TY - GEN A1 - Simon, Franz-Georg A1 - Scholz, Philipp A1 - Gleis, Markus ED - Thiel, Stephanie ED - Thome-Kozminesky, Elisabeth ED - Quicker, Pater ED - Gosten, Alexander ED - Stengler, Ella T1 - Einstufung von Aschen und Schlacken aus der Abfallverbrennung im Hinblick auf die weitere Verwertung N2 - There are two mirror entries in the European Waste Catalogue for bottom ash and slag from waste incineration: 19 01 11* and 19 01 12. Entry 19 01 11* describes a waste material containing hazardous substances. It was shown that only the hazardous property HP14 (ecotoxic) is of relevance for the classification. If substances with the hazard statement code (HSC) H400, H410, H411, H412 and H413 are present in incineration bottom ash (IBA) above certain level the waste is classified as hazardous, otherwise it is non-hazardous (in this case 19 01 12). It was further shown that only Cu, Zn and Pb compounds have an impact on the classification using a summation rule: 100xΣ c(H410) + 10xΣ c(H411) + Σ c(H412). Limit value is 25 percent. It is obvious that H410 substances have the highest impact. Therefore, the knowledge of the elemental composition of IBA is not sufficient because the content of distinct chemical compounds (with the respective molecular weight) is needed. When the exact speciation is not known a worst-case approach has to be applied. A practical guideline for the estimation of HP14 was developed based on the definition of 4 substance groups: 1. Metals and alloys, 2. Water-soluble substances, 3. Oxides and carbonates and 4. Substances not soluble in weak acids. In substance group 1 only fine Zn powder has the HSC H410. Water-soluble substances are assumed to be H410 substances. Their concentrations are, however, regularly below the cut-off value of 0.1 %. The amount of substance group 3 is estimated by a selective extraction with maleic acid. According to the worst-case approach it is assumed that CuCO3xCu(OH)2 and ZnO represent the respective Cu and Zn species in IBA because these substances have the highest stochiometric factor. Even with this worst-case approach results from operators of IBA treatment plant showed that the limit value of 25 % is not exceeded. The requirements for utilization of IBA in Germany are defined in the Secondary Building Materials Decree (Ersatzbaustoffverordnung EBV) which was set into force in August 2023. Leaching methods (batch test or column test) with a liquid-to-solid ratio of 2 l/kg are applied. IBA fulfills the requirements for class HMVA-2. Actually, even a classification of IBA as hazardous (i.e 19 01 11*) would not affect utilization but handling and transport. KW - Rostasche KW - Ökotoxizität KW - Ersatzbaustoffverordnung KW - XANES-Spektroskopie PY - 2024 SN - 978-3-944310-90-9 VL - 1 SP - 402 EP - 414 PB - TK-Verlag CY - Neuruppin ET - 1 AN - OPUS4-59465 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Roesch, Philipp A1 - Schinnen, Andrea A1 - Riedel, Maren A1 - Sommerfeld, Thomas A1 - Sawal, G. A1 - Bandow, N. A1 - Vogel, Christian A1 - Kalbe, Ute A1 - Simon, Franz-Georg T1 - Investigation of pH-dependent extraction methods for PFAS in (fluoropolymer-based) consumer products: A comparative study between targeted and sum parameter analysis N2 - Here, we report a comparative study of different sum parameter analysis methods for the extraction of per- and polyfluoroalkyl substances (PFAS) from manufactured consumer products, which can be measured by combustion ion chromatography (CIC). Therefore, a hydrolysis-based extraction method was further developed, which accounts for the addition of hydrolyzable covalently bound polyfluoroalkylated side-chain polymers (SFPs) to the extractable organic fluorine portion of the mass balance proposed as "hydrolyzable organically bound fluorine" (HOF). To test this hypothesis, the method was applied to 39 different consumer products containing fluoropolymers or monomeric PFAS taken from four different categories: outdoor textiles, paper packaging, carpeting, and permanent baking sheets. We also evaluated the method's efficiency by extracting four synthesized fluorotelomer polyacrylate reference compounds. The total fluorine (TF) and extractable organically bound fluorine (EOF) values were measured through CIC using established protocols. The TF values ranged from sub-ppb to %-levels, depending on the compound class. All samples showed results for hydrolyzed organofluorine (HOF) between 0.03 and 76.3 μg/g, while most EOF values were lower (150 µg/kg, because of different diffusion properties for various PFAS, but also kinetic exchange limitations. However, the DGT approach has the advantage that almost no sample preparation is necessary. Moreover, the PFAS adsorption on the DGT binding layer was investigated via surface sensitive spectroscopical methods, such as Fourier-transform infrared (FT-IR) and fluorine K-edge X-ray absorption near-edge structure (XANES) spectroscopy. T2 - DGT Konferenz CY - Paris, France DA - 11.10.2023 KW - Combustion Ion Chromatography KW - Per- and Polyfluoroalkyl substances (PFAS) KW - Sewage sludge PY - 2023 AN - OPUS4-58575 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Becker, Roland A1 - Scholz, Philipp A1 - Jung, Christian A1 - Weidner, Steffen T1 - Thermo-Desorption Gas Chromatography-Mass Spectrometry for investigating the thermal degradation of polyurethanes N2 - Thermo-Desorption Gas Chromatography-Mass Spectrometry (TD-GC-MS) was used to investigate the thermal degradation of two different polyurethanes (PU). PU samples were heated at different heating rates and the desorbed products were collected in a cold injection system and thereafter submitted to GC-MS. Prospects and limitations of the detection and quantification of semi-volatile degradation products were investigated. A temperature dependent PU depolymerization was found at temperatures above 200 °C proved by an increasing release of 1,4-butanediol and methylene diphenyl diisocyanate (MDI) representing the main building blocks of both polymers. Their release was monitored quantitatively based on external calibration with authentic compounds. Size Exclusion Chromatography (SEC) of the residues obtained after thermodesorption confirmed the initial competitive degradation mechanism indicating an equilibrium of crosslinking and depolymerization as previously suggested. Matrix-Assisted Laser Desorption Ionization (MALDI) mass spectrometry of SEC fractions of thermally degraded PUs provided additional hints on degradation mechanism. KW - Thermo-desorption KW - Mass spectrometry KW - Polyurethanes KW - Thermal degradation PY - 2023 U6 - https://doi.org/10.1039/D3AY00173C SN - 1759-9660 SP - 1 EP - 6 PB - Royal Society for Chemistry AN - OPUS4-57307 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Roesch, Philipp A1 - Vogel, Christian A1 - Wittwer, Philipp A1 - Huthwelker, T. A1 - Borca, C. A1 - Sommerfeld, Thomas A1 - Kluge, Stephanie A1 - Piechotta, Christian A1 - Kalbe, Ute A1 - Simon, Franz-Georg T1 - Taking a Look at the Surface: µ-XRF Mapping and Fluorine K-edge µ-XANES Spectroscopy of Organofluorinated Compounds in Environmental Samples and Consumer Products N2 - For the first time, µ-X-ray fluorescence (µ-XRF) mapping combined with fluorine K-edge µ-X-ray absorption near-edge structure (µ-XANES) spectroscopy was applied to depict per- and polyfluoroalkyl substances (PFAS) contamination and inorganic fluoride in samples concentrations down to 100 µg/kg fluoride. To demonstrate the matrix tolerance of the method, several PFAS contaminated soil and sludge samples as well as selected consumer product samples (textiles, food contact paper and permanent baking sheet) were investigated. µ-XRF mapping allows for a unique element-specific visualisation at the sample surface and enables localisation of fluorine containing compounds to a depth of 1 µm. Manually selected fluorine rich spots were subsequently analysed via fluorine K-edge µ-XANES spectroscopy. To support spectral interpretation with respect to inorganic and organic chemical distribution and compound class determination, linear combination (LC) fitting was applied to all recorded µ-XANES spectra. Complementarily, solvent extracts of all samples were target-analysed via LC-MS/MS spectrometry. The detected PFAS sum values range from 20 to 1136 µg/kg dry weight (dw). All environmentally exposed samples revealed higher concentration of PFAS with a chain length >C8 (e.g. 580 µg/kg dw PFOS for Soil1), whereas the consumer product samples showed a more uniform distribution with regard to chain lengths from C4 to C8. Independent from quantified PFAS amounts via target analysis, µ-XRF mapping combined with µ-XANES spectroscopy was successfully applied to detect both point-specific concentration maxima and evenly distributed surface coatings of fluorinated organic contaminants in the corresponding samples. KW - PFAS KW - XRF KW - LC-MS/MS KW - XANES KW - Fluoride KW - Soil PY - 2023 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-576109 SN - 2050-7887 SP - 1 EP - 12 PB - Royal Society of Chemistry AN - OPUS4-57610 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -