TY - JOUR A1 - Zocca, Andrea A1 - Müller, Bernd R. A1 - Laquai, René A1 - Kupsch, Andreas A1 - Wieder, Frank A1 - Benemann, Sigrid A1 - Wilbig, Janka A1 - Günster, Jens A1 - Bruno, Giovanni T1 - Microstructural characterization of AP40 apatite-wollastonite glass-ceramic N2 - The microstructure of an apatite-wollastonite (code name AP40) glass-ceramic is analyzed in this study by combining 2D microscopy, phase analysis, X-ray absorption and synchrotron X-ray refraction computed tomography (XCT and SXRCT, respectively). It is shown that this combination provides a useful toolbox to characterize the global microstructure in a wide scale range, from sub-micrometer to millimeter. The material displays a complex microstructure comprising a glassy matrix with embedded fluorapatite and wollastonite small crystals. In this matrix, large (up to 200 μm) spike-shaped structures are distributed. Such microstructural features are oriented around a central sphere, thereby forming a structure resembling a sea urchin. A unique feature of SXRCT, in contrast to XCT, is that internal interfaces are visualized; this allows one to show the 3D distribution of these urchins with exceptionally good contrast. Furthermore, it is revealed that the spike-shaped structures are not single crystals, but rather composed of sub-micrometric crystals, which are identified as fluorapatite and diopside phases by SEM-EDX analysis. KW - Glass-ceramic KW - X-ray refraction KW - Computed tomography KW - Microstructure PY - 2023 DO - https://doi.org/10.1016/j.ceramint.2022.12.130 SN - 0272-8842 VL - 49 IS - 8 SP - 12672 EP - 12679 PB - Elsevier Science CY - Amsterdam AN - OPUS4-57452 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lanzino, Maria Carolina A1 - Le, Long-Quan R. V. A1 - Wilbig, Janka A1 - Rheinheimer, Wolfgang A1 - Seidenstuecker, Michael A1 - Günster, Jens A1 - Killinger, Andreas T1 - Thin GB14 coatings on implants using HVSFS N2 - Enhancing osseointegration, the process by which medical implants securely bond to bone, is crucial for improving patient outcomes in orthopedics and dental surgery. Calcium alkali orthophosphates, with their superior bioactivity, resorbability, and chemical resemblance to bone minerals, have emerged as promising candidates for implant coatings. These materials offer improved solubility and lower melting points due to the substitution of calcium with potassium and sodium, along with the addition of magnesium oxide. This study investigates GB14 calcium alkali orthophosphate coatings applied via High Velocity Suspension Flame Spraying (HVSFS), a technique that enables precise control over coating properties. A porosity target of >10% was set to promote bone growth, and we achieved porosities up to 13%, ensuring better cell penetration and stability at the implant-bone interface. Coatings were produced using different gas parameters and distances, with their microstructure and phase composition analyzed using scanning electron microscope (SEM), Vickers hardness testing and X-ray diffraction (XRD). Additionally, roughness and porosity were also assessed. Different coating’s microstructures were achieved by varying stand-off distance and gas parameters. Increasing stand-off distance while reducing gas stoichiometry enabled the production of calcium alkali orthophosphate coatings with fewer cracks, higher porosity and a hardness level comparable to that of state-of-the-art tricalcium phosphate (TCP) coatings. The sample with optimized properties in terms of achieved microstructure and topography was selected for in vitro testing using MG63 osteosarcoma cells to evaluate cell proliferation and adhesion. WST (I) assay, LDH assay, and live/dead staining confirmed the biocompatibility of the coatings, highlighting the potential of HVSFS to enhance osseointegration and outperform conventional methods in implantology. No relevant cytotoxicity could be shown and cells show a good proliferation over time. These results highlight thus the potential of HVSFS to produce thin, bioactive and resorbable coatings to enhance osseointegration. KW - Bio ceramics KW - Spray coating PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623983 DO - https://doi.org/10.3389/fmats.2024.1522447 SN - 2296-8016 VL - 11 IS - 1522447 SP - 1 EP - 14 PB - Frontiers Media SA AN - OPUS4-62398 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sänger, Johanna Christiane A1 - Schwentenwein, Martin A1 - Bermejo, Raúl A1 - Günster, Jens T1 - Hybridizing Lithography-Based Ceramic Additive Manufacturing with Two-Photon-Polymerization N2 - Stereolithography processes such as lithography-based ceramic manufacturing (LCM) are technologies that can produce centimeter-sized structures in a reasonable time frame. However, for some parts specifications, they lack resolution. Two-photon-polymerization (2PP) ensures the highest geometric accuracy in additive manufacturing so far. Nevertheless, building up parts in sizes as large as a few millimeters or even centimeters is a time-consuming process, which makes the production of 2PP printed parts very costly. Regarding feedstock specification, the requirements for 2PP are different to those for LCM, and generally, feedstocks are designed to meet requirements for only one of these manufacturing technologies. In an attempt to fabricate highly precise ceramic components of a rather large size, it is necessary to develop a feedstock that suits both light-based technologies, taking advantage of LCM’s higher productivity and 2PP’s accuracy. Hybridization should bring the desired precision to the region of interest on reasonably large parts without escalating printing time and costs. In this study, specimens gained from a transparent feedstock with yttria stabilized zirconia (YSZ) particles of 5 nm at 70 wt% were presented. The resin was originally designed to suit 2PP, while being also printable with LCM. This work demonstrates how hybrid parts can be sintered into full YSZ ceramics. KW - Additive Manufacturing KW - Transparent ceramic KW - Nano-powder PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-584541 DO - https://doi.org/10.3390/app13063974 SN - 2076-3417 VL - 13 IS - 6 SP - 1 EP - 9 PB - MDPI CY - Basel AN - OPUS4-58454 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sänger, Johanna C. A1 - Riechers, Birte A1 - Pauw, Brian Richard A1 - Maaß, Robert A1 - Günster, Jens T1 - Microplastic response of 2PP‐printed ceramics N2 - AbstractTwo‐photon polymerization (2PP) additive manufacturing (AM) utilizes feedstocks of ceramic nanoparticles of a few nanometers in diameter, enabling the fabrication of highly accurate technical ceramic design with structural details as small as 500 nm. The performance of these materials is expected to differ from conventional AM ceramics, as nanoparticles and three‐dimensional printing at high resolution introduce new microstructural aspects. This study applies 2PP‐AM of yttria‐stabilized zirconia to investigate the mechanical response behavior under compressive load, probing the influence of smallest structural units induced by the line packing during the printing process, design of sintered microblocks, and sintering temperature and thereby microstructure. We find a dissipative mechanical response enhanced by sintering at lower temperatures than conventional. The pursued 2PP‐AM approach yields a microstructured material with an increased number of grain boundaries that proposedly play a major role in facilitating energy dissipation within the here printed ceramic material. This microplastic response is further triggered by the filigree structures induced by hollow line packing at the order of the critical defect size of ceramics. Together, these unique aspects made accessible by the 2PP‐AM approach contribute to a heterogeneous nano‐ and microstructure, and hint toward opportunities for tailoring the mechanical response in future ceramic applications. KW - Manufacturing KW - Mechanical properties KW - Microstructure KW - Plasticity KW - Zirconia: yttria stabilized PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-605176 DO - https://doi.org/10.1111/jace.19849 SN - 1551-2916 VL - 107 IS - 10 SP - 6636 EP - 6645 PB - Wiley CY - Oxford AN - OPUS4-60517 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ginés-Palomares, Juan-Carlos A1 - Baasch, Julian A1 - Stapperfend, Simon A1 - Facchini, Leonardo A1 - Linke, Stefan A1 - Stoll, Enrico A1 - Günster, Jens T1 - Laser Melting vs. Laser Sintering: Large Area Heat Processing of Lunar South Pole Simulant N2 - A key component of future lunar missions is the concept of In-Situ Resource Utilization (ISRU), which involves the use of local resources to support human missions and reduce dependence on Earth-based supplies. This paper investigates the thermal processing capability of lunar regolith without the addition of binders, with a focus on large-scale applications for the construction of lunar habitats and infrastructure. The study used a simulant of lunar regolith found on the Schrödinger Basin in the South Pole region. This regolith simulant consists of 20 wt% basalt and 80 wt% anorthosite. Experiments were conducted using a high power CO2 laser to sinter and melt the regolith in a 80 mm diameter laser spot to evaluate the effectiveness of direct large area thermal processing. Results indicated that sintering begins at approximately 1,180 °C and reaches full melt at temperatures above 1,360 °C. Sintering experiments with this material revealed the formation of dense samples up to 11 mm thick, while melting experiments successfully produced larger samples by overlapping molten layers and additive manufacturing up to 50 mm thick. The energy efficiency of the sintering and melting processes was compared. The melting process was about 10 times more energy efficient than sintering in terms of material consolidation, demonstrating the promising potential of laser melting technologies of anorthosite-rich regolith for the production of structural elements. KW - Additive Manufacturing KW - Laser melting KW - ISRU KW - Moon KW - Regolith PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-639614 DO - https://doi.org/10.1016/j.amf.2025.200226 SN - 2950-4317 VL - 4 IS - 3 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-63961 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - You, Zengchao A1 - Hoffmann, V. A1 - Morcillo, Dalia A1 - Agudo Jácome, Leonardo A1 - Leonhardt, Robert A1 - Winckelmann, Alexander A1 - Richter, Silke A1 - Recknagel, Sebastian A1 - Abad Andrade, Carlos Enrique T1 - Investigation of aluminum current collector degradation in lithium-ion batteries using glow discharge optical emission spectrometry N2 - In this work, we employed glow discharge optical emission spectrometry (GD-OES) depth profiling as a fast and semi-quantitative method to investigate the aluminum (Al) current collector degradation in commercial lithium cobalt oxide (LCO) pouch cells with no Al2O3 pretreatment. After battery aging, a heterogeneous deposit was found on the surface of the cathode. Gray hotspot areas within an extensive pale white region were formed. Consistent with energy dispersive X-ray (EDX) analysis of micro-cross sections milled via targeted focused ion beam (FIB), an Al-containing layer of approximately 3 µm can be observed using GD-OES. We attribute one main cause of this layer is the degradation of the Al current collector. The nonuniform growth of this layer was investigated by performing GD-OES depth profiling at different in-plane positions. We found that the gray area has a higher mass concentration of Al, probably in metallic form, whereas the white area was probably covered more homogeneously with Al2O3, resulting from the inhomogeneous distribution of the pitting positions on the current collector. Compared to FIB-EDX, GD-OES enables a faster and more convenient depth profile analysis, which allows the more productive characterization of lithium-ion batteries (LIBs), and consequently benefits the development of preferable battery materials. KW - GD-OES KW - depth profiles KW - Li-ion battery KW - battery aging mechanism KW - current collector corrosion PY - 2023 DO - https://doi.org/10.1016/j.sab.2023.106681 SN - 0584-8547 VL - 205 SP - 106681 PB - Elsevier B.V. CY - Amsterdam, Netherlands AN - OPUS4-57383 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wang, Lei A1 - Darvishi Kamachali, Reza T1 - Incorporating elasticity into CALPHAD-informed density-based grain boundary phase diagrams reveals segregation transition in Al-Cu and Al-Cu-Mg alloys N2 - The phase-like behavior of grain boundaries (GBs), recently evidenced in several materials, is opening up new possibilities in the design of alloy microstructures. In this context, GB phase diagrams are contributing to a predictive description of GB segregation and (interfacial) phase changes. The influence of chemo-mechanical solute-GB interactions on the GB phase diagram remains elusive so far. This is particularly important for multi-component alloys where the elastic interactions among solute atoms, of various sizes and bonding energies, can prevail, governing a complex co-segregation phenomenon. Recently, we developed a density-based model for GB thermodynamics that intrinsically accounts for GB elasticity in pure elements. In this work, we incorporate the homogeneous and heterogeneous elastic energies associated with the solutes into the density-based framework. We derive the multi-component homogeneous elastic energy by generalizing the continuum misfitting sphere model and extend it for GBs. The density-based free energy functional directly uses bulk CALPHAD thermodynamic data. The model is applied to binary and ternary Al alloys. We reveal that the elastic energy can profoundly affect the GB solubility and segregation behavior, leading to Cu segregation in otherwise Cu-depleted Al GBs. Consequently, GB segregation transition, i.e., a jump in the GB segregation as a function of alloy composition, is revealed in Al-Cu and Al-Cu-Mg alloy systems with implications for subsequent GB precipitation in these alloys. CALPHAD-informed elasticity-incorporated GB phase diagrams enable addressing a broader range of GB phenomena in engineering multi-component alloys. KW - Grain boundary thermodynamics KW - Density-based model KW - Al alloys KW - Grain boundary phase diagram KW - CALPHAD KW - Elastic energy PY - 2021 DO - https://doi.org/10.1016/j.commatsci.2021.110717 VL - 199 SP - 110717 PB - Elsevier B.V. AN - OPUS4-53058 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stephan-Scherb, Christiane A1 - Lehmusto, Juho A1 - Falk, Florian A1 - Sobol, Oded A1 - Pint, Bruce T1 - Comprehensive insights into competitive oxidation/sulfidation reactions on binary ferritic alloys at high temperatures N2 - Interpreting high-temperature corrosion induced by mixed-gas atmospheres is challenging due to the different contributions of oxidizing gases. Here, a comprehensive study on the combined oxidation/sulfidation using label molecules is presented. Fe-Cr model alloys with 2 wt% and 9 wt% Cr were isothermally exposed using a volumetric mixture of 0.5%S16O2/27%H218O and 0.5%S16O2/7%H218O at 650 ◦C for 5 h and then characterized by secondary ion mass spectroscopy (SIMS). Additionally, the reactions were followed in-situ utilizing energy dispersive X-ray diffraction. The study showed that both S16O2 and H218O contribute to the oxidation of the alloys but to different extents depending on the Cr-content. KW - SEM KW - Steel KW - Iron KW - SIMS PY - 2022 DO - https://doi.org/10.1016/j.corsci.2022.110236 SN - 0010-938X VL - 203 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-58992 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Darvishi Kamachali, Reza T1 - A model for grain boundary thermodynamics N2 - Systematic microstructure design requires reliable thermodynamic descriptions of each and all microstructure elements. While such descriptions are well established for most bulk phases, thermodynamic assessment of microstructure defects is challenging because of their individualistic nature. In this paper, a model is devised for assessing grain boundary thermodynamics based on available bulk thermodynamic data. We propose a continuous relative atomic density field and its spatial gradients to describe the grain boundary region with reference to the homogeneous bulk and derive the grain boundary Gibbs free energy functional. The grain boundary segregation isotherm and phase diagram are computed for a regular binary solid solution, and qualitatively benchmarked for the Pt–Au system. The relationships between the grain boundary's atomic density, excess free volume, and misorientation angle are discussed. Combining the current density-based model with available bulk thermodynamic databases enables constructing databases, phase diagrams, and segregation isotherms for grain boundaries, opening possibilities for studying and designing heterogeneous microstructures. KW - Phase Diagram KW - Thermodynamics KW - Grain boundary PY - 2020 VL - 10 IS - 45 SP - 26728 EP - 26741 AN - OPUS4-51268 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jacobson, David A1 - Darvishi Kamachali, Reza A1 - Thompson, Gregory T1 - Coupling density phase field models with atomistic potentials N2 - A density-based phase field model is developed where the free energy functional is explicitly linked with molecular dynamics and is referred to as the Molecular Phase Field Method (MoPF). MoPF simulations involve expressing interatomic potentials in terms of density to form a density based free energy functional. Inputs to this functional are taken from atomistics such that the phase field density profile matches the corresponding density profile from atomistic simulations. We analyze our results by comparing the MoPF calculated excess interfacial energies with excess interfacial energies calculated using molecular dynamics associated with several nickel grain boundaries. Additionally, a comparison is made between our results and the interfacial energies of a \Sigma7 boundary across a variety of FCC systems simulated using density functional theory. The MoPF method is able to successfully predict grain boundary free energy trends between grain boundary and material types offering an atomistically informed mesoscale formulation for studying grain boundary physics. KW - Density-based Phase-Field Modelling KW - Atomistic Simulation KW - Grain Boundary PY - 2024 DO - https://doi.org/10.1016/j.commatsci.2023.112763 VL - 233 SP - 1 EP - 6 PB - Elsevier AN - OPUS4-59360 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -