TY - JOUR A1 - Darvishi Kamachali, Reza T1 - A model for grain boundary thermodynamics JF - RSC Advances N2 - Systematic microstructure design requires reliable thermodynamic descriptions of each and all microstructure elements. While such descriptions are well established for most bulk phases, thermodynamic assessment of microstructure defects is challenging because of their individualistic nature. In this paper, a model is devised for assessing grain boundary thermodynamics based on available bulk thermodynamic data. We propose a continuous relative atomic density field and its spatial gradients to describe the grain boundary region with reference to the homogeneous bulk and derive the grain boundary Gibbs free energy functional. The grain boundary segregation isotherm and phase diagram are computed for a regular binary solid solution, and qualitatively benchmarked for the Pt–Au system. The relationships between the grain boundary's atomic density, excess free volume, and misorientation angle are discussed. Combining the current density-based model with available bulk thermodynamic databases enables constructing databases, phase diagrams, and segregation isotherms for grain boundaries, opening possibilities for studying and designing heterogeneous microstructures. KW - Phase Diagram KW - Thermodynamics KW - Grain boundary PY - 2020 VL - 10 IS - 45 SP - 26728 EP - 26741 AN - OPUS4-51268 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Darvishi Kamachali, Reza A1 - Rockenhäuser, Christian A1 - Saxena, A. A1 - Skrotzki, Birgit A1 - Umer Bilal, M. A1 - Ramirez, Daniela Valencia A1 - Schwarze, C. A1 - Häusler, I. T1 - Chemo-mechanical Coupling Effect During Precipitation in AlLi and AlLiCu systems N2 - The chemo-mechanical coupling effect during precipitation in AlLi and AlLiCu systems is presented and effects of chemo-mechanical coupling on materials with different microstructures is discussed. The results of the simulations are then compared to electron-microscopical investigations. T2 - Plenary meeting DFG Priority program 1713 ("Chemomechanics") CY - Bochum, Germany DA - 17.12.2018 KW - Al-Li alloys KW - Phase field simulation KW - Precipitation KW - Inverse ostwald ripening KW - Transmission electron microscopy PY - 2018 AN - OPUS4-46961 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Darvishi Kamachali, Reza T1 - Interfacial Spinodals N2 - Despite their finite spatial extent, interfaces can have profound impacts on microstructure properties. This is because of their distinct phase-like properties distinguishing them from the adjacent homogeneous bulk structure. When noticed by solute atoms, interfaces can experience their own chemical phase changes. In this talk, we investigate the constrained states of chemically decomposed phases at interfaces. A density-based theory of interfaces is proposed to describe the confined chemical decomposition at general grain boundaries. Here the grain boundary is viewed as a lesser dense, defected structure with reference to the corresponding bulk structure. Using this picture, the thermodynamic origins of interfacial spinodal phenomena are revealed. We also show that transient interfacial spinodals can be activated over a large alloy composition range, enabling kinetic engineering of interfacial chemistry. T2 - TMS 2021 CY - Online meeting DA - 15.03.2021 KW - Microstrucrue Design KW - Spinodal Decomposition KW - Interfacial Spinodal PY - 2021 AN - OPUS4-52338 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Darvishi Kamachali, Reza A1 - da Silva, A. A1 - McEniry, E. A1 - Gault, B. A1 - Neugebauer, J. A1 - Raabe, D. T1 - Segregation-assisted spinodal and transient spinodal phase separation at grain boundaries JF - NPJ Computational Materials N2 - Segregation to grain boundaries affects their cohesion, corrosion, and embrittlement and plays a critical role in heterogeneous nucleation. In order to quantitatively study segregation and low-dimensional phase separation at grain boundaries, here, we apply a density-based phase-field model. The current model describes the grain-boundary thermodynamic properties based on available bulk thermodynamic data, while the grain-boundary-density profile is obtained using atomistic simulations. To benchmark the performance of the model, Mn grain-boundary segregation in the Fe–Mn system is studied. 3D simulation results are compared against atom probe tomography measurements conducted for three alloy compositions. We show that a continuous increase in the alloy composition results in a discontinuous jump in the segregation isotherm. The jump corresponds to a spinodal Phase separation at grain boundary. For alloy compositions above the jump, we reveal an interfacial transient spinodal phase separation. The transient spinodal phenomenon opens opportunities for knowledge-based microstructure design through the chemical manipulation of grain boundaries. The proposed density-based model provides a powerful tool to study thermodynamics and kinetics of segregation and phase changes at grain boundaries. KW - Grain Boundary Spinodal KW - Densty-based Thermodynamics KW - Microstrucrue Design PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519497 DO - https://doi.org/10.1038/s41524-020-00456-7 VL - 6 IS - 1 SP - 191 PB - Nature AN - OPUS4-51949 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Darvishi Kamachali, Reza A1 - Wang, L. T1 - Elastic energy of multi-component solid solutions and strain origins of phase stability in high-entropy alloys JF - Scripta materialia N2 - The elastic energy of mixing for multi-component solid solutions is derived by generalizing Eshelby's sphere-in-hole model. By surveying the dependence of the elastic energy on the chemical composition and lattice misfit, we derive a lattice strain coefficient λ*. Studying several high-entropy alloys and superalloys, we propose that most solid solution multi-component alloys are stable when λ*<0.16, generalizing the Hume-Rothery atomic-size rule for binary alloys. We also reveal that the polydispersity index δ, frequently used for describing strain in multi-component alloys, directly represents the elastic energy e with e=qδ², q being an elastic constant. Furthermore, the effects of (i) the number and (ii) the atomic-size distribution of constituting elements on the phase stability of high-entropy alloys were quantified. The present derivations and discussions open for richer considerations of elastic effects in high-entropy alloys, offering immediate support for quantitative assessments of their thermodynamic properties and studying related strengthening mechanisms. KW - Ordering KW - High-entropy alloys KW - Alloy design KW - Strain energy KW - Phase stability PY - 2022 DO - https://doi.org/10.1016/j.scriptamat.2021.114226 SN - 1359-6462 VL - 206 SP - 1 EP - 6 PB - Elsevier CY - Amsterdam AN - OPUS4-53427 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Darvishi Kamachali, Reza A1 - Wang, Lei A1 - Lin, L. L. A1 - Manzoni, Anna Maria A1 - Skrotzki, Birgit A1 - Thompson, G. B. T1 - CALPHAD-informed density-based grain boundary thermodynamics N2 - The Gibbs free energy of a grain boundary is a complex thermodynamic function of temperature, pressure, and composition. These complexities add to the intrinsic crystallographic and chemical constraints imposed by the adjacent bulk phase. Recently we have proposed a density-based model for assessing grain boundary thermodynamics that enables a CALPHAD-informed description of the grain boundary. As such, the Gibbs free energy of the grain boundary is directly linked with available CALPHAD thermodynamic data. In this talk, new aspects of interfacial segregation and phase transformation are revealed by benchmarking the current model for various experimental cases, including several steels, high-entropy alloys and aluminum alloys. The effects of elastic interactions on the grain boundary segregation and the application of the model to a nanocrystalline Pt-Au alloy, with numerous grain boundaries of various characters, will be discussed. T2 - DPG (Deutsche Physiker Gesellschaft) CY - Online meeting DA - 27.09.2021 KW - Density-based model KW - Defects thermodynamics KW - Defects phase diagram KW - CALPHAD KW - Crystal Defects PY - 2021 AN - OPUS4-53556 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Häusler, Ines A1 - Darvishi Kamachali, Reza A1 - Hetaba, W. A1 - Skrotzki, Birgit T1 - Thickening of T-1 Precipitates during Aging of a High Purity Al–4Cu–1Li–0.25Mn Alloy JF - Materials N2 - The age hardening response of a high-purity Al–4Cu–1Li–0.25Mn alloy (wt. %) during isothermal aging without and with an applied external load was investigated. Plate shaped nanometer size T1 (Al2CuLi) and θ′ (Al2Cu) hardening phases were formed. The precipitates were analyzed with respect to the development of their structure, size, number density, volume fraction and associated transformation strains by conducting transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM) studies in combination with geometrical Phase analysis (GPA). Special attention was paid to the thickening of T1 phase. Two elementary types of single-layer T1 precipitate, one with a Li-rich (Type 1) and another with an Al-rich (Defect Type 1) central layer, were identified. The results show that the Defect Type 1 structure can act as a precursor for the Type 1 structure. The thickening of T1 precipitates occurs by alternative stacking of These two elementary structures. The thickening mechanism was analyzed based on the magnitude of strain associated with the precipitation transformation normal to its habit plane. Long-term aging and aging under load resulted in thicker and structurally defected T1 precipitates. Several types of defected precipitates were characterized and discussed. For θ′ precipitates, a ledge mechanism of thickening was observed. Compared to the normal aging, an external load applied to the peak aged state leads to small variations in the average sizes and volume fractions of the precipitates. KW - Al-Cu-Li-alloy KW - Precipitation KW - T1 precipitate KW - Microstructure evolution KW - Thickening KW - Creep KW - Volume fraction KW - Number density KW - Strain difference PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-471207 DO - https://doi.org/10.3390/ma12010030 SN - 1996-1944 VL - 12 IS - 1 SP - 30, 1 EP - 23 PB - MDPI AN - OPUS4-47120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Li, L. A1 - Darvishi Kamachali, Reza A1 - Li, Z. A1 - Zhang, Z. T1 - Grain boundary energy effect on grain boundary segregation in an equiatomic high-entropy alloy JF - Physical Review Materials N2 - Grain boundary (GB) Segregation has a substantial effect on the microstructure evolution and properties of polycrystalline alloys. The mechanism of nanoscale segregation at the various GBs in multicomponent alloys is of great challenge to reveal and remains elusive so far. To address this issue, we studied the GB segregation in a representative equiatomic FeMnNiCoCr high-entropy alloy (HEA) aged at 450 °C. By combining transmission Kikuchi diffraction, atom probe tomography analysis and a density-based thermodynamics modeling, we uncover the nanoscale segregation behavior at a series of well-characterized GBs of different characters. No segregation occurs at coherent twin boundaries; only slight nanoscale segregation of Ni takes place at the low-angle GBs and vicinal \Sigma 29b coincidence site lattice GBs. Ni and Mn show cosegregation of high levels at the general high-angle GBs with a strong depletion in Fe, Cr, and Co. Our density-based thermodynamic model reveals that the highly negative energy of mixing Ni and Mn is the main driving force for nanoscale cosegregation to the GBs. This is further assisted by the opposite segregation of Ni and Cr atoms with a positive enthalpy of mixing. It is also found that GBs of higher interfacial energy, possessing lower atomic densities (higher disorder and free volume), show higher segregation levels. By clarifying the origins of GB segregations in the FeMnNiCoCr HEA, the current work provides fundamental ideas on nanoscale segregation at crystal defects in multicomponent alloys. KW - Thermodynamics KW - High-Entropy Alloys KW - Grain Boundary Segregation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-508827 DO - https://doi.org/10.1103/PhysRevMaterials.4.053603 VL - 4 IS - 5 SP - 053603 PB - American Physical Society AN - OPUS4-50882 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lin, Y.-Y. A1 - Schleifer, F. A1 - Holzinger, M. A1 - Ta, N. A1 - Skrotzki, Birgit A1 - Darvishi Kamachali, Reza A1 - Glatzel, U. A1 - Fleck, M. T1 - Quantitative Shape-Classification of Misfitting Precipitates during Cubic to Tetragonal Transformations: Phase-Field Simulations and Experiments JF - Materials N2 - The effectiveness of the mechanism of precipitation strengthening in metallic alloys depends on the shapes of the precipitates. Two different material systems are considered: tetragonal γ′′ precipitates in Ni-based alloys and tetragonal θ′ precipitates in Al-Cu-alloys. The shape formation and evolution of the tetragonally misfitting precipitates was investigated by means of experiments and phase-field simulations. We employed the method of invariant moments for the consistent shape quantification of precipitates obtained from the simulation as well as those obtained from the experiment. Two well-defined shape-quantities are proposed: (i) a generalized measure for the particles aspect ratio and (ii) the normalized λ2, as a measure for shape deviations from an ideal ellipse of the given aspect ratio. Considering the size dependence of the aspect ratio of γ′′ precipitates, we find good agreement between the simulation results and the experiment. Further, the precipitates’ in-plane shape is defined as the central 2D cut through the 3D particle in a plane normal to the tetragonal c-axes of the precipitate. The experimentally observed in-plane shapes of γ′′-precipitates can be quantitatively reproduced by the phase-field model. KW - γ″ phase KW - Phase-field simulation KW - Misfitting precipitate KW - Nickel-base alloy KW - Al-Cu alloy KW - θ′ phase KW - Precipitate shape PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-522743 DO - https://doi.org/10.3390/ma14061373 VL - 14 IS - 6 SP - 1373 PB - MDPI AN - OPUS4-52274 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rockenhäuser, Christian A1 - Rowolt, C. A1 - Milkereit, B. A1 - Darvishi Kamachali, Reza A1 - Kessler, O. A1 - Skrotzki, Birgit T1 - On the long-term aging of S-phase in aluminum alloy 2618A JF - Journal of Materials Science N2 - The aluminum alloy 2618A is applied for engine components such as radial compressor wheels which operate for long time at elevated temperatures. This results in coarsening of the hardening precipitates and degradation in mechanical properties during the long-term operation, which is not taken into account in the current lifetime prediction models due to the lack of quantitative microstructural and mechanical data. To address this issue, a quantitative investigation on the evolution of precipitates during long-term aging at 190 °C for up to 25,000 h was conducted. Detailed transmission electron microscopy (TEM) was combined with Brinell hardness measurements and thorough differential scanning calorimetry (DSC) experiments. The results showthat GPB zones and S-phase Al2CuMg grow up to < 1,000 h during which the GPB zones dissolve and S-phase precipitates form. For longer aging times, only S-phase precipitates coarsen, which can be well described using the Lifshitz–Slyozov Wagner theory of ripening. A thorough understanding of the underlying microstructural processes is a prerequisite to enable the integration of aging behavior into the established lifetime models for components manufactured from alloy 2618A. KW - Long-term aging KW - Transmission electron microscopy (TEM) KW - Differential scanning calorimetry (DSC) KW - Microstructure KW - S-phase KW - Ostwald ripening PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519899 DO - https://doi.org/10.1007/s10853-020-05740-x SN - 0022-2461 VL - 56 IS - 14 SP - 8704 EP - 8716 PB - Springer Nature AN - OPUS4-51989 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -