TY - JOUR A1 - Wäsche, Rolf A1 - Yarim, Rasim A1 - Nicolaides, Dagmar T1 - Influence of Green Compaction on the Sintering Behaviour of SiC-TiC-TiB2 Composites KW - Pressureless sintering KW - SiC KW - TiC KW - TiB2 KW - Green compaction KW - Particle size KW - Microstructure PY - 2004 SN - 1013-9826 VL - 264-268 SP - 213 EP - 218 PB - Trans Tech Publ. CY - Aedermannsdorf AN - OPUS4-12054 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yarim, Rasim A1 - Wäsche, Rolf A1 - Woydt, Mathias A1 - Dörfel, Ilona T1 - Analysis of wear protecting oxide layers in the system SiC-TiC-TiB2 formed in-situ at high temperatures T2 - AIST-BAM Symposium on Materials Surface Technology in Twin Institute Programme CY - Tsukuba, Japan DA - 2003-02-18 PY - 2003 SP - 5 EP - 8 AN - OPUS4-12057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf A1 - Klaffke, Dieter A1 - Steinborn, Gabriele ED - Bartz, Wilfried J. T1 - Tribological investigations on infiltrated zirconia T2 - 15th International colloquium tribology - Automotive and Industrial Lubrication CY - Ostfildern, Germany DA - 2006-01-17 KW - Friction KW - Wear infiltration KW - Zirconia KW - Alcaline earth fluorides PY - 2006 SN - 3-924813-62-0 SP - 1(?) EP - 7(?) CY - Ostfildern AN - OPUS4-12165 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Klaffke, Dieter A1 - Wäsche, Rolf ED - Bartz, Wilfried J. T1 - Tribological Characterisation of ceramics in fretting tests at room temperature T2 - 15th International colloquium tribology - Automotive and Industrial Lubrication CY - Ostfildern, Germany DA - 2006-01-17 KW - Silicon nitride KW - Silicon carbide KW - Composits KW - Friction KW - Wear KW - Fretting PY - 2006 SN - 3-924813-62-0 SP - 1(?) EP - 10(?) CY - Ostfildern AN - OPUS4-12167 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klaffke, Dieter A1 - Wäsche, Rolf A1 - Janakiraman, N. A1 - Aldinger, F. T1 - Tribological characterisation of siliconcarbonitride ceramics derived from preceramic polymers N2 - Amorphous SiCN ceramics were prepared in a laboratory scale as disk shaped specimens with 10 mm diameter and 0.3 mm thickness. The friction and wear behaviour was characterised in gross slip fretting tests under unlubricated conditions at room temperature against steel (100Cr6) and ceramic (Al2O3). Tests with a ball-on-disk contact were performed in laboratory air with different content of water vapour. The results show clearly that the relative humidity has a significant effect on friction and wear behaviour. All tests in dry air lead to higher friction and higher wear rate than in normal air. Improved friction and wear behaviour was observed with increasing pyrolysis temperature up to 1100 °C of the SiCN specimens. This is attributed to increasingly better mechanical properties and higher stiffness of the amorphous network due to the evaporation of gaseous organic species and the formation of free graphite like carbon. KW - Ceramics KW - Preceramic polymer KW - Siliconcarbonitride KW - Friction KW - Wear PY - 2006 DO - https://doi.org/10.1016/j.wear.2005.04.031 SN - 0043-1648 VL - 260 IS - 7-8 SP - 711 EP - 719 PB - Elsevier CY - Amsterdam AN - OPUS4-12302 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Klaffke, Dieter A1 - Steinborn, Gabriele T1 - Tribological testing of Ca-Ba infiltrated zirconia KW - Friction KW - Wear KW - Ca-Ba fluoride KW - Infiltration KW - Porous zirconia PY - 2005 UR - http://www.om.ugal.ro/AnnalsFasc8Tribology/pdf/2005/9-Annals2005-3-Wasche.pdf SN - 1221-4590 SN - 1220-0824 SP - 53 EP - 59 CY - Gala¸ti AN - OPUS4-12365 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Tribological investigations on siliconcarbonitride ceramics derived from preceramic T2 - 14th International Colloquium Tribology CY - Ostfildern, Germany DA - 2004-01-13 PY - 2004 AN - OPUS4-11057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Oscicalling sliding wear behaviour of SiC, TiC, TiB2 59SiC-41TiB2 and 52SiC-24TiC-24TiB2 T2 - 14th International Colloquium Tribology CY - Ostfildern, Germany DA - 2004-01-13 PY - 2004 AN - OPUS4-11062 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kloß, Heinz A1 - Wäsche, Rolf T1 - Analytical approach for wear prediction of metallic and ceramic materials in tribological applications T2 - ECOTRIB 2007 CY - Ljubljana, Slovenia DA - 2007-06-12 KW - Wear KW - Surface temperature KW - Activation energy KW - Simulation KW - Movable cellular automata (MCA) PY - 2007 VL - I SP - 223 EP - 234 PB - Slovenská Akadémia Vied CY - Ljubljana AN - OPUS4-14972 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wäsche, Rolf A1 - Gräber, H.-G. A1 - Klaffke, Dieter T1 - Tribologische Untersuchung zum Verschleißverhalten von keramischen Zahnersatzwerkstoffen KW - Dentalkeramik KW - Bearbeitbarkeit KW - Zwischenmedium KW - pH-Wert KW - Dental ceramic KW - Machinability KW - Liquid media KW - pH-value PY - 2007 SN - 0724-3472 VL - 54 IS - 3 SP - 29 EP - 32 PB - Expert Verlag CY - Renningen AN - OPUS4-15737 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf A1 - Hartelt, Manfred A1 - Springborn, U. A1 - Köster, K. A1 - Bewilogua, K. T1 - Schwingungsverschleiß von Kohlenstoffnitridschichten CNx gegen Aluminiumoxid in Luft T2 - 48. Tribologie-Fachtagung CY - Göttingen, Deutschland DA - 2007-09-24 KW - Schwingungsverschleiß KW - CNx Schichten KW - Magnetronsputtern KW - Reibung KW - Keramik PY - 2007 SN - 978-3-00-022603-8 SP - 27/1 EP - 27/11 CY - Aachen AN - OPUS4-15921 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hartelt, Manfred A1 - Wäsche, Rolf A1 - Djahanbakhsh, Mohammad A1 - Österle, Werner T1 - Vergleich von Standard-Modell- und HIP-Simulator-Untersuchungen an Verschleißschutzschichten für Metall-Keramik-Paarungen bei Endoprothesen T2 - 48. Tribologie-Fachtagung "Reibung, Schmierung und Verschleiß - Forschung und praktische Anwendungen" CY - Göttingen, Deutschland DA - 2007-09-24 KW - Reibung KW - Verschleiß KW - Beschichtung KW - HIP-Simulation PY - 2007 SN - 978-3-00-022603-8 VL - 1 SP - 8/1 EP - 8/10 CY - Aachen AN - OPUS4-16102 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Steinborn, Gabriele A1 - Wäsche, Rolf T1 - Charakterisierung der Dispergiereigenschaften von keramischen nanodispersen Suspensionen mit der Ultraschallspektroskopie N2 - Die Dispergiereigenschaften von verschiedenen nanoskaligen Pulvern mit unterschiedlicher Kornfraktion im Bereich von 10 bis 250 nm werden in verdünnten und konzentrierten keramischen Schlickern mit der Ultraschallspektroskopie untersucht. Alle stabilen Suspensionen weisen im entsprechenden pH-Bereich eine monomodale Partikelgrößenverteilung auf. Durch die Charakterisierung der Suspensionen mit der Ultraschallspektroskopie kann eine verbesserte Bewertung hinsichtlich Homogenität und Agglomeratbildung auch für nanoskalige Pulver erhalten werden. Dies ermöglicht eine bessere Qualitätskontrolle prozessrelevanter Schritte bei der Verarbeitung. KW - Dispergieren KW - Nanopartikel KW - Suspensionen KW - Folie KW - Nanopulver KW - Dispergierung PY - 2007 DO - https://doi.org/10.1002/cite.200600141 SN - 0009-286X SN - 1522-2640 VL - 79 IS - 3 SP - 257 EP - 265 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-16271 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Steinborn, Gabriele A1 - Fritz, Ulrich A1 - Rabe, Torsten A1 - Wäsche, Rolf ED - Kriegesmann, J. T1 - Dispergierung von Nanopulvern in Foliengießschlickern KW - Dispergierung KW - Nanopulver KW - Foliengiessen PY - 2005 SN - 3-87156-091-X IS - Kap. 3.3.3.5 SP - 1 EP - 16 PB - Deutscher Wirtschaftsdienst CY - Köln AN - OPUS4-16272 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Wäsche, Rolf ED - Pohl, M. T1 - Schwingungsverschleißprüfung als Werkzeug für die Werkstoffentwicklung T2 - Tagung "Werkstoffprüfung 2007" CY - Neu-Ulm, Deutschland DA - 2007-11-29 KW - Verschleißfestigkeit KW - Werkstoffentwicklung KW - Keramik KW - Reibungsverhalten KW - Stahl PY - 2007 SN - 978-3-514-00753-6 SP - 299 EP - 304 PB - Verl. Stahleisen CY - Düsseldorf AN - OPUS4-16426 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Urchegui, M.A. A1 - Hartelt, Manfred A1 - Wäsche, Rolf A1 - Gómez, X. T1 - Analysis of different strategies to reduce fretting wear in thin steel roping wires N2 - After having checked in a previous study the influence of stroke and normal load in laboratory fretting tests accomplished with thin steel roping wires, in this paper the effect of the contact pressure (test configuration), environmental conditions (relative humidity) and reduction of the friction coefficient (lubricants) on the wear behaviour were analysed. The wires were 0.45 mm in diameter and the material was a cold-drawn eutectoid carbon steel (0.8% C) with a Tensile Strength over 2800 MPa. The tests were performed on an oscillating test rig and the volumetric wear of both specimens of the tribocouple was determined separately from three-dimensional topographies of the wear scars acquired by means of a confocal profiler, and a calculation algorithm developed in using MATLAB®. The strong effect of humidity and lubrication on wear behaviour was proved, whereas a slight effect of contact pressure was derived. KW - Wires KW - Fretting test KW - Contact pressure PY - 2008 DO - https://doi.org/10.1002/tt.52 SN - 1354-4063 SN - 1557-685X VL - 14 IS - 1 SP - 43 EP - 57 PB - Coppin CY - Deal AN - OPUS4-16677 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Podgursky, V. A1 - Adoberg, E. A1 - Surzenkov, A. A1 - Kimmari, E. A1 - Viljus, M. A1 - Mikli, V. A1 - Hartelt, Manfred A1 - Wäsche, Rolf A1 - Síma, M. A1 - Kulu, P. T1 - Dependence of the friction coefficient on roughness parameters during early stage fretting of (Al,Ti)N coated surfaces N2 - Main focus was on the correlation of the coefficient of friction (COF) with the geometrical parameters of the surface during early stage of the running-in period. TiN, TiAlN and AlTiN coatings were prepared by using rotating cathode arc evaporation unit. The roughness of the WC-Co substrate Ra ranged from 0.05 to 0.2 µm and the coating thickness was 2.3 ± 0.2 µm. Part of the samples were subjected to the surface modification by the drag grinding finishing. Geometrical parameters of the surface were evaluated by means of atomic force microscopy (AFM) and fretting tests were conducted with 10 mm diameter alumina ball under 2 N load, 100 µm slip distance and the frequency of 10 Hz. It was found that the distribution of macroparticles strongly influences the geometrical parameters of the surface and the number of macroparticles increases with increasing Al content in the coating. In the case of the positive skewness Ssq of the coating surface, the kurtosis Sku provides a statistically significant effect on the COF, namely the COF depends inversely on the kurtosis Sku. The kurtosis value for TiN was the highest among as-deposited coatings, subsequently, the slowest increase rate in the COF was observed for the TiN coating. KW - PVD coatings KW - AFM KW - Surface topography KW - COF PY - 2011 DO - https://doi.org/10.1016/j.wear.2011.03.006 SN - 0043-1648 VL - 271 IS - 5-6 SP - 853 EP - 858 PB - Elsevier CY - Amsterdam AN - OPUS4-24497 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Oxidative wear in gross slip fretting of thin steel wires T2 - ITC Hiroshima Satellite Symposium, Tribochemistry Hagi 2011 CY - Hagi, Japan DA - 2011-10-25 PY - 2011 AN - OPUS4-24609 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - The history of the Stribeck curve and the role of Adolf Martens T2 - Int. Tribology Congress / ITC Hiroshima CY - Hiroshima, Japan DA - 2011-10-30 PY - 2011 AN - OPUS4-24610 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Alumina and zirconia as tribomaterials - a review T2 - The Fourth International Conference on The Characterization and Control of Interfaces for High Quality Advanced Materials (ICCCI 2012) CY - Kurashiki, Japan DA - 2012-09-02 PY - 2012 AN - OPUS4-24612 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hartelt, Manfred A1 - Wäsche, Rolf T1 - Verschleißuntersuchungen an Dental-Implantat-Werkstoffen unter partial slip Bedingungen N2 - Im Vortrag wird neben der apparativen Prüftechnik das allgemeine methodische Vorgehen für Modell-Verschleißuntersuchungen im Bereich des partial slip vorgestellt. Im Detail wird für Dental-Implantat-Werkstoffe eine Rangfolge aufgestellt, die vergleichend die Verschleißresistenz unterschiedlicher Ti-basierter Werkstoffe zeigt. Wird durch die Kaubewegung eine mehrachsige Beanspruchung in die Kontaktflächen der Schraubverbindung eingeleitet, kann durch partial slip im Randbereich dieser Kontaktfläche ein Verschleißprozess initiiert werden, der die Lockerung des Implantats begünstigt. Eine gute Verschleißresistenz verhindert oder schiebt die vorzeitige Lockerung hinaus. Um das Werkstoffverhalten in Bezug auf eine vorzeitige Lockerung der Implantatkrone bei geschraubten zweiteiligen Implantaten zu charakterisieren, wurden zylindrische Probekörper unter partial slip Fretting-Bedingungen mit Zyklenzahlen bis n = 200 000 beansprucht. Die Frequenz der aufgebrachten Tangentialkraft betrug 2 Hz, um die Kaubewegung zu simulieren. Die tribologischen Untersuchungen wurden auf einem Eigenbau-Tribometer mit der Kontaktgeometrie „gekreuzte Zylinder“ durchgeführt. Die zylindrischen Proben wurden aus den Werkstoffen Titan Grade 4 und der Ti-Legierung Ti6AI4V gefertigt. Ein Teil dieser Ti-basierten Proben wurde oberflächengehärtet. Die bisher erzielten Ergebnisse zeigen, dass die oberflächenbehandelten Proben dazu neigen, unter der Belastung die Kontaktfläche zu vergrößern. Dies deutet auf einen Effekt bekannt als „junction growth“ und damit auf eine erhöhte Versetzungsbeweglichkeit der randschichtgehärteten Proben hin. Einen Einfluss der Zwischenstoffe konnte nicht nachgewiesen werden. T2 - 52. Tribologie-Fachtagung - Reibung, Schmierung und Verschleiß - Forschung und praktische Anwendungen CY - Göttingen, Germany DA - 26.09.2011 KW - Partial slip KW - Schwingungsverschleiß PY - 2011 SN - 978-3-00-035439-7 VL - I SP - 14/1 EP - 14/11 AN - OPUS4-24813 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hartelt, Manfred A1 - Wäsche, Rolf T1 - Verschleißuntersuchungen an Dental-Implantat-Werkstoffen unter partial slip Bedingungen KW - Modellsystem KW - Partial slip KW - Fretting regime KW - Implantat KW - Titan PY - 2012 SN - 0724-3472 VL - 59 IS - 3 SP - 18 EP - 23 PB - Expert Verlag CY - Renningen AN - OPUS4-26003 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Wear behaviour of yttrium titanate ceramics under gross slip fretting conditions T2 - Int. Conf. Nordic Countries (NordTrib 2012) CY - Trondheim, Norway DA - 2012-06-12 PY - 2012 AN - OPUS4-26014 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wäsche, Rolf T1 - Tribological behaviour of polyurethane under oscillating sliding conditions against cast iron T2 - 18. Int. Colloq. Tribology - Industrial and Automotive Lubrication CY - Ostfildern, Germany DA - 2012-01-10 PY - 2012 AN - OPUS4-25343 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -