TY - CONF A1 - Rhode, Michael T1 - Welding of high-entropy alloys - New material concept vs. old challenges N2 - HEAs represent a relatively new class of materials. The the alloy concept is fundamentally different from the most conventional materials and alloys that are used today. Recently, the focus of HEA designs is more application-based. For that purpose, the elements of interest are carefully selected and multiple phases as well as micro-structures are deliberately adjusted. Currently, only limited attention has been paid to weldability of HEA. This encompasses possible effects on metallurgy and its influence on the desired properties. It remains open if welding causes e.g. considerable number of intermetallic phases or segregations and their effect on weld joint properties. For that reason, the scope of this study is to summarize already available studies on welding of HEAs with respect to the HEA-type, the applied welding process and its influence on the weld joint properties. T2 - IIW Annual Assembly, Meeting of Commission II-A CY - Online meeting DA - 20.07.2020 KW - High-entropy alloy KW - Welding KW - Review PY - 2020 AN - OPUS4-51116 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Wasserstoffdiffusion und lokale Volta-Potentiale in Hoch- und Mittelentropie-Legierungen N2 - Hochentropie-Legierungen (HEAs) zeichnen sich durch einen Mischkristall-System aus mindestens fünf und Mittelentropie-Legierungen (MEAs) durch mindestens drei Hauptlegierungselemente aus, in äquiatomarer Zusammensetzung. Sie zeigen außergewöhnliche Anwendungseigenschaften, wie z.B. hohe Festigkeit, Duktilität oder Korrosionsbeständigkeit. Zukünftige HEA/MEA-Komponenten aufgrund ihrer Eigenschaften für wasserstoffhaltige Umgebungen (wie Behälter für kryogene oder Hochdruckspeicherung) von Interesse. Daher ist die Bewertung der Wasserstoffabsorption und die Diffusion in diesen Materialien von großer Bedeutung. Dazu wurden in unserer Studie eine CoCrFeMnNi-HEA und eine CoCrNi-MEA untersucht. Die Proben wurden elektrochemisch mit Wasserstoff beladen. Für die Ermittlung des Wasserstoffdiffusionsverhaltens wurde die thermische Desorptionsanalyse (TDA) mit unterschiedlichen Heizraten bis zu 0,250 K/s angewandt. Die nachfolgende Peakentfaltung der Signale führte zu Hochtemperatur-Desorptionsspitzen und Wasserstofftrapping auch über 280°C. Eine resultierende Gesamtwasserstoffkonzentration > 40 ppm wurde für den MEA ermittelt und > 100 ppm für den HEA. Dies deutet auf zwei wichtige Effekte hin: (1) verzögerte Wasserstoffdiffusion und (2) eine beträchtliche Menge an getrapptem Wasserstoff auch bei hoher Temperatur. Beide Effekte können hinsichtlich einer wasserstoffunterstützten Rissbildung kritisch werden, dies erfordert jedoch weitere Untersuchungen. Zusätzlich erfolgte die Bestimmung des lokalen Volta-Potentials mittels hochauflösender Kelvin-Sonden-Kraft-Mikroskopie (SKPFM). Die ermittelten Scans zeigen einen bestimmten Einfluss der Wasserstoffbeladung auf die Potentiale. T2 - Symposium on Materials and Joining Technology CY - Online meeting DA - 07.09.2020 KW - Wasserstoff KW - High-entropy alloy KW - Diffusion KW - Scanning kelvin probe force microscopy KW - Thermal desorption analysis PY - 2020 AN - OPUS4-51187 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Steger, Jörg A1 - Böllinghaus, Thomas A1 - Kannengießer, Thomas ED - Lippold, J. ED - Böllinghaus, Thomas ED - Richardson, I. M. T1 - Hydrogen degradation effects on mechanical properties in T24 weld microstructures N2 - Spectacular failure cases of fossil power stations in the recent years exhibited severe cracking in T24 welds. The results show that hydrogen-assisted cracking up to 200 °C cannot be excluded. Hence, it is important to gain a basic understanding on how hydrogen might affect the basic material properties in the respective weld microstructures. The present study focuses on hydrogen degradation of the respective weld microstructures, i.e., the weld metal and the coarse grained heat affected zone, where actually cracking appeared in practice. Tensile tests were carried out for coarse grain heataffected zone (CGHAZ) and the weld metal in uncharged and electrochemically hydrogen-charged condition. It turned out that both microstructures show distinct tendency for gradual degradation of mechanical properties in the presence of increasing hydrogen concentration. Already for a hydrogen concentration about and above 2 ml/100 g Fe, a significant ductility reduction has been observed. SEM investigations revealed that the fracture topography changes from ductile topography in uncharged condition to intergranular topography for the CGHAZ and to ductile-brittle mix for the weld metal (WM) in hydrogen charged condition. Ti-rich inclusions were identified as central regions of quasi-cleavage fracture areas in the WM. An approximation procedure is applied to quantify the degradation intensity. KW - Low alloy steels KW - Hydrogen embrittlement KW - Heat affected zone KW - Microstructure KW - Creep resisting materials PY - 2016 UR - http://link.springer.com/article/10.1007/s40194-015-0285-5 DO - https://doi.org/10.1007/s40194-015-0285-5 SN - 0043-2288 VL - 60 IS - 2 SP - 201 EP - 216 PB - Springer-Verlag GmbH CY - Heidelberg AN - OPUS4-35390 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schaupp, Thomas A1 - Rhode, Michael A1 - Kannengießer, Thomas ED - Lippold, J. ED - Böllinghaus, Thomas ED - Richardson, I. T1 - Influence of welding parameters on diffusible hydrogen content in high-strength steel welds using modified spray arc process N2 - In order to satisfy the growing requirements towards lightweight design and resource efficiency in modern steel constructions, e.g., mobile cranes and bridges, high-strength steels with typical yield strength ≥ 690 MPa are coming into use to an increasing extent. However, these steels require special treatment in welding. The susceptibility for degradation of the mechanical properties in the presence of hydrogen increases significantly with increasing yield strength. In case of missing knowledge about how and the amount of hydrogen that is uptaken during welding, hydrogen-assisted cracking (HAC) can be a negative consequence. Moreover, modern weld technology like the modified spray arc process enables welding of narrower weld seams. In this context, a reduced number of weld beads, volume, and total heat input are technical and economical benefits. This work presents the influence of welding parameters on the diffusible hydrogen content in both (1) single-pass and (2) multi-layer welds. Different hydrogen concentrations were detected by varied contact tube distance, wire feed speed, arc length, and varied arc type (transitional arc and modified spray arc). The results show that all welding parameters have significant influence on the diffusible hydrogen concentration in the single-pass welds. By increasing the number of weld beads in case of multi-layer welding, the hydrogen concentration has been reduced. Whereby, differences in hydrogen concentrations between both arc types are present. KW - Hydrogen KW - MAG welding KW - High-strength steels KW - Process parameters PY - 2018 DO - https://doi.org/10.1007/s40194-017-0535-9 SN - 0043-2288 SN - 1878-6669 VL - 62 IS - 1 SP - 9 EP - 18 PB - Springer CY - Berlin Heidelberg AN - OPUS4-43864 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Mente, Tobias A1 - Böllinghaus, Thomas T1 - Modeling of hydrogen-assisted cracking (HAC) in duplex stainless steels (DSS) N2 - Modeling of Hydrogen-Assisted Cracking (HAC) in Duplex Stainless Steels (DSS): - Hydrogen causes significant degradation in DSS and consequently HAC - Mechanisms of HAC have not been fully understood in two-phase microstructures - Mesoscale numerical modeling for HAC in DSS was created, coupled to the macroscale, enabling simulation of HAC in both phases independent from predefined crack paths T2 - International Hydrogen Conference - Material Performance in Hydrogen Environments CY - Jackson Lake Lodge, Moran, Wyoming, USA DA - 11.09.2016 KW - Hydrogen KW - Numerical modeling KW - Duplex stainless steel KW - Hydrogen assisted cracking PY - 2016 AN - OPUS4-37404 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Böllinghaus, Thomas T1 - Hydrogen absorption and diffusion in T24 steel weld joints and effect on mechanical properties N2 - The present contribution summarizes results obtained from experiments with low-alloyed boiler steel grades T24 (CrMoV alloy), T22 (CrMo) and thermally simulated T24 HAZ microstructure and pure weld metal. The hydrogen absorption and diffusion behavior was investigated by permeation experiments and thermal desorption analysis (TDA). The results showed significant weld microstructure influence on diffusion by hydrogen trapping. Trapped hydrogen was determined in the T24 BM at temperatures up to 120 °C compared to 75 °C in the T22. In addition, the T24 HAZ showed decreased diffusion coefficients (at room temperature) of approximately one magnitude compared to the BM. For the mechanical properties, tensile tests were conducted with electrochemically hydrogen charged specimens and compared to results obtained from slow strain rate tests (SSRT) in high-temperature water up to 200 °C. The as-welded HAZ had remarkably increased susceptibility compared to the BM already at low hydrogen concentration of 1-2 ppm. The SSRT were conducted for free corrosion and acidic environment and confirmed this behavior at elevated temperatures for both HAZ microstructures of T24 and T22. Summarized, each weld microstructure has specific diffusion coefficients and shows different susceptibility to degradation of the mechanical properties, i.e. delayed hydrogen assisted cracking or stress corrosion cracking. T2 - NACE Italia - 2nd Conference & Expo 2018 CY - Genoa, Italy DA - 28.05.2018 KW - Hydrogen KW - Stress corrosion cracking KW - Welding KW - Creep-resistant steel PY - 2018 SP - Paper 10, 1 EP - 7 AN - OPUS4-45081 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - "On how to influence your results" - A review on carrier gas hot extraction parameters for hydrogen determination in welded specimens N2 - Carrier gas hot extraction (CGHE) is a commonly applied technique for determination of hydrogen in welded joints using a thermal conductivity device (TCD) for quantitative measurement. The CGHE is based on the accelerated hydrogen effusion due to thermal activation at elevated temperatures. The ISO 3690 standard suggests different specimen geometries as well as necessary minimum extraction time vs. temperature. They have the biggest influence on precise hydrogen determination. The present study summarizes the results and experience of numerous test runs with different specimen temperatures, geometries and factors that additionally influence hydrogen determination. They are namely: specimen surface (polished/as-welded), limited TCD sensitivity vs. specimen volume, temperature measurement vs. effects of PID-furnace controller as well as errors due to insufficient data assessment. Summarized, the temperature is the driving force of the CGHE. Two different methods are suggested to increase the heating rate up the reach the desired extraction temperature without changing the experimental equipment. Suggestions are made to improve the reliability of hydrogen determination depended on the hydrogen signal stability during extraction accompanied by evaluation of the recorded data. Generally, independent temperature measurement with calibration specimens is useful for further data analysis, especially if this data is used for calculation of trapping kinetics by thermal desorption analysis (TDA). T2 - IIW Annual Assembly and International Conference 2018, Meeting of Commission II-E CY - Nusa Dua, Bali Island, Indonesia DA - 15.07.2018 KW - Carrier gas hot extraction (CGHE) KW - Welding KW - ISO 3690 KW - Hydrogen KW - Experimental design PY - 2018 AN - OPUS4-45520 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Richter, Tim A1 - Schröpfer, Dirk A1 - Rhode, Michael A1 - Boerner, Andreas A1 - Saliwan Neumann, Romeo A1 - Schneider, M. A1 - Laplanche, G. T1 - Influence of machining on the surface integrity of high- and medium-entropy alloys N2 - High- and medium-entropy alloys (HEAs) are a quite new class of materials. They have a high potential for applications from low to high temperatures due to the excellent combination of their structural properties. Concerning their application as components; processing properties, such as machinability, have hardly been investigated so far. Hence, machinability analyses with a focus on the influence of the milling process and its basic parameters (cutting speed, feed per cutting edge) on the resulting surface integrity of specimens from an equiatomic high- (CoCrFeMnNi) and a medium- (CoCrNi) entropy alloy have been carried out. A highly innovative milling process with ultrasonic assistance (USAM) was compared to conventional milling processes. Recent studies have shown that USAM has a high potential to significantly reduce the mechanical load on the tool and workpiece surface during milling. In this study, the basic machining and ultrasonic parameters were systematically varied. After machining, the surface integrity of the alloys was analyzed in terms of topography, defects, subsurface damage, and residual stresses. It was observed that USAM reduces the cutting forces and increases the surface integrity in terms of lower tensile residual stresses and defect density near the surfaces for the CoCrFeMnNi alloy. It was shown that the cutting forces and the metallurgical influence in the sub surface region are reduced by increasing the cutting speed and reducing the feed rate per cutting edge. With the CoCrNi alloy, the tool revealed severe wear. As a result, for this alloy no influence of the parameters on the machinability could be determined. KW - High Entropy Alloy KW - Medium Entropy Alloys KW - Ultrasonic assited machining PY - 2022 DO - https://doi.org/10.1016/j.matchemphys.2021.125271 SN - 0254-0584 VL - 275 SP - 125271 PB - Elsevier B.V. AN - OPUS4-53606 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Mechanische Eigenschaften der Längschweißnaht einer X65-Pipeline in Druckwasserstoffatmosphäre N2 - Im folgenden Beitrag werden die Ergebnisse der mechanischen Eigenschaften unter 200 bar Druckwasserstoff des Werkstoffes 316L (1.4404) vorgestellt. Dazu wurden Hohlzugproben aus konventionellem, kaltgezogenem Material herausgearbeitet und per SLM-PBF additiv gefertigten Hohlzugproben gegenübergestellt. Die Proben wurden da-bei unter Druckwasserstoff einer SSRT-Prüfung mit einer Dehnrate von 1E-5/s unterzogen. Zusätzlich zum Werkstoffzustand wurde der Einfluss des Oberflächenzustandes charakterisiert: (1) additiv gefertigten Proben mit endkonturnaher Form „as-printed“ oh-ne zusätzliche Bohrung, (2) Bohren und (3) zusätzliches Honen. Die gemessene Degradation der mechanischen Eigenschaften unter Wasserstoff hing dabei in erster Linie von der Oberfläche ab und damit indirekt vom Werkstoffzustand „as-printed“ oder kaltgezogen ab. Während die Proben mit gebohrter und/oder gehonter Oberfläche eine RRA (Relative Reduction of Area) 78 % aufwiesen, zeigten die AM-Proben eine deutlich höhere RRA von 90 %. Ein möglicher Grund dafür sind während der Fertigung ausbildende Oxidschichten, die sich durch geringe Mengen an Restsauerstoff während des AM-Prozesses ausbilden. Zur abschließenden Charakterisierung sind weitere Untersuchungen erforderlich, insbesondere für ein größeres Parameterfeld an Prüftemperaturen (Oxideinwirkung) und Dehnraten (mechanische Beständigkeit der Oxidschicht ähnlich den Einflüssen auf „klassische“ Spannungsrisskorrosion). T2 - DGM Arbeitskreis Wasserstoff CY - Neu-Isenburg, Germany DA - 26.05.2025 KW - Pipeline KW - Wasserstoff KW - Hohlzugprobe PY - 2025 AN - OPUS4-63236 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Additive gefertigte 316L-Hohlzugproben unter Druckwasserstoff - Einfluss der Oberfläche und des Werkstoffzustandes N2 - Im folgenden Beitrag werden die Ergebnisse der mechanischen Eigenschaften unter 200 bar Druckwasserstoff des Werkstoffes 316L (1.4404) vorgestellt. Dazu wurden Hohlzugproben aus konventionellem, kaltgezogenem Material herausgearbeitet und per SLM-PBF additiv gefertigten Hohlzugproben gegenübergestellt. Die Proben wurden da-bei unter Druckwasserstoff einer SSRT-Prüfung mit einer Dehnrate von 1E-5/s unterzogen. Zusätzlich zum Werkstoffzustand wurde der Einfluss des Oberflächenzustandes charakterisiert: (1) additiv gefertigten Proben mit endkonturnaher Form „as-printed“ oh-ne zusätzliche Bohrung, (2) Bohren und (3) zusätzliches Honen. Die gemessene Degra-dation der mechanischen Eigenschaften unter Wasserstoff hing dabei in erster Linie von der Oberfläche ab und damit indirekt vom Werkstoffzustand „as-printed“ oder kaltgezogen ab. Während die Proben mit gebohrter und/oder gehonter Oberfläche eine RRA (Relative Reduction of Area) 78 % aufwiesen, zeigten die AM-Proben eine deutlich höhere RRA von 90 %. Ein möglicher Grund dafür sind während der Fertigung ausbildende Oxidschichten, die sich durch geringe Mengen an Restsauerstoff während des AM-Prozesses ausbilden. Zur abschließenden Charakterisierung sind weitere Untersuchungen erforderlich, insbesondere für ein größeres Parameterfeld an Prüftemperaturen (Oxideinwirkung) und Dehnraten (mechanische Beständigkeit der Oxidschicht ähnlich den Einflüssen auf „klassische“ Spannungsrisskorrosion). T2 - DGM Arbeitskreis Wasserstoff CY - Neu-Isenburg, Germany DA - 26.05.2025 KW - Wasserstoff KW - Additive Fertigung KW - Hohlzugprobe KW - Austentitischer Stahl PY - 2025 AN - OPUS4-63239 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Richter, Tim A1 - Mayr, P. A1 - Nitsche, A. A1 - Mente, Tobias A1 - Böllinghaus, Thomas T1 - Hydrogen diffusion in creep-resistant 9% Cr P91 multi-layer weld metal N2 - Welded components of P91 9% Cr steel demand for careful welding fabrication with necessary post weld heat treatment (PWHT). Before the PWHT, a hydrogen removal heat treatment is necessary for avoidance of hydrogen assisted cracking (HAC). In this context, the microstructure and temperature-dependent hydrogen diffusion is important, and reliable diffusion coefficients of P91 weld metal are rare. For that reason, the diffusion behavior of P91 multi-layer weld metal was investigated for as-welded (AW) and PWHT condition by electrochemical permeation experiments at room temperature and carrier gas hot extraction (CGHE) from 100 to 400 °C. Hydrogen diffusion coefficients were calculated, and the corresponding hydrogen concentration was measured. It was ascertained that both heat treatment conditions show significant differences. At room temperature the AW condition showed significant hydrogen trapping expressed by to seven times lower diffusion coefficients. A preferred diffusion direction was found in perpendicular direction expressed by high permeability. The CGHE experiments revealed lower diffusion coefficients for the AW condition up to 400 °C. In this context, a hydrogen concentration of approximately 21 ml/100 g was still trapped at 100 °C. For that reason, a certain HAC susceptibility of as-welded P91 weld metal cannot be excluded, and hydrogen removal should be done before PWHT. KW - Creep resisting materials KW - Diffusion KW - Hydrogen KW - Weld metal KW - Post weld heat treatment KW - Microstructure PY - 2020 DO - https://doi.org/10.1007/s40194-019-00828-8 SN - 0043-2288 VL - 64 IS - 2 SP - 267 EP - 281 PB - Springer AN - OPUS4-50471 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hollow specimens as simplified approach for testing metallic materials under high pressure hydrogen development and utilization N2 - The hydrogen economy requires large-scale storage and transportation options like long-distance transmission pipelines. The applied materials (typically steels) must be carefully tested under different conditions (pressure, temperature, impact of impurities, etc.) for their suitability and service with hydrogen. In combination with mechanical load, as occurs in every gas network, hydrogen can induce degradation of the mechanical properties and promote finally resulting in embrittlement, i.e., the formation of cracks. The conventional testing procedures consist of autoclaves in which samples are strained under pressurized hydrogen. The test apparatus requires large amounts of hydrogen and thus a high level of safety and costs. In very specific cases, these tests might be replaced by simplified electrochemical charging. However, these test alternatives raise several questions regarding the equivalency of both testing scenarios. In the early 1980’s the idea of a so-called hollow tensile sample raised and was reinitiated 2021 in ISO TC 164 by T. Ogata (NIMS, Japan) and further developed (e.g. by Fraunhofer IWM, Germany). The idea was: the sample itself represents the autoclave instead of charging a sample from outside. For that reason, a hole is drilled through the sample and the inner surface is pressurized by hydrogen gas during the mechanical testing. Indeed, this represents the main advantage as no expensive pressure-resistant autoclave equipment for large H-volumes is necessary, which significantly reduces the safety-related issues and thus the high costs. In the following, we show recent activities at BAM Berlin on adaption of the hollow-specimen technique for slow strain rate testing (SSRT). The current research activities are focussed on macroscopic influences like the sample geometry, minimum necessary dimensions, and microscopic influences e.g., on the surface by the processing method (drill hole quality and geometric precision) as well as the gas pressure effect (mechanical deformation of surface in different media). T2 - FEMS EUROMAT 2023 CY - Frankfurt a. M., Germany DA - 04.09.2023 KW - Hydrogen KW - Hollow tensile specimen KW - High-pressure KW - Mechanical properties KW - Testing PY - 2023 AN - OPUS4-58220 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Böllinghaus, Thomas A1 - Rhode, Michael A1 - Falkenreck, T. ED - Bender, B. ED - Göhlich, D. T1 - Korrosion und Korrosionsschutz N2 - Das Kapitel beginnt mit einer kurzen Einführung über die Korrosion (Wechselwirkung zwischen einem Metall, einer korrosiven Umgebung und der der jeweiligen Konstruktion). Im zweiten Abschnitt werden die wichtigsten Formen der wässrigen elektrochemischen Korrosion (Flächenkorrosion, galvanische, selektive und interkristalline Korrosion sowie Loch- und Spaltkorrosion) betrachtet. Darüber hinaus wird die elektrochemische Korrosion unter mechanischer Belastung betrachtet (Spannungsrisskorrosion, wasserstoffunterstützte Rissbildung, Korrosionsermüdung), sowie Sonderformen der Korrosion (Erosion, Fretting und mikrobiologisch induzierte Korrosion). Der dritte Abschnitt befasst sich mit der chemischen und Hochtemperaturkorrosion (Oxidation, Aufkohlung, Hochtemperatur-Wasserstoffangriff, Aufschwefelung, Nitrierung, Halogenierung). Zusätzlich enthält das Kapitel Maßnahmen zur Vermeidung der Korrosion. KW - Korrosion KW - Korrosionsschutz KW - Spannungsrisskorrosion KW - Wasserstoff KW - Loch- u. Spaltkorrosion PY - 2021 SN - 978-3-662-59710-1 DO - https://doi.org/10.1007/978-3-662-59711-8_34 VL - 1 SP - 691 EP - 725 PB - Springer-Verlag GmbH, ein Teil von Springer Nature CY - Berlin ET - 26 AN - OPUS4-52156 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen absorption and diffusion in T24 steel weld joints and effect on mechanical properties N2 - The present contribution summarizes results obtained from experiments with low-alloyed boiler steel grades T24 (CrMoV alloy), T22 (CrMo) and thermally simulated T24 HAZ microstructure and pure weld metal. The hydrogen absorption and diffusion behavior was investigated by permeation experiments and thermal desorption analysis (TDA). The results showed significant weld microstructure influence on diffusion by hydrogen trapping. Trapped hydrogen was determined in the T24 BM at temperatures up to 120 °C compared to 75 °C in the T22. In addition, the T24 HAZ showed decreased diffusion coefficients (at room temperature) of approximately one magnitude compared to the BM. For the mechanical properties, tensile tests were conducted with electrochemically hydrogen charged specimens and compared to results obtained from slow strain rate tests (SSRT) in high-temperature water up to 200 °C. The as-welded HAZ had remarkably increased susceptibility compared to the BM already at low hydrogen concentration of 1-2 ppm. The SSRT were conducted for free corrosion and acidic environment and confirmed this behavior at elevated temperatures for both HAZ microstructures of T24 and T22. Summarized, each weld microstructure has specific diffusion coefficients and shows different susceptibility to degradation of the mechanical properties, i.e. delayed hydrogen assisted cracking or stress corrosion cracking. T2 - NACE Italia - 2nd Conference & Expo 2018 CY - Genoa, Italy DA - 28.05.2018 KW - Hydrogen KW - Stress corrosion cracking KW - Welding KW - Creep-resistant steel KW - T24 / 7CrMoVTiB10-10 PY - 2018 AN - OPUS4-45080 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Wasserstoffeffekt auf die Degradiation der mechanischen Eigenschaften von T24 Schweißgut und simulierter Grobkorn-WEZ T2 - MDDK Magdeburg CY - Magdeburg DA - 2014-11-27 PY - 2014 AN - OPUS4-32157 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Böllinghaus, Thomas A1 - Rhode, Michael A1 - Falkenreck, T. ED - Grote, K.-H. ED - Hefazi, H. T1 - 6. Corrosion and Corrosion Resistance N2 - The chapter starts with a brief introduction about corrosion, which is defined as the interdependency between a metal, a corrosive environment, and the respective component design. The second section introduces the most important forms of aqueous electrochemical corrosion (uniform corrosion, galvanic corrosion, selective and intergranular corrosion, and finally pitting and crevice corrosion in the case of passive layer forming metals). In addition, electrochemical corrosion under applied mechanical load is introduced (stress corrosion cracking, hydrogen-assisted cracking, corrosion fatigue), as well as special forms of corrosion (erosion, fretting, and microbiologically induced corrosion). The third section of this chapter introduces (mostly dry) chemical corrosion and high-temperature corrosion (oxidation, carburization, high-temperature hydrogen attack, sulfurization, nitriding, halogenation). As in the case of electrochemical corrosion, chemical corrosion can also be superimposed by mechanical loads. Finally, general facts on the testing of corrosion are introduced. KW - Corrosion KW - Corrosion testing KW - Handbook KW - Electrochemical corrosion KW - Chemical corrosion PY - 2021 SN - 978-3-030-47035-7 DO - https://doi.org/10.1007/978-3-030-47035-7_6 VL - 2021 SP - 185 EP - 213 PB - Springer Nature Switzerland AG CY - Cham (CH) ET - 2nd Edition AN - OPUS4-52423 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Rhode, Michael A1 - Münster, C. A1 - Mente, Tobias A1 - Böllinghaus, Thomas ED - Somerday, B.P. ED - Sofronis, P. T1 - Influence of experimental conditions and calculation method on hydrogen diffusion coefficient evaluation at elevated temperatures N2 - Literature provides a wide range of hydrogen diffusion coefficients for low alloyed steels used in power plants. In fact, experimental boundary conditions and calculation methods have influence on the determination of these coefficients. The diffusion and trapping behavior in creep-resistant steel 7CrMoVTiB10-10 has been studied. Based on experimental carrier gas hot extraction (CGHE) data, a numerical model has been developed to describe the hydrogen transport and respective hydrogen distribution at elevated temperatures. The numerical results suggest that common calculation methods for diffusion coefficients are limited for experimental data analysis. The sample preparation time before CGHE experiment influences the determined diffusion coefficients with the consequence that non-homogeneous hydrogen concentration profiles have to be considered in the simulations. KW - Temperature effect KW - Hydrogen diffusion KW - Creep-resistant steel KW - Hydrogen assisted cracking KW - Carrier gas hot extraction PY - 2017 SN - 978-0-7918-6138-7 DO - https://doi.org/10.1115/1.861387_ch56 SP - 495 EP - 503 PB - ASME CY - New York, USA ET - 1 AN - OPUS4-42502 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Der Weg zur Standardisierung der Hohlzugtechnik für die Nutzung mit gasförmigem Wasserstoff N2 - Dieser Kurzvortrag stellt selektierte Ergebnisse des Projektes "H2Hohlzug" im übergeordneten Projekt "TransHyDE" kurz vor. Insbesondere wird auf die Herausforderung eingegangen, wiederholbare Prüfbedingungen unter Druckwasserstoffbeanspruchung, einzuhalten. T2 - Herbstsitzung des DGM Arbeitskreises "Materialprüfung unter Wasserstoff" CY - Dortmund, Germany DA - 19.11.2024 KW - Hohlzugprobe KW - Wasserstoff KW - Materialprüfung KW - Standardisierung PY - 2024 AN - OPUS4-61718 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Additive manufacturing for components in hydrogen technologies N2 - With the introduction of a hydrogen-based energy and national economy, safety-relevant components for hydrogen technologies are becoming increasingly important. Characteristic of hydrogen technologies are, for example, harsh environmental conditions such as cryogenic or high-pressure storage, corrosion issues in fuel cells and electrolyzers, turbines, and many more. Additive manufacturing of components is becoming increasingly important and irreplaceable for the production of complex technical systems. Using the case studies of burners for gas turbines and electrodes and membranes for polymer (PEMFC) and solid oxide (SOFC) fuel cells, this article shows the potential of additive manufacturing of components. At the same time, however, the challenge of considering divergent mechanical properties depending on the direction of assembly in a "hydrogen-compatible" manner is also highlighted. Finally, the challenges posed by additive manufacturing and hydrogen for materials testing are highlighted under scenarios that are as realistic as possible. T2 - MPA-Workshop Hydrogen CY - Online meeting DA - 10.11.2022 KW - Additive manufacturing KW - Hydrogen KW - Technologies KW - Overview KW - Component PY - 2022 AN - OPUS4-56233 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Processing and application properties of multiple principal element alloys (MPEA) N2 - The presentation gives an overview of BAM's activities on processing influences and application properties of MPEAs in the form of joined and machined high and medium entropy alloys (CoCrFeMnNi and CoCrNi). In the case of welding, the focus is on defect-free welded joints with sufficient mechanical properties. In the case of machining, the focus is on the possible influence on the surface quality of the materials through adequate milling parameters. In addition, the hydrogen absorption and diffusion properties as well as the electrochemical corrosion behavior are fundamentally examined. T2 - FAU-Department Werkstoffwissenschaften, Seminar: Aktuelle Probleme der Werkstoffwissenschaften CY - Erlangen, Germany DA - 25.04.2024 KW - Welding KW - Application properties KW - Machining KW - High-entropy alloy KW - Hydrogen PY - 2024 AN - OPUS4-59975 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen diffusion in creep-resistant 9%-Cr P91 steel weld metal N2 - 9 %-Cr steel P91 is widely used in power plants due to the excellent creep-resistance. Components of this steel are typically welded and demand for careful welding fabrication, whereas a so-called post weld heat treatment (PWHT), must be conducted to increase the toughness and decrease the hardness of the martensitic as-welded (AW) microstructure. Before the PWHT, a hydrogen removal (or dehydrogenation) heat treatment is necessary as hardened AW martensitic microstructure is generally prone to delayed hydrogen assisted cracking (HAC). The microstructure and temperature dependent hydrogen diffusion is an important issue as it determines how long a potential crack-critical hydrogen concentration could remain in the microstructure. In this context, reliable hydrogen diffusion coefficients of P91 weld metal are rare. Hence, the diffusion behavior of P91 multi-layer weld metal was investigated in two different microstructure conditions: AW and further PWHT (760 °C for 4 h). Two different experimental techniques were used to cover a wide range of hydrogen diffusion temperatures: the electrochemical permeation technique (PT) at room temperature and the carrier gas hot extraction (CGHE) for a temperature range from 100 to 400 °C. From both techniques typical hydrogen diffusion coefficients were calculated and the corresponding hydrogen concentration was measured. It was ascertained that both heat treatment conditions show significant differences in hydrogen diffusivity. The biggest deviations were identified for room temperature. In this case, the AW condition shows significant hydrogen trapping and up to seven times lower diffusion coefficients. Additionally, PT investigations showed a preferred diffusion direction of hydrogen in the weld metal expressed by the diffusion coefficients and the permeability for both heat treatment conditions. The CGHE generally revealed lower diffusion coefficients for the AW microstructure up to 200 °C. In addition, the AW condition showed hydrogen concentrations up to 50 ml/100 g (considering electrochemical charging). Nonetheless, this hydrogen was not permanently (reversibly) trapped. Nonetheless, this temperature is approximately 100 °C below recommended dehydrogenation heat treatment (DHT). This has two main consequences: (I) in case of welding is interrupted or no DHT is conducted, a HAC susceptibility of hardened martensitic P91 weld metal cannot be excluded and (II) DHT can be conducted at temperatures around 200 °C below the recommended temperatures. T2 - IIW Annual Assembly, Meeting of Commission IX-C "Creep and heat resistant welds" CY - Bratislava, Slovakia DA - 07.07.2019 KW - Hydrogen KW - Diffusion KW - Weld metal KW - Microstructure KW - Post weld heat treatment PY - 2019 AN - OPUS4-48449 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Schaupp, Thomas A1 - Münster, C. A1 - Mente, Tobias A1 - Kannengießer, Thomas A1 - Böllinghaus, Thomas T1 - Hydrogen determination in welded specimens by carrier gas hot extraction - a review on the main parameters and their effects on hydrogen measurement N2 - Carrier gas hot extraction (CGHE) is a commonly applied technique for determination of hydrogen in weld joints using a thermal conductivity detector (TCD) for hydrogen measurement. The CGHE is based on the accelerated hydrogen effusion due to thermal activation at elevated temperatures. The ISO 3690 standard suggests different specimen geometries as well as necessary minimum extraction time vs. temperature. They have the biggest influence on precise hydrogen determination. The present study summarizes the results and experience of numerous test runs with different specimen temperatures, geometries (ISO 3690 type B and small cylindrical samples), and factors that additionally influence hydrogen determination. They are namely specimen surface (polished/as-welded), limited TCD sensitivity vs. specimen volume, temperature measurement vs. effects of PI-furnace controller, as well as errors due to insufficient data assessment. Summarized, the temperature is the driving force of the CGHE. Two different methods are suggested to increase the heating rate up to the desired extraction temperature without changing the experimental equipment. Suggestions are made to improve the reliability of hydrogen determination depended on the hydrogen signal stability during extraction accompanied by Evaluation of the recorded data. Generally, independent temperature measurement with dummy specimens is useful for further data analysis, especially if this data is used for calculation of trapping kinetics by thermal desorption analysis (TDA). KW - Hydrogen KW - Carrier gas hot extraction KW - Experimental design KW - Thermal conductivity device PY - 2019 DO - https://doi.org/10.1007/s40194-018-0664-9 SN - 0043-2288 VL - 63 IS - 2 SP - 511 EP - 526 PB - Springer CY - Berlin, Heidelberg AN - OPUS4-47603 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schaupp, Thomas A1 - Rhode, Michael A1 - Yahyaoui, Hamza A1 - Kannengießer, Thomas ED - Lippold, J. ED - Böllinghaus, Thomas ED - Richardson, I. T1 - Influence of heat control on hydrogen distribution in high-strength multi-layer welds with narrow groove N2 - High-strength low-alloyed (HSLA) steels with yield strength ≥ 690 MPa are gaining popularity in civil engineering and construction of heavy vehicles. With increasing yield strength, the susceptibility for degradation of the mechanical properties in the presence of diffusible hydrogen, i.e., hydrogen-assisted cracking (HAC), generally increases. HAC is a result of the critical interaction between local microstructure, mechanical load, and hydrogen concentration. In existing standards for welding of HSLA-steels, recommendations including working temperatures and dehydrogenation heat treatment (DHT) are given to Limit the amount of introduced hydrogen during welding. These recommendations are based on investigations into conventional arc welding processes. In the past decade, modern weld technologies were developed to enable welding of narrower weld seams with V-grooves of 30°, e.g., the modified spray arc process. In that connection, a reduced number of weld runs and weld volume are important technical and, economic benefits. In the present study, the hydrogen distribution in S960QL multi-layer welds with thickness of 20 mm was analyzed. The influence of different weld seam opening angles, heat input, working temperature and DHT were investigated. The results show that weldments with narrow grooves contained an increased amount of diffusible hydrogen. Hydrogen concentration has been reduced by decreasing both the heat input and working temperature. Hydrogen-free weldments were only achieved via subsequent DHT after welding. Furthermore, hydrogen distribution was experimentally determined across the weld seam thickness in HSLA gas metal arc welded multi-layer welds for the first time. KW - Hydrogen KW - GMAW KW - High-strength steels KW - Heat control KW - Heat treatment PY - 2019 DO - https://doi.org/10.1007/s40194-018-00682-0 SN - 0043-2288 SN - 1878-6669 VL - 63 IS - 3 SP - 607 EP - 616 PB - Springer CY - Berlin Heidelberg AN - OPUS4-47878 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Böllinghaus, Thomas A1 - Steffens, B. R. A1 - Rhode, Michael A1 - Shoales, G.A. T1 - Hydrogen Assisted Stress Corrosion Cracking Related Material Properties of ServiceApplied Landing Gear Ultra-High Strength Steels N2 - Aircraft main landing gear (MLG) components are commonly manufactured from low-alloyed, martensitic, ultra-high strength steels (UHSS) that have to be coated for corrosion protection, representing an expensive and environmentally harmful production step. To avoid already partly banned corrosion protection plating, the new high-alloyed UHSS, Ferrium S53 (UNS S10500), has been designed to replace lowalloyed legacy materials and has been subjected to a limited field test over five years. As with the legacy alloys, UNS S10500 has a fully hardened martensitic microstructure known to be susceptible to hydrogen assisted cracking, per se. Containing about 10 wt% Cr, steels such as S10500 are at the lower limit for corrosion resistant alloys. Similar to super-martensitic stainless steels used in the oil and gas industry, a common failure sequence in marine environments represents pitting and subsequent hydrogen assisted stress corrosion cracking (HASCC). For addressing such phenomena quantitively, as required for respective lifetime assessments of MLG components and systems, the tolerance of such materials dependent on the absorbed hydrogen concentration must be evaluated quantitatively. However, there is a lack of such valuable materials data, as well as of the fractographic behavior dependent on the hydrogen concentration that might be absorbed during HASCC. To provide an improved understanding of the hydrogen dependent mechanical and fractographic behavior, samples of the legacy AISI 4340 and the new S10500 MLG steels have electrochemically been hydrogen-saturated and subjected to tensile testing. In contrast to a previous study, this contribution for the first time focuses on materials that have been salvaged from real service used landing gear components. In this study, it has been demonstrated that the service-applied S10500 steel has not only a higher strength, but also an improved ductility in comparison to the legacy AISI 4340 steel after similar service durations that provides a higher tolerance against hydrogen concentrations that might be absorbed during potential pitting and HASCC in marine environments. In addition, it has been found that the absorbed hydrogen concentration significantly affects the fracture behavior. Interestingly, hardening of the hydrogen charged low-alloyed AISI 4340 steel changes the fracture topography from trans- toward intergranular, while hardening of the S10500 steel turned the fracture topography from inter- to transgranular at respectively high hydrogen concentrations. KW - Hydrogen assisted stress corrosion cracking KW - Ultra-high strength steel KW - Martensite KW - Modeling KW - Hydrogen dependent mechanical properties PY - 2019 DO - https://doi.org/10.5006/3028 SN - 0010-9312 SN - 1938-159X VL - 75 IS - 5 SP - 513 EP - 524 PB - NACE International AN - OPUS4-49530 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen in weld joints - An underestimated risk? - Utilization potential of gas analytics versus safety of welded components N2 - Hydrogen was once called “the versatile embrittler” [1], which summarizes very well the effect on reduction of ductility and/or toughness in technical alloys like steel. In that connection, welding is one of the most important component fabrication technologies. During welding, hydrogen can be transferred to the weld pool from manifold sources (like contaminations, residuals at the surface, etc.). As hydrogen embrittles a material, the safety of welded components with hydrogen is always a critical issue. Weld heat input causes additional changes in the microstructure like grain growth or partial dissolution of precipitates and many more. All these things influence the mechanical properties and also represent hydrogen traps. These traps decrease the hydrogen diffusion compared to the ideal lattice. The result can be so-called delayed hydrogen assisted cracking (HAC) of the weld joint due to the significantly decreased diffusivity by trapped hydrogen. This is often an underestimated risk as those cracks can appear in the weld joint even after some days! It is essential to know about hydrogen ingress during welding and the microstructure specific hydrogen diffusion. Both are depended on weld parameter influence and the chemical composition of the base material and weld metal. For that purpose, gas analytic methods like solid-state carrier gas hot extraction (CGHE) are useful tools to: (1) identify detrimental hydrogen concentrations from weld joints, (2) binding energies from hydrogen traps by thermal desorption analysis or (3) high-temperature diffusion coefficients. Those values are extremely important for welding practice in terms of recommendations on realistic hydrogen removal heat treatment (HRHT) after welding. Considering the increasing use of “digital” experiments, the data is also needed for reliable numerical simulations of HAC process or HRHT-effectiveness. The present contribution gives an overview on the influence of hydrogen on weld joints, the necessity, methods and standards for hydrogen determination (CGHE) with the aim of fabrication of safe welded and crack-free components. [1] R. A. Oriani (1987), Corrosion 43(7):390-397. doi: 10.5006/1.3583875 T2 - 20. Tagung Festkörperanalyse - FKA20 CY - Vienna, Austria DA - 01.07.2019 KW - Hydrogen KW - Welding KW - Gas analytic PY - 2019 AN - OPUS4-48402 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Launert, B. A1 - Rhode, Michael A1 - Kromm, Arne A1 - Pasternak, H. A1 - Kannengießer, Thomas ED - Olden, T.-M. ED - Muransky, O. ED - Edwards, L. T1 - Residual stress influence on the flexural buckling of welded I-girders N2 - The nonlinear analysis became a common tool to precisely assess the load-bearing behavior of steel beam and column members. The failure level is significantly influenced by different types of imperfections, among geometric also structural imperfections (residual stresses). Here are still gaps in the knowledge. Nowadays, 3-D welding simulation developed to a level where it could provide reliable estimation of weld-induced distortion and residual stresses. Nevertheless, modelling and computational effort are still in a less practicable range. In this study a simplified procedure to implement residual welding stresses in continuous large scale members is proposed and the influence on the ultimate limit state of slender members in compression is evaluated for two common structural steel grades. The results showed significant improvements in the utilization of load bearing capacity compared with simplified design methods. The comparatively general approach in this study offers potential for future optimization. T2 - ICRS 2016 - 10th International Conference on Residual Stresses CY - Sydney, Australia DA - 03.07.2016 KW - Stability Design KW - Finit Element Method KW - 2-D Welding Simulation KW - Inherent Strain KW - Plasticity-based Analysis PY - 2016 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-389210 SN - 978-1-94529117-3 SN - 978-1-94529117-6 DO - https://doi.org/10.21741/9781945291173-19 SN - 2474-395X VL - 2 SP - 109 EP - 114 PB - Materials Research Forum LLC CY - Millersville (PA), USA AN - OPUS4-38921 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne A1 - Rhode, Michael A1 - Launert, B. A1 - Dixneit, Jonny A1 - Kannengießer, Thomas A1 - Pasternak, H. ED - Olden, T.-M. ED - Muransky, O. ED - Edwards, L. T1 - Combining sectioning method and X-ray diffraction for evaluation of residual stresses in welded high strength steel components N2 - Residual stresses and distortions in welded I-girders for steel construction are relevant when evaluating the stability of steel beams and column members. The application of high strength steels allows smaller wall thicknesses compared to conventional steels. Therefore, the risk of buckling has to be considered carefully. Due to the lack of knowledge concerning the residual stresses present after welding in high strength steel components conservative assumptions of their level and distribution is typically applied. In this study I-girders made of steels showing strengths of 355 MPa and 690 MPa were welded with varying heat input. Due to the dimension of the I-girders and the complex geometry the accessibility for residual stress measurement using X-ray diffraction was limited. Therefore, saw cutting accompanied by strain gauge measurement has been used to produce smaller sections appropriate to apply X-ray diffraction. The stress relaxation measured by strain gauges has been added to residual stresses determined by X-ray diffraction to obtain the original stress level and distribution before sectioning. The combination of both techniques can produce robust residual stress values. From practical point of view afford for strain gauge application can be limited to a number of measuring positions solely to record the global amount of stress relaxation. X-ray diffraction can be applied after sectioning to determine the residual stresses with sufficient spatial resolution. T2 - ICRS 2016 - 10th International Conference on Residual Stresses CY - Sydney, Australia DA - 03.07.2016 KW - Welding KW - Residual Stress KW - Sectioning Method KW - X-Ray Diffraction KW - Component Testing PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-389206 SN - 978-1-94529117-3 SN - 978-1-94529117-6 DO - https://doi.org/10.21741/9781945291173-28 SN - 2474-395X VL - 2 SP - 163 EP - 168 PB - Materials Research Forum LLC CY - Millersville (PA), USA AN - OPUS4-38920 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pasternak, H. A1 - Launert, B. A1 - Kannengießer, Thomas A1 - Rhode, Michael T1 - Advanced residual stress assessment of plate girders through welding simulation N2 - This article provides an impression on potentials in applying nowadays welding simulation tools in construction design. This is carried out exemplary on plate girders from two structural steel grades. The calculated residual stresses are compared with measurements by sectioning method. It has been repeatedly stated that present Eurocode models fail to approximate the residual stresses. Especially for high strength steel (HSS) only limited information is available on realistic occurring residual stresses in typical I-girders. The investigations are aimed to give further guidance on these values. A few proposals on advanced models are discussed. T2 - MBST 2016 - Modern Building Materials, Structures and Techniques CY - Vilnius, Litunia DA - 26.05.2016 KW - Residual stresses KW - Plate girders KW - I-shape sections KW - High-strength steel KW - Welding simulation PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-392177 UR - http://www.sciencedirect.com/science/article/pii/S1877705817305192 DO - https://doi.org/10.1016/j.proeng.2017.02.013 SN - 1877-7058 IS - 172 SP - 23 EP - 30 PB - Elsevier CY - Amsterdam, Niederlande AN - OPUS4-39217 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A.-K. A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Hodžić, E. A1 - Pastore, S. A1 - Domitner, J. A1 - Rhode, Michael A1 - Sommitsch, C. A1 - Böllinghaus, Thomas T1 - Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure N2 - The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments. KW - Hydrogen KW - Solubility KW - Temperature KW - Tensile loading KW - Analytical calculation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586701 DO - https://doi.org/10.1002/srin.202300493 SN - 1611-3683 SP - 1 EP - 9 PB - Wiley AN - OPUS4-58670 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A A1 - Konert, Florian A1 - Sobol, Oded A1 - Rhode, Michael A1 - Domitner, J A1 - Sommitsch, C A1 - Böllinghaus, Thomas T1 - Enhanced gaseous hydrogen solubility in ferritic and martensitic steels at low temperatures N2 - Metals that are exposed to high pressure hydrogen gas may undergo detrimental failure by embrittlement. Understanding the mechanisms and driving forces of hydrogen absorption on the surface of metals is crucial for avoiding hydrogen embrittlement. In this study, the effect of stress-enhanced gaseous hydrogen uptake in bulk metals is investigated in detail. For that purpose, a generalized form of Sievert's law is derived from thermodynamic potentials considering the effect of microstructural trapping sites and multiaxial stresses. This new equation is parametrized and verified using experimental data for carbon steels, which were charged under gaseous hydrogen atmosphere at pressures up to 1000 bar. The role of microstructural trapping sites on the parameter identification is critically discussed. KW - Hydrogen KW - Thermodynamic modelling KW - Pressure-dependent solubility KW - Steel KW - Trapping PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559307 DO - https://doi.org/10.1016/j.ijhydene.2022.09.109 SN - 0360-3199 VL - 47 IS - 93 SP - 39639 EP - 39653 PB - Elsevier Ltd. AN - OPUS4-55930 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Grimault de Freitas, Tomás A1 - Rhode, Michael A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique N2 - The constantly increasing demand for renewable energy sources leads to the necessity of transporting large amounts of hydrogen. Since pipelines enable a cost-effective way for the distribution of gaseous hydrogen, the interaction of hydrogen and the pipeline materials must be carefully investigated as hydrogen can cause a degradation of the mechanical properties under certain conditions. Especially welds, which are assumed to be more susceptible to the degradation enhanced by hydrogen, are of great interest. The aim of this study is to investigate the effect of gaseous hydrogen on the mechanical properties of an X65 pipeline, and the longitudinal submerged arc welding (SAW) welded joint. The tests are conducted using the hollow specimen technique on two types of specimens: one extracted from the base material (BM) and the other extracted as a cross-weld (CW) specimen consisting of BM and weld seam. The specimens are charged in situ under a pressure of 60 bar and tested using slow strain rate (SSR) tensile tests with a nominal strain rate of 10−5 s−1. The properties obtained of specimens tested in hydrogen atmosphere are compared to the properties of comparable specimen in inert argon atmosphere as a reference. The performed tests showed a decrease of the reduction of area (RA) from 72% in inert atmosphere to 52% in hydrogen atmosphere for the CW specimen and a decrease from 73% in inert atmosphere to 51% for the BM. Metallographic analyses showed the crack initiation between fine-grained heat-affected zone (FGHAZ) and BM for the specimens tested in hydrogen atmosphere as well as for the reference specimens. This leads to the conclusion that the location of the crack initiation does not change due to the presence of gaseous hydrogen. KW - Hydrogen KW - Hollow specimen technique KW - Pipeline KW - SSRT KW - Hydrogen embrittlement KW - Cross-weld specimen PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624658 DO - https://doi.org/10.1007/s40194-025-01953-3 SN - 0043-2288 SN - 1878-6669 VL - 69 IS - 3 SP - 861 EP - 870 PB - Springer CY - Berlin AN - OPUS4-62465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen in Welded Microstructures of T24 Steel: Effect on Mechanical Properties and Corresponding Hydrogen Diffusion N2 - Low-alloyed CrMoV steels, such as T24, are widely used for welded components in fossil power stations due to their excellent creep-strength. Spectacular failure cases in the recent years exhibited severe cracking in T24 welds. The results showed that hydrogen-assisted cracking (HAC) occurring up to 200 degree Celsius cannot be excluded. Hence, a basic understanding is necessary on how hydrogen affects the material properties of welded microstructures. In this regard, each weld microstructure (HAZ and weld metal) has influence on the HAC susceptibility and respective hydrogen diffusion. Thus, the present contribution summarizes different results obtained from experiments with grades T24 (CrMoV alloy) and T22 (CrMo) and thermally simulated HAZ. Tensile tests were conducted with hydrogen charged specimens and compared to hydrogen-assisted stress corrosion cracking results obtained from slow strain rate tests (SSRT) up to 200 degree Celsius. Electrochemical permeation and degassing experiments were performed to identify a particular weld microstructure influence on hydrogen diffusion and trapping (especially in the HAZ). The results showed that T24 base material has improved resistance to hydrogen-assisted degradation/cracking. In contrast, the as-welded HAZ had remarkably increased susceptibility (tesnile tests at hydrogen concentration of 1 to 2 ppm). SSRT experiments confirmed this at elevated temperatures for both the T24 and the T22. Hence, the evaluation of a particular degradation of the mechanical properties should be performed independently for each weld microstructure. In addition, the HAZ showed decreased diffusion coefficients (at room temperature) of approximately one magnitude compared to the base materials. Trapped hydrogen was determined in the T24 at temperatures up to 120 degree Celsius compared to 75 degree Celsius in the T22. This has to be considered in case of changing operational temperatures, e.g. in the case of start-up and shutdown processes of boiler components. T2 - 10th Conference on Trends in Welding Research CY - Tokyo, Japan DA - 11.10.2016 KW - Degradation of Mechanical Properties KW - Hydrogen KW - Creep-resistant Steel KW - Weld Joint KW - Diffusion PY - 2016 AN - OPUS4-37827 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Steffens, B. R. A1 - Böllinghaus, Thomas A1 - Shoales, G. A. A1 - Rhode, Michael ED - Somerday, B. P. ED - Sofronis, P. T1 - Hydrogen dependent material properties of UHSS for aerospace applications N2 - Quantitative investigations of hydrogen dependent properties of aircraft landing gear materials have only scarcely been carried out in the past. They are essential for respective component life time assessments. To better understand the behavior of these landing gear materials in a hydrogen rich environment, specimens were charged in the condition as delivered with known concentrations of hydrogen and then mechanically tested to evaluate the degradation effects. The present contribution is focused on evaluating the hydrogen concentration dependent material properties and the respective fracture topographies of the two investigated steels, and then continued by the comparison of the results with other previously investigated martensitic steels in order to better understand the thresholds for these materials to maintain structural integrity. T2 - International Hydrogen Conference 2016 CY - Jackson Lake Lodge, Moran, WY, USA DA - 11.09.2016 KW - Material properties KW - Hydrogen assisted cracking KW - Degradation KW - Aerospace materials KW - Ultra high strength steels PY - 2017 SN - 978-0-7918-6138-7 DO - https://doi.org/10.1115/1.861387_ch12 SP - 123 EP - 131 PB - ASME CY - New York, USA AN - OPUS4-42504 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schaupp, Thomas A1 - Rhode, Michael A1 - Yahyaoui, Hamza A1 - Kannengießer, Thomas ED - Lippold, J. ED - Böllinghaus, Thomas ED - Norrish, J. ED - Scotti, A. T1 - Hydrogen-assisted cracking in GMA welding of high-strength structural steels using the modified spray arc process N2 - High-strength structural steels are used in machine, steel, and crane construction with yield strength up to 960 MPa. However, welding of these steels requires profound knowledge of three factors in terms of avoidance of hydrogen-assisted cracking (HAC): the interaction of microstructure, local stress/strain, and local hydrogen concentration. In addition to the three main factors, the used arc process is also important for the performance of the welded joint. In the past, the conventional transitional arc process (Conv. A) was mainly used for welding of high-strength steel grades. In the past decade, the so-called modified spray arc process (Mod. SA) has been increasingly used for welding production. This modified process enables reduced seam opening angles with increased deposition rates compared with the Conv. A. Economic benefits of using this arc type are a reduction of necessary weld beads and required filler material. In the present study, the susceptibility to HAC in the heat-affected zone (HAZ) of the high-strength structural steel S960QL was investigated with the externally loaded implant test. For that purpose, both Conv. A and Mod. SA were used with same heat input at different deposition rates. Both conducted test series showed same embrittlement index “EI” of 0.21 at diffusible hydrogen concentrations of 1.3 to 1.6 ml/100 g of arc weld metal. The fracture occurred in the HAZ or in the weld metal (WM). However, the test series withMod. SA showed a significant extension of the time to failure of several hours compared with tests carried out with Conv. A. KW - High-strength steel KW - GMA welding KW - Diffusible hydrogen KW - Implant test KW - Fractography PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-515330 DO - https://doi.org/10.1007/s40194-020-00978-0 SN - 1878-6669 SN - 0043-2288 VL - 64 IS - 12 SP - 1997 EP - 2009 PB - Springer CY - Berlin Heidelberg AN - OPUS4-51533 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Influence of Experimental Conditions and Calculation Method on Hydrogen Diffusion Coefficient Evaluation at Elevated Temperatures N2 - Hydrogen-assisted cracking (HAC) represents a significant failure risk for (high strength) creep resistant low-alloyed steel components in fossil-fired power plant applications at temperatures of up to and above 200 °C. This particularly applies to respective start-up and shut-down processes associated with alternating service-conditions in terms of load flexible power plants. For quantitative determination of localized crack critical hydrogen concentrations, the temperature dependent hydrogen diffusion coefficients have to be determined as exactly as possible. However, available literature provides a wide range of hydrogen diffusion coefficients for low alloyed steels with similar microstructures. Additionally, the available diffusion data seem not to be very reliable and their scatter increases with decreasing temperature. One reason is that the experimental boundary conditions can have a major impact on the determination of respective effective diffusion coefficients. Hence, the scope of this study is to evaluate the influence of the experimental boundary conditions on the derived diffusion coefficients. In addition, different methods for calculating diffusion coefficients are discussed. To elucidate such influences and to draw a line to practical application, the diffusion and trapping behavior in the creep resistant steel 7CrMoVTiB10 10 has been studied. For such purpose, hydrogen charged specimens were isothermally degassed at different temperatures using carrier gas hot extraction (CGHE). Based on experimental data, a numerical model has been developed by which the hydrogen transport behavior and the respective hydrogen distribution during CGHE can be assessed. It is demonstrated that the specimen heating rate has a large influence on the calculated diffusion coefficients under assumption of isothermal degassing which elsewhere has been underestimated in the assessment of diffusion data in creep-resistant steels. The numerical results suggest that calculation methods for diffusion coefficients are limited if compared to experimental results. It also turned out that the sample preparation time before CGHE can enormously influence determined diffusion coefficients. Consequently, non-homogeneous hydrogen concentration profiles have to be anticipated in the simulations to arrive at characteristic effusion curves consistent to respective CGHE experiments. In turn, validated diffusion coefficients are now available for the low-alloyed Cr-Mo-V steel, which can be helpful to calculate appropriate hydrogen removal heat treatment procedures. T2 - Project Meeting CAStLE CY - Colorado Springs, CO, USA DA - 07.09.2016 KW - Hydrogen KW - Diffusion Coefficient KW - Elevated Temperatures KW - Numerical Modeling KW - Carrier Gas Hot Extraction PY - 2016 AN - OPUS4-37408 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Influence of experimental conditions and calculation method on hydrogen diffusion coefficient evaluation at elevated temperatures N2 - Hydrogen-assisted cracking (HAC) represents a significant failure risk for (high strength) creep resistant low-alloyed steel components in fossil-fired power plant applications at temperatures of up to and above 200 °C. This particularly applies to respective start-up and shut-down processes associated with alternating service-conditions in terms of load flexible power plants. For quantitative determination of localized crack critical hydrogen concentrations, the temperature dependent hydrogen diffusion coefficients have to be determined as exactly as possible. However, available literature provides a wide range of hydrogen diffusion coefficients for low alloyed steels with similar microstructures. Additionally, the available diffusion data seem not to be very reliable and their scatter increases with decreasing temperature. One reason is that the experimental boundary conditions can have a major impact on the determination of respective effective diffusion coefficients. Hence, the scope of this study is to evaluate the influence of the experimental boundary conditions on the derived diffusion coefficients. In addition, different methods for calculating diffusion coefficients are discussed. To elucidate such influences and to draw a line to practical application, the diffusion and trapping behavior in the creep resistant steel 7CrMoVTiB10 10 has been studied. For such purpose, hydrogen charged specimens were isothermally degassed at different temperatures using carrier gas hot extraction (CGHE). Based on experimental data, a numerical model has been developed by which the hydrogen transport behavior and the respective hydrogen distribution during CGHE can be assessed. It is demonstrated that the specimen heating rate has a large influence on the calculated diffusion coefficients under assumption of isothermal degassing which elsewhere has been underestimated in the assessment of diffusion data in creep-resistant steels. The numerical results suggest that calculation methods for diffusion coefficients are limited if compared to experimental results. It also turned out that the sample preparation time before CGHE can enormously influence determined diffusion coefficients. Consequently, non-homogeneous hydrogen concentration profiles have to be anticipated in the simulations to arrive at characteristic effusion curves consistent to respective CGHE experiments. In turn, validated diffusion coefficients are now available for the low-alloyed Cr-Mo-V steel which might be helpful to calculate appropriate hydrogen removal heat treatment procedures, for instance. T2 - International Hydrogen Conference - Material Performance in Hydrogen Environments CY - Jackson Lake Lodge, Moran, Wyoming, USA DA - 11.09.2016 KW - Hydrogen diffusion KW - Elevated temperatures KW - Welding KW - Creep-resistant steel KW - Numerical modeling KW - Calculation PY - 2016 AN - OPUS4-37403 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Münster, C. A1 - Mente, Tobias A1 - Rhode, Michael A1 - Böllinghaus, Thomas ED - Sommitsch, C. ED - Enzinger, N. ED - Mayr, P. T1 - Modelling of hydrogen diffusion in power station steels and influence of experimental conditions on the determination of diffusion coefficients N2 - In the field of modelling hydrogen assisted cracking (HAC) phenomenon, hydrogen diffusivity is an important input parameter for numerical simulation. In terms of hydrogen diffusion coefficients, they have great impact on realistic assessment of the evolution of possible crack critical hydrogen concentrations. In addition, the chemical compositions of steels can have a strong effect on hydrogen diffusion. Unfortunately, literature provides a wide range of available hydrogen diffusion coefficients even for similar microstructures and equal temperatures. The scattering of the data can lead to significant deviations in the results of simulating the evolving hydrogen concentrations due to hydrogen uptake (by fabrication or service). Thus, the application of such data to crack-models or for component life tie predictions can be realized up to the present only by considering envelope curves of such value, corresponding to a work or bench case scenario, respectively. For improved reliability of numerical simulaitons, it is necessary to minimize the mentioned deviation of these data. Hence, this work focuses on the validation of hydrogen diffusion coefficients obtained from permeation experiments at room temperature. Two baintic steels with different alloying concepts were investigated, the creep-resistant 7CrMoVTiB10-10 and the reactor pressure vessel grade 20MnMoNi4-5. A numerical model is presented for simulation of the corresponding hydrogen diffusion during permeation experiments using the finite element software ANSYS. Three different diffusion coefficients (obtained from different common calculation methods) are considered and compared to numerical results. The vases of thes calculation methods are permeation transients which are a direct measure for hydrogen. The results of the simulated hydrogen diffusion coefficients show that only one procedure for calculation of diffusion coefficitnes is suitable in comparision to the experimental values. Thus, it is suggested to use this method for analysis of experimental results in case of hydrogen diffusion during permeation experiments. Furthermore, this work supplies validated values for the hydrogen diffusion coefficients of both steel grades. KW - Hydrogen KW - Diffusion Coefficient KW - Numerical Simulation KW - Permeation KW - Creep-resistant Steel KW - Pressure Vessel Steel PY - 2016 SN - 978-3-85125-490-7 SN - 2410-0544 SP - 435 EP - 457 PB - Technische Universität Graz CY - Graz AN - OPUS4-38917 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - THES A1 - Rhode, Michael T1 - Hydrogen Diffusion and Effect on Degradation in Welded Microstructures of Creep-resistant Low-alloyed Steels N2 - Low-alloyed heat-resistant steels have a fundamental contribution to the currently applied steel grades in pressurized and temperature loaded components like membrane walls(water walls)or pressure vessels. Here, the main advantages of the low-alloy concept can be used in terms of superior high temperature mechanical properties, workability and decreased amounts of expensive alloy elements. The main challenge for the future is to further increase the power plant thermal efficiency independent of the type of power plant concept, i.e. fossil-fired or nuclear power plant, where the material selection can directly affect reduction of CO2 emissions. In power plant design, welding is the most applied manufacturing technique in component construction. The necessary weld heat input causes metallurgical changes and phase transitions in the heat affected zone (HAZ) of the base materials and in the deposited weld metal. The weld joint can absorb hydrogen during welding or in later service - This absorption can cause degradation of mechanical properties of the materials, and in certain loading conditions, hydrogen-assisted cold cracks can occur. This cracking phenomenon can appear time delayed due to the temperature dependency of the hydrogen diffusion and the presence of a “critical” hydrogen concentration. Additionally, each specific weld microstructure shows a certain hydrogen diffusion and solubility that contribute to susceptibility of the cracking phenomenon. Therefore hydrogen cannot be neglected as possible failure effect, which was identified recently in the case of T24 creep-resistant tubeto-tube weld joints. It is necessary to identify and assess the hydrogen effect in weld joints of low-alloyed steel grades for to improve further early detection of possible failures. For each specific weld joint microstructure, it is necessary to separate the interdependencies between mechanical load and the hydrogen concentration. The diffusivity and solubility must be considered to identify hydrogen quantities in the material at any given time. In this case, the effects of mechanical loading were dealt with independently. For the characterization of the mechanical properties, hydrogen charged tensile specimens were investigated for the base materials and thermally simulated HAZ microstructures. The hydrogen diffusion was characterized with the permeation technique at room temperature and at elevated temperature ranges up to 400°C - It was investigated by interpreting the hydrogen effusion behavior with carrier gas hot extraction technique (CGHE). For realistic determination of the hydrogen diffusion coefficients, an improved method was developed encompassing accelerated specimen heating and hydrogen determination via mass spectrometer (MS). Simultaneously, the corresponding temperature dependent trapped and total hydrogen concentrations were determined. The determined experimental results showed increased susceptibility to the hydrogen affected degradation of the HAZ compared to the base material, which is independent of the investigated alloy composition. In particular, the martensitic coarse grain HAZ is the most susceptible microstructure to hydrogen-affected degradation. The results of the tensile tests allowed the definition of consistent microstructure specific failure criteria (envelope curves) versus quantified hydrogen concentrations for the reactor pressure vessel 16MND5 steel (20MnMoNi-5-5) and the creep-resistant T24 steel (7CrMoVTiB10-10). The procedure of quantifying hydrogen concentrations in HAZ microstructures is novel and supports a new method of analysis for hydrogen degradation effects. Further investigations with the T22 steel (10CrMo9-10), as compared to the creep-resistant T24 steel (7CrMoVTiB10-10), confirmed the beneficial effect of Vanadium as an alloying element to improve the resistance to degradation. In general, Mn-Mo-Ni base material grades show a higher resistance compared to Cr-Mo steels that do not include Vanadium alloying. The investigations showed the decreased diffusion coefficient of the HAZ microstructure compared to the base material microstructure. This is caused by the stronger trapping effects that are present which simultaneously increase the hydrogen solubility as well. In general, trapping effects above 100°C are negligible. It is noted that after testing the T24 grade, these trapping effects were observed above 100°C and must be considered. At elevated temperatures, the calculated hydrogen diffusion coefficients are sometimes greater than those in literature. This is primarily due to the unique applied specimen heating procedure resulting in a varied hydrogen effusion from the specimen. The significance of the obtained results can be characterized in three perspectives. First, the direct comparison of the degradation was possible in terms of microstructure-specific hydrogen effects on the mechanical properties. Second, consistent failure criteria were established to quantify degradation vs. the hydrogen concentration. Third, the determination of more accurate hydrogen diffusion coefficients is now available. From a scientific point of view, important contributions were made to further interpret the hydrogen effects on the macroscopic mechanical properties, with respect to the alloy composition and the microstructure. From a procedural standpoint, the mentioned deviation in the elevated temperature diffusion coefficients can be caused by the calculation method. This can be an explanation for the reported data scatter in the references. In terms of an economic view, the presented experimental results contribute to a safe and reliable weld workability of the steel grades. Thus, the identified temperature levels of hydrogen trapping can be applied in the definition of minimum preheat, interpass or postheat temperatures. In addition, recommendations for suitable dehydrogenation heat treatment (DHT) procedures, with accurate temperature values and holding times, can be derived from these results. In the future, the application of the mechanical and diffusion data is intended to support numerical analysis methods to provide an improved prediction of hydrogen effects on material degradation in weld microstructures. N2 - Niedriglegierte warmfeste Mn-Mo-Ni und Cr-Mo-V Stähle bilden einen wesentlichen Beitrag gegenwärtig eingesetzter Werkstoffe für druck- und temperaturführende Komponenten im Kraftwerksbau. Dies sind beispielsweise Kesselkomponenten wie Membranwände und Druckbehälter. Dabei kommen die Hauptmerkmale dieser Werkstoffgruppe (sehr gute mechanische Hochtemperatureigenschaften, Verarbeitbarkeit und niedrige Legierungskosten) zum Tragen. Die weitere Erhöhung des thermischen Wirkungsgrades ist dabei das wichtigste Ziel, der Werkstoffauswahl für die nähere Zukunft, unabhängig vom Kraftwerkskonzept. Dies trifft jedoch im Besonderen bei fossil-befeuerten Kraftwerken im Rahmen der notwendigen Reduzierung der CO2 Emissionen zu. Die schweißtechnische Komponentenfertigung ist dabei das maßgebliche Fertigungsverfahren. Das Einbringen der Schweißwärme bedingt dabei metallurgische und Gefügeveränderungen in der wärmebeeinflussten Zone des Grundwerkstoffes (WEZ) als auch im niedergeschmolzenen Schweißgut. Die Schweißverbindung kann dabei zusätzlich während oder nach dem Schweißen Wasserstoff aufnehmen. Wasserstoff hat dabei eine degradierende Wirkung auf die mechanischen Eigenschaften, die sich im Worst-Case als wasserstoffunterstützte Kaltrisse zeigen, dies vor allem auch zeitverzögert (delayed cracking) durch die temperaturabhängige Wasserstoffdiffusion. Dabei zeigt jede Schweißmikrostruktur spezifische Wasserstoffdiffusions- und Lösungscharakteristika. Die Degradation ist daher als eine Kombination sich gegenseitig beeinflussender Faktoren aus lokaler Wasserstoffkonzentration, Mikrogefüge und mechanischer Beanspruchung zu sehen. Wie aktuelle Schadensfälle in der jüngeren Vergangenheit belegten (Rissbildung bei Schweißnähten an T24 Rohr-Rohr-Verbindungen), ist Wasserstoff dabei eine potentiell zu berücksichtigende Schadensursache. Zur weiterführenden Früherkennung möglicher Schäden, ist es daher notwendig, den gefügespezifischen Wasserstoffeffekt in Schweißnähten an niedriglegierten Stählen festzustellen und zu bewerten. Die Interdependenz der mechanischen Beanspruchung und des Verbleibens einer potentiell degradierenden Wasserstoffkonzentration muss dabei für jedes Gefüge separiert werden. Daher wurden für die Charakterisierung der mechanischen Eigenschaften gefügespezifische Untersuchungen an wasserstoffbeladenen Zugproben aus Grundwerkstoffen und thermisch simulierten WEZ Gefügen untersucht. Das Diffusionsverhalten wurde mit der elektrochemischen Permeationsmethode bei Raumtemperatur und über die Interpretation des Wasserstoffeffusions-verhaltens mittels Trägergasheißextraktion bei erhöhten Temperaturen bis 400°C untersucht. Zur realistischen Abbildung des Diffusionsverhaltens, wurde dabei eine optimierte Prozedur aus Probenaufheizung und Wasserstoffeffusion entwickelt. Diese wurde zusätzlich auf ein Wasserstoffmessgerät mit gekoppeltem Massen-spektrometer (MS) übertragen. Gleichzeitig, wurden die korrespondierende getrappte, sowie die Gesamtwasserstoff-konzentration bestimmt. Die Ergebnisse zeigten, dass die WEZ eine generell erhöhte Anfälligkeit für die Degradation besitzt (im Gegensatz zum Grundwerk-stoff), unabhängig von der verwendeten Legierungsroute. Dabei nimmt die martensitische Grobkornzone die Stellung als anfälligste Mikrostruktur ein. Aus den gewonnenen Daten, konnten erstmals durchgängige gefügespezifische Kriterien(Hüllkurven) für das Versagen mit quantifizierbaren Wasserstoffkonzentrationen generiert werden. Dazu erfolgten Untersuchungen an Mn-Mo-Ni legierten Stählen (16MND5 und 20MND5 / 20MnMoNi5-5) sowie an kriechfesten Stählen T24 (7CrMoVTiB1010) und T22 (10CrMo9-10). Generell, zeigten Mn-Mo-Ni Grundwerk-stoffe eine bessere Beständigkeit als Cr-Mo(-V) Stähle. Im Fall des Cr-Mo-V Legierungskonzeptes, konnte zusätzlich die positive Wirkung von Vanadium als Legierungselement zur Erhöhung der Beständigkeit gegenüber einer Degradation bestätigt werden. Die Untersuchungen des Diffusions- und Lösungs-vermögens zeigten, dass die WEZ generell niedrigere Diffusionskoeffizienten besitzt als der Grundwerk-stoff. Dies wird durch stärkeres Trapping des Wasserstoffs beeinflusst und steigert dabei die Lösungs-fähigkeit der Mikrostruktur. Oberhalb von 100°C konnte dabei kein nennenswertes Trapping festgestellt werden, außer im Fall des T24 infolge der Zulegierung von Vanadium. Unterhalb von 100°C, zeigte sich ein deutlicher Abfall der Diffusion infolge des weiter ansteigenden Trappings. Für den betrachteten Temperatur-bereich wurden dabei effektive Wasserstoffdiffusions-koeffizienten berechnet, die zum Teil höher liegen, im Vergleich zu Literaturwerten. Dies liegt zum großen Teil in der optimierten Aufheizprozedur der Proben begründet und, daran gekoppelt, der beschleunigten Wasserstoffeffusion. Die weiterführende Bedeutung der Ergebnisse liegt in drei Bereichen begründet. Erstens, besteht jetzt die Möglichkeit der quantifizierbaren Vergleichbarkeit des gefüge-spezifischen Wasserstoff-einflusses auf die Degradation. Zweitens, wurden aus den experimentellen Daten, Kriterien für das Versagen für der spezifischen Schweißnahtgefüge abgeleitet. Drittens, stehen realistischere Diffusionskoeffizienten für eine Vielzahl von Schweißnahtgefügen zur Verfügung. Aus wissenschaftlicher Sicht ergeben sich wichtige Beiträge zur Interpretation des Wasserstoffeinflusses auf die makroskopischen mechanischen Eigenschaften hinsichtlich der Legierung bzw. Phasenzusammensetzung, wie oben angeführt. Weiterhin konnte gezeigt werden, dass Berechnungsalgorithmen in Kombination mit bestimmten experimentellen Randbedingungen, großen Einfluss auf die effektiven Wasserstoffdiffusions-koeffizienten haben. Dies kann speziell bei erhöhten Temperaturen zu Abweichungen führen, die einen weiteren Ansatz zur Erklärung (der in der Literatur) genannten Streubänder ergeben. Aus ökonomischer Sicht leisten die präsentierten Ergebnisse Beiträge zur sicheren und zuverlässigen Verarbeitung der Werkstoffe. So können anhand der identifizierten Temperaturstufen des Wasserstofftrappings Mindestvorwärm-, Zwischenlagen- bzw. Nachwärmtemperaturen für das Wasserstoffarmglühen identifiziert werden. Die Verwendung der Diffusionskoeffizienten ermöglicht zusätzlich die Abschätzung bzw. Anpassung von notwendigen Haltezeiten. Für die weitere Zukunft ist die Einbindung der mechanischen Daten in vorhandene Modelle zur numerischen Simulation und der verbesserten Vorhersage wasserstoffunterstützter Degradation von Schweißmikrostrukturen vorgesehen. T3 - BAM Dissertationsreihe - 148 KW - Hydrogen KW - Degradation of Mechanical Properties KW - Diffusion KW - Creep-resistant Steels KW - Welding PY - 2016 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-374027 SN - 978-3-9817853-3-3 SN - 1613-4249 VL - 148 SP - 1 EP - 302 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-37402 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Rhode, Michael A1 - Wandtke, Karsten A1 - Irfan, Muhammad Dary A1 - Kannengiesser, Thomas T1 - Hydrogen diffusion in thick-walled S690 saw joints: part 1—experimental determination of microstructure-dependent diffusion coefficients N2 - High-strength low-alloyed steel S690 is widely used in heavy-duty applications, such as structural components, mobile cranes, and industrial plant construction, owing to their high strength and weldability. However, thick-plate submerged arc welding (SAW) can introduce elevated hydrogen levels and residual stresses that promote time-delayed hydrogen-assisted cold cracking (HACC). Accurate, microstructure-specific diffusion data are scarce, limiting predictive HACC assessments. This study presents an experimental determination of hydrogen diffusion coefficients (DH) in two S690 variants: thermomechanically rolled (S690MC) and quenched and tempered (S690Q). Multi-layer SAW welds were produced from 30 mm thick plate material at three heat input levels, and diffusion membranes were extracted from weld metal (WM), heat-affected zone (HAZ), and base material (BM). Hydrogen permeation tests, conducted in accordance with DIN En ISO 17081, yielded flux curves normalized in time from which DH was derived using the inflection-point method. At room temperature, DH values ranged from 6 × 10−5 mm2/s to 9 × 10−5 mm2/s across all regions and heat inputs, with no significant difference between S690MC and S690Q. Weld metal exhibited marginally lower DH, attributed to enhanced hydrogen trapping, while base material measurements showed greater variability. These microstructure-resolved diffusion coefficients add quantitative data for modern S690 SAW welds and provide internally consistent input parameters for the numerical simulations presented in part 2. The results support improved parameterization for subsequent assessments of HACC risk through the optimization of welding parameters. KW - Hydrogen assisted cracking KW - Submerged arc welding KW - Diffusion KW - Electrochemical permeation KW - Microstructure PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655711 DO - https://doi.org/10.1007/s40194-026-02400-7 SN - 0043-2288 SP - 1 EP - 15 PB - Springer Science and Business Media LLC AN - OPUS4-65571 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Rhode, Michael A1 - Wandtke, Karsten A1 - Irfan, Muhammad Dary A1 - Kannengiesser, Thomas T1 - Hydrogen diffusion in thick-walled S690 SAW joints: part 2 – predictive modeling of heat input and microstructure influence N2 - High-strength low-alloy (HSLA) steels such as S690 are widely employed in thick-walled welded structures, where hydrogen-assisted cold cracking (HACC) remains a persistent concern. While microstructure-specific hydrogen diffusion coefficients (DH) for weld metal (WM), heat-affected zone (HAZ), and base material (BM) were experimentally established in Part 1 of this study, their quantitative influence on hydrogen accumulation and effusion has not yet been fully clarified. This work presents a transient, spatially resolved numerical model for simulating hydrogen transport in multi-pass submerged arc welds. The model integrates experimentally determined DH values with realistic thermal cycles and temperature-dependent boundary conditions. Developed in Python, the simulation tool is purpose-built for hydrogen diffusion in welded joints. It offers a focused, transparent alternative. It offers a focused, transparent alternative to general-purpose finite element platforms. Parametric analyses demonstrate that, although the diffusion coefficients vary by up to 50%, their impact on overall hydrogen retention is minor. In contrast, plate thickness, bead geometry, cooling time (t₈/₅), and interpass temperature exert a dominant influence on hydrogen distribution. Despite clear microstructural differences between the thermomechanically rolled (S690MC) and quenched and tempered (S690Q) variants, including opposite HAZ hardness responses (softening in S690MC, hardening in S690Q) in the (pen)ultimate weld bead, the simulations confirm that their diffusion behavior and hydrogen solubility are closely aligned. Consequently, differences in DH and solubility exert only a minor influence on hydrogen retention compared to thermal exposure and joint geometry. These findings support the interchangeable use of both steel grades in terms of HACC risk due to hydrogen diffusion kinetics under comparable welding conditions. KW - Hydrogen assisted cracking KW - Numerical simulation KW - Diffusion KW - Submerged arc welding PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655721 DO - https://doi.org/10.1007/s40194-026-02395-1 SN - 0043-2288 SP - 1 EP - 16 PB - Springer Science and Business Media LLC AN - OPUS4-65572 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Determination, Assessment and Quantification of Hydrogen in Multi-pass / Multi-layer Weld Joints by Adapted ISO 3690 Samples - DEAQuade - N2 - High-strength, low-alloy (HSLA) structural steels, such as S690 and higher grades, are used in numerous applications, enabling sustainable, lightweight structural construction. However, the welded joints of these steels can be susceptible to hydrogen-assisted cold cracking (HACC), especially in the hardened weld metal (WM) or heat-affected zone (HAZ). HACC in high-strength welds basically involves a critical combination of local, mutually dependent parameters consisting of: (1) a crack-critical microstructure; (2) sufficiently high mechanical stress; and (3) a diffusible hydrogen concentration (HD). In this context, thick-walled steel weld joints typically involve multi-layer welding with several passes. This leads to an effective, empirically known reduction in the global HD in the weld seam. This reduction is due to the repeated reheating of subsequently welded beads or layers, which reduces the local HD in the individual weld beads or layers. However, this has not yet been adequately quantified or described. Bead-on-plate tests, such as ISO 3690, cannot correctly reproduce the local HD distribution in individual welding passes (and thus, the global HD in the entire seam). Therefore, these tests lead to an extremely conservative evaluation of hydrogen ingress and the potential for "self-reduction" of HD due to increased interpass temperature during multi-layer welding, which has not yet been adequately addressed in the literature. Ideally, the local HD in each pass and the global (average) HD of the multi-layer weld would be known immediately after welding. For this reason, the study proposes an approach to address the local, track-, and layer-dependent, as well as global, hardness (HD) of multi-layer welds via a modified ISO 3690 test. To this end, representative welding parameter combinations for selected practical welding processes (e.g., SAW, GMAW, or SMAW) will be carried out as conventional bead-on-plate samples. These samples will be systematically extended by an increasing number of welding passes. Several sample series with an increasing number of beads or layers will be examined. Additionally, the initial HD is varied by methods such as targeted shielding gas variation (e.g., addition of hydrogen in GMAW) or moistened flux/coating (e.g., SAW/SMAW). Based on experimental data (temperature field measurements during welding and determination of temperature-dependent HD coefficients), a numerical hydrogen diffusion model is created. This model calculates the local HD (in the beads) and the HD across the weld cross-section. Additional variation calculations represent heat transfer conditions that were not recorded experimentally and their influence on HD distribution. Finally, we investigate the potential use of the modified ISO 3690 multi-layer geometry for application cases such as (1) predicting the effectiveness and necessity of hydrogen removal heat treatment procedures for given welding parameter sets and (2) extending the HD classification definition (e.g., allowing HD10 use for HSLA steels with RP0.2 > 690 MPa instead of HD5). Finally, an international round robin should be initiated once the concept has been successfully confirmed and verified. T2 - IIW Intermediate Meeting, Com. II-A CY - Bangkok, Thailand DA - 17.03.2026 KW - Hydrogen assisted cracking KW - Multi-pass welding KW - Diffusion KW - Cold cracking test PY - 2026 AN - OPUS4-65716 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Praktikable Prüfung der Wasserstoffverteilung in Mehrlagenschweißungen in Anlehnung an die DIN EN ISO 3690 N2 - Das Forschungsvorhaben adressiert eine zentrale Lücke und damit einhergehende Einschränkung für geschweißte hochfeste Werkstoffe in der aktuellen Normung: Die DIN EN ISO 3690 erlaubt ausschließlich die Bestimmung des diffusiblen Wasserstoffs in einlagigen Prüfraupen und bildet damit die realen Bedingungen in mehrlagigen Schweißnähten hochfester Stähle nicht ab. Durch das mehrfache wiederholte Aufwärmen wird die eingebrachte Wasserstoffkonzentration deutlich unter die konservativen, einlagigen Prüfraupen bereits während des Schweißens abgesenkt. Hierzu fehlt jedoch eine einfache, experimentelle Methoden, um die tatsächliche lokale lagenabhängige bzw. globale Wasserstoffverteilung quantifizieren zu können. Das Vorhaben entwickelt daher erstmals eine Versuchsmethodik, der reale Diffusions- und Entgasungsbedingungen von Mehrlagenschweißungen experimentell reproduziert. Dadurch werden die Nachteile der ISO 3690 (einlagige Prüfraupe, konservative Bewertung) aufgehoben und mit dem Hauptvorteil (robuste, einfache Handhabung) kombiniert. Durch gezielte Variation von Wärmeführung, Zwischenlagentemperaturen und Wasserstoffangebot werden lokale und globale Wasserstoffverteilungen quantifiziert. Ergänzt durch ein numerisches Diffusionsmodell entsteht ein skalierbares Bewertungswerkzeug, das die experimentellen Daten generalisiert und auf reale Schweißnähte überträgt. Die Ergebnisse ermöglichen: (1) eine realitätsnahe Bewertung verbleibender Wasserstoffgehalte, Kaltrisssicherheit, damit die (2) die mögliche Ausweitung der HD Klassifizierung hochfester Schweißzusätze, und (3) die Beurteilung der Effektivität und Notwendigkeit von Wärmenachbehandlungs-maßnahmen (wie „Wasserstoffarmglühen“). T2 - Sitzung des NA 092-00-05 GA Gemeinschaftsarbeitsausschuss NAS/NMP: Zerstörende Prüfung von Schweißverbindungen (DVS AG Q 4/Q 4.1) CY - Berlin, Germany DA - 24.03.2026 KW - Schweißen KW - Wasserstoff KW - ISO 3690 KW - Prüfung KW - Mehrlagennaht PY - 2026 AN - OPUS4-65784 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -