - 11 PB - Wiley AN - OPUS4-60499 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Salari, Farid A1 - Zocca, Andrea A1 - Bosetti, Paolo A1 - Hlaváček, Petr A1 - Italiano, Antonino A1 - Gobbin, Filippo A1 - Colombo, Paolo A1 - Kühne, Hans-Carsten A1 - Sglavo, Vincenzo M. T1 - Powder-bed 3D printing by selective activation of magnesium phosphate cement: Determining significant processing parameters and their effect on mechanical strength N2 - The present work addresses powder bed binder jetting additive manufacturing by selective magnesium phosphate cement activation. Despite the potential of this technology to aid the digitalization of the construction industry, the effect of processing parameters on the mechanical performance of printed materials has not yet been studied to generate a guideline for the further development of the technology. Statistical methodologies were used to screen the effect of four printing process parameters (printing speed, layer thickness, raster angle, and build direction on flexural and compressive strength). As the exploited technology works with constant fluid pressure, the physical interpretation of the effect of each factor can be considered taking into account the interactions between the binder materials in the powder bed. Analysis of variance (ANOVA) indicated that printing speed and layer thickness significantly affect mechanical performances. Furthermore, the layout of samples for the printing process is preferable to be parallel the printhead movement. An anisotropic behavior was observed, and the samples subjected to compressive forces parallel to the layer plane possessed lower strength values. This effect can be interpreted as a result of a weak area of low density in between layers, leading to a pronounced delamination under compression. Even though the strength of the printed material is not suitable for a structural concrete, it can be marginally improved by design of experiment and optimized for non-structural applications, such as for porous artificial stone. Design of experiment coupled with ANOVA methods can be used in the future to support the development of novel material mixtures, thus expanding the fields of application of this novel additive manufacturing technology. KW - Concrete 3D-printing KW - Particle-bed binder jetting KW - Design of experiment PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601654 DO - https://doi.org/10.1016/j.oceram.2024.100609 VL - 18 SP - 1 EP - 11 PB - Elsevier B.V. AN - OPUS4-60165 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhang, Fengchan A1 - Oiticica, Pedro Ramon Almeida A1 - Abad-Arredondo, Jaime A1 - Arai, Marylyn Setsuko A1 - Oliveira, Osvaldo N. A1 - Jaque, Daniel A1 - Fernandez Dominguez, Antonio I. A1 - de Camargo, Andrea Simone Stucchi A1 - Haro-González, Patricia T1 - Brownian Motion Governs the Plasmonic Enhancement of Colloidal Upconverting Nanoparticles N2 - Upconverting nanoparticles are essential in modern photonics due to their ability to convert infrared light to visible light. Despite their significance, they exhibit limited brightness, a key drawback that can be addressed by combining them with plasmonic nanoparticles. Plasmon-enhanced upconversion has been widely demonstrated in dry environments, where upconverting nanoparticles are immobilized, but constitutes a challenge in liquid media where Brownian motion competes against immobilization. This study employs optical tweezers for the three-dimensional manipulation of an individual upconverting nanoparticle, enabling the exploration of plasmon-enhanced upconversion luminescence in water. Contrary to expectation, experiments reveal a long-range (micrometer scale) and moderate (20%) enhancement in upconversion luminescence due to the plasmonic resonances of gold nanostructures. Comparison between experiments and numerical simulations evidences the key role of Brownian motion. It is demonstrated how the three-dimensional Brownian fluctuations of the upconverting nanoparticle lead to an “average effect” that explains the magnitude and spatial extension of luminescence enhancement. KW - Upconversion KW - Plasmon enhancement KW - Optical tweezers KW - Brownian motion KW - Nanoparticles PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-603551 DO - https://doi.org/10.1021/acs.nanolett.4c00379 VL - 24 IS - 12 SP - 3785 EP - 3792 PB - American Chemical Society (ACS) AN - OPUS4-60355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Paulus, Daniel A1 - Bresch, Sophie A1 - Moos, Ralf A1 - Schönauer-Kamin, Daniela T1 - Powder aerosol deposited calcium cobaltite as textured P-type thermoelectric material with power factors approaching single crystal values N2 - In this work, the thermoelectric material calcium cobaltite Ca3Co4O9 (CCO), a promising p-type conducting thermoelectric oxide with anisotropic properties, was processed by the powder aerosol deposition method (PAD) to form a dense ceramic CCO film with a thickness in the µm range. The prepared films were characterized regarding their microstructure and thermoelectric properties between room temperature and 900 °C. After heat treatment at 900 °C, the CCO PAD film in-plane shows excellent properties in terms of electrical conductivity (280 S/cm at 900 °C) and Seebeck coefficient (220 µV/K at 900 °C). The calculated power factor in-plane (ab) reaches with 1125 µW/(m K2) 40 % of the single crystal value, surpassing the known-properties of CCO bulk ceramics. Examination of the microstructure shows a strong fiber texture of the film as well as a strong coarsening of the grains during the first heat treatment up to 900 °C. KW - thermoelectrics KW - calcium cobaltite KW - thermoelectric oxide KW - aerosol deposition method (ADM) PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-606246 DO - https://doi.org/10.1016/j.jeurceramsoc.2024.116717 SN - 0955-2219 VL - 44 IS - 15 SP - 1 EP - 8 PB - Elsevier BV AN - OPUS4-60624 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Arai, Marylyn Setsuko A1 - Kim, Hyunho A1 - Pascavis, Madeleine A1 - Cha, Baekdong A1 - Brambilla, Gabriel A1 - Cho, Young Kwan A1 - Park, Jinho A1 - Vilela, Raquel R. C. A1 - de Camargo, Andrea S. S. A1 - Castro, Cesar M. A1 - Lee, Hakho T1 - Upconverting Nanoparticle-based Enhanced Luminescence Lateral-Flow Assay for Urinary Biomarker Monitoring N2 - Development of efficient portable sensors for accurately detecting biomarkers is crucial for early disease diagnosis, yet remains a significant challenge. To address this need, we introduce the enhanced luminescence lateral-flow assay, which leverages highly luminescent upconverting nanoparticles (UCNPs) alongside a portable reader and a smartphone app. The sensor’s efficiency and versatility were shown for kidney health monitoring as a proof of concept. We engineered Er3+- and Tm3+-doped UCNPs coated with multiple layers, including an undoped inert matrix shell, a mesoporous silica shell, and an outer layer of gold (UCNP@mSiO2@Au). These coatings synergistically enhance emission by over 40-fold and facilitate biomolecule conjugation, rendering UCNP@mSiO2@Au easy to use and suitable for a broad range of bioapplications. Employing these optimized nanoparticles in lateral-flow assays, we successfully detected two acute kidney injury-related biomarkers-kidney injury molecule-1 (KIM-1) and neutrophil gelatinase-associated lipocalin (NGAL)-in urine samples. Using our sensor platform, KIM-1 and NGAL can be accurately detected and quantified within the range of 0.1 to 20 ng/mL, boasting impressively low limits of detection at 0.28 and 0.23 ng/mL, respectively. Validating our approach, we analyzed clinical urine samples, achieving biomarker concentrations that closely correlated with results obtained via ELISA. Importantly, our system enables biomarker quantification in less than 15 min, underscoring the performance of our novel UCNP-based approach and its potential as reliable, rapid, and user-friendly diagnostics. KW - Biosensor KW - Upconverting nanoparticles KW - Lateral flow KW - Portable sensor KW - Kidney injury PY - 2024 DO - https://doi.org/10.1021/acsami.4c06117 SN - 1944-8244 VL - 16 IS - 29 SP - 38243 EP - 38251 PB - American Chemical Society (ACS) AN - OPUS4-60689 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - da Costa, P. F. G. M. A1 - Merízio, L. G. A1 - Wolff, N. A1 - Terraschke, H. A1 - de Camargo, Andrea Simone Stucchi T1 - Real-time monitoring of CdTe quantum dots growth in aqueous solution N2 - Quantum dots (QDs) are remarkable semiconductor nanoparticles, whose optical properties are strongly size-dependent. Therefore, the real-time monitoring of crystal growth pathway during synthesis gives an excellent opportunity to a smart design of the QDs luminescence. In this work, we present a new approach for monitoring the formation of QDs in aqueous solution up to 90 °C, through in situ luminescence analysis, using CdTe as a model system. This technique allows a detailed examination of the evolution of their light emission. In contrast to in situ absorbance analysis, the in situ luminescence measurements in reflection geometry are particularly advantageous once they are not hindered by the concentration increase of the colloidal suspension. The synthesized particles were additionally characterized using X-ray diffraction analysis, transition electron microscopy, UV-Vis absorption and infrared spectroscopy. The infrared spectra showed that 3-mercaptopropionic acid (MPA)-based thiols are covalently bound on the surface of QDs and microscopy revealed the formation of CdS. Setting a total of 3 h of reaction time, for instance, the QDs synthesized at 70, 80 and 90 °C exhibit emission maxima centered at 550, 600 and 655 nm. The in situ monitoring approach opens doors for a more precise achievement of the desired emission wavelength of QDs. KW - CdTe quantum dots KW - In situ synthesis KW - Real time growth control PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-603596 DO - https://doi.org/10.1038/s41598-024-57810-8 SN - 2045-2322 VL - 14 IS - 1 SP - 1 EP - 11 PB - Springer Science and Business Media LLC AN - OPUS4-60359 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Fritsch, Tobias A1 - Luzin, Vladimir A1 - Ferrari, Bruno A1 - Simón-Muzás, Juan A1 - Evans, Alexander A1 - Bruno, Giovanni T1 - Impact of scan strategy on principal stresses in laser powder bed fusion N2 - Additive manufacturing techniques, such as laser powder bed fusion (PBF-LB), are well known for their exceptional freedom in part design. However, these techniques are also characterized by the development of large thermal gradients during production and thus residual stress (RS) formation in produced parts. In this context, neutron diffraction enables the non-destructive characterization of the bulk RS distribution. By control of the thermal gradients in the powder-bed plane by scan strategy variation we study the impact of in-process scan strategy variations on the microstructure and the three-dimensional distribution of RS. Microstructural analysis by means of electron backscatter diffraction reveals sharp microstructure transitions at the interfaces ranging from 100-200 µm. The components of the RS tensor are determined by means of neutron diffraction and the principal stress directions and magnitudes are determined by eigenvalue decomposition. We find that the distribution of RS in the powder-bed plane corresponds to the underlying scan strategy. When the alternating scan vectors align with the x- and y sample coordinate axes, the principal stress directions co-align. In the present geometry, nearly transverse isotropic stress states develop when the scan vectors are either aligned 45° between x and y or continuously rotated by 67° between each layer. KW - Additive Manufacturing KW - Laser Powder Bed Fusion KW - Electron Backscatter Diffraction KW - Neutron Diffraction KW - Residual Stress KW - Principal Stress PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-607910 DO - https://doi.org/10.1016/j.matdes.2024.113171 SN - 0264-1275 VL - 244 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-60791 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf T1 - Viscous crack healing in soda–lime–magnesium–silicate–ZrO2 glass matrix composites N2 - AbstractThe present study investigates the influence of the crystal volume content on viscous crack healing in glass ceramic glass sealants. To ensure constant microstructure during healing, soda–lime–magnesium silicate glass matrix composites with varied volume fractions of ZrO2 filler particles were used. Crack healing was studied on radial cracks induced by Vickers indentation, which were stepwise annealed to monitor the healing progress by confocal laser scanning microscopy. Confirming previous studies, healing of radial cracks in pure glass was found delayed by global flow phenomena like crack widening and crack edge and tip rounding to minimize the sample surface. With increasing ZrO2 filler content, these global flow phenomena were progressively inhibited whereas local flow phenomena like sharp crack tip healing could still occur. As a result, crack healing was even accelerated by filler particles up to a maximum filler content of 17 vol% whereas crack healing was fully suppressed only at 33 vol% filler content. KW - Crack healing KW - Glass matrix composite KW - Solid oxide fuell cell KW - Vickers identation KW - Viscosity PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-607860 DO - https://doi.org/10.1111/jace.20002 SN - 0002-7820 SP - 1 EP - 12 PB - Wiley AN - OPUS4-60786 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Riechers, Birte A1 - Das, Amlan A1 - Dufresne, Eric A1 - Derlet, Peter M. A1 - Maaß, Robert T1 - Intermittent cluster dynamics and temporal fractional diffusion in a bulk metallic glass N2 - Glassy solids evolve towards lower-energy structural states by physical aging. This can be characterized by structural relaxation times, the assessment of which is essential for understanding the glass’ time-dependent property changes. Conducted over short times, a continuous increase of relaxation times with time is seen, suggesting a time-dependent dissipative transport mechanism. By focusing on micro-structural rearrangements at the atomic-scale, we demonstrate the emergence of sub-diffusive anomalous transport and therefore temporal fractional diffusion in a metallic glass, which we track via coherent x-ray scattering conducted over more than 300,000 s. At the longest probed decorrelation times, a transition from classical stretched exponential to a power-law behavior occurs, which in concert with atomistic simulations reveals collective and intermittent atomic motion. Our observations give a physical basis for classical stretched exponential relaxation behavior, uncover a new power-law governed collective transport regime for metallic glasses at long and practically relevant time-scales, and demonstrate a rich and highly non-monotonous aging response in a glassy solid, thereby challenging the common framework of homogeneous aging and atomic scale diffusion. KW - Glassy solids KW - Fractional diffusion KW - Coherent x-ray scattering PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608015 DO - https://doi.org/10.1038/s41467-024-50758-3 VL - 15 IS - 1 SP - 1 EP - 9 PB - Springer Science and Business Media LLC AN - OPUS4-60801 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vogel, F. A1 - Ngai, S. A1 - Zhou, X. Y. A1 - Zaiser, E. A1 - Manzoni, Anna Maria A1 - Wu, Y. A1 - Zheng, W. W. A1 - Zhang, P. A1 - Thompson, G. B. T1 - Tracking maze-like hierarchical phase separation behavior in a Fe-Si-V alloy N2 - Optimizing the properties of next-generation high-temperature and corrosion-resistant alloys is rooted in balancing structure-property relationships and phase chemistry. Here, we implement a complementary approach based on transmission electron microscopy (TEM) and atom probe tomography (APT) to ascertain aspects of hierarchical phase separation behavior, by understanding the microstructural evolution and the three-dimensional (3D) nanochemistry of a single crystal Fe79.5Si15.5V5.0 (at%) alloy. A maze-like hierarchical microstructure forms, in which a complex network of metastable disordered α plates (A2 phase) emerges within ordered α1 precipitates (D03 phase). The supersaturation in α1 (D03) precipitates with Fe and V drives the formation of α (A2) plates. The morphology of α (A2) plates is discussed concerning crystal structure, lattice misfit, and elastic strain. Phase compositions and a ternary phase diagram aid the thermodynamic assessment of the hierarchical phase separation mechanism via the Gibbs energy of mixing. A perspective on the stabilization of hierarchical microstructures beyond Fe79.5Si15.5V5.0 is elaborated by comparing hierarchical alloys. We find that the ratio of elastic anisotropy (Zener ratio) serves as a predictor of the hierarchical particles’ morphology. We suggest that the strengthening effect of hierarchical microstructures can be harnessed by improving the temporal and thermal stability of hierarchical particles. This can be achieved through phase-targeted alloying aiming at the hierarchical particles phase by considering the constituents partitioning behavior. Beyond Fe79.5Si15.5V5.0, our results demonstrate a potential pathway for improving the properties of high-temperature structural materials. KW - Atom probe tomography KW - Transmission electron microscopy KW - Hierarchical microstructure KW - Phase separation PY - 2023 DO - https://doi.org/10.1016/j.jallcom.2023.172157 SN - 0925-8388 VL - 968 SP - 1 EP - 17 PB - Elsevier B.V. AN - OPUS4-58343 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fantin, Andrea A1 - Lepore, G. O. A1 - Widom, M. A1 - Kasatikov, S. A1 - Manzoni, Anna Maria T1 - How Atomic Bonding Plays the Hardness Behavior in the Al–Co–Cr–Cu–Fe–Ni High Entropy Family N2 - A systematic study on a face‐centered cubic‐based compositionally complex alloy system Al–Co–Cr–Cu–Fe–Ni in its single‐phase state is carried out, where a mother senary compound Al₈Co₁₇Cr₁₇Cu₈Fe₁₇Ni₃₃ and five of its suballoys, obtained by removing one element at a time, are investigated and exhaustively analyzed determining the contribution of each alloying element in the solid solution. The senary and the quinaries are compared using experimental techniques including X‐ray absorption spectroscopy, X‐ray diffraction, transmission electron microscopy, and first principles hybrid Monte Carlo/molecular dynamics simulations. Chemical short‐range order and bond length distances have been determined both at the experimental and computational level. Electronic structure and local atomic distortions up to 5.2 Å have been correlated to the microhardness values. A linear regression model connecting hardness with local lattice distortions is presented. KW - High entropy alloys KW - EXAFS KW - Short-range order KW - Microhardness KW - Alloy design KW - Transmission electron microscopy KW - Lattice distortion PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593333 DO - https://doi.org/https://doi.org/10.1002/smsc.202300225 SN - 2688-4046 SP - 1 EP - 12 PB - Wiley CY - Weinheim AN - OPUS4-59333 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ikeda, Yuki A1 - Ni, H.C. A1 - Chakraborty, A. A1 - Ghassemi-Armaki, H. A1 - Zuo, J.M. A1 - Darvishi Kamachali, Reza A1 - Maaß, Robert T1 - Segregation-induced grain-boundary precipitation during early stages of liquid-metal embrittlement of an advanced high-strength steel N2 - Liquid-metal embrittlement (LME) of galvanized (Zn-coated) advanced high-strength steels is a long-known problem in materials science. Here we reveal the initial microstructural processes underneath the Zn-coating that lead to LME-microcrack initiation in the steel substrate. We track the microstructural evolution during the first tens of milliseconds and find pronounced signatures of Fe-Zn intermetallic precipitation in both ferrite grain boundaries and at internal ferrite-oxide phase boundaries. In concert with novel CALPHAD-integrated density-based thermodynamic modelling, we demonstrate that Zn-rich intermetallic phase-nucleation can occur at markedly low processing temperatures due to a segregation transition. We show that a small Znenrichment caused by Zn bulk-diffusion during the initial temperature rise in a joining process is sufficient to induce the segregation transition and subsequent nucleation of Fe-Zn intermetallic grain-boundary phases, which the experiments link to crack initiation sites. These findings direct focus onto LME-controlling microstructural and thermodynamic phenomena at temperatures below the ductility trough and the austenite formation temperature. KW - Resistance spot welding KW - Liquid-metal embrittlement KW - Steels KW - Grain boundaries PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581067 DO - https://doi.org/10.1016/j.actamat.2023.119243 VL - 259 SP - 1 EP - 12 PB - Elsevier Ltd AN - OPUS4-58106 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jacobson, D. A1 - Darvishi Kamachali, Reza A1 - Thompson, G. B. T1 - Extending Density Phase-Field Simulations to Dynamic Regimes N2 - Density-based phase-field (DPF) methods have emerged as a technique for simulating grain boundary thermodynamics and kinetics. Compared to the classical phase-field, DPF gives a more physical description of the grain boundary structure and chemistry, bridging CALPHAD databases and atomistic simulations, with broad applications to grain boundary and segregation engineering. Notwithstanding their notable progress, further advancements are still warranted in DPF methods. Chief among these are the requirements to resolve its performance constraints associated with solving fourth-order partial differential equations (PDEs) and to enable the DPF methods for simulating moving grain boundaries. Presented in this work is a means by which the aforementioned problems are addressed by expressing the density field of a DPF simulation in terms of a traditional order parameter field. A generic DPF free energy functional is derived and used to carry out a series of equilibrium and dynamic simulations of grain boundaries in order to generate trends such as grain boundary width vs. gradient energy coefficient, grain boundary velocity vs. applied driving force, and spherical grain radius vs. time. These trends are compared with analytical solutions and the behavior of physical grain boundaries in order to ascertain the validity of the coupled DPF model. All tested quantities were found to agree with established theories of grain boundary behavior. In addition, the resulting simulations allow for DPF simulations to be carried out by existing phase-field solvers. KW - CALPHAD KW - Phase-field modelling KW - Phase-Field Simulations PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581365 DO - https://doi.org/10.3390/met13081497 VL - 13 SP - 1 EP - 16 AN - OPUS4-58136 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lunkenheimer, P. A1 - Loidl, A. A1 - Riechers, Birte A1 - Zaccone, A. A1 - Samwer, K. T1 - Thermal expansion and the glass transition N2 - Melting is well understood in terms of the Lindemann criterion, which essentially states that crystalline materials melt when the thermal vibrationsof their atoms become so vigorous that they shake themselves free of the binding forces. This picture does not necessarily have to hold for glasses, where the nature of the solid–liquid cross-over is highly debated. The Lindemann criterion implies that the thermal expansion coefficients of crystals are inversely proportional to their melting temperatures. Here we find that, in contrast, the thermal expansion coefficient of glasses decreases more strongly with increasing glass temperature, which marks the liquid–solid cross-over in this material class. However, this proportionality returns when the thermal expansion coefficient is scaled by the fragility, a measure of particle cooperativity. Therefore, for a glass to become liquid, it is not sufficient to simply overcome the interparticle binding energies. Instead, more energy must be invested to break up the typical cooperative particle network that is common to glassy materials. The thermal expansion coefficient of the liquid phase reveals similar anomalous behaviour and is universally enhanced by a constant factor of approximately 3. These universalities allow the estimation of glass temperatures from thermal expansion and vice versa. KW - Glass transition KW - Lindemann criterion KW - Thermal expansion KW - Glass PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-570267 DO - https://doi.org/10.1038/s41567-022-01920-5 SN - 1745-2473 SP - 1 EP - 7 PB - Nature Publishing Group CY - London AN - OPUS4-57026 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Das, A. A1 - Ott, C. A1 - Pechimuthu, Dinesh A1 - Moosavi, Robabeh A1 - Stoica, M. A1 - Derlet, P. M. A1 - Maaß, Robert T1 - Shear-band cavitation determines the shape of the stress-strain curve of metallic glasses N2 - Metallic glasses are known to have a remarkably robust yield strength, admitting Weibull moduli as high as for crystalline engineering alloys. However, their postyielding behavior is strongly varying, with large scatter in both flow stress levels and strains at failure. Using x-ray tomography, we reveal how a strain-dependent internal evolution of shear-band cavities underlies this unpredictable postyielding response.We demonstrate how macroscopic strain softening coincides with the first detection of internal shear-band cavitation. Cavity growth during plastic flow is found to follow a power law, which yields a fractal dimension and a roughness exponent in excellent agreement with self-similar surface properties obtained after fracture. These findings demonstrate how internal microcracking coexists with shear-band plasticity along the plastic part of a stress-strain curve, rationalizing the large variability of plastic flow behavior seen for metallic glasses. KW - Shear-band cavitation KW - Metallic glasses PY - 2023 DO - https://doi.org/10.1103/PhysRevMaterials.7.023602 SN - 2475-9953 VL - 7 IS - 2 SP - 1 EP - 11 PB - American Physical Society AN - OPUS4-57042 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - Prolonging structural integrity—Fatigue of scarf repairs for wind turbine blade shell applications N2 - The influence of scarf repair variables on the mechanical properties of glass fiber reinforced polymer sandwich structures is examined for the application of wind turbine blade shell repairs. Reference shell specimens are tested under fully-reversed cyclic loading to understand the fatigue behavior of the sub-component structure within a range of in-service loads, to which shell specimens with a scarf joint repair are compared. A fatiguesuperior repair material is shown to improve the fatigue behavior of the repaired structures compared to the reference specimens. In separating layup and geometry, damage development is examined on the subcomponent scale for a structural understanding of a scarf repair using in-situ digital image correlation-based strain field measurements as well as passive thermography. Within scarf repair variables, the geometry is shown to play a larger role than layup in the fatigue performance of the repaired structure. KW - Polymer–matrix composites KW - Fatigue KW - Joints/joining PY - 2023 DO - https://doi.org/10.1016/j.compositesa.2022.107419 SN - 1359-835X VL - 167 SP - 1 EP - 11 PB - Elsevier Ltd. AN - OPUS4-56942 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ivanov, V.V. A1 - Tielemann, Christopher A1 - Avramova, K. A1 - Reinsch, Stefan A1 - Tonchev, V. T1 - Modelling crystallization: When the normal growth velocity depends on the supersaturation N2 - The crystallization proceeds by the advance of the crystal faces into the disordered phase at the expense of the material excess, the supersaturation. Using a conservation constraint for the transformation ratio α∈[0,1] as complementing the rescaled supersaturation to 1 and a kinetic law for the normal growth velocity as function of the supersaturation raised to power g, the growth order, we derive an equation for the rate of transformation dα/dt. We integrate it for the six combinations of the three spatial dimensions D = 1, 2, 3 and the two canonical values of g = 1, 2 towards obtaining expressions for αDg. The same equation, with g = 1 and D = n (n is the so called Avrami exponent) is obtained when taking only the linear in α term from the Taylor’s expansion around α = 0 of the model equation of Johnson-Mehl-Avrami-Kolmogorov (JMAK). We verify our model by fitting datasets of α21 and α31 (from α = 0 to αupper = 0.999) with JMAK to obtain from the fit n = 1.725, 2.43, resp. We show further how the values of n depend on the value of αupper to which the fit is performed starting always from 0. Towards building a validation protocol, we start with validating α21 with published results. KW - Crystallization KW - Supersaturation KW - Growth kinetics KW - Growth rate KW - JMAK model PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581706 DO - https://doi.org/10.1016/j.jpcs.2023.111542 SN - 0022-3697 VL - 181 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-58170 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Paskin, A. A1 - Couasnon, T. A1 - Perez, J. P. H. A1 - Lobanov, S. S. A1 - Blukis, R. A1 - Reinsch, Stefan A1 - Benning, L. G. T1 - Nucleation and Crystallization of Ferrous Phosphate Hydrate via an Amorphous Intermediate N2 - The fundamental processes of nucleation and crystallization are widely observed in systems relevant to material synthesis and biomineralization; yet most often, their mechanism remains unclear. In this study, we unravel the discrete stages of nucleation and crystallization of Fe3(PO4)2·8H2O (vivianite). We experimentally monitored the formation and transformation from ions to solid products by employing correlated, time-resolved in situ and ex situ approaches. We show that vivianite crystallization occurs in distinct stages via a transient amorphous precursor phase. The metastable amorphous ferrous phosphate (AFEP) intermediate could be isolated and stabilized. We resolved the differences in bonding environments, structure, and symmetric changes of the Fe site during the transformation of AFEP to crystalline vivianite through synchrotron X-ray absorption spectroscopy at the Fe K-edge. This intermediate AFEP phase has a lower water content and less distorted local symmetry, compared to the crystalline end product vivianite. Our combined results indicate that a nonclassical, hydration-induced nucleation and transformation driven by the incorporation and rearrangement of water molecules and ions (Fe2+ and PO4 3−) within the AFEP is the dominating mechanism of vivianite formation at moderately high to low vivianite supersaturations (saturation index ≤ 10.19). We offer fundamental insights into the aqueous, amorphous-to-crystalline transformations in the Fe2+−PO4 system and highlight the different attributes of the AFEP, compared to its crystalline counterpart. KW - Nucleation KW - Crystallization KW - Vivianite KW - Ferrous phosphate hydrate PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580696 DO - https://doi.org/10.1021/jacs.3c01494 SN - 0002-7863 VL - 145 IS - 28 SP - 15137 EP - 15151 PB - ACS Publications AN - OPUS4-58069 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fareed, Adnan A1 - Rosalie, Julian M. A1 - Kumar, Sourabh A1 - Kar, S. A1 - Hickel, Tilmann A1 - Fähler, S. A1 - Maaß, Robert T1 - Constrained incipient phase transformation in Ni-Mn-Ga films: A small-scale design challenge N2 - Ni-Mn-Ga shape-memory alloys are promising candidates for large strain actuation and magnetocaloric cooling devices. In view of potential small-scale applications, we probe here nanomechanically the stress-induced austenite–martensite transition in single crystalline austenitic thin films as a function of temperature. In 0.5 μm thin films, a marked incipient phase transformation to martensite is observed during nanoindentation, leaving behind pockets of residual martensite after unloading. These nanomechanical instabilities occur irrespective of deformation rate and temperature, are Weibull distributed, and reveal large spatial variations in transformation stress. In contrast, at a larger film thickness of 2 μm fully reversible transformations occur, and mechanical loading remains entirely smooth. Ab-initio simulations demonstrate how an in-plane constraint can considerably increase the martensitic transformation stress, explaining the thickness-dependent nanomechanical behavior. These findings for a shape-memory Heusler alloy give insights into how reduced dimensions and constraints can lead to unexpectedly large transformation stresses that need to be considered in small-scale actuation design. KW - Shape-memory alloys KW - Nanoindentation KW - Incipient plasticity KW - NiMaGa PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581422 DO - https://doi.org/10.1016/j.matdes.2023.112259 VL - 233 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-58142 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krauklis, A. E. A1 - Starovka, O. A1 - Gibhardt, D. A1 - Aouissi, H. A. A1 - Burlakovs, J. A1 - Sabalina, A. A1 - Fiedler, Bodo A1 - Kalinka, Gerhard T1 - Reversible and irreversible effects on the epoxy GFRP fiber-matrix interphase due to hydrothermal aging N2 - Epoxy R-Glass Fiber-Reinforced Polymer (GFRP) composite plates were hydrothermally aged at 60 ◦C for 23, 75, and 133 days. The water content reached 0.97 wt%, 1.45 wt% and 1.63 wt%, respectively. The studied GFRP matrix was inert to hydrolysis or chain scission, allowing for investigation of irreversible changes in the fiber-matrix interphase due to hydrothermal aging upon re-drying. During each period, a subset of the specimens was removed from the water bath and dried in a chamber. The weight loss upon drying was explained with epoxy leaching (impurities), sizing-rich interphase hydrolysis, glass fiber surface hydrolysis, accumulated degradation products escaping, and water changing state from bound to free. The influence of hydrothermal aging on the fiber-matrix interfacial properties was investigated. Lower interfacial strength of hydrothermally aged (wet) samples was attributed to plasticization of the epoxy, plasticization and degradation of the sizing-rich interphase (including formation of hydrolytic flaws), and hydrolytic degradation of the glass fiber surface. The kinetics of epoxy-compatible epoxysilane W2020 sizing-rich interphase hydrolysis provided an estimate of ca. 1.49%, 4.80%, and 8.49% of the total composite interphase degraded after 23, 75, and 133 days, respectively. At these conditions, the interface lost 39%, 48%, and 51% of its strength. Upon re-drying the specimens, a significant part of the interfacial strength was regained. Furthermore, an upward trend was observed, being 13%, 10% and 3% strength, respectively; thus, indicating a possibility of partial recovery of properties. KW - GFRP KW - Hydrothermal Ageging KW - Interphase KW - Water Diffusion KW - Desorption KW - Interfacial Strength PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581554 DO - https://doi.org/10.1016/j.jcomc.2023.100395 SN - 2666-6820 VL - 12 SP - 1 EP - 9 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-58155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ginés-Palomares, J.-C. A1 - Fateri, M. A1 - Schubert, T. A1 - de Peindray d’Ambelle, L. A1 - Simon, Sebastian A1 - Gluth, Gregor A1 - Günster, Jens A1 - Zocca, Andrea T1 - Material aspects of sintering of EAC-1A lunar regolith simulant N2 - Future lunar exploration will be based on in-situ resource utilization (ISRU) techniques. The most abundant raw material on the Moon is lunar regolith, which, however, is very scarce on Earth, making the study of simulants a necessity. The objective of this study is to characterize and investigate the sintering behavior of EAC-1A lunar regolith simulant. The characterization of the simulant included the determination of the phase assemblage, characteristic temperatures determination and water content analysis. The results are discussed in the context of sintering experiments of EAC-1A simulant, which showed that the material can be sintered to a relative density close to 90%, but only within a very narrow range of temperatures (20–30 °C). Sintering experiments were performed for sieved and unsieved, as well as for dried and non-dried specimens of EAC-1A. In addition, an analysis of the densification and mechanical properties of the sintered specimens was done. The sintering experiments at different temperatures showed that the finest fraction of sieved simulant can reach a higher maximum sintering temperature, and consequently a higher densification and biaxial strength. The non-dried powder exhibited higher densification and biaxial strength after sintering compared to the dried specimen. This difference was explained with a higher green density of the non-dried powder during pressing, rather than due to an actual influence on the sintering mechanism. Nevertheless, drying the powder prior to sintering is important to avoid the overestimation of the strength of specimens to be fabricated on the Moon. KW - Lunar regolith KW - Ceramics KW - Microstructure KW - Sintering KW - Softening temperature PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-592668 DO - https://doi.org/10.1038/s41598-023-50391-y SN - 2045-2322 VL - 13 SP - 1 EP - 14 PB - Springer Nature AN - OPUS4-59266 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -