TY - CONF A1 - Kiefer, P. A1 - Deubener, J. A1 - Waurischk, Tina A1 - Balzer, R. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Behrens, H. T1 - Subcritical crack growth in water bearing soda-aluminosilicate glasses N2 - The subcritical crack growth in water bearing soda-aluminosilicate glasses is compared to the crack growth in a commercial soda-lime silicate glass. The water speciation is shown for comparison of water species in the material. Differences will be discussed in the poster session. T2 - Glastechnische Tagung 2019 CY - Nürnberg, Germany DA - 13.05.2019 KW - Glass KW - Crack growth KW - Vickers KW - Water speciation PY - 2019 AN - OPUS4-48343 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Kremberg, Jan T1 - Betriebsfestigkeit von Struktur-Klebungen im Anwendungsgebiet der CS22 N2 - Moderne Segelflugzeuge sind voll-verklebte tragende FKV-Strukturen. Über die Schwingfestigkeit der Faser-Kunststoff-Verbunde (FKV) und die Lebensdauerabschätzung dieser Werkstoffklasse auf Basis verschiedener Lastspektren wurden insbesondere von Christoph Kensche verschiedenen Arbeiten durchgeführt und auch auf dem Symposium für Segelflugzeugentwicklung vorgestellt. Hingegen ist die Betriebsfestigkeit von Struktur-Klebungen im Anwendungsbereich der CS22 vergleichsweise wenig untersucht worden. Über die Jahre wurden in verschiedenen Projekten immer wieder Probleme in Struktur-Klebungen (u.a. Betriebsbelastungsversuche an Versuchs-Holmen) identifiziert, analysiert und spezielle Prüfverfahren weiter entwickelt (Projekt „Tragflügel neuer Technologie für die allgemeine Luftfahrt“, FK SIF765). Im Rahmen des LuFo-Vorhabens GeAviBoo (General Aviation Booster) wurde in zwei Arbeitspaketen das Thema erneut aufgegriffen und Betriebsbelastungsversuche an Klebproben durchgeführt. Im Rahmen des Vortrages werden die Erkenntnisse der letzten 10 Jahre aufbereitet und die neusten Ergebnisse vorgestellt. T2 - Symposium für Segelflugzeugentwicklung CY - Online meeting DA - 19.11.2020 KW - Polymer Matrix Composites KW - Betriebsfestigkeit KW - Klebung KW - General Aviation PY - 2020 AN - OPUS4-51861 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker T1 - Composite materials - focus polymer matrix composites (PMC) N2 - Lecture about polymer matrix composites as part of the first trainings event GW4SHM, properties, production, basic theory, testing. T2 - 1. Training GW4SHM-Project CY - BAM, Berlin, Germany DA - 23.11.2020 KW - Polymer matrix composites KW - Composite testing KW - NDT PY - 2020 AN - OPUS4-51868 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ávila Calderón, Luis Alexander T1 - Mechanical behaviour of AM metals: Creep of LPBF 316L and low-cycle-fatigue of LMD Ti-6Al-4V N2 - Additively manufactured metallic materials have already started to find application in safety-relevant components. However, this has only happened for certain materials and specific applications and loading conditions, since there is still an extensive lack of knowledge as well as of historical data regarding their mechanical behaviour. This contribution aims to address this lack of understanding and historical data concerning the creep behaviour of the austenitic stainless steel 316L manufactured by Laser-Powder-Bed-Fusion (L-PBF) and the low-cycle-fatigue behaviour of the titanium alloy Ti-6Al-4V manufactured by Laser-Metal-Deposition (LMD). Furthermore, it aims to assess their mechanical behaviour against their conventional counterparts. With that in mind, specimens from conventional and additive materials are tested and their mechanical behaviour analysed based on characteristic curves. To understand the damage behaviours the materials are characterized by destructive and non-destructive techniques before and after failure. T2 - 1st Workshop on In-situ Monitoring and Microstructure Development in Additive Manufacturing CY - Online Meeting DA - 10.12.2020 KW - Ti-6Al-4V KW - 316L KW - Additive manufacturing KW - Creep behaviour KW - Low-cycle-fatigue behaviour PY - 2020 AN - OPUS4-51879 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Fedelich, Bernard A1 - Feldmann, Titus A1 - Haftaoglu, Cetin A1 - Nolze, Gert A1 - Schriever, Sina A1 - Epishin, A. A1 - Camin, B. A1 - Lopez-Galilea, I. A1 - Ruttert, B. A1 - Theisen, W. T1 - Untersuchung des Kriechverhaltens einer Nickelbasis-Superlegierung bei ultrahohen homologen Temperaturen und Anwendung auf das heiß-isostatische Pressen (HIP) N2 - Mit Hilfe des HIP-Verfahrens („Hot Isostatic Pressing“) werden Poren in der einkristallinen Nickel-Basis Superlegierung CMSX-4 kontinuierlich geschrumpft und dadurch die nach der Erstarrung und der Wärmebehandlung vorhandene Porosität stark reduziert. In diesem Beitrag werden experimentelle und numerische Untersuchungen zu den Mechanismen der Porenschrumpfung zusammengefasst. Es zeigt sich, dass das Verformungsverhalten während Kriechversuchen bei der HIP-Temperatur durch Versetzungsgleitung auf oktaedrischen Ebenen dominiert wird. Dagegen zeigen Messungen der Porositätsabnahme und Simulationen des Porenschließens, dass die Kinetik der Porenschrumpfung durch das Phänomen der Leerstellendiffusion zwischen Poren und Kleinwinkelkorngrenzen („Low Angle Boundary“, LAB) bestimmt wird. Im Gegensatz führt die klassische Kristallviskoplastizität zu einer systematischen Überschätzung dieser Kinetik. Der scheinbare Widerspruch lässt sich auflösen, wenn man bedenkt, dass auf der Skala der Poren Versetzungsquellen nicht gleichmäßig verteilt sind, wie in der konventionellen Kristallplastizität implizit angenommen wird. Stattdessen wird in einem weiterführenden Modell davon ausgegangen, das Kleinwinkelkorngrenzen (LABs) als Versetzungsquellen fungieren, während die Scherspannungen sehr stark in der Nähe der Poren lokalisiert sind, was die Emission von Versetzungen deutlich reduziert. T2 - Langzeitverhalten warmfester Stähle und Hochtemperaturwerkstoffe CY - Online meeting DA - 27.11.2020 KW - HIP KW - Superlegierung KW - Kriechen PY - 2020 AN - OPUS4-51795 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Fedelich, Bernard A1 - Feldmann, Titus A1 - Haftaoglu, Cetin A1 - Nolze, Gert A1 - Schriever, Sina A1 - Epishin, A. A1 - Camin, B. A1 - Lopez-Galilea, I. A1 - Ruttert, B. A1 - Theisen, W. T1 - Untersuchung des Kriechverhaltens einer Nickelbasis-Superlegierung bei ultrahohen homologen Temperaturen und Anwendung auf das heiß-isostatische Pressen (HIP) N2 - Mit Hilfe des HIP-Verfahrens („Hot Isostatic Pressing“) werden Poren in der einkristallinen Nickel-Basis Superlegierung CMSX-4 kontinuierlich geschrumpft und dadurch die nach der Erstarrung und der Wärmebehandlung vorhandene Porosität stark reduziert. In diesem Beitrag werden experimentelle und numerische Untersuchungen zu den Mechanismen der Porenschrumpfung zusammengefasst. Es zeigt sich, dass das Verformungsverhalten während Kriechversuchen bei der HIP-Temperatur durch Versetzungsgleitung auf oktaedrischen Ebenen dominiert wird. Dagegen zeigen Messungen der Porositätsabnahme und Simulationen des Porenschließens, dass die Kinetik der Porenschrumpfung durch das Phänomen der Leerstellendiffusion zwischen Poren und Kleinwinkelkorngrenzen („Low Angle Boundary“, LAB) bestimmt wird. Im Gegensatz führt die klassische Kristallviskoplastizität zu einer systematischen Überschätzung dieser Kinetik. Der scheinbare Widerspruch lässt sich auflösen, wenn man bedenkt, dass auf der Skala der Poren Versetzungsquellen nicht gleichmäßig verteilt sind, wie in der konventionellen Kristallplastizität implizit angenommen wird. Stattdessen wird in einem weiterführenden Modell davon ausgegangen, das Kleinwinkelkorngrenzen (LABs) als Versetzungsquellen fungieren, während die Scherspannungen sehr stark in der Nähe der Poren lokalisiert sind, was die Emission von Versetzungen deutlich reduziert. T2 - Langzeitverhalten warmfester Stähle und Hochtemperaturwerkstoffe CY - Online meeting DA - 27.11.2020 KW - HIP KW - Superlegierung KW - Kriechen PY - 2020 SN - 978-3-946885-95-5 VL - 2020 SP - 28 EP - 39 PB - Forschungsvereinigung Warmfeste Stähle und Hochtemperaturwerkstoffe AN - OPUS4-51796 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Evolution of CFRP stress cracks observed by in situ X-ray refractive imaging N2 - Modern air-liners and wind turbine rotor blades are made up primarily of fiber reinforced plastics. Failure of these materials heavily impairs the serviceability and the operational safety. Consequently, knowledge of the failure behavior under static and cyclic loads is of great interest to estimate the operational strength and to compare the performance of different materials. Ideally, the damage evolution under operational load is determined with in-situ non-destructive testing techniques. Here, we report in-situ synchrotron X-ray imaging of tensile stress induced cracks in carbon fiber reinforced plastics due to inter-fiber failure. An inhouse designed compact tensile testing machine with a load range up to 15 kN was integrated into the beamline. Since conventional radiographs do not reveal sufficient contrast to distinguish cracks due to inter-fiber failure and micro cracking from fiber bundles, the Diffraction Enhanced Imaging (DEI) technique is applied in order to separate primary and scattered (refracted) radiation by means of an analyzer crystal. This technique allows fast measurements over large fields-of-view and is ideal for in-situ investigations. T2 - 12th BESSY@HZB User Meeting 2020 CY - Online meeting DA - 10.12.2020 KW - Carbon Fiber Reinforced Plastics KW - Crack evolution KW - Diffraction Enhanced Imaging KW - In situ tensile test KW - X-ray refraction PY - 2020 AN - OPUS4-51802 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mrkwitschka, Paul A1 - Abram, Sarah-Luise A1 - Kuchenbecker, Petra A1 - Würth, Christian A1 - Rühle, Bastian A1 - Resch-Genger, Ute A1 - Hodoroaba, Vasile-Dan T1 - Fine iron oxide nanoparticles as a candidate reference material for reliable measurement of particle size N2 - Background, Motivation and Objective Nanomaterials are at the core of some of the 21st century’s most promising technologies. In order to utilize and rationally design materials at the nanoscale the reliable characterization of their physico-chemical properties is highly important. Furthermore, the European Commission has taken measures via the REACH Regulations to control the classification of nanomaterials. REACH Annexes which entered into force in January 2020 require manufacturers to register nanomaterials that are traded in larger quantities (at least 1 ton). Every powder or dispersion where 50% (number distribution) of the constituent particles have sizes ≤ 100 nm in at least one dimension are defined as a nanomaterial. This creates a need for both industrial manufacturers and research and analytical service facilities to reliably characterize potential nanomaterials. Currently, BAM is working on developing reference nanoparticles, which shall expand the scarce list of worldwide available nano reference materials certified for particle size distribution, but also targeting other key parameters such as shape, structure (including porosity) and functional properties. Thus, candidate materials are considered to complement the already available spherical and monodisperse silica, Au and polystyrene reference nanoparticles, e.g. iron oxide and titanium oxide, with an average atomic number between those of silica and gold. Particularly for the imaging by electron microscopies, new nanoparticles of well-defined size in the range of 10 nm are decisive for the accurate particle segmentation by setting precise thresholds. Statement of Contribution/Methods Synthesis: Highly monodisperse iron oxide nanoparticles can be synthesized in large quantities by thermal decomposition of iron oleate or iron acetylacetonate precursors in high boiling solvents such as octadecene or dioctyl ether in the presence of oleic acid and oleylamine as capping agents. Scanning Electron Microscope: An SEM of type Supra 40 from Zeiss has been used including the dedicated measurement mode transmission in SEM (STEM-in-SEM) with a superior material contrast for the nanoparticle analysis. The software package ImageJ has been used for the analysis of the STEM-in-SEM images and to determine the particle size distribution. Dynamic Light scattering (DLS): Particles in suspension were measured in comparison by means of Zetasizer Nano (Malvern Panalytical; cumulants analysis) and NanoFlex (Microtrac; frequency power spectrum). Results/Discussion In this study iron oxide nanoparticles synthesized at BAM and pre-characterized by DLS, SEM (including the transmission mode STEM-in-SEM) are presented. The particles are spherical and highly monodisperse with sizes slightly larger than 10 nm. T2 - Nanosafe 2020 CY - Online meeting DA - 16.11.2020 KW - Reference nanomaterials KW - Imaging techniques KW - Size and size distribution KW - Reliable characterization KW - Iron oxide nanoparticles PY - 2020 AN - OPUS4-51767 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Welter, T. A1 - Müller, Ralf A1 - Deubener, J. A1 - Marzok, Ulrich A1 - Reinsch, Stefan T1 - Hydrogen Permeation Through Glass N2 - Physical storage of gaseous hydrogen under high-pressure in glassy micro-containers such as spheres and capillaries is a promising concept for enhancing safety and the volumetric capacity of mobile hydrogen storage systems. As very low permeation through the container wall is required for storage of compressed hydrogen, development of glasses of minimal hydrogen permeability is needed. For this purpose, one has to understand better the dependence of hydrogen permeability on glass structure. The paper points out that minimizing the accessible free volume is as one strategy to minimize hydrogen permeability. Based on previously measured and comprehensive literature data, it is shown that permeation is independently controlled by ionic porosity and network modifier content. Thus, ionic porosity in modified and fully polymerized networks can be decreased equally to the lowest hydrogen permeability among the glasses under study. Applying this concept, a drop of up to 30,000 with respect to the permeation of hydrogen molecules through silica glass is attainable. KW - Ionic porosity KW - hydrogen storage KW - Glass KW - Permeability KW - Solubility KW - Diffusivity PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513927 DO - https://doi.org/10.3389/fmats.2019.00342 VL - 6 SP - Article 342 AN - OPUS4-51392 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kuchenbecker, Petra T1 - Praktische Erfahrungen zur Granulometrie von Pulvern im Submikron- und Nanobereich N2 - Der Vortrag beleuchtet insbesondere die Herausforderungen die sich bei der Dispergierung der Nanopulver aufgrund der hohen Adhäsivkräfte ergeben. Die Bewertung der Probenpräparation ist nur indirekt zugänglich, aber essentiell für die Zuverlässigkeit der Messergebnisse. Anhand von Beispielen werden Lösungsvorschläge aufgezeigt. Der Vortrag schließt mit einem Vorschlag zur Strategie der Herangehensweise bei der Partikelgrößenbestimmung von Nanopulvern. T2 - Sitzung des Fachausschusses "Material- und Prozessdiagnostik" der Deutschen Keramischen Gesellschaft: Zuverlässige granulometrische Charakterisierung von Mikro- und Nanopulvern – Voraussetzung für optimierte Keramikwerkstoffe in der Energietechnik CY - Online meeting DA - 19.11.2020 KW - Nano-powder KW - particle size determination KW - dispersion KW - sample preparation PY - 2020 AN - OPUS4-51665 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ernst, A. A1 - Klein, S. A1 - Hall, T. A1 - Avila, Luis A1 - Bähre, D. T1 - Electrochemical dressing of hard tools for abrasive precision machining N2 - In this study an approach for dressing metallic bonded honing stones with hard cutting grains on the basis of electrolysis is investigated. By a combination of concepts from electrochemical machining (ECM) and electropolishing a test rig was designed and put into operation. In general, it can be stated that the Approach investigated in this paper has proved to be a suitable dressing method for honing stones. However, the dressing result is highly dependent on bond components, cutting grain size and concentration which lead to local differences in the material removal and irregular topographies. This could be overcome, for example, by setting the dressing parameters more precisely based on the best results presented in this paper. T2 - International Symposium on ElectroChemical Machining Technology CY - Saarbrücken, Germany DA - 14.11.2019 KW - Irregular topography KW - Honing KW - Electrochemical dressing KW - Honing Stone KW - Laser Scanning Microscopy KW - Electropolishing PY - 2019 SN - 978-3-00-064086-5 SP - 96 EP - 108 PB - Fertigungstechnik Saarbrücken CY - Saarbrücken AN - OPUS4-49490 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Klingelhöffer, Hellmuth T1 - Temperaturschwankungen an Extensometern - ein vielfach vernachlässigtes Thema N2 - Extensometer sind seit Jahrzehnten im Einsatz und bilden die Basis für eine präzise Dehnungsmessung in werkstoffmechanischen Versuchen. Jedoch ist die Temperaturstabilität von Extensometern häufig noch nicht ausreichend beachtet worden, um Fehler verursacht durch Temperaturschwankungen zu minimieren. Dieses wird derzeit nicht nur in Deutschland, sondern auch international zunehmend diskutiert. Datenblätter von Extensometern sind teils unvollständig besonders hinsichtlich von Temperatureinflüssen. Extensometer für den Einsatz bei höheren Temperaturen sollen z.B. laut Normen für dehnungsgeregelte Ermüdungsversuche mit Luft oder Wasser aktiv gekühlt werden. Jedoch schreiben die Normen keine Temperatur-Toleranzen für Extensometer vor. Dehnungsfehler verursacht durch Temperaturschwankungen am Extensometer bleiben meist verborgen, da die Temperatur des Extensometers standardmäßig gar nicht gemessen wird. Die Ursache von Einflüssen zur Temperaturstabilität von Extensometern wird erläutert. Ein einfaches Rechenbeispiel zeigt die Empfindlichkeit von Extensometern gegenüber Temperaturschwankungen und die Auswirkungen auf den Dehnungsfehler. Lösungsmöglichkeiten zur Optimierung werden aufgezeigt. Der Anwender von Extensometern soll sensibilisiert werden, um der Temperaturstabilität von Extensometern sowohl hinsichtlich Herstellerspezifikationen als auch bei der Anwendung von Extensometern im Prüflabor mehr Aufmerksamkeit zu schenken, um letztlich die Qualität von Versuchsergebnissen zu verbessern. Empfehlungen an Extensometerhersteller werden formuliert. Dieses Thema wird zukünftig auch in Prüfnormen mehr Aufmerksamkeit geschenkt werden. Es werden Maßnahmen zur Verbesserung der Temperaturstabilität von Extensometern Einzug in Prüfnomen finden, um letztlich verlässlichere Versuchsergebnisse zu erhalten. Es ist beabsichtigt, eine Verbesserung der Temperaturstabilität von Extensometern z.B. bei der nächsten Revision der Prüfnormen ISO 12106 und ISO 12111 für dehnungsgeregelte LCF- und TMF-Versuche zu berücksichtigen. T2 - Werkstoffprüfung 2019 CY - Neu-Ulm, Germany DA - 03.12.2019 KW - Extensometer KW - Temperaturschwankungen KW - Dehnungsfehler PY - 2019 AN - OPUS4-49961 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Klingelhöffer, Hellmuth T1 - Temperaturschwankungen an Extensometern - ein vielfach vernachlässigtes Thema N2 - Extensometer werden seit langer Zeit erfolgreich für die Ermittlung von werkstoffmecha-nischen Kennwerten eingesetzt. Allerdings wurden in den letzten Jahren immer wieder durch Temperaturschwankungen bedingte Drift an Extensometern festgestellt, die be-sonders in Langzeitversuchen zu Problemen führen können. Es wurden Ursachen für die thermische Drift von Extensometern aufgezeigt. Anhand von einem Beispiel wurde gezeigt, wie sich Temperaturschwankungen an einem Extensometer auf die Ergebnisse von werkstoffmechanischen Ermüdungsversuchen auswirken können. An einem weiteren Beispiel wurde beschrieben, dass der durch Temperaturschwankungen verursachte Dehnungsfehler eines Extensometers stark von der Höhe der Temperaturschwankung und von der Dehnungsschwingbreite abhängt und, je nach Anwendungsfall größer als 1% werden kann. Es wurde verdeutlicht, dass bisherige nach Norm vorgeschriebene Maß-nahmen oft nicht ausreichen, um Einflüsse von Temperaturschwankungen am Extenso-meter zuverlässig zu unterbinden. Vorschläge wurden aufgezeigt, um die Temperatursta-bilität von Extensometern zu verbessern. Das gesamte Temperaturmanagement von Raumtemperatur, Kühlwassertemperatur, Temperaturmessung am Extensometer etc. sollte von Grund auf neu betrachtet werden, um Verbesserungen bei der Temperatur-konstanz von Extensometern zu erlangen. Ferner wurde vorgeschlagen, Extensometer in temperaturkompensierter Ausführung zu entwickeln und zu verkaufen. Dieses sollte Ret-rofits für existierende Extensometer miteinschließen. Konkrete Maßnahmen zur Imple-mentierung in Materialprüfungsnormen müssen weiter diskutiert werden. T2 - Tagung Werkstoffprüfung 2019 CY - Neu-Ulm, Germany DA - 03.12.2019 KW - Extensometer KW - Temperaturschwankungen KW - Dehnungsfehler PY - 2019 SN - 978-3-88355-418-1 SP - 361 EP - 366 PB - Inventum GmbH CY - Sankt Augustin AN - OPUS4-49965 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stephan-Scherb, Christiane T1 - Materialschädigung durch Hochtemperaturkorrosion von koventionellen und innovativen Legierungssystemen N2 - Konventionelle und innovative Hochtemperaturwerkstoffe sind im technischen Betrieb einer Vielzahl an Belastungen ausgesetzt. Neben mechanischen Beanspruchungen stellt die chemische Belastung durch das Vorhandensein von aggressiven und korrosiven Medien (SO2, CO2, O2, H2O…) bei hoher Temperatur einen Schlüsselfaktor dar, der die Langlebigkeit der Materialien im Einsatz beeinflusst. Neben konventionellen, mikroskopischen Analyseverfahren bieten röntgenbasierte Techniken Möglichkeiten, die Grenzflächenreaktionen zwischen dem Werkstoff und den Medien während der chemischen Belastung (in situ) zu untersuchen. Neuartige Einblicke in die zugrunde liegenden Prozesse der Schädigungsmechanismen werden anhand von klassischen ferritischen Legierungen beschrieben. Das Verständnis von Schlüsselfaktoren zur Induzierung eines Schutzmechanismus ist insbesondere für die Entwicklung von neuartigen Materialklassen wie Hochentropie- und chemisch komplexe Legierungen notwendig. Erste Einblicke in Schädigungsmechanismen durch Gaskorrosion dieser innovativen Materialsysteme werden vorgestellt. T2 - AWT-VDI Werkstofftechnik Arbeitskreis Bremen CY - Leibnitz Institut für Werkstofforientierte Technologien, Germany DA - 27.11.2019 KW - In situ KW - Heißgaskorrosion KW - Hochentropielegierungen KW - XRD PY - 2019 AN - OPUS4-49844 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von Hartrott, P. A1 - Rockenhäuser, Christian A1 - Metzger, M. A1 - Skrotzki, Birgit T1 - Assessment of EN AW-2618A for high temperature applications considering aging effects N2 - The alloy EN AW-2618A was assessed regarding its properties for high temperature applications considering aging effects. T2 - BAM TMF-Workshop 2019 CY - Berlin, Germany DA - 13.11.2019 KW - Alloy 2618A KW - Degradation KW - Coarsening KW - Transmission electron microscopy KW - Dark-field transmission electron microscopy (DFTEM) PY - 2019 AN - OPUS4-49808 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waurischk, Tina A1 - Müller, Ralf A1 - Balzer, R. A1 - Kiefer, P. A1 - Reinsch, Stefan A1 - Behrens, H. A1 - Deubener, J. T1 - Subcritical crack growth in hydrous soda-lime silicate glass N2 - Glass strength and fatigue is limited by surface cracks. As subcritical crack growth (SCCG) is governed by ambient humidity, stress corrosion at the crack tip is widely accepted to be the underlying mechanism. However, as water is known to have decisive effect on glass properties and can rapidly enter the crack tip near glass region, SCCG could be affected by such water related phenomena. We tried to mimic these effects studying water dissolution and speciation, mechanical properties, and SCCG in water-bearing glasses. For this purpose, glasses up to 8 wt% water have been prepared by means of high-pressure melting of glass powder - water mixtures. As part of this effort, SCCG in dry and hydrous commercial micros¬cope slide glass (CW = 6 wt%) was studied in double cantilever beam (DCB) geometry and sub-Tg relaxation was measured by Dynamic Mechanical Analysis (DMA). For SCCG in ambient air (24% r.h.), SCCG was promoted by the presence of 6wt% bulk water with respect to the dry glass. On the other hand, stress intensity values, KI, required to cause slow crack growth (v < 10-6 ms-1) resemble literature findings for float glass of similar composition in liquid water, which might represent the maximum possible promoting effect of ambient water on SCCG. For SCCG in vacuum (10-3 mbar), dissolved bulk water causes even more pronounced effects. Most strikingly, it strongly decreases the slope of the log v(KI)-curve, which is a measure of dissipated energy during fracture. A strong increase of sub-Tg relaxation with increasing water content was confirmed by DMA. As a consequence, slow crack growth occurs at KI values as measured in the dry glass whereas fast crack growth occurs at much larger KI than that of the dry glass. Kinks and shoulders shown by the inert log v(KI)-curve indicate that bulk water does not simply affect bulk mechanical properties. T2 - 9th Otto Schott Colloquium CY - Jena, Germany DA - 09.09.2019 KW - Internal friction KW - Soda-lime silicate glass KW - Crack growth KW - Water content KW - DCB PY - 2019 AN - OPUS4-49534 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Fedelich, Bernard A1 - Grützner, Stefan A1 - Haftaoglu, Cetin A1 - Kindrachuk, Vitaliy A1 - Vöse, Markus T1 - Möglichkeiten und Grenzen der rechnerischen Bewertung der Lebensdauer von Bauteilen unter TMF: Viskoplastische Modelle N2 - In diesem Vortrag wird auf einige noch offene Frage zur Anwendung der viskoplastischen Modellierung bei Hochtemperaturermüdung. Insbesondere auf das Problem der Parameterbestimmung wird eingegangen. T2 - Workshop "Konstitutive Viskoplastische Materialmodelle" CY - Institut für Werkstoffkunde (IfW), Technische Universität Darmstadt, Germany DA - 06.11.2019 KW - TMF KW - Viskoplastisch KW - Modell KW - Hochtemperaturermüdung KW - LCF PY - 2019 AN - OPUS4-49611 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Orlov, N. K. A1 - Milkin, P. V. A1 - Evdokimov, P. A. A1 - Putlayev, V. I. A1 - Günster, Jens T1 - Sintering of sodium and potassium tcp based ceramic for bone grafting application N2 - Biomaterials for bone replacement and grafting should possess sufficient strength, be bioresorbable and demonstrate osteoconductive and osteoinductive properties. However, resorption of modern materials for bone grafting (hydroxyapatite (HA) and tricalcium phosphate (TCP)) is reported, in some cases, to be not enough, this is why the search for more soluble compounds compared to HA and TCP looks very perspective. A possible way to increase ceramics solubility leads to partial substitution of Ca2+ -ions in Ca3(PO4)2 by alkali cations, like Na+ or/and K+. Improvement of solubility stems from decreasing lattice energy of a substituted phase, as well as the increase in hydration energy of the ions releasing from the phase to ambient solution. From this viewpoint, bioceramics based on compositions from Ca3(PO4)2 - CaKPO4 - CaNaPO4 ternary system seems to be prospective for bone replacement and grafting in the sense of resorption properties. At the same time, one should bear in mind that solubility level (resorbability) is governed not only by reduction of lattice energy but also by microstructure features. Grain sizes and porosity contribute much to dissolution rate making the study of sintering of the ceramics mentioned above highly important. To control Ca3(PO4)2 - CaKPO4 - CaNaPO4 based ceramic microstructure it is necessary to know possible phase transformations in the system and the way to manage microstructure by sintering schedule or sintering process. In this work, an isothermal section for phase diagram of Ca3(PO4)2 - CaKPO4 - CaNaPO4 ternary system is studied with several techniques. According to the XRD of quenched samples, this phase triangle has four single-phase areas at 1200˚C (Figure 1). It was shown that single-phase CaK0.6Na0.4PO4 cannot be sintered to full-dense ceramics by conventional sintering regardless time-temperature schedule. Two-step sintering technique, beneficial in the case of HA-ceramics, was unsuccessful in all cases of calcium-alkali phosphate compositions. However, field-assisted sintering techniques like, e.g. Spark Plasma Sintering (SPS), can overcome this problem due to significant impact on grain boundary diffusion. In connection with this fact, grains grow much slower retaining sintering process in a pore control regime. In this work CaK0.6Na0.4PO4 low-porous ceramics was also fabricated by FAST-methods of sintering. Moreover, other alternative sintering techniques, such as reaction sintering, may be useful in accelerating ions diffusion but stopping excessive grain growth.Strength properties of ceramics were evaluated by B3B-testing, micro- and nanoindentation techniques. Fracture toughness also becomes higher with potassium content increase, guiding porosity level. Resorption properties of sintered ceramics were studied in different solutions with pH=5 and 7.4. Acknowledgements. The research of sintering processes in calcium phosphate materials were funded by RFBR according to the research project № 18-33-00974. T2 - XVI ECerS Conference 2019 CY - Turin, Italy DA - 16.06.2019 KW - Phase transformations KW - Bioceramics KW - Mixed Ca-K-Na phosphates KW - Na and K rhenanites KW - Phase diagram PY - 2019 AN - OPUS4-49622 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Günster, Jens A1 - Zocca, Andrea T1 - Dense Powder Beds for the Additive Manufacturing of Ceramics N2 - Many of the most successful and precise additive manufacturing (AM) technologies are based on the deposition layer-by-layer of a flowable powder. Since the first pioneering work at the end of the 1980th many developments have been introduced, greatly extending the use of different materials, improving the physical properties of the components built and enhancing the accuracy of the process. Still very important issues remain nowadays, hampering a completely autonomous production of parts and even restricting the freedom of design by means of these technologies. One of the major issues is the low density and stability of the parts during the building process, which implies the need of support structures: The powder bed surrounding the part has an essential role, since it should support the structure during building, until it’s ready for removal. Moreover, the microstructure of the powder bed is a template for the microstructure of the part produced. In this context, the use of submicron ceramic powders is still a challenge. Three approaches for the stabilization and densification of powder beds will be presented: The Layerwise Slurry Deposition process LSD, the gas flow assisted powder deposition and the Laser Induced Slipcasting (LIS) of ceramic powder compacts. T2 - 43rd International Conference and Exposition on Advanced Ceramics and Composites (ICACC 2019) CY - Daytona Beach, FL, USA DA - 27.01.2019 KW - Ceramics KW - Additive Manufacturing PY - 2019 AN - OPUS4-49627 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Günster, Jens T1 - Powder-based Additive Manufacturing at Micro-Gravity N2 - Are we ready for putting a human footprint on Mars? Obviously, it is possible to send technologically challenging missions to our earth neighbors with a high level of complexity, such as enabling autonomous planetary mobility. As humanity contemplates mounting manned missions to Mars, strategies need to be developed for the design and operation of hospitable environments safely working in space for years. Humans require water and air provided by complicated equipment. Its safe operation is a great challenge and implies being prepared for all eventualities. Instead of foreseeing and preparing for all possible scenarios of machine failures and accidents, it appears logic taking advantage of the flexibility of humans and providing essential equipment for the reaction on critical situations. The supply of spare parts for repair and replacement of lost equipment would be one key pillar of such a strategy. Bearing in mind the absolute distance and flight trajectories for manned missions to Mars, supplying spare parts from Earth is impossible. Thus, in space manufacturing remains the only option for a timely supply. With a high flexibility in design and the ability to manufacture ready to use components directly from a computer aided model, additive manufacturing technologies appear extremely attractive. For metal parts manufacturing the Laser Beam Melting process is the most widely used additive manufacturing process in industrial application. However, envisioning the handling of metal powders in the absence of gravitation is one prerequisite for its successful application in space. A gas flow throughout the powder bed has been successfully applied to compensate for missing gravitational forces in micro gravity experiments. The so-called Gas Flow Assisted Powder Deposition is based on a porous building platform acting as a filter for the fixation of metal particles in a gas flow driven by a pressure difference maintained by a vacuum pump. T2 - 1st Sino-German Workshop on 3D Printing in Space CY - Beijing, China DA - 20.02.2019 KW - Zero-g KW - Additive Manufacturing KW - µ-gravity PY - 2019 AN - OPUS4-49628 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Günster, Jens T1 - Powder-based Additive Manufacturing at Micro-Gravity N2 - Are we ready for putting a human footprint on Mars? Obviously, it is possible to send technologically challenging missions to our earth neighbors with a high level of complexity, such as enabling autonomous planetary mobility. As humanity contemplates mounting manned missions to Mars, strategies need to be developed for the design and operation of hospitable environments safely working in space for years. Humans require water and air provided by complicated equipment. Its safe operation is a great challenge and implies being prepared for all eventualities. Instead of foreseeing and preparing for all possible scenarios of machine failures and accidents, it appears logic taking advantage of the flexibility of humans and providing essential equipment for the reaction on critical situations. The supply of spare parts for repair and replacement of lost equipment would be one key pillar of such a strategy. Bearing in mind the absolute distance and flight trajectories for manned missions to Mars, supplying spare parts from Earth is impossible. Thus, in space manufacturing remains the only option for a timely supply. With a high flexibility in design and the ability to manufacture ready to use components directly from a computer aided model, additive manufacturing technologies appear extremely attractive. For metal parts manufacturing the Laser Beam Melting process is the most widely used additive manufacturing process in industrial application. However, envisioning the handling of metal powders in the absence of gravitation is one prerequisite for its successful application in space. A gas flow throughout the powder bed has been successfully applied to compensate for missing gravitational forces in micro gravity experiments. The so-called Gas Flow Assisted Powder Deposition is based on a porous building platform acting as a filter for the fixation of metal particles in a gas flow driven by a pressure difference maintained by a vacuum pump. T2 - 2nd Sino-German Workshop on 3D Printing in Space CY - Berlin, Germany DA - 28.10.2019 KW - µ-gravity KW - Additive Manufacturing KW - Zero-g PY - 2019 AN - OPUS4-49629 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rabe, Torsten T1 - Alternative Verfahren zur Strukturierung von Grünfolien und Laminaten N2 - Die Strukturierung keramischer Grünfolien und Laminate ist ein wesentlicher Prozessschritt in der keramischen Multilayer-Technologie und begründet die funktionelle Vielfalt keramischer Multilayer. Benötigt wird die Grünbearbeitung für die Herstellung elektrischer und thermischer Vias sowie innerer Kavitäten und Kanäle für Transport und Lagerung von Gasen und Flüssigkeiten in hochintegrierten Schaltungsträgern, Sensoren und Reaktoren. Standardverfahren in der industriellen Fertigung sind Heißschneiden, Stanzen und Laserbearbeitung. Darüber hinaus werden auch Bohren, Fräsen, Sägen und Heißprägen verwendet. Über die Erprobung weiterer Verfahren wie Wasserstrahlschneiden, Dampfstrahlätzen und Powder Blasting wird in der Literatur berichtet. Im Vortrag werden spezifische Vor- und Nachteile der eingesetzten Verfahren beleuchtet. Abschließend werden die Kriterien für die Auswahl des optimalen Strukturierungsverfahrens diskutiert. Zusammensetzung und Gefüge sowie die dadurch bedingten mechanischen und thermomechanischen Eigenschaften sowie das Absorptionsverhalten von Grünfolien sind sehr unterschiedlich. Daraus resultieren unterschiedliche optimale Bearbeitbarkeitsparameter. T2 - DKG-Seminar "Foliengieß- und Schlitzdüsenverfahen" CY - Hermsdorf, Germany DA - 05.11.2019 KW - Stanzen KW - Keramische Folien KW - Laserbearbeitung KW - Grünfolieneigenschaften PY - 2019 AN - OPUS4-49742 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Charmi, Amir T1 - Mechanical anisotropy of additively manufactured stainless steel 316l: an experimental and numerical study N2 - This work aims for a yield function description of additively manufactured (AM) parts of stainless steel 316L at the continuum-mechanical macro-scale by means of so-called virtual experiments using a crystal plasticity model at meso-scale. T2 - 1st Workshop on In-situ Monitoring and Microstructure Development in Additive Manufacturing CY - BAM, Berlin DA - 10.12.2020 KW - Anisotropy KW - Crystal plasticity KW - Additive manufacturing PY - 2020 AN - OPUS4-51941 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schilling, Markus T1 - Tensile Test: From Standard to PMD Application Ontology N2 - Data analysis methods play an important role in both the experimental and simulation-based digital description of materials but have so far been poorly structured. The platform Material Digital (PMD) should contribute to a standardized description of data processing methods in materials research. The goal is the quality assurance of the processes and the output data, the acquisition and definition of their accuracy as well as the interoperability between applications. Therefore, application ontologies are created to explicitly describe processes and test methods. In this presentation, the first efforts in creating a tensile test application ontology in accordance with the ISO standard 6892-1:2019-11 are shown. Especially, the path of ontology development to be pursued based on standards was focused. T2 - Onboarding Workshop der Plattform Material Digital (PMD) CY - Online meeting DA - 13.04.2021 KW - Ontology KW - Platform MaterialDigital KW - PMD KW - Tensile Test KW - Normung KW - Standardization PY - 2021 AN - OPUS4-52425 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kuchenbecker, Petra T1 - Granulometry of Nano Powders - a Challenge Especially for the Dispersion Process N2 - The use of increasingly finer starting powders up to nanopowders can also be observed in the field of ceramics. Their advantages consist, for example, in their lower activation energy, an increase in strength or unique optical properties. However, handling and characterization of the powders are much more difficult. The main reason for this is the very high adhesive forces between the particles and between particles and other surfaces, too. Therefore, submicron and even more so nanoparticles tend to agglomerate and their separation into primary particles during sample preparation prior to particle sizing is of particular challenge. A representative measurement sample is only obtained when it no longer contains agglomerates. The evaluation of the dispersion process and a decision on whether it was successful thus increases in importance for the reliability of the measurement results of particle sizing. The presentation uses examples to show possible approaches and provides information on possible sources of error. It is shown that successful granulometric characterisation of fine powders requires both an improved dispersion technique and very often an effective combination of two or more measurement methods. KW - Agglomerates KW - Nano-powder KW - Dispersion process PY - 2021 SN - 0173-9913 VL - 98 IS - 2 SP - 47 EP - 54 PB - Göller Verlag GmbH CY - Baden-Baden AN - OPUS4-52504 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ganesh, Rahul A1 - Gesell, Stephan A1 - Kuna, M. A1 - Fedelich, Bernard A1 - Kiefer, B. T1 - Numerical calculation of ΔCTOD for thermomechanical fatigue crack growth N2 - The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model. It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value. N2 - Zur Bewertung des Rissfortschritts unter thermomechanischer Ermüdung (TMF) ist die zyklische Rissöffnungsverschiebung ΔCTOD ein aussichtsreicher bruchmechanischer Beanspruchungsparameter. In dieser Arbeit werden unter Anwendung eines viskoplastischen, temperaturabhängigen Materialmodells geeignete FEM-Techniken für die akkurate Berechnung des ΔCTOD bei TMF erprobt und verglichen. Als beste Technik hat sich die Verwendung kollabierter Rissspitzenelemente erwiesen. Es wurde ein effizienter FEM-Algorithmus zur Simulation der Rissausbreitung mit inkrementeller Neuvernetzung entwickelt, bei dem die Verformungen und inelastischen Zustandsvariablen jeweils vom alten auf das neue Netz übertragen werden. Die erarbeiteten Techniken werden am Beispiel von zweidimensionalen Strukturen und TMF-Proben vorgestellt und diskutiert. Dabei werden wesentliche Kontrollparameter der Simulation wie optimale Grösse der Rissspitzenelemente, Länge des Rissinkrementes in Relation zur plastischen Zone und dem ΔCTOD-Wert empfohlen. T2 - 53. Tagung des Arbeitskreises "Bruchmechanik und Bauteilsicherheit" CY - Online meeting DA - 18.02.2021 KW - Crack tip opening displacement KW - Thermomechanical fatigue KW - Crack growth PY - 2021 SP - 1 EP - 10 PB - DVM (Deutscher Verband für Materialforschung und -prüfung) CY - Berlin AN - OPUS4-52519 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ganesh, Rahul A1 - Gesell, Stephan A1 - Kuna, M. A1 - Fedelich, Bernard A1 - Kiefer, B. T1 - Numerical calculation of ΔCTOD for thermomechanical fatigue crack growth N2 - The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model. It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value. T2 - 53. Tagung des Arbeitskreises "Bruchmechanik und Bauteilsicherheit" CY - Online meeting DA - 18.02.2021 KW - Crack tip opening displacement KW - Thermomechanical fatigue KW - Crack growth PY - 2021 AN - OPUS4-52520 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stephan-Scherb, Christiane T1 - Novel insights into high temperature corrosion phenomena by advanced X-ray methods N2 - A variety of materials of technological interest change their properties through contact with reactive media. Solid-gas reactions lead to a variety of reaction products on the surfaces and internal interfaces. The observation of nucleation and growth processes in the environment where they occur (in situ) from a chemical-structural perspective is especially challenging for aggressive atmospheres. The talk presents innovative approaches to study corrosion mechanisms using advanced X-ray methods. Using energy dispersive X-ray diffraction and X-ray absorption spectroscopy in different tailor made environmental reaction chambers, valuable insights into high temperature oxidation and sulfidation processes were gained. Fe-based alloys were exposed to hot and reactive atmospheres containing gases like SO2, H2O and O2 at 650°C. During the gas exposure the tailor made reaction chambers were connected to a high energy diffraction end station at the synchrotron. The crystallization and growth of oxide and sulfide reaction products at the alloy surfaces were monitored by collecting full diffraction pattern every minute. Careful examination of shape and intensity of phase-specific reflections enabled to a detailed view on growth kinetics. These studies showed, oxides are the first phases occurring immediately after experimental start. As soon as reactive gas media enter the chamber, the conditions change and different reaction products, such as sulfides start to grow. A comparison of different gas environments applied, illustrated the differences in the type of reaction products. The in situ observation of high temperature material degradation by corrosion made it possible to study the contribution of phases, which are not stable at room temperature. For instance, wuestite (Fe1-xO), was frequently observed at high temperatures in humid gases on Fe with 2 wt.% and 9 wt.% chromium, but not at room temperature. The strength of the occurrence of this phase additionally explains why, despite a higher Cr content, ferritic alloys with 9 wt.% Cr in a challenging atmosphere prevent the intrinsic formation of protective layers. The in situ observations were supplemented by careful considerations of thermodynamic boundary conditions and detailed post characterization by classical metallographic analysis. Additionally, the structure and chemistry of the dominant oxide layers were evaluated using X-ray absorption near edge structure spectroscopy. The talk will give an overview about chances and challenges for studying high temperature corrosion phenomena by advanced X-ray methods. T2 - MRS Spring Meeting CT08.02.01 CY - Online Meeting DA - 18.04.2021 KW - XRD KW - Spectroscopy KW - Corrosion KW - High temperature KW - In-situ PY - 2021 AN - OPUS4-52486 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stargardt, Patrick T1 - Modeling of the cooling behavior of thermoelectric multilayers N2 - Multilayered designs are an attractive approach towards cost-effective manufacturing of thermoelectric generators. Therefore, efforts are being made to co-fire two promising thermoelectric oxides, namely calcium cobaltite and calcium manganate. In this study, ceramic tapes, multilayer technology, and pressure-assisted sintering (PAS) were used. A major challenge for the PAS of low-sintered calcium manganate was cracking during cooling. A relationship between the properties of the release tape used during PAS and the cracking behavior was experimentally observed. To understand the origin of failure, reaction layers in the multilayer were analyzed and thermal stresses during cooling were estimated by finite element (FE) simulations. Thermal expansion, elastic properties, and biaxial strength of the thermoelectric oxides and selected reaction layers were determined on separately prepared bulk samples. The analysis showed that the reaction layers were not the cause for cracking of calcium manganate. Using the FE model, thermal stresses in different manganate multilayer designs with varying properties of the release tape were studied. The FEM study indicated, and a validation experiment proved that the thickness of the release tape has the main effect on thermal stresses during cooling in separately sintered calcium manganate. T2 - Keramik 2021 / Ceramics 2021 CY - Online Meeting DA - 19.04.2021 KW - Fem KW - Thermoelectric KW - Pressure assisted sintering PY - 2021 AN - OPUS4-52489 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kuchenbecker, Petra T1 - Sample Preparation of Nano-Powders for Particle Size Determination N2 - The use of increasingly finer starting powders up to nanopowders can also be observed in the field of ceramics. Their advantages consist, for example, in their lower activation energy, an increase in strength or unique optical properties. However, handling and characterization of the powders are much more difficult. The main reason for this is the very high adhesive forces between the particles and between particles and other surfaces, too. Therefore, submicron and even more so nanoparticles tend to agglomerate and their separation into primary particles during sample preparation prior to particle sizing is of particular challenge. A representative measurement sample is only obtained when it no longer contains agglomerates. The evaluation of the dispersion process and a decision on whether it was successful thus increases in importance for the reliability of the measurement results of particle sizing. The presentation uses examples to show possible approaches and provides information on possible sources of error. It is shown that successful granulometric characterisation of fine powders requires both an improved dispersion technique and very often an effective combination of two or more measurement methods. T2 - 96. Jahrestagung der Deutschen Keramischen Gesellschaft CY - Online Meeting DA - 19.04.2021 KW - Agglomerates KW - Nano-powder KW - Dispersion process PY - 2021 AN - OPUS4-52503 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Abel, Andreas A1 - Zapala, P. A1 - Michels, H. A1 - Skrotzki, Birgit T1 - Microstructural evolution of Fe-26Al-4Mo-0.5Ti-1B with varying wall thicknesses N2 - With an increasing demand in more efficient fuel consumption to reduce CO2 emissions, weight reductions in high-temperature materials at affordable costs gain increasing attention. One potential candidate is the intermetallic material class of iron aluminides, combining the advantages in mass savings, high temperature performance and recyclability of resources. The alloy Fe-26Al-4Mo-0.5Ti-1B was selected to study the microstructural features evolving from two casting processes, five wall thicknesses and three final conditions. Conclusions are drawn upon the correlations of processing variables, grain sizes and hardness. T2 - DGM Fachausschuss "Intermetallische Phasen" CY - Online meeting DA - 09.02.2021 KW - Intermetallics KW - Iron aluminides KW - Fe-Al alloys KW - Wall thickness KW - Microstructure PY - 2021 AN - OPUS4-52288 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stephan-Scherb, Christiane A1 - Falk, Florian A1 - Lehmusto, J. A1 - Sobol, Oded A1 - Pint, B. T1 - Elucidation of competitive oxidation/sulfidation reactions on binary ferritic alloys N2 - Ferritic-austenitic chromia-forming alloys are frequently used as boiler tubes and heat exchanger materials for fossil-,biomass, and co-fired power plants. In all applied environments several strongly corrosive gaseous species such as CO2, SO2, SO3, H2O, O2 exist, causing materials degradation by high-temperature corrosion. The elucidation of degradation mechanisms introduced by multiple gases is challenging due to the presence of different oxidizing agents contributing to the competing reactions for oxidation, sulfurization or carburization. The degradation processes can be divided into initial stages, a transitional stage and the further proceeding steady-state oxidation reaction. Especially the long-term steady-state oxidation and further materials’ life-time are strongly dependent on the initial stages. The adsorption and absorption of the reactive species at the alloy surface and the growing oxide in the initial reaction is further influenced by dissociation and re-reactions of the gas phase molecules. To understand these mechanisms from a fundamental point of view in more detail, dedicated experiments and advanced characterization techniques on various length scale need to be applied. Real-time approaches using highly energetic synchrotron X-ray diffraction showed a high potential to enlighten competitively mechanisms by following the corrosion reactions in-situ in the environment they occur. Despite various other thin film characterization techniques, time of flight secondary ion mass spectroscopy (ToF-SIMS) is a powerful tool to visualize light atoms or labeled isotopes enabling the Differentiation between different oxidizing species. It was especially shown to be applicable in challenging atmospheres containing KCl deposits or in CO/CO2/O2 environments. The present study analyses the competing oxidation/sulfidation process in a humid atmosphere on two ferritic alloys with 2 and 9 % in weight chromium by in situ energy dispersive X-ray diffraction (EDXRD) and comparative tube furnace exposure using S16O2 and H2 18O atmosphere. T2 - Conference on High Temperature Corrosion and Protection of Materials HTCPM 2021 CY - Online Meeting DA - 29.03.2021 KW - Oxidation KW - High Temperature Corrosion KW - Ferritic Alloys KW - SIMS KW - EDXRD PY - 2021 AN - OPUS4-52363 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gesell, Stephan A1 - Ganesh, Rahul A1 - Kuna, Meinhard A1 - Fedelich, Bernard A1 - Kiefer, Björn T1 - Numerical calculation of ΔCTOD for thermomechanical fatigue crack growth N2 - The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model. It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value. T2 - ESIS Technical Meeting on Numerical Methods (TC8) CY - Online meeting DA - 06.04.2021 KW - Crack tip opening displacement KW - Thermomechanical fatigue KW - Crack growth PY - 2021 AN - OPUS4-52410 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bresch, Sophie T1 - Einfluss der Pulversynthese auf die Eigenschaften thermoelektrischer Oxide N2 - Calciumcobaltit und Calciummanganat gehören zu den vielversprechendsten thermoelektrischen Oxiden im Temperaturbereich zwischen 600 °C und 800 °C an Luft. Mittels thermoelektrischer Generatoren kann ein Temperaturgradient direkt in elektrische Leistung umgewandelt werden. Für die kostengünstige Pulverherstellung von Funktionsmaterialien wird im industriellen Maßstab meist die Festphasenreaktion (bzw. Kalzinierung) verwendet. Da es sich dabei um einen Hochtemperaturprozess handelt, ist diese Kalzinierung sehr energieintensiv. In der Literatur werden sehr unterschiedliche Prozessbedingungen zur Pulversynthese thermoelektrischer Oxide genutzt. Soweit dem Autor bekannt, ist keine systematische Untersuchung des Einflusses der Pulversynthesebedingungen auf die thermoelektrischen Eigenschaften publiziert. Deshalb wurde eine systematische Untersuchung des Einflusses der Pulversynthesebedingungen (Temperatur, Haltezeit, Partikelgröße, Wiederholungen) auf die thermoelektrischen Eigenschaften von Calciumcobaltit und Calciummanganat durchgeführt. Es konnte gezeigt werden, dass sich ein höherer Energieeintrag während der Kalzinierung negativ auf die thermoelektrischen Eigenschaften auswirkt. T2 - Seminar des Lehrstuhls für Funktionsmaterialien CY - Universität Bayreuth, Bayreuth, Germany DA - 12.01.2018 KW - Kalzinierung KW - Thermoelektrika KW - Calciummanganat KW - Calciumcobaltit PY - 2018 AN - OPUS4-43772 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thiede, Tobias A1 - Mishurova, Tatiana A1 - Cabeza, S. A1 - Nadammal, Naresh A1 - Bode, Johannes A1 - Kromm, Arne A1 - Haberland, C. A1 - Bruno, Giovanni T1 - An assessment of bulk residual stress in selective laser melted Inconel 718 N2 - Having been introduced almost two decades ago, Additive Manufacturing (AM) of metals has become industrially viable for a large variety of applications, including aerospace, automotive and medicine. Powder bed techniques such as Selective Laser Melting (SLM) based on layer-by-layer deposition and laser melt enable numerous degrees of freedom for the geometrical design. Developing during the manufacturing process, residual stresses may limit the application of SLM parts by reducing the load bearing capacity as well as induce unwanted distortion depending on the boundary conditions specified in manufacturing. The residual stress distribution in IN718 elongated prisms produced by SLM was studied non-destructively by means of neutron (bulk) and laboratory X-ray (surface) diffraction. The samples with different scanning strategies, i.e. hatching length, were measured in as-build condition (on a build plate) and after removal from the build plate. The absolute values of all stress components decreased after removal from the build plate. Together with surface scan utilizing a coordinate-measuring machine (CMM), it is possible to link the stress release to the sample distortion. Obtained results indicated different residual stress states for each of the transversal, longitudinal and normal component depending on the thermal gradient in the respective direction. T2 - ECNDT 2018 CY - Götheburg, Sweden DA - 11.06.2018 KW - Additive manufacturing KW - Ressidual stress KW - Neutron diffraction PY - 2018 AN - OPUS4-45761 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Thiede, Tobias A1 - Mishurova, Tatiana A1 - Cabeza, S. A1 - Nadammal, Naresh A1 - Bode, Johannes A1 - Haberland, C. A1 - Bruno, Giovanni T1 - An assessment of bulk residual stress in selective laser melted Inconel 718 N2 - Having been introduced almost two decades ago, Additive Manufacturing (AM) of metals has become industrially viable for a large variety of applications, including aerospace, automotive and medicine. Powder bed techniques such as Selective Laser Melting (SLM) based on layer-by-layer deposition and laser melt enable numerous degrees of freedom for the geometrical design. Developing during the manufacturing process, residual stresses may limit the application of SLM parts by reducing the load bearing capacity as well as induce unwanted distortion depending on the boundary conditions specified in manufacturing. The residual stress distribution in IN718 elongated prisms produced by SLM was studied non-destructively by means of neutron (bulk) and laboratory X-ray (surface) diffraction. The samples with different scanning strategies, i.e. hatching length, were measured in as-build condition (on a build plate) and after removal from the build plate. The absolute values of all stress components decreased after removal from the build plate. Together with surface scan utilizing a coordinate-measuring machine (CMM), it is possible to link the stress release to the sample distortion. Obtained results indicated different residual stress states for each of the transversal, longitudinal and normal component depending on the thermal gradient in the respective direction. T2 - VAMAS - Workshop CY - BAM, Berlin, Germany DA - 25.06.2018 KW - Additive manufacturing KW - Neutron diffraction KW - Ressidual stress PY - 2018 AN - OPUS4-45762 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waurischk, Tina A1 - Müller, Ralf A1 - Behrens, H. A1 - Deubener, J. A1 - Balzer, R. A1 - Kiefer, P. T1 - The influence of water as volatile on crack propagation in soda-lime silicate glass N2 - The talk was given at the Spring School of the SPP1594 in Hannover and summarizes the actual findings about crack growth in water bearing soda-lime silicate glass and a comparison to other oxide glasses. T2 - Spring School des SPP1594 CY - Hannover, Germany DA - 06.03.2018 KW - DCB KW - Soda-lime silicate glass KW - Crack growth KW - Vickers KW - Water speciation PY - 2018 AN - OPUS4-45699 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waurischk, Tina A1 - Kiefer, P. A1 - Balzer, R. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Behrens, H. T1 - Wasser und Risswachstum in Silicatgläsern N2 - Die Festigkeit von Gläsern wird durch die Oberflächenqualität beeinflusst. Kommt es neben dem Auftreten von Defekten zusätzlich zum Risswachstum ausgehend hiervon, wird die Festigkeit minimiert. Das Wachstum hängt dabei maßgeblich von der Luftfeuchtigkeit ab. Dieses Ermüdungsverhalten von Gläsern besser zu verstehen und dabei die Mechanismen und den Einfluss von im Volumen eingebauten Wasser auf das unterkritische Risswachstum zu untersuchen, ist Ziel der Arbeiten. Als Teilprojekt im Rahmen des DFG Schwerpunktprogramms SPP 1594 „Ultrastrong glasses“ soll der Einfluss des im Volumen eingebauten Wassers auf die Rissspitze untersucht werden. Zusammen mit der Leibniz Universität Hannover und der TU Clausthal werden hierfür hochwasserhaltige Gläser (bis zu 8 Gew%) bei 8 kbar über die Flüssigphase synthetisiert, die makroskopisch den hohen Wasseranteil nachstellen. Die Charakterisierung erfolgt hinsichtlich des Wassereinbaus, der mechanischen Eigenschaften und des Risswachstums. Die Arbeiten in Berlin beziehen sich hierbei auf die Messungen des unterkritischen Risswachstums in Luft und Vakuum, sowie Verlustwinkelmessungen. Erste Ergebnisse zeigen Unterschiede im korrosionsbeeinflussten (langsames) und inerten (schnelles und im Vakuum stattfindendes) Risswachstumsverhalten der untersuchten Gläsern. Die Rissgeschwindigkeit beim Übergang vom korrosionsbeeinflussten zum inerten Risswachstum ist hin¬gegen für alle Gläser ähnlich und folglich ein kinetisch durch den äußeren Wassertransport an die Rissspitze bestimmter Prozess. Der Widerstand gegen Risswachstum steigt mit Tg und zusätzlich kann anhand der Verlustwinkelmessungen ein Zusammenhang zwischen der Netzwerk- und der β-Relaxation ermittelt werden. Je höher der Wassergehalt im Glas ist, desto niedriger wird Tg und einfacher das Risswachstum, welches sich durch längere Risse kennzeichnet. Besonders stark tritt dieser Effekt bei einem Überschuss an molekularem Wasser auf. T2 - 1. Fachsymposium der Glasapparatebauer CY - Munich, Germany DA - 19.04.2018 KW - Wasser KW - Risswachstum KW - Glas KW - Vickers KW - DCB PY - 2018 AN - OPUS4-45701 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waurischk, Tina A1 - Balzer, R. A1 - Kiefer, P. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Behrens, H. A1 - Deubener, J. T1 - Sub-critical crack growth in silicate glass N2 - Premature failure of glass under load is caused by sub-critical crack growth (SCCG) originate from microscopic flaws at the surface. While SCCG is related to the humidity of the ambient atmosphere, leading to stress corrosion phenomena at the crack tip, the detailed mechanism and the effect of different network formers are still not fully understood. For more clarity, various soda silicate glasses with a second network former were investigated by double cantilever beam technique: Na2O*Al2O3*SiO2 (NAS), Na2O*B2O3*SiO2 (NBS), Na2O*PbO*SiO2 (NPbS). Three effects on the crack growth velocity, v, versus stress intensity, KI, curves were found out. The slope in region I, which is limited by corrosion, increases in the order NAS < NBS ≲ NPbS. The velocity range of region II reflecting the transition between corrosion effected and inert crack growth (region III), varies within one order of magnitude between the glasses. The KI region of inert crack growth strongly scatters between 0.4 and 0.9 MPam1/2. For comparison, crack growth at different humidity in commercial soda lime silicate glass (NCS) was measured. T2 - 92nd Annual Meeting of the German Society of Glass Technology in Conjunction with the Annual Meetings of the Czech Glass Society & the Slovak Glass Society CY - Bayreuth, Germany DA - 28.05.2018 KW - Risswachstum KW - DCB KW - Glas PY - 2018 AN - OPUS4-45702 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kiefer, P. A1 - Deubener, J. A1 - Waurischk, Tina A1 - Balzer, R. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Behrens, H. T1 - Statistical analysis of Vickers induced subcritical crack growth in soda-lime silicate glasses N2 - Studies on Vickers induced subcritical crack growth are controversially discussed since the stresses that drive the crack growth are distributed three dimensionally within the material and cannot be retraced by available methods. Hence, empirical approaches are used to calculate mechanical material parameters such as the stress intensity factor KI. However, the results of these approaches show large deviations from those measured by standardized techniques such as double cantilever beam (DCB) or double cleavage drilled compression (DCDC). Yet, small specimen sizes and low specimen quantities can prevent the execution of DCB and DCDC measurements. Here we present an approach that is based on a statistical analysis of Vickers induced radial cracks. For this purpose more than 150 single radial cracks were analyzed. The cracks were generated in a commercial soda-lime silicate glass. The experiments were performed in a glovebox purged with dry nitrogen gas to minimize the influence of atmospheric water on crack growth. The temporally resolved evolution of the radial cracks was monitored in-situ using an inverted microscope equipped with a camera system directly below the Vickers indenter. An automated image analysis software was used to determine the crack length over time. The data show that the crack propagation and thereby the crack velocities are not uniformly but statistically distributed. These findings allow, using the statistical mean value of the distributions in combination with DCB data, a precise formulation of KI for each measured crack length. T2 - 92nd Annual Meeting of the German Society of Glass Technology in Conjunction with the Annual Meetings of the Czech Glass Society & the Slovak Glass Society CY - Bayreuth, Germany DA - 28.05.2018 KW - Crack growth KW - Soda-lime silicate glass KW - Vickers PY - 2018 AN - OPUS4-45703 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kiefer, P. A1 - Deubener, J. A1 - Waurischk, Tina A1 - Balzer, R. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Behrens, H. T1 - Subcritical crack growth in water bearing soda-lime silicate glasses N2 - The presence of water in the surrounding atmosphere of a propagating crack has a major influence on the subcritical crack growth. While these external phenomena are well understood, there is still a lack of knowledge on the influence of structurally bound water on crack propagation. Thus, our recent study aims on the analysis of crack propagation in water bearing soda-lime silicate glasses with up to 8 wt.% water. The samples were synthesized in an internally heated pressure vessel at 0.5 GPa. Since this preparation route limits the sample sizes, standard test geometries allowing for the determination of stress intensity factors, such as double cantilever beam, are not feasible. Thus, radial cracks in the hydrous glasses were initiated by Vickers indentation and crack growth was simultaneously captured with a camera system. An automated image analysis algorithm was used for the analysis of the crack length of each single video frame. To minimize influences by atmospheric water, all experiments were conducted in a glovebox purged with dry N2. About 150 cracks per glass composition were analyzed to provide statistical significance of the Vickers-induced SCCG. The results show that structurally bound water has a major influence on SCCG by means of crack lengths, growth rates and time of crack initiation. T2 - 92nd Annual Meeting of the German Society of Glass Technology in Conjunction with the Annual Meetings of the Czech Glass Society & the Slovak Glass Society CY - Bayreuth, Germany DA - 28.05.2018 KW - Water speciation KW - Soda-lime silicate glass KW - Crack growth KW - Vickers PY - 2018 AN - OPUS4-45704 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kiefer, P. A1 - Balzer, R. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Behrens, H. A1 - Deubener, J. T1 - Statistical analysis of subcritical crack growth in water bearing soda-lime silicate glasses N2 - The talk was given at the PNCS-ESG 2018 in Saint Malo and summarizes the actual findings about Vickers induced crack growth in water bearing soda-lime silicate glasses. T2 - 15th International Conference on the Physics of Non-Crystalline Solids & 14th European Society of Glass Conference CY - Saint Malo, France DA - 09.07.2018 KW - Water speciation KW - Vickers KW - Crack growth KW - Soda-lime silicate glass PY - 2018 AN - OPUS4-45707 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Gaber, M. T1 - VACUUM HOT EXTRACTION (VHE-MS): Concentration, diffusion and degassing of volatiles N2 - Der Vortrag gibt eine Einführung in die Methode der Vakuumheißextraktion und beschreibt die Anwendungsmöglichkeiten der an der BAMN betriebenen Anlage. T2 - Seminar Instrumentelle Analytik, Fakultät III Prozesswissenschaften, Lehrstuhl Keramik TU Berlin CY - TU Berlin, Germany DA - 26.1.2018 KW - Gasabgabe KW - Diffusion KW - Gasgehalt PY - 2018 AN - OPUS4-45665 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Gaber, M. A1 - Reinsch, Stefan T1 - Thermal Analysis and Relaxation Phenomena in Oxide Glasses N2 - Wasser beeinflusst empfindlich eine Vielzahl von thermisch aktivierten Relaxationsphänomenen in Gläsern wie die Spannungsrelaxation, das unterkritische Risswachstum, innere Reibung, Viskosität, Sinterverhalten und Kristallisation. Thermische Methoden können dabei wesentliche Beiträge zum Verständnis dieser Phänomene liefern. Der Vortrag gibt einen Überblick über die Möglichkeiten der VakuumHeißExtraktion (VHE) zur Untersuchung des Wassergehalts, des Wasserabgabeverhaltens und der Wassermobilität sowie über den Einfluss des Wassers auf die innere Reibung (DMA). N2 - Dissolved water decisively influences numerous thermally activated relaxation phenomena in glasses like stress relaxation, sub-critical crack growth, internal friction, viscosity, sintering, and crystallization. Thermoanalytical methods can essentially help for better understanding of these phenomena. The lecture introduces the Vacuum Hot Extraction method (VHE) and illustrates its possibilities for measuring water content, degassing and mobility. As another thermoanalytical method, the Dynamic Mechanical Themoanalysis (DMA), allowing to study the effect of dissolved water on the internal friction in glasses, is introduced. T2 - Spring school DFG SPP 1594 CY - Hannover, Germany DA - 06.03.2018 KW - Wasser KW - Silicatglas KW - Relaxationsphänomene KW - Relaxation KW - Thermoanalytical Methods KW - Glass KW - Dissolved water PY - 2018 AN - OPUS4-45668 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Deubener, J. A1 - Behrens, H. T1 - Wasser in Silicatglas N2 - Der Vortrag gibt einen Überblick über den Stand des Wissens zum strukturellen Einbau von Wasser in Silicat- und Boratgläsern, den Einfluss des gelösten Wassers auf deren Viskosität sowie zu den strukturellen Vorstellungen zum Wassertransport. T2 - 1. Fachsymposium der Glasapparatebauer CY - Munich, Germany DA - 19.04.2018 KW - Wasser KW - Glass KW - Struktur PY - 2018 AN - OPUS4-45669 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf T1 - Glass Sintering with Concurrent Crystallization and Foaming N2 - Glass powders are promising candidates for manufacturing a broad diversity of sintered materials like sintered glass-ceramics, glass matrix composites or glass bonded ceramics with tailored mechanical, thermal, electrical and optical properties and complex shape. Its wide and precise adjustability makes this class of materials a key component for advanced technologies. Processing of glass or composite powders often allow even more flexibility in materials design. At the same time, however, processing can have substantial effects on the glass powder surface and sinterability. Thus, mechanical damage and surface contamination can strongly enhance surface crystallization, which may retard or even fully prevent densification. Whereas sintering and concurrent crystallization have been widely studied, partially as cooperative effort of the TC7 of the ICG, and although glass powder sintering is predominantly applied for glasses of low crystallization tendency, sintering is also limited by gas bubble formation or foaming. The latter phenomenon is much less understood and can occur even for slow crystallizing glass powders. The lecture illustrates possible consequences of glass powder processing on glass sintering, crystallization and foaming. T2 - 7th Int Congress on Ceramics, Symposium Frontiers of Glass Science CY - Iguacu, Brazil DA - 17.06.2018 KW - Glass KW - Powder KW - Sintering KW - Foaming PY - 2018 AN - OPUS4-45670 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grelle, Tobias A1 - Probst, Ulrich A1 - Jaunich, Matthias A1 - Skrotzki, Birgit A1 - Wolff, Dietmar T1 - Creep investigations on aluminum seals for application in radioactive waste containers N2 - In Germany spent nuclear fuel and high level radioactive waste is stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. The used metal seals consist of three components as can be seen in the cross-sectional view in Figure 1. The innermost part is a helical spring that is surrounded by an inner jacket made of stainless steel. The outer jacket that is made of a softer material which in case of assembly in the aforementioned storage containers is silver or aluminum (i.e. Al 99.5). During application the seal is compressed and due to the restoring force of the helical spring, the outer jacket is plastically deformed and adapts to the sealing surface. Hence, leakage paths are closed and the sealing function is generated. In Germany the above-mentioned containers are licensed for up to 40 years of interim storage, which in case extended storage becomes necessary before a final repository is available will have to be extended to even longer periods. Therefore, the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads as well. At Bundesanstalt für Materialforschung und –prüfung (BAM) long-term investigations are being conducted in which seals are assembled in test flanges and aged at temperatures ranging from room temperature to 150°C for accelerated aging. The aged seals are tested semi-annually (after the first 6 months in which the seals are tested more frequently) regarding the sealing performance, the remaining seal force, and the useable resilience upon decompression. Results of these investigations have been published over the past years (e.g. Grelle, Wolff, Probst, Jaunich, & Völzke, 2017; Völzke, Wolff, Probst, Nagelschmidt, & Schulz, 2014). It was found that the seal force and the useable resilience decrease with time and temperature, which is in agreement with the result of other studies (Sassoulas et al., 2006; Wataru et al., 2016) as well. Geometry change of the outer jacket has been identified as the main reason for this seal behavior. At the prevailing operating temperatures and stresses the aluminum is subjected to creep deformation leading to a thinning of the outer jacket. Since the seal groove depth remains unchanged the helical spring expands, which in turn leads to a decrease of the generated spring and seal force. Although the main reason for the change of seal parameters over time and temperature is known, a detailed characterization of the seal behavior and a reliable prediction of the parameter development for aging times that exceed the experimental time frame have not been possible, yet. For deeper understanding of the aging processes, an Investigation program, which is covered in this contribution, is conducted at Bundesanstalt für Materialforschung und –prüfung (BAM) that focusses on the behavior of the aluminum jacket and its influence on the long-term sealing performance. The program investigates properties of material samples as well as the behavior of the seal as a component. Original sheet material of the same aluminum that is used for manufacturing of the seals is investigated in compression creep tests. For this, a DMA (dynamic mechanical analysis) machine is employed (here used for static tests) that allows for a measurement of the specimens deformation under forces of up to 500 N. The advantage of this method is that the original material can be tested in the same shape as used for the seals which is 0.5 mm thick sheet material. For investigation of tensile creep standard specimens are used, that were machined from surrogate material of the same composition and annealing condition. Furthermore, aluminum seals that are cut into smaller segments are assembled in flanges and placed in heating chambers at temperatures ranging from 23°C to 150°C. After different periods of time from 3 days to 300 days the segments are taken out of the flanges and are investigated, thus giving information on different states of aging. Measurements of the development of the seal contact width and the aluminum jacket thickness are done with an optical microscope. Further investigations on the segments will include metallography and hardness measurements. From the detailed material and component behavior including the results of the long-term seal force and useable resilience investigations a better understanding of the overall seal behavior can be gained. The aim is to contribute to the development of material models and analytical approaches for the prediction of the sealing behavior in dependence of time and temperature. T2 - International Conference on Aluminum Alloys CY - Montreal, Canada DA - 17.06.2018 KW - Metal seal KW - Creep KW - Long-term behavior PY - 2018 SN - 978-1-926872-41-4 SP - 1 EP - 2 AN - OPUS4-45844 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gaal, Mate A1 - Schadow, Florian A1 - Nielow, Dustin A1 - Trappe, Volker T1 - Air-coupled ultrasonic ferroelectret transducers with additional bias voltage for testing of composite structures N2 - Common air-coupled transducers for non-destructive testing consist of a piezocomposite material and several matching layers. Better acoustical matching to air is achieved by transducers based on charged cellular polypropylene (PP). This material has about hundred times lower acoustic impedance than any piezocomposite, having about the same piezoelectric coefficient. The piezoelectric properties of cellular PP are caused by the polarization of air cells. Alternatively, a ferroelectret receiver can be understood as a capacitive microphone with internal polarization creating permanent internal voltage. The sensitivity of the receiver can be increased by applying additional bias voltage. We present an ultrasonic receiver based on cellular PP including a high-voltage module providing bias voltage up to 2 kV. The application of bias voltage increased the signal by 12 to 15 dB with only 1 dB increase of the noise. This receiver was combined with a cellular PP transmitter in through transmission to inspect several test specimens consisting of glass-fiber-reinforced polymer face sheets and a porous closed-cell PVC core. These test specimens were inspected before and after load. Fatigue cracks in the porous PVC core and some fatigue damage in the face sheets were detected. These test specimens were originally developed to emulate a rotor blade segment of a wind power plant. Similar composite materials are used in lightweight aircrafts for the general aviation. The other inspected test specimen was a composite consisted of glass-fiber-reinforced polymer face sheets and a wooden core. The structure of the wooden core could be detected only with cellular PP transducers, while commercial air-coupled transducers lacked the necessary sensitivity. Measured on a 4-mm thick carbon-fiber-reinforced polymer plate, cellular PP transducers with additional bias voltage achieved a 32 dB higher signal-to-noise ratio than commercial air-coupled transducers. T2 - 10th International Symposium on NDT in Aerospace CY - Dresden, Germany DA - 26.10.2018 KW - Airborne ultrasonic testing KW - Air-coupled ultrasonic testing KW - Ferroelectret KW - Composites KW - Rotor blade PY - 2018 AN - OPUS4-46656 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gaal, Mate A1 - Schadow, Florian A1 - Nielow, Dustin A1 - Trappe, Volker T1 - Air-coupled ultrasonic ferroelectret transducers with additional bias voltage for testing of composite structures N2 - Common air-coupled transducers for non-destructive testing consist of a piezocomposite material and several matching layers. Better acoustical matching to air is achieved by transducers based on charged cellular polypropylene (PP). This material has about hundred times lower acoustic impedance than any piezocomposite, having about the same piezoelectric coefficient. The piezoelectric properties of cellular PP are caused by the polarization of air cells. Alternatively, a ferroelectret receiver can be understood as a capacitive microphone with internal polarization creating permanent internal voltage. The sensitivity of the receiver can be increased by applying additional bias voltage. We present an ultrasonic receiver based on cellular PP including a high-voltage module providing bias voltage up to 2 kV. The application of bias voltage increased the signal by 12 to 15 dB with only 1 dB increase of the noise. This receiver was combined with a cellular PP transmitter in through transmission to inspect several test specimens consisting of glass-fiber-reinforced polymer face sheets and a porous closed-cell PVC core. These test specimens were inspected before and after load. Fatigue cracks in the porous PVC core and some fatigue damage in the face sheets were detected. These test specimens were originally developed to emulate a rotor blade segment of a wind power plant. Similar composite materials are used in lightweight aircrafts for the general aviation. The other inspected test specimen was a composite consisted of glass-fiber-reinforced polymer face sheets and a wooden core. The structure of the wooden core could be detected only with cellular PP transducers, while commercial air-coupled transducers lacked the necessary sensitivity. Measured on a 4-mm thick carbon-fiber-reinforced polymer plate, cellular PP transducers with additional bias voltage achieved a 32 dB higher signal-to-noise ratio than commercial air-coupled transducers. T2 - 10th International Symposium on NDT in Aerospace CY - Dresden, Germany DA - 26.10.2018 KW - Airborne ultrasonic testing KW - Air-coupled ultrasonic testing KW - Ferroelectret KW - Composites KW - Transducers PY - 2018 SP - 1 EP - 6 AN - OPUS4-46657 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Falkenberg, Rainer A1 - Charmi, Amir T1 - Virtual-lab-based determination of a macroscopic yield function for additively manufactured parts N2 - Diese Arbeit beschreibt eine Methode für die Ermittlung einer Fließfunktion für additiv gefertigte Bauteile des Werkstoffs S316L. Ein Kristallplastizitätsmodell wird zunächst mit experimentellen Daten kalibriert. Anschließend werden mit diesem Modell sogenannte virtuelle Experimente durchgeführt, die die prozeßspezifische Mikrostruktur in Form von kristallographischen und morphologischen Texturen miteinbeziehen. Diese Simulationen werden mit einem representativen Volumenelement (RVE) durchgeführt, das aus EBSD/CT-Scans an additiv gefertigten Proben generiert wurde und daher die Kornstruktur und Kristallorientierungen enthält. Die virtuellen Experimente werden durchgeführt, um anhand der damit erhaltenen Fließpunkte eine anisotrope Barlat-Fließfunktion zu bestimmen. Dieser skalenübergreifende Ansatz ermöglicht die Simulation großer Strukturen, für die die Anwendung eines Kristallplastizitätsmodells numerisch zu teuer wäre. N2 - This work presents a method for the yield function determination of additively manufactured parts of S316L steel. A crystal plasticity model is calibrated with test results and used afterwards to perform so-called virtual experiments, that account for the specific process-related microstructure including crystallographic and morphological textures. These simulations are undertaken on a representative volume element (RVE), that is generated from EBSD/CT-Scans on in-house additively manufactured specimen, considering grain structure and crystal orientations. The results of the virtual experiments are used to determine an anisotropic Barlat yield function, that can be used in a macroscopical continuum-sense afterwards. This scale-bridging approach enables the calculation of large-scale parts, that would be numerically too expensive to be simulated by a crystal plasticity model. T2 - 3. Tagung des DVM-Arbeitskreises Additiv gefertigte Bauteile und Strukturen CY - Berlin, Germany DA - 07.11.2018 KW - Additive manufacturing KW - Scale-bridging KW - Crystal plasticity KW - Virtual experiments KW - Anisotropy PY - 2018 SN - 2509-8772 SP - 153 EP - 158 PB - DVM CY - Berlin AN - OPUS4-46570 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -