TY - GEN A1 - Schilling, Markus T1 - Full-Notch Creep Test Ontology (ontoFNCT) N2 - This is the stable version of the full-notch creep test ontology (OntoFNCT) that ontologically represents the full-notch creep test. OntoFNCT has been developed in accordance with the corresponding test standard ISO 16770:2019-09 Plastics - Determination of environmental stress cracking (ESC) of polyethylene - Full-notch creep test (FNCT). The OntoFNCT provides conceptualizations that are supposed to be valid for the description of full-notch creep tests and associated data in accordance with the corresponding test standard. By using OntoFNCT for storing full-notch creep test data, all data will be well structured and based on a common vocabulary agreed on by an expert group (generation of FAIR data) which is meant to lead to enhanced data interoperability. This comprises several data categories such as primary data, secondary data and metadata. Data will be human and machine readable. The usage of OntoFNCT facilitates data retrieval and downstream usage. Due to a close connection to the mid-level PMD core ontology (PMDco), the interoperability of full-notch creep test data is enhanced and querying in combination with other aspects and data within the broad field of materials science and engineering (MSE) is facilitated. The class structure of OntoFNCT forms a comprehensible and semantic layer for unified storage of data generated in a full-notch creep test including the possibility to record data from analysis and re-evaluation. Furthermore, extensive metadata allows to assess data quality and reliability. Following the open world assumption, object properties are deliberately low restrictive and sparse. KW - Ontology KW - Full-Notch Creep Test KW - FNCT KW - Knowledge Representation KW - Semantic Web Technologies KW - Data Structures KW - Data Management PY - 2024 UR - https://github.com/MarkusSchilling/ontoFNCT/blob/4abce82852190a5e444d302da077aa7404f433f0/ontoFNCT.ttl UR - https://raw.githubusercontent.com/MarkusSchilling/ontoFNCT/main/ontoFNCT.ttl PB - GitHub CY - San Francisco, CA, USA AN - OPUS4-59815 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Niebergall, Ute A1 - Marschall, Niklas A1 - Meinel, Dietmar A1 - Böhning, Martin T1 - Relation of craze to crack length during slow crack growth phenomena in high‐density polyethylene JF - Polymer Engineering & Science N2 - The craze‐crack mechanism occurring in high‐density polyethylene (HDPE) causing slow crack growth and environmental stress cracking is investigated in detail with respect to the relation of crack length and the related craze zone. This is essential for the understanding of the resulting features of the formed fracture surface and their interpretation in the context of the transition from crack propagation to ductile shear deformation. It turns out that an already formed craze zone does not inevitably result in formation of a propagating crack, but could also undergo ductile failure. For the examination, the full notch creep test (FNCT) was employed with a subsequent advanced fracture surface analysis that was performed using various imaging techniques: light microscopy, laser scanning microscopy, scanning electron microscopy, and X‐ray micro computed tomography scan. FNCT specimens were progressively damaged for increasing durations under standard test conditions applying Arkopal, the standard surfactant solution, and biodiesel as test media were used to analyze the stepwise growth of cracks and crazes. From considerations based on well‐established fracture mechanics approaches, a theoretical correlation between the length of the actual crack and the length of the preceding craze zone was established that could be evidenced and affirmed by FNCT fracture surface analysis. Moreover, the yield strength of a HDPE material exposed to a certain medium as detected by a classic tensile test was found to be the crucial value of true stress to induce the transition from crack propagation due to the craze‐crack mechanism to shear deformation during FNCT measurements. Highlights - Progress of crack formation in high‐density polyethylene is analyzed by different imaging techniques - Determined growth rates depend on distinction between craze zone and crack - The ratio of the present crack to the anteceding craze zone is validated theoretically - The transition from crack propagation to ductile shear deformation is identified - An already formed craze zone may still fail by ductile mechanisms KW - Craze-crack mechanism KW - Environmental stress cracking (ESC) KW - Full notch creep test (FNCT) KW - Laser scanning microscopy (LSM) KW - Slow crack growth (SCG) KW - X-ray computed tomography (CT) PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601831 DO - https://doi.org/10.1002/pen.26698 SN - 1548-2634 VL - 64 IS - 6 SP - 2387 EP - 2403 PB - Wiley AN - OPUS4-60183 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pavasarytė, Lina A1 - Azevedo do Nascimento, Allana A1 - Cysne Barbosa, Ana Paula A1 - Trappe, Volker A1 - Melo, Daniel T1 - Effects of particle size and particle concentration of poly (ethylene-co-methacrylic acid) on properties of epoxy resin JF - Journal of Applied Polymer Sciene N2 - Self-healing polymers have been developed to improve durability and reduce costs associated with maintenance during service. The addition of thermoplastics to thermosets to produce mendable polymers appears as a promising selfhealing technique. In this study, poly (ethylene-co-methacrylic acid) (EMAA) was added to epoxy resin and the effects of EMAA addition on epoxy properties were evaluated. Specimens with two different contents of thermoplastic and particles sizes were manufactured. A two-level full factorial experimental design was used to evaluate the effect of particle size and particle content on properties of epoxy modified with addition of EMAA. Tensile tests and dynamic mechanical analysis (DMA) were used and the evaluated responses were tensile strength, modulus of elasticity, and glass transition temperature (Tg). X-ray computed tomography (XCT) was used to investigate particle size and concentration after manufacturing. It was found that the particle concentration has greater effects on stress–strain behavior of epoxy while Tg was not significantly affected by neither of the analyzed entrance variables. KW - Fracture KW - Self-healing KW - Epoxy KW - Thermoplastic PY - 2024 DO - https://doi.org/10.1002/app.55677 SP - 1 EP - 14 PB - Wiley online library AN - OPUS4-60205 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Kalinka, Gerhard A1 - Loose, Florian T1 - Carbon fibre composites exemplarily research at BAM N2 - Lightweighting as a cross-cutting technology contributes significantly to achieve the European Green Deal goals. Based on, but not limited to, advanced materials and production technologies, the demand for natural resources and CO2 emmissions are reduced by lightweighting during production, as well as use phase. Therefore, lightweighting is a crucial transformation technology assisting in decoupling economic growth from resource consumption. In this manner, lightweighting contributes significantly as a key technology of relevance for many industrial sectors such as energy, mobility, and infrastructure, towards resource efficiency, climate action and economic strength, as well as a resilient Europe. To strengthen international partnerships, addressing global issues of today at the edge of science with high performance lightweight material based on carbon fibers, an overview about the BAM expertise in carbon fiber reinforced materials is given. T2 - Meeting KCarbon CY - Berlin, Germany DA - 15.06.2023 KW - Lightweighting KW - Carbon Fibers KW - Recycling KW - Push-out Test KW - multi scale testing PY - 2023 AN - OPUS4-58094 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Schilling, Markus A1 - Marschall, Niklas A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Dataset of comprehensive Full-notch creep tests (FNCT) of selected high-density polyethylene (PE-HD) materials N2 - The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770. The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature. KW - Polyethylene KW - Environmental Stress Cracking KW - Full-notch creep test KW - PE-HD KW - Crack growth PY - 2023 DO - https://doi.org/10.5281/zenodo.10143351 PB - Zenodo CY - Geneva AN - OPUS4-58835 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ghafafian, Carineh A1 - Trappe, Volker T1 - Prolonging structural integrity—Fatigue of scarf repairs for wind turbine blade shell applications JF - Composites Part A N2 - The influence of scarf repair variables on the mechanical properties of glass fiber reinforced polymer sandwich structures is examined for the application of wind turbine blade shell repairs. Reference shell specimens are tested under fully-reversed cyclic loading to understand the fatigue behavior of the sub-component structure within a range of in-service loads, to which shell specimens with a scarf joint repair are compared. A fatiguesuperior repair material is shown to improve the fatigue behavior of the repaired structures compared to the reference specimens. In separating layup and geometry, damage development is examined on the subcomponent scale for a structural understanding of a scarf repair using in-situ digital image correlation-based strain field measurements as well as passive thermography. Within scarf repair variables, the geometry is shown to play a larger role than layup in the fatigue performance of the repaired structure. KW - Polymer–matrix composites KW - Fatigue KW - Joints/joining PY - 2023 DO - https://doi.org/10.1016/j.compositesa.2022.107419 SN - 1359-835X VL - 167 SP - 1 EP - 11 PB - Elsevier Ltd. AN - OPUS4-56942 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Ghafafian, Carineh T1 - Scarf-joint repairs under fatigue loading investigated for sandwich shell applications N2 - Wind turbine rotor blades are produced as aerodynamic, three-dimensionally formed sandwich shell structures using mainly glass fiber reinforced plastics (GFRP). The GFRP used today have the potential to withstand the harsh operating conditions of rotor blades over the projected service life of 20 years. Premature damages that occur can be traced primarily back to design and/or manufacturing imperfections, as well as unusually high load scenarios (for instance lightning strikes, or strong winds combined with system control errors). Therefore, rotor blades have to be repaired several times (on average 2-3 times) during their projected service life. Approximately 70% of these are repairs of small- to medium-sized sandwich shells, carried out by technicians directly accessing the blade by suspended roping at the wind turbine location. The goal is to execute repairs that will last over the remaining service life, i.e. be sustainable. Within the framework of a research project carried out at BAM, Division 5.3 Polymer Matrix Composites, Department 5 for Materials Engineering, not only was the geometric shape (round vs. square in relation to the top view) varied, but also the layup of the scarf repair structure, variables that have not been studied systematically to-date. Sub-component scale sandwich shell specimens with representative repairs were used in this work in addition to coupon-scale specimens that are more commonly seen in literature. These sub-component shell specimens were tested using a unique shell test bench under loading conditions representative of wind turbine blade shell operating conditions with respect to fatigue strength. Using non-destructive testing methods (field strain measurement and thermography), damage development and distribution was monitored and analyzed in-situ. As a result, a concept was developed in which the repaired areas showed at least equivalent if not higher fatigue strength than the reference shells that were not repaired. T2 - ICFC9 - The 9th International Conference on the Fatigue of Composites CY - Vicenza, Italy DA - 21.06.2023 KW - Repair of sandwich shell structures KW - Non-destructive testing KW - Wind turbine blades PY - 2023 AN - OPUS4-57929 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krauklis, A. E. A1 - Starovka, O. A1 - Gibhardt, D. A1 - Aouissi, H. A. A1 - Burlakovs, J. A1 - Sabalina, A. A1 - Fiedler, Bodo A1 - Kalinka, Gerhard T1 - Reversible and irreversible effects on the epoxy GFRP fiber-matrix interphase due to hydrothermal aging JF - Composites Part C N2 - Epoxy R-Glass Fiber-Reinforced Polymer (GFRP) composite plates were hydrothermally aged at 60 ◦C for 23, 75, and 133 days. The water content reached 0.97 wt%, 1.45 wt% and 1.63 wt%, respectively. The studied GFRP matrix was inert to hydrolysis or chain scission, allowing for investigation of irreversible changes in the fiber-matrix interphase due to hydrothermal aging upon re-drying. During each period, a subset of the specimens was removed from the water bath and dried in a chamber. The weight loss upon drying was explained with epoxy leaching (impurities), sizing-rich interphase hydrolysis, glass fiber surface hydrolysis, accumulated degradation products escaping, and water changing state from bound to free. The influence of hydrothermal aging on the fiber-matrix interfacial properties was investigated. Lower interfacial strength of hydrothermally aged (wet) samples was attributed to plasticization of the epoxy, plasticization and degradation of the sizing-rich interphase (including formation of hydrolytic flaws), and hydrolytic degradation of the glass fiber surface. The kinetics of epoxy-compatible epoxysilane W2020 sizing-rich interphase hydrolysis provided an estimate of ca. 1.49%, 4.80%, and 8.49% of the total composite interphase degraded after 23, 75, and 133 days, respectively. At these conditions, the interface lost 39%, 48%, and 51% of its strength. Upon re-drying the specimens, a significant part of the interfacial strength was regained. Furthermore, an upward trend was observed, being 13%, 10% and 3% strength, respectively; thus, indicating a possibility of partial recovery of properties. KW - GFRP KW - Hydrothermal Ageging KW - Interphase KW - Water Diffusion KW - Desorption KW - Interfacial Strength PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581554 DO - https://doi.org/10.1016/j.jcomc.2023.100395 SN - 2666-6820 VL - 12 SP - 1 EP - 9 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-58155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kalinka, Gerhard T1 - Testing the fibre matrix interface of short glass fibre reinforced PMCs with using the push out technique N2 - With this presentation, the push-out technique is explained. The focus of the experimental work is on the characterization of the fiber-matrix interface of short fiber reinforced composites. The reinforcing component was glass fibers and the matrix polymer was PA6.6 and PPA. It is demonstrated for the first time that the push-out technique ca be applied on injection molded short fiber PMC and is sensitive to the mechanical interface properties. Further studies are planned on the influence of multiple processing, the temperature and humidity. T2 - Composirtes United Workshop „Fiber Matrix Interphases“ CY - Online meeting DA - 09.11.2023 KW - Polymer Matrix Composite KW - Glass Fibres KW - PA6.6 KW - PPA KW - Push-out Test KW - Interface Strength PY - 2023 AN - OPUS4-59053 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rabe, T. A1 - Kalinka, Gerhard A1 - Mieller, Björn T1 - Manufacturing and deformation behavior of alumina and zirconia helical springs at room temperature JF - Journal of the American Ceramic Society N2 - Ceramic helical springs with identical dimensions were produced by hard machining from alumina, alumina toughened zirconia (ATZ), and tetragonal zirconia polycrystals (TZP) stabilized with different oxides. According to the results of the spring constant determination under deformation rates of 3 mm/min, the deformation behavior of all ceramic springs obeys to Hook’s law. However, variation of the deformation rate, tests under constant load, and spring recovery behavior revealed differences in the deformation behavior of alumina, TZP, and ATZ springs. Alumina springs exhibited time-independent deformation in all tests. In contrast, anelastic deformation at room temperature was demonstrated in all springs containing TZP. This deformation is completely reversible over a period of several days. Anelastic behavior is particularly pronounced in Y-TZP springs, whereas Ce-TZP springs exhibit comparatively very low but still reliably detectable anelasticity. Oxygen vacancies in the TZP ceramic are considered the most likely explanation for the anelastic behavior of TZP springs at room temperature. KW - Alumina KW - Creep KW - Elastic properties KW - Zirconia PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-571858 DO - https://doi.org/10.1111/jace.19085 SN - 0002-7820 SP - 1 EP - 14 PB - Wiley-Blackwell CY - Oxford [u.a.] AN - OPUS4-57185 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Böhning, Martin A1 - Schilling, Markus A1 - Thuy, Maximilian A1 - Niebergall, Ute T1 - Environmental Stress Cracking in PE-HD – Assessment of Crack Propagation and Mechanisms by Optical Methods N2 - Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules. A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth. For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography. T2 - 34th Polymer Degradation Disscussion Group (PDDG) Conference CY - Dubrovnik, Croatia DA - 12.06.2023 KW - Polyethylen KW - Full Notch Creep Test KW - Environmental Stress Cracking KW - Fracture Surface Analysis PY - 2023 AN - OPUS4-57711 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Rissentwicklung in CFK-Laminaten nachgewiesen durch in situ Röntgen-Refraktion N2 - In Leichtbauanwendungen sind Materialien mit geringen Dichten und hohen Festigkeiten gefragt. Insbesondere Faser-Kunststoff-Verbunde (FKV) erfüllen diese Anforderungen und werden zunehmend für Strukturbauteile eingesetzt. Die Oberflächen moderner Rotorblätter von Windkraftanlagen werden aus FKV gefertigt. Das Versagen dieser Materialien hat massiven Einfluss auf die Einsatzfähigkeit der gesamten Windkraftanlage. Daher ist die Kenntnis des Versagensverhaltens dieser Komponenten unter statischer und zyklischer Belastung von großem Interesse, um die Betriebsbeanspruchung abzuschätzen. Im Idealfall wird die Schadensentwicklung unter Betriebslast mit zerstörungsfreien in-situ-Prüfverfahren ermittelt. Hier berichten wir über die Beobachtung der Rissentwicklung in Carbon-Faserverstärkten Kunststoffen (CFK) unter kontinuierlicher Zugbelastung durch in-situ Synchrotron-Röntgenrefraktionsradiographie. Eine selbst entwickelte elektromechanische Zugprüfmaschine mit einem Kraftbereich bis zu 15 kN wurde in den Strahlengang an der BAMline (BESSY II) integriert. Da in herkömmlichen (Absorptions-) Radiographien Defekte wie Zwischenfaserbrüche oder Faser-Matrix-Enthaftung keinen ausreichenden Kontrast verursachen, wird zur Kontrastanhebung die Röntgenrefraktion benutzt. Hier wird das sogenannte Diffraction Enhanced Imaging (DEI) angewandt, um Primär- und gebrochene Strahlung mit Hilfe eines Analysatorkristalls zu trennen. Diese Technik ermöglicht schnelle Messungen mit einem Gesichtsfeld von einigen Quadratmillimetern (hier: 14 mm × 7.2 mm) und ist ideal für in-situ Untersuchungen. Die Bildgebung und der Zugversuch erfolgen mit einer Bildfrequenz von 0.7 / s und einer Dehnrate von 0.00055 / s . Bei 0°/90° Fasergelegen treten die ersten Zwischenfaserrisse bei 380 MPa (Dehnung 0.8 %) auf. Vor dem Versagen bei ca. 760 MPa (Dehnung 2.0 %) beobachten wir die Ausbildung eines nahezu äquidistanten Rissmusters (Risse in ca. 1 mm Abstand), das sich im geschädigten Zustand über die gesamte Probe erstreckt. T2 - DACH-Jahrestagung 2023 CY - Friedrichshafen, Germany DA - 15.05.2023 KW - Röntgen-Refraktion KW - Synchrotronstrahlung KW - CFK KW - Rissentwicklung PY - 2023 AN - OPUS4-57622 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kupsch, Andreas A1 - Trappe, Volker A1 - Müller, Bernd R. A1 - Bruno, Giovanni T1 - Rissentwicklung in CFK-Laminaten nachgewiesen durch in situ Röntgen-Refraktion T2 - DGZfP-Berichtsband BB 180 N2 - In Leichtbauanwendungen sind Materialien mit geringen Dichten und hohen Festigkeiten gefragt. Insbesondere Faser-Kunststoff-Verbunde (FKV) erfüllen diese Anforderungen und werden zunehmend für Strukturbauteile eingesetzt. Die Oberflächen moderner Rotorblätter von Windkraftanlagen werden aus FKV gefertigt. Das Versagen dieser Materialien hat massiven Einfluss auf die Einsatzfähigkeit der gesamten Windkraftanlage. Daher ist die Kenntnis des Versagensverhaltens dieser Komponenten unter statischer und zyklischer Belastung von großem Interesse, um die Betriebsbeanspruchung abzuschätzen. Im Idealfall wird die Schadensentwicklung unter Betriebslast mit zerstörungsfreien in-situ-Prüfverfahren ermittelt. Hier berichten wir über die Beobachtung der Rissentwicklung in Carbon-Faserverstärkten Kunststoffen (CFK) unter kontinuierlicher Zugbelastung durch in-situ Synchrotron-Röntgenrefraktionsradiographie. Eine selbst entwickelte elektromechanische Zugprüfmaschine mit einem Kraftbereich bis zu 15 kN wurde in den Strahlengang an der BAMline (BESSY II) integriert. Da in herkömmlichen (Absorptions-) Radiographien Defekte wie Zwischenfaserbrüche oder Faser-Matrix-Enthaftung keinen ausreichenden Kontrast verursachen, wird zur Kontrastanhebung die Röntgenrefraktion benutzt. Hier wird das sogenannte Diffraction Enhanced Imaging (DEI) angewandt, um Primär- und gebrochene Strahlung mit Hilfe eines Analysatorkristalls zu trennen. Diese Technik ermöglicht schnelle Messungen mit einem Gesichtsfeld von einigen Quadratmillimetern (hier: 14 mm × 7.2 mm) und ist ideal für in-situ Untersuchungen. Die Bildgebung und der Zugversuch erfolgen mit einer Bildfrequenz von 0.7 / s und einer Dehnrate von 0.00055 / s . Bei 0°/90° Fasergelegen treten die ersten Zwischenfaserrisse bei 380 MPa (Dehnung 0.8 %) auf. Vor dem Versagen bei ca. 760 MPa (Dehnung 2.0 %) beobachten wir die Ausbildung eines nahezu äquidistanten Rissmusters (Risse in ca. 1 mm Abstand), das sich im geschädigten Zustand über die gesamte Probe erstreckt. T2 - DACH-Jahrestagung 2023 CY - Friedrichshafen, Germany DA - 15.05.2023 KW - Röntgen-Refraktion KW - Synchrotronstrahlung KW - CFK KW - Rissentwicklung PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576230 SN - 978-3-947971-29-9 VL - BB 180 SP - 1 EP - 8 AN - OPUS4-57623 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Thuy, Maximilian A1 - Brauch, N. A1 - Niebergall, Ute A1 - Alig, I. A1 - Oehler, H. A1 - Böhning, Martin T1 - Environmental Stress Cracking of PE-HD Induced by Liquid Test Media Representing Crop Protection Formulations T2 - Advances in Accelerated Testing and Predictive Methods in Creep, Fatigue, and Environmental Cracking N2 - Packaging containers for dangerous goods that include aggressive liquids require that any packaging material that is based on high-density polyethylene has a high degree of stability and durability. This work is focused on testing the environmental stress cracking of the high-density polyethylenes used for such containers in contact with crop protection formulations, in particular, two model liquids established in Germany as standardized test media representatives for crop protection formulations containing the various admixtures typical for such products. One of the liquids is water-based and contains mostly surface-active ingredients, while the other is solvent-based and includes some emulsifiers. Originally established for pin impression tests, these model liquids and their individual components were here used for the first time as environmental media in the Full Notch Creep Test, which addresses the resistance against environmental stress cracking. The Full Notch Creep Test was carried out on five high-density polyethylene types with both model liquids, and also on one selected material with its components. The evaluation was focused on the fracture surface structures, which were visualized by a scanning electron microscope and by optical in situ imaging of the notch opening. While the water-based model liquid and its surface-active individual components induced environmental stress cracking with the characteristic pattern for a craze-crack mechanism and so-called brittle fracture on the surface, the solvent-based model liquid and its soluble ingredients exhibited rather ductile failure behavior, caused by the plasticizing effect on the polymer that reduced the yield stress of the high-density polyethylene. For both cases, fracture surface analysis, together with side views of the crack opening, showed a clear relation between surface pattern, notch deformation (e.g., by blunting), or crack opening due to crack growth with time to failure and the solubility of the liquids in high-density polyethylene. KW - Environmental stress cracking KW - Fracture surface KW - Full Notch Creep Test KW - Crop protection formulations KW - High-density polyethylene PY - 2023 DO - https://doi.org/10.1520/STP164320210095 SP - 317 EP - 341 PB - ASTM International CY - West Conshohocken, PA (USA) AN - OPUS4-57459 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Altmann, Korinna A1 - Marzik, Julian T1 - Roving-Alterung und mechanische Eigenschaften N2 - Im statistischen Mittel steht eine Windkraftanlage (WKA) in Deutschland alle 6 Jahre wegen eines Schadens an den Rotorblättern und verursacht Kosten von 20k€-40k€ infolge Ertragsausfall und Reparaturkosten. Bei über 30.000 WKA in Deutschland verursacht dies jährlichen Kosten von 100-200 Mio. €. Zu 70% sind die Ursachen Fertigungsfehler. Diesem Themenkomplex widmet sich FB-5.3 in Kooperation mit FBs der Zerstörungsfreien Prüfung (Abt. 8) schon seit Jahren. Im aktuellen Projekt geht es um einen vorzeitigen Verschleiß der Rotorblätter infolge der Verwendung gealterter Glasfaser-Rovings. (GF). Die Entwicklung moderner Windkraftanlagen hatte in Europa seinen Ursprung in den 90er Jahren. OEMs und GF-Hersteller waren dicht beisammen. Die Globalisierung des Marktes führt heute zu einer weltweiten Verschiffung der GF in feucht-warmen Containern. Je nach Beschaffenheit (Chemie) der Schlichten (Oberflächenbehandlung) von GF können diese stark altern (Hydrolyse-Effekte) und die Festigkeit kann im Bauteil um bis zu 50% abgemindert sein. In einer Kooperation mit der Rotorblattallianz, einem Zusammenschluss der OEMs, Halbzeugherstellern und Forschungsinstituten, wurden schon vor 5 Jahren in einem Forschungsprojekt (FB-5.3; VH 5538) die chemischen Mechanismen der Alterung exemplarisch für eine Glasfaser-Roving-Type aufgeklärt. Im aktuellen Projekt (FB-5.3; VH 5304) wird ein beschleunigtes Alterungsverfahren (erhöhte Temperatur und Feuchte) am Roving im un-impregnierten Zustand entwickelt und die Festigkeit nachfolgend nach Einbettung in eine Epoxid-Harz-Matrix bestimmt. Je nach Alterungszustand zeigt sich eine Abnahme der Zwischenfaserbruchfestigkeit von bis zu 50%. Nicht alle Glasfaser-Roving-Typen zeigen diesen Effekt. Es ist gelungen für OEMs und Halbzeughersteller ein handhabbares Verfahren zur innerbetrieblichen Qualitätssicherung zu entwickeln, da die wenigsten Firmen über komplexe Analyseverfahren, wie an der BAM, verfügen. T2 - Composite United - AG Faserverbund in der Windenergie CY - Braunschweig, Germany DA - 09.05.2023 KW - Faserkunststoffverbunde KW - Windenergie KW - Alterung PY - 2023 AN - OPUS4-58409 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Trappe, Volker A1 - Sachs, Patrick T1 - Dynamic mechanical analysis of epoxy-matrix cross linking measured in-situ using an elastomer container N2 - A new patented dynamic mechanical analysis (DMA) is presented, where the tensile, bending- or torsional stiffness of a media can be characterized in-situ during the phase transition from liquid to solid. An epoxy system, e.g. Hexion L285/H287, is filled into an elastomer container, such as a silicone tube. This can be mounted into a conventional DMA and, based on a linear viscoelastic approach, the storage modulus (E’;G’), the loss modulus (E’’;G’’) and the loss angle tan(delta) can be measured at constant temperature as a function of time in order to investigate the liquid to sol-gel to solid transition. With this new method, the stiffness increase as a result of the cure process can be directly measured more precisely than with a rheometer in a shear plate set-up, because using an elastomer container gives a defined cross section for calculating the Young’s modulus. T2 - 20th European Conference on Composite Materials, ECCM20 CY - Lausanne, Switzerland DA - 26.06.2022 KW - Dynamic mechanical analysis (DMA) KW - Thermoset polymers KW - Cure process KW - Cross linking PY - 2022 AN - OPUS4-55213 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thuy, Maximilian A1 - Pedragosa-Rincon, M. A1 - Niebergall, Ute A1 - Oehler, H. A1 - Alig, I. A1 - Böhning, Martin T1 - Environmental Stress Cracking of High-Density Polyethylene Applying Linear Elastic Fracture Mechanics JF - Polymers N2 - The crack propagation rate of environmental stress cracking was studied on high-density polyethylene compact tension specimens under static loading. Selected environmental liquids are distilled water, 2 wt% aqueous Arkopal N100 solution, and two model liquid mixtures, one based on solvents and one on detergents, representing stress cracking test liquids for commercial crop protection products. The different surface tensions and solubilities, which affect the energetic facilitation of void nucleation and craze development, are studied. Crack growth in surface-active media is strongly accelerated as the solvents induce plasticization, followed by strong blunting significantly retarding both crack initiation and crack propagation. The crack propagation rate for static load as a function of the stress intensity factor within all environments is found to follow the Paris–Erdogan law. Scanning electron micrographs of the fracture surface highlight more pronounced structures with both extensive degrees of plasticization and reduced crack propagation rate, addressing the distinct creep behavior of fibrils. Additionally, the limitations of linear elastic fracture mechanisms for visco-elastic polymers exposed to environmental liquids are discussed. KW - Crack propagation KW - Environmental stress cracking KW - Fracture toughness KW - Crop protection products KW - High-density polyethylene KW - Craze–crack mechanism KW - Linear elastic fracture mechanics KW - Stress intensity factor PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550476 DO - https://doi.org/10.3390/polym14122415 SN - 2073-4360 VL - 14 IS - 12 SP - 1 EP - 21 PB - MDPI CY - Basel AN - OPUS4-55047 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lamoriniere, S. A1 - Mitchell, P. J. A1 - Ho, K. A1 - Kalinka, Gerhard A1 - Shaffer, M. S. P. A1 - Bismarck, A. T1 - Carbon nanotube enhanced carbon Fibre-Poly(ether ether ketone) interfaces in model hierarchical composites JF - Composites Science and Technology N2 - Poly (ether ether ketone) (PEEK) has a high continuous service temperature, excellent mechanical properties, and good solvent and abrasion resistance, which can be further improved through the addition of carbon nanotubes (CNTs). CNT-PEEK nanocomposites are promising matrices for continuous carbon fibre composites; powder processing can mitigate the high melt viscosities in these systems. In this study, model single fibre (hierarchical) composites were produced by embedding sized and desized carbon fibres in nanocomposite CNTPEEK powders followed by single fibre pull-out tests to assess interfacial characteristics. Carbon fibre-PEEK interfacial shear strength is typically 40–45 MPa. Increasing CNT loadings increased fibre-matrix interfacial shear strength linearly up to ~70 MPa at 5.0 wt%, which was attributed to the CNT-based mechanical modification of the PEEK matrix. Apparent interfacial shear strength was inversely correlated with the embedded fibre length irrespective of carbon fibre sizing or CNT loading, indicating brittle fracture of the fibre-matrix interface. Pulled out carbon fibres were still coated with the matrix, which indicated strong adhesion at the interface in all samples, likely related to a transcrystalline region. Adhesion was, however, negatively affected by the presence of epoxy sizings. Frictional shear strength was independent of embedded fibre length and CNT content for all samples. KW - Keywords: Poly(ether ether ketone) KW - Carbon fibres KW - Carbon nanotubes KW - Interfacial strength KW - Debonding PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-550052 DO - https://doi.org/10.1016/j.compscitech.2022.109327 SN - 0266-3538 VL - 221 SP - 1 EP - 8 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-55005 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Guerra, E. S. S. A1 - Silva, B. L. A1 - Melo, J. D. D. A1 - Kalinka, Gerhard A1 - Barbosa, A. P. C. T1 - Microscale evaluation of epoxy matrix composites containing thermoplastic healing agent JF - Composites Science and Technology N2 - Among the strategies to produce healable thermosetting systems is their modification by the addition of thermoplastic particles. This work investigates the influence of poly(ethylene-co-methacrylic acid) (EMAA) on fibermatrix interfacial properties of a glass fiber reinforced epoxy matrix composite. Epoxy-EMAA interactions were evaluated using differential scanning calorimetry (DSC) and infrared spectroscopy. The effects of EMAA on the epoxy network formation were evidenced by changes in glass transition temperature, cure kinetics and alteration of chemical groups during cure. Interfacial shear strength (IFSS) measurements obtained by single fiber pull-out tests indicate similar interfacial properties for pure and EMAA modified epoxy. Additionally, the potential for self-healing ability of an EMAA modified epoxy was demonstrated. However, IFSS after a healing cycle for the EMAA modified epoxy was lower as compared to the pure epoxy, because of the lower fiber-EMAA interfacial shear strength. So, thermoplastic healing agents has not only to fill cracks in the matrix material, but also have to be optimized regarding its interface properties to the reinforcing fibers. KW - Interfacial strength KW - Fiber/matrix bond KW - Self-healing KW - Polymer-matrix composites (PMC) PY - 2022 DO - https://doi.org/10.1016/j.compscitech.2022.109843 SN - 0266-3538 VL - 232 SP - 1 EP - 9 PB - Elsevier Ltd. CY - Niederlande AN - OPUS4-56379 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Alig, I. A1 - Oehler, H. A1 - Brauch, Niels A1 - Thuy, Maximilian A1 - Niebergall, Ute A1 - Böhning, Martin T1 - Charakterisierung von Behälterwerkstoffen aus Polyethylen N2 - Das langsame Risswachstum (slow crack growth, SCG) sowie der umgebungsbedingte Spannungsriss (environmental stress cracking, ESC) sind relevante Schädigungsmechanismen für teilkristalline Werkstoffe auf Basis von Polyethylen hoher Dichte (PE-HD). Der Vortrag gibt einerseits einen Überblick über die grundlegenden Struktur-Eigenschafts-Beziehungen in diesem Kontext, andererseits werden auch verschiedene praxisorientierte Prüfverfahren vorgestellt. Letztere wurden in gemeinsamen Forschungsprojekten von BAM und LBF mit dem Schwerpunkt Gefahrgutbehälter bzw. Pflanzenschutzmittel vergleichend untersucht und durch weitergehende Analytik ergänzt. T2 - 16. Tagung des Arbeitskreises Polymeranalytik Webkonferenz, Fraunhofer LBF und FGK CY - Online meeting DA - 22.03.2022 KW - Polyethylen KW - Full Notch Creep Test KW - Environmental Stress Cracking KW - Spannungsriss PY - 2022 AN - OPUS4-54547 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -