TY - CONF A1 - Rütters, H A1 - Fischer, S A1 - Le, Quynh Hoa A1 - Bettge, Dirk A1 - Bäßler, Ralph A1 - Maßmann, J A1 - Ostertag-Henning, C A1 - Lennard Wolf, J A1 - Pumpa, M A1 - Lubenau, U A1 - Knauer, S A1 - Jaeger, P A1 - Neumann, A A1 - Svensson, K A1 - Pöllmann, H A1 - Lempp, C A1 - Menezes, F A1 - Hagemann, B T1 - Towards Defining Reasonable Minimum Composition Thresholds – Impacts of Variable CO2 Stream Compositions on Transport, Injection and Storage N2 - The collaborative project “Impacts of impurities in CO2 streams captured from different emitters in a regional cluster on transport, injection and storage (CLUSTER)” aimed to set up recommendations on how to define “reasonable minimum composition thresholds” that CO2 streams should meet when accessing CO2 transport pipeline networks. Within CLUSTER, we investigated potential impacts of CO2 streams with different and temporally variable compositions and mass flow rates along the whole CCS chain. Investigations included, amongst others, impacts on: • corrosion of pipeline steel, • pipeline network design and related transport costs, • alteration of well bore cements, • pressure development and rock integrity, • geochemical reactions, and • petrophysical and geomechanical rock properties. All investigations are based on a generic CCS chain scenario. In this scenario, CO2 streams are captured from a spatial cluster of eleven emitters and collected in a regional pipeline network. Emitters comprise seven fossil fuel-fired power plants equipped with different capture technologies, two cement plants, one refinery and one integrated iron and steel plant. In total, 19.78 Mio t CO2 (including impurities) are captured in the emitter cluster annually. The combined CO2 stream is transported in a trunk line with a length of 400 km (100 km of these offshore) and is injected into five generic storage structures. The storage reservoirs are saline aquifers of the Buntsandstein. The investigations revealed beneficial and deteriorating impacts of different impurities and combinations thereof. Overall, no fundamental technical obstacles for transporting, injecting and storing CO2 streams of the modelled variable compositions and mass flow rates were observed. Based on the results, the CLUSTER project team recommends not to define “minimum composition thresholds” for CO2 streams as strict threshold values for each individual impurity in the stream. Instead, CO2 stream compositions and variabilities for specific CCS projects should be constrained with regard to a set of parameters including i) the overall CO2 content, ii) maximum contents of relevant impurities or elements, iii) acceptable variability of CO2 stream composition, and iv) impurity combinations to be avoided. T2 - The 15th Greenhouse Gas Control Technologies Conference CY - Online meeting DA - 15.03.2021 KW - Corrosion KW - Impurities KW - CO2 quality KW - Pipeline network KW - Whole-chain CCS scenario KW - Recommendations PY - 2021 U6 - https://doi.org/10.2139/ssrn.3816427 SP - 1 EP - 18 PB - Elservier AN - OPUS4-52940 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Knauer, S A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Jaeger, P T1 - Contact angle and corrosion of a Water – CO2 system on X70 and S41500 at 278 K and pressures up to 20 MPa N2 - Interfacial properties related to wettability and corrosion in CO2 transport pipelines are experimentally determined by the sessile and the pendant drop methods. The contact angle of a water drop in a compressed CO2 atmosphere is analyzed on an X70 pipeline carbon steel and compared to that on a martensitic steel S41500 to elucidate the effect of corrosion process on active wetting behaviour. The measurements are performed with liquid CO2 at 278 K and pressures ranging from 5 to 20 MPa. The results show that the contact angle (CA) increases with pressure from 132 ° to 143 ° for S41500 and from 117 ° to 137 ° for X70 and decreases with drop age by 20 ° to 24 ° regardless of the pressure and of the fact that corrosion only occurs on X70, which is confirmed by scanning electron microscopy, element mapping and energy dispersive x-ray spectrometry (EDS) analysis. At higher pressure, the contact angles on both materials converge. Further, related properties like density and interfacial tension were determined. CO2 - saturated water has a higher density than pure water: At 5 MPa saturated water reaches a density of 1017 kg⋅m^(-3) and at 20 MPa 1026 kg⋅m^(-3) compared to pure water with a density of 1002 kg⋅m^(-3) and 1009 kg⋅m^(-3), respectively. In this pressure range the IFT drops from 33 mN⋅m^(-1)at 5 MPa to 23 mN⋅m^(-1) at 20 MPa. KW - Carbon capture KW - Utilization, and storage (CCUS) technology KW - Contact angle KW - Wetting KW - Corrosion KW - Condensate KW - Impurities KW - Carbon steel PY - 2019 UR - https://www.sciencedirect.com/science/article/pii/S1750583618309472?dgcid=author U6 - https://doi.org/10.1016/j.ijggc.2019.06.021 SN - 1750-5836 SN - 1878-0148 VL - 89 SP - 33 EP - 39 PB - Elsevier, ScienceDirect AN - OPUS4-48601 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Knauer, S A1 - Jaeger, P A1 - Kratzig, Andreas A1 - Bettge, Dirk A1 - Kranzmann, Axel T1 - Droplet corrosion of CO2 transport pipeline steels in simulated oxyfuel flue gas N2 - The research focus of this study was set on the corrosion process of condensate as droplets on the surface of carbon steels (X52, X70) martensitic steel UNS S41500, and super austenite UNS N08031 in CO2 atmosphere with impurities at 278 K (to simulate the offshore transportation condition in a buried pipeline). The possibility of dew/droplet formation on the steel surface and wetting behavior of corresponding materials were evaluated by contact angle measurement in dense CO2 at 278 K. To observe the effect of impurities (SO2 and O2) on droplet corrosion process, exposure tests were carried out in the mixed atmosphere with a drop, 1 ‑ 10 µL in volume, of CO2 saturated ultra-pure water on steel surface. Comparable exposure tests were carried out with the same gas mixture and the same volume of water, as vapor, to observe the droplet formation and the corrosion process that follows. Effects of surface roughness on the droplet formation and its corrosion process were further studied and showed no significant role upon long time exposure. The results from droplet experiments were compared to those from the bulk electrolyte for the further recommendation on the quality control of gas stream along with the use of carbon steels as transport pipelines in CCS - Carbon Capture and Storage system. KW - CCUS, supercritical/dense phase CO2, carbon steels, martensitic steel, superaustenite steel, droplet corrosion PY - 2018 UR - http://corrosionjournal.com/doi/abs/10.5006/2927 U6 - https://doi.org/10.5006/2927 SN - 0010-9312 SN - 1938-159X VL - 74 IS - 12 SP - 1406 EP - 1420 PB - NACE International CY - Houston, Texas, USA AN - OPUS4-46903 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -