TY - CONF A1 - von Hartrott, P. A1 - Rockenhäuser, Christian A1 - Schriever, Sina A1 - Skrotzki, Birgit T1 - Correlation of the precipitate size evolution and the creep rate of the aluminium alloy EN AW 2618A at 190 °C T2 - Proceedings of the International Conference on Aluminium Alloys 16 N2 - A short description of the work done on the topic "Correlation of the precipitate size evolution and the creep rate of the aluminium alloy EN AW 2618A at 190 °C" is given. T2 - International Conference on Aluminium Alloys 16 CY - Montreal, Canada DA - 17.06.2018 KW - Alloy 2618A KW - Degradation KW - Aluminium KW - Creep KW - Coarsening PY - 2018 SN - 978-1-926872-41-4 SP - 99 AN - OPUS4-45284 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von Hartrott, P. A1 - Rockenhäuser, Christian A1 - Metzger, M. A1 - Skrotzki, Birgit T1 - Assessment of EN AW-2618A for high temperature applications considering aging effects N2 - The alloy EN AW-2618A was assessed regarding its properties for high temperature applications considering aging effects. T2 - BAM TMF-Workshop 2019 CY - Berlin, Germany DA - 13.11.2019 KW - Alloy 2618A KW - Degradation KW - Coarsening KW - Transmission electron microscopy KW - Dark-field transmission electron microscopy (DFTEM) PY - 2019 AN - OPUS4-49808 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Skrotzki, Birgit T1 - Aging processes in precipitation hardened aluminum alloys N2 - The mechanical strength of wrought high-strength aluminum alloys is essentially based on precipitation hardening, possibly in combination with prior forming, e. g. by stretching. Important parameters for achieving an optimum combination of hardness, strength, ductility, toughness, and further properties such as corrosion resistance are age-hardening temperature and time. During thermal (mechanical) treatment, nucleation and growth of precipitates takes place, leading to the desired degree of hardening. In aluminum alloys, precipitation sequences are usually passed through, i. e. a sequence of metastable precipitates is formed before the stable phase can precipitate. The optimum combination of properties is therefore based on a certain (optimum) microstructure, which can, however, change during the use of a component, since the microstructure is not stable. This happens in particular when the operating temperatures are close to the aging temperature and/or the operating times are sufficiently long. An external mechanical load may accelerate the processes. The presentation gives some examples for this. T2 - Materials Science and Engineering Congress MSE 2022 CY - Darmstadt, Germany DA - 27.9.2022 KW - Aluminium alloy KW - Precipitation hardening KW - Aging KW - Degradation PY - 2022 AN - OPUS4-55877 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scholz, Philipp A1 - Wachtendorf, Volker A1 - Elert, Anna Maria A1 - Falkenhagen, Jana A1 - Becker, Roland A1 - Hoffmann, Katrin A1 - Resch-Genger, Ute A1 - Tschiche, Harald A1 - Reinsch, Stefan A1 - Weidner, Steffen ED - Scholz, Philipp T1 - Analytical toolset to characterize polyurethanes after exposure to artificial weathering under systematically varied moisture conditions JF - Polymer Testing N2 - Polyether and -ester urethanes (PU) were exposed to artificial weathering at 40 °C and artificial UV radiation in a weathering chamber. In 3 parallel exposures, humidity was varied between dry, humid, and wet conditions. Material alteration was investigated by various analytical techniques like size exclusion chromatography (SEC), liquid chromatography-infrared spectroscopy (LC-FTIR), thermal-desorption gas chromatography-mass spectrometry (TD-GC-MS), fluorescence mapping and dynamic mechanical analysis (DMA). Our results show that depending on the weathering conditions, different degradation effects can be observed. By means of SEC an initial strong decrease of the molar masses and a broadening of the mass distributions was found. After a material dependent time span this was followed by a plateau where molar mass changes were less significant. A minor moisture-dependent degradation effect was only found for polyester PU. Fluorescence measurements on two materials revealed an increase in the luminescence intensity upon weathering process reaching a saturation level after about 500 h. The changes in the optical properties observed after different exposure conditions and times were very similar. The TD-GC-MS data showed the fate of the stabilizers and antioxidant in the course of weathering. LC-FTIR measurements revealed a change in peak intensities and the ratio of urethane and carbonyl bands. KW - Polyurethane KW - Artificial weathering KW - Moisture KW - Crosslinking KW - Degradation PY - 2019 UR - https://www.sciencedirect.com/science/article/pii/S0142941819303708 DO - https://doi.org/10.1016/j.polymertesting.2019.105996 SN - 0142-9418 VL - 78 SP - 105996, 1 EP - 9 PB - Elsevier CY - Amsterdam AN - OPUS4-48625 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - von Hartrott, P. A1 - Metzger, M. A1 - Schriever, Sina A1 - Augenstein, E. A1 - Karlin, J. A1 - Piesker, Benjamin A1 - Schweizer, Ch. A1 - Skrotzki, Birgit T1 - Lebensdauerberechnung von Aluminium-Radialverdichterrädern unter Berücksichtigung der Werkstoffalterung T2 - Tagungsband R583 FVV Frühjahrstagung 2018 N2 - In this project, a procedure was developed to improve the lifetime assessment precision of exhaust turbo charger radial compressor wheels made from the age hardenable aluminum alloy EN AW-2618A. This comprises particularly the consideration of material aging, which has to be anticipated during operation of such components under relevant service conditions (temperature, time, stress). First of all, a solid experimental database was established for the investigated material. This includes a mechanical as well as a microstructural characterization of the as-received state (T61) and after aging up to 25,000 h at relevant service temperatures (160 °C, 180 °C, 190 °C). The microstructural investigations focused on the development of the radii of the cylindrical hardening phase, which coarsens during aging. The relation between aging temperature, time and mechanical load (if applicable) was established for the first time to this extent. An interrelationship to describe the coarsening was established. The effect of aging on hardness, strength, creep behavior and fatigue lifetime (LCF, TMF) was studied and a correlation to the microstructure was established. The results of the creep tests were used to calibrate a modified hyperbolic sine creep model. A time and temperature dependent deformation model according to Chaboche, which describes the relevant phenomena of high temperature deformation and cyclic plasticity, was extended. It now considers material aging by describing the strength not only as a function of temperature but also as a function of aging, i.e. of the mean radius of the precipitates. A similar procedure was applied to extend the model in order to assess the fatigue lifetime. The calculated lifetimes of LCF and TMF tests completed during this project match well with the experimental results. Only one LCF test with a hold time of 900 s in tension deviates clearly from the mean value and shows the limits of the time independent damage model. Tests with shorter hold times of 60 s are within the scatter band, likewise the different aging conditions. A damage accumulation model additionally describing the progressive aging during lifetime was developed and implemented. Besides considering aging in the deformation and lifetime assessment, it is also possible to judge complex loading cycles in a postprocessing by rain flow classification of typical complex loading cycles. The methodology and the models were implemented into the Finite-Element software Abaqus and Ansys and are available for numerical assessment of components. N2 - In diesem Forschungsvorhaben wurde ein Verfahren entwickelt, um die Genauigkeit der Lebensdauerbewertung für Abgasturbolader (ATL)-Verdichterräder aus der ausscheidungs-härtbaren Aluminiumlegierung EN AW-2618A zu verbessern. Dies umfasst insbesondere die Berücksichtigung der Werkstoffalterung, mit der beim Einsatz dieser Bauteile unter entsprechender Betriebsbeanspruchung (Temperatur, Zeit, Spannung) gerechnet werden muss. Zunächst wurde eine solide experimentelle Datenbasis für den untersuchten Werkstoff geschaffen. Dies umfasste sowohl eine mechanische als auch eine mikrostrukturelle Charakterisierung des Ausgangszustands (T61) sowie von ausgelagerten Zuständen bis zu 25.000 h bei betriebsrelevanten Temperaturen (160 °C, 180 °C, 190 °C). Bei den Untersuchungen zur Mikrostruktur wurde der Fokus auf die Entwicklung der Radien der stäbchen-förmigen aushärtenden Phase gelegt, die während der Alterung vergröbern. Der Zusammenhang zwischen Auslagerungstemperatur, -zeit und ggfs. mechanischer Belastung wurde erstmals in diesem Umfang quantifiziert und entsprechende Gesetzmäßigkeiten zur Beschreibung der Vergröberung ermittelt. Vergleichend dazu wurde der Einfluss der Alterung auf die Härte, die Festigkeit, das Kriechverhalten und die Ermüdungslebensdauer (LCF, TMF) bestimmt, so dass eine Korrelation zur Mikrostruktur vorliegt. Die Ergebnisse der Kriechversuche wurden zur Kalibrierung eines modifizierten Sinus-hyperbolicus-Kriechmodells verwendet. Ein zeit- und temperaturabhängiges Verformungsmodell nach Chaboche, welches die wesentlichen Phänomene der Hochtemperaturverformung und der Wechselplastizität beschreibt, wurde erweitert und berücksichtigt nun die Werkstoffalterung, indem die Festigkeit nicht nur als Funktion der Temperatur, sondern auch des Alterungszustands (d. h. des mittleren Radius der Ausscheidungen) dargestellt wird. Für die Erweiterung des Modells zur Bewertung der Ermüdungslebensdauer wurde analog verfahren. Die berechnete Lebensdauer der im Verlauf des Vorhabens durchgeführten LCF- und TMF-Versuche stimmt gut mit den experimentellen Ergebnissen überein. Lediglich ein LCF-Versuch mit einer Haltezeit von 900 s im Zug weicht deutlich vom Mittelwert ab und zeigt die Grenzen des zeitunabhängigen Schädigungsmodells auf. Versuche mit kürzeren Haltezeiten bis zu 60 s liegen im Streuband, ebenso die verschiedenen Alterungszustände. Eine Schädigungsakkumulation unter Berücksichtigung der fortschreitenden Alterung über der Lebensdauer wurde entwickelt und implementiert. Neben der Berücksichtigung der Alterung in der Verformungs- und Lebensdaueranalyse besteht auch die Möglichkeit, komplexe Belastungszyklen in einem Postprozessing zu bewerten, indem Rainflow-Klassierungen typischer komplexer Belastungszyklen vorgenommen werden. Die Methodik und die Modelle wurden in die Finite-Elemente-Programme Abaqus und Ansys implementiert und stehen für die rechnerische Bewertung von Bauteilen zur Verfügung. T2 - FVV Frühjahrstagung 2018 CY - Bad Neuenahr, Germany DA - 22.03.2018 KW - Aluminium KW - Centrifugal compressor wheel KW - Dark-field transmission electron microscopy (DFTEM) KW - Degradation KW - S-phase PY - 2018 SP - 97 EP - 130 AN - OPUS4-44604 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Rockenhäuser, Christian A1 - von Hartrott, P. A1 - Metzger, M. A1 - Karlin, J. A1 - Skrotzki, Birgit A1 - Schweizer, C. T1 - Lebensdauerberechnung von Aluminium-Radialverdichterrädern unter Berücksichtigung der Werkstoffalterung N2 - Die Mikrostruktur von ausscheidungsgehärteten Aluminiumlegierungen ist von herausragender Bedeutung für ihre Festigkeit, da nur Werkstoffe mit gezielt eingestellter Mikrostruktur für Radialverdichterräder ausreichende Festigkeiten erreichen. Diese optimierte Mikrostruktur ändert sich jedoch während des Betriebs, denn die Bauteile werden bei Temperaturen eingesetzt, die nahe der Aushärtetemperatur liegen oder sogar darüber hinausgehen und folglich ist mit Alterung der Mikrostruktur und damit einhergehender Degradation der Eigenschaften zu rechnen. Diese Effekte konnten bisher in der Lebensdauervorhersage nicht berücksichtigt werden, da ihre diesbezüglichen Auswirkungen lediglich qualitativ bekannt waren. In diesem Forschungsvorhaben wurde daher für die Legierung EN AW-2618A einerseits eine sorgfältige und umfassende Charakterisierung der Gefügeentwicklung für anwendungsrelevante Temperaturen und Zeiten bis zu 25.000 h vorgenommen und andererseits eine solide Datenbasis bezüglich der mechanischen Eigenschaften (Zugfestigkeit, Kriechwiderstand, LCF-, TMF-Verhalten) und ihren Änderungen geschaffen. Darauf aufbauend wurde ein Verfahren entwickelt, um die Genauigkeit der Lebensdauerbewertung für Abgasturbolader (ATL)-Verdichterräder aus EN AW-2618A zu verbessern. Ein zeit- und temperaturabhängiges Verformungsmodell nach Chaboche, welches die wesentlichen Phänomene der Hochtemperaturverformung und der Wechselplastizität beschreibt, wurde erweitert und berücksichtigt nun die Werkstoffalterung, indem die Festigkeit nicht nur als Funktion der Temperatur, sondern auch des Alterungszustands (d. h. des mittleren Radius der Ausscheidungen) dargestellt wird. Für die Erweiterung des Modells zur Bewertung der Ermüdungslebensdauer unter Rainflow-klassierten Betriebslastkollektiven wurde analog verfahren. Die berechnete Lebensdauer der im Verlauf des Vorhabens durchgeführten LCF- und TMF-Versuche stimmt gut mit den experimentellen Ergebnissen überein. KW - Alloy 2618A KW - Degradation KW - Dark-field transmission electron microscopy (DFTEM) KW - S-Phase KW - Aluminum PY - 2018 SP - 1 EP - 123 AN - OPUS4-44618 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - von Hartrott, P. A1 - Metzger, M. A1 - Schriever, Sina A1 - Augenstein, E. A1 - Karlin, J. A1 - Piesker, Benjamin A1 - Schweizer, C. A1 - Skrotzki, Birgit T1 - Lifetime Assessment of Aluminium radial compressor wheels considering material ageing N2 - The results of the project "Lifetime Assessment of Aluminium radial compressor wheels considering material ageing" were presented. T2 - FVV Frühjahrstagung 2018 CY - Bad Neuenahr, Germany DA - 22.03.2018 KW - Alloy 2618A KW - Degradation KW - S-phase KW - Dark-field transmission electron microscopy KW - Aluminum PY - 2018 AN - OPUS4-44706 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - Häusler, I. A1 - Piesker, B. A1 - Skrotzki, Birgit T1 - Influence of prestraining on the aging response of an Al-Cu-Li alloy N2 - The influence of prestraining on the aging response of an Al-Cu-Li alloy is investigated by preparation of different strain states (3 %, 4 %, 6 %) of the initial aging state. The Brinell hardness of the subsequently aged samples (up to 60 h aging time) was measured and it was found that the increasing dislocation concentration in the 3 different initial states leads to faster hardness increases and slightly higher maximum hardness. T2 - Microscopy Conference 2019 (MC2019) CY - Berlin, Germany DA - 01.09.2019 KW - Al-Cu-Li alloys KW - Degradation KW - Hardness PY - 2019 AN - OPUS4-48953 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - von Hartrott, P. A1 - Metzger, M. A1 - Skrotzki, Birgit T1 - Digital material representation of alloy 2618A for the lifetime assessment of radial compressor wheels N2 - The concept of digital material representation is introduced and the aluminium alloy 2618A is discussed as an example of this concept regarding the simulation of material ageing based on nanoscaled precipitates. T2 - Microscopy Conference 2019 (MC2019) CY - Berlin, Germany DA - 01.09.2019 KW - Alloy 2618A KW - Degradation KW - Coarsening KW - Transmission electron microscopy KW - Digital material representation PY - 2019 AN - OPUS4-48954 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - Skrotzki, Birgit T1 - The long-term ageing process of alloy 2618A N2 - The long-term ageing process of alloy 2618A was introduced and discussed The dark-field transmission electronmicroscopical resilts werde shown and evaluated regarding the precipitate radii. The influence of the precipitate radii regarding ageing was used for a preliminary ageing assessment. T2 - 19th International Microscopy Congress (IMC19) CY - Sydney, Australia DA - 09.09.2018 KW - Alloy 2618A KW - Degradation KW - Coarsening KW - S-phase KW - Dark-field transmission electron microscopy (DFTEM) PY - 2018 AN - OPUS4-46120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - Skrotzki, Birgit T1 - The long-term ageing process of alloy 2618A N2 - The long-term ageing process of alloy 2618A was introduced and discussed The dark-field transmission electronmicroscopical resilts werde shown and evaluated regarding the precipitate radii. The influence of the precipitate radii regarding ageing was used for a preliminary ageing assessment. T2 - 19th International Microscopy Congress (IMC19) CY - Sydney, Australia DA - 09.09.2018 KW - Alloy 2618A KW - Degradation KW - Coarsening KW - S-phase KW - Dark-field transmission electron microscopy (DFTEM) PY - 2018 AN - OPUS4-46123 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - Häusler, Ines A1 - Darvishi Kamachali, Reza A1 - Heidl, Daniel A1 - Skrotzki, Birgit T1 - Influence of heat treatment and creep loading on an Al-Cu-Li alloy N2 - The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process. T2 - 19th International Microscopy Congress (IMC19) CY - Sydney, Australia DA - 09.09.2018 KW - Aluminium KW - Degradation KW - Coarsening KW - Dark-field transmission electron microscopy PY - 2018 AN - OPUS4-46129 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rockenhäuser, Christian A1 - Häusler, Ines A1 - Darvishi Kamachali, Reza A1 - Heidl, Daniel A1 - Skrotzki, Birgit T1 - Influence of heat treatment and creep loading on an Al-Cu-Li alloy N2 - The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process. T2 - 19th International Microscopy Congress (IMC19) CY - Sydney, Australia DA - 09.09.2018 KW - Aluminium KW - Degradation KW - Coarsening KW - Dark-field transmission electron microscopy PY - 2018 AN - OPUS4-46131 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mueller, Axel A1 - Becker, Roland A1 - Dorgerloh, Ute A1 - Simon, Franz-Georg A1 - Braun, Ulrike T1 - The effect of polymer aging on the uptake of fuel aromatics and ethers by microplastics JF - Environmental Pollution N2 - Microplastics are increasingly entering marine, limnic and terrestrial ecosystems worldwide, where they sorb hydrophobic organic contaminants. Here, the sorption behavior of the fuel-related water contaminants benzene, toluene, ethyl benzene and xylene (BTEX) and four tertiary butyl ethers to virgin and via UV radiation aged polypropylene (PP) and polystyrene (PS) pellets was investigated. Changes in material properties due to aging were recorded using appropriate polymer characterization methods, such as differential scanning calorimetry, Fourier transform infrared spectroscopy, gel permeation chromatography, X-ray photoelectron spectroscopy, and microscopy. Pellets were exposed to water containing BTEX and the ethers at 130-190 mg/L for up to two weeks. Aqueous sorbate concentrations were determined by headspace gas chromatography. Sorption to the polymers was correlated with the sorbate's Kow and was significant for BTEX and marginal for the ethers. Due to substantially lower glass transition temperatures, PP showed higher sorption than PS. Aging had no effect on the sorption behavior of PP. PS sorbed less BTEX after aging due to an oxidized surface layer. KW - BTEX KW - Polypropylene KW - Polystyrene KW - Sorption KW - Degradation PY - 2018 DO - https://doi.org/10.1016/j.envpol.2018.04.127 SN - 0269-7491 VL - 240 SP - 639 EP - 646 PB - Elsevier CY - Amsterdam AN - OPUS4-44990 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mair, Georg A1 - Gesell, Stephan T1 - Betriebsfestigkeit von Composite-Wasserstoffspeichern Erster Ansatz zur Simulation der Auswirkung der erstmaligen Prüfung T2 - VDI-Berichte 2345 N2 - Druckbehälter werden vor ihrer Inbetriebnahme obligatorisch einer hydraulischen Prüfung bis zum sog. Prüfdruck belastet. Damit sollen fehlerhaft gefertigte Individuen erkannt und ausgesondert werden. Mit dieser Prüfung werden aber auch diejenigen Einzelbehälter ausgesondert, die ohne einem nachvollziehbaren Fertigungsfehler, nur auf Basis der statistischen Streuung ggf. eine Festigkeit unterhalb des Prüfdrucks aufweisen. Da der Prüfdruck im Fall der Wasserstoffspeicher mindestens 20% über dem maximal zulässigem Betriebsdruck liegt, wäre damit ein Versagen im Betrieb ausgenommen, gäbe es die verschiedenen Alterungs- bzw. Ermüdungseffekt nicht. Um den Einfluss der erstmaligen Prüfung auf eine angenommene ausfallfreie Zeit bewerten zu können, wird hier die Alterung und die erstmalige Prüfung in Kombination analysiert. Hierzu wird auf Basis der Restfestigkeitsdaten aus einer umfangreichen Prüfkampagne ein Ansatz für die Beschreibung der Alterung ermittelt und auf andere Lastzustände übertragen. So kann für das Baumuster, das der o.g. Prüfkampagne zugrunde lag, mithilfe einer Monte-Carlo-Simulation gezeigt werden, dass mindestens 10.000 LW vor einem ersten Alterungsversagen mit 1 aus 1 Mio. In Abhängigkeit der Anzahl der Individuen, die bei der erstmaligen Prüfung versagen, und der Streuung der gesamten Population, kann diese Mindestfestigkeit auf realistisch 50.000 Lastwechsel steigen. Damit ist gezeigt, dass aufgrund der erstmaligen Prüfung eine Mindestfestigkeit erzeugt wird, die stark vom Alterungsverhalten abhängt. Im Ergebnis heißt dies, dass in den Vorschriften aktuell die Bedeutung des Mindestberstdrucks in der Baumusterprüfung überschätzt und die möglichst betriebsbegleitende Erfassung der Alterung unterschätzt sind. T2 - 29. Fachtagung Technische Zuverlässigkeit 2019 CY - Nürtingen, Germany DA - 07.05.2019 KW - Alterung KW - Berstdruck KW - Streuung KW - Degradation KW - statistische Auswertung KW - ausfgallfreie Lastwechsel PY - 2019 SN - 978-3-18-092345-1 SN - 0083-5560 SP - 223 EP - 234 PB - VDI-Verlag GmbH CY - Düsseldorf AN - OPUS4-50181 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mair, Georg A1 - Becker, B. A1 - Gesell, Stephan A1 - Wang, Bin T1 - Monte-Carlo-analysis of minimum load cycle requirements for composite cylinders for hydrogen JF - International Journal of Hydrogen Energy N2 - Hydrogen is an attractive energy carrier that requires high effort for safe storage. For ensuring safety, storage cylinders must undergo a challenging approval process. Relevant standards and regulations for composite cylinders used for the transport of hydrogen and for its onboard storage are currently based on deterministic (e.g. ISO 11119-3) or to some respect semi-probabilistic criteria (UN GTR No. 13; with respect to burst strength). This paper provides a systematic analysis of the load cycle properties resulting from these regulations and standards. Their characteristics are compared with the probabilistic approach of the Federal Institute for Materials Research and Testing BAM. The most important aspect of comparing different concepts is the rate for accepting designs with potentially unsafe or critical safety properties. This acceptance rate is analysed by operating Monte-Carlo simulations over the available range of production properties. T2 - ICHS 2017 CY - Hamburg, Germany DA - 11.09.2017 KW - Safety assessment KW - Failure rate KW - Ageing KW - Degradation KW - End of life KW - Production scatter PY - 2018 DO - https://doi.org/10.1016/j.ijhydene.2018.09.185 SN - 0360-3199 VL - 44 IS - 17 SP - 8833 EP - 8841 PB - Elsevier Ltd AN - OPUS4-46341 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erdmann, Maren A1 - Niebergall, Ute A1 - Wachtendorf, Volker A1 - Böhning, Martin T1 - Evaluation of UV-induced embrittlement of PE-HD by Charpy impact test JF - Journal of Applied Polymer Science N2 - The impact fracture behavior of two common high-density polyethylene grades for container applications were intensively studied by the instrumented Charpy impact test after well-defined exposure to UV-irradiation. Individual stages of the impact event, such as crack initiation and crack propagation energy as well as maximum impact load, were investigated from the recorded load–deflection curves. UV-induced material property changes were further investigated by infrared spectroscopy, differential scanning calorimetry, and dynamic-mechanical analysis as well as density measurements. Based on the results of the Charpy impact test, three indicators were identified to describe the extend of photooxidation on high-density polyethylene: (a) a reduced Charpy impact strength—at least to half of its initial value for a distinctly brittle impact fracture, (b) a marked decrease in the crack propagation contribution to the impact strength, and (c) an increase of the brittle features of the fracture surface. KW - Degradation KW - Mechanical properties KW - Packaging KW - Polyolefins KW - Polyethylene PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509130 DO - https://doi.org/10.1002/APP.49069 SN - 0021-8995 VL - 137 IS - 36 SP - 49069 PB - Wiley AN - OPUS4-50913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erdmann, Maren A1 - Böhning, Martin A1 - Niebergall, Ute T1 - Physical and chemical effects of biodiesel storage on high-density polyethylene: Evidence of co-oxidation JF - Polymer Degradation and Stability N2 - The physical and chemical effects of diesel and biodiesel fuels on two high-density polyethylene (PE-HD) types were investigated. Both semi-crystalline PE-HD are common thermoplastic materials for container and storage tank applications. Biodiesel, a composition of unsaturated fatty acid esters from renewable resources, was chosen as it is regarded a possible green alternative to fossil fuels. The study aims at identifying significant differences between biodiesel and conventional diesel fuels based on the differences in the chemical nature of the two. The physical effects of the fuels on the polymer at first comprises the sorption behavior, i.e. kinetics and final equilibrium concentration. Not only are both fuels absorbed by the amorphous phase of the semi-crystalline PE-HD, they also induce a plasticization effect that modifies the molecular mobility and therefore also the characteristic yielding properties, manifest in the obtained stress-strain curves. The chemical effects related to degradation phenomena is investigated by a long-term storage scenario using partially immersed tensile test specimens in diesel and biodiesel. We were able to confirm the proposed co-oxidation mechanism by Richaud et al. for polyethylene-unsaturated penetrant systems on a larger scale based on practical tensile tests. One of the investigated polyethylene grades subjected to tensile drawing showed a significant loss of plastic deformation and the onset of premature failure after 150 days of storage in biodiesel. Further biodiesel storage showed a systematically reduced elongation at break before necking. None of these effects were observed in diesel. Oxidation of fuels and polymer after progressing storage times were analyzed by the evolution of carbonyl species in FT-IR/ATR spectroscopy. KW - Biodiesel KW - Degradation KW - Long-term storage KW - Sorption KW - Diesel PY - 2019 DO - https://doi.org/10.1016/j.polymdegradstab.2019.01.018 SN - 0141-3910 VL - 161 IS - 1 SP - 139 EP - 149 PB - Elsevier CY - Amsterdam AN - OPUS4-47268 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Agudo Jácome, Leonardo A1 - Suárez Ocaño, Patricia T1 - The Al4-xZr5(Ox-y) Trojan horse in the AlMo0.5NbTiTa0.5Zr refractory high entropy superalloy N2 - Unlike conventional alloys, which typically consist of one main element, high-entropy alloys (HEAs) contain five or more principal elements, which broaden chemical complexity and with it a realm of synergistic mechanisms. The AlMo0.5NbTa0.5TiZr HEA initiated a subclass of Al-containing refractory (r)HEAs that has recently drawn attention [2]. The alloy has a superalloy-resembling B2/bcc nanostructure, which inspired its name refractory high entropy superalloy (RSA). With high-temperature (HT) compressive strengths beyond conventional Ni-based superalloys, this nanostructure could be used for improved HT structural applications. However, in the application-relevant HT regime the Al-Zr-rich B2 phase decomposes to form a hexagonal Al-Zr-based intermetallic (Al4-xZr5; x: 0..1) [3,4]. This work explores the fascinating yet fatal micromechanisms associated to this phase transformation, in the context of creep, annealing and oxidation experiments performed between 800 and 1200 °C. The material was produced by arc-melting and heat treatment in argon, which lead to grain boundaries decorated with up to 7%. Interrupted constant-load creep tests were performed under vacuum (at 10-4 Pa), at 900–1100 °C with external tensile stresses of 30–120 MPa. Oxidation experiments were separately conducted for 24 hours at 800 and 1000 °C in both dry (21% O2 + 79% N2) and humid (8% O2 + 74% N2 + 18% H2O) air. After the experiments, the samples were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy to reveal degradation mechanisms. Crystallographic texture, orientation relationships and stabilization of an oxygen-containing iso structure (Al4-xZr5(Ox-y); y: 0..x) of the Al-Zr-rich intermetallic are found and discussed. T2 - BCC Superalloy Network Opening Workshop CY - Reutte, Austria DA - 08.02.2024 KW - High entropy alloy KW - Superalloy KW - Degradation KW - Electron microscopy KW - Microstructure PY - 2024 AN - OPUS4-59833 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -