TY - JOUR A1 - Riechers, Birte A1 - Das, Amlan A1 - Rashidi, Reza A1 - Dufresne, Eric A1 - Maaß, Robert T1 - Metallic glasses: Elastically stiff yet flowing at any stress N2 - Crystalline solids have a minimum stress needed to displace atoms or to move defects. This stress defines the true elastic limit and is generally a sizeable share of the macroscopic yield stress. Here we demonstrate that a metallic glass, an amorphous solid with a yield stress in the giga-pascal regime, lacks such a true microscopic elastic limit. Leveraging in-situ coherent x-ray scattering, we uncover a strongly accelerated atomic-scale transport upon the application of a stress as small as 0.005 times the yield stress. With increasing stress levels, the distribution of structural relaxation times changes from compressed exponential to simple exponential form, revealing a stress–temperature equivalence in the time-scale domain. These findings strongly promote a microstructurally heterogeneous picture of metallic glasses, in which a part of the amorphous microstructure controls macroscopic yielding whereas another part admits microplastic flow at any stress. KW - Metallic glasses KW - Microstructure PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624530 DO - https://doi.org/10.1016/j.mattod.2024.11.015 VL - 82 SP - 92 EP - 98 PB - Elsevier B.V. AN - OPUS4-62453 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fareed, Adnan A1 - Rosalie, Julian A1 - Kar, Satyakam A1 - Fähler, Sebastian A1 - Maaß, Robert T1 - Small-scale functional fatigue of a Ni-Mn-Ga Heusler alloy N2 - Functional fatigue of shape-memory alloys is a considerable threat to the reliable service of actuation devices. Here, we demonstrate the essentially degradation-free cyclic phase-transformation behavior of Ni-Mn-Ga microcrystals up to one million stress-driven superelastic cycles. Cyclic dissipation amounts to about 1/5 of the bulk counterpart and remains unaffected during cycling, even after the introduction of dislocation structures via plastic straining. Plastic yielding and the transformation stress largely exceed the known bulk values. However, the transformation-stress is found to depend on plastic pre-straining, which suggests that the size-affected transformation stress is sensitive to the initial defect structure and that it can be tuned by a targeted introduction of dislocations. These findings demonstrate the high suitability of Ni-Mn-Ga as a robust shape-memory alloy in small-scale functional device engineering. KW - Superelasticity KW - Shape-memory alloys KW - Functional fatigue KW - Ni-Mn-Ga PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600695 DO - https://doi.org/10.1016/j.actamat.2024.119988 VL - 274 SP - 1 EP - 10 PB - Elsevier B.V. AN - OPUS4-60069 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Riechers, Birte A1 - Das, Amlan A1 - Dufresne, Eric A1 - Derlet, Peter M. A1 - Maaß, Robert T1 - Intermittent cluster dynamics and temporal fractional diffusion in a bulk metallic glass N2 - Glassy solids evolve towards lower-energy structural states by physical aging. This can be characterized by structural relaxation times, the assessment of which is essential for understanding the glass’ time-dependent property changes. Conducted over short times, a continuous increase of relaxation times with time is seen, suggesting a time-dependent dissipative transport mechanism. By focusing on micro-structural rearrangements at the atomic-scale, we demonstrate the emergence of sub-diffusive anomalous transport and therefore temporal fractional diffusion in a metallic glass, which we track via coherent x-ray scattering conducted over more than 300,000 s. At the longest probed decorrelation times, a transition from classical stretched exponential to a power-law behavior occurs, which in concert with atomistic simulations reveals collective and intermittent atomic motion. Our observations give a physical basis for classical stretched exponential relaxation behavior, uncover a new power-law governed collective transport regime for metallic glasses at long and practically relevant time-scales, and demonstrate a rich and highly non-monotonous aging response in a glassy solid, thereby challenging the common framework of homogeneous aging and atomic scale diffusion. KW - Glassy solids KW - Fractional diffusion KW - Coherent x-ray scattering PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608015 DO - https://doi.org/10.1038/s41467-024-50758-3 VL - 15 IS - 1 SP - 1 EP - 9 PB - Springer Science and Business Media LLC AN - OPUS4-60801 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fareed, Adnan A1 - Rosalie, Julian A1 - Kumar, Sourabh A1 - Kar, S. A1 - Hickel, Tilmann A1 - Fähler, S. A1 - Maaß, Robert T1 - Constrained incipient phase transformation in Ni-Mn-Ga films: A small-scale design challenge N2 - Ni-Mn-Ga shape-memory alloys are promising candidates for large strain actuation and magnetocaloric cooling devices. In view of potential small-scale applications, we probe here nanomechanically the stress-induced austenite–martensite transition in single crystalline austenitic thin films as a function of temperature. In 0.5 μm thin films, a marked incipient phase transformation to martensite is observed during nanoindentation, leaving behind pockets of residual martensite after unloading. These nanomechanical instabilities occur irrespective of deformation rate and temperature, are Weibull distributed, and reveal large spatial variations in transformation stress. In contrast, at a larger film thickness of 2 μm fully reversible transformations occur, and mechanical loading remains entirely smooth. Ab-initio simulations demonstrate how an in-plane constraint can considerably increase the martensitic transformation stress, explaining the thickness-dependent nanomechanical behavior. These findings for a shape-memory Heusler alloy give insights into how reduced dimensions and constraints can lead to unexpectedly large transformation stresses that need to be considered in small-scale actuation design. KW - Shape-memory alloys KW - Nanoindentation KW - Incipient plasticity KW - NiMaGa PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581422 DO - https://doi.org/10.1016/j.matdes.2023.112259 VL - 233 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-58142 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wang, Zengquan A1 - Riechers, Birte A1 - Derlet, Peter M. A1 - Maaß, Robert T1 - Atomic cluster dynamics causes intermittent aging of metallic glasses N2 - In the past two decades, numerous relaxation or physical aging experiments of metallic glasses have revealed signatures of intermittent atomic-scale processes. Revealed via intensity cross-correlations from coherent scattering using X-ray photon correlation spectroscopy (XPCS), the observed abrupt changes in the time-domain of atomic motion does not fit the picture of gradual slowing down of relaxation times and their origin continues to remain unclear. Using a binary Lennard-Jones model glass subjected to microsecond-long isotherms, we show here that temporally and spatially heterogeneous atomic-cluster activity at different length-scales drive the emergence of highly non-monotonous intensity cross-correlations. The simulated XPCS experiments reveal a variety of time-dependent intensity-cross correlations that, depending on both the structural evolution and the 𝑞-space sampling, give detailed insights into the possible structural origins of intermittent aging measured with XPCS. KW - Metallic glasses KW - Aging KW - Molecular dynamics KW - XPCS PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595415 DO - https://doi.org/10.1016/j.actamat.2024.119730 SN - 1359-6454 VL - 267 SP - 1 EP - 9 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-59541 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fantin, Andrea A1 - Manzoni, Anna Maria A1 - Springer, H. A1 - Darvishi Kamachali, Reza A1 - Maaß, Robert T1 - Local lattice distortions and chemical short-range order in MoNbTaW N2 - Extended X-ray absorption fine structure (EXAFS) conducted on an equiatomic MoNbTaW bcc medium-entropy alloy that was annealed at 2273 K reveals unexpectedly small 1st and 2nd shell element-specific lattice distortions. An experimental size-mismatch parameter, δexp, is determined to be ca. 50% lower than the corresponding calculated value. Around W, short-range order (SRO) preferring 4d elements in the 1st and 2nd shells persists. A Nb-W ordering is found, which is reminiscent of ordering emerging at lower temperatures in the B2(Mo,W;Ta,Nb)- and B32(Nb,W)-phases. With high-temperature ordering preferences in fcc also foreshadowing low-temperature phase, these findings suggest a general feature of high-temperature SRO. KW - High Entropy Alloys KW - Short-range order KW - Lattice distortions KW - EXAFS PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-598164 DO - https://doi.org/10.1080/21663831.2024.2326014 SN - 2166-3831 VL - 12 IS - 5 SP - 346 EP - 354 PB - Taylor & Francis AN - OPUS4-59816 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rashidi, Reza A1 - Riechers, Birte A1 - Rosalie, Julian A1 - Maaß, Robert T1 - Annealing-dependent elastic microstructure in a Zr-based metallic glass N2 - In this letter, we demonstrate the robust presence of an elastic microstructure in a Zr-based metallic glass (MG) with a characteristic length-scale of the order of 100 nm. This length scale increases systematically towards the MG surface in differently sized casts, whereas thermal relaxation homogenizes both the internal length-scale gradient and the magnitude of the elastic fluctuations. Strongest changes during relaxation arise in the stiffest parts of the elastic microstructure. These findings indicate that the elastic microstructure emerges due to cooling constraints and may therefore be a microstructural manifestation of the internal residual stresses that arise during MG-solidification. KW - Metallic glass KW - Heterogeneity KW - Elastic microstructure KW - Nanoindentation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-610962 DO - https://doi.org/10.1016/j.scriptamat.2024.116380 VL - 255 SP - 1 EP - 5 PB - Elsevier B.V. CY - Amsterdam, Niederlande AN - OPUS4-61096 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hoffmann, M. A1 - Schubert, Nils A1 - Günster, Jens A1 - Stawarczyk, B. A1 - Zocca, Andrea T1 - Additive manufacturing of glass-ceramic dental restorations by layerwise slurry deposition (LSD-print) N2 - This study is dedicated to the additive manufacturing of a feldspar glass-ceramic for dental applications by LSD-print (layerwise slurry deposition) technology, a variation of binder jetting using water-based ceramic slurries as feedstock. This technology was investigated for the manufacturing of single tooth restoration demonstrators with good aesthetic properties, and to compare the additively manufactured material with a commercial reference. Model restorations with > 99 % relative density were processed with a debinding and firing cycle of 45 min, however the whole process chain accounts for up to 30 hours. Significant differences between LSD-printed and reference materials were found for fracture strength, fracture toughness and Martens parameters. Printing orientation affected shrinkage and fracture strength, but not fracture toughness and Martens parameters. Nevertheless, the results suggest that the LSD-print technology processing the developed slurry is a promising option for manufacturing dental restorations meeting class 1a requirements according to DIN EN ISO 6871:2019–01. KW - Additive Manufacturing KW - 3D-printing KW - LSD-print KW - Dental ceramics KW - Glass-ceramic KW - Debinding KW - Firing KW - Sinter-crystallization PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624768 DO - https://doi.org/10.1016/j.jeurceramsoc.2025.117235 VL - 45 IS - 7 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-62476 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Karl, D. A1 - Duminy, T. A1 - Lima, P. A1 - Kamutzki, F. A1 - Gili, A. A1 - Zocca, Andrea A1 - Günster, Jens A1 - Gurlo, A. T1 - Clay in situ resource utilization with Mars global simulant slurries for additive manufacturing and traditional shaping of unfired green bodies N2 - The wet processing of regolith simulant for clay in situ resource utilization (ISRU) on Mars is presented. The two raw materials from the Mars global simulant family, one without clay (MGS-1) and one with clay - sodium montmorillonite smectite - (MGS-1C) were milled and mixed to produce a simulant with small particle size and reduced clay content (MGS-1C/8). All three simulants and the pure clay raw material were extensively characterized using XRF, synchrotron XRD, gas adsorption and gas pycnometry methods. In a straightforward processing approach, MGS-1C/8 was mixed with water and different dispersant approaches were investigated, all of which gave stable slurries. Particle size distribution, rheology, ion concentration, pH and electrical conductivity of these slurries were characterized. The slurry systems can easily be adapted to fit all typical ceramic shaping routes and here parts of varying complexity from slip casting, throwing on a potter's wheel and additive manufacturing, including material extrusion (robocasting) and binder jetting (powder bed 3D printing) were produced. The unique properties of the sodium montmorillonite clay, which is readily accessible in conjunction with magnesium sulfate on the Martian surface, acted as a natural nanosized binder and produced high strength green bodies (unfired ceramic body) with compressive strength from 3.3 to 7.5 MPa. The most elaborate additive manufacturing technique layerwise slurry deposition (LSD) produced water-resistant green bodies with a compressive strength of 30.8 ± 2.5 MPa by employing a polymeric binder, which is similar or higher than the strength of standard concrete. The unfired green bodies show sufficient strength to be used for remote Habitat building on Mars using additive manufacturing without humans being present. KW - Mars KW - Smectite KW - Clay ISRU KW - MGS-1 regolith simulant KW - 3D printing KW - Additive manufacturing PY - 2020 DO - https://doi.org/10.1016/j.actaastro.2020.04.064 VL - 174 SP - 241 EP - 253 PB - Elsevier Ltd. AN - OPUS4-50870 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baesso, Ilaria A1 - Karl, D. A1 - Spitzer, Andrea A1 - Gurlo, A. A1 - Günster, Jens A1 - Zocca, Andrea T1 - Characterization of powder flow behavior for additive manufacturing N2 - The flow behavior of powders has an essential role in many industrial processes, including powder bed additive manufacturing. The characterization of the flow behavior is challenging, as different methods are available, and their suitability for an application in additive manufacturing is still controversial. In this study, six standardized methods (measurement of bulk density by ISO 60 and by ASTM B329, angle of repose by ISO 4324, discharge time by ISO 6186 and by ASTM B964-16, and Hausner Ratio by ASTM 7481 – 18), the rotating drum method (by GranuDrum) and powder rheometry (Anton Paar powder cell), were applied to five size fractions of a crushed quartz sand powder and compared. A statistical approach is proposed and discussed to correlate the obtained flowability indexes with the packing density of powder beds deposited layer-by-layer, and these correlations are compared between methods. Overall, the measurement of bulk density by ASTM B329 that showed the best correlation with the powder bed density. Advanced methods such as the rotating drum method and powder rheometry did not demonstrate particularly good correlations, however they provided complementary information which can be useful to assess the dynamic behavior of powders. KW - Powder flow KW - Flowability KW - Powder bed additive manufacturing KW - Powder rheology PY - 2021 DO - https://doi.org/10.1016/j.addma.2021.102250 SN - 2214-8604 VL - 47 SP - 1 EP - 14 PB - Elsevier CY - Amsterdam AN - OPUS4-53229 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -