TY - JOUR A1 - Launert, B. A1 - Rhode, Michael A1 - Kromm, Arne A1 - Pasternak, H. A1 - Kannengießer, Thomas T1 - Measurement and numerical modeling of residual stresses in welded HSLA component-like I-girders N2 - The present contribution shows the residual stress results obtained from experiments with the sectioning method in comparison to global(structural) welding simulation models on component-like (i.e., large scale) I-girders made of structural steel grades S355 and S690QL. Plates were welded by conventional gas metal arc welding using two different heat inputs. In addition, the base material was assumed to be stress-free. Based on these results, conclusions and recommendations for the design of welded I-girders are drawn. T2 - IIW - Annual Assembly 2016 CY - Melbourne, Australia DA - 10.07.2016 KW - Residual Stresses KW - Microalloyed Steels KW - Girders KW - MAG Welding KW - Numerical Simulation PY - 2016 DO - https://doi.org/10.1007/s40194-016-0413-x SN - 1878-6669 SN - 0043-2288 VL - 61 IS - 2 SP - 223 EP - 229 PB - Springer CY - Berlin, Heidelberg AN - OPUS4-38919 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Kromm, Arne T1 - Reparaturschweißen zukünftiger, in Betrieb befindlicher Wasserstoffpipelines N2 - Wasserstoff leistet als Energieträger der Zukunft einen entscheidenden Beitrag zur nachhaltigen Energieversorgung, wobei der Transport auf Basis des europäischen Ferngasleitungsnetzes erfolgen wird. Bisherige Untersuchungen zur Werkstoffkompatibilität zeigen, dass die hier verwendeten, niedriglegierten Rohrstähle für Wasserstofftransport unter normalen Betriebsbedingungen (≤ 60 °C, max. 100 bar) grundsätzlich geeignet sind. Die Eignung kann nicht ohne Weiteres übertragen werden, sobald Reparaturschweißungen beispielsweise aufgrund von Wartungsarbeiten an druckführenden, in Betrieb befindlichen, Hochdruckgasleitungen erfolgen. Aus technisch-ökonomischen Gründen werden Schweißarbeiten dabei im Betrieb unter fortwährendem Druck und Gasfluss durchgeführt. Dies soll auch bei Wasserstoffpipelines erfolgen. Dazu im Erdgasnetz angewandte und etablierte Konzepte sind beispielsweise das „Hot-Tapping“ und „Stoppling“. Beim „Hot-Tapping“ wird eine druckführende Pipeline durch Anflanschen eines abgeschlossenen, druckdichten Systems aus Absperrventil und Bohrvorrichtung angebohrt. Dazu müssen sogenannte Überschieber (aus vorgeformten Zylinderhalbschalen) durch Längsnaht verbunden und dann mit Rohrrundnähten am Produktrohr verbunden werden. Für das zum überwiegenden Teil durchgeführte E-Hand-Schweißen sind dabei Vorwärmtemperaturen von ca. 100 °C bzw. 250 °C für die maximale Zwischenlagentemperatur einzuhalten. Besonderer Fokus liegt auf der Betrachtung dünnwandiger Leitungen, da hier beim Schweißen der Rundnähte die Austenitisierungstemperatur an der Innenseite der Pipeline überschritten wird. Dadurch wird eine signifikant höhere Wasserstoffaufnahme in den Leitungsstahl vermutet, mit einer möglichen Degradation der mechanischen Kennwerte bzw. Rissbildung. Durch die langen Schweiß- und Abkühlzeiten wird der Rohrleitungsstahl zudem teilweise stundenlang Temperaturen von bis zu 250 °C ausgesetzt. Neben der klassischen „Versprödung“ muss daher eventuell auch ein sogenannter Hochtemperatur-Wasserstoffangriff betrachtet werden. Diese vorliegende Studie gibt Einblick zur Übertragbarkeit der bekannten Konzepte aus der Erdgastechnik zum Reparaturschweißen. Dazu werden Möglichkeiten und Grenzen momentaner Prüfkonzepte sowie deren Weiterentwicklungen aufgezeigt. Dies umfasst bspw. geeignete Methodiken zur Werkstoffprüfung als auch skalierte Bauteilversuche unter realistischen Druckgas-Betriebsbedingungen einer Pipeline. In diesem Rahmen erfolgt auch die Kurzvorstellung des Kooperationsprojektes von BAM, DVGW und Ferngasnetzbetreibern „H2-SuD“ zum Einfluss der Temperaturführung und Rohrgeometrie auf die Wasserstoffaufnahme. T2 - DVS CONGRESS 2024 CY - Erfurt, Germany DA - 16.09.2024 KW - Reparaturschweißen KW - Pipeline KW - Wasserstoff KW - Im Betrieb PY - 2024 SN - 978-3-96144-269-0 VL - 395 SP - 341 EP - 349 AN - OPUS4-61478 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Herausforderungen beim Schweißen im Betrieb an Wasserstoff-Ferngasleitungen N2 - Als Energieträger der Zukunft kommt grünem Wasserstoff große Bedeutung bei der Energiewende und der zukünftigen, nachhaltigen Energieversorgung zu Teil. Zum effizienten und sicheren Transport des Wasserstoffs ist die Bereitstellung einer Pipeline-Infrastruktur geplant. Die meisten Länder verfolgen hierbei die Strategie der Umwidmung bestehender Erdgastransportleitungen, ergänzt durch Errichtung neuer Pipelines. Die bestehenden Erdgasnetze sind dabei aus unterschiedlichsten Rohrgeometrien und Materialien zusammengesetzt. Bei der Umwidmung von Erdgaspipelines zum Transport von Wasserstoff müssen daher Fragen der Materialverträglichkeit hinsichtlich des als Wasserstoffversprödung bekannten Phänomens der Beeinträchtigung der mechanischen Eigenschaften metallischer Werkstoffe durch Wasserstoff betrachtet werden. Bisherige Forschungsergebnisse und Feldversuche deuten darauf hin, dass die niedriglegierten, ferritischen Stähle, aus denen die Ferngasleitungen des Erdgasnetzes überwiegend bestehen, für den Transport von Wasserstoff unter normalen Betriebsbedingungen geeignet sind. Eine Frage, die bislang weniger Aufmerksamkeit erhielt, ist die, wie sich das Schweißen im Betrieb an Wasserstoffpipelines auf die Materialkompatibilität auswirkt. Im Erdgasnetz sind etablierte Verfahren wie beispielsweise das „Hot-Tapping“ unumgänglich für die Instandhaltung und Erweiterung des Netzes. Hierbei werden an eine im Betrieb befindliche Pipeline geteilte T-Stücke aufgeschweißt, über die die Pipeline dann mit geeigneten Bohrvorrichtungen während eines ununterbrochenen Betriebs angebohrt werden kann. Um zu beurteilen, ob diese Verfahren gefahrlos auf Wasserstoffpipelines übertragen werden können, müssen Problemstellungen betrachtet werden, die sich durch den Wärmeeintrag ins Material beim Schweißen ergeben. Wasserstofflöslichkeit und Diffusionsgeschwindigkeit sind temperaturabhängig. Erhöhte Temperaturen könnten eine Wasserstoffaufnahme ins Material bewirken, die zu einer kritischen Degradation der mechanischen Eigenschaften des Materials führen könnte. Die Temperaturen, die beim Schweißen erreicht werden, führen lokal zur Überschreitung der Austenitisierungstemperatur. Austenit weist eine deutlich höhere Löslichkeit von Wasserstoff auf, während die Diffusionsgeschwindigkeit des Wasserstoffs in dieser Phase deutlich herabgesetzt ist. Es wird vermutet, dass dies zu einer lokal erhöhten Wasserstoffkonzentration führt. Damit geht ein erhöhtes Risiko einer kritischen Materialdegradation einher. Durch die lange Zeitdauer beim Schweißen von mehrlagigen Rundkehlnähten an großen Pipelines, einschließlich einer möglichen Vorwärmprozedur, ist weiterhin zu klären, ob der aus Anwendungsfällen in der Petrochemie bekannte Hochtemperaturwasserstoffangriff auftritt. Der vorliegende Beitrag liefert einen Überblick über das Schweißen im Betrieb an Gaspipelines, hierbei auftretenden Herausforderungen bei der möglichen Anwendung auf Wasserstoffleitungen. Dabei werden auch aktuelle Forschungsprojekte zum Thema Schweißen an Wasserstoffpipelines im Betrieb eingehend diskutiert. In diesem Zusammenhang werden erste Ergebnisse des gemeinschaftlichen Forschungsprojektes „H2-SuD: Einfluss des Schweißens auf die Wasserstoffaufnahme und Degradation im Betrieb befindlicher H2-Ferngasleitungen“ des Deutschen Vereins des Gas- und Wasserfaches (DVGW), der Bundesanstalt für Materialforschung und -prüfung (BAM) und deutscher Gasnetzbetreiber (Open Grid Europe, ONTRAS Gastransport, u.v.m.) präsentiert. T2 - 53. Sondertagung - Schweißen im Anlagen-und Behälterbau 2025 CY - Munich, Germany DA - 18.03.2025 KW - Materialdegradation KW - Pipeline KW - Schweißen KW - Wasserstoff PY - 2025 SN - 978-3-96144-290-4 (Print) SN - 978-3-96144-291-1 (E-Book) VL - 2025 SP - 106 EP - 115 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-62911 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Schweißen im Wasserstoffanlagen- und Behälterbau - Eine Kurzübersicht N2 - Wasserstoff erfüllt die zentrale Rolle für die Umwandlung der bisherigen fossil-basierten Energieerzeugung und -nutzung auf eine dekarbonisierte, nachhaltige Form. Dazu muss der Wasserstoff erzeugt, gespeichert, transportiert werden, bevor er wieder der Nutzung zugeführt wird. Hierzu sind entlang der gesamtem Prozesskette Wasserstofftechnologien notwendig, die einen sicheren Betrieb erfordern. Hierbei kommt dem schweißtechnischen Anlagen- und Behälterbau wesentliche Bedeutung zu, insbesondere (aber nicht ausschließlich) für Speicherung und Transport des Wasserstoffes. Der vorliegende Beitrag gibt einen kurzen Überblick, wo und wie die konventionelle Schweißtechnik hierzu wichtige Beiträge leistet. Die additive Fertigung, also das „Drucken“ von Bauteilen wird dabei zunehmend wichtiger, entlang der gesamtem Prozesskette der Wasserstofftechnologien. Gleichwohl darf nicht unterschätzt werden, dass auch wesentlicher Bedarf an der Erweiterung und teilweiser Neufassung von bestehenden Regel- und Normenwerken besteht. T2 - 51. Sondertagung "Schweißen im Behälter- und Anlagenbau" CY - Munich, Germany DA - 01.03.2023 KW - Wasserstoff KW - Anlagenbau KW - Schweißen KW - Studie KW - Pipeline PY - 2023 SN - 978-3-96144-219-5 VL - 387 SP - 83 EP - 88 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-57075 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Schweißen im Betrieb an Wasserstoff-Ferngasleitungen N2 - Wasserstoff gilt als Energieträger für die Erreichung der Klimaziele und einer nachhaltigen zukünftigen Energieversorgung. Für den notwendigen Transport des Wasserstoffs in großem Maßstab und über weite Entfernungen ist eine zuverlässige Pipeline-Infrastruktur erforderlich. Umfassende weltweite Forschungsprojekte deuten auf die allgemeine Kompatibilität der verwendeten überwiegend ferritischen Stähle für die vorgesehenen Betriebsbedingungen von bis zu 60 °C bei 100 bar Wasserstoff hin. Dies ist jedoch nicht direkt übertragbar auf schweißtechnische Reparatur- und Wartungsarbeiten an im Betrieb befindlichen Pipelines. Ein im Erdgasnetz etabliertes Verfahren stellt das „Hot-Tapping“ dar, bei dem eine unter Druck stehende Pipeline im Betrieb angebohrt wird. Hierfür kommt ein an die Rohrleitung geschweißtes Formstück zum Einsatz, das die Montage der Bohr-/Lochschneidemaschine ermöglicht. In den Richtlinien EIGA 121/14 bzw. AIGA 033/14 wird darauf hingewiesen, dass das Anbohren von Wasserstoffleitungen kein Routineverfahren darstellt: “[…] a hydrogen hot-tap shall not be considered a routine procedure […]“. Dieser Aussage liegt unter anderem zugrunde, dass das Anschweißen des Formstücks an das Rohr und alle zu erwartenden Wärmebehandlungen vor und nach dem Schweißen eine lokale Temperaturerhöhung verursachen. Insbesondere auch an der Rohrinnenfläche, die dem Wasserstoff ausgesetzt ist. Diese erhöhten Temperaturen begünstigen die Absorption und Diffusion von Wasserstoff in das Material. Besonders zu beachten ist außerdem die lokal auftretende kurzzeitige Austenitisierung des Materials, die eine lokal stark erhöhte Wasserstoffkonzentration verursachen kann. Aus den genannten Gründen gibt diese Studie einen kurzen Überblick über die derzeit weltweit verfügbaren Forschungsprojekte zum Schweißen von Wasserstoff-Pipelines im Betrieb. Vorgestellt werden unter anderem erste Ergebnisse des Kooperationsforschungsprojektes H2SuD, das derzeit an der BAM bearbeitet wird. T2 - 6. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 20.02.2025 KW - Materialdegradation KW - Pipeline KW - Schweißen KW - Wasserstoff PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632731 SN - 978-3-8440-9961-4 SN - 978-3-8191-0041-3 DO - https://doi.org/10.21268/20250506-12 SN - 2364-0804 SN - 3052-3524 N1 - Serientitel: Fortschrittsberichte der Materialforschung und Werkstofftechnik – Series title: Bulletin of Materials Research and Engineering VL - 15 SP - 381 EP - 390 PB - Shaker Verlag CY - Düren AN - OPUS4-63273 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Parameters and challenges for reliable hydrogen determination in welded joints by carrier gas hot extraction N2 - For the hydrogen-based energy economy of tomorrow, the construction of the necessary infrastructure will play a central role. Most materials used to date, such as welded steels, can be prone to hydrogen embrittlement under certain conditions. This includes the classic delayed cold cracking during welding as well as degradation phenomena during service of components in hydrogen-containing environment. For the evaluation of any hydrogen effect, for example, on the mechanical properties of a welded metallic material, the hydrogen content must be precisely determined. In the case of weld seams, the carrier gas hot extraction (CGHE) according to ISO 3690 is meanwhile state-of-the-art. CGHE is based on accelerated hydrogen degassing due to the thermal activation of hydrogen at elevated temperatures. In addition to the quantification of hydrogen, thermal desorption analysis (TDA) with varying heating rates can be used to determine and evaluate the hydrogen trapping at microstructural defects in the material. For both techniques, experimental and metrological influences must be considered, which have a major effect on the result. For example, ISO 3690 suggests different sample geometries and minimum extraction times for CGHE. This study summarizes the results and experiences of numerous investigations at the Federal Institute for Materials Research and Testing (BAM) with different sample temperatures and geometries (ISO 3690 type B and cylindrical TDA samples) regarding the influence of the sample surface (polished/welded), measurement accuracy depending on the sample volume and the insufficient monitoring of the effect of PI control on the extraction temperature. A deviating extraction temperature from the target temperature can significantly falsify the measurement results. Based on the results, methods are shown which allow the desired extraction temperature to be reached quickly without physically interfering with the measuring equipment. This serves to significantly improve the reliability of the hydrogen measurement through increased signal stability and accelerated hydrogen desorption. In general, an independent temperature measurement with dummy samples is recommended for the heating procedure of choice to exclude possible undesired temperature influences before the measurement. The methods described can be transferred directly to industrial applications KW - Welding KW - Hydrogen measurement KW - ISO 3690 KW - Carrier gas hot extraction PY - 2024 DO - https://doi.org/10.37434/tpwj2024.04.01 SN - 0957-798X VL - 4 SP - 3 EP - 10 PB - International Association Welding AN - OPUS4-60071 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kromm, Arne A1 - Schröpfer, Dirk A1 - Steger, J. A1 - Kannengießer, Thomas ED - Seefeldt, M. T1 - Residual stress formation in component related stress relief cracking tests of a welded creep-resistant steel N2 - Submerged arc welded (SAW) components of creep-resistant low-alloyed Cr-Mo-V steels are used for thick-walled heavy petrochemical reactors (wall-thickness up to 475 mm) as well as employed in construction of modern high-efficient fossil fired power plants. These large components are accompanied by significant restraints during welding fabrication, especially at positions of different thicknesses like welding of nozzles. As a result, residual stresses occur, playing a domi-nant role concerning so-called stress relief cracking (SRC) typically during post weld heat treat-ment (PWHT). Besides specific metallurgical factors (like secondary hardening due to re-precipitation), high tensile residual stresses are a considerable influence factor on SRC. For the assessment of SRC susceptibility of certain materials mostly mechanical tests are applied which are isolated from the welding process. Conclusions regarding the influence of mechanical factors are rare so far. The present research follows an approach to reproduce loads, which occur during welding of real thick-walled components scaled to laboratory conditions by using tests designed on different measures. A large-scale slit specimen giving a high restraint in 3 dimensions by high stiffness was compared to a medium-scale multi-pass welding U-profile specimen showing a high degree of restraint in longitudinal direction and a small-scale TIG-re-melted specimen. The small-scale specimens were additionally subjected to mechanical bending to induce loads that are found during fabrication on the real-scale in heavy components. Results show for all three cases compa-rable high tensile residual stresses up to yield strength with high gradients in the weld metal and the heat affected zone. Those high tensile stresses can be significant for cracking during further PWHT. T2 - European Conference on Residual Stresses 2018 - ECRS-10 CY - Leuven, Belgium DA - 11.09.2018 KW - Welding KW - Residual stresses KW - Stress Relief Cracking (SRC) KW - Creep-resistant steel KW - Post Weld Heat Treatment (PWHT) PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-459683 SN - 978-1-9452-9188-3 SN - 978-1-9452-9189-0 DO - https://doi.org/10.21741/9781945291890-29 SN - 2474-395X SN - 2474-3941 VL - 6 SP - 185 EP - 190 PB - Materials Research Forum LLC CY - Millersville, PA, USA AN - OPUS4-45968 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Czeskleba, Denis A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Vermeidung von Kaltrissen in UP-Dickblechschweißungen aus hochfesten Stählen N2 - Der Einsatz hochfester Stähle wie S690 erlaubt durch geringeren Materialeinsatz nicht nur eine immer wichtiger werdende Verringerung von CO₂-Emissionen, sondern auch eine effektive Kosten- und Gewichtsreduktion dickwandiger Bauteile. Insbesondere bei Wandstärken von bis zu 200 mm ist das Unterpulver- (UP-)Mehrdrahtschweißen aufgrund seiner hohen Effizienz eine gängige Praxis. Allerdings steigt bei hochfesten Stählen, hier vorliegend S690, die Gefahr wasserstoffunterstützter Kaltrisse (HAC), aufgrund ihrer Mikrolegierungskonzepte im Zusammenspiel mit hohen Eigenspannungen aus dem Schweißprozess und resultierend aus hohen Bauteilsteifigkeiten. Zusätzlich kann die erhebliche Aufmischung von Grund- und Zusatzwerkstoff beim UP-Schweißen zu risskritischen Gefügen führen, in denen der diffusible Wasserstoff besonders schädlich wirkt. Für Gefüge UP-geschweißter Bauteile liegen keine gesicherten Daten bezüglich Wasserstoffdiffusionskoeffizienten bzw. HAC-Rissanfälligkeit vor. Insbesondere die mikrostrukturabhängige Diffusion von durch den UP-Schweißprozess eingebrachtem Wasserstoff war nicht hinreichend gesichert. Ziel des Forschungsvorhabens war es daher, einen Beitrag zur kaltrisssicheren UP-Schweißverarbeitung hochfester Dickbleche zu leisten. Hierzu wurden systematisch unterschiedliche GW (S690 TM/QL) untersucht, die sich insbesondere in ihren Mikrostrukturen unterscheiden. Diese zeigten in Voruntersuchungen stark divergente Härteverteilungen im Besonderen in der letzten Lage der Schweißung, sodass ein ebenfalls stark divergentes Diffusionsverhalten postuliert wurde. Zunächst wurde der Wasserstoffeintrag über die Draht-Pulver-Kombination gemäß ISO 3690 ermittelt. Anschließend erfolgten mehrlagige Schweißungen sowohl unter freiem Schrumpfen als auch unter äußerer Zwängung. Eine detaillierte Gefügecharakterisierung und mechanisch-technologische Prüfungen, sowie Eigenspannungsmessungen ermöglichten die Bewertung der Rissanfälligkeit bei variierter Wärmeführung (schweißgeschwindigkeitsgesteuert). Zur quantitativen Beschreibung der Wasserstoffdiffusion wurden das Schweißgut (SG), die Wärmeeinflusszone (WEZ) und die Grundwerkstoffe (GW) mittels elektrochemischer Beladung und Trägergasheißextraktion (TGHE), sowie Permeationsversuchen untersucht. Basierend auf den ermittelten Diffusionskoeffizienten wurden numerische Modelle erstellt, um den Einfluss verschiedener Diffusionskoeffizienten auf die Wasserstoffverteilung in der Schweißnaht zu evaluieren. Entgegen dem Postulat wurden keine signifikanten Unterschiede in der Wasserstoff-Diffusionsgeschwindigkeit gemessen. Beide GW-Klassen (QL vs. TM) als auch das SG und die WEZ wiesen für diesen Werkstofftyp charakteristische Diffusionskoeffizienten mit nur geringen Unterschieden auf. Dies zusammen mit den nur sehr geringen Unterschieden in der Ausprägung der Eigenspannungen und mechanisch-technologischen Eigenschaften der Nähte, weisen auf eine hohe Kaltrisssicherheit hin. Die in allen Untersuchungen geringen Unterschiede zwischen QL und TM sprechen, hinsichtlich des HAC-Risikos aufgrund einer differenten Wasserstoffdiffusion, für die Austauschbarkeit der beiden Werkstoffe in der Produktion. KW - Wasserstoffrisse KW - Unterpulverschweißen KW - Wasserstoffdiffusion PY - 2025 SP - 1 EP - 150 AN - OPUS4-63127 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas A1 - Czeskleba, Denis T1 - Simulation of hydrogen distribution in submerged arc welded heavy plates as tool for evaluating cold cracking sensitivity for offshore structures N2 - Foundation structures for offshore wind turbines are typically made of heavy plate struc-tural steels, such as S420ML, welded by submerged arc welding. Due to the welding process conditions, higher amounts of hydrogen can be introduced. In this context, large plate thicknesses result in long diffusion paths and a prolonged diffusion time for hydrogen at ambient temperature and possible delayed hydrogen-assisted cold cracking. As a result, hydrogen can accumulate in areas of high mechanical stress and strain. Due to the delayed diffusion, a minimum waiting time of up to 48 h must be observed before non-destructive testing can be performed. In addition, the assessment of possible cold crack locations is very complex. For this reason, a numerical model of a component-like weld test was developed to simulate the temperature field during welding and subsequent cooling. A hydrogen diffusion model based on the temporal-local temperature distribution was established. It was applied to simulate the change of hydrogen distribution as a function of temperature cycle during multi-layer welding and further for the entire waiting time interval ≤ 48 h. As a result, crack critical areas could be evaluated in terms of accu-mulated hydrogen. An advantage of the diffusion model is the simulation of a normalized concentration, i.e. between "0" (no hydrogen) and "1" (max. concentration), which can be scaled to experimentally determined hydrogen concentrations. Finally, selected results for increased real hydrogen ingress are presented, which confirm the relatively high crack resistance of the S420 submerged arc welded joint. KW - Hydrogen assisted cracking KW - Diffusion KW - Numerical simulation KW - Offshore steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632416 DO - https://doi.org/10.21268/20250507-6 SP - 1 EP - 12 PB - Technische Universität Clausthal CY - Clausthal-Zellerfeld, Deutschland AN - OPUS4-63241 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Hadick, C. A1 - Schu, K. T1 - Component test concept for evaluation of in-service welding on pressurized hydrogen pipelines N2 - Hydrogen is set as the energy carrier of tomorrow and most countries will achieve large-scale hydrogen transport through the conversion of the natural gas (NG) grid and the construction of new pipelines. The interaction between hydrogen and the pipeline materials differs fundamentally from that of NG, as hydrogen is readily absorbed into the material. Considering the possible hydrogen embrittlement (HE), the compatibility of the pipeline materials (low-alloyed steels with a wide strength/thickness range) must be investigated. However, pipelines require intervention for maintenance, repair, or grid expansion with welding on/onto the pipelines while in service, i.e. the well-known "hot tapping" and "plugging" or “stoppling”. The challenges compared to NG can be broadly divided into the possible austenitization of the inner pipe material exposed to hydrogen and the welding itself. Both result in a significant increase in hydrogen solubility and could potentially pose challenges in terms of HE. Emphasis is placed on the word "could" because knowledge of "hot tapping" on hydrogen pipelines is scarce due a lack of service experience. To this end, this study proposes a concept for a component-like demonstrator with the objectives: (1) safe feasibility of "hot tapping" on pressurized model hydrogen pipeline sections, (2) facilitate ex-post sample extraction for the purpose of quantifying the absorbed hydrogen concentrations, and (3) ensure in-situ temperature measurement during welding to monitor the pipeline surface temperature. For safety reasons in the event of an unintentional "burn-through", a solid cylinder was inserted in the demonstrator to restrict the hydrogen gas volume to a small, pressurized layer. Reference pipeline surface temperature measurements were ensured on comparable, unpressurized geometries. The investigated range of welding conditions was investigated for representative material/thickness combinations (DN50 to DN200), suggesting the feasibility of the demonstrator for the determination of reliable in-service welding conditions for both installed and new pipelines for hydrogen service. T2 - 20th Pipeline Technology Conference ptc2025 CY - Berlin, Germany DA - 06.05.2025 KW - In-service KW - Hydrogen KW - Pipeline KW - Repair welding KW - component test PY - 2025 SP - 1 EP - 11 AN - OPUS4-63168 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Ausscheidungsverhalten und Eigenschaften der schweißbedingten Wärmeeinflusszonen hochfester Stähle in Abhängigkeit der Mikrolegierungsroute N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragverhaltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberechnungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Ausscheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Abkühlbedingungen geschaffen. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - WEZ-Erweichung KW - Mikrolegierungseinflüsse KW - Thermodynamische Modellierung PY - 2022 SP - 1 EP - 6 AN - OPUS4-56168 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kromm, Arne A1 - Kannengießer, Thomas ED - Babu, S. S. ED - Bhadeshia, H.K. ED - Cross, C.E. ED - David, S.A. ED - DebRoy, T. ED - DuPont, J.N. ED - Koseki, T. ED - Liu, S. T1 - Residual stresses in multi-layer component welds T2 - 9th International conference on trends in welding research CY - Chicago, Illinois, USA DA - 2012-06-04 KW - Shrinkage restraint KW - Component welding KW - Submerged arc welding KW - Multi-run weld KW - Residual stresses KW - Reaction force KW - XRD KW - Large scale test PY - 2013 SN - 978-1-62708-998-2 SP - 48 EP - 54 PB - ASM international AN - OPUS4-27954 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Mente, Tobias A1 - Steppan, E. A1 - Kannengießer, Thomas A1 - Steger, J. T1 - Hydrogen trapping in T24 Cr-Mo-V steel weld joints - microstructure effect vs. experimental influence on activation energy for diffusion N2 - Hydrogen-assisted cracking is a critical combination of local microstructure, mechanical load and hydrogen concentration. Welded microstructures of low-alloyed creep-resistant Cr-Mo-V steels show different hydrogen trapping kinetics. This influences the adsorbed hydrogen concentration as well as the diffusion by moderate or strong trapping. A common approach to describe hydrogen traps is by their activation energy that is necessary to release hydrogen from the trap. In the present study, Cr-Mo-V steel T24 (7CrMoVTiB10-10) base material and TIG weld metal were investigated. Electrochemically hydrogen charged specimens were analyzed by thermal desorption analysis (TDA) with different linear heating rates. The results show two different effects. At first, the microstructure effect on trapping is evident in terms of higher hydrogen concentrations in the weld metal and increased activation energy for hydrogen release. Secondly, it is necessary to monitor the real specimen temperature. A comparison between the adjusted heating rate and the real specimen temperature shows that the calculated activation energy varies by factor two. Thus, the trap character in case of the base material changes to irreversible at decreased temperature. Hence, the effect of the experimental procedure must be considered as well if evaluating TDA results. Finally, realistic temperature assessment is mandatory for calculation of activation energy via TDA. KW - Creep-resistant steel KW - Hydrogen assisted cracking KW - Thermal desorption analysis KW - Welding KW - Microstructure KW - Diffusion PY - 2018 DO - https://doi.org/10.1007/s40194-017-0546-6 SN - 0043-2288 SN - 1878-6669 VL - 62 IS - 2 SP - 277 EP - 287 PB - Springer CY - Berlin, Heidelberg AN - OPUS4-44505 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Update on "Call for interested people to contribute to series of comprehensive papers on welding and joining of components for sustainable energy systems" N2 - Based on the initial call in March 2024, an update time-frame is introduced on the working plan for a comprehensive review paper series on joining and welding technologies for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport with focus on hydrogen and wind energy. T2 - 77th IIW Annual Assembly and International Conference, Meeting of Commission II-A CY - Ixia, Rhodes, Greece DA - 07.07.2024 KW - Review paper KW - Research study KW - Hydrogen KW - Joining KW - Welding PY - 2024 AN - OPUS4-60674 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik für die neue Wasserstoffökonomie – Werkstoffe, Schweißtechnologien, Perspektiven – N2 - Die Studie gibt einen Überblick über die Aspekte der Fügetechnik und ihrer Bedeutung in Wasserstofftechnologien. Dazu werden die Grundlagen der Technologiefelder Wasserstofferzeugung, -speicherung, -transport und -nutzung vorgestellt und der Stand der Technik der fügetechnischen Fertigung von Komponenten in Wasserstofftechnologien zusammengefasst. Dabei werden nicht nur exklusiv Metalle betrachtet. Anhand repräsentativer Beispiele aus der Praxis, Forschung und Entwicklung wird die Bedeutung der Fügetechnik in Wasserstofftechnologien klar herausgestellt und mögliche Perspektiven für die Zukunft abgeleitet. Hier ist ersichtlich, dass Fügetechnologien wesentliche Bedeutung für die erfolgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien haben, von der Erzeugung bis zur Anwendung. Aus gesamtwirtschaftlicher Sicht umfassen die Schwerpunkte bzw. Trends der Fügetechnik dabei: die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie die sichere Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstoffanwendung wird die effiziente massentaugliche Produktion von Brennstoffzellen immer wichtiger. Es ist zudem klar ersichtlich, dass die additive Fertigung bereits jetzt ein hohes Potential für Komponenten von Wasserstofftechnologien besitzen und dieses wachsen wird. Aus den perspektivischen Anwendungen ergeben sich zudem Herausforderungen und Forschungsbedarfe für die notwendigen nationalen und internationalen Regelwerke und technischen Normen. Schwerpunktmäßig sind hierbei die bereits bestehenden Empfehlungen und kodifizierten Regeln vollständig zu adaptieren und in die Aus- und Weiterbildung von fügetechnischem Fachpersonal einzubetten. KW - Fügetechnik KW - Wasserstoff KW - Werkstoffe KW - Prozesse KW - Perspektiven PY - 2021 UR - https://www.dvs-media.eu/de/neuerscheinungen/4425/dvs-studie-zur-fuegetechnik-fuer-die-neue-wasserstoffoekonomie-werkstoffe-schweisstechnologien-perspektiven SN - 978-3-96144-157-0 SN - 978-3-96144-158-7 VL - 373 SP - 1 EP - 59 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53498 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schroeder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Ausscheidungsverhalten und Eigenschaften der schweißbedingten Wärmeeinflusszonen hochfester Stähle in Abhängigkeit der Mikrolegierungsroute N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustäh-len mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragver-haltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberech-nungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Aus-scheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Ab-kühlbedingungen geschaffen. T2 - Forschungsseminar BAM, BMDK CY - Magdeburg, Germany DA - 05.12.2022 KW - WEZ-Erweichung KW - Thermodynamische Simulation KW - Mikrolegierungseinfluss KW - Hochfester Feinkornbaustahl KW - Modifizierter Sprühlichtbogen PY - 2023 AN - OPUS4-56837 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kannengießer, Thomas A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien - Forschungsbedarf für die Branche N2 - Die Studie gibt einen kurzen Überblick über die jetzige Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Forschungsbedarfe für die Branche in den einzelnen Technologiefeldern Wasserstofferzeu-gung, -speicherung, -transport und -nutzung. Fügetechnologien haben dabei wesentliche Bedeutung für die er-folgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien. Die Schwerpunkte bzw. For-schungsbedarfe ergeben sich bspw. durch die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie durch Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstofferzeugung und -anwendung wird z.B. die Entwicklung effiziente Massenproduktionsmethoden von Elektrolyseuren und Brennstoff-zellen einen wichtigen Meilenstein bilden und laserbasierte Fügetechnologien sind hier zum Teil schon etabliert. Die additive Fertigung nimmt dabei eine Querschnittsposition ein und besitzt hohes Anwendungspotential für die Zukunft z.B. für die Fertigung von Komponenten in Gasturbinen. Aus den technischen Fragestellungen und For-schungsbedarfen ergeben sich zudem Herausforderungen für die notwendige Neu- und Weiterentwicklung von technischen Regelwerken und Normen und den Eingang in die Aus- und Weiterbildung von fügetechnischem Fachpersonal. T2 - DVS Congress 2021 CY - Essen, Germany DA - 14.09.2021 KW - Wasserstoff KW - Fügetechnik KW - Forschung KW - Technologie PY - 2021 AN - OPUS4-53321 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Diffusionsmessungen in UP-Mehrlagenschweißgut als effektives Tool gegen verzögerte Kaltrissbildung in Dickblechschweißungen N2 - Offshore-Windenergieanlagen bilden einen zentralen Bestandteil der zukünftigen Energieerzeugung. Hierzu notwendige Gründungs- und Turmstrukturen werden vorrangig aus UP-geschweißten Blechen aus hochfesten niedriglegierten Stählen mit Dicken bis zu 200 mm hergestellt. Die großen Blechdicken begünstigen hohe Schweißeigenspannungen und lange Diffusionswege für z. B. über den Schweißprozess eingebrachten Wasserstoff. Damit steigt das Risiko für eine wasserstoffunterstützte Kaltrissbildung (WKB) an. Zum sichereren Ausschluss von WKB in den geschweißten Komponenten wird in Abhängigkeit der Nahtgröße, Wärmeeinbringung und Stahlsorte eine Mindestwartezeit (MWZ) von bis zu 48 h empfohlen, bevor die zerstörungsfreie Prüfung durchgeführt wird. Es ist allerdings offen, ob die empfohlene MWZ zu konservativ ist. Einflüsse sind hier bspw. die schwierige Bewertung des Wasserstoffdiffusionsverhaltens im heterogenen UP-Mehrlagen-Schweißgut (SG) im Vergleich zum Grundwerkstoff (GW). Zudem sind nur sehr begrenzt H-Diffusionskoeffizienten für UP-Mehrlagen-SG als Grundlage zur Abschätzung des Zeitintervalls einer möglichen verzögerten Kaltrissbildung (somit MWZ) oder auch für Nachwärmprozeduren zur Wasserstoffreduktion (keine MWZ) verfügbar. Verlässliche H-Diffusionskoeffizienten sind daher ein adäquates Tool zur Bewertung des Risikos einer verzögerten WKB. Dieser Beitrag beschreibt Untersuchungen zur Charakterisierung der Wasserstoffdiffusionsverhalten in UP-Mehrlagen-SG eines 60 mm dicken Bleches einer Offshore-Stahlgüte. Dazu wurden Proben unterschiedlicher Dicke aus dem reinen Schweißgut extrahiert und über elektrochemische Permeation und Trägergasheißextraktion im Temperaturbereich bis 400 °C sehr interessante Ergebnisse zu den korrespondierenden Diffusionskoeffizienten erarbeitet. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - UP-Schweißen KW - Wasserstoff KW - Kaltriss KW - Permeation KW - Diffusion PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 448 EP - 459 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53369 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik für die neue Wasserstoffökonomie N2 - Die Herausforderungen für die Fügetechnikbranche, die sich durch die neuen Wasserstoff-Technologiefelder „Erzeugung“, „Speicherung“, „Transport“ und „Nutzung“ ergeben, sind sehr vielfältig. Der DVS-Bericht 373 gibt dazu einen tieferen Einblick. Der hier vorliegende Kurzbericht stellt dazu ausgewählte Praxisbeispiele, zugehörige Herausforderungen und sich ergebende Chancen vor. Fügetechnologien haben dabei wesentliche Bedeutung für das erfolgreiche Umsetzen und Herstellen der benötigten technischen Komponenten, wie anhand der Themenkomplexe „Wasserstoff-Pipelines“ und „additive Fertigung“ betrachtet wird. Zudem ergeben sich Herausforderungen für die notwendigen Regelwerke und Normen, die nahezu vollständig angepasst oder geschaffen werden müssen. KW - Wasserstoff KW - Fügetechnik KW - Studie KW - Werkstoffe KW - Schweißen PY - 2022 UR - https://www.schweissenundschneiden.de/artikel/fuegetechnik-fuer-die-neue-wasserstoffoekonomie SN - 0036-7184 VL - 74 IS - 3 SP - 142 EP - 144 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-54563 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kromm, Arne A1 - Mente, Tobias A1 - Czeskleba, Denis A1 - Brackrock, Daniel A1 - Kannengießer, Thomas T1 - Bauteilversuch zur Bewertung der wasserstoffunterstützten Rissanfälligkeit geschweißter, dickwandiger Offshore-Gründungsstrukturen N2 - Offshore-Windenergieanlagen erfordern Gründungskonzepte aus unterpulver-(UP-)geschweißten Dickblechen (bspw. der Güte S420ML). Während der Schweißfertigung kann eine zeitverzögerte wasserstoffunterstützte Kaltrissbildung auftreten, deren Bewertung aufgrund der Bauteilgröße von Offshore-Strukturen sehr komplex ist. Deswegen wurde eine bauteilähnliche Geometrie (Mock-Up) entwickelt, um reale Steifigkeitsverhältnisse auf den Labormaßstab zu übertragen. Zusätzliche Versteifungen simulieren die Wirkung einer Einspannung bzw. Schrumpfbehinderung der Schweißnaht. Über die Verwendung von Schweißpulvern mit definierter Feuchte wurden zudem ein Extremszenario der Wasserstoffaufnahme simuliert. Entsprechend der vorgegebenen Mindestwartezeit für die ZfP von bis zu 48 h wurde die Schweißnaht zerstörungsfrei mit Phased-Array-Ultraschall-Prüfung (PAUT) geprüft und die Eigenspannungen über Röntgendiffraktometrie (XRD) bestimmt. Zusätzlich wurde die Wasserstoffverteilung in der Schweißverbindung numerisch simuliert. Außer zulässigen Defekten (wie Poren), wurde keine verzögerte Kaltrissbildung in den Mock-Ups festgestellt, was auf hohe Rissbeständigkeit hindeutet. T2 - Tagung Werkstoffprüfung 2023 CY - Berlin, Germany DA - 23.11.2023 KW - Kaltrissbildung KW - Wasserstoff KW - Offshore KW - Schweißen KW - Bauteiltest PY - 2023 DO - https://doi.org/10.48447/WP-2023-219 SP - 316 EP - 321 CY - Berlin AN - OPUS4-58908 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Koshkina, Olga A1 - Bantz, C. A1 - Würth, Christian A1 - Lang, Thomas A1 - Resch-Genger, Ute A1 - Maskos, Michael T1 - Fluorophore-labeled siloxane-based nanoparticles for biomedical applications N2 - We present the synthesis and characterization of multifunctional fluorophore-labeled poly(organosiloxane) nanoparticles with core-shell architecture, where the fluorescent dye is incorporated into the core. Grafting of heterobifunctional poly(ethylene oxide) (PEO) onto the particle surface leads to water-soluble biocompatible nanoparticles. Two different strategies have been used for the synthesis: The encapsulation of dye-labeled monomers during the polycondensation with additional PEO coating and subsequent dye labeling by covalent attachment of the fluorescent dye rhodamine B to the (chloromethylphenyl)siloxane groups in the core after polymerization and grafting of PEO onto the surface. Comparison of the fluorescence quantum yields of the nanoparticles before and after PEO coating show a decrease in quantum yield after PEO coating. KW - Biocompatibility KW - Core-shell KW - Fluorescence KW - Fluorescence quantum yield KW - Nanoparticles KW - PEO PY - 2011 DO - https://doi.org/10.1002/masy.201100041 SN - 1022-1360 SN - 0258-0322 SN - 1521-3900 VL - 309/310 IS - 1 SP - 141 EP - 146 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-25143 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Masoud Nia, Niloufar A1 - Nietzke, Jonathen A1 - Kannengiesser, Thomas T1 - Ti and Nb microalloying of HSLA steels and its effect on hydrogen diffusion and trapping N2 - Fine-grain, high-strength, low-alloy (HSLA) structural steels with yield strengths > 600 MPa are now the state of the art in construction applications such as mobile cranes and civil engineering. HSLA grades derive their strength from a combination of specific heat treatment and the underlying chemical composition. In this context, Ti or Nb are essential to obtain a fine-grained microstructure as well as the necessary carbides or nitrides for precipitation strengthening. In this context, the specific effect of Ti or Nb-rich compounds on hydrogen trapping and diffusion is well known for special laboratory cast alloys, but unknown for realistic steel compositions. For this reason, a series of S690Q-based alloys were synthesized, close to a real steel composition, but with well controlled Ti or Nb additions in different amounts. Specimens were obtained from these alloys by electrochemical discharge machining (EDM). The specimens were tested using the well-established electrochemical permeation technique. From the experimental results, the hydrogen diffusion coefficients and the analytical subsurface hydrogen concentration were calculated. In addition, the hydrogen trapping behavior at elevated temperatures was interpreted by thermal desorption analysis (TDA) using different heating rates of hydrogen charged samples. The results showed that in contrast to metallurgically "pure" laboratory cast alloys, realistic chemical compositions were similar in their hydrogen trapping behavior, despite some small differences. All investigated steel grades exhibited shallow and reversible hydrogen trapping, regardless of their chemical composition. Of course, the experiments only allowed the calculation of effective diffusion coefficients and trapping energies, which represent an average of the entire microstructure. Nevertheless, HSLA steels are typically joined by arc welding, which includes the risk of delayed hydrogen assisted cracking. From the point of view of welding practice, however, a more or less identical hydrogen diffusion behavior means that no special "metallurgically specific", justifiable measures need to be considered, despite the well-established processes such as "soaking" or dehydrogenation heat treatment. T2 - MPAC 2025 CY - Stuttgart, Germany DA - 06.10.2025 KW - HACC KW - Hydrogen KW - HSLA PY - 2025 AN - OPUS4-64337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -