TY - JOUR A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Kannengießer, Thomas A1 - Gibmeier, J. A1 - Vollert, F. T1 - Assessment of the Solidification Cracking Susceptibility of Welding Consumables in the Varestraint Test by Means of an Extended Evaluation Methodology N2 - Various test methods are available for assessing the susceptibility of materials to solidification cracking during welding. In the widely used Varestraint test, the crack length is selected as a criterion as a function of the applied bending strain. Unfortunately, the crack length does not characterize the material behavior alone but depends to varying degrees on the individual test parameters used, which makes the interpretation of the results difficult. In addition, the crack length is not comparable under different test conditions. To overcome these disadvantages, we have developed a novel evaluation methodology that decouples the machine influence from the material behavior. The measured crack length is related to the maximum possible value specified by welding speed and deformation time. This relative crack length is calculated numerically, considering the orientation of the cracks. Experiments on two high-alloy martensitic welding consumables show that, in contrast to the conventional evaluation, a comparison of different welding parameters becomes possible. Furthermore, the strain rate proved to be a suitable crack criterion in agreement with Prokhorov's hot cracking model. KW - Welding KW - Solidification cracking KW - Varestraint test PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-545780 SN - 1438-1656 SP - 2101650 PB - Wiley online library AN - OPUS4-54578 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thomas, Maximilian A1 - Vollert, F. A1 - Weidemann, Jens A1 - Gibmeier, J. A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Surface- and volume-based investigation on influences of different Varestraint testing parameters and chemical compositions on solidification cracking in LTT filler metals N2 - The subject of this study is how, and to what extent, Varestraint/Transvarestraint test results are influenced by both testing parameters and characteristics of evaluation methods. Several different high-alloyed martensitic LTT (low Transformation temperature) filler materials, CrNi and CrMn type, were selected for examination due to their rather distinctive solidification cracking behaviour, which aroused interest after previous studies. First, the effects of different process parameter sets on the solidification cracking response were measured using standard approaches. Subsequently, microfocus X-ray computer tomography (μCT) scans were performed on the specimens. The results consistently show sub-surface cracking to significant yet varying extents. Different primary solidification types were found using wavelength dispersive X-ray (WDX) analysis conducted on filler metals with varying Cr/Ni equivalent ratios. This aspect is regarded as the main difference between the CrNiand CrMn-type materials in matters of cracking characteristics. Results show that when it comes to testing of modern highperformance alloys, one set of standard Varestraint testing parameters might not be equally suitable for all materials. Also, to properly accommodate different solidification types, sub-surface cracking has to be taken into account. KW - Solidification cracking KW - Varestraint testing KW - MVT KW - LTT filler metal KW - Microfocus X-ray computer tomography (μCT) PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-506039 VL - 64 SP - 913 EP - 923 PB - Springer Nature CY - Heidelberg, New York AN - OPUS4-50603 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Liepold, Philipp A1 - Kannengießer, Thomas A1 - Schröpfer, Dirk T1 - Einfluss der Schweiß- und Prüfparameter bei der Heißrissbewertung hochfester Schweißzusatzwerkstoffe N2 - Die Heißrissneigung beim Schweißen kann mittels einer ganzen Reihe von Prüfverfahren ermittelt werden. Eine etablierte Methode ist die sogenannte Varestraint-Prüfung, welche auch an der Bundesanstalt für Materialforschung und -prüfung (BAM) als modifizierter Varestraint/Transvarestraint-Test (MVT) zum Einsatz kommt. Die Ergebnisse von Varestraint-Prüfungen hängen jedoch stets in unter-schiedlichem Maße von der individuellen Prüfmaschinenauslegung und den verwendeten Prüfparametern ab. Dies kann zu einer uneinheitlichen Bewertung des Rissverhaltens führen, wenn die Risslänge konventionell als Kriterium für die Rissneigung herangezogen wird. Scheinbare Abhängigkeiten von Prozessparametern erschweren dann die Interpretation der Ergebnisse. Eine neuartige Bewertungsmethodik entkoppelt den Maschineneinfluss vom Materialverhalten und verwendet die Dehnrate als Risskriterium. T2 - 5. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 23.02.2023 KW - Heißrisse KW - Varestraint-Test PY - 2023 SN - 978-3-8440-9105-2 SN - 2364-0804 VL - 12 SP - 357 EP - 365 PB - Shaker CY - Düren AN - OPUS4-57993 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Kannengiesser, Thomas A1 - Gibmeier, Jens T1 - On the interpretation of Varestraint and Transvarestraint hot cracking test results N2 - The Varestraint test and its variant Transvarestraint are one of the most widely used techniques for evaluating a material solidification cracking sensitivity during welding. The result of such tests is a crack length which is proportional to the material’s cracking susceptibility. Nevertheless, the welding and load parameters can unintentionally influence the crack length, which in some cases can distort the material evaluation. An approach is described as to how these effects can be assessed with the aid of a digital crack analysis. The crack lengths are compared position-dependently with their possible propagation due to the weld pool movement during continuous loading. The index derived from this can be used by the operator to evaluate his test parameters. In addition, a comparison of the results of different Varestraint setups is made possible. Alongside experimental results, a numerical sensitivity analysis is presented on how individual welding and loading parameters can affect the crack lengths. KW - Varestraint test KW - Solidification cracking KW - Weldability PY - 2024 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-595089 SN - 0043-2288 SP - 1 EP - 13 PB - Springer Science and Business Media LLC AN - OPUS4-59508 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -