TY - GEN A1 - Bradley, Ian A1 - Otremba, Frank A1 - Scarponi, G. E. A1 - Romero-Navarrete, José A. ED - Ao, S.-I. ED - Kim, H. K. ED - Amouzegar, M. A. T1 - Boiling and thermohydraulics within pressure vessels N2 - Exposure of pressure vessels to fire can result in catastrophic explosion and escalation of accidents. The safe transportation of cargo in pressure vessels therefore requires knowledge of what will happen to the cargo in the event of a vehicle derailment or rollover resulting in fire exposure. The chapter presents an overview of selected testing and modelling work undertaken to understand the thermohydraulic processes within a vessel that drive pressurization during fire. A series of experiments highlighting the importance of adequate design and selection of protection systems are summarized. It is concluded that pressure relief alone is typically insufficient to prevent vessel rupture, but the combination of relief and thermal coatings can be effective. KW - BLEVE KW - Explosion KW - LPG KW - PIV KW - Pressure vessel KW - Thermohydraulics PY - 2020 SN - 978-981-15-6847-3 SN - 978-981-15-6848-0 U6 - https://doi.org/https://doi.org/10.1007/978-981-15-6848-0_13 SP - 158 EP - 172 PB - Springer Nature CY - Singapore AN - OPUS4-51138 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Zaghdoudi, M. A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar ED - Altenbach, H. ED - Hitzler, L. ED - Johlitz, M. ED - Merkel, M. ED - Öchsner, A. T1 - Analysis of Heterogeneous Ageing of HNBR O-Rings N2 - Abstract Hydrogenated nitrile butadiene rubber (HNBR) elastomer was thermo-oxidatively aged at different temperatures up to 150 °C. Fourier transform infrared spectroscopy (FTIR), compression stress relaxation (CSR) and international rubber hardness degree (IRHD) microhardness were used to characterise the chemo-mechanical changes of HNBR O-rings during thermo-oxidative ageing. FTIR shows the development of carbonyl, methyl and ester groups but the nitrile content was not affected by ageing. The effect of sample geometry during CSR was investigated. CSR data were converted through integrated kinetic laws. The conversion has proven its sensibility to detect heterogeneous ageing. This was confirmed by the IRHD measure-ments across the section of O-rings. The influence of compression during ageing was assessed through IRHD measurements across the section of compressed and uncom-pressed aged O-rings. The DLO effect was more pronounced in compressed O-rings. By applying the model of Wise et al., theoretical IRHD and oxidation profiles were determined on the basis of IRHD experimental data of compressed O-rings. Good agreements between the experimental and the theoretical IRHD profiles in the core region were obtained. However, near the edge, the theoretical IRHD values were overestimated. KW - Ageing KW - Rubber seals KW - Stress relaxation KW - Modelling PY - 2024 SN - 978-3-031-49042-2 U6 - https://doi.org/10.1007/978-3-031-49043-9 SN - 1869-8433 SP - 331 EP - 348 PB - Springer Nature CY - Cham, Switzerland AN - OPUS4-59769 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Goral, Milan A1 - Kömmling, Anja A1 - Probst, Ulrich A1 - Wossidlo, Peter A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Völzke, Holger T1 - Langzeitversuche über 10 Jahre an Federkern-Metalldichtungen mit Aluminium- bzw. Silberummantelungen N2 - Federunterstützte Metalldichtungen mit Aluminium(Al)- oder Silber(Ag)-Ummantelung werden u.a. in Behältern für Wärme entwickelnde radioaktive Abfälle eingesetzt, da diese Dichtungen eine sehr gute Dichtheit gewährleisten sowie Langlebigkeit und Beständigkeit gegenüber erhöhten Temperaturen und radioaktiver Strahlung aufweisen. Auch wenn die Sicherheit solcher Behälter und der verwendeten Dichtungen vielfach belegt wurde, sind sie Gegenstand andauernder Forschung, etwa im Hinblick auf eine absehbar benötigte verlängerte Zwischenlagerdauer. Aus diesem Grund werden an der Bundesanstalt für Materialforschung und -prüfung (BAM) im Fachbereich 3.4 „Sicherheit von Lagerbehältern“ seit über 20 Jahren Versuche an solchen Metalldichtungen durchgeführt. Dabei sollen zusätzliche Erkenntnisse hinsichtlich der Sicherheitsreserven der Dichtungen in unterstellten Störfallszenarien (axiale Bewegung des Deckelsystems bzw. Aufweitung der Nutgeometrie) und insbesondere detailliertere Erkenntnisse zum Langzeitverhalten gewonnen werden. KW - Federunterstützte Metalldichtungen KW - Transport- und Lagerbehälter für radioaktive Stoffe KW - Langzeitversuche KW - Alterung KW - Dichtheit KW - Leckagerate KW - Helium-Dichtheitsprüfung PY - 2023 VL - 2023 SP - 43 EP - 63 PB - ISGATEC GmbH CY - Mannheim AN - OPUS4-56399 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -