TY - CONF A1 - An, Biwen Annie A1 - Kunte, Hans-Jörg A1 - Koerdt, Andrea ED - Eibergen, N. ED - Poulassichidis, T. T1 - Microbiologically Influenced Corrosion (MIC) by Halophilic (Salt-Loving) Nitrate and Sulfate-Reducing Microorganisms N2 - The survey of Canadian shale sites showed a dominance of halophilic microorganisms, including Halomonas (HA). Nitrate-amended incubations of the field samples under high salinity (14.6% NaCl), revealed a dominance of HA (>72%) and an accumulation of nitrite. Nitrite accumulation directly inhibited the growth of SRB, thereby decreasing their souring and corrosion risks. However, accumulated nitrite may also contribute to iron corrosion, which will be tested by using different concentrations of nitrate as an electron acceptor to HA. Different salinities are further tested on HA strains supplemented with iron coupons to determine their effects on iron corrosion rates. HA incubated with separate cultures of corrosive methanogen and SRB were tested to determine whether a positive or adverse effect will occur between them. Lastly, analyses of iron coupons will be conducted using TOF-SIMS, FIB-SEM and EDS for corrosion product characterization T2 - Corrosion 2021 CY - Online Meeting DA - 19.04.2021 KW - MIC KW - Bacteria KW - Halophile KW - Corrosion KW - Environmental condition KW - Korrosion KW - High salinity PY - 2021 UR - https://my.nace.org/PaperTrail/Authors/Submission.aspx?id=2914f145-7f8f-ea11-813a-005056a95a7c SP - Paper C2021-16284, 1 AN - OPUS4-52479 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Koerdt, Andrea A1 - An, Biwen Annie A1 - Deland, Eric ED - Eibergen, N. ED - Poulassichidis, T. T1 - Novel Multiport Flow-Column Corrosion Monitoring System (MFC) Revealed High Corrosion Rates by Corrosive Methanogenic Archaea N2 - MFC was used to study the corrosiveness of iron-utilizing methanogen, Methanobacterium IM1 under flow conditions. Comparing against electrical SRM, Desulfovibrio ferrophilus IS5, results showed under standard mesophilic conditions, average corrosion rates of Methanobacterium IM1 was double that of SRM. The highest corrosion rate of Methanobacterium IM1 reached up to 0.60 mm/yr under neutral conditions, and severe pitting was observed on the iron surface. Furthermore, the corrosion products of Methanobacterium IM1 were characterized with TOF-SIM, FIB-SEM and EDX, and preliminary results revealed FeCO3 is not the only corrosion product of Mi-MIC, as previously reported. Under low pH conditions, the maximum corrosion rate of Methanobacterium IM1 reached 1.57 mm/yr, which resulted in severed deformity of the iron specimen. Additional comparisons using different types of incubation material were conducted to standardize MFC MIC testing. T2 - Corrosion 2021 CY - Online Meeting DA - 19.04.2021 KW - MIC KW - Microbiologically influenced corrosion KW - Biocorrosion KW - Hi-Tension KW - Environmental condition KW - Flow Model KW - Modelling KW - Korrosion PY - 2021 UR - https://my.nace.org/PaperTrail/Authors/Submission.aspx?id=2b6387be-7390-ea11-813a-005056a95a7c SP - Paper C2021-16303, 1 AN - OPUS4-52480 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -