TY - CONF A1 - Paul, Andrea A1 - Heilmann, M. T. A1 - Schmid, Thomas A1 - Maiwald, Michael T1 - Multivariate classification of Raman spectra from synthetic polymers – an approach for the improved detection of microplastics N2 - The increasing pollution of terrestrial and aquatic ecosystems with plastic debris, which leads to the accumulation of microscopic plastic particles of still unknown fate, is an upcoming problem of our time. In order to monitor the degree of contamination and to understand the underlying processes of degradation and internalization of plastic debris, analytical methods are urgently needed, which help to identify and quantify microplastics. Currently, expensive collected and purified materials enriched on filters are investigated by (micro) infrared spectroscopy (FTIR). Few studies using micro-Raman spectroscopy have been published as well. In contrast to FTIR, Raman spectroscopy can handle wet samples, but it suffers from interference of fluorescent materials. Both micro-FTIR- and micro-Raman, always include time consuming scanning and mapping procedures followed by the manual inspection and measurement of selected particles. T2 - 11. Kolloquium Arbeitskreis Prozessanalytik CY - Wien, Austria DA - 30.11.2015 KW - Prozessanalytik KW - Microplastics KW - Mikroplastik KW - Raman-Spektroskopie KW - Polymers KW - Multivariate classification PY - 2015 SP - 80 EP - 81 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-38847 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hübert, Thomas A1 - Hattermann, Hilke A1 - Griepentrog, Michael T1 - Sol-gel-derived nanocomposite coatings filled with inorganic fullerene-like WS2 N2 - Silica coatings filled with nanoscaled inorganic fullerene-like tungsten disulphide (IF-WS2) have been prepared through a sol–gel process on stainless steel substrates, and the structure and mechanical properties have been investigated. The precursor was prepared from a mixture of colloidal silica, 3-glycidoxypropyltrimethoxysilane (GLYMO), water and ethanol, adjusted to pH 4 with HNO3. In this solution WS2 is dispersed and in some cases immediately before coating ethylenediamine (ED) is added. The stainless steel substrates are dip-coated, dried in air and heat-treated in the temperature range of either 150–360 °C in air or up to 900 °C in vacuum. The solidification process is followed by differential thermal analysis (DTA). The resulting brown coloured coatings have a thickness of 1.5–4 µm. Scanning electron microscopy investigations (SEM) show that the WS2 nanoparticles are embedded as small aggregates in a hybrid silica matrix. X-ray diffraction (XRD) measurements prove that most of the tungsten disulphide embedded in the matrix can be protected against oxidation even after curing the samples at temperatures up to 900 °C. Hardness and modulus of the hybrid silica films were measured through an instrumented indentation test. Increasing the temperature of the heat treatment yields an increase of hardness from 0.3 to 1 GPa and of modulus from 3 to 17 GPa. The amount of up to 10 wt.% WS2 in the coatings has no remarkable influence on hardness and modulus of the samples. KW - Nanocomposites KW - Tungsten disulphide KW - Sol-gel KW - Mechanical properties PY - 2009 DO - https://doi.org/10.1007/s10971-009-1896-3 SN - 0928-0707 SN - 1573-4846 VL - 51 IS - 3 SP - 295 EP - 300 PB - Kluwer Academic Publ. CY - Dordrecht AN - OPUS4-19713 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hübert, Thomas A1 - Unger, Brita A1 - Bücker, Michael T1 - Sol-gel derived TiO2 wood composites N2 - The sol–gel process was applied to enhance properties of pine sapwood. For this purpose wood prisms were soaked in nanoscaled precursor solutions prepared from titanium(IV) n-butoxide and titanium(IV) iso-propoxide, respectively, using vacuum impregnation technique. The wet composites were cured by special program with final heat treatment at 103 °C. Weight percent gains (WPG) of the wood specimen in the range of 19-25% were obtained due to these procedures. SEM investigations show that precursor solutions penetrate into the whole wood body and the titania formed after heat treatment in the composites is deposited in the pores (lumen) and partly in the cell walls of the wooden matrix. The moisture sorption was investigated in long term tests for a period of some months by storage at 20-23 °C in humid air (relative humidity of 99%) and ambient atmosphere (relative humidity 40-60%), respectively. For untreated reference samples the moisture sorption results in increasing of mass and volume according to saturation values of 24 and 13%, respectively, after about 15 days. The incorporation of titania reduces the saturation values of the moisture sorption by up to 12% in mass and by up to 5% in volume at a relative humidity of 99%. Thus, an enhancement of the dimensional stability of about 60% is obtained at best. The results demonstrate that modification of wood with sol-gel derived precursors can enhance its dimensional stability, which prevents the formation of cracks. Because of that reduced moisture sorption biological attacks should be delimited. Additionally, thermal analyses show a retarded combustion of the wood matrix due to titania infiltration. KW - Titania KW - Sol-gel KW - Nanocomposites KW - Wood protection KW - Water sorption PY - 2010 DO - https://doi.org/10.1007/s10971-009-2107-y SN - 0928-0707 SN - 1573-4846 VL - 53 IS - 2 SP - 384 EP - 389 PB - Kluwer Academic Publ. CY - Dordrecht AN - OPUS4-20892 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Coniglio, Nicolas A1 - Cross, Carl Edward A1 - Michael, Thomas A1 - Lammers, Marco T1 - Defining a critical weld dilution to avoid solidification cracking in aluminum N2 - Al-Mg-Si alloys are known to be highly susceptible to solidification cracking except when using an appropriate filler metal (e.g., 4343 or 5356), although the amount of dilution required to avoid cracking has never been a well-defined quantity. The aim of the present study is to determine a relationship between filler metal dilution, local strain rate conditions, and cracking susceptibility. Making use of the controlled tensile weldability (CTW) test and local strain extensometer measurements, a boundary has been established between crack and non-crack conditions for different local strain rates and dilution amounts, holding all other welding parameters constant. This boundary, presented in the form of critical strain rate-dilution map, defines the critical amount of 4043 filler metal required to avoid solidification cracking when arc welding 6060 aluminium, depending upon local strain rate. T2 - Light Alloy Seminar CY - Clausthal, Germany DA - 2006-11-20 KW - Dilution KW - Solidification Cracking KW - Al-Mg-Si Alloys KW - 6060 Aluminium KW - Arc Welding KW - Strain Rate KW - 4043 Filler Dilution PY - 2008 SN - 0043-2296 SN - 0096-7629 VL - 87 IS - 8 SP - 237 EP - 247 PB - American Welding Society CY - New York, NY AN - OPUS4-18311 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erhard, Anton A1 - Goedecke, Thomas A1 - Pötzsch, Klaus-Michael A1 - Pagenkopf, Marion T1 - Vibrations- und Stoßbelastungen an IBCs und Tankfahrzeugen N2 - Die unterschiedlichen Stoß- und Vibrationsbelastungen bei der Fahrt auf Straßen oder im freien Gelände dürften den meisten Lesern aus dem täglichen Leben bekannt sein. Je nach Ausführung und Zustand des Feder-/Dämpfungssystems eines Fahrzeuges spürt der menschliche Körper unterschiedliche Belastungen, die die Schmerzgrenze erreichen können. Diese dynamischen Belastungen werden auch auf Ladung, in unserem Fall auf die Gefahrgutumschließungen und auf das Gefahrgut, übertragen. Derartige Belastungen können durch entsprechende Stapelung und Sicherung der Ladung in ihren Auswirkungen gemindert werden. Für andere Belastungen, z. B. Stoß durch einen Auffahrunfall, sind Schutzsysteme am Heck des Fahrzeugs gefordert. Bei Tankfahrzeugen kann eine Beschädigung des Tanks durch einen solchen Auffahrschutz gemindert werden. Im vorliegenden Beitrag werden Ergebnisse von Vibrationsmessungen an Lastkraftwagen mit den Ergebnissen des Vibrationstests an einem Intermediate Bulk Container (IBC) verglichen. Berechnungen zum Auffahrschutz an Tankfahrzeugen werden Messergebnissen gegenübergestellt. KW - Gefahrgutverpackungen KW - Belastung KW - Tankfahrzeug KW - Unfallszenarien PY - 2010 DO - https://doi.org/10.3139/120.110100 SN - 0025-5300 N1 - Geburtsname von Pagenkopf, Marion: Nitsche, M. - Birth name of Pagenkopf, Marion: Nitsche, M. VL - 52 IS - 1-2 SP - 63 EP - 70 PB - Hanser CY - München AN - OPUS4-20835 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Österle, Werner A1 - Griepentrog, Michael A1 - Gross, Thomas A1 - Urban, Ingrid T1 - Chemical and microstructural changes induced by friction and wear of brakes N2 - The chemical and microstructural changes occurring during braking simulation tests at the surface of a conventional brake pad material were investigated mainly by scanning and transmission electron microscopy and surface analytical techniques. It can be shown that patches of a third body material develop, comprising a compositional mix of all constituents of the pad and iron oxides from the disk. Milled debris particles still have the crystal structure of barite, the major phase of the pad material, but the grain size is reduced drastically to the nanometer scale. The major wear mechanism is delamination of filler particles from the organic binder, supported by local degradation of the phenolic resin during asperity heating. Quartz crystals are preserved thereby adopting the function of primary contact areas. KW - Brake KW - Third body material KW - Friction layer KW - Electron microscopy PY - 2001 DO - https://doi.org/10.1016/S0043-1648(01)00785-2 SN - 0043-1648 VL - 251 SP - 1469 EP - 1476 PB - Elsevier CY - Amsterdam AN - OPUS4-2371 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stelling, Karen A1 - Michael, Thomas A1 - Schobbert, Helmut T1 - Erstarrungsverhalten und Schweißeignung austenitischer Stähle beim Laserstrahl- und Hybridschweißen KW - Laser KW - Laserstrahlschweißen KW - Hybridschweißen KW - Austenitischer Stahl KW - Ferrit KW - Austeniti KW - Erstarrung PY - 2006 SN - 0036-7184 VL - 58 IS - 10 SP - 526 EP - 534 PB - Verl. für Schweißen u. Verwandte Verfahren, DVS-Verl. CY - Düsseldorf AN - OPUS4-13933 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schendler, Thomas A1 - Michael-Schulz, Heike T1 - Schutzmaßnahmen bei der Lagerung von ammoniumnitrathaltigen Zubereitungen T2 - Technische Jahreskonferenz der BG Chemie CY - Berlin, Germany DA - 2006-05-23 PY - 2006 AN - OPUS4-13859 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stelling, Karen A1 - Michael, Thomas A1 - Schobbert, Helmut T1 - Solidification behaviour and weldability of austenitic steels in laser and hybrid welding N2 - Within the framework of an AiF (The German Federation of Industrial Research Associations) project, investigations were conducted into the solidification behaviour of various high-alloy austenitic steels in laser and laser-GMA hybrid welding. For comparison purposes, reference was made to pure gas metalarc welding tests. It was possible to raise the welding speeds in hybrid welding compared with the individual gas metal-arc (GMA) and laser welding processes. The central subjects of the investigations were the type of solidification and the connected hot cracking behaviour during welding. In this respect, particular attention was paid not only to the kinetic effects during solidification which may be caused by the high solidification rates in laser and hybrid welding but also to their consequences. KW - Welding KW - Austenitic stainless steel KW - Solidification KW - Laser KW - Hybrid welding PY - 2007 SN - 1612-3433 VL - 6 IS - 3 SP - 171 EP - 175 PB - DVS - German Welding Society CY - Düsseldorf AN - OPUS4-15068 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Unger, Brita A1 - Bücker, Michael A1 - Reinsch, Stefan A1 - Hübert, Thomas T1 - Chemical aspects of wood modification by sol-gel-derived silica N2 - It has been shown that tetraethoxysilane-derived precursors are suitable solutions for impregnating pine sapwood to improve its dimensional stability. Tailored sol–gel syntheses result in precursors with nano-scaled silica species which are able to penetrate into the cell walls of wood. The physical fixation of those species inside the cell walls was verified by ESEM/EDX investigations. There is evidence that the silica species are chemically bonded to wood components. Nonreacted alkoxy groups can exist in the wood composites after impregnation. The amount of these organic residues depends on the composition of the precursors, especially their condensation degree and reactivity. Treatments for finishing the composites after the impregnation step to get clean products and stable properties are discussed in this context. An explanation of the complex relationship between solids content in the impregnation solutions and percentage weight gain and bulking of the composites is given. It can be demonstrated that high WPG values (>20 %) are pre-conditions for an effective protection of the resulting composites but they only guarantee efficient improvements if connected with the incorporation of the inorganic component inside the cell walls. Therefore, the sol–gel syntheses have to be carried out in such a manner that very small (<2 nm) as well as reactive species are sufficiently available. This demands syntheses using sub-stoichiometric water contents (H2O/TEOS <4, better <2). KW - Silica-wood composites KW - Sol-gel derived precursors KW - Curing KW - Fixation of silica KW - Dimensional stability PY - 2013 DO - https://doi.org/10.1007/s00226-012-0486-7 SN - 0043-7719 SN - 1432-5225 VL - 47 IS - 1 SP - 83 EP - 104 PB - Springer CY - Berlin AN - OPUS4-26258 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Noack, Volker A1 - Michael, Thomas T1 - Weichplasmaschweißen - Qualitativ hochwertige Überlappverbindungen an korrosionsbeständigen Werkstoffen T2 - Große Schweißtechnische Tagung CY - Kassel, Deutschland DA - 2002-09-25 PY - 2002 SN - 3-87155-679-3 N1 - Serientitel: DVS-Berichte – Series title: DVS-Berichte IS - 220 SP - 308 EP - 315 PB - Verl. für Schweißen und Verwandte Verfahren, DVS-Verl. CY - Düsseldorf AN - OPUS4-1750 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Experimental and numerical characterization of hydrogen diffusion in thick-walled submerged arc welded joint of S420G2+M offshore steel grade N2 - Offshore wind turbines are an important goal in national energy strategies worldwide. Foundation structures are manufactured from submerged arc welded (SAW) plates with thicknesses up to 200 mm. In that connection, high-strength steels like the S420G2+M are more and more applied offering the possibility for increased stability and load-bearing capacity of the foundations. These offshore steel grades can show a susceptibility for delayed hydrogen assisted cold cracking of the weld joints. For that purpose, a minimum waiting time (MWT) of up to 48 h (dependent on applied standards) is recommended before non-destructive testing is allowed and conducted. But this concept is based on older steel grades that have been used for three or more decades. Nowadays, the metallurgical improvements (clean steels, proper rolling, and heat treatment) of base materials and well as welding consumables must be anticipated. Hence, the MWT concept should be critically discussed as it is assumed to be very conservative. For that reason, the focus of this study was to investigate the diffusion behavior in S420G2+M steel and its multi-layer SAW joint. Electrochemical permeation experiments were carried at room temperature. Boundary conditions were anticipated in terms of using different sample thicknesses. From the experimental data, hydrogen diffusion coefficients and absorbed diffusible hydrogen concentrations had been calculated. It was shown that hydrogen diffusion in the base material is increased compared to the weld metal. In addition, the sample thickness had a significant on the calculated diffusion coefficients. The minimum and maximum diffusion coefficients had been used for numerical modelling of the hydrogen diffusion in the welding joint. It became clear that a MWT must be always regarded together with a critical initial diffusible hydrogen concentration for the evaluation of a possible delayed cracking as diffusion times were mostly > 48 h due to the thick plates. T2 - 4th International Conference on Metals and Hydrogen - Steely & Hydrogen 2022 CY - Ghent, Belgium DA - 11.10.2022 KW - Hydrogen KW - Submerged arc welding KW - Diffusion KW - Minimum waiting time KW - Electrochemical permeation PY - 2022 SP - 1 EP - 11 CY - Ghent, Belgium AN - OPUS4-56075 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Czeskleba, Denis A1 - Kannengießer, Thomas T1 - Untersuchung von Spannungsrelaxationsrissmechanismen mittels Simulation einachsiger Spannungszustände in der Grobkornzone von UP-geschweißtem CrMoV-Stahl N2 - Druckbehälter mit großen Wandstärken (250+ mm) aus hochwarmfesten, niedriglegierten Stählen werden hauptsächlich Mehrdraht-Unterpulver-(UP) geschweißt. Der damit verbundene hohe Energieeintrag führt unter anderem zu hohen lokalen Schweißeigenspannungen, welche bei unsachgemäßer Prozessführung der notwendigen Wärmenachbehandlung (PWHT) zu Spannungsrelaxationsrissen (SRR) führen. In den Bewertungskriterien zur Spannungsrelaxationsrissanfälligkeit finden weder die, mit klassischen, freischrumpfenden Schweißversuchen nicht abbildbaren, erhöhten Eigenspannungen aus der Schrumpfbehinderung der Bauteilsteifigkeit Beachtung, noch die damit einhergehenden metallurgischen Effekte wie bspw. das Ausscheidungswachstum während der PWHT und damit einhergehende Härteunterschiede an den Korngrenzen bzw. die vorzeitige Alterung durch Bildung differenter Sonderkarbide. Die Aufheizrate des PWHT als Einflussfaktor für die SRR-Bildung bleibt derzeit ebenfalls unbeachtet. Daher wurde eine Versuchsmethodik entwickelt, die eine mögliche SRR-Anfälligkeit durch die Kopplung von thermischer und mechanischer Beanspruchung untersucht. Dazu wurden Proben mit unterschiedlichen Gefügen thermisch simuliert und während des PHWT repräsentativ mit sehr hohen Lasten/Eigenspannungen mechanisch beansprucht. Dazu wurde an Kleinzugproben für das as-welded UP-Schweißgut und die thermisch simulierte GKZ eines 13CrMoV9-10 die Dehnung des Prüfbereichs bei variablen Querspannungen und Aufheizraten gemessen. Diese aufheizraten- und gefügeabhängige Längenänderung der Probe wurde durch mathematische Prozeduren analysiert. Damit war es möglich, singuläre werkstoffliche Effekte auf μm-Ebene (Ausscheidungswachstum) als summarische Längen- bzw. Volumenänderung per klassischer Kurvendiskussion zu beschreiben. Die erste und zweite Ableitung zeigten eine ausscheidungsabhängige Härtezunahme, welche von der Spannung und Aufheizrate im geringen Maß linear abhängig war. Gleichzeitig sind Volumenänderungen bei Bildung und Wachstum differenter Sonderkarbide bekannt, welche zusammen mit gefügespezifischen Untersuchungen und der neuen Versuchsmethodik zu einer verbesserten Beurteilung der SRR-Anfälligkeit von geschweißten CrMoV-Stählen beitragen sollen. Prinzipiell ist die vorgestellte Methodik jedoch werkstoff- und zustandsoffen, d.h. sowohl für Grundwerkstoff e als auch definierte Wärmebehandlungsbedingungen geeignet. Dies ermöglicht erstmals die Schaffung einer Transfergröße zwischen Labor und realen Schweißungen, unter Beibehaltung der Bauteilsteifigkeit, d.h. vereinfachte, aber realistische Eigenspannungsabbildung als Grundlage für weitergehende gefügespezifische metallurgische Effekte während des PWHT. T2 - DVS Congress 2022 CY - Koblenz, Germany DA - 19.09.2022 KW - UP-Schweißen KW - Spannungsrelaxationsriss KW - Wärmenachbehandlung KW - Ersatzgeometrie KW - Prüfverfahren PY - 2022 SN - 978-3-96144-190-7 VL - 382 SP - 69 EP - 75 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-55946 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Call for interested people to contribute to series of comprehensive papers on welding and joining of components for sustainable energy systems N2 - Joining and welding technologies are of high importance for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport. In that connection, offshore and on-shore installed wind turbines are of high interest for the generation of electrical energy as well as photo-voltaic systems (solar cells). The electricity can be either directly transported or conversed via power-to-gas e.g., to hydrogen. In that scope, electrolyzer up to MW-range are of interest as well as the conver-sion back to electricity via fuel cells. In addition, hydrogen is a key element of the decarburization of in-dustries as well as the mobility sector encompassing sea, air and land transportation driven by hydrogen or its derivates. Well-known examples cover the direct reduction of iron ore to replace the conventional blast furnace process up to gas turbines or fuel cells for home-end use. All mentioned technologies re-quire reliable components, which are to a high extend dependent on joining and especially welding pro-cessing of materials. Especially, the (petro-) chemical industry has many years of experience with both materials used in hydrogen applications. The challenge is e.g., the transition to mass production of sys-tem components of electrolyzers/fuel cells and for distribution grids. At this point, the scalability of cur-rently applied joining processes often limits the economic efficiency, whereas especially laser welding or additive manufacturing will be of high interest. In that connection, it is very important to provide answers by joint research of universities, institutes, and industrial companies. Very often, solutions are already available and “just” have to be investigated and adapted for the new application, like repair welding of NG pipelines. For that reason, we want to set up a series of comprehensive papers with the aforementioned title. The idea is to get an in-depth but manageable overview of the importance of joining technologies in sustaina-ble energy generation, conversion, and transport encompassing current processes, limitations, and fur-ther perspectives. In that connection, the additive manufacturing is gaining more and more attention. If applicable, current challenges in the adaption or creation of new standards/regulations shall be addressed. T2 - IIW Intermediate Meeting, Com. II-A CY - Incheon, Republic of Korea DA - 12.03.2024 KW - Hydrogen KW - Welding KW - Comprehensive study KW - Component manufatcturing KW - Additive manufacturing PY - 2024 AN - OPUS4-59676 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik in Wasserstofftechnologien - Forschungsbedarf für die Branche (Kurzversion) N2 - Die Studie gibt einen kurzen Überblick über die jetzige Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Forschungsbedarfe für die Branche in den einzelnen Technologiefeldern Wasserstofferzeugung, -speicherung, -transport und -nutzung. Fügetechnologien haben dabei wesentliche Bedeutung für die erfolgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien. Die Schwerpunkte bzw. Forschungsbedarfe ergeben sich bspw. durch die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie durch Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstofferzeugung und -anwendung wird z.B. die Entwicklung effiziente Massenproduktionsmethoden von Elektrolyseuren und Brennstoffzellen einen wichtigen Meilenstein bilden und laserbasierte Fügetechnologien sind hier zum Teil schon etabliert. Die additive Fertigung nimmt dabei eine Querschnittsposition ein und besitzt hohes Anwendungspotential für die Zukunft z.B. für die Fertigung von Komponenten in Gasturbinen. Aus den technischen Fragestellungen und Forschungsbedarfen ergeben sich zudem Herausforderungen für die notwendige Neu- und Weiterentwicklung von technischen Regelwerken und Normen und den Eingang in die Aus- und Weiterbildung von fügetechnischem Fachpersonal. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - Wasserstoff KW - Fügetechnik KW - Forschung KW - Werkstoff KW - Bedarf PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 612 EP - 624 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53370 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Czeskleba, Denis A1 - Kannengießer, Thomas T1 - Kurzbericht zum Projekt „Entwicklung von Wärmenachbehandlungskonzepten zur Vermeidung von Spannungsrelaxationsrissen an Bauteilen aus hochwarmfesten Stählen“ (DVS-Nr. 01.2261 / IGF-Nr. 20171 N) N2 - Komponenten aus dickwandigen, hochwarmfesten CrMoV-Stählen erfordern eine anspruchsvolle UP-Schweißverarbeitung. Dabei muss die notwendige Wärmenachbehandlung der Schweißnaht (PWHT) sicher beherrscht werden. Hier kann u.U. Bauteilversagen infolge von Spannungsrelaxationsrissbildung (SRR) auftreten. Bislang erfolgt die Beurteilung der SRR-Neigung primär über Ersatzgrößen, wie temperaturbedingte Änderung der Härte und Duktilität. Die Wirkung der konstruktiven Schrumpfbehinderung einer Schweißnaht auf die SRR ist bislang völlig unbekannt. Hier setzt das Forschungsprojekt an, hinsichtlich der Gewinnung und Optimierung der Parameter für die PWHT unter realitätsnahen Bauteilsteif igkeiten (def inierte Einspannbedingung) mit dem Ziel der SRR-Vermeidung. Am Beispiel des niedriglegierten, hochwarmfesten Stahls 13CrMoV9-10 wurden UP- Schweißungen unter industriepraktischen Bedingungen freischrumpfend bzw. unter definierter Schrumpfbehinderung durchgeführt. Diese wurden mit unterschiedlichen PWHT-Szenarien (Variation der Auf heizrate und Endtemperatur) beaufschlagt. Die Ergebnisse des Projektes DVS 01.2261 / IGF 20171 N werden in diesem Beitrag vorgestellt, wie Aussagen zur SRR-Suszeptibilität in Abhängigkeit von Mikrostruktur und vorliegender mehrachsiger mechanischer Beanspruchung der Schweißnaht vor/während des PWHT. Für einen kritischen Zustand sind hohe Kräfte / Spannungen notwendig, die in freischrumpfenden Schweißversuchen u.U. nicht abbildbar sind. Die Berücksichtigung des mikrostrukturspezifischen Ausscheidungsverhaltens (in Schweißgut und Wärmeeinflusszone) unter realitätsnahen Einspannbedingungen ist für die Bewertung einer SRR-Suszeptibilität notwendig. Instrumentierte Schweißversuche unter definierter Schrumpfbehinderung ermöglichen hier das Monitoring der entstehenden Reaktionskräfte, -momente bzw. -spannungen. Ausgehend von diesem Referenzzustand erfolgte die Applikation der PWHT-Szenarien bzw. deren praktische Überprüfung. Zusätzlich wurde eine Ersatzprüfmethodik entwickelt, die die Betrachtung der mikrostrukturspezifischen SRR-Suszeptibilität unter Beibehaltung der äußeren Schrumpfbehinderung der Schweißnaht während des PWHT ermöglicht. Hierdurch wird die Bauteilübertragbarkeit ermöglicht und eine Transfergröße geschaffen, welche die Bauteilbewertung hinsichtlich der SRR-Neigung umfasst. T2 - DVS Congress 2022 CY - Koblenz, Germany DA - 19.09.2022 KW - UP-Schweißen KW - Spannungsrelaxationsriss KW - Forschungsprojekt KW - Dickblech KW - Wärmebehandlung PY - 2022 SN - 978-3-96144-190-7 SP - 76 EP - 82 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-55944 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Experimentelle Bestimmung und thermodynamische Modellierung des Ausscheidungsverhaltens in der WEZ eines S690QL bei unterschiedlichen Mikrolegierungsrouten N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Normstreckgrenze > 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente bzw. ihrer Karbide und/oder Nitride ist teilweise komplett konträr, insbesondere bei Auflösung und Wiederausscheidung in der WEZ bei identischem Schweißzusatz. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragverhaltens der Schweißverbindung erschwert. Zuzüglich können moderne Schweißprozesse, wie MSG mit modifiziertem Sprühlichtbogen (mod. SLB) durch ihre hohe Wärmeeinwirkung die Phasenumwandlung in der Wärmeeinflusszone negativ beeinflussen. Eine unerwünschte Eigenschaft ist dabei die Erweichung (engl.: softening) der WEZ, wie auch u.U. der gegenteilige Effekt der Aufhärtung (engl.: hardening). Vor diesem Hintergrund werden im Rahmen eines DFG-Vorhabens systematisch Mikrolegierungsrouten mit variierenden Ti- und Nb-Gehalten des hochfesten und vergüteten Feinkornbaustahls S690QL untersucht. Dazu wird das MAGSchweißen mit mod. SLB verwendet, welches durch hohe Abschmelzleistung gekennzeichnet ist und schmalere Fugenöffnungswinkel (α = 30°) ermöglicht. An diesen Schweißungen wird der Effekt der metallurgischen Zusammensetzung in Kombination mit hoher Wärmeeinwirkung auf die Ausbildung einer kritischen WEZ-Gefügezone mit Erweichung und/oder exzessiver Aufhärtung untersucht. Ein besonderes Augenmerk wird auf die Phasenumwandlungen und das Ausscheidungsverhalten im Gefüge der Wärmeeinflusszone gelegt. Neben umfangreichen metallographischen Untersuchungen einzelner WEZ-Bereiche wurden, unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberechnungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation und Ausscheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Abkühlbedingungen geschaffen. Das Ziel ist es, mittels erster Untersuchungen den Einfluss der Wärmeeinwirkung auf die Gefügeausbildung in der WEZ zu zeigen. Insbesondere wird hier auf die Auswirkung der unterschiedlichen Mikrolegierungskonzepte (Ti oder Nb) geachtet. T2 - DVS CONGRESS 2022 - Große Schweißtechnische Tagung CY - Koblenz, Germany DA - 19.09.2022 KW - WEZ-Erweichung KW - Hochfester Feinkornbaustahl KW - ThermoCalc KW - Thermodynamische Simulation KW - Mikrolegierungselemente KW - Modifizierter Sprühlichtbogen PY - 2022 SN - 978-3-96144-189-1 SN - 978-3-96144-190-7 VL - 382 SP - 131 EP - 137 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-55834 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Welding KW - Hydrogen pipeline KW - Review PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638847 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63884 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Czeskleba, Denis A1 - Irfan, Muhammad Dary A1 - Wandtke, Karsten A1 - Kaiser, Sebastian A1 - Kannengießer, Thomas T1 - Wasserstoffdiffusion in hochfesten UP-Schweißverbindungen – einfacher als gedacht N2 - Hochfeste Baustähle werden im modernen Stahlbau aus wirtschaftlichen und konstruktiven Gründen zunehmend eingesetzt, z. B. im Gebäude-, Anlagen- oder Mobilkranbau. Durch den Einsatz von Stählen mit höheren 690 MPa) können durch die Reduzierung der Wanddicke erhebliche Gewichtsreduzierungen und geringere Verarbeitungskosten erreicht werden, insbesondere bei der Verwendung des Unterpulverschweißen (UP) durch seine hohe Abschmelzleistung. Aufgrund ihrer speziellen Mikrostruktur haben hochfeste Stähle eine begrenzte Duktilität und sind anfälliger für wasserstoffunterstützte Kaltrisse (HACC). Darüber hinaus führen große mittels UP geschweißter Blechdicken zu hohen Schweißeigenspannungen und langen Diffusionswegen für z.B. durch den Schweißprozess eingebrachten Wasserstoff. Abgesicherte Diffusionskoeffizienten für UP-Schweißungen dieser Festigkeitsklasse sind als Grundlage für die Abschätzung des Zeitintervalls einer möglichen verzögerten Kaltrissbildung oder für Nachwärmung zur Wasserstoffreduktion nur sehr begrenzt verfügbar. Aus diesem Grund wurden experimentelle Versuche zur mikrostruktur-spezifischen Diffusion in S690-Schweißungen durchgeführt. Dazu wurde ein thermomechanisch (TM) gewalzter bzw. vergüteter (QL) Zustand dieses Werkstoffs betrachtet, sowie das jeweilige charakteristische Schweißgut und WEZ. Dazu wurden den Schweißmikrostrukturen lokal Proben entnommen und über Permeations- bzw. Warmauslagerungsversuche die gefügespezifische Diffusion von Raumtemperatur bis 400°C charakterisiert. Im Gegensatz zu bekannten Effekten des Wärmebehandlungszustandes der Grundwerkstoffe auf die Diffusion in MSGSchweißverbindungen, zeigten die Wasserstoffdiffusionskoeffizienten über alle untersuchten Gefügezustände keine signifikanten Unterschiede, insbesondere nicht für die lokale WEZ diverser, untersuchter Streckenergiebereiche. Aus praktischer Anwendersicht können daher dickwandige UP-Verbindungen hinsichtlich einer verzögerten Wasserstoffdiffusion nur anhand der einfach ermittelbaren Diffusionskoeffizienten für den Grundwerkstoffkoeffizient beurteilt werden. Zudem zeigte sich, dass der unterschiedliche Walz- und Wärmebehandlungszustand (TM vs. QL) in UP-Schweißnähten eine untergeordnete Rolle für die Wasserstoffdiffusion und damit für die mögliche Zeitverzögerung der Kaltrissbildung hat. Ergänzende numerische Simulationen der Wasserstoffverteilung bestätigten das Verhalten. T2 - DVS Congress 2025 CY - Essen, Germany DA - 16.09.2025 KW - Unterpulverschweißen KW - Wasserstoffdiffusion KW - Wasserstoffunterstützte Kaltrissbildung KW - Wasserstoffrisse PY - 2025 SN - 978-3-96144-299-7 DO - https://doi.org/10.53192/DVSC20250330 VL - 401 SP - 330 EP - 340 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-64132 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Prabitz, Konstantin Manuel A1 - Antretter, Thomas A1 - Rethmeier, Michael A1 - El-Sari, Bassel A1 - Schubert, Holger A1 - Hilpert, Benjamin A1 - Gruber, Martin A1 - Sierlinger, Robert A1 - Ecker, Werner T1 - Numerical and experimental assessment of liquid metal embrittlement in externally loaded spot welds N2 - Zinc-based surface coatings are widely applied with high-strength steels in automotive industry. Some of these base materials show an increased brittle cracking risk during loading. It is necessary to examine electrogalvanized and uncoated samples of a high strength steel susceptible to liquid metal embrittlement during spot welding with applied external load. Therefore, a newly developed tensile test method with a simultaneously applied spot weld is conducted. A fully coupled 3D electrical, thermal, metallurgical and mechanical finite element model depicting the resistant spot welding process combined with the tensile test conducted is mandatory to correct geometric influences of the sample geometry and provides insights into the sample’s time dependent local loading. With increasing external loads, the morphology of the brittle cracks formed is affected more than the crack depth. The validated finite element model applies newly developed damage indicators to predict and explain the liquid metal embrittlement cracking onset and development as well as even ductile failure. KW - Resistance spot welding KW - Finite element simulation KW - Advanced high-strength steel KW - Liquid metal embrittlement KW - Damage prediction KW - Tensile resistance spot welding experiment PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-594848 DO - https://doi.org/10.1007/s40194-024-01696-7 SN - 0043-2288 SP - 1 EP - 10 PB - Springer Science and Business Media LLC AN - OPUS4-59484 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Pasternak, H. A1 - Launert, B. A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Erhöhung der Tragfähigkeit geschweißter I-Träger aus hochfestem Baustahl durch verbesserte Ansätze zur Berücksichtigung von Eigenspannungen N2 - In vielen Bereichen des modernen Stahlbaus kommen geschweißte Vollwandträger, wie I-Träger zum Einsatz. Im Gegensatz zu Walzprofilen können die Bauhöhe, die Querschnittsform und die Blechdicken an die Beanspruchung angepasst werden, wodurch sich wirtschaftliche Vorteile erzielen lassen. Dabei werden heutzutage immer häufiger hochfeste Feinkornbaustähle mit (Mindest-) Fließgrenzen bis 690 MPa eingesetzt. Zur verbesserten Ausnutzung des Tragfähigkeitspotenzials geschweißter Profile aus diesen Stählen existieren keine geeigneten Modelle zur Erfassung der schweißfertigungsbedingten Eigenspannungen an realen Komponenten. Diese Daten werden durch konservative Annahmen angenähert. Die potentielle Tragfähigkeit geschweißter Konstruktionen wird daher in der Regel unterschätzt. Die Eigenspannungsannahmen in DIN EN 1993 basieren auf starken Vereinfachungen, bspw. im Rahmen sog. „Ersatzstabnachweise“. Diese setzen die Proportionalität der Eigenspannungsamplituden zur Fließgrenze voraus. Vergleichsrechnungen mit einem parametrisierten Eigenspannungsmodell zeigten mögliche Abweichungen in den berechneten Tragfähigkeiten über mehrere Knicklinien. Die Festlegungen hinsichtlich der anzuwendenden Knicklinie beeinflussen jedoch die Blechdicken und somit in erheblichem Maße auch die Fertigungskosten. Als Optimierungsstrategie wurden in diesem Forschungsprojekt deswegen unterschiedliche anwendungsorientierte Modellansätze entwickelt, welche mithilfe nichtlinearer Traglastberechnungen, die höhere Ausnutzung von Tragfähigkeitsreserven ermöglichen sollen. Forschungsziel war somit primär die Entwicklung und Bereitstellung entsprechender Berechnungsansätze. Experimentell wurde hierzu der Eigenspannungszustand von konventionell geschweißten Strukturen am Beispiel der im Stahlbau besonders häufig verwendeten I-Träger aus zwei gängigen Baustählen, einem unlegierten Baustahl S355J2+N und einem Feinkornbaustahl S690QL, erfasst und durch numerische Schweißstruktursimulationen ergänzt. Anschließend erfolgte die Ableitung eines vereinfachten Berechnungsmodells zur weiteren Berücksichtigung in nichtlinearen Tragfähigkeitsberechnungen. Die Erkenntnisse sollen in einen entsprechenden Anwenderleitfaden, herausgegeben durch das Technical Committee 8 der Europäischen Konvention für Stahlbau, einfließen und diesbezüglich als Orientierung einer möglichen zukünftigen Anpassung der Knicklinien in DIN EN 1993-1-1 dienen. Im Projekt wurden die genannten Stähle in zwei typischen Dickenkombinationen von 25/15 mm und 20/10 mm (Gurt- und Stegbleche) zu Großprobekörpern „I-Träger“ unter industrienahen Fertigungsbedingungen mittels Metall-Aktivgasschweißen gefügt. Diese erzeugten die typischen Eigenspannungen, die in solchen Trägern nach der Fertigung vorliegen. Während des Schweißens wurden die Temperaturfelder durch Thermoelemente aufgezeichnet. Die Eigenspannungen wurden nach dem Schweißen experimentell durch eine Kombination aus mechanischem Zerlegen (Zerlegemethode) und anschließender mobiler Röntgendiffraktometrie (XRD) festgestellt. Der Einfluss der industriell üblichen Brennschnittkantenvorbereitung der Bleche auf die finalen Eigenspannungszustände wurde experimentell zusätzlich an kleinmaßstäblichen Proben untersucht. Metallographische Analysen (Schliffbilder und Härtemessungen) komplettierten das experimentelle Programm der FE 2 (BAM, Berlin). Die Ergebnisse zeigten, dass beim mechanischen Zerlegen bereits ein Großteil der Eigenspannungen herausgelöst wurde. Eine Aussage zu den nahtnahen Zugeigenspannungen war allerdings erst durch die Überlagerung mit der XRD möglich. Dabei zeigte der S690QL überwiegend ein besseres Verhalten als der S355J2+N, welches sich unter anderem in abgesenkten Zugeigenspannungen im Verhältnis zur jeweiligen Fließgrenze äußerte. Die maximalen Eigenspannungen wurden dabei zumeist in der Wärmeeinflusszone (WEZ) der Schweißnaht gemessen, unabhängig von der eingebrachten Streckenenergie oder der Festigkeit des Grundwerkstoffs. Die baupraktische Annahme, dass die maximalen Eigenspannungen in Höhe der Fließgrenze vorliegen können, wurde nur in Einzelfällen und nur für den S355J2+N bestätigt. Die experimentellen Ergebnisse zeigten für die Druckeigenspannungen ebenfalls reduzierte relative Eigenspannungswerte des S690QL. Dies zeigt die notwendige weitere Optimierung bei der Wahl der Bewertungsansätze für Eigenspannungen auf die Tragfähigkeit. Die erzeugten Messwerte dienten im weiteren Verlauf als Eingangswerte für die Modellentwicklung und die numerischen Simulationen an I-Trägern durch die FE 1 (LSH, Cottbus). Die numerischen Schweißsimulationen erfolgten in Simufact.Welding® für die Simulationsmodelle mit „klassischem“ Schweißsimulationsansatz sowie in Ansys® für vereinfachte Simulationen und Näherungsansätze. Die Modelle lieferten insgesamt vergleichbare Ergebnisse für die Längseigenspannungen mit teils jedoch erheblichen Unterschieden in den Rechenzeiten. Durch eine angepasste Vernetzung konnte die Rechenzeit in allen Fällen deutlich reduziert werden. Aufgrund der verwendeten Bauteilgrößen ist die Anwendung der Modellierung mit Volumenelementen allerdings meistens nicht praktikabel. Für typische Trägerschweißungen bieten stattdessen Querschnittsmodelle mit der Annahme eines verallgemeinerten ebenen Verzerrungszustands eine mögliche Alternative. Der Abgleich der Ergebnisse mit den Experimenten lieferte zusammenfassend überwiegend gute bis befriedigende Übereinstimmungen. Die experimentell festgestellten Tendenzen wurden dabei in allen Fällen richtig vorhergesagt. Eine umfassende Bewertung der erzielbaren Genauigkeiten war bisher nicht möglich. Dies lag einerseits daran, dass die Datendichte der mit der durch die Zerlegung gewonnen Ergebnisse gering war. Anderseits lieferten die überlagerten Ergebnisse mit der XRD in Teilen, insbesondere in den interessierenden Druckbereichen, widersprüchliche Aussagen zum Eigenspannungseinfluss, was bisher nicht abschließend geklärt werden konnte. Darüber hinaus entstanden etwaige Abweichungen in den Simulationen auch durch die zugrunde gelegten Materialdaten selbst. Diese entsprachen Standarddatensätzen aus Materialbibliotheken. Die Skalierung dieser erfolgte gleichmäßig über den gesamten Temperaturbereich. Insbesondere für den S690QL existierten zu wenige belastbare Materialkennwerte. Entsprechende Versuche konnten im Rahmen dieses Vorhabens nicht mit durchgeführt werden. Dennoch konnten hinsichtlich eines vereinfachten Berechnungsvorgehens zur Berücksichtigung der Schweißeigenspannungen in Tragfähigkeitsberechnungen einige wichtige Erkenntnisse gewonnen werden. Auf Basis der in den numerischen Schweißsimulationsmodellen ermittelten plastischen Dehnungsmuster, auch „Eigenspannungsquellen“, wurde eine vereinfachte Simulationsvorgehensweise vorgeschlagen und verifiziert. Die dabei eingeführten Vereinfachungen wurden im Hinblick auf die Berechnung ausschließlich der plastischen Längsdehnungen bzw. der Längseigenspannungen gewählt. Die Anwendbarkeit ist daher auf ausreichend lange Schweißträger mit Längsnähten beschränkt. Einige Modellmodifikationen zur weiteren Vereinfachung bzw. Modellimplementierung in die strukturmechanische Berechnung an großen Komponenten wurden vorgestellt. Abschließend erfolgt die Einstufung in eine mögliche Knicklinie auf Basis eines mittels GMNIA (geometrisch und materiell nichtlineare Analyse mit Imperfektionen) Berechnungen simulierten Streubands der Tragfähigkeiten mittels Abaqus® und Ansys®. Die anfängliche Hypothese einer günstigeren Knicklinie eines S690QL im Vergleich zum S355J2+N wurde dabei rechnerisch bestätigt. Der experimentelle Nachweis mittels entsprechender Trägerfähigkeitsversuche ist allerdings noch ausstehend. KW - Schweißeigenspannungen KW - Numerische Simulation KW - Traglastverhalten KW - I-Träger KW - Hochfeste Stähle PY - 2018 SN - 978-3-946885-32-0 VL - Forschung für die Praxis P 1035 SP - 1 EP - 144 PB - Verlag und Vertriebsgesellschaft mbH CY - Düsseldorf AN - OPUS4-45271 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Mikrolegierungseinfluss auf das Ausscheidungsverhalten und die mechanischen Eigenschaften geschweißter hochfester Baustähle N2 - Mikrolegierungselemente, wie Nb und Ti, sind für die signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa unerlässlich. Normvorgaben zur chemischen Zusammensetzung geben dabei nur obere Grenzwerte für die Hersteller vor. Weiterhin wirken sich bereits kleine Abweichungen in der Legierungsroute teilweise drastisch auf die mechanischen Eigenschaften aus. Somit wird eine adäquate Vorhersage der Schweißeignung und der Integrität der Schweißverbindung aufgrund der variierenden Mikrogefüge erschwert bis unmöglich. Unerwünschte Nebeneffekte sind die mögliche Erweichung der Wärmeeinflusszone (WEZ) als auch der gegenteilige Effekt der Aufhärtung. Vor diesem Hintergrund werden erstmals systematisch die unterschiedlichen Mikrolegierungsrouten mit variierenden Ti und Nb-Gehalten an Versuchsschmelzen untersucht. Die Stahlgüte S690QL bildet dabei die Grundlage der chemischen Zusammensetzung sowie der entsprechenden Wärmebehandlung. Zur Untersuchung der jeweiligen Schweißeignung wurden Dreilagen-Schweißungen mittels moderner MAG-Hochleistungsschweißprozesse durchgeführt und kritische Gefügebereiche mit hoher Erweichung/Aufhärtung identifiziert. Der Fokus der analytischen Betrachtungen lag hier auf der Identifikation der Phasenumwandlungen beim Abkühlen und auf dem metallurgischen Ausscheidungsverhalten. Zusätzlich wurden isotherme und nicht-isotherme Phasenberechnungen mit der Software Thermo-Calc durchgeführt. Mechanisch-technologische Untersuchungen zur Kerbschlagzähigkeit mittels Kerbschlagbiegeversuchen durchgeführt wurden, bestätigen dabei die Ergebnisse der thermodynamischen Simulation bezüglich des Ausscheidungsverhaltens während der Temperatur-Zeit Schweißzyklen. Daraus lässt sich der Einfluss der Wärmeeinwirkung beim Schweißen auf die Gefügeausbildung in der WEZ und der korrespondierenden mechanischen Eigenschaften qualitativ beschreiben. T2 - DVS Congress 2023 Große Schweißtechnische Tagung CY - Essen, Germany DA - 11.09.2023 KW - WEZ-Erweichung KW - Mikrolegierungseinflüsse KW - Hochfester Feinkornbaustahl KW - Kerbschlagzähigkeit PY - 2023 SN - 978-3-96144-230-0 VL - 389 SP - 218 EP - 225 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-59419 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Nietzke, Jonathan A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Investigation of stress relief crack susceptibility of CrMoV steels coarse grain HAZ via simulation of uniaxial stress conditions during PWHT N2 - Creep-resistant steels such as the 13CrMoV9-10, used in the construction of thick-walled pressure vessels, are most commonly submerged arc welded (SAW). These steels can develop stress relief cracks (SRC) if the mandatory post weld heat treatment (PWHT) is performed improperly. Current PWHT parameters, such as heating rate and holding time at a specific holding temperature, are based on both empirical experience and conventional free shrinking welding experiments to characterize the SRC-susceptibility of the weld. These cannot adequately depict the higher residual stresses caused by the structurally induced stiffness of the surrounding construction. This study discusses the development of a repeatable, precise, and time-efficient methodology to study the effects of different stress levels and heating rates on the SRC susceptibility of the coarse grain heat-affected zone (CGHAZ). For that purpose, samples were thermically treated to simulate a coarse grain heat-affected zone (CGHAZ) and subsequently exposed to representative levels of stress during the heating phase of a PWHT. The recorded stress and heating rate–dependent strains were mathematically analyzed via curve tracing/calculus to identify interdependent effects. This procedure facilitates the measurement of material characteristics such as carbide growth on grain boundaries at the µm-scale via an integrated value over the entire sample volume. The first and second derivatives show a slight, precipitate-dependent, increase in hardness of the sample, depending on the heating rate and applied stress. This new methodology generates an improved assessment of the SRC susceptibility of SAW microstructures of creep-resistant CrMoV steels. KW - Submerged arc welding KW - Creep-resistant steel KW - Stress relief cracking KW - Component-like test KW - Post weld heat treatment PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576007 DO - https://doi.org/10.1007/s40194-023-01539-x SN - 0043-2288 SP - 1 EP - 9 PB - Springer Nature CY - Basel (CH) AN - OPUS4-57600 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Kromm, Arne A1 - Mente, Tobias A1 - Brackrock, Daniel A1 - Czeskleba, Denis A1 - Kannengießer, Thomas T1 - Component test for the assessment of delayed hydrogen-assisted cracking in thick-walled SAW joints for offshore applications N2 - Offshore wind turbines continuously increase in size and weight and demand adequate offshore foundations concepts like monopiles, tripods, or jackets. These components are typically constructed using submerged arc welding (SAW) with high-strength thick steel plates like the S420ML. During welding, the occurrence of delayed hydrogen-assisted cracking (HAC) must be anticipated. HAC is a critical combination of the local hydrogen concentration within a susceptible microstructure under certain mechanical load, i.e., the occurring (welding) residual stresses. The welding sequence of the thick-walled plates complicates the residual stress distribution due to the necessary repeated thermal cycling, i.e., welding seam/layer deposition to fill the joint. For that purpose, SAW with two-wire-technique was used to weld a specially designed and prototype-like mock-up of a real component with a thickness of 50 mm, filled with over 20 passes and a seam length of 1000 mm. Additional welded stiffeners simulated the effect of a high restraint, to achieve critical HAC conditions. The necessity of a minimum waiting time (MWT) before the NDT can be conducted (to exclude HAC) was critically verified by the application of ultrasonic testing of the welded joint at different time-steps of the NDT of up to 48 h after the completion welding. The residual stresses were determined by a robot XRD goniometer. Tensile residual stresses up to the yield limit are found both in the weld metal and in the heat-affected zone. Numerical modeling allowed the qualitative estimation of the hydrogen diffusion in the weld. No noticeable HAC occurrence was identified and confirms the high cracking resistance of the investigated material. Finally, the applicability of the MWT concept should be critically discussed. KW - Hydrogen KW - Cold cracking KW - Minimum Waiting Time KW - Offshore steel grade KW - Component test PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-591981 DO - https://doi.org/10.1007/s40194-023-01658-5 SP - 1 EP - 15 PB - Springer Science and Business Media LLC AN - OPUS4-59198 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Thermodynamic prediction of precipitations behaviour in HAZ of a gas metal arc welded S690QL with varying Ti and Nb content N2 - For a significant increase in the strength of high-strength fine-grained structural steels with a nominal yield strength ≥690 MPa, the addition of microalloying elements such as Nb and Ti is required. The standard specifications for the chemical composition of these steels (e.g., in EN 10025-6) often only give the manufacturer limit contents to achieve the defined properties. The effect of the alloying elements in the heat affected zone (HAZ) is sometimes completely contrary. This makes it difficult to adequately predict the batch dependency regarding weldability and the load-bearing behaviour of the welded joint. Three different micro-alloyed steels of the grade S690QL were produced on a laboratory scale, focusing on different Nb and Ti contents. To investigate the tempering effect, these were gas metal arc welded in three layers. In addition to metallographic investigations of individual HAZ areas, thermodynamic phase calculations were carried out using Thermo-Calc, following variations in the chemical composition. This provides an understanding of phase transformation, precipitation growth, and dissolution during welding as a function of temperature and cooling conditions. The results show a divergent metallurgical behaviour in the HAZ of the three different micro-alloyed steels. Thereby, the Ti micro-alloyed grade showed a strong softening of the HAZ in contrast to the Nb micro-alloyed grade. This can be attributed to a contrary precipitation behaviour during welding. KW - High-strength structural steel KW - Gas metal arc welding KW - HAZ-softening KW - Microalloying influences KW - Thermodynamic simulation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-579988 DO - https://doi.org/10.1007/s40194-023-01550-2 SN - 0043-2288 SP - 1 EP - 10 PB - Springer AN - OPUS4-57998 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Influence of microalloying on precipitation behavior and notch impact toughness of welded high‑strength structural steels N2 - Microalloying elements such as Nb and Ti are essential to increase the strength of quenched and tempered high-strength low alloy (HSLA) structural steels with nominal yield strength ≥ 690 MPa and their welded joints. Standards such as EN 10025–6 only specify limits or ranges for chemical composition, which leads to variations in specific compositions between steel manufacturers. These standards do not address the mechanical properties of the material, and even small variations in alloy content can significantly affect these properties. This makes it difficult to predict the weldability and integrity of welded joints, with potential problems such as softening or excessive hardening of the heat-affected zone (HAZ). To understand these metallurgical effects, previous studies have investigated different microalloying routes with varying Ti and Nb contents using test alloys. The high-strength quenched and tempered fine-grained structural steel S690QL is the basic grade regarding chemical composition and heat treatment. To evaluate weldability, three-layer welds were made using high-performance MAG welding. HAZ formation was investigated, and critical microstructural areas were identified, focusing on phase transformations during cooling and metallurgical precipitation behavior. Isothermal thermodynamic calculations for different precipitations were also carried out. Mechanical properties, especially Charpy notch impact toughness, were evaluated to understand the influence of different microalloys on the microstructure of the HAZ and mechanical properties. KW - High-strength structural steel KW - Gas metal arc welding KW - HAZ-softening KW - Notch impact toughness KW - Microalloying influences KW - Thermodynamic simulation PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608548 DO - https://doi.org/10.1007/s40194-024-01827-0 SN - 0043-2288 SP - 1 EP - 13 PB - Springer AN - OPUS4-60854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Mente, Tobias T1 - Zuverlässige Wasserstoff Bestimmung in Metallen und ihren Schweißverbindungen: Parameter, Einflüsse, Grenzen N2 - Im Zuge der wasserstoffbasierten Energiewirtschaft von morgen, kommt der Errichtung der dementsprechenden Infrastruktur die zentrale Rolle zu. Der überwiegende Teil bisher eingesetzter und meist geschweißter Werkstoffe, wie Stähle, kann unter bestimmten Bedingungen zur Wasserstoffversprödung neigen. Dies umfasst die klassische verzögerte Kaltrissbildung während der Schweißverarbeitung als auch Versprödungsphänomene während des Betriebs. Für die Bewertung eines jeden Wasserstoffeffektes auf bspw. die mechanischen Eigenschaften eines geschweißten metallischen Werkstoffes, muss der Wasserstoffgehalt präzise bestimmt werden, Im Fall von Schweißnähten ist die beispielsweise nach der ISO 3690, die klassische isotherme Trägergas-Heißextraktion (TGHE). Die TGHE basiert dabei auf der beschleunigten Wasserstoffentgasung aufgrund der thermischen Aktivierung des Wasserstoffs bei erhöhten Temperaturen. Neben der reinen Quantifizierung des Wasserstoffs, kann über die thermische Desorptionsanalyse (TDA) mit variierten Heizraten, der Bindungszustand an mikrostrukturellen Defekten im Material festgestellt und bewertet werden. Für beide Techniken sind experimentelle und messtechnische Einflüsse zu beachten, die großen Effekt auf das Ergebnis haben. Für die TGHE schlägt die ISO 3690 schlägt beispielswiese verschiedene Probengeometrien sowie Mindestextraktionszeiten vor. Die vorliegende Studie fasst Ergebnisse und Erfahrungen zahlreicher Untersuchungen an der Bundesanstalt für Materialforschung und -prüfung (BAM) mit unterschiedlichen Probentemperaturen und Geometrien (ISO 3690 Typ B und zylindrische TDA-Proben) zusammen hinsichtlich: Einfluss der Probenoberfläche (poliert/geschweißt), Messgenauigkeiten in Abhängigkeit des Probenvolumens sowie die unzureichende Überwachung des Effektes des PI-Reglers auf die Extraktionstemperatur. Insbesondere eine abweichende Extraktionstemperatur zur eingestellten Temperatur, kann die Messergebnisse wesentlich verfälschen. Basierend auf den Ergebnissen werden Methoden aufgezeigt, um schnell die gewünschte Extraktionstemperatur zu erreichen, ohne physisch in das Messequipment eingreifen zu müssen. Dies dient der wesentlichen Verbesserung der Zuverlässigkeit der Wasserstoffmessung durch erhöhte Signalstabilität und beschleunigte Wasserstoffdesorption. Im Allgemeinen ist eine unabhängige Temperaturmessung mit Dummy-Proben für die gewählte Heizprozedur angeraten, um mögliche unerwünschte Temperatureinflüsse bereits vor der Messung auszuschließen. Die beschriebenen Methoden können ohne großen Aufwand direkt in die industrielle Anwendung überführt werden. T2 - DVS Congress 2023 CY - Essen, Germany DA - 11.09.2023 KW - Wasserstoff KW - Schweißen KW - Forschung KW - ISO 3690 PY - 2023 SN - 978-3-96144-230-0 VL - 389 SP - 435 EP - 442 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-58309 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Launert, B. A1 - Rhode, Michael A1 - Pasternak, H. A1 - Kannengießer, Thomas ED - Dubina, D. ED - Ungureanu, V. T1 - Welding Residual Stresses in High-strength Steel. Experimental Results N2 - This article presents the latest results of an ongoing national research project on improved models for the prediction of welding residual stresses of thick-plated welded I-girders. The experimental program is presented and the importance of different influencing factors on the residual stresses is discussed in detail. All results are compared for mild (S355J2+N) and high strength (S690QL) steel. Finally, conclusions for further works are drawn. T2 - SDSS 2016 - The International Colloquium on Stability and Ductility of Steel Structures - SDSS 2016 CY - Timisoara, Romania DA - 30.05.2016 KW - Residual Stresses KW - Welding KW - High-Strength Steel KW - I-Girder KW - Component Test PY - 2016 SN - 978-92-9147-133-1 VL - 2016 SP - 517 EP - 524 PB - Ernst & Sohn AN - OPUS4-37890 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pasternak, H. A1 - Launert, B. A1 - Rhode, Michael A1 - Kannengießer, Thomas ED - Zingoni, A. T1 - Residual Stresses and Imperfections in Welded High-strength I-shape Sections N2 - This article addresses the imperfections caused by the weld assembly in I-shape sections made of two structural steel grades. Load influencing imperfections are assumed as deviations from the ideal shape (e.g. bending distortion) and longitudinal residual stresses. The quality of a numerically aided design of components exposed to either compression and/or bending is significantly affected, depending on these parameters. The Eurocode (EC3) provides robust simplified models. As a result, the Ultimate Limit State (ULS) is approached on a conservative basis. The following investigations are aimed at providing further guidance on these values in component-like specimens. The long term goal is an improved understanding of the load-bearing capacity of such sections. As a first step in this process, the experimental and corresponding numerical studies are presented. T2 - 6th International Conference on Structural Engineering, Mechanics and Computation (SEMC 2016) CY - Cape Town, South Africa DA - 05.09.2016 KW - Residual Stresses KW - Welding KW - High-strength Steel KW - Numerical Modeling KW - Component PY - 2016 SN - 978-1-138-02927-9 VL - 2016 SP - 1139 EP - 1146 PB - CRC Press, Taylor & Francis Group CY - Boca Raton, FL, USA AN - OPUS4-37888 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Einfluss unterschiedlicher Mikrolegierungsrouten eines S690QL auf das Ausscheidungsverhalten in der Wärmeeinflusszone N2 - Mikrolegierungselementen, wie Nb und Ti sind für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa unerlässlich. Normvorgaben zur chemischen Zusammensetzung dieser Stähle geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Mikrolegierungselemente bzw. ihrer Karbide und/oder Nitride ist teilweise komplett konträr, insbesondere bei Auflösung und Wiederausscheidung in der WEZ bei identischem Schweißzusatz. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragverhaltens der Schweißverbindung erschwert. Eine unerwünschte Eigenschaft ist dabei die Erweichung der WEZ, wie auch u.U. der gegenteilige Effekt der Aufhärtung. Vor diesem Hintergrund werden im Rahmen eines DFG-Vorhabens systematisch Mikrolegierungs-routen mit variierenden Ti- und Nb-Gehalten des hochfesten und vergüteten Feinkornbaustahls S690QL untersucht. Dazu wird das MAG-Schweißen mit modifizierten Sprühlichtbogen verwendet, welches durch hohe Abschmelzleistung gekennzeichnet ist und schmalere Nahtöffnungswinkel (α = 30°) ermöglicht. An Dreilagen-Schweißungen wird der Effekt der metallurgischen Zusammensetzung in Kombination mit hoher Wärmeeinwirkung auf die Ausbildung einer kritischen WEZ-Gefügezone mit Erweichung und/oder exzessiver Aufhärtung untersucht. Ein besonderes Augenmerk wird auf die Phasenumwandlungen und das Ausscheidungsverhalten im Gefüge der Wärmeeinflusszone gelegt. Neben umfangreichen metallographischen Untersuchungen einzelner WEZ-Bereiche wurden, unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberechnungen mittels Thermo-Calc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation und Ausscheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Abkühlbedingungen geschaffen. Das Ziel ist es, den Einfluss der Wärmeeinwirkung auf die Gefügeausbildung in der WEZ und dessen mechanischer Eigenschaften zu analysieren. Insbesondere wird hier auf die Auswirkung der unterschiedlichen Mikrolegierungskonzepte (Ti oder Nb) geachtet. T2 - 5. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 23.02.2023 KW - WEZ Erweichung KW - Thermodynamische Simulation KW - Mikrolegierungseinfluss KW - Schweißen von hochfesten FKB PY - 2023 SN - 978-3-8440-9105-2 VL - 12 SP - 332 EP - 343 PB - Shaker Verlag AN - OPUS4-58006 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Repair Welding of In-Service Hydrogen Pipelines - Concepts and Challenges N2 - Hydrogen is set as the energy carrier of tomorrow for a more sustainable fossil fuel free future. As this necessitates a reliable transport infrastructure, repurposing of the existing natural gas grid is planned. With regards to the well-known effect of hydrogen embrittlement, the compatibility of utilized materials must be investigated. First comprehensive studies on pipeline material hydrogen compatibility indicate that these materials can be applied to a certain extent. Nonetheless, the material compatibility is currently of high interest and focus of numerous research projects worldwide. However, pipelines require frequent maintenance and repair work. As part of these, in some cases it is necessary to do weldments onto pipelines while they are pressurized. This in-service welding introduces additional challenges for the material compatibility. Due to the resulting high temperatures, the metallurgical changes in the material and of course the presence of high-pressure hydrogen in the pipeline, additional investigations need to be conducted to ensure that no critical material degradation because of increased hydrogen absorption occurs and an overall material compatibility is given. For this reason, the present paper introduces in-service welding on pipelines. An overview of current research projects that deal with the application of in-service welding specifically on hydrogen pipelines and the emerging problems when applying these techniques on hydrogen pipelines is given. Methods of material testing, their limits and possible solutions are presented and discussed. T2 - 2024 15th International Pipeline Conference CY - Calgary, Alberta, Canada DA - 23.09.2024 KW - Hydrogen KW - Pipeline KW - Welding KW - In-Service PY - 2024 SN - 978-0-7918-8856-8 DO - https://doi.org/10.1115/IPC2024-133052 SP - 1 EP - 6 PB - The American Society of Mechanical Engineers (ASME) CY - New York AN - OPUS4-62262 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Steppan, Enrico A1 - Mantzke, Philipp A1 - Steffens, Benjamin A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Thermal desorption analysis for hydrogen trapping in microalloyed high-strength steels N2 - Hydrogen can have an extreme degradation effects in steels, particularly concerning the mechanical properties. These effects can lead to hydrogen-assisted cracking in microalloyed high-strength steels during fabrication and/or operation in industrial applications. In order to study these effects, electrochemically charged tensile specimens were tested to elucidate the degradation of their properties. The carrier gas hot extraction (CGHE) method, which functionally combines a mass spectrometer with a thermal desorption analysis (TDA) process, was used for the detection of ultra-low diffusible hydrogen concentrations in the material specimens. The mass spectrometer provided rapid and automatic determination of hydrogen concentration, whereas the TDA presented the activation energy within the respective test specimen at the specific temperature. Additionally, specimen temperature was carefully monitored to reduce the evaluation error for local effusion peaks. A quenching and deformation dilatometer was used for the analysis of typical heat-affected zones during the welding process for a high reproducibility of the homogenous microstructures that were studied. The present work shows the interaction between hydrogen and lattice defects in different microalloyed materials and heat-affected zones of weldable fine-grained steels. These steels were prepared in a quenched and tempered condition and in a thermo-mechanically rolled condition. These preparations were made according to German standard DIN EN 10025-6 and to DIN EN 10149-2, respectively. The trapping characteristics of two steel grades, S690QL and S700MC, were studied with respect to the activation energy dependent on carbon content and microalloying elements such as Ti, Nb, Mo, Cr, and V. The two steel grades exhibited several types of traps: carbide formations, dislocations, and/or grain boundaries were common, which can influence activation energy and hydrogen solubility. The type and dimension of inclusions or particles also affected the hydrogen trapping behavior. A decrease of carbon and specific alloying elements in thermo-mechanically hot rolled steels led to a change in the activation energy binding the trapped hydrogen. This thermo-mechanically hot rolled steel revealed an increased interaction between hydrogen and precipitations. The higher carbon content in the quenched and tempered steel led to a higher interaction between hydrogen and iron carbide, specifically in the martensitic phase. Furthermore, the trapping behavior in heat-affected zones showed a significant increase in activation energy, especially in the coarse-grained microstructure. These previously mentioned various effects were studied to better understand the degradation of mechanical properties in these two steels. KW - Microalloyed steels KW - Hydrogen embrittlement KW - Heating KW - Chemical analysis KW - Microstructure KW - Heat-affected zone PY - 2017 DO - https://doi.org/10.1007/s40194-017-0451-z SN - 0043-2288 SN - 1878-6669 VL - 61 IS - 4 SP - 637 EP - 648 PB - Springer CY - Berlin Heidelberg AN - OPUS4-40190 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schaupp, Thomas A1 - Rhode, Michael T1 - Influence of welding parameters on diffusible hydrogen content in high-strength steels using modified spray arc process N2 - In order to satisfy the growing requirements towards lightweight design and resource efficiency in modern steel constructions, e.g. mobile cranes and bridges, high-strength steels with typical yield strength ≥ 690 MPa are coming into use to an increasing extent. However, these steels require special treatment in welding. The susceptibility for degradation of the mechanical properties in presence of hydrogen increases significantly with increasing yield strength. In case of missing knowledge about how and which amount of hydrogen is uptaken during welding, hydrogen assisted cracking can be a negative consequence. Moreover, modern weld technology like the modified spray arc process enables welding of narrower weld seams. In this context, a reduced number of weld beads, volume and total heat input are technical and economic benefits. This work presents the influence of welding parameters on the diffusible hydrogen content in both (1) single-pass and (2) multi-layer welds. Different hydrogen concentrations were detected by varied contact tube distance, wire feed speed, arc length as well as varied arc type (transitional arc and modified spray arc). The results showed, that all welding parameters had significant influence on the diffusible hydrogen concentration in the single-pass welds. By increasing the number of weld beads in case of multi-layer welding, the hydrogen concentration have been substantially reduced. Whereby, differences in hydrogen concentrations between both arc types are present. T2 - IIW Intermediate Meeting: Commission II-A CY - Trollhättan, Sweden DA - 06.03.2017 KW - Hydrogen concentration KW - MAG Welding KW - High-strength steel KW - Welding parameters PY - 2017 AN - OPUS4-39396 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Steger, Jörg T1 - Approach for calculation of apparent hydrogen diffusion coefficients with permeation experiments in CrMoV steel weld joints N2 - Electrochemical permeation experiments were conducted at room temperature with the low alloyed creep resistant Steel grade T24 (7CrMoVTiB10-10). T24 weid metal specimens were machined from multi-layer manual TIG-welds. From the experimental data, apparent hydrogen diffusion coefficients are calculated for both. The diffusion coefficients varied distinctly with the used calculation method (classical time-lag and inflection point method). Derived from analytical calculation of the permeation transients, an adapted time-lag method is suggested for improved assessrnent of diffusivity. Additionally, the results indicated that the hydrogen diffusivity of the base metal (BM) is increased compared to the weid metal (WM). T2 - Steel & Hydrogen - 2nd International conference on metals and hydrogen CY - Gent, Belgium DA - 05.05.2014 PY - 2014 SN - 978-9081-7942-13 N1 - Serientitel: Steely hydrogen conference proceedings – Series title: Steely hydrogen conference proceedings SP - p28, 670 EP - 674 AN - OPUS4-31449 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Steppan, Enrico A1 - Kannengießer, Thomas A1 - Steger, Jörg ED - Lippold, J. T1 - Effect of hydrogen on mechanical properties of heat affected zone of a reactor pressure vessel steel grade N2 - The steel grade 20MnMoNi5-5 (according to German DIN standard or 16MND5 according to French AFNOR standard) is widely applied in (weld) fabrication of reactor pressure vessel components. Thus, a wide range of welding technologies (like submerged arc welding (SAW) or tungsten inert gas (TIG)) is used resulting in different heat affected zone (HAZ) microstructures. During weld fabrication, the weld joints may take up hydrogen. Especially, the HAZ shows an increased susceptibility for a degradation of the mechanical properties in presence of hydrogen. In addition, the hydrogen-assisted degradation of mechanical properties is influenced by three main local factors: hydrogen concentration, microstructure, and load condition. Hence, the base material (BM) and two different simulated non-tempered as-quenched HAZ microstructures were examined using hydrogen-free and hydrogen-charged tensile specimens. The results indicate that the effect of hydrogen on the degradation is significantly increased in case of the HAZ compared to the BM. In addition, hydrogen has remarkable effect in terms of reduction of ductility. It was ascertained that the degradation of the mechanical properties increases in the order of BM, bainitic HAZ, and the martensitic HAZ. Scanning electron microscope (SEM) investigation showed a distinct change of the fracture topography depended on the microstructure with increasing hydrogen concentration in case of the as-quenched HAZ microstructures. KW - Mechanical properties KW - Pressure vessel steels KW - Heat affected zone KW - Hydrogen KW - Hydrogen embrittlement KW - Low alloy steels PY - 2016 UR - http://link.springer.com/article/10.1007/s40194-016-0325-9 DO - https://doi.org/10.1007/s40194-016-0325-9 VL - 60 IS - 4 SP - 623 EP - 638 PB - Springer-Verlag GmbH CY - Heidelberg, Germany AN - OPUS4-36454 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Giese, Marcel A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Kadoke, Daniel A1 - Kruse, Julius T1 - Local strain behaviour in cross weld tensile specimens of microalloyed high strength steels using digital image correlation N2 - This study specifically examines the role of the microalloying element titanium (Ti) in achieving the desired mechanical properties of quenched and tempered high-strength fine-grain structural steels, with a nominal yield strength of ≥ 690 MPa. Current specifications limit chemical composition only by defining upper thresholds, but even minor variations in Ti content can substantially alter mechanical properties. Consequently, accurate prediction of weldability and welded joint integrity becomes challenging, as variations in Ti lead to distinct microstructural characteristics, potentially causing undesirable softening or hardening effects in the heat-affected zone (HAZ). To address these complexities, two distinct titanium concentrations were systematically investigated for the first time using specially developed laboratory-cast alloys. Both alloying configurations were based on the standard S690QL grade, with consistent chemical composition and heat treatment parameters maintained across the samples. For the weldability analysis, three-layer welds were executed using gas metal arc welding (GMAW), allowing for the identification of critical microstructural zones within the HAZ that exhibit significant softening or hardening. The influence of the softened HAZ region on failure mechanisms was assessed through transverse tensile tests. Digital image correlation (DIC) was employed to capture local strain variations across different HAZ regions in situ. With a custom-developed mirror system, local strains in microstructural zones on both the top and bottom surfaces of the weld were recorded simultaneously. This setup enabled a detailed analysis of how weld seam geometry (e.g., V-groove configuration) influences strain gradients. Additionally, the investigation of localized deformation provided insights into how variations in Ti content within the HAZ affect global strain, fracture constriction, fracture location, and overall fracture behavior. T2 - MPA Seminar 2024 Materials Processes Applications CY - Stuttgart, Germany DA - 08.10.2024 KW - HAZ-Softening KW - Digital Image Correlation KW - Cross weld tensile test PY - 2024 AN - OPUS4-61488 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Gibmeier, J. A1 - Rethmeier, Michael T1 - In-situ-Analyse der Phasenumwandlungskinetik während des Schweißens N2 - Zugeigenspannungen, wie sie beim Schweißprozess durch inhomogene Temperaturverteilungen und Schrumpfungen hervorgerufen werden, können die Lebensdauer geschweißter Verbindungen signifikant herabsetzen. Eine neue und außerordentlich attraktive Methode, um Druckeigenspannungen bereits während des Schweißens gezielt einzustellen, gelingt mit sogenannten LTT (Low Transformation Temperature)-Legierungen. LTT-Legierungen weisen eine martensitische Phasenumwandlung bei relativ niedrigen Temperaturen auf, wobei die damit verbundene Volumenexpansion zu einer Reduktion der Schrumpfeigenspannungen bzw. Erzeugung von Druckeigenspannungen führt. Zum direkten Nachweis der Phasenumwandlungen und der damit verbundenen resultierenden Schweißeigenspannungen wurden erstmals In-situ-Schweißexperimente unter Nutzung hoch energetischer, polychromatischer Synchrotronstrahlung (Weißstrahl) realisiert, um die Umwandlungskinetik während eines realen Schweißprozesses und die daraus resultierenden Schweißeigenspannungen zu analysieren. Es wird gezeigt, dass mit LTT-Legierungen signifikante Druckeigenspannungen in der Schweißnaht erreicht werden. PY - 2010 SN - 0025-5300 VL - 52 IS - 4 SP - 204 EP - 210 PB - Hanser CY - München AN - OPUS4-21219 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brauser, Stephan A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - In-situ synchrotron diffraction and digital image correlation technique for characterizations of retained austenite stability in low-alloyed transformation induced plasticity steel N2 - Direct measurement and quantification of phase transformation in a low-alloyed transformation induced plasticity steels depending on the tensile load as well as determination of the real true stress and true strain values were carried out in-situ using high energy synchrotron radiation. Digital image correlation technique was used to quantify more precisely the true strain values. The aim of the work was to obtain a better understanding of the phase transformation of commercial low-alloyed transformation induced plasticity steel depending on the true strain and true stress values. KW - Transformation induced plasticity KW - In-situ synchrotron diffraction KW - Austenite stability KW - Digital image correlation PY - 2010 DO - https://doi.org/10.1016/j.scriptamat.2010.08.007 SN - 1359-6462 SN - 1872-8456 VL - 63 IS - 12 SP - 1149 EP - 1152 PB - Elsevier CY - Oxford AN - OPUS4-22164 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heinze, Christoph A1 - Kromm, Arne A1 - Schwenk, Christopher A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - Welding residual stresses depending on solid-state transformation behaviour studied by numerical and experimental methods N2 - The development of high-strength structural steels with yield strengths up to 1000 MPa results in the requirement of suitable filler materials for welding. Recently designed low transformation temperature (LTT) alloys offer appropriate strength. The martensitic phase transformation during welding induces compressive residual stress in the weld zone. Therefore, the mechanical properties of welded joints can be improved. The present paper illustrates numerical simulation of the residual stresses in LTT-welds taking into account the effect of varying Ms/Mf-temperatures, and therefore different retained austenite contents, on the residual stresses. Residual stress distributions measured by synchrotron diffraction are taken as evaluation basis. A numerical model for the simulation of transformation affected welds is established and can be used for identification of appropriate Ms-temperatures considering the content of retained austenite. KW - Welding simulation KW - Residual stress KW - Low transformation temperature filler material KW - Martensitic transformation KW - Retained austenite PY - 2011 DO - https://doi.org/10.4028/www.scientific.net/MSF.681.85 SN - 0255-5476 VL - 681 SP - 85 EP - 90 PB - Trans Tech Publications CY - Aedermannsdorf, Switzerland AN - OPUS4-23357 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brauser, Stephan A1 - Kromm, Arne A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - In-situ analysis of solid state phase transformation in TRIP-aided steels by synchrotron diffraction N2 - Energy dispersive synchrotron diffraction (EDXRD) analysis and 3 dimensional digital image correlations were conducted to investigate the stress and strain effected transformation behavior during tensile loading of low alloyed TRansformation Induced Plasticity (TRIP) steel. This technique allowed for phase specific stress measurement during certain tensile load steps in the elastic and also plastic regime. Additionally the simultaneous determination of the load dependent phase content was realized. The results show that the martensite transformation starts only after exceeding the overall yield point and is finished before reaching the uniform elongation, whereas a large portion of the austenite remains unchanged in the structure. Furthermore, the martensite transformation related to the stress in the γ-phase and α-phase was analyzed and quantified. KW - Synchrotron KW - EDXRD KW - Phase transformation KW - TRIP steel KW - Digital image correlation KW - Residual stress PY - 2011 UR - https://www.jstage.jst.go.jp/article/qjjws/29/3/29_3_81s/_pdf DO - https://doi.org/10.2207/qjjws.29.81s SN - 0288-4771 VL - 29 IS - 3 SP - 81 EP - 85 CY - Tokyo, Japan AN - OPUS4-24693 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brauser, Stephan A1 - Kromm, Arne A1 - Dabah, Eitan A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - Thermal stability of retained austenite in low alloyed TRIP-steel determined by high energy synchrotron radiation N2 - TRIP-steels offer a good combination between strength and ductility. Therefore TRIP-steels are widely used in the automobile industries. The aim of this work is to study the stability of involved phases during heating and to identify the kinetics of the occuring phase transformations. For that purpose, in-situ diffraction measurements, using high energy synchrotron radiation were conducted. The analysis revealed the decomposition of the metastable austenitic phase into carbide and ferrite along the heating process and the regeneration of the austenite by further heating of the sample. KW - Austenite stability KW - Phase transformation KW - TRIP steel KW - Energy dispersive synchrotron X-ray diffraction PY - 2014 DO - https://doi.org/10.4028/www.scientific.net/MSF.772.129 SN - 0255-5476 VL - 772 SP - 129 EP - 133 PB - Trans Tech Publications CY - Aedermannsdorf, Switzerland AN - OPUS4-29700 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Rethmeier, Michael A1 - Gibmeier, J. A1 - Genzel, C. T1 - Residual stresses and in-situ measurement of phase transformation in low transformation temperature (LTT) welding materials PY - 2009 SN - 1097-0002 SN - 0069-8490 SN - 0376-0308 VL - 52 SP - 755 EP - 762 CY - Newtown Square, Pa., USA AN - OPUS4-19817 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schwenk, C. A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - Restraint conditions and welding resiudal stresses in self-restrained cold cracking test N2 - In the last decade, high-strength fine grained steels and welding consumables have gained a strong raise of application ranging from mobile cranes to bridge constructions. However, the cracking susceptibility of these steels increases significantly in correspondence with the achieved improvements in yield strength and the loss in plastic deformation reserves. In order to determine this behavior a series of different standardized cold cracking tests has been developed. One remaining major problem of these tests is the uncertainty about the quantitative intensity of the restraint conditions as well as the corresponding welding residual stresses. Consequently, the comparison of different tests and welding conditions as well as the transferability of the results onto real parts is difficult at best. The main topic of this paper is the analysis of the restraint conditions and their link with the welding induced residual stresses. The importance of the given standardized selfrestrained tests and first results about the transferability of results onto real parts are discussed. The influence of the test specimen geometry on the restraint conditions of the test is investigated for a selected test with numerical Simulation using commercial FEA software. Additionally, the residual stresses caused by the welding process are measured and linked with the restraint conditions which are defined mainly by the geometry parameters. Finally the transferability of the selected cold cracking test results is validated experimentally. The test results of a multilayer weld on high-strength fine grained steel of real size weldments are investigated. For these experiments a 16 MN large scale testing facility is used which is capable of applying the high reaction forces and clamping conditions found at large scale demonstrator parts. The results show the importance of the quantitative knowledge of the restraint conditions and the welding residual stresses on the cold cracking resistance. T2 - 8th International Conference on Trends in Welding Research CY - Pine Mountain, USA DA - 01.06.2008 KW - Cold Cracking Test KW - Intensity of Restraint PY - 2008 DO - https://doi.org/10.1361/cp2008twr766 SP - 766 EP - 771 PB - ASM international AN - OPUS4-47623 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Hydrogen KW - Repair welding KW - Pipeline PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638944 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czerwensky, Michael A1 - Birkholz, M. A1 - Kanschat, P. A1 - Weiss, Thomas A1 - Lips, K. T1 - Low-temperature electron-paramagnetic-resonance study of extrinsic and intrinsic defects in CuGaSe2 KW - Electron-paramagnetic resonance KW - EPR PY - 1999 SN - 1098-0121 SN - 0163-1829 SN - 0556-2805 SN - 1095-3795 SN - 1550-235X VL - 59 IS - 19 SP - 12268 EP - 12271 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-785 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Frasca, Daniele A1 - Schulze, Dietmar A1 - Wachtendorf, Volker A1 - Krafft, Bernd A1 - Morys, Michael A1 - Böhning, Martin A1 - Rybak, Thomas T1 - Multilayer graphene rubber nanocomposites N2 - Multilayer Graphene (MLG), a nanoparticle with a specific surface of BET = 250 m²/g and thus made of only approximately 10 graphene sheets, is proposed as a nanofiller for rubbers. When homogenously dispersed, it works at low loadings enabling the replacement of carbon black (CB), increase in efficiency, or reduction in filler concentration. Actually the appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing and mechanical properties of different rubbers, as shown for Chlorine-Isobutylene-Isoprene Rubber (CIIR), Nitrile-Butadiene Rubber (NBR), Natural Rubber (NR), and Styrene-Butadiene Rubber (SBR). A mere 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of carbon black. Similar equivalents are observed for MLG/CB mixtures. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards fire behavior. The later shown by the reduction in heat release rate in the cone calorimeter. The higher the nanofiller concentration is (3 phr, 5 phr, and 10 phr was investigated), the greater the improvement in the properties of the nanocomposites. Moreover, the MLG nanocomposites improve stability of mechanical properties against weathering. An increase in UV-absorption as well as a pronounced radical scavenging are proposed and were proved experimentally. To sum up, MLG is interesting as a multifunctional nanofiller and seems to be quite ready for rubber development. T2 - TOP 2016, VIII International Conference on “Times of Polymers and Composites” CY - Naples, Italy DA - 19.06.2016 KW - Graphene KW - Nanocomposite KW - Rubber PY - 2016 SN - 978-0-7354-1390-0 DO - https://doi.org/10.1063/1.4949621 SN - 0094-243X SN - 1551-7616 VL - 1736 SP - 020046, 1 EP - 4 PB - AIP AN - OPUS4-36864 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Measurement and numerical modeling of residual stress distribution in welded HSLA component-like I-girders N2 - Currently, residual stresses in welded HSLA (high strength low alloyed steels) are considerded by simplified “robust” procedures fixed in common standards (such as Eurocode 3). The models are mostly based on specimens from mild steel with lower strength. For HSLA, necessary material data is less available for realistic assessment of the appearing residual stresses in typical I-girders. Hence, the economic benefit of HSLA steels in scope of load bearing capacity cannot fully be exploit. Thus, the scope of this work is the measurement of weld residual stresses in component-like I-girders S355 and S690 by sectioning method and subsequent verification by global structural welding simulation. T2 - IIW Intermediate Meeting, Meeting of commision II-A CY - Madrid, Spain DA - 29.02.2016 KW - I-girder KW - Weld residual stresses KW - Numerical simulation KW - Sectioning method PY - 2016 AN - OPUS4-35543 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Brauser, Stephan A1 - Kannengießer, Thomas A1 - Rethmeier, Michael T1 - High-energy synchrotron diffraction study of a transformation induced plasticity steel during tensile deformation N2 - Energy-dispersive x-ray diffraction offers the possibility for measurement and evaluation of diffraction spectra containing information of various diffraction lines of all contributing crystalline phases of a material. Combined strain imaging and diffraction analysis was conducted during the tensile test of a low alloyed transformation-induced plasticity (TRIP) steel in order to investigate the transformation induced plasticity, strain hardening, and load partitioning effects. Optical strain imaging allowed for determination of localized true strains from three-dimensional deformations measured in situ. High-energy synchrotron radiation has permitted diffraction analysis in transmission mode to gather information from the material interior. Phase-specific stress evolution during loading could be observed applying the sin2ψ technique during certain load steps. The strains of the individual lattice planes were determined in different locations under varying angles between loading and perpendicular direction. Using energy-dispersive methods it was also possible to determine the transformation behaviour during elastic and plastic regime taking into account a large number of diffraction lines. The results show that the approach practised here enables one to pull together macroscopic and phase-specific microscopic material behaviour in order to improve existing models for prediction of complex load situations. KW - EDXRD KW - Transformation-induced plasticity (TRIP) KW - Residual stress KW - Synchrotron KW - Martensite transformation PY - 2011 DO - https://doi.org/10.1177/0309324711403969 SN - 0309-3247 SN - 2041-3130 VL - 46 IS - 7 SP - 581 EP - 591 PB - Sage CY - London AN - OPUS4-24604 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kannengießer, Thomas A1 - Rethmeier, Michael A1 - Portella, Pedro Dolabella A1 - Ewert, Uwe A1 - Redmer, Bernhard T1 - Assessment of hot cracking behaviour in welds N2 - Hot crack assessment during production and processing of metallic materials is an essential prerequisite for the safety of welded structures. The hot cracking investigations presented here were carried out as part of a study aimed at the development of Cr/Ni low transformation temperature filler materials. Low transformation temperature alloys open up the possibility for welding high strength steels. The externally loaded Modified Varestraint Transvarestraint hot cracking test was employed in the experiments described. The hot cracking resistance was evaluated with the help of light microscopy applied at the specimen surface. The proportionality between hot cracking susceptibility and Cr/Ni alloy content was explained by the altered solidification kinetics and by the enlarged solidification interval. The internal crack paths and the three-dimensional structure of the crack net in the material volume were examined using X-ray computer tomography. The total crack lengths for different material depths and circumjacent rectangular volumes, respectively, were be determined. An increasing hot cracking susceptibility with increasing Cr/Ni alloy content was also be established for the specimen volume. KW - Hot cracking KW - Low transformation temperature (LTT) alloy KW - Modified varestraint transvarestraint (MVT) hot cracking test KW - X-ray computer tomography PY - 2011 DO - https://doi.org/10.3139/146.110545 SN - 1862-5282 VL - 102 IS - 8 SP - 1001 EP - 1006 PB - Carl Hanser CY - München AN - OPUS4-24400 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Hadick, C. A1 - Schu, K. T1 - Quantification of hydrogen uptake during in-service hydrogen pipeline welding N2 - Hydrogen must be transported on a large scale from producers to consumers to ensure the energy transition. The necessary pipeline grid is achieved by conversion of the natural gas (NG) grid and building new pipelines. Welding during service as part e.g. of “hot-tapping” is unavoidable for maintenance/repair/expansion. Based on existing studies, the basic material compatibility of (low-alloyed) pipeline steels with hydrogen is postulated. However, this cannot be assumed for the case of in-service welding on pipelines in pressurized condition. The reason is the increased temperature e.g. by preheating and (in particular) during welding of the single passes. As a result, the inner pipeline surface undergoes multiple short-term heating but to high temperatures. In particular, the first passes can result in a temperature close to the austenitic transformation of the material for small wall thicknesses. Both increase the hydrogen uptake into the welded joint. If hydrogen embrittlement is likely to occur, depends on the hydrogen uptake, which must be quantified. For this purpose, welding experiments on pressurized demonstrators were conducted. The hydrogen uptake at 100 bar was compared to reference experiments with nitrogen. A new sample extraction routine for the quantification of the weld-zone specific hydrogen uptake was established. Comprehensive experiments with different steels (P235, L360, L485), wall thicknesses (4.1 mm to 7.8 mm) and diameters (DN50 and DN200) were conducted. In addition, the influence of the welding layer sequence on the hydrogen uptake between single- and multi-layer welds was investigated. Analytical approaches were used to approximate the hydrogen uptake in the respective weld zones. The main findings were that the layer sequence and especially the wall thickness have a large influence on the hydrogen uptake. T2 - 20th Pipeline Technology Conference ptc2025 CY - Berlin, Germany DA - 06.05.2025 KW - In-service KW - Hydrogen KW - Pipeline KW - Repair welding KW - component test PY - 2025 SP - 1 EP - 12 AN - OPUS4-63166 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -