TY - JOUR A1 - Buzolin, R. H. A1 - Richter, Tim A1 - Pixner, F. A1 - Rhode, Michael A1 - Schröpfer, Dirk A1 - Enzinger, N. T1 - Microstructure characterisation of multi-principal element alloys welds produced by electron beam welding N2 - This work explores the feasibility of producing bead-on-plate welds of a CrCoNi medium entropy alloy and a CrMnFeCoNi high entropy alloy using electron beam welding. The alloys were welded in two states: one in an as-cold-rolled condition and the other in an annealed condition. In addition, the materials are welded with two different parameters. The FCC microstructure of the welds is investigated using scanning electron microscopy assisted by energy-dispersive X-ray spectroscopy and electron-backscattered diffraction. The impact of the weld on the microstructure is discussed. The heat-affected zone is negligible for the annealed condition of both medium and high entropy alloys since there is no driving force for recrystallisation and the exposure time to high temperature is insufficient for grain coarsening. The texture formed in the fusion zone is also discussed and compared to the texture in the base metal and the heat-affected zone. Although the grain growth along the (100) crystallographic direction is preferential in all cases, the crystallographic texture type differs from each weld. Higher hardness values are measured in the medium entropy alloy’s base metal and fusion zone than in the high entropy alloy. KW - Multi-principal element alloy KW - Electron backscattered diffraction KW - Electron beam welding KW - High-entropy alloy KW - Microstructure characterization PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-568129 DO - https://doi.org/10.1016/j.matdes.2023.111609 SN - 1873-4197 VL - 225 SP - 1 EP - 14 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-56812 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Buzolin, R.H. A1 - Richter, Tim A1 - Pixner, F. A1 - Rhode, Michael A1 - Schröpfer, Dirk A1 - Enzinger, N. T1 - Microstructure and texture characterisation of friction stir welded CoCrNi and CoCrFeMnNi multi-principle element alloys N2 - This work investigates the microstructure formed in friction stir welds of FCC alloys, focused on two multiprincipal alloys: a CoCrFeMnNi high-entropy alloy (HEA) and a CoCrNi medium-entropy alloy (MEA). A commercial stainless steel AISI 304 is used for comparison. The largest nugget was formed in the MEA, while the smallest was formed in the HEA. Grain refinement occurs in the stirred zone in all welds. Discontinuous dynamic recrystallisation is the predominant restoration mechanism during friction stir welding of the three investigated alloys. A sharp decrement in the Σ3 boundary fraction occurs in the stirred zone of the AISI 304 and HEA welds, while comparable values with the base metal are found for the MEA weld. The peak in the maximum index of crystallographic texture is observed on the advancing side of the stirred zone of the AISI 304 weld. A strong <001> θ-fibre texture is formed in the advancing side of the nugget in the AISI 304 from a well-established {123} <634> S-type texture in the base metal. Multiple crystallographic texture components without specific fibres are identified in most regions of the welds, indicating the complex shear path history during friction stir welding. KW - Microstructure KW - Multiple principal element alloy KW - Friction stir welding KW - Electron backscattered diffraction KW - Crystallographic texture PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-572987 DO - https://doi.org/10.1016/j.mtcomm.2023.105870 VL - 35 SP - 1 EP - 14 PB - Elsevier Ltd. CY - Amsterdam (NL) AN - OPUS4-57298 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Böllinghaus, Thomas A1 - Steffens, B. R. A1 - Rhode, Michael A1 - Shoales, G.A. T1 - Hydrogen Assisted Stress Corrosion Cracking Related Material Properties of ServiceApplied Landing Gear Ultra-High Strength Steels N2 - Aircraft main landing gear (MLG) components are commonly manufactured from low-alloyed, martensitic, ultra-high strength steels (UHSS) that have to be coated for corrosion protection, representing an expensive and environmentally harmful production step. To avoid already partly banned corrosion protection plating, the new high-alloyed UHSS, Ferrium S53 (UNS S10500), has been designed to replace lowalloyed legacy materials and has been subjected to a limited field test over five years. As with the legacy alloys, UNS S10500 has a fully hardened martensitic microstructure known to be susceptible to hydrogen assisted cracking, per se. Containing about 10 wt% Cr, steels such as S10500 are at the lower limit for corrosion resistant alloys. Similar to super-martensitic stainless steels used in the oil and gas industry, a common failure sequence in marine environments represents pitting and subsequent hydrogen assisted stress corrosion cracking (HASCC). For addressing such phenomena quantitively, as required for respective lifetime assessments of MLG components and systems, the tolerance of such materials dependent on the absorbed hydrogen concentration must be evaluated quantitatively. However, there is a lack of such valuable materials data, as well as of the fractographic behavior dependent on the hydrogen concentration that might be absorbed during HASCC. To provide an improved understanding of the hydrogen dependent mechanical and fractographic behavior, samples of the legacy AISI 4340 and the new S10500 MLG steels have electrochemically been hydrogen-saturated and subjected to tensile testing. In contrast to a previous study, this contribution for the first time focuses on materials that have been salvaged from real service used landing gear components. In this study, it has been demonstrated that the service-applied S10500 steel has not only a higher strength, but also an improved ductility in comparison to the legacy AISI 4340 steel after similar service durations that provides a higher tolerance against hydrogen concentrations that might be absorbed during potential pitting and HASCC in marine environments. In addition, it has been found that the absorbed hydrogen concentration significantly affects the fracture behavior. Interestingly, hardening of the hydrogen charged low-alloyed AISI 4340 steel changes the fracture topography from trans- toward intergranular, while hardening of the S10500 steel turned the fracture topography from inter- to transgranular at respectively high hydrogen concentrations. KW - Hydrogen assisted stress corrosion cracking KW - Ultra-high strength steel KW - Martensite KW - Modeling KW - Hydrogen dependent mechanical properties PY - 2019 DO - https://doi.org/10.5006/3028 SN - 0010-9312 SN - 1938-159X VL - 75 IS - 5 SP - 513 EP - 524 PB - NACE International AN - OPUS4-49530 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Nietzke, Jonathan A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Investigation of stress relief crack susceptibility of CrMoV steels coarse grain HAZ via simulation of uniaxial stress conditions during PWHT N2 - Creep-resistant steels such as the 13CrMoV9-10, used in the construction of thick-walled pressure vessels, are most commonly submerged arc welded (SAW). These steels can develop stress relief cracks (SRC) if the mandatory post weld heat treatment (PWHT) is performed improperly. Current PWHT parameters, such as heating rate and holding time at a specific holding temperature, are based on both empirical experience and conventional free shrinking welding experiments to characterize the SRC-susceptibility of the weld. These cannot adequately depict the higher residual stresses caused by the structurally induced stiffness of the surrounding construction. This study discusses the development of a repeatable, precise, and time-efficient methodology to study the effects of different stress levels and heating rates on the SRC susceptibility of the coarse grain heat-affected zone (CGHAZ). For that purpose, samples were thermically treated to simulate a coarse grain heat-affected zone (CGHAZ) and subsequently exposed to representative levels of stress during the heating phase of a PWHT. The recorded stress and heating rate–dependent strains were mathematically analyzed via curve tracing/calculus to identify interdependent effects. This procedure facilitates the measurement of material characteristics such as carbide growth on grain boundaries at the µm-scale via an integrated value over the entire sample volume. The first and second derivatives show a slight, precipitate-dependent, increase in hardness of the sample, depending on the heating rate and applied stress. This new methodology generates an improved assessment of the SRC susceptibility of SAW microstructures of creep-resistant CrMoV steels. KW - Submerged arc welding KW - Creep-resistant steel KW - Stress relief cracking KW - Component-like test KW - Post weld heat treatment PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576007 DO - https://doi.org/10.1007/s40194-023-01539-x SN - 0043-2288 SP - 1 EP - 9 PB - Springer Nature CY - Basel (CH) AN - OPUS4-57600 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Delgado Arroyo, Diego A1 - Richter, Tim A1 - Schröpfer, Dirk A1 - Boerner, Andreas A1 - Rhode, Michael A1 - Lindner, T. A1 - Preuß, B. A1 - Lampke, T. T1 - Influence of Milling Conditions on AlxCoCrFeNiMoy Multi-Principal-Element Alloys N2 - Multi-Principal-Element or High-Entropy Alloys (MPEAs/HEAs) have gained increasing interest in the past two decades largely due to their outstanding properties such as superior mechanical strength and corrosion resistance. However, research studies on their processability are still scarce. This work assesses the effect of different machining conditions on the machinability of these novel alloys, with the objective of advancing the introduction of MPEA systems into industrial applications. The present study focuses on the experimental analysis of finish-milling conditions and their effects on the milling process and resulting surface finish of CoCrFeNi, Al0.3CoCrFeNi and Al0.3CoCrFeNiMo0.2 alloys fabricated via Spark Plasma Sintering. Ball-nose-end milling experiments have been carried out various milling parameters such as cutting speed, feed per cutting edge, and ultrasonic assistance. In situ measurements of cutting forces and temperature on the tool edge were performed during the experiments, and surface finish and tool wear were analyzed afterwards. The results exhibited decreasing cutting forces by means of low feed per cutting edge and reduced process temperatures at low cutting speed, with the use of ultrasonic-assisted milling. It was shown that the machinability of these modern alloys through conventional, as well as modern machining methods such as ultrasonic-assisted milling, is viable, and common theories in machining can be transferred to these novel MPEAs. KW - Multi-principal element alloys KW - Finish milling KW - Spark plasma sintering KW - Ultrasonic-assisted milling KW - Microstructure characterization PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-572990 DO - https://doi.org/10.3390/coatings13030662 VL - 13 IS - 3 SP - 1 EP - 18 PB - MDPI (Multidisciplinary Digital Publishing Institute) CY - Basel (CH) AN - OPUS4-57299 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A A1 - Konert, Florian A1 - Sobol, Oded A1 - Rhode, Michael A1 - Domitner, J A1 - Sommitsch, C A1 - Böllinghaus, Thomas T1 - Enhanced gaseous hydrogen solubility in ferritic and martensitic steels at low temperatures N2 - Metals that are exposed to high pressure hydrogen gas may undergo detrimental failure by embrittlement. Understanding the mechanisms and driving forces of hydrogen absorption on the surface of metals is crucial for avoiding hydrogen embrittlement. In this study, the effect of stress-enhanced gaseous hydrogen uptake in bulk metals is investigated in detail. For that purpose, a generalized form of Sievert's law is derived from thermodynamic potentials considering the effect of microstructural trapping sites and multiaxial stresses. This new equation is parametrized and verified using experimental data for carbon steels, which were charged under gaseous hydrogen atmosphere at pressures up to 1000 bar. The role of microstructural trapping sites on the parameter identification is critically discussed. KW - Hydrogen KW - Thermodynamic modelling KW - Pressure-dependent solubility KW - Steel KW - Trapping PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559307 DO - https://doi.org/10.1016/j.ijhydene.2022.09.109 SN - 0360-3199 VL - 47 IS - 93 SP - 39639 EP - 39653 PB - Elsevier Ltd. AN - OPUS4-55930 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A.-K. A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Hodžić, E. A1 - Pastore, S. A1 - Domitner, J. A1 - Rhode, Michael A1 - Sommitsch, C. A1 - Böllinghaus, Thomas T1 - Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure N2 - The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments. KW - Hydrogen KW - Solubility KW - Temperature KW - Tensile loading KW - Analytical calculation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586701 DO - https://doi.org/10.1002/srin.202300493 SN - 1611-3683 SP - 1 EP - 9 PB - Wiley AN - OPUS4-58670 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Welding KW - Hydrogen pipeline KW - Review PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638847 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63884 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Repair Welding of In-Service Hydrogen Pipelines - Concepts and Challenges N2 - Hydrogen is set as the energy carrier of tomorrow for a more sustainable fossil fuel free future. As this necessitates a reliable transport infrastructure, repurposing of the existing natural gas grid is planned. With regards to the well-known effect of hydrogen embrittlement, the compatibility of utilized materials must be investigated. First comprehensive studies on pipeline material hydrogen compatibility indicate that these materials can be applied to a certain extent. Nonetheless, the material compatibility is currently of high interest and focus of numerous research projects worldwide. However, pipelines require frequent maintenance and repair work. As part of these, in some cases it is necessary to do weldments onto pipelines while they are pressurized. This in-service welding introduces additional challenges for the material compatibility. Due to the resulting high temperatures, the metallurgical changes in the material and of course the presence of high-pressure hydrogen in the pipeline, additional investigations need to be conducted to ensure that no critical material degradation because of increased hydrogen absorption occurs and an overall material compatibility is given. For this reason, the present paper introduces in-service welding on pipelines. An overview of current research projects that deal with the application of in-service welding specifically on hydrogen pipelines and the emerging problems when applying these techniques on hydrogen pipelines is given. Methods of material testing, their limits and possible solutions are presented and discussed. T2 - 2024 15th International Pipeline Conference CY - Calgary, Alberta, Canada DA - 23.09.2024 KW - Hydrogen KW - Pipeline KW - Welding KW - In-Service PY - 2024 SN - 978-0-7918-8856-8 DO - https://doi.org/10.1115/IPC2024-133052 SP - 1 EP - 6 PB - The American Society of Mechanical Engineers (ASME) CY - New York AN - OPUS4-62262 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Grimault de Freitas, Tomás A1 - Rhode, Michael A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique N2 - The constantly increasing demand for renewable energy sources leads to the necessity of transporting large amounts of hydrogen. Since pipelines enable a cost-effective way for the distribution of gaseous hydrogen, the interaction of hydrogen and the pipeline materials must be carefully investigated as hydrogen can cause a degradation of the mechanical properties under certain conditions. Especially welds, which are assumed to be more susceptible to the degradation enhanced by hydrogen, are of great interest. The aim of this study is to investigate the effect of gaseous hydrogen on the mechanical properties of an X65 pipeline, and the longitudinal submerged arc welding (SAW) welded joint. The tests are conducted using the hollow specimen technique on two types of specimens: one extracted from the base material (BM) and the other extracted as a cross-weld (CW) specimen consisting of BM and weld seam. The specimens are charged in situ under a pressure of 60 bar and tested using slow strain rate (SSR) tensile tests with a nominal strain rate of 10−5 s−1. The properties obtained of specimens tested in hydrogen atmosphere are compared to the properties of comparable specimen in inert argon atmosphere as a reference. The performed tests showed a decrease of the reduction of area (RA) from 72% in inert atmosphere to 52% in hydrogen atmosphere for the CW specimen and a decrease from 73% in inert atmosphere to 51% for the BM. Metallographic analyses showed the crack initiation between fine-grained heat-affected zone (FGHAZ) and BM for the specimens tested in hydrogen atmosphere as well as for the reference specimens. This leads to the conclusion that the location of the crack initiation does not change due to the presence of gaseous hydrogen. KW - Hydrogen KW - Hollow specimen technique KW - Pipeline KW - SSRT KW - Hydrogen embrittlement KW - Cross-weld specimen PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624658 DO - https://doi.org/10.1007/s40194-025-01953-3 SN - 0043-2288 SN - 1878-6669 VL - 69 IS - 3 SP - 861 EP - 870 PB - Springer CY - Berlin AN - OPUS4-62465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -