TY - JOUR A1 - Krüger, Simone A1 - Wachtendorf, Volker A1 - Rauth, W. A1 - Klimmasch, T. A1 - Krüger, P. T1 - Screening the weathering stability of automotive coatings by chemiluminescence JF - Journal of coatings technology and research N2 - Chemiluminescence (CL) is a sensitive method of investigating the thermo-oxidative stability of polymers in the early stages of degradation. Therefore, CL measurements were applied to different automotive coatings to evaluate their degradation behavior during artificial weathering. In this work, CL measurements were carried out for different automotive coatings to follow their degradation behavior during artificial weathering. The CL emission depends on sample-specific parameters like stabilizer, matrix, or hardener; experimental parameters like the oxygen partial pressure; and exposure parameters like the duration of weathering. The potential of CL could be demonstrated by classifying materials into categories of good, medium, and low degradation performance at a much earlier stage of weathering exposure than in combination with the usual visual detection of weathering effects. KW - Accelerated weathering KW - Coating KW - Chemiluminescence KW - Sensitive detection KW - Weathering PY - 2008 DO - https://doi.org/10.1007/s11998-007-9071-7 SN - 1547-0091 SN - 1935-3804 VL - 5 IS - 1 SP - 17 EP - 24 PB - Springer CY - Blue Bell, Pa. AN - OPUS4-16723 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Appajaiah, Anilkumar A1 - Wachtendorf, Volker A1 - Daum, Werner T1 - Climatic exposure of polymer optical fibers: Thermooxidative stability characterization by chemiluminescence JF - Journal of applied polymer science N2 - The optical transmission stability was investigated for commercially available polymer optical fibers (POFs) which were exposed to a climate of 92°C and 95% relative humidity for about 3300 h. The optical transmission stability of POFs was correlated to their thermooxidative stability. POFs possessed identical core material, poly(methyl methacrylate), but they differed in the materials used for the claddings. The optical transmission was measured online using a prototype device called multiplexer. The chemiluminescence (CL) technique was applied to characterize the thermooxidative stability and degradation of POFs. CL analysis reveals the thermooxidative degradation of bare POFs (core and cladding), predominantly of the claddings, as a result of climatic exposure. Ultraviolet-visible transmittance measurements demonstrated more changes in the claddings as compared to the cores due to degradation. The CL and optical measurements data indicated that the optical transmission stability of POFs was dependent mainly on the thermooxidative stability of the claddings and their chemical compositions. KW - Ageing KW - Polymer optical fiber KW - Degradation KW - Chemiluminescence KW - Transparency PY - 2007 DO - https://doi.org/10.1002/app.23955 SN - 0021-8995 SN - 1097-4628 VL - 103 IS - 3 SP - 1593 EP - 1601 PB - Wiley InterScience CY - Hoboken, NJ AN - OPUS4-19072 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Krüger, Simone A1 - Wachtendorf, Volker A1 - Hennecke, Manfred T1 - Chemiluminescence: A promising new testing method for plastic optical fibers JF - Journal of lightwave technology N2 - The thermo-oxidative degradation of a polymeric optical cable is investigated by chemiluminescence, The results are reliable and reproducible. Two distinct processes are reported marked by a peak and a plateau behavior versus the time, respectively. Both processes are ruled by thermally activated processes. Beside the dependencies of temperature and time, the influence of absorbed water is discussed. Chemiluminescence is proposed as a promising candidate for a suitable testing method assessing the thermo-oxidative stability of plastic optical fibers and cables. it requires not more than a simple one-day testing procedure and has the advantage that it can be carried out even within the lo cv temperature ranges of the cables' intended use. KW - Chemiluminescence KW - Chemilumineszenz PY - 1999 DO - https://doi.org/10.1109/50.803022 SN - 0733-8724 SN - 1558-2213 VL - 17 IS - 11 SP - 2291 EP - 2296 PB - Institute of Electrical and Electronics Engineers CY - New York, NY AN - OPUS4-718 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part II: Experimental set-up and examination JF - JCT coatingsTech KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 5 SP - 38 EP - 44 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21494 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wachtendorf, Volker A1 - Geburtig, Anja T1 - Chemiluminescence for the early detection of weathering effects of coatings - Part I: Fundamentals JF - JCT coatingsTech KW - Chemiluminescence KW - Weathering KW - Polymer KW - Oxidation PY - 2010 SN - 1547-0083 VL - 7 IS - 4 SP - 66 EP - 71 PB - Federation of Societies for Coatings Technology CY - Blue Bell, Pa. AN - OPUS4-21493 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -