TY - JOUR A1 - Scholz, Philipp A1 - Falkenhagen, Jana A1 - Wachtendorf, Volker A1 - Brüll, Robert A1 - Simon, Franz-Georg T1 - Investigation on the Durability of a Polypropylene Geotextile under Artificial Aging Scenarios JF - Sustainability N2 - Geosynthetics are widely used in various civil engineering applications, such as geotextiles in coastal protection, and display a sustainable alternative to natural mineral materials. However, the full benefits of using geosynthetics can only be gained with a long service lifetime of the products. With the use of added stabilizers to the polymers, service lifetimes can be achieved in the range of 100 years. Therefore, accelerated aging methods are needed for the assessment of the long-term performance of geotextiles. In the present study, the behavior of geosynthetic materials made of polypropylene was investigated under artificial aging conditions involving elevated temperatures ranging from 30 to 80 °C, increased oxygen pressures ranging from 10 to 50 bar in water-filled autoclaves, and UV irradiation under atmospheric conditions. ATR-IR spectroscopy was employed to detect the increase in the carbonyl index over various aging durations, indicating the oxidative degradation of the geotextile. The most pronounced increase was observed in the case of aging through UV irradiation, followed by thermal aging. Elevated pressure, on the other hand, had a lower impact on oxidation. High-temperature size exclusion chromatography was utilized to follow the reduction in molar mass under different degradation conditions, and the results were consistent with those obtained from ATR-IR spectroscopy. In polyolefins such as polypropylene, Hindered Amine Stabilizers (HAS) are used to suppress oxidation caused by UV radiation. The quantitative analysis of HAS was carried out using a UV/Vis method and HPLC. The degradation of UV stabilizers during the aging of geotextiles is responsible for the oxidation and the reduction in the molar mass of polypropylene. From the results, it can be concluded that applications of PP geotextile without soil or sand cover might cause the risk of the formation of microplastic particles. Material selection, design, and maintenance of the construction must follow best practices, including the system’s removal or replacement at end-of-life. Otherwise, a sustainable use of geotextiles in civil engineering is not possible. KW - Geotextiles KW - Microplastic KW - Size exclusion chromatography KW - Accelerated aging PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599739 DO - https://doi.org/10.3390/su16093559 SN - 2071-1050 VL - 16 IS - 9 SP - 1 EP - 15 PB - MDPI AG CY - Basel AN - OPUS4-59973 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schoknecht, Ute A1 - Mathies, Helena A1 - Lisec, Jan T1 - Leaching and transformation of film preservatives in paints induced by combined exposure to ultraviolet radiation and water contact under controlled laboratory conditions JF - Water N2 - Stormwater from urban areas can transport biocidally active substances and related transformation products from buildings into the environment. The occurrence of these substances in urban runoff depends on the availability of water, and on ultraviolet radiation exposure that causes photolytic reactions. In a systematic laboratory study, painted test specimens were exposed to either ultraviolet radiation, water contact, or a combination of both. Leaching of the biocidally active substances carbendazim, diuron, octylisothiazolinone, terbutryn, and selected transformation products of terbutryn and diuron were observed under various exposure conditions. Remaining concentrations of these substances in the paint were quantified. It was demonstrated that the distribution of active substances and transformation products in eluates and in the coatings themselves differs with exposure conditions. Strategies for environmental monitoring of biocide emissions need to consider the most relevant transformation products. However, environmental concentrations of biocidally active substances and transformation products depend on earlier exposure conditions. As a consequence, monitoring data cannot describe emission processes and predict expected leaching of biocidally active substances from buildings if the data are collected only occasionally. KW - Substance release KW - Construction products KW - Biocides KW - Transformation KW - UV radiation KW - Water contact PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532114 DO - https://doi.org/10.3390/w13172390 SN - 2073-4441 VL - 13 IS - 17 SP - 1 EP - 16 PB - MDPI CY - Basel AN - OPUS4-53211 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blasenbauer, D. A1 - Huber, F. A1 - Lederer, J. A1 - Quina, M. A1 - Blanc-Biscarat, D. A1 - Bogush, A. A1 - Bontempi, E. A1 - Blondeau, J. A1 - Chimenos, J. A1 - Dahlbo, H. A1 - Fagerqvist, J. A1 - Giro-Paloma, J. A1 - Hjelmar, O. A1 - Hyks, J. A1 - Keaney, J. A1 - Lupsea-Toader, M. A1 - O’Caollai, C. A1 - Orupõld, K. A1 - Pajak, T. A1 - Simon, Franz-Georg A1 - Svecova, L. A1 - Syc, M. A1 - Uvang, R. A1 - Vaajasaari, K. A1 - van Caneghem, J. A1 - van Zomeren, A. A1 - Vasarevičius, S. A1 - Wégner, K. A1 - Fellner, J. T1 - Legal situation and current practice of waste incineration bottom ash utilisation in Europe JF - Waste Management N2 - Almost 500 municipal solid waste incineration plants in the EU, Norway and Switzerland generate about 17.6 Mt/a of incinerator bottom ash (IBA). IBA contains minerals and metals. Metals are mostly separated and sold to the scrap market and minerals are either disposed of in landfills or utilised in the construction sector. Since there is no uniform regulation for IBA utilisation at EU level, countries developed own rules with varying requirements for utilisation. As a result from a cooperation network between European experts an up-to-date overview of documents regulating IBA utilisation is presented. Furthermore, this work highlights the different requirements that have to be considered. Overall, 51 different parameters for the total content and 36 different parameters for the emission by leaching are defined. An analysis of the defined parameter reveals that leaching parameters are significantly more to be considered compared to total content parameters. In order to assess the leaching behaviour nine different leaching tests, including batch tests, up-flow percolation tests and one diffusion test (monolithic materials) are in place. A further discussion of leaching parameters showed that certain countries took over limit values initially defined for landfills for inert waste and adopted them for IBA utilisation. The overall utilisation rate of IBA in construction works is approximately 54 wt%. It is revealed that the rate of utilisation does not necessarily depend on how well regulated IBA utilisation is, but rather seems to be a result of political commitment for IBA recycling and economically interesting circumstances. KW - Bottom ash KW - Leaching tests KW - Utilisation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-500161 DO - https://doi.org/10.1016/j.wasman.2019.11.031 SN - 0956-053X VL - 102 SP - 868 EP - 883 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-50016 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vogel, Christian A1 - Roesch, Philipp A1 - Wittwer, Philipp A1 - Piechotta, Christian A1 - Lisec, Jan A1 - Sommerfeld, Thomas A1 - Kluge, Stephanie A1 - Herzel, Hannes A1 - Huthwelker, T. A1 - Borca, C. A1 - Simon, Franz-Georg T1 - Levels of per- and polyfluoroalkyl substances (PFAS) in various wastewater-derived fertilizers – analytical investigations from different perspectives JF - Environmental Science: Advances N2 - Solid wastewater-based fertilizers were screened for per- and polyfluoroalkyl substances (PFAS) by the extractable organic fluorine (EOF) sum parameter method. The EOF values for ten sewage sludges from Germany and Switzerland range from 154 to 7209 mg kg−1. For thermal treated sewage sludge and struvite the EOF were lower with values up to 121 mg kg−1. Moreover, the application of PFAS targeted and suspect screening analysis of selected sewage sludge samples showed that only a small part of the EOF sum parameter values can be explained by the usually screened legacy PFAS. The hitherto unknown part of EOF sum parameter contains also fluorinated pesticides, pharmaceutical and aromatic compounds. Because these partly fluorinated compounds can degrade to (ultra-)short PFAS in wastewater treatment plants they should be considered as significant sources of organic fluorine in the environment. The combined results of sum parameter analysis and suspect screening reveal the need to update current regulations, such as the German fertilizer ordinance, to focus not solely on a few selected PFAS such as perfluorooctane sulfonic acid (PFOS) and perfluorooctanoic acid (PFOA) but consider an additional sum parameter approach as a more holistic alternative. Moreover, diffusion gradient in thin-films (DGT) passive samplers were utilized as an alternative simplified extraction method for PFAS in solid wastewater-based fertilizers and subsequently quantified via combustion ion chromatography. However, the DGT method was less sensitive and only comparable to the EOF values of the fertilizers in samples with >150 mg kg−1, because of different diffusion properties for various PFAS, but also kinetic exchange limitations. KW - Combustion Ion Chromatography KW - Per- and Polyfluoroalkyl substances (PFAS) KW - Sewage sludge KW - Fertilizer PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-583429 DO - https://doi.org/10.1039/d3va00178d VL - 2 IS - 10 SP - 1436 EP - 1445 PB - Royal Society of Chemistry (RSC) AN - OPUS4-58342 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bruno, M. A1 - Abis, M. A1 - Simon, Franz-Georg A1 - Grönholm, R. A1 - Hoppe, M. A1 - Fiore, S. T1 - Material flow, economic and environmental assessment of municipal solid waste incineration bottom ash recycling potential in Europe JF - Journal of Cleaner Production N2 - In 2018 municipal solid waste (MSW) incineration in Europe produced nearly 19 Mt of bottom ash (BA); only 46 %-wt. was treated, often in poorly performing plants, leaving behind 10 Mt of untreated and unrecovered BA, destined to landfill. This work was based on the inventory of BA across Europe, and on the hypothesis to achieve complete BA valorisation through two assumptions: treating 100% BA and minimizing the loss of valuable fractions due to technical limitations of state-of-the-art processes in comparison to advanced innovative processes. The research involved three phases: characterization of potential secondary raw materials (metals and mineral fraction) currently lost from untreated (the surplus compared to treatment capacity) and unrecovered BA (the fine fraction) through material flow analysis; environmental assessment (energy balance and net GHG emissions) of complete BA valorisation; investigation of the economic feasibility of complete BA Valorisation through state-of-the-art technologies. The resulting 2.14 Mt loss of valuable materials included 1 Mt Mineral fraction and 0.97 Mt ferrous metals, mostly from untreated BA, and 0.18 Mt non-ferrous metals, mostly from unrecovered BA. The energy balance and GHGs emissions required by the treatment of the currently untreated and unrecovered fractions of BA resulted in energy and GHGs emissions savings. Economic profitability was driven by iron and copper recycling and avoided landfill fees. Profitability was achieved by two thirds of considered countries (average values: NPV 83 M€, ROI 20%, payback time 11 years) with BA mass flow exceeding 0.02 Mt. KW - Bottom ash KW - Circular Economy KW - Thermal treatment PY - 2021 DO - https://doi.org/10.1016/j.jclepro.2021.128511 SN - 0959-6526 VL - 317 SP - 1 EP - 13 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-53051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Simon, Franz-Georg A1 - Kalbe, Ute T1 - Measurement of the Environmental Impact of Materials JF - Materials N2 - This Special Issue, ‘Measurement of the Environmental Impact of Materials’, is focused on the impact that materials have on the environmental compartments of soil, water and air. Leaching and emission processes, including underlying mechanisms, are a recurring topic in most published articles in the present Special Issue. Contributions have come from three continents and numerous countries (USA, Germany, France, Latvia, Poland, Russia, Japan, Korea and Thailand) indicating the global dimension of the subject. KW - Leaching KW - Recycling KW - Nano-materials PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-545099 DO - https://doi.org/10.3390/ma15062208 SN - 1996-1944 VL - 15 IS - 6 SP - 1 EP - 3 PB - MDPI CY - Basel AN - OPUS4-54509 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Syc, M. A1 - Simon, Franz-Georg A1 - Hyks, J. A1 - Braga, R. A1 - Biganzoli, L. A1 - Costa, G. A1 - Funari, V. A1 - Grosso, M. T1 - Metal recovery from incineration bottom ash: state-of-the-art and recent developments JF - Journal of Hazardous Materials N2 - Municipal solid waste incineration (MSWI) is one of the leading technologies for municipal solid waste (MSW) treatment in Europe. Incineration bottom ash (IBA) is the main solid residue from MSWI, and its annual European production is about 20 million tons. The composition of IBA depends on the composition of the incinerated waste; therefore, it may contain significant amounts of ferrous and non-ferrous (NFe) metals as well as glass that can be recovered. Technologies for NFe metals recovery have emerged in IBA treatment since the 1990s and became common practice in many developed countries. Although the principles and used apparatus are nearly the same in all treatment trains, the differences in technological approaches to recovery of valuable components from IBA – with a special focus on NFe metals recovery – are summarized in this paper. KW - Bottom ash KW - Metal recovery KW - Waste-to-energy KW - Non-ferrous metals KW - Iron scrap PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-504927 DO - https://doi.org/10.1016/j.jhazmat.2020.122433 SN - 0304-3894 VL - 393 SP - 122433 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-50492 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vogel, Christian A1 - Helfenstein, J. A1 - Massey, M. A1 - Sekine, R. A1 - Kretzschmar, R. A1 - Beiping, L. A1 - Peter, T. A1 - Chadwick, O. A1 - Tamburini, F. A1 - Rivard, C. A1 - Herzel, Hannes A1 - Adam, Christian A1 - Pradas del Real, A. A1 - Castillo-Michel, H. A1 - Zuin, L. A1 - Wang, D. A1 - Félix, R. A1 - Lassalle-Kaiser, B. A1 - Frossard, E. T1 - Microspectroscopy reveals dust-derived apatite grains in acidic, highly-weathered Hawaiian soils JF - Geoderma N2 - Dust deposition is an important source of phosphorus (P) to many ecosystems. However, there is little evidence of dust-derived P-containing minerals in soils. Here we studied P forms along a well-described climatic Gradient on Hawaii, which is also a dust deposition gradient. Soil mineralogy and soil P forms from six sites along the climatic gradient were analyzed with bulk (X-ray diffraction and P K-edge X-ray absorption near edge structure) and microscale (X-ray fluorescence, P K-edge X-ray absorption near edge structure, and Raman) analysis methods. In the wettest soils, apatite grains ranging from 5 to 30 μm in size were co-located at the micro-scale with quartz, a known continental dust indicator suggesting recent atmospheric deposition. In addition to co-location with quartz, further evidence of dust-derived P included backward trajectory modeling indicating that dust particles could be brought to Hawaii from the major global dust-loading areas in central Asia and northern Africa. Although it is not certain whether the individual observed apatite grains were derived from long-distance transport of dust, or from local dust sources such as volcanic ash or windblown fertilizer, these observations offer direct evidence that P-containing minerals have reached surface layers of highly-weathered grassland soils through atmospheric deposition. KW - Phosphorus KW - soil KW - microspectroscopy KW - Raman spectroscopy KW - XANES spectroscopy KW - x-ray diffraction PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-511522 DO - https://doi.org/10.1016/j.geoderma.2020.114681 SN - 0166-0918 SN - 1872-6259 VL - 381 SP - 114681-1 EP - 114681-11 PB - Elsevier CY - Amsterdam AN - OPUS4-51152 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hodgkinson, I. A1 - Maletz, R. A1 - Simon, Franz-Georg A1 - Dornack, C. T1 - Mini-review of waste-to-energy related air pollution and their limit value regulations in an international comparison JF - Waste Management & Research N2 - The concept of circular economy supports mitigation of climate change and other environmental pressures to the planet. Circulating materials in anthropogenic processes come with the risk of accumulating hazardous substances and compounds. In this concept, waste incineration or waste-to-energy (WtE) is a necessary technology to remove these compounds from the life cycle. In this mini-review, contaminants of major importance in the flue gas from waste incineration plants and their environmental impact are discussed. Air pollution of WtE is often seen as the most relevant environmental impact of this treatment option. The emission values parameter set for different countries is presented and compared. The most stringent legally set of emission values could be found in parts of Europe and South Korea. Japan also permits similar strict values when authorising individual incineration plants. In North America, the values are partially less strict as the best available technologies in Europe suggest being possible. Emerging economies, such as India and China, have shown efforts to improve their environmental protection standards but still have room to improve. This could be set in relation to other industrial emitting processes and therefore could be used to assess the relevance of this industry sector to the national emission inventories. KW - Waste incineration KW - Waste-to-energy KW - Limit values KW - Regulation KW - Emission KW - Air pollution control PY - 2021 DO - https://doi.org/10.1177/0734242X211060607 SN - 0734-242X SN - 1096-3669 VL - 40 IS - 7 SP - 849 EP - 858 PB - Sage Publishing CY - London AN - OPUS4-53858 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zweigle, J. A1 - Capitain, C. A1 - Simon, Fabian Michael A1 - Roesch, Philipp A1 - Bugsel, B. A1 - Zwiener, C. T1 - Non-extractable PFAS in functional textiles − Characterization by complementary methods: oxidation, hydrolysis, and fluorine sum parameters JF - Environmental Science: Processes & Impacts N2 - Per- and polyfluoroalkyl substances (PFAS) are widely used for durable water-repellent finishing of different fabrics and textiles like outdoor clothing, carpets, medical textiles and more. Existing PFAS extraction techniques followed by target analysis are often insufficient in detecting widely used side-chain fluorinated polymers (SFPs) that are barely or non-extractable. SFPs are typically copolymers consisting of a non-fluorinated backbone with perfluoroalkyl side-chains to obtain desired properties. We compared the accessible analytical information and performance of complementary techniques based on oxidation (dTOP assay, PhotoTOP), hydrolysis (THP assay), standard extraction, extractable organic fluorine (EOF), and total fluorine (TF) with five functional textiles and characterized 7 further textiles only by PhotoTOP oxidation. The results show that when applied directly to textile samples, oxidation by dTOP and PhotoTOP and also hydrolysis by the THP are able to capture large fractions of the TF in form of perfluoroalkyl side-chains present in the textiles while methods relying on extracts (EOF, target and non-target analysis) were much lower (e.g., factor ~25-50 lower). The conversion of large fractions of the measured TF into PFCAs or FTOHs from fluorinated side chains is in contrast to previous studies. Concentrations ranged from