TY - JOUR A1 - Artinov, Antoni A1 - Bakir, Nasim A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Weld pool shape observation in high power laser beam welding N2 - The geometry of the melt pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. In this study, a butt configuration of 15 mm thick structural steel and transparent quartz glass was used to observe the weld pool geometry by means of high-speed camera and an infrared camera recording. The observations show that the dimensions of the weld pool vary depending on the depth. The areas close to the weld pool surface take a teardrop-shape. A bulge-region and its temporal evolution were observed approximately in the middle of the depth of the weld pool. Additionally, a 3D transient thermal-fluid numerical simulation was performed to obtain the weld pool shape and to understand the formation mechanism of the observed bulging effect. The model takes into account the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties up to evaporation temperature. The numerical results showed good accordance and were furthermore used to improve the understanding of the experimentally observed bulging effect. T2 - LANE Conference 2018 CY - Fürth, Germany DA - 03.09.2018 KW - High power laser beam welding KW - Weld pool shape KW - Bulging KW - Numerical process simulation PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-458759 DO - https://doi.org/10.1016/j.procir.2018.08.043 SN - 2212-8271 VL - 74 SP - 683 EP - 686 PB - Elsevier Ltd. CY - Amsterdam [u.a.] AN - OPUS4-45875 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Pavlov, V. A1 - Zavjalov, S. A1 - Volvenko, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Novel metrology to determine the critical strain conditions required for solidification cracking during laser welding of thin sheets N2 - This paper represents the results for proposed optical flow method based on the Lucas-Kanade (LK) algorithm applied to two different problems. The following observations can be made: - The estimated strain and displacement for conducted tensile test are generally very close to those measured with conventional DIC-technique. - The LK technique allows measurement of strain or displacement without special selection of a region of interest. Using a novel optical measurement technique together with the optical flow algorithm, a twodimensional deformation analysis during welding was conducted. This technique is the first to provide a measurement of the full strain field locally in the immediate vicinity of the solidification front. Additionally, the described procedure of the optical measurement allows the real material-dependent values of critical strain characterizing the transition to hot cracking during laser welding processes to be determined. T2 - Beam Technologies and Laser Application CY - Sankt Petersburg, Russia KW - Hot cracking test KW - Local critical strain KW - Solidification cracking KW - Laser beam welding KW - Novel metrology PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-467226 DO - https://doi.org/10.1088/1742-6596/1109/1/012047 SN - 1742-6596 VL - 1109 IS - 012047 SP - 1 EP - 9 PB - IOP Publ. CY - Bristol AN - OPUS4-46722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Pavlov, V. A1 - Volvenko, S. A1 - Rethmeier, Michael T1 - In situ determination of the critical straining condition for solidification cracking during laser beam welding N2 - A self-restraint hot cracking test (free edge test) was used in combination with a novel optical measurement technique to determine the critical straining conditions for solidification cracking for the stainless steel grade 1.4828 (AISI 309). The Lucas-Kanade algorithm for the optical flow (OF) calculation was implemented to obtain the full-field displacement and then the full-field strain. The use of external laser illumination with appropriate filters allows to obtain good image quality with good contrast. The critical straining conditions required for solidification cracking can be obtained by means the proposed technique in the immediate vicinity of the solidification front. A very good repeatability was demonstrated for the used measurement technique. The critical straining conditions for solidification cracking for the tested steel und under this welding conditions has been detected KW - Laser beam welding KW - Solidification cracking KW - Critical strain KW - Critical strain rate KW - Optical flow PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513070 DO - https://doi.org/10.1016/j.procir.2020.09.104 SN - 2212-8271 VL - 94 SP - 666 EP - 670 PB - Elsevier AN - OPUS4-51307 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - The bulging effect and its relevance in high power laser beam welding N2 - The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and an infrared camera is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs more frequently during partial penetration above 6 mm and complete penetration above 8 mm penetration depth, respectively. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root. T2 - 18th Nordic Laser Materials Processing Conference (18th NOLAMP) KW - High-power laser beam welding KW - Bulge effect KW - Solidification cracking KW - Multi-physical modelling KW - Metal mixing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539149 DO - https://doi.org/10.1088/1757-899X/1135/1/012003 VL - 1135 IS - 012003 SP - 1 EP - 11 PB - IOP Publishing AN - OPUS4-53914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of an external applied AC magnetic field on the melt pool dynamics at high-power laser beam welding N2 - The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets. T2 - 18th Nordic Laser Materials Processing Conference (18th NOLAMP) KW - Laser beam welding KW - AC magnetic field KW - Melt pool dynamics KW - Filler wire mixing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539231 DO - https://doi.org/10.1088/1757-899X/1135/1/012017 VL - 1135 IS - 012017 SP - 1 EP - 10 PB - IOP Publishing AN - OPUS4-53923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application» KW - Laser hybrid welding KW - Magnetic bath support KW - Plasma-cut samples KW - Thick plate welding PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539248 DO - https://doi.org/10.1088/1742-6596/2077/1/012007 VL - 2077 IS - 012007 SP - 1 EP - 8 PB - IOP Publishing AN - OPUS4-53924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of the weld pool geometry on solidification cracking in partial penetration high power laser beam welding N2 - Solidification cracking is still a serious problem in laser beam welding, especially in the welding of thick-walled plates. The influence of weld pool geometry on solidification cracking in partial penetration welding of thick plates is investigated within scope of this study. Therefore, a specific experimental setup of steel and quartz glass in butt configuration and on the side with high-speed camera were used to record the weld pool shape. In addition, the influence of laser inclination angle on the weld pool geometry and on solidification crack formation was investigated. The results show a bulge in the weld pool root, which is separated from an upper region by a necking region. This leads to a case where there are three different longitudinal region lengths with different solidification zones. This temporal sequence of solidification strongly promotes the formation of solidification cracks in the weld root. T2 - 12th CIRP Conference on photonic technologies (LANE 2022) CY - Fürth, Germany DA - 04.09.2022 KW - Laser beam welding KW - Partial penetration KW - Weld pool shape PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563940 DO - https://doi.org/10.1016/j.procir.2022.08.174 VL - 111 SP - 397 EP - 400 PB - Elsevier B.V. AN - OPUS4-56394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Improvement of Charpy impact toughness by using an AC magnet backing system for laser hybrid welding of thick S690QL steels N2 - The study deals with the influence of the heat input and the resulting cooling times on the microstructure and Charpy impact toughness of single-pass laser hybrid welded 20-mm thick high-strength steel S690QL. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured in-situ using a pyrometer and an optical fibre in three different depths of the seam where Charpy impact test specimens were also later taken. Thereby, three different heat inputs from 1.3 kJ/mm to 2 kJ/mm were investigated. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required impact toughness of 38 J/cm2 could be reached in dependance on applied heat input, especially at the heat input of 1.6 kJ/mm. T2 - 12th CIRP conference on photonic technologies [lane 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Thick-plate welding KW - Laser hybrid welding KW - Electromagnetic backing KW - Charpy impact toughness KW - Thermal cycles PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563731 DO - https://doi.org/10.1016/j.procir.2022.08.067 VL - 111 SP - 462 EP - 465 PB - Elsevier B.V. AN - OPUS4-56373 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Huo, W. A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Wolter, K. T1 - Strain Prediction Using Deep Learning during Solidification Crack Initiation and Growth in Laser Beam Welding of Thin Metal Sheets N2 - The strain field can reflect the initiation time of solidification cracks during the welding process. The traditional strain measurement is to first obtain the displacement field through digital image correlation (DIC) or optical flow and then calculate the strain field. The main disadvantage is that the calculation takes a long time, limiting its suitability to real-time applications. Recently, convolutional neural networks (CNNs) have made impressive achievements in computer vision. To build a good prediction model, the network structure and dataset are two key factors. In this paper, we first create the training and test sets containing welding cracks using the controlled tensile weldability (CTW) test and obtain the real strain fields through the Lucas–Kanade algorithm. Then, two new networks using ResNet and DenseNet as encoders are developed for strain prediction, called StrainNetR and StrainNetD. The results show that the average endpoint error (AEE) of the two networks on our test set is about 0.04, close to the real strain value. The computation time could be reduced to the millisecond level, which would greatly improve efficiency. KW - Convolutional neural network KW - Strain fields prediction KW - Laser beam welding KW - Solidification cracking PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-570565 DO - https://doi.org/10.3390/app13052930 VL - 13 IS - 5 SP - 1 EP - 15 PB - MDPI AN - OPUS4-57056 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Huo, Wenjie A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Wolter, Katinka T1 - Detection of solidification crack formation in laser beam welding videos of sheet metal using neural networks N2 - AbstractLaser beam welding has become widely applied in many industrial fields in recent years. Solidification cracks remain one of the most common welding faults that can prevent a safe welded joint. In civil engineering, convolutional neural networks (CNNs) have been successfully used to detect cracks in roads and buildings by analysing images of the constructed objects. These cracks are found in static objects, whereas the generation of a welding crack is a dynamic process. Detecting the formation of cracks as early as possible is greatly important to ensure high welding quality. In this study, two end-to-end models based on long short-term memory and three-dimensional convolutional networks (3D-CNN) are proposed for automatic crack formation detection. To achieve maximum accuracy with minimal computational complexity, we progressively modify the model to find the optimal structure. The controlled tensile weldability test is conducted to generate long videos used for training and testing. The performance of the proposed models is compared with the classical neural network ResNet-18, which has been proven to be a good transfer learning model for crack detection. The results show that our models can detect the start time of crack formation earlier, while ResNet-18 only detects cracks during the propagation stage. KW - Artificial Intelligence KW - Software PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586116 DO - https://doi.org/10.1007/s00521-023-09004-y SN - 0941-0643 VL - 35 IS - 34 SP - 24315 EP - 24332 PB - Springer Science and Business Media LLC AN - OPUS4-58611 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hartwig, Philipp A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Scheunemann, Lisa A1 - Schröder, Jörg A1 - Rethmeier, Michael T1 - A Physically Motivated Heat Source Model for Laser Beam Welding N2 - In this contribution, we present a physically motivated heat source model for the numerical modeling of laser beam welding processes. Since the calibration of existing heat source models, such as the conic or Goldak model, is difficult, the representation of the heat source using so-called Lamé curves has been established, relying on prior Computational Fluid Dynamics (CFD) simulations. Lamé curves, which describe the melting isotherm, are used in a subsequent finite-element (FE) simulation to define a moving Dirichlet boundary condition, which prescribes a constant temperature in the melt pool. As an alternative to this approach, we developed a physically motivated heat source model, which prescribes the heat input as a body load directly. The new model also relies on prior CFD simulations to identify the melting isotherm. We demonstrate numerical results of the new heat source model on boundary-value problems from the field of laser beam welding and compare it with the prior CFD simulation and the results of the Lamé curve model and experimental data. KW - Welding simulation KW - Heat source models KW - Laser beam welding KW - Thermal analysis PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-600899 DO - https://doi.org/10.3390/met14040430 VL - 14 IS - 4 SP - 1 EP - 26 PB - MDPI CY - Basel AN - OPUS4-60089 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Karkhin, V. A1 - Bakir, Nasim A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Lamé curve approximation for the assessment of the 3D temperature distribution in keyhole mode welding processes N2 - A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby, the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection, and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature. The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g., the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments. KW - Lamé curves approximation KW - Equivalent heat source KW - Thermal cycles KW - Numerical modeling KW - Keyhole mode welding PY - 2020 DO - https://doi.org/10.2351/7.0000076 VL - 32 IS - 2 SP - 022042-1 EP - 022042-8 PB - AIP Publishing AN - OPUS4-50768 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Determination of critical local straining conditions for solidification cracking at laser beam welding by experimental and numerical methods N2 - AbstractThe phenomenon of solidification cracking has been the subject of numerous research projects over the years. Great efforts have been made to understand the fundamentals of hot cracking. It is generally agreed that solidification cracks form in the solidification range between the liquidus and solidus temperatures under the combination of thermal, metallurgical and mechanical factors. There is still a need to determine the time‐resolved strain distribution in the crack‐sensitive region in order to analyse the local critical conditions for solidification cracking phenomena. This was a strong motivation for the development of a measurement system used in this study to estimate the local strains and strain rates in the zone where the solidification crack is expected to occur. The laser beam welding experiments were conducted using the Controlled‐Tensile‐Weldability test (CTW test) to apply an external strain condition during welding to generate solidification cracks. The CTW test is a test method for investigating the susceptibility of laser‐welded joints to solidification cracking, in which the sample can be subjected to a defined strain at a defined strain rate during welding.In combination with experimental investigations, numerical simulations provide spatially detailed and time‐dependent information about the strain development during the welding process, especially regarding the critical conditions for solidification cracking. Therefore, this tool was also used in the present study to evaluate the accuracy of measurement methods and to estimate experimentally derived values and their concrete influence on the formation of solidification cracks. By integrating experimental methods and numerical simulations, this study investigates the spatially resolved and temporally changing development of strain during welding, with a particular focus on the critical conditions that lead to the formation of solidification cracks. The use of numerical simulations serves a dual purpose by validating the accuracy of measurement methods and examining experimentally determined values for their actual influence on the formation of solidification cracks. A three‐dimensional finite element (FE) model implemented with ANSYS is used to simulate strains and stresses during welding. The credibility of the model was first established by validation using experimental temperature measurements. Subsequently, structural simulations were carried out under external load. The results of the simulations showed commendable agreement with the strain measurements performed using the developed technique. KW - Laser beam welding KW - Solidification cracking KW - FEM simulation PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-612044 DO - https://doi.org/10.1002/pamm.202400020 SN - 1617-7061 VL - 24 IS - 2 SP - 1 EP - 16 PB - Wiley AN - OPUS4-61204 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gumenyuk, Andrey A1 - Üstündağ, Ömer A1 - Pelz, Till A1 - Bakir, Nasim A1 - Gerhards, Benjamin A1 - Schleser, Markus A1 - Rethmeier, Michael T1 - Single pass laser vacuum welding of thick steel plates using electromagnetic support N2 - The increasing demand for renewable energy produced by offshore wind turbines goes along with an increased demand in the production of offshore wind turbine foundations, so called “monopiles”, which are made by joining thick metal sheets. The industrial standard of multi-layer submerged arc welding (SAW) for joining of thick metal sheets is the current bottleneck in the production of monopiles. A possible increase in productivity by the implementation of high-power laser welding in a newly developed mobile vacuum chamber (MoVac) and an electromagnetic root support is the subject of this study. Single run butt welds are performed in flat position on S355 mild steel of thicknesses up to 80 mm using a disc laser system with 1030 nm wavelength and a maximum output of 60 kW. The laser optic is fixed on the MoVac-System which is held and manipulated by an articulated robot. KW - Laser beam welding KW - Laser welding with mobile vacuum PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-612068 DO - https://doi.org/10.1016/j.procir.2024.08.145 VL - 124 SP - 418 EP - 423 PB - Elsevier BV AN - OPUS4-61206 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gumenyuk, Andrey A1 - Bakir, Nasim A1 - Rethmeier, Michael T1 - Two-colour thermography for measurement of temperature distribution in laser beam welding N2 - Solidification cracking is a frequently observed phenomenon in laser beam welding of austenitic stainless steels and other metallic alloys. Characterisation of cracking susceptibility requires knowledge of the precise and spatially resolved temperature distribution near the solidification front in the welding process. Thermography is a standard tool that provides a qualitative estimate of the 2D temperature field. The general disadvantage of this method is its dependence on the emission characteristics of the measured object. For welding applications, these can vary significantly in the temperature range above and below the melting temperature. For this purpose, we have developed a thermography-based measurement technique using a SWIR camera system in combination with two narrow bandpass filters that use the principle of two-wavelength pyrometry to estimate absolute temperature values. This technique was used to determine the temperature distributions and gradients near the solidification front of laser-welded austenitic steel. The results were validated by other measurements. KW - Laser beam welding KW - Two-colour thermography KW - Solidification cracking PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-612070 DO - https://doi.org/10.1016/j.procir.2024.08.155 VL - 124 SP - 468 EP - 471 PB - Elsevier BV AN - OPUS4-61207 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Akyel, Fatma A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, Christian A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of heat input on cooling rates and mechanical properties of laser hybrid welded thick structural steels N2 - Laser hybrid welding presents several challenges when used to weld thick steels. A typical weld is divided into the arcdominated and laser-dominated zone. These zones lead to variations in the mechanical properties of the weld. The laserdominated zone is of particular importance regarding mechanical properties, notably Charpy impact toughness, due to the high cooling rates and the absence of filler wire. The low heat input of the laser can lead to martensitic microstructure causing hardening and deterioration of impact toughness. The high heat input of the arc can lead to grain coarsening and even loss of impact toughness. This study examines the influence of heat input on the cooling rates, microstructure and mechanical properties of single-pass laser hybrid welded steels of S355J2 and EH36 with thicknesses up to 30 mm. The experiments were performed with a 20-kW fibre laser and a contactless electromagnetic weld backing in the butt-joint configuration in 1G welding position. The cooling time was measured in three different locations near the fusion lines corresponding to different heights of the seam using a special configuration with pyrometers, collimators and optical fibres. The test specimens for the Charpy impact testing and tensile testing were extracted in three different depths. The experiments indicated that a heat input of 1.6 kJ/mm–2 kJ/mm, 2 kJ/mm–2.4 kJ/mm and 3.7 kJ/mm were recommended when single-pass laser hybrid welding of 20-, 25-, and 30-mm-thick structural steels regarding the minimum requirements of the mechanical properties, respectively. KW - Laser hybrid welding KW - Heat input KW - Mechanical properties KW - Charpy impact toughness KW - Cooling rate PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625282 DO - https://doi.org/10.1007/s40194-025-01924-8 SN - 1878-6669 SP - 1 EP - 15 PB - Springer CY - United Kingdom AN - OPUS4-62528 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of solidification cracking susceptibility of laser welded joints of austenitic stainless steels N2 - Laser welding is a widely established manufacturing process in many industry sectors. Solidification cracking represents one of the most inadequately solved problems in welding and has major economic implications. The avoidance of hot crack forms for most fusion welding processes poses a key challenge for an important range of metallic construction materials and affects not only the manufacturers of welding equipment and material manufacturers, but also a large number of customers using welding technologies, as well as welding technical standardization and research. Solidification cracking susceptibility was examined with the help of the Controlled Tensile Weldability Test (CTW) developed by Federal Institute for Materials Research and Testing (BAM), Berlin. The test is based on the fact that hot crack formation depends on a critical strain that emerges within a critical temperature range, the so called brittle temperature range (BTR). Using this test and defined investigation programme a centreline solidification crack was generated. By controlling the applied strain during the laser beam welding process, it was possible to determine the critical strain and strain rate that led to solidification cracking formation. The hot cracking susceptibility of the tested stainless steels was qualified and quantified. The results demonstrate that the crack length increases with increasing applied strain. Furthermore, the strain rate has a significant influence on the formation of the solidification crack. T2 - 3rd International conference in Africa and Asia CY - Luxor, Egypt DA - 02.11.2015 KW - Laser beam welding KW - Hot cracking KW - Solidification cracking KW - Hot cracking test PY - 2015 SP - A-29, 1 EP - A-29, 9 AN - OPUS4-36522 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Anwendung der digitalen Bildkorrelationstechnik zur Untersuchung der Heißrissanfälligkeit laserstrahlgeschweißter Verbindungen mit dem CTW-Test N2 - In dieser Studie wurde die Heißrissanfälligkeit beim Laserstrahlschweißen für die Werkstoffe 1.4376, 1.4301 und 1.4828 mit Hilfe des CTW­ Test quantifiziert. Bei den Versuchen konnten Erstarrungsrisse in den Proben generiert werden. Zusätzlich können mit der Bildkorrelations-Technik die lokalen Dehnungen und Dehnungs­raten während des Heißrisstests gemessen wer­ den. In Verbindung mit einem externen Dioden­laser zum Beleuchten der zu messende Oberflä­che und lnterferenzfiltern an den Kameras konn­ten die DIC Messungen ohne optische Störungen durchgeführt werden. Die Ergebnisse zeigen, dass die Heißrissbildung bei einer externen Belastung von 3 % für die Stahlsorte 1.4376 zu erwarten ist. Für die Stahls­ orte 1.4301 beträgt dieser Grenzwert 2 % und 1,5 % für die Stahlgüte 1.4828. Außerdem ist zu beobachten, dass die Gesamtrisslänge mit zu­ nehmender äußerer Zugbeanspruchung steigt T2 - 35. Assistentenseminar Füge- und Schweißtechnik CY - Institut für Werkstoff- und Fügetechnik der Otto-von­ Guericke-Universität Magdeburg DA - 01.12.2014 KW - Digitale Bildkorrelationstechnik KW - Heißrissanfälligkeit KW - Untersuchung laserstrahlgeschweißter Verbindungen KW - CTW-Test PY - 2016 SN - 978-3-945023-55-6 VL - 2016/34 SP - 50 EP - 54 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-38065 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Wieland, H.-J. ED - Brockmann, S. T1 - Investigation of solidification cracking susceptibility in laser welded H400 austenitic stainless steel using digital image correlation technique N2 - One trend in today’s structural design for automobiles is towards application of stainless Steel in addition to traditional carbon Steel. This is mainly due to the advantages offered by stainless steel to the designer, i.e. its high corrosion resistance, heat resistance, strength and formability. Welding of austenitic stainless steel involves a high risk of solidification cracking due to low melting eutectics containing different kinds of impurities and to accumulated strain behind the weld pooi in the mushy zone. As a result, the quality of stainless steel welded joints will greatly be affected which may give cause for safety concerns. The intention of this study was to investigate the hot cracking sensitivity of laser welded fully austenitic stainless steels and to determine the critical local strain and strain rate from the formation of solidification cracks. C02-laser welding experiments were conducted using the steel X8CrMnNi19-6-3 (Nirosta H400). Solidification cracking susceptibility was examined with the help of the Controlled Tensile Weldability (CTW) Test developed by BAM Federal Institute for Materials Research and Testing in Berlin. The critical strain and strain rate of solidification cracking was measured at the surface of the workpiece directed to the laser beam in the close vicinity of the weld pool by using the Digital Image Correlation (DIC) technique and diode laser as the illuminating source. T2 - SCT2014 - 4th International conference on steels in cars and trucks CY - Braunschweig, Germany DA - 15.06.2014 KW - Hot cracking KW - Stainless steels KW - Critical strains KW - Strain rates KW - Hot cracking test KW - CTW test KW - Digital image correlation PY - 2014 SN - 978-3-514-00813-7 SP - 299 EP - 307 PB - Verl. Stahleisen GmbH CY - Düsseldorf AN - OPUS4-31166 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Experimental and numerical study on the influence of the laser hybrid parameters in partial penetration welding on the solidification cracking in the weld root N2 - In this study, the influence of the welding speed, the arc power, and the laser focal position on the solidification crack formation for partial penetration laser hybrid–welded thick-walled plates was investigated. The solidification cracking in the weld root is a result of interaction between metallurgical and geometrical and thermomechanical factors. Experimentally, a direct correlation between the welding speed and the crack number was observed. That is by reducing the welding velocity, the crack number was decreased. The focal position shows also a significant influence on the crack number. By focusing the laser on the specimen surface, the crack number has been significantly diminished. The wire feed speed showed a very slight influence on the crack formation. That is due to the large distance between the critical region for cracking and the arc region. The numerical model shows a high stress concentration in the weld root for both components (vertical and transversal). Numerically, the reduced welding speed showed a strong impact on stress, as the model demonstrated a lower stress amount by decreasing the welding speed. The metallurgical factors, such as the assumed accumulation of the low-melting eutectics in the weld root, should be a contribution for solidification cracking, where the tensile stress is acting. KW - Laser hybrid welding KW - Solidification cracking KW - Partial penetration welding KW - Weld root KW - Numerical simulation PY - 2020 DO - https://doi.org/10.1007/s40194-020-00847-w VL - 64 SP - 501 EP - 511 PB - Springer AN - OPUS4-50625 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -