TY - JOUR A1 - Quackatz, Lukas A1 - Gornushkin, Igor B. A1 - Griesche, Axel A1 - Kannengießer, Thomas A1 - Treutler, Kai A1 - Wesling, Volker T1 - In situ chemical analysis of duplex stainless steel weld by laser induced breakdown spectroscopy N2 - The high corrosion resistance and good mechanical properties of duplex stainless steel (DSS) are due to its special chemical composition, which is a balanced phase ratio of ferrite (α) and austenite (γ). Many industrial applications require the integration of DSS components. For this, Gas tungsten arc welding (GTAW) is an excellent choice, as it allows an automated operation with high reproducibility. However, when the weld pool solidifies, critical ratios of α- and γ- phases can occur, which lead to solidification cracking, increased susceptibility to corrosion, and a decrease in ductility and critical strength. Previous studies have shown that these defects can be caused by the accumulation of manganese and chromium in the heat affected zone (HAZ), requiring ongoing monitoring of this accumulation. A suitable method for such monitoring is laser-induced breakdown spectroscopy (LIBS), which can be used in two operating modes: calibration using standard reference samples and calibration-free. Unlike conventional quantitative LIBS measurements, which require reference samples to generate a calibration curve, calibration-free LIBS (CF-LIBS) allows chemical compositions to be determined solely from the emission spectrum of the plasma. Numerous publications show that CF-LIBS is a fast and efficient analytical method for the quantitative analysis of metal samples. In this work, CF-LIBS is applied to spectra obtained during GTAW DSS welding and the result is compared with those obtained by PLS analysis. A good correlation was found between both types of analysis, demonstrating the suitability of the CF-LIBS method for this application. The CF-LIBS method has a significant advantage over conventional LIBS due to the rapid in situ measurement of concentrations of major alloying elements without calibration procedure. This, combined with fast feedback and appropriate adjustment of welding parameters, helps prevent welding defects. KW - Duplex stainless steels KW - In situ measurement KW - LIBS KW - GMAW PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597940 DO - https://doi.org/10.1016/j.sab.2024.106899 SN - 0584-8547 VL - 214 SP - 1 EP - 7 PB - Elsevier B.V. AN - OPUS4-59794 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Willeke, Maraike A1 - Giese, Marcel A1 - Lorenz, Swenja A1 - Treutler, Kai A1 - Schröpfer, Dirk A1 - Wesling, Volker A1 - Kannengießer, Thomas T1 - Effect of alloy modification on the wear protection coatings made of Ni- and Co-based materials and surface machinability via ultrasonic milling process N2 - AbstractWear-resistant coatings are required for highly efficient and economical steel components in equipment, process, and power plant engineering to withstand high corrosive, tribological, thermal, and mechanical stresses. Co-alloys are used as wear-resistant coatings for steel components, tailored to the specific application. The substitutability of Co alloys with Ni-based wear protection systems, in addition to price and supply uncertainties, is facilitated by the combination of innovative welding and machining processes such as ultrasonic-assisted milling. The aim of the study is to improve the machinability of two different hard-facing alloys while maintaining the same wear protection potential. Therefore, the wear-resistant alloys NiMoCrSi (Colmonoy C56) and CoMnCrSi (Tribaloy T400) were modified by the alloying additions Nb, Hf, and Ti and then applied to a carbon-manganese steel S355 using the plasma transfer arc (PTA) welding process. The influence of the alloying additions on the microstructure as KW - Wear resistance KW - Co-based alloy KW - Ni-based alloy KW - PTA welding process KW - Ultrasonic assisted milling process PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623931 DO - https://doi.org/10.1007/s00170-024-14955-0 SN - 0268-3768 SP - 1 EP - 17 PB - Springer Science and Business Media LLC AN - OPUS4-62393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Quackatz, Lukas A1 - Westin, Elin Marianne A1 - Griesche, Axel A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Treutler, Kai A1 - Wesling, Volker A1 - Wessman, Sten T1 - Assessing ferrite content in duplex stainless weld metal: WRC ‘92 predictions vs. practical measurements N2 - AbstractThe weldability of stainless steels is largely controlled by the chemical composition, and alloys with ferritic or ferritic-austenitic solidification show the highest resistance to hot cracking. As the resulting phase balance also affects the final properties, it may be beneficial to both foresee and measure the weld metal ferrite content. The WRC ‘92 constitution diagram is currently the most accurate prediction tool available, but it does not take the cooling rate into consideration and the precision may be less accurate for stainless steels with high ferrite numbers (FNs). This study aims to assess the reliability of the WRC ‘92 diagram for weld metals with FN  50. The chemical composition was altered through gas tungsten arc welding (GTAW) of UNS S32205 with ER347 filler wire that had been coated using physical vapor deposition (PVD) with either niobium (Nb), copper (Cu), nickel (Ni), manganese (Mn), carbon (C), or silicon (Si). The actual ferrite content was evaluated using image analysis, FeriteScope and X-ray diffraction (XRD). While predictions from the WRC ‘92 diagram were deemed acceptable for Ni, Si, and Mn, notable deviations were observed for Nb, Cu, and C. The FeriteScope exhibited a consistent trend with image analysis, albeit with slightly higher FN values, wider scatter, and the conversion factor from FN to vol% is open for discussion. The lowest accuracy and largest spread were obtained using non-contact XRD, rendering it unsuitable for ferrite measurements of welds. These findings underscore the need for improved prediction tools and appropriate measurement methods for assessing ferrite content in duplex weld metals. KW - Duplex stainless steel KW - Welding KW - Phase balance KW - Microscopy KW - Microstructure PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-618777 DO - https://doi.org/10.1007/s40194-024-01878-3 SN - 1878-6669 VL - 69 IS - 1 SP - 31 EP - 45 PB - Springer CY - Berlin AN - OPUS4-61877 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Quackatz, Lukas A1 - Westin, Elin Marianne A1 - Griesche, Axel A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Treutler, Kai A1 - Wesling, Volker A1 - Wessman, Sten T1 - Assessing ferrite content in duplex stainless weld metal: WRC ‘92 predictions vs. practical measurements N2 - AbstractThe weldability of stainless steels is largely controlled by the chemical composition, and alloys with ferritic or ferritic-austenitic solidification show the highest resistance to hot cracking. As the resulting phase balance also affects the final properties, it may be beneficial to both foresee and measure the weld metal ferrite content. The WRC ‘92 constitution diagram is currently the most accurate prediction tool available, but it does not take the cooling rate into consideration and the precision may be less accurate for stainless steels with high ferrite numbers (FNs). This study aims to assess the reliability of the WRC ‘92 diagram for weld metals with FN  50. The chemical composition was altered through gas tungsten arc welding (GTAW) of UNS S32205 with ER347 filler wire that had been coated using physical vapor deposition (PVD) with either niobium (Nb), copper (Cu), nickel (Ni), manganese (Mn), carbon (C), or silicon (Si). The actual ferrite content was evaluated using image analysis, FeriteScope and X-ray diffraction (XRD). While predictions from the WRC ‘92 diagram were deemed acceptable for Ni, Si, and Mn, notable deviations were observed for Nb, Cu, and C. The FeriteScope exhibited a consistent trend with image analysis, albeit with slightly higher FN values, wider scatter, and the conversion factor from FN to vol% is open for discussion. The lowest accuracy and largest spread were obtained using non-contact XRD, rendering it unsuitable for ferrite measurements of welds. These findings underscore the need for improved prediction tools and appropriate measurement methods for assessing ferrite content in duplex weld metals. KW - Duplex stainless steel KW - Phase fraction prediction KW - WRC diagram PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623682 DO - https://doi.org/10.1007/s40194-024-01878-3 VL - 69 SP - 31 EP - 45 PB - Springer Science and Business Media LLC AN - OPUS4-62368 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Giese, Marcel A1 - Gräbner, Maraike A1 - Schröpfer, Dirk A1 - Treutler, Kai A1 - Lorenz, Svenja A1 - Kannengießer, Thomas A1 - Wesling, Volker T1 - Alloy modification and ultrasonic-assisted milling of wear-resistant alloys with defined surfaces N2 - The reduction of CO2 emissions is closely linked to the development of highly efficient and economical steel components in plant and process engineering. To withstand the high combined corrosive, tribological, thermal, and mechanical stresses, wear-resistant coatings tailored to the application and steel grade are used. In addition to the increasing demand to substitute conventional cobalt alloys with nickel alloys, there is also a growing need for defined or functional surfaces of high integrity. Due to high tool wear, milling operations required to produce the complex geometries of the components are often not economically feasible for SMEs. By means of alloy modification of the filler metals for nickel-based plasma build-up welded wear-resistant coatings and by the use of innovative ultrasonic-assisted milling processes more favourable machinability shall be achieved without reducing the wear protection potential. In this paper, the influence of the microstructure and precipitation morphology adjusted by means of alloy modification on the machinability is investigated. This is done based on a wear protection alloy NiCrMoSiFeB (trade name: Colmonoy 56 PTA) typically used for screw machines, which substitutes conventional CoCr alloys (Stellite). Metallurgical investigations and in-situ measurements of occurring process forces and temperatures at the tool cutting edge during milling as well as subsequent investigations of tool wear and surface integrity allow a detailed analysis and correlation between microstructural properties and machinability. For the cast samples, a clear change in the microstructure and hardness can be seen through the addition of Al, Ti, or Nb. These differences lead to an improvement in the machining process for Nb. Al and Ti cause long-needled or star-shaped precipitations and hardness increases, which lead to higher cutting forces and increased tool wear. KW - Cladding KW - Wear resistant alloys KW - Alloy modification KW - Post-processing KW - Ultrasonic assisted milling KW - Renewable energy PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-622918 DO - https://doi.org/10.1007/s40194-024-01786-6 SN - 1878-6669 VL - 68 SP - 2567 EP - 2575 PB - Springer Science and Business Media LLC CY - Berlin ; Heidelberg AN - OPUS4-62291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Graebner, Maraike A1 - Giese, Marcel A1 - Treutler, Kai A1 - Lorenz, Swenja A1 - Schröpfer, Dirk A1 - Wesling, Volker A1 - Kannengießer, Thomas T1 - Processing of crack-free Nickel- and Cobalt-based wear protection coatings and defined surfaces by subsequent milling processes N2 - In the area of plant engineering, steel components are provided with a wear protection coating for efficient use to protect them against corrosive, tribological, thermal and mechanical stresses. The use of innovative ultrasound-assisted milling processes and plasma-welded nickel- and cobalt-based wear protection coatings are being investigated to determine how more favourable machinability can be achieved while retaining the same wear protection potential. The focus is on the NiCrSiFeB alloy, which is intended to replace CoCr alloys in the area of screw machines. The utilization of ultrasonic-assisted milling for the machining of coating materials is a novel approach. The modification of hard facing layers in terms of microstructure and precipitation morphology as well as suitability for machining is investigated and compared with the CoCr alloy. The alloy modifications are generated by a PTA process by systematically adjusting the preheating and interpass temperatures, a crack-free wear-resistant layer can be generated, which is subsequently machined by a milling process. In addition to the crack-free properties, the microstructure, the bonding as well as the mixing between the NiCrSiFeB alloy and a 1.8550 as well as between the CoCr alloy and a 1.4828 are analysed and compared in the joining areas. In addition, heating and cooling rates are determined and a chemical analysis of the weld metals is performed. Furthermore, it was found that the build-up layers of NiCrSiFeB alloy are more difficult to machine using the milling process than the CoCr alloy, as higher milling forces are required. KW - PTA welding KW - Wear-resistant alloys KW - Ultrasonic assisted milling KW - Wear KW - Cadding KW - Milling KW - Ni-based alloy KW - Co-based alloy PY - 2024 DO - https://doi.org/10.1177/14644207241265778 SN - 1464-4207 SP - 1 EP - 17 PB - SAGE Publications AN - OPUS4-60799 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Giese, Marcel A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Gräbner, Maraike A1 - Treutler, Kai A1 - Wesling, Volker T1 - Legierungsmodifikation und Einsatz hybrider Fräsprozesse zur Optimierung der Zerspanungssituation Ni-basierter Verschleißschutzauftragschweißungen mit definierten Oberflächen N2 - Die Verringerung der CO2-Emissionen ist eng mit der Entwicklung hocheffizienter und wirtschaftlicher Komponenten aus Stahl in der Anlagen- und Verfahrenstechnik verknüpft. Um den hohen kombinier-ten korrosiven, tribologischen, thermischen und mechanischen Beanspruchungen stand zu halten, werden auf Anwendungsfall und Stahlwerkstoff abgestimmte Verschleißschutzschichten eingesetzt. Neben der zunehmenden Forderung konventionelle Kobalt- durch Nickellegierungen zu ersetzen, wächst auch der Bedarf nach definierten Ober- bzw. Funktionsflächen hoher Güte. Aufgrund hohen Werkzeugverschleißes ist die erforderliche Fräsbearbeitung zu Herstellung der komplexen Geomet-rien der Bauteile für KMU oftmals wirtschaftlich nicht möglich. Mittels Legierungsmodifikation der Schweißzusätze für nickelbasierte plasmaauftraggeschweißte Verschleißschutzschichten und durch den Einsatz innovativer ultraschallunterstützter Fräsprozesse soll eine günstigere Zerspanbarkeit er-reicht werden, ohne das Verschleißschutzpotential zu mindern. Im vorliegenden Beitrag wird der Ein-fluss der mittels Legierungsmodifikation eingestellten Gefüge- und Ausscheidungsmorphologie auf die Zerspanbarkeit untersucht. Dies erfolgt anhand einer typischerweise für Schneckenmaschinen einge-setzten Verschleißschutzlegierung NiCrMoSiFeB-Legierung („Colmonoy 56 PTA“), die konventionelle CoCr-Legierungen (Stellite) substituiert. Metallurgische Untersuchungen und In-situ-Messungen auf-tretender Prozesskräfte an der Werkzeugschneide beim Fräsen sowie anschließende Untersuchungen von Werkzeugverschleiß und Oberflächenintegrität ermöglichen eine detaillierte Analyse und Korrela-tion zwischen mikrostrukturellen Eigenschaften und Zerspanbarkeit. T2 - DVS Congress 2023 CY - Essen, Germany DA - 11.09.2023 KW - Werkzeugverschleiß KW - Oberflächenintegrität KW - Ultraschallunterstütztes Fräsen KW - Zerspankräfte PY - 2023 SP - 742 EP - 747 AN - OPUS4-59210 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Giese, Marcel A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Müller, Thomas A1 - Treutler, Kai A1 - Wesling, Volker T1 - Legierungsmodifikation und Einsatz hybrider Fräsprozesse zur Optimierung der Zerspanungssituation Ni-basierter Verschleißschutzauftragschweißungen mit definierten Oberflächen N2 - Die Bestrebungen zur Verringerung der CO2-Emissionen erfordern hochbelastbare und effiziente Komponenten aus Stahl in der Anlagen-, Verfahrens- und Kraftwerkstechnik. Hierfür sind in zunehmendem Maße auf den Anwendungsfall und Stahlwerkstoff abgestimmte Verschleißschutzschich-ten und definierte, zerspante Oberflächen notwendig. Die hohen Härten dieser Schichten und der Einsatz konventioneller Co-basierter Verschleißwerkstoffe führen oftmals zu unwirtschaftlichen Bauteilen, gerade aufgrund hohen Werkzeugverschleißes bei der Zerspanung mit geometrisch bestimmter Schneide. Er-kenntnisse über den Einsatz Ni-basierter Verschleißwerkstoffe und die Optimierung der Zerspanbarkeit mittels Legierungsmodifikationen und moderner hybrider Fräsprozesse ohne Verschlechterung der Ver-schleißschutzeigenschaften sind deshalb für die Anwender und Verarbeiter zur wirtschaftlichen Fertigung hochbelasteter Stahlbauteile wesentlich. Der vorliegende Beitrag stellt die Untersuchungsmethodik eines aktuell laufenden Vorhabens der TU Clausthal und BAM, Berlin, vor. Fokus liegt hierbei auf den hochin-strumentierten Fräsexperimenten, die eine reproduzierbare Analyse und Korrelation zwischen den mik-rostrukturellen Eigenschaften der auftraggeschweißten Legierungen, dem Zerspanprozess und der Zer-spanbarkeit, insbesondere der resultierenden Oberflächenintegrität, ermöglichen sollen. T2 - Tagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - Werkzeugverschleiß KW - Oberflächenintegrität KW - Ultraschallunterstütztes Fräsen KW - Zerspankräfte PY - 2022 SP - 368 EP - 374 AN - OPUS4-59211 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Engelking, Loenz A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Eissel, Antonia A1 - Treutler, Kai A1 - Wesling, Volker T1 - Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten N2 - Die additive Fertigung mittels Schweißverfahren bietet große ökonomische Vorteile für eine ressourceneffiziente Bauteilherstellung. Offene Fragen bezüglich Homogenität, Anisotropie der Schweißgefüge und den damit verbundenen Bauteileigenschaften stehen einer wirtschaftlichen Verarbeitung oftmals im Wege. Finale Bauteilgeometrie und Oberflächengüte erfordern meist komplementäre subtraktive Fertigungsschritte. Werkstoffe für hochbelastbare Komponenten sind oftmals schwer span bar. In einem Vorhaben der BAM und des ISAF wurde untersucht, wie die Modifikation der AM-Schweißzusätze und das ultraschallunterstützte Fräsen (US) die Zerspanungssituation verbessern. Der vorliegende Artikel stellt wesentliche Zusammenhänge zwischen Legierung, Gefüge und Zerspanung zweier schwer spanbarer Hochleistungslegierungen (FeNi und CoCr) dar. Großes Potenzial zeigte neben dem US die Modifikation mit Zr und Hf bei Zulegierung in das Schweißgut mittels Beschichtung von Massivdrähten bzw. Herstellung von Fülldrähten. KW - Additive Fertigung (AM) KW - Ultraschallunterstütztes Fräsen (US) KW - Werkstoffmodifikation KW - Oberflächenintegrität KW - Zerspanbarkeit schwer spanbarer Legierungen KW - Ressourceneffizienz in Prozessketten KW - Hochleistungslegierungen KW - Technologietransfer für KMU PY - 2025 SN - 978-3-96144-304-8 VL - 2026 SP - 290 EP - 298 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-65246 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Graebner, Maraike A1 - Giese, Marcel A1 - Lorenz, Svenja A1 - Treutler, Kai A1 - Schröpfer, Dirk A1 - Wesling, Volker A1 - Kannengießer, Thomas T1 - Wear resistance of modified NiMoCrSi claddings in relation to the resulting surface machinability via ultrasonic-assisted milling N2 - In the field of plastics processing, extruder screws are subjected to significant wear stresses. The extruder screw is the main wear component in those production machines and is usually coated with intermetallic wear protection alloys composed of Ni-based alloys, specifically Colmonoy C56 PTA (NiMoCrSi). There is a growing demand for providing an economic machinability of these alloys to achieve defined contours with a sufficient surface integrity. Recent investigations exhibit promising results applying ultrasonic milling for such hard-to-cut materials. The Colmonoy C56 is modified by various alloying additions Ti, Nb, Mo, Hf, and Al, and then cladded on a steel S355 via Plasma Transferred Arc process. The effect of alloying additions on the microstructure is analyzed regarding their resistance to abrasive and adhesive wear. With Miller test ASTM G75 the influence of alloying elements on resistance to abrasive wear for two abrasive materials is investigated (high-grade corundum F220 and quartz powder). The wear loss is not increased for additions of Nb and Ti compared to the base material C56. Modifications with Hf or Al reduces the resistance to abrasive wear and significantly increases material loss. The extruder screw is also subject to adhesive wear, which can be quantified by means of the pin-roll test. It is demonstrated that the addition of Hf, for example, contributes to a reduction in wear loss. Aim of the investigations is to find suitable modifications for the wear claddings of C56 for a sufficient machineability, without compemising the wear resistant. The machinability is considerably affected by the alloy additions, and is determined using ultrasonic-assisted milling. The addition of hafnium reduces machinability, i.e. significantly increases cutting forces. The incorporation of Nb exhibits a significant reduction of cutting forces, and results in reduced tool wear and an enhanced of surface integrity (roughness, density of defects, residual stresses). KW - Colmonoy C56 KW - PTA welding KW - Adhesive wear KW - Abrasive wear KW - Ultrasonic-assisted milling process KW - Surface integrity KW - Service life and efficiency KW - Substitution of critical raw materials PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651530 DO - https://doi.org/10.1016/j.wear.2025.205830 SN - 0043-1648 VL - 571 SP - 1 EP - 10 PB - Elsevier B.V. AN - OPUS4-65153 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -