TY - GEN A1 - Simon, Franz-Georg A1 - Scholz, Philipp A1 - Gleis, Markus ED - Thiel, Stephanie ED - Thome-Kozminesky, Elisabeth ED - Quicker, Pater ED - Gosten, Alexander ED - Stengler, Ella T1 - Einstufung von Aschen und Schlacken aus der Abfallverbrennung im Hinblick auf die weitere Verwertung N2 - There are two mirror entries in the European Waste Catalogue for bottom ash and slag from waste incineration: 19 01 11* and 19 01 12. Entry 19 01 11* describes a waste material containing hazardous substances. It was shown that only the hazardous property HP14 (ecotoxic) is of relevance for the classification. If substances with the hazard statement code (HSC) H400, H410, H411, H412 and H413 are present in incineration bottom ash (IBA) above certain level the waste is classified as hazardous, otherwise it is non-hazardous (in this case 19 01 12). It was further shown that only Cu, Zn and Pb compounds have an impact on the classification using a summation rule: 100xΣ c(H410) + 10xΣ c(H411) + Σ c(H412). Limit value is 25 percent. It is obvious that H410 substances have the highest impact. Therefore, the knowledge of the elemental composition of IBA is not sufficient because the content of distinct chemical compounds (with the respective molecular weight) is needed. When the exact speciation is not known a worst-case approach has to be applied. A practical guideline for the estimation of HP14 was developed based on the definition of 4 substance groups: 1. Metals and alloys, 2. Water-soluble substances, 3. Oxides and carbonates and 4. Substances not soluble in weak acids. In substance group 1 only fine Zn powder has the HSC H410. Water-soluble substances are assumed to be H410 substances. Their concentrations are, however, regularly below the cut-off value of 0.1 %. The amount of substance group 3 is estimated by a selective extraction with maleic acid. According to the worst-case approach it is assumed that CuCO3xCu(OH)2 and ZnO represent the respective Cu and Zn species in IBA because these substances have the highest stochiometric factor. Even with this worst-case approach results from operators of IBA treatment plant showed that the limit value of 25 % is not exceeded. The requirements for utilization of IBA in Germany are defined in the Secondary Building Materials Decree (Ersatzbaustoffverordnung EBV) which was set into force in August 2023. Leaching methods (batch test or column test) with a liquid-to-solid ratio of 2 l/kg are applied. IBA fulfills the requirements for class HMVA-2. Actually, even a classification of IBA as hazardous (i.e 19 01 11*) would not affect utilization but handling and transport. KW - Rostasche KW - Ökotoxizität KW - Ersatzbaustoffverordnung KW - XANES-Spektroskopie PY - 2024 SN - 978-3-944310-90-9 VL - 1 SP - 402 EP - 414 PB - TK-Verlag CY - Neuruppin ET - 1 AN - OPUS4-59465 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Simon, Franz-Georg A1 - Scholz, Philipp A1 - Ling, Ruisi A1 - Koralewska, Ralf A1 - Gleis, Markus T1 - Aschen und Schlacken aus der Abfallverbrennung im Lichte der Ersatzbaustoffverordnung N2 - Aschen und Schlacken aus der thermischen Abfallbehandlung stellen mit rund 25% Massenanteil die größte Reststofffraktion dar. In Deutschland fallen pro Jahr rund 6 Millionen Tonnen an. Während sich die Verwertung der metallischen Anteile problemlos gestaltet, werden an die mineralische Fraktion Anforderungen bezüglich der möglichen Freisetzung von Schwermetallen sowie Chlorid und Sulfat gestellt. In der Ersatzbaustoffverordnung sind für Aschen und Schlacken aus der Abfallverbrennung zwei Materialklassen mit unterschiedlich hohen Anforderungen an die Umweltverträglichkeit definiert. Im Rahmen eines Forschungsprojekts wurde untersucht, ob mit Abtrennung der Feinfraktion von 0–2mm die höhere Materialklasse HMVA-1 erreicht werden kann. Im Ergebnis wurde eine Verbesserung des Auslaugverhaltens erzielt, doch nicht in dem Maß, dass eine Qualität nach HMVA-1 erreicht wird. Rostaschen halten aber die Anforderungen zur Deponierung auf einer DK I-Deponie sowie die Anforderungen zur Verwertung gemäß HMVA-2 sicher ein. KW - Rostasche KW - Auslaugtest KW - Ersatzbaustoff PY - 2024 DO - https://doi.org/10.37307/j.1863-9763.2024.07.08 SN - 1863-9763 VL - 56 IS - 7 SP - 407 EP - 411 PB - Erich Schmidt Verlag GmbH & Co. KG CY - Berlin AN - OPUS4-60601 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GOVDOC A1 - Simon, Franz-Georg A1 - Wöhlecke, Andreas T1 - 8. Nachtrag zum Zulassungsschein 12/BAM IV.3/09/00 für eine Schutzschicht bestehend aus einer sandgefüllten Schutzbahn für Kunststoffdichtungsbahnen in Deponieabdichtungen N2 - 8. Nachtrag zum Zulassungsschein 12/BAM IV.3/09/00 für eine Schutzschicht bestehend aus einer sandgefüllten Schutzbahn für Kunststoffdichtungsbahnen in Deponieabdichtungen der Fa. G quadrat GmbH, Krefeld. KW - Zulassung KW - Deponie KW - Schutzschicht KW - Kunststoffdichtungsbahn PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-604877 SP - 1 EP - 29 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-60487 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Vogel, Christian A1 - Doolette, A. A1 - Huang, J. T1 - Combining DGT and 31P NMR spectroscopy to determine phosphorus species in soil N2 - The amount of plant-available phosphorus (P) in soil strongly influences the yield of plants in agriculture. Therefore, various simple chemical extraction methods have been developed to estimate the plant-available P pools in soil. More recently, several experiments with the DGT technique have shown that it has a much better correlation to plant-available P in soils than standard chemical extraction methods (e.g. calcium-acetate-lactate (CAL), Colwell, Olsen, water) when soils with different characteristics are considered. However, the DGT technique cannot give information on the plant-available P species in the soil. Therefore, we combined DGT with solution 31P nuclear magnetic resonance (NMR) spectroscopy. This was achieved by using a modified DGT device in which the diffusive layer had a larger pore size, the binding layer incorporated an adsorption material with a higher capacity, and the device had a larger exposure area. The spectroscopic investigation was undertaken after elution of the deployed DGT binding layer in a NaOH solution. Adsorption tests using solutions of known organic P compounds showed that a sufficient amount of these compounds could be adsorbed on the binding layer in order for them to be analyzed by solution 31P NMR spectroscopy. Furthermore, various intermediates of the hydrolysis of trimetaphosphate in soil could be also analyzed over time. T2 - DGT Konferenz CY - Paris, France DA - 11.10.2023 KW - Soil KW - Phosphorus KW - Plant-availability PY - 2023 AN - OPUS4-58574 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Vogel, Christian A1 - Roesch, Philipp A1 - Wittwer, Philipp A1 - Lisec, Jan A1 - Borca, C. A1 - Huthwelker, T. A1 - Simon, Franz-Georg T1 - Combining DGT and combustion ion chromatography (CIC) as screening tool for per- and polyfluoroalkyl substances (PFAS) contamination in wastewater-based fertilizers N2 - Per- and polyfluoroalkyl substances (PFAS) are a large group of organofluorine surfactants used in the formulations of thousands of consumer goods. The continuous use of PFAS in household products and the discharge of PFAS from industrial plants into the sewer system have been resulted in contaminated effluents and sewage sludge from wastewater treatment plants (WWTPs) which became an important pathway for PFAS into the environment. Because sewage sludge is often used as fertilizer its application on agricultural soils has been observed as significant input path for PFAS into our food chain. To produce high-quality phosphorus fertilizers for a circular economy from sewage sludge, PFAS and other pollutants (e.g. pesticides and pharmaceuticals) must be separated from sewage sludge. Normally, PFAS are analyzed using PFAS protocols typically with time-consuming extraction steps and LC-MS/MS target quantification. However, for screening of PFAS contaminations in wastewater-based fertilizers also the DGT technique can be used for the PFAS extraction. Afterwards, combustion ion chromatography (CIC) can be applied to analyze the “total” amount of PFAS on the DGT binding layer. The DGT method was less sensitive and only comparable to the extractable organic fluorine (EOF) method values of the fertilizers in samples with >150 µg/kg, because of different diffusion properties for various PFAS, but also kinetic exchange limitations. However, the DGT approach has the advantage that almost no sample preparation is necessary. Moreover, the PFAS adsorption on the DGT binding layer was investigated via surface sensitive spectroscopical methods, such as Fourier-transform infrared (FT-IR) and fluorine K-edge X-ray absorption near-edge structure (XANES) spectroscopy. T2 - DGT Konferenz CY - Paris, France DA - 11.10.2023 KW - Combustion Ion Chromatography KW - Per- and Polyfluoroalkyl substances (PFAS) KW - Sewage sludge PY - 2023 AN - OPUS4-58575 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR T1 - Amts- und Mitteilungsblatt, Band 53, Heft 1 T3 - Amts- und Mitteilungsblatt der BAM - 1/2023 KW - Anerkennungen KW - Zulassungen KW - Richtlinien PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-574038 SN - 0340-7551 VL - 53 IS - 1 SP - 1 EP - 340 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-57403 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Simon, Franz-Georg A1 - Scholz, Philipp A1 - Gleis, Markus T1 - Aschen und Schlacken aus der Abfallverbrennung; Gefährlich oder nicht? N2 - In Deutschland fallen aktuell pro Jahr über 5 Mio. Tonnen Hausmüllverbrennungs-aschen (HMVA) an. Eine Verwertung dieser Aschen und Schlacken ist in Deutschland möglich und findet überwiegend im Deponiebau statt. Für die Verwertung sind in der Ersatzbaustoffverordnung Eluatgrenzwerte für Schwermetalle und einige andere Parameter vorgesehen. Der Umgang mit HMVA könnte durch eine Einstufung als gefährlicher Abfall erschwert werden. Maßgeblich für die Einstufung eines Abfalls als gefährlich oder ungefährlich sind die gefahrenrelevanten Eigenschaften HP 1 bis HP 15 nach Anhang III der Richtlinie 2008/98/EG über Abfälle mit dort festgelegten Konzentrationsgrenzen. Für HMVA ist im Wesentlichen nur der Parameter HP 14 (Ökotoxizität) von Bedeutung. Dafür sind entscheidend die Gehalte an chemischen Verbindungen mit den Gefahrenhinweiscodes (hazard statement code, HSC) H400, H410, H411, H412 und H413. Eine detaillierte Diskussion zu den übrigen Gefahreneigenschaften bei HMVA findet sich in der Literatur. Die Einstufung als gefährlicher Abfall erfolgt nach festgelegten Rechenregeln. Die BAM bearbeitet ein durch das UBA gefördertes Forschungsprojekt zur Erfassung und Bewertung von Analysedaten zu Aschen und Schlacken aus Abfallverbrennungsanlagen. Die Ergebnisse des Vorhabens sollen bei der Weiterentwicklung des vorhandenen Konzeptes für eine bundeseinheitlichen Untersuchung und abfallrechtlichen Einordnung von Aschen und Schlacken aus deutschen Abfallverbrennungsanlagen unterstützend herangezogen werden. Im Vortrag werden Verfahren zur quantitativen Bestimmung der einstufungsrelevanten Verbindungen vorgestellt: 1.) der Praxisleitfaden von ITAD und IGAM, 2.) Methode basierend auf der Bioverfügbarkeit und 3.) Methode basierend auf Speziierungsanalyse. T2 - Jahrestreffen 2023 der DECHEMA-Fachgruppen AuW und TRO CY - Dresden, Germany DA - 06.03.2023 KW - Rostasche KW - Speziierungsanalyse KW - Abfallbehandlung PY - 2023 AN - OPUS4-57346 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Vogel, Christian T1 - Investigation of per and polyfluoroalkyl substances (PFAS) in soils and groundwater through fluorine K-edge XANES spectroscopy – potential for collaboration N2 - Per- and polyfluoroalkyl substances (PFAS) are a group of anionic, cationic and zwitterionic synthetic products, in which the hydrogen atoms on the carbon skeleton of at least one carbon atom have been completely replaced by fluorine atoms and which include more than 4730 compounds, depending on the definition. As a result of continuous and prolific use, mainly in aviation firefighting foams, thousands of industrial and military installations have been found to contain contaminated soil, groundwater and surface water. Furthermore, current decontamination strategies of PFAS-burdened soils mainly consist of adsorption methods using adsorbents for fixation of PFAS in the ground. Hence, there is a great demand for innovative developments and chemical treatment technologies, dealing with new strategies of tackling the PFAS problem. Thus, we investigated mechanochemical treatment of PFAS contaminated soils with various additives in a ball mill and analyzed the PFAS defluorination. In this presentation the advantages of fluorine K-edge X-ray absorption near-edge structure (XANES) spectroscopy for various environment samples are shown. T2 - SESAME-Germany Info Day CY - Hamburg, Germany DA - 21.04.2023 KW - Soil KW - Per- and Polyfluoroalkyl substances (PFAS) KW - Synchotron KW - X-ray absorption near-edge structure (XANES) spectroscopy PY - 2023 AN - OPUS4-57365 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Vogel, Christian T1 - PFAS analytics and their relation to PFAS remediation N2 - Per- and polyfluoroalkyl substances (PFAS) are a large group of more than 10,000 anionic, cationic, zwitterionic or neutral organofluorine surfactants. As a result of continuous and prolific use, mainly in aviation firefighting foams, thousands of industrial and military installations have been found to contain contaminated soil, groundwater and surface water. While liquid chromatography tandem mass spectrometry (LC-MS/MS) is commonly used technique to characterize targeted PFAS in environmental samples, there are more than 10,000 different PFAS known, which have various headgroups and properties. Therefore, several analytical techniques are available to analyse various groups or pools of PFAS or “all” PFAS as a sum parameter. Current decontamination strategies of PFAS-burdened soils mainly consist of adsorption methods using adsorbents for fixation of PFAS in the ground. A second option is the utilization of a “pump and treat” process, cycling polluted soils through a washing plant leading to the concentration of the pollutants in the fine fraction. Both approaches are cost-intensive and not intended for the direct decomposition of all PFAS contaminants. Hence, there is a great demand for innovative developments and chemical treatment technologies, dealing with new strategies of tackling the PFAS problem. Previously, mechanochemical treatment of polychlorinated organic compounds in soils showed an efficient dechlorination. Thus, we investigated mechanochemical treatment of PFAS contaminated soils with various additives in a ball mill and analyzed the PFAS defluorination with gas chromatography mass spectrometry (GC-MS) and liquid chromatography tandem mass spectrometry (LC-MS/MS), respectively, as well es the fluoride mineralization by ion chromatography (IC) and fluorine K-edge X-ray absorption near-edge structure (XANES) spectroscopy. T2 - International workshop of CAR-PFAS (Consortium for analysis and remediation of per- and polyfluoroalkyl substances) Japan CY - Tokyo, Japan DA - 17.10.2023 KW - Mechanochemical treatment KW - Per- and Polyfluoroalkyl substances (PFAS) KW - XANES spectroscopy KW - Soil PY - 2023 AN - OPUS4-58609 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Simon, Franz-Georg A1 - Frieling, Sophie T1 - Sorptionsverhalten von Antimon an Eisenoxidverbindungen N2 - Aschen und Schlacken aus der thermischen Abfallbehandlung enthalten eine Vielzahl von Schwermetallverbindungen. Für Antimon, Chrom, Kupfer, Molybdän und Vanadium werden in der neuen Ersatzbaustoffverordnung (Bundesregierung, 2021) Eluatgrenzwerte für die Verwertung festgelegt. Aschen und Schlacken werden aus der Abfallverbrennungsanlage nass ausgetragen und vor einer Verwertung in der Regel mehrere Wochen gelagert. Dabei finden hydraulische Reaktionen statt und enthaltenes CaO wird zu einem Großteil in Calciumcarbonat umgewandelt. Während wässrige Eluate von frischen Aschen pH-Werte von 12 und höher aufweisen, sind die Eluate nach einigen Wochen weniger stark alkalisch. Die gemessenen Schwermetallkonzentrationen sind daher dann auch deutlich niedriger, mit Ausnahme von Antimon (Sb) und Vanadium (V). Hier steigen die Konzentration mit der Lagerungsdauer. Grund sind sinkende Konzentrationen von Ca-Ionen, die sonst zu einer Ausfällung von Antimonaten und Vanadaten führen. Zu hohe Eluatwerte von Sb und V können jedoch durch Sorption an Eisenoxidverbindungen gemindert werden. Dazu wurden Sorptionsexperimente mit verschiedenen Eisenoxidverbindungen durchgeführt. T2 - 5. Internationales Bergbausymposium WISSYM 2023 CY - Dresden, Germany DA - 25.09.2023 KW - Rostasche KW - Sorption KW - Ersatzbaustoff PY - 2023 UR - https://www.wismut.de/de/download.php?download=Wi_WISSYM2023_Abstracts_END_klein.pdf SP - 247 EP - 250 AN - OPUS4-58701 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Simon, Franz-Georg A1 - Frieling, Sophie T1 - Sorptionsverhalten von Antimon an Eisenoxidverbindungen N2 - Aschen und Schlacken aus der thermischen Abfallbehandlung enthalten eine Vielzahl von Schwermetallverbindungen. Für Antimon, Chrom, Kupfer, Molybdän und Vanadium werden in der neuen Ersatzbaustoffverordnung Eluatgrenzwerte für die Verwertung festgelegt. Aschen und Schlacken werden aus der Abfallverbrennungsanlage nass ausgetragen und vor einer Verwertung in der Regel mehrere Wochen gelagert. Dabei finden hydraulische Reaktionen statt und enthaltenes CaO wird zu einem Großteil in Calciumcarbonat umgewandelt. Während wässrige Eluate von frischen Aschen pH-Werte von 12 und höher aufweisen, sind die Eluate nach einigen Wochen weniger stark alkalisch. Die gemessenen Schwermetallkonzentrationen sind daher dann auch deutlich niedriger, mit Ausnahme von Antimon (Sb) und Vanadium (V). Hier steigen die Konzentration mit der Lagerungsdauer. Grund sind sinkende Konzentrationen von Ca-Ionen, die sonst zu einer Ausfällung von Antimonaten und Vanadaten führen. Zu hohe Eluatwerte von Sb und V können durch Sorption an Eisenoxidverbindungen gemindert werden. Als besonders wirkungsvoll hat sich Schwertmannit (Eisen-Oxyhydroxysulfat) erwiesen. Es entsteht durch Oxidation von pyrithaltigem Material durch Mikroorganismen und wird deshalb in Gebieten gefunden, in denen Braunkohle abgebaut wurde, z.B. in der Lausitz. Weitere untersuchte Eisenoxidverbindungen waren Hämatit und Schlämme aus der Abtrennung von Eisen und Mangan in Wasserwerken. T2 - 5. Internationales Bergbausymposium WISSYM 2023 CY - Dresden, Germany DA - 25.09.2023 KW - Rostasche KW - Sorption KW - Ersatzbaustoffe PY - 2023 AN - OPUS4-58702 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Simon, Franz-Georg A1 - Meggyes, Tamas ED - Zhang, H. X. T1 - Sustainable Remediation Methods for Metals and Radionuclides N2 - Sustainability has become the conscientious and future-oriented principle of modern resource management and environmental protection because caring for the future is tantamount to providing manageable and healthy surroundings for ourselves. For the foreseeable future, geotechnical and environmental engineers must therefore be concerned with ensuring a healthy balance between extraction, processing, manufacturing, utilization, recycling, and disposal of materials and products. KW - Permeable reactive barriers KW - Uranium mining KW - Groundwater KW - Electrochemical remediation PY - 2023 SN - 978-1-0716-2465-4 DO - https://doi.org/10.1007/978-1-0716-2466-1_63 SN - 2629-2378 SP - 251 EP - 284 PB - Springer Science+Business Media CY - Berlin, Heidelberg ET - 1 AN - OPUS4-58018 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kittner, Maria A1 - Altmann, Korinna A1 - Kalbe, Ute A1 - Hamann, S. A1 - Weyer, R. T1 - Bewertung der Freisetzung von Mikroplastik aus Sportböden auf Kunststoffbasis N2 - Projektvorstellung "Bewertung der Freisetzung von Mikroplastik aus Sportböden auf Kunststoffbasis": Motivation, Konzept, Umsetzung, erste analytische Ergebnisse der TED-GC/MS T2 - 24. Projekttage der Zukunft Bau Forschungsförderung CY - Bonn, Germany DA - 13.06.2023 KW - Mikroplastik KW - TED-GC/MS KW - Kunststoffrasen KW - Lysimeter KW - Beschleunigte Alterung PY - 2023 AN - OPUS4-58441 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kittner, Maria A1 - Altmann, Korinna A1 - Kalbe, Ute A1 - Hamann, S. A1 - Weyer, R. T1 - Bewertung der Freisetzung von Mikroplastik aus Sportböden auf Kunststoffbasis N2 - Projektvorstellung "Bewertung der Freisetzung von Mikroplastik aus Sportböden auf Kunststoffbasis": Konzept, Umsetzung, erste Mikroplastik-Ergebnisse. T2 - Projektbegleitkreissitzung des Projektes "„Ermittlung und Minderung von Mikroplastik- und Schadstoffemissionen von Kunststoffrasen-Sportplätzen (MiMiK)“ CY - Sittensen, Germany DA - 25.09.2023 KW - Mikroplastik KW - TED-GC/MS KW - Kunststoffrasen KW - Lysimeter KW - Beschleunigte Alterung PY - 2023 AN - OPUS4-58442 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wöhlecke, Andreas ED - Al-Akel, S. T1 - Die Spannungsrissbeständigkeit von Kunststoffdichtungsbahnen aus PE-HD und die Zulassungsrichtlinie für Schutzschichten N2 - Kunststoffdichtungsbahnen (KDB) aus PE-HD (Polyethylen hoher Dichte) werden häufig zur Abdichtung von Bauwerken in der Geotechnik verwendet. Diese Produkte werden aus einem Kunststoff mit relativ komplexer Zusammensetzung hergestellt. Um eine Aussage über die Haltbarkeit von KDB aus PE-HD treffen zu können, muss das Materialverhalten berücksichtigt werden. In diesem Zusammenhang sind die wichtigsten Aspekte der Dauerhaftigkeit die Spannungsrissbeständigkeit und die Beständigkeit gegen Oxidation. Verschiedene PE-Sorten weisen eine unterschiedliche Spannungsrissbeständigkeit auf. Um dieser Eigenschaft von PE-HD zu begegnen, werden nur KDB aus sehr hochwertigen Rohstoffen zugelassen. Auf der anderen Seite werden hohe Anforderungen an die umgebenden Schichten, wie Auflager und Schutzschicht gestellt, um möglichst geringe Spannungen zu erzeugen und damit Dehnungen die Dehnungen der KDB gering zu halten. Bestimmte Medien, die bei den betreffenden Prüfungen verwendet werden, dürfen nicht mehr in der EU in Verkehr gebracht werden. Im Folgenden sollen die Zusammenhänge in Kürze dargestellt werden. Darüber hinaus sollen Diskussionen und Änderungen der Zulassungsrichtlinie für Schutzschichten im und durch den Fachbeirat vorgestellt werden. T2 - 19. Leipziger Deponiefachtagung CY - Leipzig, Germany DA - 14.03.2023 KW - Spannungsrissbeständigkeit KW - Deponie KW - Kunststoffdichtungsbahn PY - 2023 SN - 978-3-943443-53-0 VL - 19 SP - 25 EP - 32 PB - PRESSEL Digitaler Produktionsdruck AN - OPUS4-57194 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wöhlecke, Andreas T1 - Die Spannungsrissbeständigkeit von Kunststoffdichtungsbahnen aus PE-HD und die Zulassungsrichtlinie für Schutzschichten N2 - Kunststoffdichtungsbahnen (KDB) aus PE-HD (Polyethylen hoher Dichte) werden häufig zur Abdichtung von Bauwerken in der Geotechnik verwendet. Diese Produkte werden aus einem Kunststoff mit relativ komplexer Zusammensetzung hergestellt. Um eine Aussage über die Haltbarkeit von KDB aus PE-HD treffen zu können, muss das Materialverhalten berücksichtigt werden. In diesem Zusammenhang sind die wichtigsten Aspekte der Dauerhaftigkeit die Spannungsrissbeständigkeit und die Beständigkeit gegen Oxidation. Verschiedene PE-Sorten weisen eine unterschiedliche Spannungsrissbeständigkeit auf. Um dieser Eigenschaft von PE-HD zu begegnen, werden nur KDB aus sehr hochwertigen Rohstoffen zugelassen. Auf der anderen Seite werden hohe Anforderungen an die umgebenden Schichten, wie Auflager und Schutzschicht gestellt, um möglichst geringe Spannungen zu erzeugen und damit Dehnungen die Dehnungen der KDB gering zu halten. Bestimmte Medien, die bei den betreffenden Prüfungen verwendet werden, dürfen nicht mehr in der EU in Verkehr gebracht werden. Im Folgenden sollen die Zusammenhänge in Kürze dargestellt werden. Darüber hinaus sollen Diskussionen und Änderungen der Zulassungsrichtlinie für Schutzschichten im und durch den Fachbeirat vorgestellt werden. T2 - 19. Leipziger Deponiefachtagung CY - Leipzig, Germany DA - 14.03.2023 KW - Deponie KW - Kunststoffdichtungsbahn KW - Spannungsrissbeständigkeit PY - 2023 AN - OPUS4-57195 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR T1 - Amts- und Mitteilungsblatt, Band 53, Heft 3 T3 - Amts- und Mitteilungsblatt der BAM - 3/2023 KW - Anerkennungen KW - Zulassungen KW - Richtlinien PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-585302 SN - 0340-7551 VL - 53 IS - 3 SP - 463 EP - 516 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-58530 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wöhlecke, Andreas ED - Egloffstein, Thomas ED - Burkhardt, Gerd T1 - Zum Spannungsrissverhalten von PE-HD Kunststoffdichtungsbahnen und zu aktuellen Themen aus dem Fachbeirat der BAM N2 - Kunststoffdichtungsbahnen (KDB) aus PE-HD (Polyethylen hoher Dichte) werden häufig zur Abdichtung von Bauwerken in der Geotechnik verwendet. Diese Produkte werden aus einem Kunststoff mit relativ komplexer Zusammensetzung hergestellt. Um eine Aussage über die Haltbarkeit von KDB aus PE-HD treffen zu können, muss das Materialverhalten berücksichtigt werden. In diesem Zusammenhang sind die wichtigsten Aspekte der Dauerhaftigkeit die Spannungsrissbeständigkeit und die Beständigkeit gegen Oxidation. Verschiedene PE-Sorten weisen eine unterschiedliche Spannungsrissbeständigkeit auf. Um dieser Eigenschaft von PE-HD zu begegnen, werden nur KDB aus sehr hochwertigen Rohstoffen zugelassen. Auf der anderen Seite werden hohe Anforderungen an die umgebenden Schichten, wie Auflager und Schutzschicht gestellt, um möglichst geringe Spannungen zu erzeugen und damit Dehnungen die Dehnungen der KDB gering zu halten. Bestimmte Medien, die bei den betreffenden Prüfungen verwendet werden, dürfen nicht mehr in der EU in Verkehr gebracht werden. Im Folgenden sollen die Zusammenhänge in Kürze dargestellt werden. Darüber hinaus sollen Diskussionen und Änderungen im Zusammenhang mit der Zulassungsrichtlinie für KDB vorgestellt werden. Der aktuelle Stand der Diskussion im Zusammenhang mit den verwendeten Tensiden in Bezug auf die Spannungsrissprüfung und weiterer Prüfungen wird aufgezeigt. Änderungen der Fremdprüfung von sogenannten Sandschutzmatten, des Standards zur Qualitätsüberwachung (SQÜ) von Kunststoff Dränelementen (KDE) und der Anpassung der Formulierungen zum Überbau der in Abdichtungen verwendeten Produkte werden in Kürze aufgezeigt. T2 - Karlsruher Deponie- und Altlastenseminar 2023 CY - Karlsruhe, Germany DA - 18.10.2023 KW - Spannungsrissbeständigkeit KW - Deponie KW - Kunststoffdichtungsbahn PY - 2023 SN - 978-3-939662-33-4 VL - 44 SP - 17 PB - ICP Eigenverlag Bauen und Umwelt CY - Karlsruhe AN - OPUS4-58633 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wöhlecke, Andreas T1 - Zum Spannungsrissverhalten von PE-HD Kunststoffdichtungsbahnen und zu aktuellen Themen aus dem Fachbeirat der BAM N2 - Kunststoffdichtungsbahnen (KDB) aus PE-HD (Polyethylen hoher Dichte) werden häufig zur Abdichtung von Bauwerken in der Geotechnik verwendet. Diese Produkte werden aus einem Kunststoff mit relativ komplexer Zusammensetzung hergestellt. Um eine Aussage über die Haltbarkeit von KDB aus PE-HD treffen zu können, muss das Materialverhalten berücksichtigt werden. In diesem Zusammenhang sind die wichtigsten Aspekte der Dauerhaftigkeit die Spannungsrissbeständigkeit und die Beständigkeit gegen Oxidation. Verschiedene PE-Sorten weisen eine unterschiedliche Spannungsrissbeständigkeit auf. Um dieser Eigenschaft von PE-HD zu begegnen, werden nur KDB aus sehr hochwertigen Rohstoffen zugelassen. Auf der anderen Seite werden hohe Anforderungen an die umgebenden Schichten, wie Auflager und Schutzschicht gestellt, um möglichst geringe Spannungen zu erzeugen und damit Dehnungen die Dehnungen der KDB gering zu halten. Bestimmte Medien, die bei den betreffenden Prüfungen verwendet werden, dürfen nicht mehr in der EU in Verkehr gebracht werden. Im Folgenden sollen die Zusammenhänge in Kürze dargestellt werden. Darüber hinaus sollen Diskussionen und Änderungen im Zusammenhang mit der Zulassungsrichtlinie für KDB vorgestellt werden. Der aktuelle Stand der Diskussion im Zusammenhang mit den verwendeten Tensiden in Bezug auf die Spannungsrissprüfung und weiterer Prüfungen wird aufgezeigt. Änderungen der Fremdprüfung von sogenannten Sandschutzmatten, des Standards zur Qualitätsüberwachung (SQÜ) von Kunststoff Dränelementen (KDE) und der Anpassung der Formulierungen zum Überbau der in Abdichtungen verwendeten Produkte werden in Kürze aufgezeigt. T2 - Karlsruher Deponie- und Altlastenseminar 2023 CY - Karlsruhe, Germany DA - 18.10.2023 KW - Deponie KW - Kunststoffdichtungsbahn KW - Spannungsrissbeständigkeit PY - 2023 AN - OPUS4-58634 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR T1 - Amts- und Mitteilungsblatt, Band 52, Heft 3 T3 - Amts- und Mitteilungsblatt der BAM - 3/2022 KW - Anerkennungen KW - Zulassungen KW - Richtlinien PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-558323 SN - 0340-7551 VL - 52 IS - 3 SP - 159 EP - 404 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-55832 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -