TY - JOUR A1 - Sadowski, A. A1 - Seidel, M. A1 - Al-Lawati, H. A1 - Azizi, E. A1 - Balscheit, Hagen A1 - Böhm, M. A1 - Chen, Lei A1 - van Dijk, I. A1 - Doerich-Stavridis, C. A1 - Kunle Fajuyitan, O. A1 - Filippidis, A. A1 - Winther Fischer, A. A1 - Fischer, C. A1 - Gerasimidis, S. A1 - Karampour, H. A1 - Kathirkamanathan, L. A1 - Subramanian, S. A1 - Topkaya, Cem A1 - Wagner, H. N. R. A1 - Wang, J. A1 - Wang, J. A1 - Kumar Yadav, K. A1 - Yun, X. A1 - Zhang, P. T1 - 8-MW wind turbine tower computational shell buckling benchmark - Part 1: An international ‘round-robin’ exercise JF - Engineering failure analysis N2 - An assessment of the elastic-plastic buckling limit state for multi-strake wind turbine support towers poses a particular challenge for the modern finite element analyst, who must competently navigate numerous modelling choices related to the tug-of-war between meshing and computational cost, the use of solvers that are robust to highly nonlinear behaviour, the potential for multiple near-simultaneously critical failure locations, the complex issue of imperfection sensitivity and finally the interpretation of the data into a safe and economic design. This paper reports on an international ‘round-robin’ exercise conducted in 2022 aiming to take stock of the computational shell buckling expertise around the world which attracted 29 submissions. Participants were asked to perform analyses of increasing complexity on a standardised benchmark of an 8-MW multi-strake steel wind turbine support tower segment, from a linear elastic stress analysis to a linear bifurcation analysis to a geometrically and materially nonlinear buckling analysis with imperfections. The results are a showcase of the significant shell buckling expertise now available in both industry and academia. This paper is the first of a pair. The second paper presents a detailed reference solution to the benchmark, including an illustration of the Eurocode-compliant calibration of two important imperfection forms. KW - Wind turbine tower KW - Computational KW - Shell buckling KW - Benchmark PY - 2023 DO - https://doi.org/10.1016/j.engfailanal.2023.107124 SN - 1350-6307 VL - 148 SP - 1 EP - 23 PB - Elsevier Science CY - Oxford AN - OPUS4-57019 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Huang, K. A1 - Liu, H. A1 - Kraft, Marco A1 - Shikha, S. A1 - Zheng, X. A1 - Agren, H. A1 - Würth, Christian A1 - Resch-Genger, Ute A1 - Zhang, Y. T1 - A protected excitation-energy reservoir for efficient upconversion luminescence JF - Nanoscale N2 - Lanthanide-doped upconversion nanoparticles (UCNPs) are of great interest for biomedical applications. Currently, the applicability of UCNP bionanotechnology is hampered by the generally low luminescence intensity of UCNPs and inefficient energy Transfer from UCNPs to surface-bound chromophores used e.g. for photodynamic therapy or analyte sensing. In this work, we address the low-Efficiency issue by developing versatile core-Shell nanostructures, where high-concentration sensitizers and activators are confined in the core and Shell Region of representative hexagonal NaYF2:Yb,Er UCNPs. After Doping concentration optimization, the sensitizer-rich core is able to harvest/accumulate more excitation energy and generate almost one order of Magnitude higher luminescence intesity than conventional homogeneously doped nanostructures. At the same time, the activator Ions located in the Shell enable a ~6 times more efficient resonant energy Transfer from UCNPs to surface-bound acceptor dye molecules due to the short distance between donor-acceptor pairs. Our work provides new insights into the rational design of UCNPs and will greatly encrease the General applicability of upconversion nanotechnologies. KW - Fluorescence KW - Lanthanide KW - Upconversion KW - Brightness KW - Quantification KW - Nanoparticle KW - Absolute fluorometry KW - NIR KW - IR KW - Quantum yield KW - Integrating sphere spectroscopy KW - Method KW - Energy transfer KW - Shell KW - Particle architecture PY - 2017 DO - https://doi.org/10.1039/c7nr06900f SN - 2040-3372 SN - 2040-3364 VL - 10 IS - 1 SP - 250 EP - 259 PB - The Royal Society of Chemistry AN - OPUS4-43893 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dai, X. A1 - Zhang, W. A1 - Li, H. A1 - Huang, T. A1 - Li, M. A1 - Quan, C. A1 - Zhang, Q. A1 - Davies, S. R. A1 - Warren, J. A1 - Lo, M.-F. A1 - Kakoulides, E. A1 - Gören, A. C. A1 - Marbumrung, S. A1 - Pfeifer, Dietmar A1 - Ün, I. A1 - Gündüz, S. A1 - Yilmaz, H. A1 - Kankaew, P. A1 - Sudsiri, N. A1 - Shearman, K. A1 - Pookrod, P. A1 - Polzer, J. A1 - Radeck, W. T1 - CCQM-K104 key comparison (avermectin B(1)a) on the characterization of organic substances for chemical purity JF - Metrologia N2 - Under the Comité Consultatif pour la Quantité de Matière (CCQM), a key comparison, CCQM-K104, was coordinated by the National Institute of Metrology (NIM). The comparison was designed to demonstrate a laboratory's performance in determining the mass fraction of the main component in a complex high purity organic material. Nine NMIs or DIs participated in the comparison. Eight participants reported their results. An additional impurity was resolved from the avermectin B1a peak and was tentatively identified as an unknown impurity by NMIA (National Measurement Institute (Australia)). It was subsequently identified by NIM as a diastereoisomer of avermectin B1a at the C-26 position. Final reference value (KCRV) = 924.63 mg/g, with uncertainty (k=1) = 3.89 mg/g, and expanded uncertainty = 8.97 mg/g. The degrees of equivalence with the avermectin B1a KCRV for each participant were reported. The measurement results and degrees of equivalence should be indicative of the performance of a laboratory's measurement capability for the purity assignment of organic compounds of high structural complexity (relative molecular mass range of 500 Da -1000 Da and low polarity (-log KOW ≤ -2). KW - NMR KW - Key comparision KW - CCQM PY - 2017 DO - https://doi.org/10.1088/0026-1394/54/1A/08019 SN - 0026-1394 VL - 54 SP - 2 EP - 32 AN - OPUS4-45381 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Li, X.M. A1 - Li, H.M. A1 - Zhang, Q.H. A1 - Lu, X.H. A1 - Li, S.Q. A1 - Koch, Matthias A1 - Polzer, J. A1 - Hackenber, R. A1 - Moniruzzaman, M. A1 - Khan, M. A1 - Kakoulides, E. A1 - Pak-Wing, K. A1 - Richy, A1 - Chi-Shing, N. A1 - Lu, T. A1 - Gui, E.M. A1 - Cheow, P.S. A1 - Teo, T.L. A1 - Rego, E. A1 - Garrido, B. A1 - Carvalho, L. A1 - Leal, R. A1 - Violante, F. A1 - Baek, S.Y. A1 - Lee, S. A1 - Choi, K. A1 - Kim, B. A1 - Bucar-Miklavcic, M. A1 - Hopley, C. A1 - Nammoonnoy, J. A1 - Murray, J. A1 - Wilson, W. A1 - Toman, B. A1 - Itoh, N. A1 - Gokcen, T. A1 - Krylov, A. A1 - Mikheeva, A. T1 - CCQM-K146 low-polarity analyte in high fat food: benzo a pyrene in olive oil JF - Metrologia N2 - The demonstration of competency and equivalence for the assessment of levels of contaminants and nutrients in primary foodstuffs is a priority within the 10-year strategy for the OAWG Track A core comparisons. The measurements are core challenges for reference material producers and providers of calibration Services. This key comparison related to low polarity analytes in a high fat, low protein, low carbohydrate food matrix and Benzo[a]pyrene in edible oil was the model System selected to align with this class within the OAWG strategy. Evidence of successful participation in formal, relevant international comparisons is needed to document measurement capability claims (CMCs) made by national metrology institutes (NMIs) and designated institutes (Dis). 16 National Metrology Institutions participated in the Track A Key Comparison CCQM-K146 Low-Polarity Analyte in high fat food: Benzo[a]pyrene in Olive Oil. Participants were requested to evaluate the mass fractions, expressed in µg/kg, of Benzo[a]pyrene in the olive oil material. The KCRV was determined from the results of all NMIs/DIs participating in the key comparison that used appropriately validated methods with demonstrated metrological traceability. Different methods such as liquid-liquid extraction, GPC and SPE were applied in the sample pretreatment and HPLC-FLD, HPLC-MS/MS, and GC-MS or GC-MS/MS were applied for detection by the participants. The mass fractions for BaP were in the range of (1.78 to 3.09) µg/kg with Standard uncertainties of (0.026 to 0.54) µg/kg, with corresponding relative Standard uncertainties from 0.9% to 21%. Five labs withdrew their result from the Statistical evaluation of the KCRV for technical reasons. One lab was excluded from the KCRV evaluation, as they did not meet the CIPM metrological traceability requirements. A Hierarchical Bayes option was selected for the KCRV value, which was determined as 2.74 µg/kg with a Standard uncertainty of 0.03 µg/kg. The 10 institutes those were included in the calculation of the consensus KCRV all agreed within their Standard uncertainties. Successful participation in CCQM-K146 demonstrates the measurement capabilities in determining mass fraction of organic compounds, with molecular mass of 100 g/mol to 500 g/mol, having low polarity pKow < -2, in mass fraction range from 0.1 µg/kg to 1000 µg/kg in a high fat, low protein, low carbohydrate food matrix. KW - Metrology KW - CCQM KW - Food KW - PAH PY - 2020 DO - https://doi.org/10.1088/0026-1394/57/1a/08017 VL - 57 IS - 1a SP - 08017 AN - OPUS4-52435 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bulakhe, R. N. A1 - Nguyen, V. Q. A1 - Lee, Y. R. A1 - Zhang, H. A1 - Zhang, S. A1 - Shim, J.-J. A1 - Tuma, Dirk T1 - Chemically grown 3D copper hydroxide electrodes with different morphologies for high-performance asymmetric supercapacitors JF - Journal of Industrial and Engineering Chemistry N2 - The present study investigated decoration of Cu(OH)₂ with different morphologies by copper precursors on 3D nickel foam. The Cu(OH)₂-A (nano flower)electrode showed an excellent capacitance of 1332 Fg⁻¹ at current density of 2 Ag⁻¹ compared to the Cu(OH)₂-C (nano ribbon, 1100 Fg⁻¹) and Cu(OH)₂-S (nano Long leaf, 1013 Fg⁻¹) electrodes. An asymmetric supercapacitor (ASC) was fabricated and showed a Maximum capacitance of 165 Fg⁻¹ at current density of 2 Ag⁻¹ with high energy density of 66.7 Wh kg⁻¹ and power density of 5698 W kg⁻¹ with excellent stability of 80 % after 10,000 cycles. KW - Copper hydroxide KW - Nickel foam KW - Supercapacitor PY - 2018 DO - https://doi.org/10.1016/j.jiec.2018.05.043 SN - 1226-086X SN - 1876-794X VL - 66 SP - 288 EP - 297 PB - Elsevier B. V. CY - Amsterdam AN - OPUS4-45930 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sun, F. A1 - Wang, C. A1 - Osenberg, M. A1 - Dong, K. A1 - Zhang, S. A1 - Yang, C. A1 - Wang, Y. A1 - Hilger, A. A1 - Zhang, J. A1 - Dong, S. A1 - Markötter, Henning A1 - Manke, I. A1 - Cui, G. T1 - Clarifying the Electro-Chemo-Mechanical Coupling in Li10SnP2S12 based All-Solid-State Batteries JF - Advanced Energy Materials N2 - A fundamental clarification of the electro-chemo-mechanical coupling at the solid–solid electrode|electrolyte interface in all-solid-state batteries (ASSBs) is of crucial significance but has proven challenging. Herein, (synchrotron) X-ray tomography, electrochemical impedance spectroscopy (EIS), time-of-flight secondary-ion mass spectrometry (TOF-SIMS), and finite element analysis (FEA) modeling are jointly used to decouple the electro-chemo-mechanical coupling in Li10SnP2S12-based ASSBs. Non-destructive (synchrotron) X-ray tomography results visually disclose unexpected mechanical deformation of the solid electrolyte and electrode as well as an unanticipated evolving behavior of the (electro)chemically generated interphase. The EIS and TOFSIMS probing results provide additional information that links the interphase/electrode properties to the overall battery performance. The modeling results complete the picture by providing the detailed distribution of the mechanical stress/strain and the potential/ionic flux within the electrolyte. Collectively, these results suggest that 1) the interfacial volume changes induced by the (electro)chemical reactions can trigger the mechanical deformation of the solid electrode and electrolyte; 2) the overall electrochemical process can accelerate the interfacial chemical reactions; 3) the reconfigured interfaces in turn influence the electric potential distribution as well as charge transportation within the SE. These fundamental discoveries that remain unreported until now significantly improve the understanding of the complicated electro-chemo-mechanical couplings in ASSBs. KW - All-solid-state batteries KW - Lithium metal batteries KW - Solid electrolytes KW - Sulfide solid electrolytes KW - Synchrotron X-ray tomography PY - 2022 DO - https://doi.org/10.1002/aenm.202103714 SN - 1614-6832 SP - 2103714 PB - Wiley VHC-Verlag AN - OPUS4-54431 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zheng, Y. A1 - Zhang, S. A1 - Ma, J. A1 - Sun, F. A1 - Osenberg, M. A1 - Hilger, A. A1 - Markötter, Henning A1 - Wilde, F. A1 - Manke, I. A1 - Hu, Z. A1 - Cui, G. T1 - Codependent failure mechanisms between cathode and anode in solid state lithium metal batteries: mediated by uneven ion flux JF - Science Bulletin N2 - An in-depth understanding of the degradation mechanisms is a prerequisite for developing the nextgeneration all solid-state lithium metal battery (ASSLMB) technology. Herein, synchrotron X-ray computed tomography (SXCT) together with other probing tools and simulation method were employed to rediscover the decaying mechanisms of LiNi0.8Co0.1Mn0.1O2 (NCM)|Li6PS5Cl (LPSCl)|Li ASSLMB. It reveals that the detachment and isolation of NCM particles cause the current focusing on the remaining active regions of cathode. The extent of Li stripping and the likelihood of Li+ plating into LPSCl facing the active NCM particles becomes higher. Besides, the homogeneity of Li stripping/plating is improved by homogenizing the electrochemical reactions at the cathode side by LiZr2(PO4)3 (LZP) coating. These results suggest a codependent failure mechanism between cathode and anode that is mediated by uneven Li ion flux. This work contributes to establish a holistic understanding of the degradation mechanisms in ASSLMBs and opens new opportunities for their further optimization and evelopment. KW - Current density distribution KW - Lithium ion flux KW - Solid-state lithium metal batteries KW - Codependent failure mechanism KW - Cathode deactivation PY - 2023 DO - https://doi.org/10.1016/j.scib.2023.03.021 SN - 2095-9273 VL - 68 IS - 8 SP - 813 EP - 825 PB - Elsevier B.V. AN - OPUS4-57309 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zerbst, Uwe A1 - Bruno, Giovanni A1 - Buffière, J.-Y. A1 - Wegener, T. A1 - Niendorf, T. A1 - Wu, T. A1 - Zhang, X. A1 - Kashaev, N. A1 - Meneghetti, G. A1 - Hrabe, Nik A1 - Madia, Mauro A1 - Werner, Tiago A1 - Hilgenberg, Kai A1 - Koukolikova, M. A1 - Prochazka, R. A1 - Dzugan, J. A1 - Möller, B. A1 - Beretta, S. A1 - Evans, Alexander A1 - Wagener, R. A1 - Schnabel, K. T1 - Damage tolerant design of additively manufactured metallic components subjected to cyclic loading: State of the art and challenges JF - Progress in materials science N2 - This article is an outcome of a workshop on Fatigue of Additive Manufactured Metallic Components jointly organized by the Federal Institute for Materials Research and Testing (BAM) Berlin, Germany and the National Institute of Standards and Technology (NIST) Boulder, CO, U.S.A. The aim of the workshop was a comprehensive discussion of the specific aspects of additively manufactured (AM) components in regard to failure under cyclic loading. Undoubtedly, a better understanding and the further development of approaches for damage tolerant component design of AM parts are among the most significant challenges currently facing the use of these new technologies. This article presents a thorough overview of the workshop discussions. It aims to provide a review of the parameters affecting the damage tolerance of AM parts with special emphasis on the process parameters intrinsic to the AM technologies, the resulting defects and residual stresses. Based on these aspects, concepts for damage tolerant component design for AM are reviewed and critically discussed. KW - Additive manufacturing KW - Fatigue loading KW - Component assessment KW - Damage tolerance KW - Defects KW - Residual stresses PY - 2021 DO - https://doi.org/10.1016/j.pmatsci.2021.100786 SN - 0079-6425 VL - 121 PB - Elsevier CY - Amsterdam AN - OPUS4-51937 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhang, X. A1 - Zhang, J. A1 - Wang, H. A1 - Rogal, J: A1 - Li, H.-Y. A1 - Wei, S.-H. A1 - Hickel, Tilmann T1 - Defect-characterized phase transition kinetics JF - Applied physics reviews N2 - Phase transitions are a common phenomenon in condensed matter and act as a critical degree of freedom that can be employed to tailor the mechanical or electronic properties of materials. Understanding the fundamental mechanisms of the thermodynamics and kinetics of phase transitions is, thus, at the core of modern materials design. Conventionally, studies of phase transitions have, to a large extent, focused on pristine bulk phases. However, realistic materials exist in a complex form; their microstructures consist of different point and extended defects. The presence of defects impacts the thermodynamics and kinetics of phase transitions, but has been commonly ignored or treated separately. In recent years, with the significant advances in theoretical and experimental techniques, there has been an increasing research interest in modeling and characterizing how defects impact or even dictate phase transitions. The present review systematically discusses the recent progress in understanding the kinetics of defect-characterized phase transitions, derives the key mechanisms underlying these phase transitions, and envisions the remaining challenges and fruitful research directions. We hope that these discussions and insights will help to inspire future research and development in the field. KW - Kinetics KW - Atomistic models KW - Phase transitions KW - Defects PY - 2022 DO - https://doi.org/10.1063/5.0117234 SN - 1931-9401 VL - 9 IS - 4 SP - 1 EP - 42 PB - AIP CY - New York, NY AN - OPUS4-56507 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kruschwitz, Sabine A1 - Zhang, Z. A1 - Weller, A. A1 - Nordsiek, S. T1 - Effect of evaporative drying on complex conductivity spectra of sandstones JF - Geophysics N2 - Dehydration is a common process occurring in natural environments, rocks, and building materials. Suitable methods for monitoring the changing moisture content should be identified. We have investigated the impact of dehydration of sandstones on complex conductivity spectra. Spectral induced polarization measurements were performed on five sandstone samples during evaporative drying. The complex conductivity spectra indicate considerable changes with decreasing saturation. The relationship between conductivity and saturation can be described by a power law known as the second empirical Archie equation. Separate saturation exponents have been determined for the real and imaginary parts of conductivity. The imaginary part of conductivity indicates higher saturation exponents for the investigated sandstones compared to the real part. Obviously, the saturation exponents depend on the method used for changing water saturation. Evaporative drying, which is used in our experiments, causes an increase of pore-water salinity and results in lower saturation exponents for the real part of conductivity but higher exponents for the imaginary part in comparison with the classical imbibition/Drainage technique. We evaluate a theoretical approach that considers the influence of pore water salinity on the saturation exponents of the real and imaginary parts of conductivity. The complex conductivity spectra are processed by a Debye decomposition procedure. The resulting integrating parameters such as direct current resistivity, total chargeability, normalized chargeability, and mean relaxation time indicate a power law dependence on saturation. Our experiments indicate that the imaginary part of conductivity and normalized chargeability have a high sensitivity related to the drying process of rocks and might be suitable indicators to Monitor the changes of moisture content in sandstones. KW - Saturation KW - Spectral induced polarization KW - Sandstones KW - Evaporative drying PY - 2019 DO - https://doi.org/10.1190/GEO2018-0054.1 SN - 0016-8033 VL - 84 IS - 1 SP - MR61 EP - MR72 PB - SEG - Society of Exploration Geophysicists CY - Tulsa, Okla. AN - OPUS4-47499 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -