TY - CONF A1 - Neumann, Martin A1 - Gleim, Tobias A1 - Gradt, Thomas A1 - Wille, Frank T1 - Friction coefficients for wood-wood and wood-steel interfaces in impact limiters for transport casks N2 - Wood is widely used in impact limiters of transport casks for radioactive material. Encapsulated by an outer and inner steel structure, spruce wood is often applied in layers of alternating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard target. In order to get detailed information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C to for a wood-wood combination. T2 - 20th International Symposium on the Packaging and Transportation of Radioactive Materials CY - Juan-les-Pins, France DA - 11.06.2023 KW - Wood KW - Friction KW - Transport cask PY - 2023 SP - 1 EP - 11 AN - OPUS4-57334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Neumann, Martin A1 - Gleim, Tobias A1 - Gradt, Thomas T1 - Friction coefficients for wood-wood and wood-steel high pressure contact under temperatures between -40 °C and 90 °C N2 - Wood is widely used in impact limiters of Transport casks for radioactive material. Encapsulated by an outer and inner Steel structure, spruce wood is offen applied in layers of altemating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard component. In order to get detailed Information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature ränge between -40 °C and 90 °C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40 °C to 0.22 for 90 °C for wood-steel combinations and from 0.3 at -40 °C to 0.24 at 90 °C to for a wood-wood combination. KW - Wood KW - Friction KW - Transport cask KW - Radioactive material PY - 2023 U6 - https://doi.org/10.24053/TuS-2023-0007 SN - 0724-3472 VL - 70 IS - 2 SP - 5 EP - 12 PB - expert verlag AN - OPUS4-57787 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -