TY - CONF A1 - Reinsch, Stefan T1 - Surface-Initiated Microstructure Formation in Glass Ceramics N2 - Up to now, oriented surface crystallization phenomena are discussed controversially, and related studies are restricted to few glasses. For silicate glasses we found a good correlation between the calculated surface energy of crystal faces and oriented surface nucleation. Surface energies were estimated assuming that crystal surfaces resemble minimum energy crack paths along the given crystal plane. This concept was successfully applied by Rouxel in calculating fracture surface energies of glasses. Several oriented nucleation phenomena can be herby explained assuming that high energy crystal surfaces tend to be wetted by the melt. This would minimize the total interfacial energy of the nucleus. Furthermore, we will discuss the evolution of the microstructure and its effect on the preferred crystal orientation. T2 - 26th International Congress on Glass CY - Berlin, Germany DA - 03.07.2022 KW - Glass KW - Oriented surface crystallization KW - Surface energy KW - Bond energy KW - Nucleation mode PY - 2022 AN - OPUS4-56070 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Chen, Y.-F. A1 - Contreras Jaimes, A. T1 - Datengetriebener Workflow für die beschleunigte Entwicklung von Glas (GlasDigital) N2 - Das Projekt GlasDigital wurde im allgemeinen vorgestellt, sowie die einzelnen Zwischenstände der verschiedenen Arbeitspakete aller Projektpartner präsentiert. Die allgemeine Porjektvorstellung ist auf deutsch. Die Zwischenstände der Arbeitsinhalte sind auf englisch. T2 - PMD Vollversammlung CY - Berlin, Germany DA - 03.11.2022 KW - Oxidglas KW - Robotische Glasschmelzanlage KW - ML KW - Ontologie KW - Digitaler Zwilling KW - Bildanalyse PY - 2022 AN - OPUS4-56491 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Weh, Lothar A1 - Reinsch, Stefan T1 - Oberflächenprofile partiell kristallisierter Silikatgläser T2 - 73. Glastechnische Tagung CY - Halle (Saale), Deutschland DA - 1999-05-31 KW - Kristallisation KW - Silikatgläser PY - 1999 SP - 26 EP - 29 CY - Frankfurt/Main AN - OPUS4-819 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Agea Blanco, Boris A1 - Blaess, C. A1 - Reinsch, Stefan A1 - Brauer, D. A1 - Müller, Ralf T1 - Sintering and foaming of barium and calcium silicate glass powders N2 - Sintering and foaming of barium and calcium silicate glass powder compacts have been studied for different powder milling. Sintering was measured by means of heating microscopy backed up by XRD, DTA, Vacuum Hot Extraction (VHE) and electron microscopy. Foaming intensity strongly increased with decreasing glass partiefe size. Although powder compacts were uniaxially pressed and sintered in ambient air, foaming was affected by the milling atmosphere and most intensive for milfing in C02. Conformingly, VHE studies revealed that foaming of fully sintered samples was mainly driven by C02, even for powders milled in technical air, Ar and N2. Prolonged storage of air milled barium silicate glass powders in ambient air before pressing and sintering caused further increase of foaming intensity. These findings indicate that carbonaceous species are preferentially trapped to or close beneath the powder surface during milling and later storage. The temperature range of C02 degassing from fully sintered barium and calcium silicate g/ass powder compacts fits the temperature ranges of decomposition of BaC03 and CaC03 mix-milled with the respective barium and calcium silicate glass powders. T2 - IMAPS/ACerS 11th International CICMT conference and exhibition CY - Dresden, Germany DA - 20.04.2015 KW - Sintering KW - Foaming KW - Silicate glass powders KW - Barium and calcium silicate plass powders KW - Degassing PY - 2015 SN - 978-1510804562 SP - 31 EP - 37 AN - OPUS4-35250 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Rössler, C. A1 - Bauer, Ute A1 - Müller, Ralf A1 - Deubener, J. A1 - Behrens, H. T1 - Water, the other network modifier in borate glasses N2 - In the present study we have investigated whether the effect of water on properties of borate glasses resembles that of alkali oxide. Soda-lime-borate glasses with nominal compositions of x Na2O, 10 CaO, (90-x) B2O3 (x = 5, 15 and 25 mol%) were doped with up to 8 wt.% H2O by processing glass powder + distilled water in platinum capsules in an internally heated gas pressure vessel at 1523 K and 500 MPa. The water content of hydrous glasses was determined by Karl-Fischer titration and near-infrared spectroscopy. The glass transition temperature T-g. was derived from DTA and micropenetration experiments for which the effect of water loss at the surface of the hydrous glasses was studied. Heating glass samples at 10 K min(-1) in the DTA resulted in T-g values which are close to T-12 isokom temperatures confirming the equivalence of enthalpy relaxation and viscous relaxation for borate glasses. For all three glass series it is shown that T-g strongly decreases whereas the liquid fragility strongly increases upon the addition of water. These findings reveal that H2O primarily causes breaking of B-O-B bonds rather than supporting 4-fold coordinated boron as it is well-known for alkali oxides in this concentration range. (C) 2015 Elsevier B.V. All rights reserved. KW - Wasserhaltige Gläser KW - Viskosität KW - Boratgläser KW - Thermische Analyse KW - Viscosity KW - Borate glasses KW - Thermal analysis KW - Water-bearing glasses PY - 2016 DO - https://doi.org/10.1016/j.jnoncrysol.2015.10.010 SN - 0022-3093 VL - 432 SP - 208 EP - 217 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-35123 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reinsch, Stefan A1 - Eberstein, Markus A1 - Müller, Ralf A1 - Schiller, Wolfgang Arno A1 - Schweiger, M. T1 - Lastabhängige Schwindung von Glaspulvern N2 - Glasig-kristalline Sinterwerkstoffe werden für vielfältige Anwendungen eingesetzt. Bei einem hohen Glasanteil ist ein Einfluss geringer Lasten auf das Schwindungsverhalten möglich, so dass es zu Fehlinterpretationen des Schwindungsverhaltens bei gebräuchlichen Horizontaldilatometer kommen kann. T2 - 75. Glasetechnische Tagung CY - Wernigerode, Germany DA - 21.05.2001 KW - Glasig-kristalline Sinterwerkstoffe KW - Schwindungsverhalten KW - Horizontaldilatometer PY - 2001 AN - OPUS4-35786 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Agea Blanco, Boris A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Sintering and foaming of barium silicate glass powder compacts N2 - The manufacture of sintered glasses and glass-ceramics, glass matrix composites, and glass-bounded ceramics or pastes is often affected by gas bubble formation. Against this background, we studied sintering and foaming of barium silicate glass powders used as SOFC sealants using different powder milling procedures. Sintering was measured by means of heating microscopy backed up by XPD, differential thermal analysis, vacuum hot extraction (VHE), and optical and electron microscopy. Foaming increased significantly as milling progressed. For moderately milled glass powders, subsequent storage in air could also promote foaming. Although the powder compacts were uniaxially pressed and sintered in air, the milling atmosphere significantly affected foaming. The strength of this effect increased in the order Ar ≈ N2 < air < CO2. Conformingly, VHE studies revealed that the pores of foamed samples predominantly encapsulated CO2, even for powders milled in Ar and N2. Results of this study thus indicate that foaming is caused by carbonaceous species trapped on the glass powder surface. Foaming could be substantially reduced by milling in water and 10 wt% HCl. KW - Glass powder KW - Sintering KW - Foaming KW - SOFC PY - 2016 UR - http://journal.frontiersin.org/article/10.3389/fmats.2016.00045/full?&utm_source=Email_to_authors_&utm_medium=Email&utm_content=T1_11.5e1_author&utm_campaign=Email_publication&field=&journalName=Frontiers_in_Materials&id=214488 DO - https://doi.org/10.3389/fmats.2016.00045 SN - 2296-8016 VL - 3 SP - Article 45, 1 EP - 10 AN - OPUS4-38303 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reinsch, Stefan T1 - Glass transition and viscosity of hydrous soda-lime-borate glasses N2 - Boron oxide glasses usually show low glass transition temperature Tg due to the three-fold oxygen coordination of boron. Adding of alkali and alkaline earth oxides to the glass composition will not decrease but increase Tg due to a change in boron coordination from trigonal to tetrahedral, known as the boron anomaly. Only for higher fractions of alkali oxides, non-bridging oxygens (NBO) are progressively formed in competition with tetrahedrally coordinated boron, which leads to a decrease in viscosity. ln contrast to this well-known behavior of alkali oxides (R2O), there is little known about adding H2O to borate glasses. The present work therefore aims in shedding light on the rheological properties of hydrous soda lime borate glasses with particular focus on the role of water. For doing so, we determined Tg as a function of Na2O and H2O content using differential thermal analysis (DTA) backed up by micropenetration viscosity measurements. Results show that water decreases Tg for all glasses and water concentrations under study (< 8 wt.% total water). Obviously, water mostly causes the formation of NBO having no significant influence on boron coordination as seen for alkaline. T2 - Crystallization 2015 CY - Shanghai, China DA - 07.04.2016 KW - Borate glasses KW - Thermal analyses KW - Viscosity KW - Water-bearing glasses PY - 2016 AN - OPUS4-38318 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Waurischk, Tina A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Kiefer, P. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. T1 - Crack Growth in Hydrous Soda-Lime Silicate Glass N2 - Stable crack growth was measured for nominal dry and water-bearing (6 wt%) soda-lime silicate glasses in double cantilever beam geometry and combined with DMA studies on the effects of dissolved water on internal friction and glass transition, respectively. In vacuum, a decreased slope of logarithmic crack growth velocity versus stress intensity factor is evident for the hydrous glass in line with an increase of b-relaxation intensity indicating more energy Dissipation during fracture. Further, inert crack growth in hydrous glass is found to be divided into sections of different slope, which indicates different water related crack propagation mechanism. In ambient air, a largely extended region II is observed for the hydrous glass, which indicates that crack growth is more sensitive to ambient water. KW - Internal friction KW - Soda-lime silicate glass KW - Water content KW - Stable crack growth KW - DCB geometry KW - Stress intensity factor PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506829 DO - https://doi.org/10.3389/fmats.2020.00066 VL - 7 SP - Articel 66 AN - OPUS4-50682 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Maiwald, M. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Automated Analysis of Slow Crack Growth in Hydrous Soda-Lime Silicate Glasses N2 - To explore the impact of ambient and structural water on static fatigue, the initiation and growth of 3279 Vickers induced median radial cracks were automatically recorded and analyzed. We find that humidity is more efficient in initiating cracks and promoting their growth than water, which is dissolved in the glass structure. In particular for slow crack growth (< 3x10-6 m s-1), tests in dry nitrogen showed a considerable decrease in the crack growth exponent with increasing water content of the glasses. On the other hand, if tests were performed in humid air, the crack growth exponent was independent of the water content of the hydrous glasses, while stress intensity decreased slightly. These observations indicate that water promotes the processes at the crack-tip regardless of its origin. However, ambient water is more efficient. KW - Indentation fracture toughness KW - Slow crack growth KW - Automated analysis KW - Hydrous glass KW - Vickers indentation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513085 DO - https://doi.org/10.3389/fmats.2020.00268 VL - 7 SP - 268 AN - OPUS4-51308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Welter, T. A1 - Müller, Ralf A1 - Deubener, J. A1 - Marzok, Ulrich A1 - Reinsch, Stefan T1 - Hydrogen Permeation Through Glass N2 - Physical storage of gaseous hydrogen under high-pressure in glassy micro-containers such as spheres and capillaries is a promising concept for enhancing safety and the volumetric capacity of mobile hydrogen storage systems. As very low permeation through the container wall is required for storage of compressed hydrogen, development of glasses of minimal hydrogen permeability is needed. For this purpose, one has to understand better the dependence of hydrogen permeability on glass structure. The paper points out that minimizing the accessible free volume is as one strategy to minimize hydrogen permeability. Based on previously measured and comprehensive literature data, it is shown that permeation is independently controlled by ionic porosity and network modifier content. Thus, ionic porosity in modified and fully polymerized networks can be decreased equally to the lowest hydrogen permeability among the glasses under study. Applying this concept, a drop of up to 30,000 with respect to the permeation of hydrogen molecules through silica glass is attainable. KW - Ionic porosity KW - hydrogen storage KW - Glass KW - Permeability KW - Solubility KW - Diffusivity PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513927 DO - https://doi.org/10.3389/fmats.2019.00342 VL - 6 SP - Article 342 AN - OPUS4-51392 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gomes Fernandes, Roger A1 - Al-Mukadam, Raschid A1 - Bornhöft, Hansjörg A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Selle, Susanne A1 - Deubener, Joachim T1 - Viscous Sintering of Acid Leached Glass Powders N2 - The process of viscous flow sintering is a phenomenon that is closely linked to the surface properties of the glass particles. In this work, we studied the extreme case of acid-leaching of soda-lime-silicate glass beads of two different particle size distributions and its effects on non-isothermal viscous sintering of powder compacts. Depth profiling of the chemical composition after leaching revealed a near-surface layer depleted in alkali and alkaline earth ions, associated with concurrent hydration as mass loss was detected by thermogravimetry. Heating microscopy showed that acid treatment of glasses shifted the sinter curves to higher temperatures with increasing leaching time. Modelling of the shrinkage with the cluster model predicted a higher viscosity of the altered surface layer, while analysis of the time scales of mass transport of mobile species (Na+, Ca2+ and H2O) during isochronous sintering revealed that diffusion of Na+ can compensate for concentration gradients before sintering begins. Also, exchanged water species can diffuse out of the altered layer, but the depletion of Ca2+ in the altered surface layer persists during the sinter interval, resulting in a glass with higher viscosity, which causes sintering to slow down. KW - Glass powder KW - Viscous sintering KW - Acid-leaching KW - Sinter retardation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-589008 DO - https://doi.org/10.52825/glass-europe.v1i.681 VL - 1 SP - 37 EP - 53 AN - OPUS4-58900 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Welter, T. A1 - Müller, Ralf A1 - Deubener, J. T1 - Hydrogen Permeability of Tectosilicate Glasses for Tank Barrier Liners N2 - The permeation of hydrogen gas was studied in meta-aluminous (tectosilicate) glass powders of Li2O×Al2O3×SiO2 (LAS), Na2O×Al2O3×SiO2 (NAS) and MgO×Al2O3×SiO2 (MAS) systems by pressure loading and vacuum extraction in the temperatures range 210–310 °C. With this method, both the solubility S and the diffusivity D were determined, while the permeability was given by the product SD. For all glasses, S was found to decrease with temperature, while D increased. Since the activation energy of diffusion of H2 molecules exceeded that of dissolution, permeation increased slightly with temperature. When extrapolated to standard conditions (25 °C), the permeability of tectosilicate glasses was found to be only 10-22–10-24 mol H2 (m s Pa)-1, which is 8–10 magnitudes lower than most polymers. Thin glass liners of these compositions are expected to be the most effective barrier for tanks of pressurised hydrogen. KW - Hydrogen permeation KW - Aluminosilicate glasses KW - Hydrogen storage tank KW - Glass liner PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587284 DO - https://doi.org/10.52825/glass-europe.v1i.425 VL - 1 SP - 1 EP - 11 AN - OPUS4-58728 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Behrens, Harald A1 - Ageo-Blanco, Boris A1 - Reinsch, Stefan A1 - Wirth, Thomas T1 - Foaming Species and Trapping Mechanisms in Barium Silicate Glass Sealants N2 - Barium silicate glass powders 4 h milled in CO2 and Ar and sintered in air are studied with microscopy, total carbon analysis, differential thermal Analysis (DTA), vacuum hot extraction mass spectroscopy (VHE-MS), Fourier-transformed infrared (FTIR) spectroscopy, X-ray photoelectron spectroscopy (XPS), and time-of-flight secondary-ion mass spectrometry (TOF-SIMS). Intensive foaming of powder compacts is evident, and VHE studies prove that foaming is predominantly caused by carbonaceous species for both milling gases. DTA Shows that the decomposition of BaCO3 particles mix-milled with glass powders occurs at similar temperatures as foaming of compacts. However, no carbonate at the glass surface could be detected by FTIR spectroscopy, XPS, and TOF-SIMS after heating to the temperature of sintering. Instead, CO2 molecules unable to rotate identified by FTIR spectroscopy after milling, probably trapped by mechanical dissolution into the glass bulk. Such a mechanism or microencapsulation in cracks and particle aggregates can explain the contribution of Ar to foaming after intense milling in Ar atmosphere. The amount of CO2 molecules and Ar, however, cannot fully explain the extent of foaming. Carbonates mechanically dissolved beneath the surface or encapsulated in cracks and micropores of particle aggregates are therefore probably the major foaming source. KW - Milling KW - Foaming KW - Glass powder KW - Sintering PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-531227 DO - https://doi.org/10.1002/adem.202100445 SN - 1438-1656 VL - 24 IS - 6 SP - 2100445-1 EP - 2100445-13 AN - OPUS4-53122 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chladek, J. A1 - Müller, Ralf A1 - Weh, Lothar A1 - Reinsch, Stefan T1 - Viscous flow and surface crystallization caused by Vickers indentation PY - 2004 SN - 0927-4472 VL - 77 IS - 1 SP - 1 EP - 6 PB - Elsevier CY - Amsterdam AN - OPUS4-6235 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Herstellung von Gläsern mittlerer Wassergehalte T2 - 79. Glastechnische Tagung CY - Würzburg, Deutschland DA - 2005-05-23 KW - Glas KW - Wassergehalt PY - 2005 SN - 3-921089-43-3 SP - 4 Seiten PB - Deutsche Glastechnische Gesellschaft CY - Offenbach AN - OPUS4-7606 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Eberstein, Markus A1 - Thiel, A. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Schiller, Wolfgang Arno T1 - Lösungs- und Kristallisationsvorgänge beim Sintern von Glasmatrix-Kompositen T2 - 79. Glastechnische Tagung CY - Würzburg, Deutschland DA - 2005-05-23 KW - Glaspulver KW - Glasmatrix-Komposit KW - Sintern KW - Kristallisation PY - 2005 SN - 3-921089-43-3 SP - 7 Seiten PB - Deutsche Glastechnische Gesellschaft CY - Offenbach AN - OPUS4-10377 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Eberstein, Markus A1 - Thiel, A. A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Schiller, Wolfgang Arno T1 - Sinterkinetik von Glasmatrix-Kompositen mit reaktiver Dispersphase T2 - 80. Glastechnische Tagung CY - Dresden, Deutschland DA - 2006-06-12 PY - 2006 SN - 3-921089-46-8 SP - 4 Seiten PB - Verl. d. Dt. Glastechn. Ges. CY - Offenbach AN - OPUS4-14046 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reinsch, Stefan T1 - Partial solution of dispersed alpha-Al2O3-particles in alumoborosilicate glass T2 - 81. GlastechnischeTagung und 4. DGG-Symposium "Novel Optical Technologies" CY - Aachen, Germany DA - 2007-06-04 PY - 2007 AN - OPUS4-15494 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reinsch, Stefan T1 - Effect of dispersed Al2O2-particles on sintering of glass matrix composites T2 - 10th International Conference and Exhibition of the European Ceramic Society CY - Berlin, Germany DA - 2007-06-17 PY - 2007 AN - OPUS4-15495 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Reinsch, Stefan A1 - Meng, S. A1 - Eberstein, Markus A1 - Thiel, A. A1 - Müller, Ralf A1 - Deubener, J. T1 - Partial Solution of Dispersed alpha-Al2O3-Particles in Alumoborosilicate Glass T2 - 81. Glastechnische Tagung CY - Aachen, Deutschland DA - 2007-06-04 KW - Glasmatrixkomposite KW - Lösung KW - Sintern PY - 2007 SN - 978-3-921089-52-1 IS - CD-ROM SP - 1 EP - 5 PB - Deutsche Glastechnische Gesellschaft CY - Offenbach AN - OPUS4-16108 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Eberstein, Markus A1 - Reinsch, Stefan A1 - Schiller, Wolfgang Arno A1 - Deubener, J. A1 - Thiel, A. T1 - Effect of rigid inclusions on sintering of low temperature co-fired ceramics KW - Sintering KW - Glass Matrix Composites KW - Rigid Inclusion KW - Effective Viscosity KW - Kinetic Modelling KW - LTCC PY - 2007 SN - 1753-3562 SN - 0017-1050 SN - 0031-9090 SN - 1750-6697 VL - 48 IS - 4 SP - 259 EP - 266 PB - Society of Glass Technology CY - Sheffield AN - OPUS4-16211 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Gaber, Martin A1 - Müller, Ralf A1 - Schiller, Wolfgang Arno T1 - Rate controlled debindering of glass ceramic composites N2 - Green compacts of ceramics, glass ceramic composites and sinter glass ceramics contain different amounts of organic materials added as pressing aids or binders. Before sintering, these organics have to burn out completely. In oxidising atmospheres, the debindering process is mostly exothermic and therefore difficult to control. This uncontrolled heat production due to locally enhanced debindering and respective gas release may cause damages in the green compact microstructure. Therefore, debindering is usually operated with very low heating rates (< 3 K/min) which requires long processing times of many hours. In this paper, we will show that it is possible to reduce the processing time for debindering dramatically by using the decomposition rate of the organic binder, detected by the weight loss of the sample, as a control factor of the furnace. T2 - 9th ESG (European Society of Glass) Conference with the Annual Meeting of the ICG Glass - "The challenge for the 21st century" CY - Trencin, Slovakia DA - 2008-06-22 KW - Debindering KW - Thermo gravimetry KW - Glass ceramic composites PY - 2005 SN - 1022-6680 SN - 1662-8985 VL - 39-40 SP - 583 EP - 586 PB - Trans Tech Publ. CY - Zurich AN - OPUS4-17840 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, J. A1 - Behrens, H. A1 - Müller, Ralf A1 - Zietka, S. A1 - Reinsch, Stefan T1 - Kinetic fragility of hydrous soda-lime-silica glasses N2 - The effect of hydration on the kinetic fragility of soda-lime-silica glasses was investigated by viscometry in the glass transition range. Water-bearing glasses were prepared from industrial float glass (FG) and a ternary model glass (NCS = 16Na2O 10CaO 74SiO2 in mol%) by bubbling steam through the melt at 1480 °C and up to 7 bar. Additionally, a sodium borosilicate glass (NBS = 16Na2O 10B2O3 74SiO2 in mol%) was hydrated under equal conditions. As detected by infrared spectroscopy water dissolves in the glasses exclusively as OH-groups. The hydration resulted in a total water content CW up to ~ 0.2 wt% for FG, NCS and NBS glasses. Kinetic fragility, expressed by the steepness index m, was determined from the temperature dependence of η at the glass transition. Viscosity data from previous studies on hydrous float glasses (CW > 1 wt%) were surveyed together with literature data on the (H2O)–Na2O–CaO–SiO2, (H2O)–Na2O–SiO2 and (H2O)–SiO2 systems to expand the range of water concentration and bulk composition. We could demonstrate that m decreases for all glasses although water is dissolved as OH and should depolymerize the network. An empirical equation of the general type m = a - b logCW where a, b are fitting parameters, enables m to be predicted, for each glass series as function of the water content CW. The enlarged data base shows that the parameter B of the Arrhenius viscosity-temperature relation decreases much stronger than the isokom temperature at the glass transition. KW - Soda-lime-silica KW - Fragility KW - Viscosity KW - Water in glass PY - 2008 DO - https://doi.org/10.1016/j.jnoncrysol.2008.04.021 SN - 0022-3093 VL - 354 IS - 42-44 SP - 4713 EP - 4718 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-18187 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reinsch, Stefan T1 - Sinterkinetik von Glasmatrix-Kompositen T2 - Symp. HLK 2008, Keramik in Wissenschaft und Praxis CY - Hamburg, Germany DA - 2008-02-26 PY - 2008 AN - OPUS4-18226 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Eberstein, Markus A1 - Deubener, J. A1 - Thiel, A. A1 - Schiller, Wolfgang Arno T1 - Effects of dispersed Al2O3 particles on sintering of LTCC N2 - The sintering of Low Temperature Co-fired Ceramics prepared from alumoborosilicate glass- and Al2O3 powders of similar small particle size was studied by dilatometry, heating microscopy, microstructure analysis, glass- and effective viscosity measurements. The steric effect of Al3O3 inclusions was studied using a gnon-reactiveh model composite. With increasing Al3O3 volume fraction (Φ ≤ 0.45), sintering decelerates and its final stage shifts to higher temperature. The attainable shrinkage is reduced as Al2O3 particle clusters bearing residual pores become more frequent. The kinetics of sintering could be described formally superposing the weighed contributions of differentially sized and randomly composed glass-crystal particle clusters and assuming a sintering rate controlled by the effective matrix viscosity, which increases with Φ and with progressive wetting of Al2O3 particles during densification. The "reactive" model composite shows significant dissolution of Al2O3 into the glass, which has two opposed effects on sintering: reducing Φ and increasing glass viscosity. For the present case (Φ = 0.25), the latter effect dominates and sintering is retarded by Al2O3 dissolution. Crystallization of wollastonite starts after full densification. Dissolution of Al2O3 was found to promote the subsequent growth of anorthite. KW - LTCC KW - Glass matrix composites KW - Al2O3-inclusions KW - Sintering kinetics PY - 2005 SN - 1022-6680 SN - 1662-8985 VL - 39-40 SP - 375 EP - 380 PB - Trans Tech Publ. CY - Zurich AN - OPUS4-18441 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -