TY - CONF A1 - Wolff, Dietmar A1 - Jaunich, Matthias A1 - Stark, Wolfgang T1 - Investigating the performance of rubber seals at low temperatures N2 - Rubbers are widely used as main sealing materials for Containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. The save enclosure of the radioactive container inventory has to be guaranteed according to legislation and appropriate guidelines for long term storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is necessary to ensure a proper material choice which is certainly also influenced by additional factors as e.g. the aging behavior. T2 - 14th International high-level radioactive waste management conference CY - Albuquerque, New Mexico, USA DA - 28.04.2013 KW - Rubber seals KW - Elastomers KW - Compression set KW - Low temperature KW - Leakage rate PY - 2013 SN - 978-1-62748-644-6 SP - 1 EP - 7(Paper # 6888) PB - Omnipress AN - OPUS4-28530 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Comparison of low temperature properties of different elastomer materials investigated by a new method for compression set measurement N2 - The method for the determination of compression set values with a Dynamic Mechanical Analysis (DMA) setup at low temperatures, which was presented previously, allows a much faster and readily automated procedure than the standardized compression set test according to ISO 815-2. This method is applied to a series of different elastomeric materials that are commonly used for sealing applications. The results of the compression set test are compared with results from thermal analysis to allow an in depth comparison of the material behaviour at low temperatures. Furthermore, a comparison between two EPDM materials is presented. These materials show very similar properties determined by thermo analytical methods such as Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) but differ clearly in their compression set behaviour. This comparison shows the importance and value of information of the compression set test in addition to thermal analysis to judge the behaviour of sealing materials and confirms the relevance of the new compression set test method for the investigation of low temperature properties of elastomers. KW - Sealing material KW - Elastomer KW - Compression set KW - Dynamic mechanical analysis KW - Low temperature behaviour PY - 2012 U6 - https://doi.org/10.1016/j.polymertesting.2012.07.016 SN - 0142-9418 VL - 31 IS - 8 SP - 987 EP - 992 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-26538 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Stark, Wolfgang T1 - Low temperature properties of rubber seals - Results of component tests - N2 - Rubbers are widely used as sealing material in various applications. In many fieldsthefunction of seal materials at lowtemperatures is required. Therefore the understanding of faiiure mechanisms that lead to leakage at low temperatures is of high importance. Therefore the lower Operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the Standard tests a faster and more efficient technique was developed and applied. In addition the breakdown temperature of the sealing function of O-ring seals at lowtemperatures is measured in a component test Setup in dependence of the material and the degree of compression. KW - Seal KW - O-ring KW - Low temperature KW - Component test KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Bauteilversuche KW - Druckverformungsrest PY - 2013 SN - 0948-3276 SN - 0022-9520 VL - 66 IS - 7-8 SP - 26 EP - 30 PB - Hüthig CY - Heidelberg AN - OPUS4-28894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Grelle, Tobias A1 - Jaunich, Matthias A1 - Goral, Milan A1 - Wolff, Dietmar T1 - Three-dimensional thermal expansion of neat and irradiated (U)HMWPE materials at elevated temperatures N2 - The thermal expansion of polymeric parts can be an issue in many applications where the available space is limited, or exact dimensions of the part are required. For this study, a device was designed and built that allowed measuring the thermal expansion simultaneously in all three spatial directions on cubic samples with real-scale dimensions (78 mm edge length). The results are shown between 25 °C and 125 °C for two PE materials, one HMWPE and one tempered UHMWPE, for non-irradiated samples as well as cubes that have been irradiated with 100 and 400 kGy. The results measured with the new device were very similar to those measured with conventional thermo-mechanical analysis equipment and to literature data of UHMWPE. The HMWPE material shows a much larger thermal expansion coefficient in one direction compared to the other two directions during the first heating due to frozen stresses from the pressing step during material manufacturing. These stresses are mostly released by the expansion during the first heating, so that the expansion during the second heating is more uniform. The overall volumetric expansion is the same for both heating runs. By contrast, the tempered UHMWPE material shows no significant difference between first and second heating run, as the stresses from processing could already relax in the tempering step. The irradiation treatment does not affect the values significantly for the given test set-up. KW - Lupolen KW - Ultra high molecular weight polyethylene KW - GUR KW - Coefficient of thermal expansion KW - High temperature PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-563987 SN - 0142-9418 VL - 117 SP - 1 EP - 8 PB - Elsevier Ltd. AN - OPUS4-56398 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Oxidative ageing of elastomers: Experiment and modelling N2 - During an extensive test programme at the Bundesanstalt für Materialforschung und prüfung, material property changes of EPDM O-rings were investigated at different ageing times and two ageing temperatures of 125∘C and 150∘C. To exclude possible diffusion-limited oxidation (DLO) effects that can distort the data, IRHD microhardness measurements were taken over the cross section of compressed O-rings. Continuous stress relaxation measurements were taken on samples free of DLO effects. The additional effect of physical processes to irreversible chemical ones during a long-term thermal exposure is quantified by the analysis of compression set measurements under various test conditions. By combining the different experimental methods, characteristic times relative to the degradation processes were determined. On the basis of experimental data, a microphysically motivated model that takes into account reversible and irreversible processes was developed. The parameter identification strategy of the material model is based on our experimental investigations on homogeneously aged elastomer O-rings. The simulated results are in good agreement with the experiments. KW - Compression stress relaxation KW - Compression set KW - IRHD microhardness KW - Modelling PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-545910 SN - 1432-0959 SP - 1 EP - 9 PB - Springer CY - Berlin AN - OPUS4-54591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - A numerical approach to correlate compression stress relaxation and compression set of elastomer O-rings with tightness N2 - The excellent mechanical properties of elastomer seals at a wide range of temperatures as well as their high versatility and recovery potential under several load conditions make these materials well suitable for the application in containers designed for transport and disposal of negligible heat generating radioactive waste. While a seal exchange at defined intervals is typical in many conventional applications, it is impossible or at least hard to perform when principles of minimization of radiation exposure have to be considered which prohibit an avoidable cask handling. An extensive knowledge of the change of the elastomer properties during aging and the availability of reliable end-of-lifetime criteria to guarantee the safe enclosure of the radioactive material for the required time are mandatory. As BAM is involved in most of the national cask licensing procedures and in the evaluation of cask-related long-term safety issues, great efforts have already been made and are still ongoing to scientifically support this task. Among other representative types of elastomers, specimen made from ethylene propylene diene rubber (EPDM) were tested before, during and after aging to capture the with respect to application most important of their complex mechanical properties. Exemplary results of these investigations were used to calibrate material models implemented in the commercial finite element software ABAQUS/Standard®. The finite element model already presented in previous works uses a sequential temperature displacement coupling. The calculated compression stress relaxation (CSR) and compression set (CS) values do satisfactorily match the experimental results. In many investigations performed at BAM both values (CSR and CS) were identified as key indicators of elastomer’s long-term performance. However, the possibility to correlate these equivalent indicators with performance values such as tightness and leakage rate, measurable in the mounted state, is an important goal of our future work. In the presented study the ABAQUS® feature of “pressure penetration” is introduced in the suggested finite element model for this purpose. It provides the possibility to simulate the penetration of a gas into a possible gap between flange and O-ring causing an opening of a leakage path. Three dimensional and axis-symmetric finite element models were generated to represent flat and grooved flanges of different dimensions. The sensitivity of the feature to several input parameters is investigated and the observed behavior of the O-ring is correlated with the results of performed leakage tests. T2 - ASME 2021 Pressure Vessels & Piping Conference (PVP2021) CY - Online meeting DA - 13.07.2021 KW - Elastomer KW - Tightness KW - Leakage KW - Compression set KW - Compression stress relaxation PY - 2021 SN - 978-0-7918-8535-2 U6 - https://doi.org/10.1115/PVP2021-61976 SP - 1 EP - 8 PB - American Society of Mechanical Engineers (ASME) CY - New York, NY, USA AN - OPUS4-54422 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Ageing of HNBR, EPDM and FKM O-rings N2 - HNBR, EPDM and FKM O-rings were aged uncompressed and compressed at 75 °C, 100 °C, 125 °C and 150 °C for up to 1 year. HNBR exhibited the strongest ageing effects with high increases of hardness and glass transition temperature. Furthermore, heterogeneous ageing caused by diffusion-limited oxidation effects had a significant influence for HNBR at ageing temperatures of 125 °C and 150 °C. EPDM showed similar property changes as HNBR, but less pronounced. FKM displayed only minor ageing effects. O-rings aged in compression exhibited considerable compression set (CS). CS data was used for a time-temperature shift and resulting master curve construction. Leakage rate measurements showed that O-rings can remain leak tight under static conditions even if material properties have already deteriorated strongly. N2 - HNBR-, EPDM- und FKM-O-Ringe wurden unverpresst und verpresst für bis zu 1 Jahr bei 75 °C, 100 °C, 125 °C und 150 °C gealtert. HNBR wies mit hohen Anstiegen von Härte und Glasübergangstemperatur die stärksten Alterungseffekte auf. Weiterhin hatte heterogene Alterung aufgrund von diffusionsbegrenzten Oxidationseffekten einen wesentlichen Einfluss auf HNBR bei Alterungstemperaturen von 125 °C und 150 °C. EPDM zeigte ähnliche Eigenschaftsänderungen wie HNBR, allerdings schwächer ausgeprägt. FKM wies nur geringfügige Alterungseffekte auf. O-Ringe, die verpresst gealtert wurden, hatten eine starke bleibende Verformung (DVR). Die gemessenen DVRWerte wurden für eine Zeit-Temperatur-Verschiebung und die Konstruktion einer Masterkurve genutzt. Leckageratenmessungen zeigten, dass O-Ringe unter statischen Bedingungen dicht bleiben können, auch wenn die Materialeigenschaften schon stark degradiert sind. KW - Aging KW - Degradation KW - Leakage KW - Compression KW - Seal PY - 2016 SN - 0022-9520 SN - 0948-3276 VL - 69 IS - 4 SP - 36 EP - 42 PB - Hüthig CY - Heidelberg, Germany AN - OPUS4-36336 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - An approach to improve the understanding of elastomeric seals in use in storage containers N2 - Elastomers are widely used as main sealing materials in Containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste Containers. They are applied due to their special material properties and easy use [1]. For this application several challenging prerequisites must be met for the essential reliable Operation of the seal. T2 - 45th Annual meeting on nuclear technology CY - Frankfurt, Germany DA - 06.05.2014 PY - 2014 SN - 978-3-926956-99-6 SP - 1 EP - 4 AN - OPUS4-31250 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wolff, Dietmar A1 - Jaunich, Matthias A1 - Probst, Ulrich A1 - Nagelschmidt, Sven T1 - Understanding the long-term behavior of sealing systems and neutron shielding material for extended dry cask storage N2 - In Germany, the concept of dry interim storage in dual purpose metal casks before disposal is being pursued for spent nuclear fuel (SF) and high active waste (HAW) management. However, since there is no repository available today, the initially planned and established dry interim storage license duration of up to 40 years will be too short and its extension will become necessary. For such a storage license extension it is required to assess the long-term performance of SF and all safety related storage system components in order to confirm the viability of extended storage. The main safety relevant components are the thick-walled dual purpose metal casks. These casks consist of a monolithic cask body with integrated neutron shielding components (polymers, e.g. polyethylene) and a monitored double lid barrier system with metal and elastomeric seals. The metal seals of this bolted closure system guarantee the required leak-tightness whereas the elastomeric seals allow for leakage rate measurement of the metal seals. This paper presents an update on running long-term tests on metal seals at different temperatures under static conditions over longer periods of time. In addition, first results of our approach to understand the aging behavior of different elastomeric seals and neutron radiation shielding material polyethylene are discussed. T2 - PSAM 12 - Probabilistic safety assessment and management CY - Honolulu, Hawaii, USA DA - 22.06.2014 KW - Extended storage KW - Dual purpose casks KW - Metal seals KW - Elastomeric seals KW - Neutron shielding material PY - 2014 SP - 1 EP - 9 AN - OPUS4-32072 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - A new method to evaluate the low temperature function of rubber sealing materials N2 - A new method for the evaluation of the low temperature properties of rubber materials is presented. The method emulates the standardized compression set measurement, which is frequently used for sealing materials, but can be performed within a considerably shorter time. The results are compared with the standard test and found to be qualitatively the same. Slight differences are discussed on the basis of the differences in the measurement procedures. Further data evaluation is done by fitting functions to describe the material behaviour. KW - Sealing material KW - Elastomer KW - Compression set KW - Dynamic mechanical analysis KW - Low temperature behaviour PY - 2010 U6 - https://doi.org/10.1016/j.polymertesting.2010.07.006 SN - 0142-9418 VL - 29 IS - 7 SP - 815 EP - 823 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-21914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Low temperature properties of rubber seals N2 - Rubber is widely used as sealing material in various applications. In many fields the sealing function at low temperatures is necessary. Therefore the understanding of failure mechanisms is of high importance. Rubbers are normally used above their glass-rubber transition region but the minimum working temperature limit is not defined precisely. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of the standardized compression set according to ISO 815 respectively a modified test using the DMA equipment. N2 - Tiefentemperaturverhalten von Elastomerdichtungen Elastomere werden vielfach als Dichtungsmaterial für verschiedene Anwendungen eingesetzt. In vielen Bereichen ist die Funktion der Dichtung auch bei tiefen Temperaturen erforderlich. Daher ist das Verständnis des Versagensmechanismus von großer Bedeutung. Normalerweise werden Elastomere oberhalb ihres Glass-Gummi Übergangsbereiches eingesetzt aber die minimale Einsatztemperatur ist nicht exakt definiert. Daher ist es sinnvoll diese untere Temperatureinsatzgrenze in Abhängigkeit von den Materialeigenschaften zu bestimmen. Die Ergebnisse der DSC und der DMA werden mit den Ergebnissen des standardisierten Druckverformungsrestes nach ISO 815 und einer abgewandelten Messung mit der DMA kombiniert. KW - Sealing material KW - Elastomer KW - Compression set KW - Dynamic mechanical analysis KW - Low temperature behaviour PY - 2011 SN - 0948-3276 SN - 0022-9520 IS - 03 SP - 52 EP - 55 PB - Hüthig CY - Heidelberg AN - OPUS4-23422 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Revealing effects of chain scission during ageing of EPDM rubber using relaxation and recovery experiment N2 - Both chain scission and crosslinking reactions occur during ageing of EPDM rubber. However, with many conventional polymer analysis methods such as hardness and DMA, it is hardly possible to obtain information about the contribution of each reaction type to the measured data. For example, hardness and Tg both increase during ageing of EPDM, indicating crosslinking during ageing, but it is not clear whether this is partly counterbalanced by chain scission reactions which would lower hardness and Tg. An indication that chain scission reactions probably counteract the hardness or Tg increase by crosslinking is given by Compression Set (CS) measurements. CS exhibits a higher change than hardness or Tg, as CS increases additively through both chain scission and crosslinking reactions. In order to elucidate the share of chain scission reactions in the total degradation, a method testing relaxation and recovery behaviour using DMA equipment was applied. The method revealed the strong influence of chain scissions, leading to more pronounced relaxation and higher residual strain after compression. KW - Compression set KW - DMA KW - Nnetwork KW - Crosslinking PY - 2016 U6 - https://doi.org/10.1016/j.polymertesting.2016.10.026 SN - 0142-9418 SN - 1873-2348 IS - 56 SP - 261 EP - 268 PB - Elsevier Ltd. AN - OPUS4-38012 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Beckmann, Jörg A1 - Schade, U. A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Aziz, E. F. T1 - THz and Mid IR Fourier transform spectroscopy on polyethylene irradiated with Gamma- Co60 radiation N2 - THz and mid IR spectroscopy of high molecular PE (HMW) and ultra high molecular PE (UHMW) reveals modifications of the molecular structure induced by γ-Co60 radiation. UHMW-PE and HMW-PE can be distinguished. The integral absorption in the B1u THz-region can quantitatively describe the amorphization of crystallinity. The formation of trans vinylene unsaturations and the decay of vinyl can be followed by mid IR spectroscopy T2 - IRMMW-THz 2014 - 39th International conference on infrared, millimeter, and terahertz waves CY - Tucson, Arizona, USA DA - 14.09.2014 KW - Thz and Mid IR Fourier transform spectroscopy KW - Polyethylene KW - Gamma-Co-60 radiation KW - Fourier transform spectroscopy KW - Infrared spectroscopy KW - Light absorption KW - Molecular electronic states KW - Polymers KW - MidIR Fourier transform spectroscopy KW - Terahertz spectroscopy KW - THz spectroscopy KW - γ-Co60radiation KW - HMW KW - High molecular PE KW - Ultrahigh molecular PE KW - Molecular structure modifications KW - UHMW-PE KW - HMW-PE KW - Integral absorption KW - B1uTHz-region KW - Crystallinity amorphization KW - Transvinylene unsaturation formation KW - Vinyl decay KW - Absorption KW - Radiation effects KW - Temperature measurement KW - Spectroscopy PY - 2014 UR - http://ieeexplore.ieee.org/stamp/stamp.jsp?tp=&arnumber=6956355&isnumber=6955975 SN - 978-1-4799-3877-3 U6 - https://doi.org/10.1109/IRMMW-THz.2014.6956355 IS - IEEE Catalog No.: CFP14IMM-ART SP - 1 EP - 2 AN - OPUS4-32699 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Grelle, Tobias A1 - Wolff, Dietmar A1 - Jaunich, Matthias T1 - Leakage behaviour of elastomer seals under dynamic unloading conditions at low temperatures N2 - In technical applications, static seals are sometimes also subjected to dynamic loadings. Therefore, the leakage behaviour under dynamic conditions has to be evaluated as well. For this purpose, FKM elastomer seals have been tested by using newly designed equipment that allows for rapid partial release of the seal and simultaneous leakage rate measurement at a wide range of test temperatures. Furthermore, material characterisation was done by using Dynamic Mechanical Analysis, Differential Scanning Calorimetry and Compression Set. It was shown that, under static conditions, the leakage rate increased significantly during cooling at temperatures around 18 K lower than the glass transition range. On reheating, the seal’s functionality was restored in the high temperature region of the glass rubber transition. In the subsequent dynamic release tests, that comprised a reduction of the seal compression within 1 s from 25 % to 23 %, increased leakage rates were observed in the high temperature region of the glass transition range. It was shown that the temperature that is critical for increased leakage is significantly lower under static conditions compared to dynamic conditions. The obtained leakage rates for static tests and dynamic release tests at different temperatures were analysed with reference to results of the material characterisation. KW - Sealing material KW - Rubber KW - Partial release KW - Low temperature behaviour KW - Leakage rate PY - 2017 U6 - https://doi.org/10.1016/j.polymertesting.2016.12.018 SN - 0142-9418 SN - 1873-2348 VL - 58 SP - 219 EP - 226 PB - Elsevier Ltd. CY - Oxford, UK AN - OPUS4-38911 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Erroneous or Arrhenius: A Degradation Rate-Based Model for EPDM during Homogeneous Ageing N2 - To improve the predictive capability of long-term stress relaxation of elastomers during thermo-oxidative ageing, a method to separate reversible and irreversible processes was adopted. The separation is performed through the analysis of compression set after tempering. On the Basis of this separation, a numerical model for long-term stress relaxation during homogeneous ageing is proposed. The model consists of an additive contribution of physical and chemical relaxation. Computer simulations of compression stress relaxation were performed for long ageing times and the results were validated with the Arrhenius treatment, the kinetic study and the time-temperature superposition technique based on experimental data. For chemical relaxation, two decay functions are introduced each with an activation energy and a degradative process. The first process with the lower activation energy dominates at lower ageing times, while the second one with the higher activation energy at longer ageing times. A degradation-rate based model for the evolution of each process and ist contribution to the total system during homogeneous ageing is proposed. The main advantage of the model is the possibility to quickly validate the interpolation at lower temperatures within the range of slower chemical processes without forcing a straight-line extrapolation. KW - Kinetic study KW - Arrhenius KW - TTS KW - Modeling KW - Chemical processes KW - Stress relaxation PY - 2020 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-512931 SN - 2073-4360 VL - 12 IS - 9 SP - 1 EP - 21 AN - OPUS4-51293 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Goral, Milan A1 - Wolff, Dietmar T1 - Insights for lifetime predictions of O-ring seals from five-year long-term aging tests N2 - O-rings made of HNBR, EPDM and FKM were aged in the compressed and uncompressed state at 150 °C, 125 °C, 100 °C, 75 °C, 60 °C and 23 °C for aging times of up to five years. Hardness was measured and increased with aging time and temperature for HNBR and EPDM, but it remained practically constant for FKM. Indenter modulus measurements were performed on the lateral O-ring surface (that was free of DLO effects) to assess an influence of the compression during aging, but none was detected. The equilibrium compression set (CS) exhibited faster and stronger degradation than hardness and was used for lifetime predictions using the time-temperature superposition (TTS) principle. With an end-of-lifetime criterion of 70 % CS, lifetimes of 4.5 years, 50 years and 526 years at 75 °C were estimated for HNBR, EPDM and FKM, respectively. The activation energies derived from an Arrhenius plot of the shift factors from the TTS were 85 kJ/mol, 99 kJ/mol and 78 kJ/mol for HNBR, EPDM and FKM, respectively, revealing that a higher activation energy does not necessarily mean that the material has a higher lifetime at lower temperatures. Furthermore, the measured lifetime of EPDM O-rings at 100 °C (5 years) was compared to that predicted on the basis of the lifetime at 150 °C as well as 125 °C using the corresponding shift factors. The error of the prediction was only ± 4 %. However, this precise prediction could only be achieved using the five-year long-term aging data. When using only data from aging times up to 0.5 years and 2 years, the lifetime of EPDM O-rings at 100 °C was underestimated by 31 % and 22 %, respectively. KW - HNBR KW - EPDM KW - FKM KW - DLO KW - Hardness KW - Compression set KW - Rubber KW - Elastomer KW - Degradation PY - 2020 U6 - https://doi.org/10.1016/j.polymdegradstab.2020.109278 VL - 179 SP - 109278 PB - Elsevier Ltd. AN - OPUS4-51060 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Effects of heterogeneous aging in compressed HNBR and EPDM O-ring seals N2 - Seals used in containers for dangerous goods need to maintain leak tightness for several decades. For investigating the change in seal material properties during aging, a comprehensive aging program on both uncompressed and compressed EPDM and HNBR seals was started. In order to obtain results closely related to practical conditions, O-rings with a full-scale cord diameter of 10 mm were aged. However, this set-up can lead to heterogeneous aging caused by diffusion-limited oxidation (DLO) effects. These effects depend on material, dimensions, time and temperature. Heterogeneous aging results in distorted bulk properties such as compression stress relaxation and compression set (CS) suggesting that HNBR has better performance than EPDM at 150 °C but which is not the case at 100 °C. The presence of heterogeneous material properties was shown by hardness measurements across the seal cross-section. If DLO-affected data is excluded, extrapolations of CS data are possible using time-temperature shifts and Arrhenius graphs. Exemplary CS values of 50 % and 80 % would be reached after approx. 10 years and 29 years, respectively for HNBR and after approx. 400 years and 1100 years, respectively for EPDM. KW - Ageing KW - Rubber KW - Compression KW - DLO KW - Extrapolation KW - Lifetime prediction PY - 2016 U6 - https://doi.org/10.1016/j.polymdegradstab.2016.01.012 VL - 126 SP - 39 EP - 46 PB - Elsevier Science CY - Oxford AN - OPUS4-35775 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Influence of gamma irradiation on low temperature properties of rubber seal materials N2 - In many fields the function of seal materials is required at low temperatures. Therefore the understanding of failure mechanisms at low temperatures is of high importance. In some applications elastomeric seals are used in environments with increased irradiation backgrounds, as e.g. in containers for radioactive waste. This paper reports on the influence of gamma irradiation on the low temperature properties of different fluorocarbon rubber (FKM) materials. The samples were irradiated with gamma doses of up to 600 kGy and the induced changes of material properties were tested by methods sensitive to the rubber-glass transition, like DSC and DMA. Additionally, compression set measurements were performed to give information about recovery behaviour at low temperatures. KW - Seal KW - O-ring KW - Low temperature KW - Gamma irradiation KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Gamma-Bestrahlung KW - Druckverformungsrest PY - 2015 SN - 0948-3276 SN - 0022-9520 VL - 68 IS - 6 SP - 85 EP - 89 PB - Hüthig CY - Heidelberg AN - OPUS4-33552 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Grelle, Tobias A1 - Wolff, Dietmar A1 - Jaunich, Matthias T1 - Temperature-dependent leak tightness of elastomer seals after partial and rapid release of compression N2 - A device has been designed, built and tested that allows the investigation of effects of dynamic loads on the leak tightness of elastomer seals at low temperatures. With the test setup, the compression of the tested seal can be reduced by a defined degree in a time period of less than 1 s. For the evaluation of the leak tightness, leakage rates can be determined. It was shown that the rapid partial release of an elastomer seal leads to its failure already at the beginning of the rubber–glass transition and, therefore, at significantly higher temperatures than the loss of leak tightness observed under static conditions. KW - Sealing material KW - Elastomer KW - Dynamic loading KW - Low temperature behaviour KW - Leakage rate PY - 2015 U6 - https://doi.org/10.1016/j.polymertesting.2015.09.009 SN - 0142-9418 VL - 48 SP - 44 EP - 49 PB - Elsevier Ltd. CY - Amsterdam [u.a.] AN - OPUS4-34445 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Scission, cross-linking, and physical relaxation during thermal degradation of elastomers N2 - Elastomers are susceptible to chemical ageing, i.e., scission and cross-linking, at high temperatures. This thermally driven ageing process affects their mechanical properties and leads to limited operating time. Continuous and intermittent stress Relaxation measurements were conducted on ethylene propylene diene rubber (EPDM) and hydrogenated nitrile butadiene rubber (HNBR) samples for different ageing times and an ageing temperature of 125 °C. The contributions of chain scission and cross-linking were analysed for both materials at different ageing states, elucidating the respective ageing mechanisms. Furthermore, compression set experiments were performed under various test conditions. Adopting the two-network model, compression set values were calculated and compared to the measured data. The additional effect of physical processes to scission and cross-linking during a long-term thermal exposure is quantified through the compression set analysis. The characteristic times relative to the degradation processes are also determined. KW - Ageing KW - Scission KW - Cross-linking KW - Compression set KW - Physical relaxation PY - 2019 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-486091 SN - 2073-4360 VL - 11 IS - 8 SP - 1280, 1 EP - 12 PB - MDPI AN - OPUS4-48609 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Pourmand, P. A1 - Wolff, Dietmar A1 - Hedenqvist, M. T1 - Analysis of O-ring seal failure under static conditions and determination of end-of-lifetime criterion N2 - Determining a suitable and reliable end-of-lifetime criterion for O-ring seals is an important issue for long-term seal applications. Therefore, seal failure of ethylene propylene diene rubber (EPDM) and hydrogenated nitrile butadiene rubber (HNBR) O-rings aged in the compressed state at 125 °C and at 150 °C for up to 1.5 years was analyzed and investigated under static conditions, using both non-lubricated and lubricated seals. Changes of the material properties were analyzed with dynamic-mechanical analysis and permeability experiments. Indenter modulus measurements were used to investigate DLO effects. It became clear that O-rings can remain leak-tight under static conditions even when material properties have already degraded considerably, especially when adhesion effects are encountered. As a feasible and reliable end-of-lifetime criterion for O-ring seals under static conditions should include a safety margin for slight dimensional changes, a modified leakage test involving a small and rapid partial decompression of the seal was introduced that enabled determining a more realistic but still conservative end-of-lifetime criterion for an EPDM seal. KW - EPDM KW - HNBR KW - Seal failure KW - Leak-tightness KW - DLO KW - Oxygen permability KW - DMA KW - Indenter modulus PY - 2019 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-486125 SN - 2073-4360 VL - 11 IS - 8 SP - 1251, 1 EP - 19 PB - MDPI CY - Basel, CH AN - OPUS4-48612 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Zaghdoudi, Maha A1 - Weber, Mike A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Numerical Modelling of Compression Stress Relaxation and Compression Set of Elastomer O-Ring During Aging N2 - Elastomer seals are used in many industrial applications due to their excellent mechanical properties at a wide range of temperatures. Their high versatility and recovery potential under several load conditions make them well suitable for the application in containers designed for transport, storage and/or disposal of radioactive materials. In containers for low and intermediate level radioactive waste, elastomer seals are used as barrier seals, and as auxiliary seals in storage and transportation casks (dual purpose casks) for heat generating radioactive waste, such as spent fuel and high-level waste. While a seal exchange at defined intervals is typical in many conventional applications, it is impossible or at least hard to perform when principles of minimization of radiation exposure have to be considered and prohibit an unnecessary cask handling. An extensive knowledge of the change of the elastomer’s properties during aging and the availability of reliable end-of-lifetime criteria to guarantee the permanent safe enclosure of the radioactive material is mandatory. As BAM is involved in most of the national cask licensing procedures and in the evaluation of cask-related long-term safety issues, great efforts have been already made and are still planned to scientifically support this task. Compression stress relaxation and compression set were identified as key indicators of elastomer long-term performance and quantitatively investigated in comprehensive test programs. Among other representative types of elastomers, specimens made from ethylene propylene diene rubber (EPDM) were tested before, during and after aging to capture the most important of their complex mechanical properties. In the presented study, exemplary results were used to simulate the compression stress relaxation and the compression set of elastomer O-rings during aging. Regarding the influence of temperature, the time-temperature superposition principle is applied in the relaxation analysis of elastomer O-rings. The proposed model is implemented in the commercial finite element software ABAQUS/Standard® [1] with a sequential temperature displacement coupling. Numerical results match the experimental compression stress relaxation measurements well. The prediction of compression set values after long-term aging shows a relatively good agreement with the experimental results. Nevertheless, all input parameters derived from the specimen tests, additional assumptions concerning boundary conditions and modeling strategy are discussed with regard to the identified slight discrepancies. The possibility to extend the finite element model to represent the O-ring seal’s ability to recover after a (fast) partial release is taken into account. T2 - ASME 2020 Pressure Vessels & Piping Conference (PVP2020) CY - Online meeting DA - 03.08.2020 KW - Compression Set KW - O-ring KW - Simulation KW - Sequential analysis KW - Ageing KW - stress relaxation PY - 2020 SN - 978-0-7918-8388-4 U6 - https://doi.org/10.1115/PVP2020-21270 SP - PVP2020-21270 PB - ASME AN - OPUS4-51490 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Chatzigiannakis, E. A1 - Beckmann, Jörg A1 - Wachtendorf, Volker A1 - von der Ehe, Kerstin A1 - Braun, Ulrike A1 - Jaunich, Matthias A1 - Schade, U. A1 - Wolff, Dietmar T1 - Discoloration Effects of High-Dose gamma-Irradiation and Long-Term Thermal Aging of (U) HMW-PE N2 - Two polyethylene types with ultra-high (UHMWPE) and high molecular weight (HMW-PE) used as neutron radiation shielding materials in casks for radioactive waste were irradiated with doses up to 600 kGy using a 60Co gammasource. Subsequently, thermal aging at 125∘C was applied for up to one year. Degradation effects in the materials were characterized using colorimetry, UV-Visspectroscopy, IR spectroscopy, and DSC. Both materials exhibited a yellowing upon irradiation.The discoloration of UHMW-PE disappeared again after thermal aging.Therefore, the yellowing is assumed to originate fromannealable color centers in the formof free radicals that are trapped in the crystalline regions of the polymer and recombine at elevated temperatures. For the antioxidantcontaining HMWPE, yellowing was observed after both irradiation and thermal aging. The color change was correlated mainly to decomposition products of the antioxidant in addition to trapped radicals as in UHMW-PE. Additionally, black spots appeared after thermal aging of HMW-PE. KW - Irradiation KW - UHMWPE KW - Colour center KW - Yellowness index PY - 2017 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-423992 SN - 1687-9422 VL - 2017 IS - Article ID 1362491 SP - 1 EP - 10 PB - Hindawi AN - OPUS4-42399 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - von der Ehe, Kerstin A1 - Wolff, Dietmar A1 - Jaunich, Matthias T1 - Effect of high-dose gamma irradiation on (U)HMWPE neutron shielding materials N2 - High and ultra-high molecular weight polyethylenes were gamma-irradiated with doses up to 600 kGy. The changes in the material properties were analysed using DSC, DMA, IR spectroscopy, as well as measurements of density and insoluble content. The irradiation led to an increase of the degree of crystallinity because of chain scissions during irradiation, leading to shorter and thus more mobile chains. Both the plateau value of the shear modulus G′ and the insoluble content increased with Irradiation dose, indicating the formation of additional crosslinks. Furthermore, IR spectroscopy revealed irradiation induced oxidation and the formation of double bonds, indicating that some of the hydrogen atoms responsible for the neutron shielding capability have been released. KW - Ultra high molecular weight KW - Polyethylene KW - Gamma irradiation KW - Crosslinking KW - Oxidation PY - 2018 U6 - https://doi.org/10.1016/j.radphyschem.2017.02.014 SN - 0969-806X VL - 142 SP - 29 EP - 33 PB - Elsevier AN - OPUS4-42941 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Jaunich, Matthias A1 - Kömmling, Anja A1 - Wolff, Dietmar ED - Grellmann, W. ED - Langer, B. T1 - Investigations of elastomeric seals – Low temperature performance and aging behavior N2 - Due to their simple and reliable application, elastomers are used for many tasks. Many fields of application like transport, aviation and process technology, entail low temperatures where proper functionality of the employed seals has to be ensured. Therefore, understanding the low temperature behavior of elastomeric seals is important for safe seal operation to restrict the temperature application range. For all areas of application, the question of seal lifetime is also important for replacement or maintenance intervals. The lifetime is especially important in applications that allow no seal replacement. Since the seal can determine the lifetime of storage in such cases, reliable lifetime estimation is necessary for these applications, and requires an extensive knowledge of the specific aging behavior. KW - Seal KW - Rubber KW - Ageing KW - Replacement PY - 2017 SN - 978-3-319-41877-3 SN - 978-3-319-41879-7 U6 - https://doi.org/10.1007/978-3-319-41879-7_30 SN - 0933-033X SN - 2196-2812 VL - 247 SP - 431 EP - 443 PB - Springer Verlag AN - OPUS4-41167 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Pourmand, P. A1 - Wolff, Dietmar A1 - Gedde, U.W. T1 - Influence of ageing on sealability of elastomeric O-rings N2 - At BAM, which is the federal institute for materials research and testing in Germany, it is one of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes the assessment of the service lifetime of elastomeric seals that are part of the container lid system with regard to the requirements for long-term safety (40 years and more) of the containers. Therefore, we started an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) which are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) up to 1.5 years. In order to assess sealability, O-rings are aged in compression by 25 % (corresponding to the compression during service) between plates as well as in flanges that allow leakage rate measurements. For comparison, uncompressed O-rings are aged as well. Further methods characterising seal performance are compression stress relaxation (CSR) reflecting the loss of sealing force of a compressed seal over time, and compression set (CS) which represents the recovery behaviour of a seal after release from compression. Additionally, hardness is measured for information about the change of mechanical properties. The experimental results indicate that while hardness, CSR and CS show considerable degradation effects, the leakage rate stays relatively constant or even decreases until shrinkage combined with the loss of resilience of the aged seal leads to leakage. This demonstrates that static leakage rate, which is the only available direct seal performance criterion, has only limited sensitivity towards the degradation of the seal material. CS data is extrapolated using time-temperature shifts and Arrhenius graphs. An exemplary CS of 50 % would be reached after approx. 1.2, 17 and 29 years at 60 °C for HNBR, EPDM and FKM respectively. T2 - PolymerTec 2016 CY - Merseburg, Germany DA - 15.06.2016 KW - Compression KW - Leakage KW - Degradation KW - Rubber KW - Lifetime PY - 2017 U6 - https://doi.org/10.1002/masy.201600157 SN - 1022-1360 SN - 1521-3900 VL - 373 IS - 1 SP - UNSP 1600157, 1 EP - 10 PB - WILEY-V C H VERLAG GMBH CY - Weinheim AN - OPUS4-40958 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Understanding the recovery behaviour and the degradative processes of EPDM during ageing N2 - Recovery is an important measure for seal applications representing to which extent the elastomer regains its initial shape after deformation and release of an applied force. Compression set (CS) indicates the degree of recovery. Ethylene propylene diene rubber (EPDM) was aged at 75 ◦C, 100 ◦C, 125 ◦C and 150 ◦C for different ageing times up to five years and compression set measurements were performed at different times after disassembly and after additional tempering. Short- and long-term recovery up to one year after release for samples aged at 125 ◦C and 150 ◦C was also studied. To assess the curvature in the Arrhenius diagram that may occur due to non-sufficiently aged specimens, a degradation-rate based model was fitted to the CS data after tempering. For each ageing temperature, two decay fit functions were proposed, each with an activation energy and a corresponding degradative process. The influence of ageing on the leak-tightness after fast small partial release is investigated and estimated through the analysis of the shift factors from time temperature superposition (TTS) of CS measurements at different times after disassembly. Shift factors of CS measurement after 1 s and after additional tempering are in good agreement. KW - Compression set KW - Ageing KW - Recovery KW - Degradative processes KW - Leakage rate PY - 2023 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-573699 SN - 0142-9418 VL - 121 SP - 107987 PB - Elsevier Ltd. AN - OPUS4-57369 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grelle, Tobias A1 - Wolff, Dietmar A1 - Probst, Ulrich A1 - Jaunich, Matthias A1 - Völzke, Holger T1 - Investigation of the time and temperature dependent behavior of metal seals in radioactive waste containers N2 - The Bundesanstalt für Materialforschung und –Prüfung (BAM) runs an investigation program on the long-term behavior of multi-component metal seals. Such seals are used in a wide area of applications including transport and storage casks for spent nuclear fuel and high level radioactive waste. The seal function is mainly based on the compression of the inner helical spring, which generates the necessary seal force to keep the sealing surfaces in close contact. This in turn leads to a plastic deformation of the outer jacket of the seal, comprised of highly ductile aluminum or silver that adapts to the sealing surfaces of cask body and bolted lid, thus providing high Level leak tightness. In Germany, those casks are licensed for Interim storage periods of up to 40 years or more if extended Interim storage would become necessary before a final repository is available. Thus, the sealing performance has to be evaluated, including factors like elevated temperature due to decay heat or mechanical loads due to transport under normal as well as accident conditions. Long-term investigations at BAM have been running over the last nine years to identify and evaluate the seal performance by measuring the remaining seal force, the useable resilience and the leakage rate after various time intervals at temperatures ranging from room temperature up to 150 °C. It was found that the seal force and useable resilience decrease with time and temperature, caused by creep deformation of the outer jacket. In order to obtain an analytical description for the seal behavior and to achieve more information on the material behavior under application conditions a comprehensive investigation program with Focus on aluminum as outer jacket material was launched. The program includes material investigations such as compression and tension creep tests with representative basic materials. An additional test setup allows for the continuous measurement of the remaining seal force at temperatures of up to 150 °C. Furthermore, seal segments are compressed and stored in heating chambers, thus producing segments at different stages of the aging process. The segments are investigated regarding the development of the contact area width, jacket thickness and microstructural changes. This data will be used to develop material models and an analytical description of the time and temperature dependent long-term sealing behavior. This paper explains the current status of gained test results and modelling approaches and closes with an outlook to the future Project plans. T2 - ASME 2018 Pressure Vessels and Piping Conference CY - Prague, Czech Republic DA - 15.07.2018 KW - Metal seal KW - Creep KW - Long-term behavior PY - 2018 SP - PVP2018-84584, 1 EP - 6 AN - OPUS4-46110 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Zencker, Uwe A1 - Völzke, Holger A1 - Schulze, Dietmar A1 - Probst, Ulrich T1 - Testing and Numerical Simulation of Elastomers - From Specimen Tests to Simulation of Seal Behavior under Assembly Conditions N2 - Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level radioactive waste as well as in construction of the already licensed Konrad repository for low and intermediate level radioactive waste, extended periods of interim storage become more relevant in Germany. BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues. The long-term performance of elastomer seals for lid systems of transport and storage casks, whether used as auxiliary seals in spent fuel casks or as primary seals for low and intermediate level waste packages, is an important issue in this context. The polymeric structure of these seals causes a complex mechanical behavior with time-dependent sealing force reduction. The results of a comprehensive purpose-designed test program consisting of basic compression and tension tests as well as relaxation tests on unaged specimens of representative types of elastomers (fluorocarbon rubber (FKM) and ethylene propylene diene rubber (EPDM)) at different temperatures and strain rates are presented. They were used to identify the constitutive behavior and to obtain parameters for finite element material models provided by the computer code ABAQUS®. After estimating the influence of uncertainties such as Poisson’s ratio and friction coefficient by sensitivity analyses, the chosen parameters had to prove their suitability for the finite element simulation of the specimen tests themselves. Based on this preliminary work the simulation of a specific laboratory test configuration containing a typical elastomer seal with circular cross section is presented. The chosen finite element material model and the implemented parameters had to show that they are able to represent not only the specimen behavior under predominantly uniaxial load but also the more complex stress states in real components. Deviations between the measured and calculated results are pointed out and discussed. For the consideration of long-term effects in the simulation of elastomer behavior, test results of aged specimens are needed. First information about a new test program, started recently and planned to provide these data, are given. T2 - ASME 2017 Pressure Vessels & Piping Conference (PVP2017) CY - Waikoloa, Hawaii, USA DA - 16.07.2017 KW - Time dependent effects KW - Low temperature behavior KW - Elastomeric seals KW - Aging KW - Simulation KW - Testing PY - 2017 SN - 978-0-7918-5802-8 VL - 7 SP - Article UNSP V007T07A035, 1 EP - 8 AN - OPUS4-41841 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Kömmling, Anja A1 - Horn, Jutta A1 - Völzke, Holger A1 - Wolff, Dietmar T1 - Long-Term Performance of Elastomer seals - From Aging Tests to Lifetime Estimations N2 - Elastomers show a high versatility which makes them ideal materials for sealing applications in various fields. Especially under changing application conditions the high recovery potential of this class of material is beneficial to compensate temperature or pressure fluctuation, and geometrical changes resulting from mechanical loads in e.g. accident conditions. Out of these reasons elastomers are also used in containers for low and intermediate level radioactive waste and for spent fuel transportation casks. In casks designed for low and intermediate level waste elastomer seals can act as primary seal responsible for the containment function whereas in spent fuel storage and transportation casks (dual purpose casks (DPC)) elastomer seals are used as auxiliary seals to allow leakage rate measurements of metal barrier seals. An inherent prerequisite for this kind of application is the Long time-scale of operation without or with limited possibility of seal replacement. In Germany an interim storage license for DPC`s is typically issued for 40 years, a timeframe which might increase in the future due to challenges of the final repository siting procedure. For low and intermediate level waste, also long time periods are required before final disposal can be achieved. Therefore, the performance of elastomer seals over extended time periods is, as for other applications, of high importance. A typical approach to ensure long-term functionality is to perform accelerated aging tests to calculate an estimated lifetime by assuming e.g. Arrhenius like equations for the timetemperature relationship. This approach requires a suitable end of life criterion considering the application of interest. This often can represent a challenge on its own. As BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues we initiated several test programs for investigating the behavior of elastomer seals. Experiments concerning the low temperature performance down to -40 °C and the influence of gamma irradiation have been started first. Currently the thermal aging behavior of elastomer seals, which is the topic of this contribution, is examined. For our aging investigations we use a broad approach to first determine the property changes in different elastomer materials due to thermo-oxidative aging at elevated temperatures and secondly, we test how the typical methods of lifetime extrapolation can be applied to these results. This Approach enables us to detect and exclude undesired side effects which very often influence lifetime estimations. In this contribution, our recent results are extended. The results show that lifetime estimation based on single material properties can be misleading and therefore a combination of several methods is recommended. T2 - ASME 2018 Pressure Vessels and Piping Conference CY - Prague, Czech Republic DA - 15.07.2018 KW - Seal performance KW - Rubber KW - Ageing PY - 2018 VL - PVP2018 SP - 84631-1 EP - 84631-8 AN - OPUS4-46346 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Zencker, Uwe A1 - Völzke, Holger A1 - Schulze, Dietmar T1 - Testing and numerical simulation of elastomeric seals under consideration of time dependent effects N2 - Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level waste and in construction of the already licensed Konrad repository for low and intermediate level waste, extended periods of interim storage will become more relevant in Germany. BAM is involved in most of the cask licensing procedures and is responsible for the evaluation of cask-related long-term safety issues. Elastomeric seals are widely used as barrier seals for containers for low and intermediate level radioactive waste. In addition they are also used as auxiliary seals in spent fuel storage and transportation casks (dual purpose casks (DPC)). To address the complex requirements resulting from the described applications, BAM has initiated several test programs for investigating the behavior of elastomeric seals. These include experiments concerning the hyperelastic and viscoelastic behavior at different temperatures and strain rates, the low temperature performance down to -40°C, the influence of gamma irradiation and the aging behavior. The first part of the paper gives an overview of these tests, their relevant results and their possible impact on BAM’s work as a consultant in the framework of approval and licensing procedures. The second part presents an approach of the development of a finite element model using the finite element code ABAQUS®. The long-term goal is to simulate the complex elastomeric behavior in a complete lid closure system under specific operation and accident conditions. T2 - ASME 2016 Pressure Vessels & Piping Conference (PVP2016) CY - Vancouver, BC, Canada DA - 17.07.2016 KW - Elastomeric seals KW - Testing KW - Low temperature behavior KW - Aging KW - Simulation KW - Time dependent effects PY - 2016 SN - 978-0-7918-5045-9 VL - 7 SP - Paper 63192, 1 EP - 10 AN - OPUS4-37046 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Goral, Milan A1 - Wolff, Dietmar A1 - Völzke, Holger ED - Krüssenberg, A. T1 - Overview of metal seal tests performed at BAM and implications for extended interim storage N2 - The investigation of the long-term performance of sealing systems employed in containers of radioactive waste and spent nuclear fuel is one research focus area for division 3.4 \Safety of Storage Containers" at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for spent nuclear fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal Performance and the main part is focussed on the time and temperature dependent behaviour. Our aim is to understand the longterm behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation. In this contribution an overview of the performed tests and their respective results is given. A focus lies on a comparison between seals with large torus diameter in comparison to small diameters. T2 - Safety of Extended Dry Storage of Spent Nuclear Fuel SEDS2020: International online-workshop CY - Online meeting DA - 03.06.2020 KW - Metal seal KW - Seal performance KW - Long-term investigation KW - Ageing PY - 2020 U6 - https://doi.org/10.3139/124.200071 SN - 0932-3902 VL - 85 IS - 6 SP - 440 EP - 443 PB - Carl Hanser Verlag CY - München AN - OPUS4-51833 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -