TY - JOUR A1 - Frenzel, Olivia A1 - Westphalen, Tanja A1 - Kaminski, Katja A1 - Kluge, Stephanie A1 - Bücker, Michael A1 - Piechotta, Christian T1 - Evaluation and Validation of an Accelerated Weathering Procedure to Characterise the Release of Bisphenol A from Polycarbonate Under Exposure to Simulated Environmental Conditions N2 - Bisphenol A (BPA) has been listed as a substance of very high concern (SVHC) due to its endocrine-disrupting properties according to REACH in 2017. European competent authorities have prepared a REACH restriction proposal to reduce BPA levels in the environment. The proposed limit for the concentration of free BPA and other bisphenols in articles is 10 mg kg−1. If exceeded, migration testing can demonstrate that no more than 0.04 mg L−1 is released from the product or material over its lifetime. German authorities are drafting a new restriction proposal after the original was temporarily withdrawn. The residual and migration limits mentioned above were key requirements from the previous restriction proposal. Numerous national and international standards exist for assessing how environmental factors affect the physical and chemical properties of products and materials—such as notch impact strength and tensile strength—but these standards do not cover the release of pollutants. A standardised procedure that covers all aspects of artificial weathering and monitors the subsequent release of pollutants is necessary, especially in the context of the regulation of these substances. An accelerated weathering procedure was established for non-protected samples. This material was not intended for outdoor applications. The testing procedure applied a typical weathering scenario that represents Central European climate conditions. The procedure was validated and applied to samples under distinct quality assurance aspects. Released BPA is quantified via an organic isotope dilution LC-MS/MS method. In parallel, identical samples were weathered outdoors on a weathering rack. Haze and yellowness index are measured to compare outdoor and weathering chamber results. KW - Artificial weathering KW - Polycarbonate KW - Bisphenol A KW - Simulated environmental conditions PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-645020 DO - https://doi.org/10.3390/app151910361 SN - 2076-3417 VL - 15 IS - 19 SP - 1 EP - 15 PB - MDPI AG AN - OPUS4-64502 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bandow, N. A1 - Aitken, M. D. A1 - Geburtig, Anja A1 - Kalbe, Ute A1 - Piechotta, Christian A1 - Schoknecht, Ute A1 - Simon, Franz-Georg A1 - Stephan, Ina T1 - Using Environmental Simulations to Test the Release of Hazardous Substances from Polymer-Based Products: Are Realism and Pragmatism Mutually Exclusive Objectives? N2 - The potential release of hazardous substances from polymer-based products is currently in the focus of environmental policy. Environmental simulations are applied to expose such products to selected aging conditions and to investigate release processes. Commonly applied aging exposure types such as solar and UV radiation in combination with water contact, corrosive gases, and soil contact as well as expected general effects on polymers and additional ingredients of polymer-based products are described. The release of substances is based on mass-transfer processes to the material surfaces. Experimental approaches to investigate transport processes that are caused by water contact are presented. For tailoring the tests, relevant aging exposure types and release quantification methods must be combined appropriately. Several studies on the release of hazardous substances such as metals, polyaromatic hydrocarbons, flame retardants, antioxidants, and carbon nanotubes from polymers are summarized exemplarily. Differences between natural and artificial exposure tests are discussed and demonstrated for the release of flame retardants from several polymers and for biocides from paints. Requirements and limitations to apply results from short-term artificial environmental exposure tests to predict long-term environmental behavior of polymers are presented. KW - Environmental simulations KW - Polymer-based products KW - Artificial weathering KW - Degradation KW - Leaching KW - Soil contact PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509310 DO - https://doi.org/10.3390/ma13122709 SN - 1996-1944 VL - 13 IS - 12 SP - Paper 2709, 22 PB - MDPI CY - Basel, Switzerland AN - OPUS4-50931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -