TY - JOUR A1 - Sturm, Patrick A1 - Gluth, Gregor A1 - Brouwers, H.J.H. A1 - Kühne, Hans-Carsten T1 - Synthesizing one-part geopolymers from rice husk ash N2 - One-part geopolymers offer advantages over conventional geopolymers with regard to handling and storage of feedstocks. However, they often suffer from a low degree of reaction, a high amount of crystalline byproducts, and consequently low strength. In this study, one-part geopolymers were produced from rice husk ash (RHA) and sodium aluminate, and investigated by XRD, ATR-FTIR, SEM and compressive strength testing. The compressive strength of the material was 30 MPa, i.e. significantly higher than for comparable one-part geopolymers. This is attributed to an almost complete reaction of the RHA and the absence of crystalline byproducts (zeolites) in the hardened geopolymer. KW - Alkali-activation KW - Geopolymers KW - One-part formulation KW - Bio-based materials KW - Rice husk ash PY - 2016 DO - https://doi.org/10.1016/j.conbuildmat.2016.08.017 SN - 0950-0618 VL - 124 SP - 961 EP - 966 PB - Elsevier Ltd. AN - OPUS4-37226 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Greiser, Sebastian A1 - Gluth, Gregor A1 - Sturm, Patrick A1 - Jäger, Christian T1 - 29Si{27Al}, 27Al{29Si} and 27Al{1H} double-resonance NMR spectroscopy study of cementitious sodium aluminosilicate gels (geopolymers) and gel-zeolite composites N2 - The influence of starting materials and synthesis route on the properties and the structure of cementitious sodium aluminosilicate gels is not fully understood, partly due their amorphous nature and the fact that they often contain residual reactants, which can make the results of single-pulse NMR spectroscopy applied to these materials difficult to interpret or ambiguous. To overcome some of these limitations, 29Si{27Al} TRAPDOR NMR as well as 27Al{29Si} and 27Al{1H} REDOR NMR spectroscopy were applied to materials synthesized by the one-part alkali-activation route from three different amorphous silica starting materials, including rice husk ash. The latter led to formation of a fully amorphous sodium aluminosilicate gel (geopolymer), while the materials produced from the other silicas contained amorphous phase and crystalline zeolites. Application of the double-resonance NMR methods allowed to identify hydrous alumina gel domains in the rice husk ash-based material as well as significantly differing amounts of residual silica in the three cured materials. Four-coordinated Al existed not only in the aluminosilicate gel framework but also in a water-rich chemical environment with only a small amount of Si in proximity, likely in the alumina gel or possibly present as extra-framework Al in the aluminosilicate gel. The results demonstrate how the employment of different silica starting materials determines the phase assemblage of one-part alkali-activated materials, which in turn influences their engineering properties such as the resistance against chemically/biologically aggressive media. KW - Alkali-activated materials KW - Solid-state NMR KW - Aluminium hydroxide KW - Rice husk ash PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-469353 DO - https://doi.org/10.1039/C8RA09246J SN - 2046-2069 VL - 8 IS - 70 SP - 40164 EP - 40171 PB - Royal Society of Chemistry (RSC) CY - London AN - OPUS4-46935 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Henning, Ricky A1 - Sturm, Patrick A1 - Geddes, D.A. A1 - Keßler, S. A1 - Walkley, B. A1 - Gluth, Gregor T1 - The influence of curing temperature on the strength and phase assemblage of hybrid cements based on GGBFS/FA blends N2 - Hybrid cements are composites made of Portland cement or Portland clinker and one or more supplementary cementitious materials like slag, fly ash or metakaolin, activated with an alkali salt. To date, their hydration mechanism and the phase formation at various temperatures is insufficiently understood, partly due to the large variability of the raw materials used. In the present study, three hybrid cements based on ground granulated blast furnace slag, fly ash, Portland clinker and sodium sulfate, and an alkali-activated slag/fly ash blend were cured at 10 and 21.5°C, and subsequently analyzed by XRD, 27Al MAS NMR, and TGA. The compressive strength of the hybrid cements was higher by up to 27% after 91-day curing at 10°C, compared to curing at 21.5°C. The experimental results as well as thermodynamic modeling indicate that the differences in compressive strength were related to a different phase assemblage, mainly differing amounts of strätlingite and C-N-A-S-H, and the associated differences of the volume of hydration products. While the strätlingite was amorphous to X-rays, it could be identified by 27Al MAS NMR spectroscopy, TGA and thermodynamic modeling. The microstructural properties of the hybrid cements and the alkali-activated slag/fly ash blend as well as the compatibility between thermodynamic modeling results and experimental data as a function of curing temperature and time are discussed. KW - Hybrid cements KW - Strätlingite KW - Thermodynamic modelling KW - Hydration PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-557767 DO - https://doi.org/10.3389/fmats.2022.982568 SN - 2296-8016 VL - 9 SP - 1 EP - 16 PB - Frontiers AN - OPUS4-55776 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Henning, Ricky A1 - Sturm, Patrick A1 - Keßler, S. A1 - Gluth, Gregor ED - Lothenbach, B. ED - Wieland, E. ED - Altmaier, M. T1 - Influence of salt aggregate on the degradation of hybrid alkaline cement (HAC) concretes in magnesium chloride-rich saline solution simulating evaporite rock N2 - Concretes produced from salt aggregate and hybrid alkaline cements, an alkali-activated slag/fly ash blend, or a Portland cement were exposed to a magnesium chloride-rich saline solution ([Mg2+] = 3.6 m, [Cl−] = 8.3 m), representing a solution formed after contact of surface water with evaporite rock (rock salt) in a nuclear waste repository. The hydration and deterioration of the concretes were studied with X-ray diffraction, thermogravimetric analysis, pH mapping and permeability measurements. The results show that calcium silicate hydrate (C-S-H) or sodium-substituted calcium aluminium silicate hydrate (C-N-A-S-H) and Friedel's salt were the major reaction products in the concretes prior to exposure to the saline solution. During exposure to the saline solution, increasing amounts of C-S-H/C-N-A-S-H dissolved, and gypsum and a secondary AFm phase formed. The durability of the concretes improved with increasing amounts of Portland clinker in the cements, due to the associated differences in permeability and chemical resistance. Nevertheless, a massive increase of permeability occurred for all concretes, likely caused by crack formation due to the formation of gypsum from anhydrite in the salt aggregate. Thus, the behavior of the concretes differed from, and was more complex than, the behavior of plain cement pastes. T2 - Joint 6th International Workshop on Mechanisms and Modelling of Waste/Cement Interactions (JCCW 2023) CY - Prague, Czech Republic DA - 20.11.2023 KW - Nuclear waste repository KW - Evaporite rock KW - Magnesium chloride brine KW - Concrete KW - Hybrid alkaline cement PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599928 DO - https://doi.org/10.1016/j.apgeochem.2024.106027 SN - 0883-2927 SN - 1872-9134 VL - 168 SP - 1 EP - 14 PB - Elsevier AN - OPUS4-59992 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Johann, Sergej A1 - Baensch, Franziska A1 - Sturm, Patrick A1 - Tiebe, Carlo A1 - Pötschke, Samuel A1 - Lay, Vera ED - Holl, H. T1 - HF RFID-based measurement comparison for method optimization in M2 concrete and alkali-activated mortars N2 - Monitoring of repositories for radioactive waste requires techniques which can be applied long-term under harsh conditions. In this work, the reliability and suitability of materials and a capacitive sensor for measuring relative humidity are investigated, which are to be embedded in the special concrete components for the closure structures of underground repository. Preliminary tests with accelerated aging of the materials used, validation of the sensors under difficult conditions, investigations of the surfaces after aging by pH 14 solution, defined exposure of the sensors in a climatic chamber and the microscope images are discussed. The results will be used for further development and optimization of the RFID based sensor systems which can be applied to monitor the condition of different building structures without cabling. T2 - 37th Danubia - Adria Symposium on Advances in Experimental Mechanics CY - Linz, Austria DA - 21.09.2021 KW - Alkali-activated mortars KW - Passive sensor interface KW - RFID KW - Structural health monitoring KW - Smart structures PY - 2022 DO - https://doi.org/10.1016/j.matpr.2022.03.465 SN - 2214-7853 VL - 62 IS - 5 SP - 2571 EP - 2576 PB - Elsevier CY - Amsterdam AN - OPUS4-54697 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sturm, Patrick A1 - Moye, J. A1 - Gluth, Gregor A1 - Vogler, Nico A1 - Taffe, A. A1 - Kühne, Hans-Carsten ED - Rossignol, S. ED - Gluth, Gregor T1 - Properties of alkali-activated mortars with salt aggregate for sealing structures in evaporite rock N2 - Concrete structures for sealing of tunnels in the host rock are an essential part of systems for nuclear waste storage. However, concretes based on blended cements or magnesium oxychloride cements, which are commonly considered for this application, can deteriorate severely due to a significant heat of hydration and associated deformation and cracking. Alkali-activated materials (AAMs) offer a potential solution to this problem because of their low heat release during hardening. To explore their suitability for the construction of sealing structures in evaporite rock, various AAMs with salt aggregate were studied regarding fresh properties, heat release, mechanical properties and microstructure. The heat of reaction of the AAMs was up to 55% lower than that of a blended cement designed for sealing structures, indicating significant benefits for the intended application. Other relevant properties such as mechanical strength and permeability depended strongly on the mix-design of the AAMs and curing conditions. KW - Alkali-activated materials KW - Geopolymers KW - Nuclear waste storage KW - Sealing structures KW - Evaporite rock PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519422 DO - https://doi.org/10.1016/j.oceram.2020.100041 SN - 2666-5395 VL - 5 IS - Special issue: Alkali-activated materials and geopolymers in ceramics and beyond SP - 1 EP - 8 PB - Elsevier CY - Amsterdam AN - OPUS4-51942 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kazlagić, Anera A1 - Russo, Francesco A1 - Vogl, Jochen A1 - Sturm, Patrick A1 - Stephan, D. A1 - Gluth, Gregor ED - Resch-Genger, Ute ED - Koch, Matthias ED - Meermann, Björn ED - Weller, Michael G. T1 - Development of a sample preparation procedure for Sr isotope analysis of Portland cements N2 - The 87Sr/86Sr isotope ratio can, in principle, be used for provenancing of cement. However, while commercial cements consist of multiple components, no detailed investigation into their individual 87Sr/86Sr isotope ratios or their influence on the integral 87Sr/86Sr isotope ratio of the resulting cement was conducted previously. Therefore, the present study aimed at determining and comparing the conventional 87Sr/86Sr isotope ratios of a diverse set of Portland cements and their corresponding Portland clinkers, the major component of these cements. Two approaches to remove the additives from the cements, i.e. to measure the conventional 87Sr/86Sr isotopic fingerprint of the clinker only, were tested, namely, treatment with a potassium hydroxide/sucrose solution and sieving on a 11-µm sieve. Dissolution in concentrated hydrochloric acid/nitric acid and in diluted nitric acid was employed to determine the 87Sr/86Sr isotope ratios of the cements and the individual clinkers. The aim was to find the most appropriate sample preparation procedure for cement provenancing, and the selection was realised by comparing the 87Sr/86Sr isotope ratios of differently treated cements with those of the corresponding clinkers. None of the methods to separate the clinkers from the cements proved to be satisfactory. However, it was found that the 87Sr/86Sr isotope ratios of clinker and cement generally corresponded, meaning that the latter can be used as a proxy for the clinker 87Sr/86Sr isotope ratio. Finally, the concentrated hydrochloric acid/nitric acid dissolution method was found to be the most suitable sample preparation method for the cements; it is thus recommended for 87Sr/86Sr isotope analyses for cement provenancing. KW - Cement KW - Provenancing KW - Sr isotopes KW - Portland clinker KW - Dissolution PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-542239 DO - https://doi.org/10.1007/s00216-021-03821-7 SN - 1618-2642 SN - 1618-2650 VL - 414 IS - 15 (Topical collection: Analytical methods and applications in the materials and life sciences) SP - 4379 EP - 4389 PB - Springer CY - Berlin AN - OPUS4-54223 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -