TY - CONF A1 - Bandow, Nicole A1 - Kalbe, Ute A1 - Schoknecht, Ute T1 - Leaching of brominated flame retardants - eluate analysis using XRF N2 - Brominated flame retardants have widely been used for more than 50 years and have been frequently detected in environmental samples as surface water and fish. Leaching from construction products was identified as one possible source. The use of substances as e.g. hexabromocyclododecane (HBCCD) was restricted recently due to increasing concern about negative impacts on the environment and human health caused by the persistent, bio accumulative and toxic properties. New polymeric brominated flame retardants have been developed to replace HBCCD in expanded polystyrene (XPS), which is used for insulation of buildings. It is assumed that the release from the polymer is much smaller in comparison to release of small molecules as HBCCD. The release from the polymer may include monomers or small fragments of different size. Thus, a sum parameter is needed. According to Schlummer et al. it is possible to detect brominated molecules using X-ray fluorescence spectroscopy by determination of brome content in XPS extracts. As only small brominated compounds can be extracted it also allows for the differentiation between the two classes of compounds. This method was applied to verify the presence of different kinds of flame retardants in XPS samples and to evaluate the leaching behavior. T2 - ESAS CANAS CY - Berlin, Germany DA - 21.03.2018 KW - Leaching KW - XPS KW - Flame-retardant KW - XRF PY - 2018 AN - OPUS4-44562 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Simon, Franz-Georg A1 - Kalbe, Ute A1 - Bandow, Nicole T1 - Potential use of incineration bottom ash in construction – Evaluation of environmental impact N2 - The results from a long-term lysimeter experiment with incineration bottom ash irrigated with artificial rain are reported. Whereas chloride concentration dropped significantly, the release of antimony increased during the course of the experiment as a result of aging processes. T2 - 10th International Conference on the Environmental and Technical Implications of Construction with Alternative Materials, WASCON 2018 CY - Tampere, Finland DA - 06.06.2018 KW - Leaching KW - MSWI Bottom Ash KW - Lysimeter KW - Antimony PY - 2018 SN - 978-951-758-631-3 SN - 0356-9403 SP - 108 EP - 110 AN - OPUS4-45416 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bandow, Nicole A1 - Jürgens, Frederike A1 - Schoknecht, Ute T1 - Leachiing tests - a useful tool for the environmental impact assessment of construction products? N2 - Construction products and waste materials used for construction can be in contact with the environment and may release potential harmful compounds. Information on the total content of these substances in the product is not sufficient to assess its envrionmental impact since it does not consider realistic exposure conditions.The impact of these compounds is often assessed by using the total content in the product. This estimation lacks realistic exposure conditions. Concerning the pathway to soil and groundwater by contact with rain or seepage water leaching tests, which were developed and standardized by the European Committee for Standardization, are available. While for secondary construction products and waste this investigation of the leaching behaviour is standard procedure and is already part of regulation in Germany (draft ordinance on reuse of mineral waste) and within Europe (landfill directive) the release from primary construction products got in the focus more recently. Several monitoring studies found unexpected high concentrations of substances used as herbicides and fungicides in surface water and stormwater originating from urban areas. As some of these compounds are even banned for the use in agricultural applications in Europe alternative sources as roof materials and façade coatings exposed to rain were suggested. Further field and laboratory tests confirmed construction products as sources of these substances in water. The aim of this presentation is to show exemplary results of existing leaching methods and underline the strength and weaknesses of the test system with selected examples from our work. We especially draw the attention to the research which is still needed to close the gap between the results of leaching experiments and the subsequent risk assessment of the products. T2 - SETAC Europe CY - Rome, Italy DA - 13.05.2018 KW - Leaching KW - DSLT KW - Construction products PY - 2018 AN - OPUS4-44949 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bandow, Nicole A1 - Finkel, M. A1 - Grathwohl, P. A1 - Kalbe, Ute T1 - Influence of flow rate and particle size on local equilibrium in column percolation tests using crushed masonry N2 - Column leaching tests are frequently used and accepted for investigation of release of hazardous substances from solid materials. Independent of differences due to the field of application or national regulations, column tests assume that local equilibrium is established in the experiment which facilitates transfer of results to field conditions. In the process of harmonization and standardization within Europe the question on the influence of flow rate and grain size distribution on the local equilibrium was raised. Thus, a set of experiments using two different masonry materials with varying grain size distribution and flow rate were conducted including stop/flow experiments. Results are compared to a numerical model which takes intraparticle pore diffusion-controlled release of Mo and V into the percolating water into account. Due to the relatively high intraparticle porosity of the materials (24–29%) data and model indicate that initially equilibrium-state conditions prevail followed by rapidly decreasing concentrations. The model fits data for Mo and V reasonably well; however, after the initial decline of concentrations (at L/S > 2) extended tailing is observed especially of elements occurring as oxides, which is not captured by the model. KW - Leaching KW - Porosity KW - Stop/flow experiments model KW - Intraparticle diffusion KW - Vanadium KW - Molybdenum PY - 2019 U6 - https://doi.org/10.1007/s10163-019-00827-3 SN - 1438-4957 SN - 1611-8227 VL - 21 IS - 3 SP - 642 EP - 651 PB - Springer Japan AN - OPUS4-47265 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Bandow, Nicole A1 - Jürgens, Frederike A1 - Schoknecht, Ute T1 - Beregnete Bauteile und Bauprodukte: Entwicklung von Vergabekriterien für den Blauen Engel mit Hilfe von Auslaugtests N2 - Auslaugversuche wurden mit verschiedenen Bauprodukten durchgeführt, die unter Anwendungsbe-dingungen mit Niederschlägen in Kontakt kommen können. In das Testprogramm wurden Lacke für Außenanwendungen, Wärmedämmverbundsysteme, Dachziegel und polymere Dachfolien einbezogen. Mit diesen Produkten wurden der von CEN TC 351 entwickelte dynamische Oberflächenauslaugtest (DSLT) und Immersionstests nach EN 16105 durchgeführt. Emissionsverläufe wurden sowohl für an-organische Komponenten als auch für organische Substanzen in den Eluaten ermittelt. Auslaugbare organische Substanzen wurden zuvor in Screeningtests identifiziert. Um die mögliche Freisetzung von Stoffen aus Bauprodukten beurteilen zu können, ist es erforderlich, Emissionsverläufe zu beschreiben. Dazu sind die verwendeten Testverfahren geeignet. Um Baupro-dukte mit einem Blauen Engel als „Produkte mit geringer Auslaugung“ auszuloben, müssen die aus-laugbaren Substanzen komplett bekannt sein. Für organische Verbindungen ist das noch eine Heraus-forderung. Außerdem erfordert die Bewertung der Testergebnisse sowohl Übertragungsmodelle, die Vorhersagen über freisetzbare Stoffmengen unter Anwendungsbedingungen ermöglichen, als auch Vorgaben zu tolerierbaren Umweltkonzentrationen. Hier besteht noch Handlungsbedarf. N2 - Leaching tests were performed on different construction products that can be exposed to precipitation during service life. Varnishes for outdoor application, exterior thermal insulation systems, roof tiles and polymeric roof membranes were included in the test program. Leaching tests according to the dynamic surface leaching test (DSLT) as developed by CEN TC 351 and the immersion test according to EN 16105 were performed using these products. Emission curves were determined for inorganic as well as organic substances in the eluates. Leachable organic sub-stances in the eluates were identified by screening tests prior to the leaching tests. It is necessary to describe emission curves to be able to evaluate possible release of substances from construction products. The applied leaching tests are suitable to describe leaching processes. All leach-able substances need to be known in order to award the ecolabel ‘Blue Angel’. This is still challenging in case of organic substances. In addition, evaluation of the test results requires transfer models to predict leachable amounts under service conditions as well as requirements on concentrations that can be tolerated in environmental compartments. There is still need for action to solve these topics. KW - Bauprodukte KW - Auslaugtests KW - Blauer Engel KW - Construction Products KW - Leaching PY - 2018 SN - 1862-4359 VL - 67/2018 SP - 1 EP - 89 CY - Dessau-Rosslau AN - OPUS4-45799 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -