TY - CONF A1 - Wolff, Dietmar A1 - Jaunich, Matthias A1 - Stark, Wolfgang T1 - Investigating the performance of rubber seals at low temperatures N2 - Rubbers are widely used as main sealing materials for Containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. The save enclosure of the radioactive container inventory has to be guaranteed according to legislation and appropriate guidelines for long term storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is necessary to ensure a proper material choice which is certainly also influenced by additional factors as e.g. the aging behavior. T2 - 14th International high-level radioactive waste management conference CY - Albuquerque, New Mexico, USA DA - 28.04.2013 KW - Rubber seals KW - Elastomers KW - Compression set KW - Low temperature KW - Leakage rate PY - 2013 SN - 978-1-62748-644-6 SP - 1 EP - 7(Paper # 6888) PB - Omnipress AN - OPUS4-28530 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Low temperature - For a seal this depends on the applied material T2 - DKT 2012 - German Rubber Conference CY - Nuremberg, Germany DA - 2012-07-02 PY - 2012 IS - 10-2330_5-L-1530 SP - 1 EP - 4 PB - Deutsche Kautschuk-Gesellschaft CY - Frankfurt am Main AN - OPUS4-26190 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wolff, Dietmar A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Böhning, Martin T1 - Performance of neutron radiation shielding material (U)HMW-PE influenced by gamma radiation T2 - PSAM 11 ESREL 2012 - 11th International probabilistic safety assessment and management conference & The annual european safety and reliability conference CY - Helsinki, Finland DA - 2012-06-25 KW - (U)HMW-PE KW - Gamma irradiation KW - Shielding material KW - Cask for storage and transport of radioactive materials PY - 2012 SP - 1 EP - 8(?) AN - OPUS4-26176 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Behaviour of rubber seals at low temperatures - results of component tests - N2 - The investigation of low temperature properties of elastomeric sealing materials by means of thermo-analytical methods is a sound way to get information about the glass transition process. The breakdown temperature of the sealing function of O-ring seals was measured in a component test setup depending on material and degree of compression. An in depth explanation of the observed component tests behaviour is currently in preparation. It requires the results of thermo-analytical methods and measurements as the compression set (not shown here). With that, a model was developed to describe the correlation between physical material parameters and observed component behaviour. T2 - Jahrestagung Kerntechnik 2013 CY - Berlin, Germany DA - 14.05.2013 PY - 2013 SP - 1 EP - 6 AN - OPUS4-28574 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - UHMW-PE - a shielding material with special properties influenced by radiation N2 - Ultra high molecular weight polyethylene (UHMW-PE) - due to its high hydrogen content - is used as neutron shielding material in casks for storage and transport of radioactive materials. Besides this, UHMW-PE - as a high-performance polymer - has been used for several years in medical technology due to its excellent slip and wear properties. Due to the special properties of UHMW-PE which result basically from its extreme chain lengths and its high degree of crystallinity, it is predestinated for the aforementioned applications. In both cases, irradiation and its impact on the molecular structure of polyethylene play an important role. In the first case, irradiation exists as a by-product of inserting the radioactive material in the cask. Hence PE has to withstand any type of degradation affecting safety relevant aspects to be applicable for long term radiation shielding purposes for instance over a period of 40 years. In the second case irradiation is applied deliberately for purposes such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better Chemical stability. Specifically concerning their use in the field of medical technology, different types of UHMW-PE have been objects of numerous publications. It is generally accepted that two parallel and competitive processes, based on chain scission and reactions of Ccentered radicals and molecular fragments, occur in PE as a consequence of radiation: radical recombination accounts for crosslinking, together with some disproportionation, formation of low molecular weight fragments, and recrystallization. Furthermore, formation of oxygenated structures in the presence of traces of oxygen is an antagonist of the C-centered radicals. Radiation induced scission preferentially takes place in the amorphous phase and noncrystalline surface of the crystals. It is followed by folding of molecular fragments, crystallinity growth and increased perfection in the crystal lamellae [4, 5]. Chain scission results in shorter polymer molecules, fewer entanglements, and consequently, increased molecular mobility. The scope of our investigation comprises an estimation of the radiation and thermal impact on the molecular and supra molecular structure of the two types of PE used for neutron shielding cask components. A further point which is worth to explore is to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermogravimetry (TG). Additionally FT-IR and solubility measurements have been performed. In our studies we focused on the UHMW-PE material GUR 4120 which was y irradiated at RT and compared to the untreated material. T2 - Jahrestagung Kerntechnik 2011 CY - Berlin, Germany DA - 17.05.2011 PY - 2011 SP - 1 EP - 5 AN - OPUS4-24620 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Böhning, Martin A1 - Goering, Harald T1 - Radiation induced structural changes of (U)HMW polyethylene with regard to its application for radiation shielding N2 - The special properties of high molecular weight polyethylene (HMW-PE) and ultra high molecular weight polyethylene (UHMW-PE) result basically from their extreme chain lengths and their high degree of crystallinity. As high-performance polymers, they are used for a variety of applications. UHMW-PE in particular is often utilized for endoprothesis (due to its excellent slip and wear properties) and due to its high hydrogen content as a neutron moderator in casks for storage and transport of radioactive materials. To prepare the material for instance for its use as a total joint replacement, it is exposed to radiation for several reasons, such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better chemical stability. To be applicable for long term radiation shielding purposes for instance over a period of 40 years, PE has to withstand any type of degradation affecting safety relevant aspects. The scope of our investigation comprises an estimation of the radiation impact on the molecular and supra molecular structure of two types of PE and to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermo Gravimetric Analysis (TGA). Additionally FT-IR spectroscopy as well as density and gas sorption measurements were carried out. Due to the poor solubility of HMW-PE and UHMW-PE, some classical analytical techniques are not applicable. But TA-methods represent a feasible approach to detect structural and morphological features of these materials as well as changes caused by external influences, such as thermal treatment and/or irradiation. With the combination of the applied TA-techniques it is possible to distinguish between crosslinking and degradation. T2 - PATRAM 2010 - 16th International symposium on the packaging and transport of radioactive materials CY - London, UK DA - 2010-10-03 PY - 2010 SP - 1 EP - 8 (T25/Paper 173) AN - OPUS4-24621 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Schulz, Sebastian A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Characterization of the low temperature behaviour of rubber sealing materials N2 - Rubbers are often used for seal applications due to their special material properties and easy use. In many applications the material is exposed to low temperatures during Operation. Therefore it is important to know the material behavior at low temperatures to determine the temperature ränge that allows a Safe Operation of the seal, e.g. in storage and transport Containers for radioactive materials. The seal function of an elastomer is limited in temperature by the rubber-glass transition during which the material properties change from rubber-like to stiff and glass-like. For a given application this correlation is not trivial and therefore needs an in-depth investigation under consideration of the physical properties and the application conditions. In this work different analytical methods are used to characterize the material behavior at low temperature in the ränge of the glass-rubber-transition and are compared with the quality of Operation of a component which is here defined by the detected leakage rate. T2 - Technomer 2011 - 22. Fachtagung über Verarbeitung und Anwendung von Polymeren CY - Chemnitz, Deutschland DA - 10.11.2011 PY - 2011 SN - 978-3-939382-10-2 IS - Kap. 3.7 SP - 1 EP - 4 AN - OPUS4-24971 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Hoster, B. T1 - In-situ vulcanization monitoring by ultrasonic wave propagation T2 - 8. Kautschuk-Herbst-Kolloquium CY - Hannover, Deutschland DA - 2008-11-26 KW - Vulcanization KW - Cure monitoring KW - Ultrasound PY - 2008 SP - 133 AN - OPUS4-18574 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Stark, Wolfgang ED - Riedl, A. T1 - Was passiert bei tiefen Temperaturen? - Dichtungsverhalten im Bereich des Glasübergangs N2 - Elastomere werden vielfach als Dichtungsmaterial für verschiedene Anwendungen eingesetzt. In vielen Bereichen ist die Funktion der Dichtung auch bei tiefen Temperaturen erforderlich. Daher ist das Verständnis des Versagensmechanismus von großer Bedeutung. Normalerweise werden Elastomere oberhalb ihres Glass-Gummi Umwandlungsbereiches eingesetzt, wobei die minimale Einsatztemperatur nicht exakt definiert ist. Daher ist es sinnvoll, diese untere Temperatureinsatzgrenze in Abhängigkeit von den Materialeigenschaften zu bestimmen. Hierfür werden die Ergebnisse der thermischen Analyse mit den Resultaten des Druckverformungsrests aus einer abgewandelten Messung mit der Dynamisch Mechanischen Analyse (DMA) kombiniert. Weiterhin werden Ergebnisse von Bauteilversuchen vorgestellt und diskutiert. Die vorgestellten Untersuchungen wurden zum großen Teil auf Untersuchungen im Rahmen der Dissertation von M. Jaunich durchgeführt. T2 - XVIII. Dichtungskolloquium - Sichere und zuverlässige Dichtverbindungen CY - Rheine, Germany DA - 25.09.2013 KW - Dichtung KW - Glasübergang KW - Elastomer KW - Druckverformungsrest PY - 2013 SN - 978-3-8027-2216-5 SP - 51 EP - 58 PB - Vulkan AN - OPUS4-29221 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Druckverformungsrest bei tiefen Temperaturen N2 - Für Elastomenwerkstoffe im Allgemeinen und im Bereich der Dichtungstechnik im Besonderen ist der Druckverformungsrest eine wichtige Kenngröße zur Beurteilung der Eignung eines Werkstoffs bzw. der Funktion eines Bauteils. Er ermöglicht eine Einschätzung des zeitabhängigen Rückstellverhaltens eines Werkstoffs nach Deformation. Dieses ist für Dichtungen von besonderer Bedeutung, da der Test deren Einbauzustand nachstellt. Oft wird er, bei der Prüfung unter erhöhten Temperaturen, zur Beurteilung des Alterungsverhaltens verwendet und kann anhand eines definierten Versagenskriteriums zur Lebensdauerabschätzung eingesetzt werden. Bei tiefen Temperaturen dient er dazu, die limitierende Einsatztemperatur zu bestimmen. Dabei spielt eine Alterung im eigentlichen Sinne nur eine untergeordnete Rolle, wohl aber physikalische Effekte wie Tieftemperaturkristallisation und Glasübergang. Diese Effekte sind weit weniger durch lange Lagerzeiten beeinflusst als die eigentliche Alterung. Die Versuchsdurchführung unterscheidet sich je nach angewandter Norm und kann einen deutlichen Einfluss auf den Druckverformungsrest haben. Alle standardisierten Methoden sind aufgrund der langen Lagerzeiten relativ langwierig und erfordern das regelmäßige Eingreifen durch den Prüfer. Zusätzlich sehen einige Methoden nur die Bestimmung eines einzelnen Wertes nach einer definierten Zeit vor. Um die Messungen zu beschleunigen wurde eine Methode entwickelt, die automatisch die erforderlichen Messungen bei mehreren Temperaturen durchführt. Dazu wird ein Prüfgerät der Dynamisch Mechanischen Analyse verwendet, das kontinuierlich die Deformation während eines frei programmierbaren Temperaturzyklus misst, wodurch eine sehr große Datenmenge verfügbar ist. Ein Vergleich der neuen Methode mit den Ergebnissen des nach ISO 815 genormten Messprinzips ergibt eine gute Übereinstimmung. Ergebnisse der neuen Methode werden vorgestellt und die Vorzüge der kontinuierlichen Datenerfassung, z.B. für die Materialauswahl, diskutiert. Die vorgestellten Ergebnisse beziehen sich zum großen Teil auf die in beschriebenen Untersuchungen und Ergebnisse. T2 - Technomer 2013 - 23. Fachtagung über Verarbeitung und Anwendung von Polymeren CY - Chemnitz, Germany DA - 14.11.2013 PY - 2013 SN - 978-3-939382-11-9 IS - Kapitel V 3.4 SP - 1 EP - 8 AN - OPUS4-29616 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -