TY - CONF A1 - Simon, Franz-Georg A1 - Kalbe, Ute A1 - Bandow, Nicole T1 - Potential use of incineration bottom ash in construction – Evaluation of environmental impact T2 - Proceedings WASCON 2018, No Cradle, no Grave - Circular Economy N2 - The results from a long-term lysimeter experiment with incineration bottom ash irrigated with artificial rain are reported. Whereas chloride concentration dropped significantly, the release of antimony increased during the course of the experiment as a result of aging processes. T2 - 10th International Conference on the Environmental and Technical Implications of Construction with Alternative Materials, WASCON 2018 CY - Tampere, Finland DA - 06.06.2018 KW - Leaching KW - MSWI Bottom Ash KW - Lysimeter KW - Antimony PY - 2018 SN - 978-951-758-631-3 SN - 0356-9403 SP - 108 EP - 110 AN - OPUS4-45416 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kalbe, Ute A1 - Vogel, Christian A1 - Simon, Franz-Georg T1 - Antimony in incineration bottom ash – Leaching behavior and conclusions for treatment processes T2 - SUM 2020 Proceedings N2 - Antimony (Sb) is used in industrial products mainly as flame retardant in plastic material. Due to such additives in plastics, about a half of Sb ends up in municipal solid waste incineration at the end-of-life and consequently in relevant amounts in the generated bottom ash. In contact with water, the initial leachability is low, as antimonates form sparingly soluble compounds with Ca2+. Following the carbonation of the incineration bottom ash (IBA) during the proceeding ageing the pH in the leachates decreases. With decreasing concentration of Ca in the eluate the solution equilibrium changes and antimonates dissolve. In Germany it is intended to regulate Sb in IBA with the planned implementation of the so called Mantelverordnung (MantelVO, containing provisions on the utilisation of mineral waste) in the near future. The limit values set in the draft might be critical for IBA and therefore pose a risk for the utilisation of the mineral fraction of IBA in the well-established recycling routes. T2 - SUM 2020 – 5th Symposium on Urban Mining and Circular Economy CY - Online meeting DA - 18.11.2020 KW - Bottom ash KW - Leaching KW - Antimony PY - 2020 SP - 1 EP - 4 AN - OPUS4-51622 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kalbe, Ute A1 - Simon, Franz-Georg T1 - Potential use of incineration bottom ash in construction – Evaluation of the environmental impact JF - Waste and Biomass Valorization N2 - Knowledge of the long-term leaching behavior of potentially harmful substances is crucial for the assessment of the environmental compatibility of reusing municipal solid-waste incineration bottom ash (MSWI BA) in construction, i.e., as a road base layer. BA fractions obtained from wet-processing aiming at the improvement of environmental quality were used to investigate the mobility of relevant substances. Eluates from laboratory-scaled leaching procedures (column percolation and lysimeters) were analyzed to learn about the long-term release of substances. Unsaturated conditions and artificial rainwater (AR) were used in the lysimeter tests to simulate field conditions. In addition, batch test eluates were generated at usual liquid-to-solid ratios (L/S) for compliance testing purposes. A variety of cations and anions was measured in the eluates. The wet treatment reduces the leaching of chloride and particularly sulfate by more than 60%. The release of typical contaminants for the treated MSWI BA such as the heavy metals Cu and Cr was well below 1% in the conducted leaching tests. An increase in the Sb concentration observed in the lysimeter experiments starting at L/S 0.75 L/kg and in the column experiment at L/S 4 L/kg is assumed to be related to decreasing concentrations of Ca and thus to the dissolution of sparingly soluble calcium antimonate. The same leaching mechanism applies with V, but the concentration levels observed are less critical regarding relevant limit values. However, on the long term the behavior of Sb could be problematic for the application of MSWI BA in construction. KW - MSWI bottom ash KW - Leaching KW - Batch tests KW - Lysimeter KW - Antimony PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-508421 DO - https://doi.org/10.1007/s12649-020-01086-2 SN - 1877-2641 VL - 11 IS - 12 SP - 7055 EP - 7065 PB - Springer AN - OPUS4-50842 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -