TY - CONF A1 - Richter, Matthias T1 - Primary References for the Determination of Sulphur Impurities in Hydrogen N2 - Fuel cell electric vehicles are expanding quickly from light-duty to heavy-duty applications, such as buses or trucks. Hydrogen fuel quality needs to comply with ISO 14687:2025 to avoid any harmful impact on the vehicles. Total sulphur is one of the most impactful contaminants to a fuel cell system and has a threshold of 4 nmol/mol. In the European Partnership for Metrology (EPM) project Met4H2, BAM together with VSL, the National Metrology Institute of the Netherlands, developed novel gaseous primary reference materials (PRM) to improve the accuracy of the analysis of 7 sulphur compounds (hydrogen sulphide, carbonyl sulphide, methyl mercaptan, ethyl mercaptan, dimethyl sulphide, diethyl sulphide, and tetrahydrothiophene) for the quality control of hydrogen as fuel gas at this challenging amount fraction. These PRM were cross-validated using thermal desorption gas chromatography with a sulphur chemiluminescence detector (TD-GC/SCD). The results are presented and limits discussed. T2 - Joint workshop EMN for Energy Gases CY - Delft, Netherlands DA - 26.03.2025 KW - Sulphur impurities KW - Hydrogen KW - GC/SCD KW - Reference gas standards PY - 2025 AN - OPUS4-62818 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hoffmann, V. A1 - Uhlemann, M. A1 - Richter, Silke A1 - Pfeifer, jens T1 - Calibration capacity of hot-pressed hydrogen standards for glow discharge optical emission and mass spectrometry N2 - Mixed copper and titanium hydride powder was hot-pressed and characterized by Carrier Gas Hot Extraction, XRay Diffraction, Thermal Gravimetric Analysis coupled with Mass Spectrometry, and Scanning Electron Microscopy. The hot-pressed and five conventional samples were applied for calibration of hydrogen in Glow Discharge Optical Emission and Mass Spectrometry. Up to the introduction of 15 ng/s hydrogen the Emission yield model is useful in Glow Discharge Optical Emission Spectrometry. A correlation between saturation and even reversal of the emission yield of the spectral lines H121, H486 and H656 and low sputtering rates was found. Hydrogen effects exist for the spectral lines of Cu(II) 219 and Ti(I) 399. In Glow Discharge Mass Spectrometry, a linear dependency of the 1H ion current on the sputtered mass per time exists over the total range of hydrogen content investigated. Hydrogen effects also exist for the sensitivity of 48Ti and 63Cu. The sputtering rate of two-phase materials depends linearly on the sputtered mass per time of one phase, which allows the sputtering rate of two-phase materials with known composition to be predicted. KW - Hot-pressing KW - GD-OES KW - GD-MS KW - Calibration KW - Hydrogen KW - Titanium hydride KW - Sputtering KW - Two-phase system PY - 2021 DO - https://doi.org/10.1016/j.sab.2020.106039 VL - 176 SP - 106039 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-52074 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Wetzel, Annica A1 - Oczan, Ozlem A1 - Nietzke, Jonathan A1 - Richter, Tim A1 - Schröpfer, Dirk T1 - Hydrogen diffusion and local Volta potential in high- and medium-entropy alloys N2 - High-entropy alloys (HEAs) are characterized by a solid solution of minimum five and medium-entropy alloys (MEAs) of minimum three principal alloying elements in equiatomic proportions. They show exceptional application properties, such as high-strength and ductility or corrosion resistance. Future HEA/MEA-components could be exposed to hydrogen containing environments like vessels for cryogenic or high-pressure storage where the hydrogen absorption and diffusion in these materials is of interest. In our study, we investigated the HEA Co20Cr20Fe20Mn20Ni20 and the MEA Co33.3Cr33.3Ni33.3. For hydrogen ingress, cathodic charging was applied and diffusion kinetic was measured by high-resolution thermal desorption spectros-copy using different heating rates up to 0.250 K/s. Peak deconvolution resulted in high-temperature desorption peaks and hydrogen trapping above 280 °C. A total hydrogen concentration > 40 ppm was identified for the MEA and > 100 ppm for HEA. This indicates two important effects: (1) delayed hydrogen diffusion and (2) considerable amount of trapped hydrogen that must be anticipated for hydrogen assisted cracking phenomenon. Local electrochemical Volta potential maps had been measured for the hydrogen free condition by means of high-resolution Scanning Kelvin Probe Force Microscopy (SKPFM). T2 - Symposium on Materials and Joining Technology CY - Online meeting DA - 07.09.2020 KW - Hydrogen KW - High-entropy alloy KW - Diffusion KW - Scanning kelvin probe force microscopy KW - Corrosion PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-511684 DO - https://doi.org/10.1088/1757-899X/882/1/012015 VL - 882 SP - 1 EP - 15 PB - IOP Publishing CY - Bristol AN - OPUS4-51168 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Richter, Tim T1 - Hydrogen diffusion and desorption characteristics of a CoCrFeMnNi high entropy and a CoCrNi medium entropy alloy N2 - High-entropy alloys (HEAs) are innovative high-performance materials that have attracted more and more research attention. HEAs are characterized by a solid solution of typically five equiatomic metallic elements. In addition, medium-entropy alloys (MEA, with three elements) are of interest and become more and more important. Depending on the alloy concept, HEAs and MEAs show exceptional mechanical properties, especially high-strength and ductility combinations at both cryogenic and elevated temperatures combined with excellent corrosion resistance. Future structural HEA/MEA components can be exposed to potential applications with hydrogen containing environments like high-temperature water in pressurized nuclear reactors or aerospace structures. Other potential applications could be in materials for vessel walls in the field of cryogenic and high-pressure hydrogen storage. So far, the susceptibility of HEAs/MEAs to hydrogen assisted cracking (if any) and the hydrogen diffusion is not investigated in detail yet and can limit or extend possible applications of HEA/MEA as structural materials. In our work, we focused on the hydrogen absorption, diffusion, and distribution in a HEA (CoCrFeMnNi the original Cantor-alloy) and a MEA (CoCrNi). Cathodic hydrogen charging was carried out for the hydrogen ingress, and thermal desorption analysis (TDA) revealed complex hydrogen trapping in both alloy types up to 300 °C. The absorbed total hydrogen concentrations were > 100 ppm for the HEA and > 40 ppm for MEA. In addition, the assessment of the peak deconvolution is not trivial and must consider both experimental and microstructure influences. T2 - 4th International Conference on Metals and Hydrogen - Steely & Hydrogen 2022 CY - Ghent, Belgium DA - 11.10.2022 KW - Hydrogen KW - High-entropy alloy KW - Multiple principal element alloy KW - Thermal desorption analysis KW - Diffusion PY - 2022 SP - 1 EP - 11 CY - Ghent, Belgium AN - OPUS4-56076 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Richter, Tim T1 - Characterization of Hydrogen Diffusion in a Thick-walled Submerged Arc Multi-Layer Weld Joint N2 - The energy production of the future will be dominated by CO2-emission free techniques like wind turbines and become essential in scope of the planned hydrogen economy. As onshore installation capacity is limited, the in-crease of the number of offshore wind turbines (OWT) is a major goal. In that connection, the OWTs continuously increase in size and weight and demand adequate foundations concepts like monopiles or tripods. These compo-nents are typically manufactured from welded mild steel plates with thickness up to 200 mm. The predominant welding technique is submerged arc welding (SAW) with up to five wires. In accordance with the standards, the occurrence of delayed hydrogen assisted cracking is anticipated by either a hydrogen removal heat treatment (HRHT) or a so-called minimum waiting time (MWT) before non-destructive testing (NDT) of the respective weld joint is allowed. The reason for the MWT is the necessary time for the hydrogen diffusion at ambient temperature due the high plate thickness. Both the effectiveness of a HRHT at elevated temperatures or the MWT at ambient temperature can be estimated by calculation of the diffusion time. This time depends on reliable hydrogen diffu-sion coefficients and these are rare in literature. For that reason, this study presents the hydrogen diffusion coef-ficients obtained from a multi-layer SAW joint of an offshore steel grade. Two different experimental techniques were used to identify the respective diffusion behavior: (1) hydrogen desorption experiments with a carrier gas hot extraction analyzer at elevated temperatures for the characterization of a HRHT and (2) the electrochemical permeation technique at ambient temperature for the characterization of an MWT. From both experiments, the respective diffusion coefficients were calculated. The obtained DCs are different from those reported in literature, i.e., the duration or applicability of a HRHT or MWT must be critically discussed. T2 - European Congress and Exhibition on Advanced Materials and Process - Euromat 2021 CY - Online meeting DA - 13.09.2021 KW - Welding KW - Offshore KW - Wind turbine KW - Hydrogen KW - Cracking PY - 2021 AN - OPUS4-53296 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Richter, Tim A1 - Mayr, P. A1 - Nitsche, A. A1 - Mente, Tobias A1 - Böllinghaus, Thomas T1 - Hydrogen diffusion in creep-resistant 9% Cr P91 multi-layer weld metal N2 - Welded components of P91 9% Cr steel demand for careful welding fabrication with necessary post weld heat treatment (PWHT). Before the PWHT, a hydrogen removal heat treatment is necessary for avoidance of hydrogen assisted cracking (HAC). In this context, the microstructure and temperature-dependent hydrogen diffusion is important, and reliable diffusion coefficients of P91 weld metal are rare. For that reason, the diffusion behavior of P91 multi-layer weld metal was investigated for as-welded (AW) and PWHT condition by electrochemical permeation experiments at room temperature and carrier gas hot extraction (CGHE) from 100 to 400 °C. Hydrogen diffusion coefficients were calculated, and the corresponding hydrogen concentration was measured. It was ascertained that both heat treatment conditions show significant differences. At room temperature the AW condition showed significant hydrogen trapping expressed by to seven times lower diffusion coefficients. A preferred diffusion direction was found in perpendicular direction expressed by high permeability. The CGHE experiments revealed lower diffusion coefficients for the AW condition up to 400 °C. In this context, a hydrogen concentration of approximately 21 ml/100 g was still trapped at 100 °C. For that reason, a certain HAC susceptibility of as-welded P91 weld metal cannot be excluded, and hydrogen removal should be done before PWHT. KW - Creep resisting materials KW - Diffusion KW - Hydrogen KW - Weld metal KW - Post weld heat treatment KW - Microstructure PY - 2020 DO - https://doi.org/10.1007/s40194-019-00828-8 SN - 0043-2288 VL - 64 IS - 2 SP - 267 EP - 281 PB - Springer AN - OPUS4-50471 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -