TY - JOUR A1 - Scheibe, Maximilian A1 - Binkowski, Sigrid A1 - Benemann, Sigrid A1 - Saliwan Neumann, Romeo T1 - Comparing different preparation techniques for the characterisation of niobium carbides N2 - Of the up to 85.000 tons of niobium that are produced at the present, 90% are used as a property defining micro alloying element [1,2] in: a. High- and highest strength alloys for car bodies, b. Structural steels in the construction industry and, c. Steels for pipelines and the petrochemical industry, whereby it is mostly added for alloying in the ränge of 80-250 ppm. PY - 2014 IS - 19 SP - 1 EP - 12 AN - OPUS4-32432 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nolze, Gert A1 - Wagner, G. A1 - Saliwan Neumann, Romeo A1 - Skála, R. A1 - Geist, V. T1 - Investigation of the orientation relationships of carlsbergite in the North Chile iron meteorite KW - Orientation realtionships KW - CrN KW - (Fe,Ni)3P PY - 2005 SN - 1086-9379 SN - 0026-1114 SP - 14 pages PB - Allen Press CY - Lawrence, Kan. AN - OPUS4-7592 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kianinejad, Kaveh A1 - Darvishi Kamachali, Reza A1 - Khedkar, Abhinav A1 - Manzoni, Anna Maria A1 - Agudo Jácome, Leonardo A1 - Schriever, Sina A1 - Saliwan Neumann, Romeo A1 - Megahed, Sandra A1 - Heinze, Christoph A1 - Kamrani, Sepideh A1 - Fedelich, Bernard T1 - Creep anisotropy of additively manufactured Inconel-738LC: Combined experiments and microstructure-based modeling N2 - The current lack of quantitative knowledge on processing-microstructure–property relationships is one of the major bottlenecks in today’s rapidly expanding field of additive manufacturing. This is centrally rooted in the nature of the processing, leading to complex microstructural features. Experimentally-guided modeling can offer reliable solutions for the safe application of additively manufactured materials. In this work, we combine a set of systematic experiments and modeling to address creep anisotropy and its correlation with microstructural characteristics in laser-based powder bed fusion (PBF-LB/M) additively manufactured Inconel-738LC (IN738LC). Three sample orientations (with the tensile axis parallel, perpendicular, and 45° tilted, relative to the building direction) are crept at 850 °C, accompanied by electron backscatter secondary diffraction (EBSD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) investigations. A crystal plasticity (CP) model for Ni-base superalloys, capable of modeling different types of slip systems, is developed and combined with various polycrystalline representative volume elements (RVEs) built on the experimental measurements. Besides our experiments, we verify our modeling framework on electron beam powder bed fusion (PBF-EB/M) additively manufactured Inconel-738LC. The results of our simulations show that while the crystallographic texture alone cannot explain the observed creep anisotropy, the superlattice extrinsic stacking faults (SESF) and related microtwinning slip systems play major roles as active deformation mechanisms. We confirm this using TEM investigations, revealing evidence of SESFs in crept specimens. We also show that the elongated grain morphology can result in higher creep rates, especially in the specimens with a tilted tensile axis. KW - Additive manufactured Ni-base superalloys KW - Creep KW - Crystal plasticity KW - Superlattice extrinsic stacking faults PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601576 DO - https://doi.org/10.1016/j.msea.2024.146690 SN - 0921-5093 VL - 907 SP - 1 EP - 16 PB - Elsevier B.V. AN - OPUS4-60157 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nolze, Gert A1 - Saliwan Neumann, Romeo A1 - Buchheim, Michaela T1 - Microstructure investigations of iron meteorites by EBSD and EDS analyses N2 - Meteorites are a unique and inspiring material for microstructural studies because if their very specific genesis. Iron meteorites have been formed under unimaginable cooling rates of a few ten Kelvins per million years so that the observable transformation of the formerly huge Fe-Ni single crystals of taenite occurred under nearly-equilibrium conditions. Octahedrites (meteorites having a Ni content between 6...15%) are characterized by ribbons of the low-temperature Fe-Ni phase kamacite separated by rims of residual taenite. This very specific feature is known as Widmanstaetten structure and has been investigated by synchrotron radiation in order to cover a higher volume fraction for a statistically relevant description of orientation relationships. However, plessite – a microstructure mainly consisting of the same phases – reflects the orientation relationship between kamacite and taenite as well. For their characterization, a scanning electron microscope is very suitable in order to investigate crystal orientations or identify phases. Despite the apparently ideal formation circumstances of iron meteorites, Ni concentration profiles prove non-equilibrium conditions. Combined EDS (energy dispersive spectroscopy) and EBSD (electron backscatter diffraction) measurements at a selected plessitic region of the Cape York iron shows that a correlation exists between Ni-concentration and the locally detected orientation relationship. T2 - 15th European Microscopy Congress CY - Manchester, UK DA - 16.09.2012 KW - Phase identification KW - Corrosion KW - Chloride KW - Dermbach PY - 2012 SP - 90 AN - OPUS4-37775 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Engelhardt, Monika A1 - Gesatzke, Wolfgang A1 - Österle, Werner A1 - Müller, Urs A1 - Rooch, Heidemarie A1 - Saliwan Neumann, Romeo A1 - Urban, Ingrid T1 - Makro- und Mikrogefüge von Bremsbelägen KW - Bremsbelag KW - Polymermatrix-Verbundstoff KW - Röntgenfluoreszenzanalyse KW - REM KW - FIB KW - TEM PY - 2005 SN - 3-88355-343-3 SN - 0343-3579 N1 - Serientitel: Sonderbände der praktischen Metallographie – Series title: Sonderbände der praktischen Metallographie IS - 37 SP - 105 EP - 110 PB - Werkstoff-Informationsges. CY - Frankfurt AN - OPUS4-10996 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. I. A1 - Link, T. A1 - Nolze, Gert A1 - Svetlov, I. L. A1 - Bokshtein, B. S. A1 - Rodin, A. O. A1 - Saliwan Neumann, Romeo A1 - Oder, Gabriele T1 - Diffusion processes in multicomponent nickel-base superalloy-nickel system N2 - Optical and scanning electron microscopy, as well as electron microprobe analysis and electron backscatter diffraction, have been used to study diffusion processes that occur in a diffusion pair that consistsof a single-crystal CMSX-10 nickel-base superalloy and polycrystalline nickel, at temperatures of 1050–1250°C. It has been found that, in this system, the distributions of γ-stabilizing elements (Cr, Co, W, and Re) are described by the Boltzmann solution for diffusion between two semiinfinite plates of a binary alloy. The processing of these distributions has shown that the diffusion coefficients of Cr, Co, W, and Re in the multicomponent system are close to those in binary alloys of these elements with Ni. The diffusion redistribution of the elements leads to the dissolution of the γ′ phase in the nickel-base superalloy, growth of nickel grains toward the superalloy constituent of the diffusion pair, and the formation of porosity on both sides of the migrating interface, which is determined from a crystal misorientation of the alloy single crystal and nickel grains. KW - Ni-base superalloy KW - Interface KW - Diffusion KW - Phase transformation KW - Porosity PY - 2014 SN - 0031-918X VL - 115 IS - 1 SP - 21 EP - 29 AN - OPUS4-37980 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mosquera Feijoo, Maria A1 - Oder, Gabriele A1 - Saliwan Neumann, Romeo A1 - Buchheim, Michaela A1 - Kranzmann, Axel A1 - Olbricht, Jürgen T1 - Impact of Sample Geometry and Surface Finish on VM12‑SHC Ferritic–Martensitic Steel Under Cyclic Steam Atmosphere Operating Conditions N2 - The steam side oxidation of ferritic–martensitic VM12-SHC steel was investigated under thermo-cyclic conditions in water steam at 620/320 °C and 30 bar with a focus on assessing the influence of pre-oxidation time, specimen geometry and surface finish. The specimens were pre-oxidized under isothermal conditions in water steam at 620 °C and 30 bar for 500 h or 1500 h. After pre-oxidation treatment, all specimens were subjected up to 258 thermal cycles. Three different geometries—rectangular coupons, U-shaped ring segments and ring samples—were investigated to evaluate the influence of open/closed shape, and flat/curved surface on corrosion rate. At the same time, two types of surface finish were considered: “as received” and “ground.” The formation of a protective scale by pre-oxidation was investigated. EBSD and ESMA analyses revealed that the Cr-content of the alloy appeared to be insufficient for obtaining a protective oxide scale under studied conditions, at the same time the anayses confirmed that initial oxidation depends on presence of minor alloying elements as Si and Mn, strong oxide formers which can alter the kinetics and morphology of the corrosion reaction. Moreover, rectangular coupons with small wall thickness and flat surface exhibited the highest corrosion rate, while “ground” curved samples showed only local oxidation. This indicates that for same pre-oxidation time, oxidation kinetics is controlled by curvature. KW - Cyclic steam oxidation KW - 12%Cr steel KW - Specimen geometry KW - Surface treatments PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-551808 DO - https://doi.org/10.1007/s11085-022-10114-6 SN - 0030-770X SP - 1 EP - 18 PB - Springer AN - OPUS4-55180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Epishin, A. A1 - Link, T. A1 - Svetlov, I. L. A1 - Nolze, Gert A1 - Saliwan Neumann, Romeo A1 - Lucas, H. T1 - Mechanism of porosity growth during homogenisation in single crystal nickel-based superalloys N2 - Several mechanisms for porosity growth in single crystal nickel-based superalloys during homogenisation heat treatment have been proposed in the literature. They were carefully checked using different experimental methods, namely quantitative light microscopy, scanning electron microscopy, transmission electron microscopy, X-ray diffraction and density measurements. It is shown that the main mechanism is the Kirkendall–Frenkel effect, i.e. generation of voids due to uncompensated efflux of Al atoms from dissolving γ/γ′-eutectic areas. The Al diffusion is supported by the afflux of vacancies from surrounding γ-matrix which results in porosity growth. This conclusion is confirmed by the estimation of the vacancy afflux towards the dissolving eutectic. KW - Ni-base superalloy KW - Eutectic KW - Vacancies KW - Porosity PY - 2013 VL - 104 IS - 8 SP - 776 EP - 782 PB - Carl Hanser Verlag AN - OPUS4-37983 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scheibe, Maximilian A1 - Binkowski, Sigrid A1 - Benemann, Sigrid A1 - Saliwan Neumann, Romeo T1 - Vergleich verschiedener Präparationstechniken zur Charakterisierung von Niobcarbiden N2 - 90% von den heute bis zu 85.000 Tonnen gewonnenen Niob gehen als eigenschaftsbestimmendes Mikrolegierungselement ein in: a. hoch- und höchstfeste Karosseriebaulegierungen, b. Strukturstähle im Bauwesen und, c. Pipelinestähle nebst Stählen in der Petrochemie, wobei es dort zumeist in Bereich von 80-250 ppm zulegiert wird. T2 - 14. Internationale Metallographie-Tagung CY - Leoben, Austria DA - 17.09.2014 PY - 2014 SN - 978-3-88355-403-7 N1 - Serientitel: Sonderbände der Praktischen Metallographie / Fortschritte in der Metallographie – Series title: Sonderbände der Praktischen Metallographie / Fortschritte in der Metallographie IS - 46 SP - 51 EP - 58 AN - OPUS4-31484 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kianinejad, Kaveh A1 - Fedelich, Bernard A1 - Darvishi Kamachali, Reza A1 - Schriever, Sina A1 - Manzoni, Anna Maria A1 - Agudo Jácome, Leonardo A1 - Megahed, Sandra A1 - Kamrani, Sepideh A1 - Saliwan Neumann, Romeo T1 - Experimentally informed multiscale creep modelling of additive manufactured Ni-based superalloys N2 - Excellent creep resistance at elevated temperatures, i.e. T / T_m> 0.5, due to γ-γ’ microstructure is one of the main properties of nickel-based superalloys. Due to its great importance for industrial applications, a remarkable amount of research has been devoted to understanding the underlying deformation mechanism in a wide spectrum of temperature and loading conditions. Additive manufactured (AM) nickel-based superalloys while being governed by similar γ-γ’ microstructure, exhibit AM-process specific microstructural characteristics, such as columnar grains, strong crystallographic texture (typically <001> fiber texture parallel to build direction) and compositional inhomogeneity, which in turn leads to anisotropic creep response in both stationary and tertiary phases. Despite the deep insights achieved recently on the correlation between process parameters and the resulting microstructure, the anisotropic creep behavior and corresponding deformation mechanism of these materials are insufficiently understood so far. One reason for this is the lack of capable material models that can link the microstructure to the mechanical behavior. To overcome this challenge, a multiscale microstructure-based approach has been applied by coupling crystal plasticity (CP) and polycrystal model which enables the inclusion of different deformation mechanisms and microstructural characteristics such as crystallographic texture and grain morphology. The method has been applied to experimental data for AM-manufactured INCONEL-738LC (IN738). The effect of different slip systems, texture, and morphology on creep anisotropy at 850°C has been investigated. Results suggest a strong correlation between superlattice extrinsic stacking fault (SESF) and microtwinning and observed creep anisotropy. T2 - EUROMAT 23 CY - Frankfurt a. M., Germany DA - 04.09.2023 KW - IN738LC KW - Creep anisotropy KW - Crystal plasticity PY - 2023 AN - OPUS4-58263 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schulz, Wencke A1 - Feigl, Michael A1 - Dörfel, Ilona A1 - Saliwan Neumann, Romeo A1 - Nofz, Marianne A1 - Kranzmann, Axel T1 - Alumina coatings against carburization and oxidation under oxyfuel conditions T2 - 1st International conference on materials for energy CY - Karlsruhe, Germany DA - 2010-07-04 PY - 2010 SN - 978-3-89746-117-8 SP - 1012 AN - OPUS4-24179 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chandra, Kamlesh A1 - Kranzmann, Axel A1 - Saliwan Neumann, Romeo A1 - Oder, Gabriele A1 - Rizzo, F. T1 - High temperature oxidation behavior of 9-12 % Cr ferritic/martensitic steels in a simulated dry oxyfuel environment N2 - The materials in oxyfuel power plant will be subjected to CO2– and SO2–rich gases on the fireside. The oxidation behaviour of two 9–12 % Cr steels T92 and VM12 was studied under dry oxyfuel environment in the temperature range of 580–650 °C for up to 1,000 h. The oxide structure and morphology were analyzed using various experimental techniques. A complex temperature dependence of oxidation rate is observed for both T92 and VM12 whereby the oxidation rate decreased with increasing temperature. This is attributed to increased Cr-enrichment in the inner scale with increasing temperature. T92 and VM12 alloys are also susceptible to carburization in an oxyfuel environment. KW - Oxyfuel environment KW - Ferritic/martensitic steel KW - Oxidation KW - High temperature corrosion KW - Carburization KW - Steel KW - EPMA KW - SEM PY - 2015 DO - https://doi.org/10.1007/s11085-014-9521-4 SN - 0030-770X SN - 1573-4889 VL - 83 IS - 3-4 SP - 291 EP - 316 PB - Springer CY - New York, NY AN - OPUS4-32737 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Engelking, Lorenz A1 - Madia, Mauro A1 - Schröpfer, Dirk A1 - Kruse, Julius A1 - Saliwan Neumann, Romeo A1 - Kannengießer, Thomas T1 - Influence of Ultrasonic-Assisted Milling on Surface Integrity and Fatigue Strength of a Low Alloy Steel N2 - The milling process significantly influences the surface integrity of metallic components through machining induced near surface residual stresses. Modern hybrid machining processes, such as ultrasonic-assisted milling (USAM), offer the potential to induce beneficial near-surface compressive residual stresses compared to the near-surface tensile residual stresses typically resulting from conventional milling (CM). This study investigates the effects of USAM compared to CM on the near-surface residual stress state and fatigue performance of a S355J2C low-alloy steel. Milling experiments and subsequent rotating bending tests revealed that USAM significantly reduces cutting force by approximately 45% and induces near-surface compressive re sidual stresses as low as −733MPa. This leads to a significant improvement in fatigue strength estimated in approximately 34% compared to polished specimens and 11% compared to the CM. These findings highlight the potential of USAM to enhance the fatigue performance of components made of steel. KW - Fatigue strength KW - Residual stress KW - Surface integrity KW - Surface roughness KW - Ultrasonic-assisted milling PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-657358 DO - https://doi.org/10.1111/ffe.70259 SP - 1 EP - 11 PB - Wiley AN - OPUS4-65735 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -