TY - JOUR A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Bender, R. A1 - Féron, D. A1 - Mills, D. A1 - Ritter, S. A1 - de Graeve, I. A1 - Dugstad, A. A1 - Grassini, S. A1 - Hack, T. A1 - Halama, M. A1 - Han, E.-H. A1 - Harder, T. A1 - Hinds, G. A1 - Kittel, J. A1 - Krieg, R. A1 - Leygraf, C. A1 - Martinelli, L. A1 - Mol, A. A1 - Neff, D. A1 - Nilsson, J.-O. A1 - Odnevall, I. A1 - Paterson, S. A1 - Paul, S. A1 - Prosek, T. A1 - Raupach, M. A1 - Revilla, R. I. A1 - Ropital, F. A1 - Schweigart, H. A1 - Szala, E. A1 - Therryn, H. A1 - Tidblad, J. A1 - Virtanen, S. A1 - Volovitch, P. A1 - Watkinson, D. A1 - Wilms, M. A1 - Winning, G. A1 - Zheludkevich, M. T1 - La corrosion: un défi pour une société durable N2 - Une transition mondiale vers des systèmes énergétiques plus durables, abordables et fiables a été initiée par l’accord de Paris et l’Agenda 2030 des Nations unies pour un développement durable. Il s’agit là d’un défi industriel majeur car les systèmes et infrastructures énergétiques résilients au changement climatique exigent de se positionner pour le long terme. Se pencher sur le comportement dans la durée des matériaux structurels - principalement des métaux et des alliages - s’impose alors comme une nécessité. Dans cette optique, « La corrosion : un défi pour une société durable »présente une série de cas montrant l’importance de la tenue à la corrosion et de la protection anticorrosion des métaux et des alliages pour le développement de systèmes durables, économiques et fiables de production d’énergie. KW - Corrosion KW - Coûts de la corrosion KW - Protection KW - Anticorrosion KW - Stratégies deprévention PY - 2023 DO - https://doi.org/10.51257/a-v1-cor2000 SN - 2555-5383 VL - 2023 IS - Avril SP - 1 EP - 23 CY - Saint-Denis, France AN - OPUS4-57927 LA - fra AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Le, Quynh Hoa A1 - Kratzig, Andreas A1 - Bettge, Dirk A1 - Knauer, S. T1 - Factors Influencing Droplet Corrosion in Dense Phase CO2 N2 - This work examined the factors that influence the droplet corrosion of CO2 pipeline steels caused by oxyfuel flue gases in dense phase CO2 at 278 K, simulating the underground transport conditions. The wetting properties were studied by contact angle measurement, revealing pH and time dependency on the reactive wetting behaviors of carbon steel X70. Exposure tests with CO2 saturated water droplet on steel surface showed that the impurities (220 ppmv SO2 and 6700 ppmv O2) diffused into the droplet and then reacted with metal surfaces in dense phase condition, forming the corrosion products. The corrosion rate was confirmed strongly depending on the droplet volume as well as the SO2 concentration. Condensation experiments carried out on freshly polished coupons in CO2 with 200 ppmv H2O, 220 ppmv SO2 and 6700 ppmv O2, showed that the formation and aggregation of droplets is time and temperature dependent. At 278 K, condensation happened stronger and the corrosion products, mainly consisted of dense hydrated FeSO3/FeSO4. While at 288 K, more fluffy corrosion products consisting of iron oxide/hydroxide and hydrated FeSO3/FeSO4 were found. Further exposure tests on carbon steel coupons with different surface roughness did not reveal the difference in weight loss/gain and therefore the corrosion rate. T2 - NACE International Corrosion Conference 2019 CY - Nashville, TN, USA DA - 24.03.2019 KW - Carbon Capture, Utilization and Storage (CCUS) KW - Supercritical/dense phase CO2 KW - Carbon steel KW - Droplet corrosion KW - Condensation PY - 2019 AN - OPUS4-47916 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Aristia, Gabriela A1 - Le, Quynh Hoa T1 - Study of Polyaniline/Silicon Dioxide based Coating on Carbon Steel in Artificial Geothermal Brine N2 - By using the available resources in Indonesia, such as silicon dioxide and marine coating base, the PANI/SiO2 modified alkyd coating was able to protect carbon steel in a deaerated artificial geothermal water. The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure. Electrochemical tests indicated that there was no significant change in the Ecorr between the coated and uncoated carbon steel at room temperature. At 150 °C, the coated carbon steel has a lower potential than that of carbon steel, indicating that the coating is protecting carbon steel cathodically or slowing down the corrosion reaction. Finally, a long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water up to 150 °C for 6 months. T2 - World Geothermal Congress CY - Online meeting DA - 15.06.2021 KW - Coatings KW - Corrosion KW - Polyaniline KW - Sibayak KW - SiO2 KW - Geothermal PY - 2021 AN - OPUS4-52831 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Yevtushenko, Oleksandra A1 - Le, Quynh Hoa A1 - Bettge, Dirk T1 - Corrosion Effects on Materials Considered for CC(U)S Applications N2 - Commercially available carbon steels are suitable for compression and pipelines as long as moisture content and impurities are limited. (water 50 to 100 ppmv, SO2 and NO2 ca. 100 ppmv) Corrosion rates increase with increasing water content. (0.2 – 20 mm/a) Condensation of acids and therefore droplet formation is always possible, even at low water contents. A low SO2 content within the CO2-stream might be more important than a low water content. Cr13-steels showed a general susceptibility to shallow pitting and pitting. So, they seem to be not suitable for CCUS applications. Low alloyed steels showed better corrosion behavior (predictable uniform corrosion). For direct contact with saline aquifer fluids only high alloyed steels shall be used. T2 - EFC Webinar CY - Online Meeting (Chongqing, China) DA - 18.05.2022 KW - Corrosion KW - CO2 quality KW - CO2 KW - CCS KW - CCU KW - Pipeline PY - 2022 AN - OPUS4-54854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Yevtushenko, Oleksandra A1 - Le, Quynh Hoa A1 - Bettge, Dirk T1 - Suitability of Metallic Materials in CC(U)S Applications N2 - Commercially available carbon steels are suitable for compression and pipelines as long as moisture content and impurities are limited. (water 50 to 100 ppmv, SO2 and NO2 ca. 100 ppmv). Corrosion rates increase with increasing water content. (0.2 – 20 mm/a). Condensation of acids and therefore droplet formation is always possible, even at low water contents. A low SO2 content within the CO2-stream might be more important than a low water content. Cr13-steels showed a general susceptibility to shallow pitting and pitting. So, they seem to be not suitable for CCUS applications. Low alloyed steels showed better corrosion behavior. � (predictable uniform corrosion) For direct contact with saline aquifer fluids only high alloyed steels shall be used. T2 - EUROCORR 2021 CY - Budapest, Hungary DA - 20.09.2021 KW - Carbon capture storage KW - Corrosion KW - Steel KW - CCS KW - CCU KW - CO2 PY - 2021 AN - OPUS4-53461 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Le, Quynh Hoa A1 - Yevtushenko, Oleksandra A1 - Bettge, Dirk T1 - Corrosion Aspects for Materials to be Used in CC(U)S Applications N2 - This contribution provides current findings regarding materials susceptibility for carbon capture, utilization and storage (CCUS) applications. Basing on results gathered in 2 German long-term projects (COORAL and CLUSTER) suitable materials are introduced as well as dominating impurities of the CO2-stream and corrosion mechanisms. Investigations cover the whole CCUS process chain and provide material recommendations for certain parts. T2 - 1st International Conference on Corrosion Protection and Application CY - Chongqing, China DA - 09.09.2019 KW - Carbon KW - Capture KW - Storage KW - Utilization KW - CCS KW - CCU KW - CO2 KW - Corrosion PY - 2019 AN - OPUS4-49302 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph A1 - Le, Quynh Hoa A1 - Bettge, Dirk T1 - Electrochemical behaviors of casing steel/mortar interface in CO2 saturated aquifer fluid N2 - To reveal the corrosion resistance of casing steel/mortar interface in CO2 injection condition, sandwich samples were prepared and exposed up to 20 weeks in aquifer fluid under 10 MPa and 60 °C. Cross section analysis revealed the crevice corrosion as main mechanism instead of pitting corrosion despite very high concentration of Cl in NGB. EDS element line scan analysis of the 20-week-exposed metal/mortar coupon showed Chloride distribution, which still not reached the metal/mortar interface, explaining no pitting was observed. It was confirmed that FeCO3 cannot protect the steel surface in CO2 saturated NGB. To verify the protective possibility of passivation happened on casing steel/mortar interface, simulated pore solution was synthesized and used to passivate the steel for 42 days. OCP and EIS confirmed the formation of passive layer. The 42 day passivated layer was broken during the first minute of exposure in CO2 saturated NGB. However, due to high concentration of Ca2+, a new carbonate CaCO3 dense layer was formed, increased the corrosion resistance of steel surface. T2 - EUROCORR 2022 CY - Berlin, Germany DA - 28.08.2022 KW - Corrosion KW - Geothermal KW - CO2 KW - Mortar PY - 2022 AN - OPUS4-55621 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -