TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Böhning, Martin A1 - Goering, Harald T1 - Radiation induced structural changes of (U)HMW polyethylene with regard to its application for radiation shielding N2 - The special properties of high molecular weight polyethylene (HMW-PE) and ultra high molecular weight polyethylene (UHMW-PE) result basically from their extreme chain lengths and their high degree of crystallinity. As high-performance polymers, they are used for a variety of applications. UHMW-PE in particular is often utilized for endoprothesis (due to its excellent slip and wear properties) and due to its high hydrogen content as a neutron moderator in casks for storage and transport of radioactive materials. To prepare the material for instance for its use as a total joint replacement, it is exposed to radiation for several reasons, such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better chemical stability. To be applicable for long term radiation shielding purposes for instance over a period of 40 years, PE has to withstand any type of degradation affecting safety relevant aspects. The scope of our investigation comprises an estimation of the radiation impact on the molecular and supra molecular structure of two types of PE and to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermo Gravimetric Analysis (TGA). Additionally FT-IR spectroscopy as well as density and gas sorption measurements were carried out. Due to the poor solubility of HMW-PE and UHMW-PE, some classical analytical techniques are not applicable. But TA-methods represent a feasible approach to detect structural and morphological features of these materials as well as changes caused by external influences, such as thermal treatment and/or irradiation. With the combination of the applied TA-techniques it is possible to distinguish between crosslinking and degradation. T2 - PATRAM 2010 - 16th International symposium on the packaging and transport of radioactive materials CY - London, UK DA - 2010-10-03 PY - 2010 SP - 1 EP - 8 (T25/Paper 173) AN - OPUS4-24621 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Stark, Wolfgang T1 - Tieftemperaturverhalten von Elastomerdichtungen - Eigenschaftsbestimmung für den Einsatz in Transport- und Lagerbehältern für radioaktive Stoffe N2 - Die Messung des dynamischen Speichermoduls mit der Dynamisch-Mechanischen-Analyse ermöglicht einen schnellen Überblick über das temperaturabhängige Verhalten von elastomeren Dichtungsmaterialien. Ein direkter Rückschluss von der so ermittelten Glasübergangstemperatur Tg auf die Versagenstemperatur einer Dichtung ist aber ohne zusätzliche Messungen bisher nicht möglich. Mit den Ergebnissen des Druckverformungsrestes DVR und des DVRDMA ist eine ge-nauere Beschreibung der Tieftemperatureigenschaften und dadurch der Funktion von elastomeren Dichtungsmaterialien möglich. Messungen ergeben beispielsweise, dass sich das EPDM bei einer Temperatur von -40 °C laut der Dynamisch Mechanischen Analyse noch im gummielastischen Bereich befindet. Die DVRDMA-Werte zeigen eine Rückstellung um mehr als 40 % der Ausgangsdeformation in wenigen Minuten. Mit derart detailliert bestimmten Eigenschaften lassen sich Rückschlüsse auf einsatzspezifische Anforderungen wie z. B. die Dichtwirkung in Abhängigkeit von Betriebstemperatur und mechanischer Belastungsgeschwindigkeit ziehen, so dass je nach Einsatzbedingungen für die Dichtungen eine geeignete Materialauswahl getrof-fen werden kann. T2 - Jahrestagung Kerntechnik 2010 CY - Berlin, Deutschland DA - 2010-05-04 KW - Dichtungen KW - Elastomere KW - Tieftemperaturverhalten PY - 2010 IS - Sektion 5 / 503 SP - 1 EP - 4 CY - Berlin AN - OPUS4-21272 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Low temperature properties of rubber seals T2 - 9th Fall rubber colloquium CY - Hannover, Germany DA - 2010-11-03 KW - Dichtungen KW - Elastomere KW - Tieftemperaturverhalten PY - 2010 SN - 978-3-9814076-0-0 SP - 175 EP - 178 AN - OPUS4-22331 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Tieftemperaturverhalten von Elastomerdichtungen T2 - Jahrestagung Kerntechnik CY - Berlin, Germany DA - 2010-05-04 PY - 2010 AN - OPUS4-20684 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Low temperature properties of rubber seals T2 - 9. Rubber Fall Colloquium CY - Hanover, Germany DA - 2010-11-03 PY - 2010 AN - OPUS4-21207 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Elastomerprüfung in der Kälte, DVR und Glasübergang T2 - Treffen der Deutschen Kautschukgesellschaft e. V. Bezirksgruppe Ost CY - Berlin, Germany DA - 2010-05-27 PY - 2010 AN - OPUS4-21208 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Böhning, Martin A1 - Goering, Harald A1 - Wolff, Dietmar T1 - Detection of structural changes of (U)HMW-PE induced by gamma irradiation T2 - 14th International conference "Polymeric materials" CY - Halle (Saale), Germany DA - 2010-09-15 PY - 2010 SN - 978-3-86829-282-4 SP - 1 EP - 6 PB - Druck-Zuck GmbH CY - Halle / Saale AN - OPUS4-21997 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - von der Ehe, Kerstin A1 - Wolff, Dietmar A1 - Völzke, Holger A1 - Stark, Wolfgang T1 - Understanding the low temperature properties of rubber seals T2 - PATRAM 2010 CY - London, England DA - 2010-10-03 PY - 2010 AN - OPUS4-21502 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - A new method to evaluate the low temperature function of rubber sealing materials N2 - A new method for the evaluation of the low temperature properties of rubber materials is presented. The method emulates the standardized compression set measurement, which is frequently used for sealing materials, but can be performed within a considerably shorter time. The results are compared with the standard test and found to be qualitatively the same. Slight differences are discussed on the basis of the differences in the measurement procedures. Further data evaluation is done by fitting functions to describe the material behaviour. KW - Sealing material KW - Elastomer KW - Compression set KW - Dynamic mechanical analysis KW - Low temperature behaviour PY - 2010 U6 - https://doi.org/10.1016/j.polymertesting.2010.07.006 SN - 0142-9418 VL - 29 IS - 7 SP - 815 EP - 823 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-21914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - von der Ehe, Kerstin A1 - Wolff, Dietmar A1 - Völzke, Holger A1 - Stark, Wolfgang T1 - Understanding the low temperature properties of rubber seals N2 - Rubbers are widely used as main sealing materials for containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. The save encapsulation of the radioactive container inventory has to be guaranteed according to legislation and appropriate guidelines for long term storage periods as well as down to temperatures of -40 °C during transport. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of rubbers are strongly temperature dependent. At low temperatures this is caused by the rubber-glass transition (abbr. glass transition). During continuous cooling the material changes from rubber-like entropy-elastic to stiff energy-elastic behaviour, that allows nearly no strain or retraction, due to the glass transition. Hence rubbers are normally used above their glass transition but the minimum working temperature limit is not defined precisely, what can cause problems during application. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the standard tests a faster technique was developed. Additionally, the breakdown temperature of the sealing function of complete O-ring seals is measured in a component test setup to compare it with the results of the other tests. The experimental setup is capable of measuring the leakage rate at low temperatures by the pressure rise method. A fluorocarbon rubber (FKM) was selected for this investigation as it is often used for radioactive waste containers. Some materials (seals and test sheets) were purchased from a commercial seal producer and some materials were compounded and cured at BAM in form of rubber sheets. T2 - PATRAM 2010 - 16th International symposium on the packaging and transport of radioactive materials CY - London, UK DA - 2010-10-03 KW - Dichtungen KW - Elastomere KW - Tieftemperaturverhalten PY - 2010 SP - 1 EP - 7 (Session T41 / Paper 169) AN - OPUS4-23887 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -