TY - JOUR A1 - Ferrari, Bruno A1 - Fantin, Andrea A1 - Said, D. A1 - Fitch, A. N. A1 - Suárez Ocano, Patricia A1 - Mishurova, Tatiana A1 - Roveda, Ilaria A1 - Kromm, Arne A1 - Darvishi Kamachali, Reza A1 - Bruno, Giovanni A1 - Evans, Alexander A1 - Requena, G. A1 - Agudo Jácome, Leonardo A1 - Serrano Munoz, Itziar T1 - The impact of scanning strategy on cell structures in PBF-LB/M/IN718: an in situ synchrotron x-ray diffraction study N2 - In additive manufacturing, any change of the process parameters, such as scanning strategy, directly affects the cooling rates, heat accumulation, and overall thermal history of the build. Consequently, parts built with different process parameters tend to have different levels of crystallographic texture, residual stress, and dislocation density. These features can influence the properties of the material and their development during post-processing operations. In this study, IN718 prisms were built by laser powder bed fusion (PBF-LB/M) using two different scanning strategies (continuous 67° rotations around the build direction, ROT, and alternating 0°/67° scans, ALT) to provide two different as-built conditions. In situ time-resolved synchrotron diffraction was performed during a solution heat treatment at 1027 °C for 1 h. Ex situ scanning electron microscopy was used to support and complement the in situ observations. An approach to quantify the effect of elemental microsegregation at the cell walls is developed based on the deconvolution of asymmetric γ-nickel matrix peaks. Following this approach, the scanning strategies are shown to affect the as-built fraction of cell walls in the material, resulting in a difference of approximately 5 %, in weight fraction, between ROT and ALT (19 % vs. 24 %, respectively). This microsegregation was observed to be rapidly homogenized during the heating ramp, and no significant changes to the peak shape in the γ peaks occurred during the isothermal part of the heat treatment, regardless of the scanning strategy. KW - Additive manufacturing KW - Inconel 718 KW - Synchrotron x-ray diffraction KW - Heat treatment KW - Laser powder bed fusion KW - Cellular microstructure PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-650958 DO - https://doi.org/10.1016/j.jmrt.2025.11.214 SN - 2238-7854 VL - 41 SP - 593 EP - 608 PB - Elsevier B.V. AN - OPUS4-65095 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Siefke, Lennart A1 - Linden, Anna T1 - Towards a robust automated surface inspection method for CT-scanned cannulas N2 - For certain cardiovascular diseases, cannulas are implanted into the blood circuit. To match the patients individual anatomy of the heart, there is research for cannulas to be custom-designed and manufactured aided by 3D printing. However, cannulas have to hold very high standards with regard to the smoothness of their surfaces, as rough patches can lead to formation of blood clots. Therefore, this work uses computer vision to detect such patches as part of quality assurance. First, the produced cannula is scanned using a precise CT scanner and transformed into a 3D mesh object. Rough patches in an otherwise smooth but curved surface are detected by using cosine similarity between neighboring faces and a statistical evaluation. In the end, this method is able to raise a warning when curved surfaces are not smooth enough and visualizes the problematic patches. However, there is just limited access to test data currently and the scanner used needs to be upgraded. T2 - 3D in Science & Applications (3D-iSA) 2024 CY - Berlin, Germany DA - 26.11.2024 KW - Algorithm KW - Additive manufacturing KW - Surface evaluation PY - 2025 UR - https://www.gfai.de SN - 978-3-942709-34-7 SP - 66 EP - 70 AN - OPUS4-63057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Linden, Anna T1 - AMVAD - Additive manufacturing for ventricular assist devices N2 - Some children are born with a univentricular heart, meaning their heart has only one pumping chamber instead of two. To improve circulation, patients often undergo the Fontan procedure, which reroutes blood flow — but this can put stress on other organs. In some cases, ventricular assist devices, or VADs, are used to support the heart’s pumping function. This involves an artificial pump connected directly to the patient's heart via silicone-based cannulas. Unique anatomical conditions introduce special challenges for cannula geometry. Additive manufacturing offers innovative solutions by enabling the production of personalized medical devices. The aim of the project is to develop the manufacturing workflow for the individualized cannula from digital imaging of the patient and customized design to additive manufacturing. Besides technical feasibility, validating the entire process is crucial for regulatory approval. The selection and testing of suitable additive manufacturing processes and biocompatible materials for individualized silicone cannulas, ensuring compliance with quality standards for high-risk medical products, will be presented. T2 - AMBER Spotlight On: 3D Printing meets Health & Biotech CY - Berlin, Germany DA - 16.09.2025 KW - Additive manufacturing KW - Medical device KW - Liquid silicone rubber PY - 2025 AN - OPUS4-64101 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Agudo Jácome, Leonrado T1 - Low-Cycle Fatigue Behavior of Laser Powder Bed Fused Inconel 718 at Room and High Temperature N2 - The nickel-base superalloy Inconel 718 (IN718) is one of the most commonly used Ni-based superalloys for high temperature structural applications for its remarkable strength, as well as creep, fatigue, and corrosion resistance up to 650 °C. While IN718 has traditionally been employed as cast or wrought material, it is difficult to machine because of its high strength and toughness. The additive manufacturing of IN718 components made by metal AM has thus gained extensive attention to produce expensive near-net shaped components of high-temperature alloys such as IN718, for it saves material and costs in processing and machining steps. Among all metal additive manufacturing (AM) technologies, laser powder bed fusion (PBF-LB/M) is the most widespread, IN718 being one of the most common alloys produced with it. However, high cooling rates associated to the PBF-LB/M process, hinders the primary strengthening phases γ’’ and γ’ to form, as these cooling rates induce a dislocation cellular substructure, at which walls primary Laves phases bind segregating Nb, Ti and Mo. Many of the therefore needed heat-treatment strategies can then promote Laves-phase transformation into the stable δ phase along the cell and grain boundaries. Laves and δ phases, as well as grain-boundary primary carbides may have adverse effects on mechanical properties. The mostly needle-shaped δ phase was namely found to have a detrimental effect on creep rupture life while no direct effect on LCF fatigue life was evident. In this work room- and high-temperature (650 °C) low-cycle fatigue behavior of PBF-LB/M IN718 is investigated in the four-step heat-treated state and compared to wrought IN718. The microstructure of both materials is characterized across length scales via microscopy methods. The fatigue life at room temperature of the PBF-LB/M IN718 material is slightly lower than that for the wrought material, which is reversed at 650 °C. The cyclic stress response for both materials is marked by cyclic softening that is more pronounced at higher test temperatures. Multiple secondary cracks form at high strain amplitudes, at both room and high temperatures. High testing temperatures enhance specially crack formation at the transitions of regions between elongated grains and columns of stacked grains with ripple patterns in the PBF-LB/M material. Additional to this behavior, pronounced crack branching and deflection indicate that the cracks are controlled by sharp micromechanical gradients. T2 - EUROMAT 2025 CY - Granada, Spain DA - 14.09.2025 KW - Additive manufacturing KW - Low-cycle fatigue KW - Microstructural characterization KW - Ni-base superalloy PY - 2025 AN - OPUS4-64354 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Suarez Ocano, Patricia T1 - Influence of heat-treatment-induced microstructural evolution on the Low Cycle Fatigue behavior of 316L stainless steel fabricated by Laser Powder Bed Fusion N2 - Additive manufacturing, particularly the laser powder bed fusion (PBF-LB/M) process, has gained significant attention in recent years due to its ability to produce complex geometries with enhanced mechanical properties. Among the various materials used, 316L stainless steel is highly favored for cyclically loaded components due to its exceptional mechanical strength, high-temperature performance, and corrosion resistance, making it widely applicable across various industries. 316L SS fabricated by PBF-LB/M (PBF-LB/M/316L) exhibits a unique hierarchical microstructure, with high density of low-angle grain boundaries (LAGBs), nano-dispersed silicates, chemical micro-segregations, and solidification-induced cellular structures. Particularly, the submicron-sized cellular features enriched with chromium (Cr) and molybdenum (Mo), along with high dislocation densities, contribute to a superior strength-ductility balance compared to conventionally manufactured 316L SS. The dispersed silicate particles act also as a strengthening phase, impeding dislocation movement and enhancing plastic deformation resistance. This study explores the effect of heat treatments on the low-cycle fatigue (LCF) behavior of PBF-LB/M/316L at room temperature (RT) and 600 °C. First, three heat treatment conditions were applied to the as-built material: 450 °C for 4 hours (HT450/4), 800 °C for 3 hours (HT800/3), and 900 °C for 1 hour (HT900/1) to investigate their influence on microstructural evolution. Microstructural analysis revealed that the HT450/4 condition preserved the cellular structure with high dislocation density, while the HT800/3 condition showed partial dissolution of cells together with reduction in segregated elements along the cell walls and a reduced dislocation density. The HT900/1 condition resulted in complete segregation and cellular structure dissolution with comparable dislocation density to HT800/3 while maintaining the crystallographic texture and grain morphology. Intermetallic χ phase was mostly observed at the grain boundaries in HT800/3, but not in HT900/1. Fully reversed LCF tests were conducted under strain-controlled conditions with a strain amplitude of 0.8 %. Tests were interrupted at specific intervals to analyze the interaction between hierarchical microstructural features and deformation mechanisms in the three heat-treated conditions. Due to the pronounced dislocation cell structures and elemental segregation, the microstructure of the HT450/4 condition significantly impact deformation and damage mechanisms during cyclic loading, which in turn, differ from the conventional produced counterparts. The results provide insights into the relationship between microstructural features and fatigue performance, highlighting key deformation and failure mechanisms under cyclic loading. T2 - FEMS 2025 EUROMAT 18th European Congress and Exhibition on Advanced Materials and Processes CY - Granada, Spain DA - 14.09.2025 KW - Additive manufacturing KW - 316L stainless steel KW - Heat treatments KW - Low Cycle Fatigue KW - Microstructure PY - 2025 AN - OPUS4-64238 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Evans, Alexander A1 - Schröder, Jakob A1 - Pirling, T. A1 - Ulbricht, Alexander A1 - Suárez Ocaño, Patricia A1 - Bruno, Giovanni T1 - Resolving the Subsurface Residual Stress Maximum in Laser Powder Bed-Fused 316L Stainless Steel by Diffraction-Based Analysis N2 - Laser powder bed fusion (PBF-LB/M) is a metal additive manufacturing process. Due to the complex nature of the layer-wise, repeated heating and cooling cycles, it tends to generate high-magnitude residual stresses. If not correctly understood and mitigated through in- or post-process approaches, these residual stresses can be detrimental as they are often tensile at the surface. However, determining the magnitude and location of peak tensile residual stresses is not trivial as they are often located subsurface. This work focuses on determining the magnitude and location of these deleterious tensile residual stresses in a PBF-LB/316L specimen. Two diffraction-based Methods are used to reveal the relationship between the residual stresses and the underlying microstructure. On the one hand, high spatial resolution Neutron diffraction is used to determine triaxial stresses from the bulk to a depth of 0.15 mm. On the other hand, laboratory X-ray diffraction coupled with electrolytical layer removal allows the biaxial residual stress depth profile to be probed from the surface to a depth of about 0.6 mm. The results show a good agreement between the two methods. The peak residual stress is shown to be 500 MPa, which appears as a plateau between 0.08 and 0.35 mm in depth. KW - Residual stress KW - Diffraction KW - Laser Powder Bed Fusion KW - 316L KW - Additive manufacturing KW - Microstructure KW - AGIL PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-652138 DO - https://doi.org/10.1007/s11837-025-07719-y SN - 1543-1851 VL - 77 IS - 12 SP - 9726 EP - 9737 PB - Springer Nature AN - OPUS4-65213 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Suárez Ocaño, Patricia A1 - Ávila Calderón, Luis A1 - Agudo Jácome, Leonardo A1 - Rehmer, Birgit A1 - Mohr, Gunther A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Effect of 700–900 °C heat treatments and room and high temperature tensile deformation on the microstructure of laser powder bed fused 316L stainless steel N2 - The effect of post-processing heat treatments on the hierarchical microstructure evolution and mechanical strength of the austenitic stainless steel 316L produced by laser powder bed fusion has been investigated. Heat treatments between 700 and 900 ◦C and 0.5 to 3 h, were applied to samples treated at 450 ◦C for 4 h. The results showed a stable microstructure at all studied temperatures and times in terms of grain size, morphology, aspect ratio, density of low-angle grain boundaries, and texture. However, temperature and time promoted the diffusion of segregated elements together with a reduction in dislocation density and disappearance of the cellular structure. This was associated with a reduction in hardness and tensile proof strength at both room and high temperature. In addition, microstructural characterization coupled with thermodynamic CALPHAD-based equilibrium calculations showed that the formation of carbides and intermetallic phases was already visible after annealing at 800 ◦C for 3 hours, although these intermetallics did not affect the tensile properties at this level. Analysis of the microstructure evolution after tensile deformation showed differences in the deformation mechanisms at room and high temperature, with twinning and martensitic transformation occurring at room temperature, the latter not widely reported for additively manufactured 316L. Finally, comparisons with similar materials produced under comparable conditions showed differences in the tensile properties, attributed to differences in chemical composition and the associated presence of stacking faults in the undeformed state. KW - Additive manufacturing KW - 316L stainless steel KW - Heat treatments KW - Tensile properties KW - Microstructure PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632471 DO - https://doi.org/10.1016/j.msea.2025.148469 SN - 0921-5093 VL - 939 SP - 1 EP - 24 PB - Elsevier CY - Amsterdam AN - OPUS4-63247 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Suarez Ocano, Patricia T1 - Exploring the impact of heat treatment on room and high temperature strength of 316L stainless steel fabricated by PBF-LB N2 - Laser Powder Bed Fusion (PBF-LB/M) enables the fabrication of 316L stainless steel components with superior strength and intricate geometries. The alloy PBF-LB/M/316L features a fully austenitic microstructure with hierarchical characteristics— such as fine dislocation structures, segregated elements, low-angle grain boundaries, and nano-dispersed silicates—that enhance strength and ductility. Additionally, it includes metallurgical defects and residual stresses. Apart from process control, heat treatments (HTs) are used to tailor the microstructure for specific loading conditions. This study investigate the effects of post-processing HTs on the hierarchical microstructure and tensile properties of PBF-LB/M/316L at room and high temperature. The heat treatments, ranging from 400 °C to 900 °C for 1 to 4 hours, focus on sub-recrystallization temperatures to preserve the microstructural hierarchy. The HTs applied had minimal impact on the grain shape, size, or texture of PBF-LB/M/316L. However, significant modifications occurred in the solidification cellular substructure after HTs at 800 °C and 900 °C, when compared to a heat-treated condition at 450 °C. HTs at 800 °C notably decreased dislocation density and enlarged cellular structures, though they remained partially intact. After 1 hour at 900 °C, the cellular substructure dissipated, correlating with a further reduction in dislocation density. These microstructural changes resulted in a decreased yield strength and increased work hardening capacity at both room and high temperature, highlighting the critical link between HT parameters, microstructural evolution, and mechanical performance. T2 - The 20th International Conference on Strength of Materials (ICSMA 20) CY - Kyoto, Japan DA - 02.06.2025 KW - Additive manufacturing KW - 316L stainless steel KW - Heat treatments KW - Tensile properties KW - Microstructure PY - 2025 AN - OPUS4-63914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller-Elmau, Johanna T1 - Transparent feedstocks for photon-based addiTve manufacturing technologies for powder processing of ceramics N2 - Photon-based additive manufacturing technologies such as SLA, DLP, LCM, moreover volumetric two-photon-polymerization, Xolography and holographic technologies promise the highest accuracy and dimensional freedom. But to transfer the light through the feedstock it needs sufficient transparency at the used light wavelength. Ceramic particles used for powder processing routes act as scattering sites and therefore hinder the light transmission, unless… The particle size and particle size distribution are chosen small and narrow enough. Particles which are smaller than roughly 1/10th of the light wavelength, mostly nanoparticles around 5nm size, decrease scattering vastly. This turns resins even with homogeneously distributed ceramic weight fraction of up to 80% transparent again. Feedstocks could be prepared for the highly accurate two-photon-polymerization gaining the smallest yttria stabilized zirconia structures with a resolution of 500nm and unique mechanical properties. The same feedstocks could be applied to DLP and LCM as layer-by-layer AM-technologies for bigger parts. Hybridizing both technologies lead to ceramic parts with microscopic accuracy at macroscopic dimensions. The feedstock was even applied to the volumetric Xolography with the highest transparency requirement so far and to versatile and flexible holographic AM. Highly filled nano-particle containing transparent ceramic feedstocks open the way for technical ceramics in high precision manufacturing where the performance and durability and accessibility are increased and created by the unique ceramic properties such as mechanical strength, chemical and thermal resistance and biocompatibility T2 - 2025 International Conference on Additive Manufacturing Technology Frontiers and Applications CY - Xi'an, China DA - 11.04.2025 KW - Tranparent KW - Ceramic KW - Additive manufacturing PY - 2025 AN - OPUS4-65069 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller-Elmau, Johanna A1 - Meyer, Frank A1 - Goebbert, Christian A1 - Günster, Jens T1 - Manufacturing Ceramics with Light N2 - Additive manufacturing of extremely complex and filigree geometries from ceramic materials is a fascinating topic as ceramic materials are especially suitable for extremely small structures thanks to their physicochemical properties: they are chemically stable and do not corrode, while exhibiting unique mechanical properties especially in the micrometre range (Fig. 1). In addition, the ceramic structures made of yttria-stabilized zirconia (YSZ) shown in the figure are transparent, which makes them interesting candidates for the development of miniaturized optical components. The refractive index of YSZ measures 2,2 and is therefore considerably higher than that of polymer-based materials or glasses. The possibility of building this type of structure is enabled with the use of ceramic slurries with sufficiently high Transparency for the volumetric process of two-photon polymerization, which uses a femtosecond-short-pulse laser to structure photo-crosslinkable resins in the volume of one droplet. Slurries with even further optimized transparency allow even the application of xolography, a volumetric process that builds components with relatively low resolution, but in relatively large volumes and higher productivity. In the scope of the research presented here, for the first time, this process is applied to sintered ceramic materials. To be able to use minute ceramic structures as real components, an approach for the hybridization of processes ispresented in which components in the centimetre range, with relatively low resolution, are combined with very high-resolution nanostructures. KW - Additive manufacturing KW - Zirconia KW - Two-photon-polymerization KW - Nanopowder PY - 2025 SN - 0173-9913 VL - 4 SP - 34 EP - 41 PB - Göller Verlag GmbH CY - Baden-Baden AN - OPUS4-65070 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller-Elmau, Johanna T1 - 2PP of ceramic N2 - Photon-based additive manufacturing technologies such as SLA, DLP, LCM, moreover volumetric two-photon-polymerization (2PP), Xolography and holographic technologies promise the highest accuracy and dimensional freedom. To transfer the light through the feedstock it needs sufficient transparency. Ceramic particles used for powder processing routes act as scattering sites and therefore hinder the light transmission, unless… The particle size and particle size distribution are chosen small and narrow enough. Particles smaller than roughly 1/10th of the light wavelength, mostly nanoparticles around 5nm size, decrease scattering vastly. This turns resins even with homogeneously distributed ceramic weight fraction of up to 80% transparent again. Feedstocks were prepared for the highly accurate two-photon-polymerization gaining the smallest yttria stabilized zirconia structures with a resolution of 500nm and unique mechanical properties. The same feedstock was applied to DLP and LCM as layer-by-layer AM-technologies for bigger parts. Hybridizing both technologies enables ceramic parts with microscopic accuracy at macroscopic dimensions. The feedstock was even applied to the volumetric Xolography with the highest transparency requirement so far and to versatile and flexible holographic AM. What are the next steps? Can those proof-of -concept studies be transferred to industrial applications and what are the hurdles on the way? How to make the stretch between fundamental research and application-oriented development? T2 - Smart Made 2025 CY - Osaka, Japan DA - 01.10.2025 KW - Tranparent KW - Ceramic KW - Additive manufacturing PY - 2025 AN - OPUS4-65062 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Blaeß, Carsten T1 - Binder jetting of crystallizing bioactive glass powders N2 - Customized artificial bone replacement implants made of resorbable bioactive glass (BG) have not yet become widely accepted in clinical use. This is mainly due to the contrariness of sintering ability and appropriate bioactivity. Concurrent crystallization often prevents the generation of dense sinter bodies, especially for additive manufactured 3D scaffolds. The presented study investigates the limits and advantages of crystallization of powder compacts manufactured by binder jetting and uniaxial pressing for different particle size fractions (psf) of two BGs. T2 - CeramicAM 2024 - 1º CY - Sao Paulo, Brasil DA - 19.09.2024 KW - Bioactive glass KW - Sintering KW - Crystallization KW - Additive manufacturing PY - 2024 AN - OPUS4-62594 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dzugan, J. A1 - Lucon, E. A1 - Koukolikova, M. A1 - Li, Y. A1 - Rzepa, S. A1 - Yasin, M.S. A1 - Shao, S. A1 - Shamsaei, N. A1 - Seifi, M. A1 - Lodeiro, M. A1 - Lefebvre, F. A1 - Mayer, U. A1 - Olbricht, Jürgen A1 - Houska, M. A1 - Mentl, V. A1 - You, Z. T1 - ASTM interlaboratory study on tensile testing of AM deposited and wrought steel using miniature specimens N2 - An interlaboratory study, involving eigth international laboratories and coordinated by COMTES FHT (Czech Republic), was conducted to validate tensile measurements obtained using miniature specimens on additively manufactured (AM) components and artifacts. In addition to AM 316L stainless steel (316L SS), a wrought highstrength steel (34CrNiMo6V, equivalent to AISI 4340) was also used. Based on the results, a precision statement in accordance with ASTM E691 standard practice was developed, intended for inclusion in a proposed annex to the ASTM E8/E8M tension testing method. The primary outcomes of the study highlighted the agreement between yield and tensile strength measured from miniature and standard-sized tensile specimens. Furthermore, most tensile properties exhibited similar standard deviations, offering users insight into the efficacy of miniature specimen applications. KW - 316L stainless steel KW - Additive manufacturing KW - High-strength steel KW - Miniature specimens KW - Tensile tests PY - 2024 DO - https://doi.org/10.1016/j.tafmec.2024.104410 SN - 0167-8442 VL - 131 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-60180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kindrachuk, Vitaliy T1 - Computational investigation of DGG kinetics by phase-field method N2 - Non-equilibrium microstructure evolution in additive manufacturing (AM) is a major barrier for establishing a safe and sustainable application of AM in industrial processes. The constant heat source in the AM continuously affects the just-solidified grains beneath the melting pool, leading to directional grain growth (DGG). While real-time measurements of the non-equilibrium microstructure evolution is challenging, here developing a computational framework to systematically explore DGG becomes imperative. We have advanced a comprehensive approach, integrating mean-field modeling and phase-field simulations, to elucidate the dynamics of DGG under an external driving force. Our simulations unveil a steady-state power-law grain growth kinetics during DGG, characterized by the interplay between curvature-driven dynamics at grain boundary junctions and directional driving forces. T2 - Tagung DGM Additive Fertigung CY - Bremen, Germany DA - 12.06.2024 KW - Directional grain growth KW - Phase-field simulation KW - Additive manufacturing PY - 2024 AN - OPUS4-60750 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kindrachuk, Vitaliy A1 - Darvishi Kamachali, Reza T1 - Mean-field modeling and phase-field simulation of grain growth under directional driving forces N2 - Directional grain growth is a common phenomenon in the synthetic and natural evolution of various polycrystals. It occurs in the presence of an external driving force, such as a temperature gradient, along which grains show a preferred, yet competitive, growth. Novel additive manufacturing processes, with intense, localized energy deposition, are prominent examples of when directional grain growth can occur, beneath the melting pool. In this work, we derive a phenomenological mean-field model and perform 3D phase-field simulations to investigate the directional grain growth and its underlying physical mechanisms. The effect of the intensity of driving force is simulated and systematically analyzed at the evolving growth front as well as various cross-sections perpendicular to the direction of the driving force. We found that although the directional growth significantly deviates from normal grain growth, it is still governed by a power law relation α tⁿ with an exponent n ~ 0.6–0.7. The exponent n exhibits a nontrivial dependence on the magnitude of the directional driving force, such that the lowest growth exponent is observed for intermediate driving forces. We elaborate that this can originate from the fact that the forces at grain boundary junctions evolve out of balance under the influence of the directional driving force. With increasing the driving forces, the growth exponent asymptotically approaches a value of n ≈ 0.63, imposed by the largest possible grain aspect ratio for given grain boundary energies. The current combined mean-field and phase-field framework pave the way for future exploration in broader contexts such as the evolution of complex additively manufactured microstructures. KW - Additive manufacturing KW - Phase-field simulation KW - Grain growth KW - Mean-field modelling KW - Directional grain growth PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593210 DO - https://doi.org/10.1016/j.mtla.2023.101989 SN - 2589-1529 VL - 33 SP - 1 EP - 10 PB - Elsevier AN - OPUS4-59321 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Piesker, Benjamin A1 - Ávila Calderón, Luis A1 - Mohr, Gunther A1 - Rehmer, Birgit A1 - Agudo Jácome, Leonardo A1 - Hilgenberg, Kai A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Tensile and Low‐Cycle Fatigue Behavior of Laser Powder Bed Fused Inconel 718 at Room and High Temperature N2 - This study investigates the room‐ and high‐temperature (650 °C) tensile and low‐cycle‐fatigue behavior of Inconel 718 produced by laser powder bed fusion (PBF‐LB/M) with a four‐step heat treatment and compares the results to the conventional wrought material. The microstructure after heat treatment is characterized on different length scales. Compared to the wrought variant, the elastic and yield properties are comparable at both test temperatures while tensile strength, ductility, and strain hardening capacity are lower. The fatigue life of the PBF‐LB/M variant at room temperature is slightly lower than that of the wrought material, while at 650 °C, it is vice versa. The cyclic stress response for both material variants is characterized by cyclic softening, which is more pronounced at the higher test temperature. High strain amplitudes (≥0.7%) at room temperature and especially a high testing temperature result in the formation of multiple secondary cracks at the transitions of regions comprising predominantly elongated grain morphology and columns of stacked grains with ripple patterns in the PBF‐LB/M material. This observation and pronounced crack branching and deflection indicate that the cracks are controlled by sharp micromechanical gradients and local crystallite clusters. KW - Additive manufacturing KW - Fatigue damage KW - Heat treatment KW - Inconel 718 KW - Laser powder bed fusion KW - Low-cycle fatigue KW - Tensile strength PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599316 DO - https://doi.org/10.1002/adem.202302122 SN - 1527-2648 SP - 1 EP - 17 PB - Wiley AN - OPUS4-59931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bhadeliya, Ashok A1 - Rehmer, Birgit A1 - Fedelich, Bernard A1 - Jokisch, Torsten A1 - Skrotzki, Birgit A1 - Olbricht, Jürgen T1 - High Temperature Fatigue Crack Growth in Nickel-Based Alloys Refurbished by Additive Manufacturing N2 - Hybrid additive manufacturing plays a crucial role in the restoration of gas turbine blades, where, e.g., the damaged blade tip is reconstructed by the additive manufacturing process on the existing blade made of a parent nickel-based alloy. However, inherent process-related defects in additively manufactured material, along with the interface created between the additively manufactured and the cast base material, impact the fatigue crack growth behavior in bi-material components. This study investigates the fatigue crack growth behavior in bi-material specimens of nickel-based alloys, specifically, additively manufactured STAL15 and cast alloy 247DS. The tests were conducted at 950 °C with stress ratios of 0.1 and −1. Metallographic and fractographic investigations were carried out to understand crack growth mechanisms. The results revealed significant retardation in crack growth at the interface. This study highlights the potential contributions of residual stresses and microstructural differences to the observed crack growth retardation phenomenon, along with the conclusion from an earlier study on the effect of yield strength mismatch on crack growth behavior at a perpendicular interface in bi-material specimens. T2 - Superalloys 2024 Conference CY - Champion, Pennsylvania, USA DA - 08.09.2024 KW - Fatigue crack growth KW - Bi-material structure KW - Additive manufacturing KW - Nickel-based alloys PY - 2024 SN - 978-3-031-63937-1 DO - https://doi.org/10.1007/978-3-031-63937-1_92 SN - 2367-1181 SN - 2367-1696 VL - 15th SP - 994 EP - 1001 PB - Springer CY - Cham AN - OPUS4-60907 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Suárez Ocano, Patricia T1 - Effect of heat treatment on the hierarchical microstructure and properties of 316L stainless steel produced by Laser Powder Bed Fusion (PBF-LB/M). N2 - Laser Powder Bed Fusion (PBF-LB/M) of AISI 316L stainless steel has gained popularity due to its exceptional capacity to produce complex geometries and hierarchical microstructures, which can increase the yield strength while maintaining good ductility. Nevertheless, owing to high thermal gradients encountered during the process, the as printed 316L stainless steel often exhibit microstructural heterogeneities and residual stresses, which can limit its performance in demanding environments. Hence, employing heat treatments which balance the reduction of residual stresses while retaining improved static strength may be beneficial in various scenarios and applications. This study investigates the impact of post-processing heat treatments on the microstructure of 316L stainless steel manufactured via PBF-LB/M, along with its correlation with micro-hardness properties. To this end, 6 different heat treatments, i.e., 450 °C for 4h, 700 °C for 1h, 700 °C for 3h, 800 °C for 1h, 800 °C for 3h, and 900 °C for 1h, were applied to different specimens and Vickers hardness measurements (HV1) were performed in all states. At 800 °C, although the cellular structure appears to be retained, there is an observable increase in cellular size. However, while treatments exceeding 900 °C indicate no significant grain growth compared to other conditions, the cellular structure is entirely dissolved, which leads to a reduced Vickers hardness. The effect of the heat treatments on other microstructural features such as grain size and morphology, melt pool boundaries (MPB), crystallographic texture, chemical segregation, dispersoids and phase stability are also discussed in the present work T2 - 4th Symposium on Materials and Additive Manufacturing CY - Berlin, Germany DA - 12.06.2024 KW - Additive manufacturing KW - Heat treatment KW - Microstructure PY - 2024 AN - OPUS4-60304 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sänger, Johanna A1 - König, N.F. A1 - De Marzi, A. A1 - Zocca, Andrea A1 - Franchin, G. A1 - Bermejo, R. A1 - Colombo, P. A1 - Günster, Jens T1 - Linear volumetric additive manufacturing of zirconia from a transparent photopolymerizable ceramic slurry via Xolography N2 - Advanced ceramics printed with photon-based additive manufacturing deals with anisotropic mechanical properties from the layer-by-layer manufacturing. Motivated by the success in using highly filled transparent slurries containing nanoparticles for powder-based two-photon-polymerization (2PP) for advanced ceramic printing, this works approach is the transfer to Xolography, a volumetric additive manufacturing technology based on linear two-photon excitation and without recoating steps. This paper reports the results of a preliminary investigation optimizing the photocurable slurry to the requirements of Xolography in terms of transparency, over a significantly larger mean free path, compared to 2PP. A feedstock filled with 70 % weight fraction of ceramic particles (∼30 vol%) exhibiting an exceptionally high degree of transparency in the relevant wavelength range of 400–800 nm was prepared from 5 nm zirconia nanoparticles. The high transparency of the photocurable slurry is attributed to the near-monomodal particle size distribution of the zirconia nanoparticles used. KW - Additive manufacturing KW - Xolography KW - Ceramic PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608908 DO - https://doi.org/10.1016/j.oceram.2024.100655 SN - 2666-5395 VL - 19 SP - 1 EP - 9 PB - Elsevier BV AN - OPUS4-60890 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Günster, Jens T1 - Ceramic Processing with Light N2 - In order to be able to manipulate ceramic powder compacts and ceramic suspensions (slurries) in their volume with light, a minimum transparency of the materials is required. Compared to polymers and metals, ceramic materials are characterized by the fact that they have a wide electronic band gap and therefore a wide optical window of transparency. The optical window generally ranges from less than 0.3 µm to 5 µm wavelength. Therefore, to focus light into the volume of a ceramic powder compact, its light scattering properties need to be tailored. In this study, we present the physical background and material development strategies for the application of two-photon polymerization (2PP), Xolography and selective volumetric sintering for the additive manufacturing of structures in the volume of ceramic slips and green compacts. T2 - CMCEE 14 CY - Budapest, Hungary DA - 18.08.2024 KW - Ceramic KW - Additive manufacturing KW - Light PY - 2024 AN - OPUS4-60892 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -