TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - UHMW-PE - a shielding material with special properties influenced by radiation N2 - Ultra high molecular weight polyethylene (UHMW-PE) - due to its high hydrogen content - is used as neutron shielding material in casks for storage and transport of radioactive materials. Besides this, UHMW-PE - as a high-performance polymer - has been used for several years in medical technology due to its excellent slip and wear properties. Due to the special properties of UHMW-PE which result basically from its extreme chain lengths and its high degree of crystallinity, it is predestinated for the aforementioned applications. In both cases, irradiation and its impact on the molecular structure of polyethylene play an important role. In the first case, irradiation exists as a by-product of inserting the radioactive material in the cask. Hence PE has to withstand any type of degradation affecting safety relevant aspects to be applicable for long term radiation shielding purposes for instance over a period of 40 years. In the second case irradiation is applied deliberately for purposes such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better Chemical stability. Specifically concerning their use in the field of medical technology, different types of UHMW-PE have been objects of numerous publications. It is generally accepted that two parallel and competitive processes, based on chain scission and reactions of Ccentered radicals and molecular fragments, occur in PE as a consequence of radiation: radical recombination accounts for crosslinking, together with some disproportionation, formation of low molecular weight fragments, and recrystallization. Furthermore, formation of oxygenated structures in the presence of traces of oxygen is an antagonist of the C-centered radicals. Radiation induced scission preferentially takes place in the amorphous phase and noncrystalline surface of the crystals. It is followed by folding of molecular fragments, crystallinity growth and increased perfection in the crystal lamellae [4, 5]. Chain scission results in shorter polymer molecules, fewer entanglements, and consequently, increased molecular mobility. The scope of our investigation comprises an estimation of the radiation and thermal impact on the molecular and supra molecular structure of the two types of PE used for neutron shielding cask components. A further point which is worth to explore is to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermogravimetry (TG). Additionally FT-IR and solubility measurements have been performed. In our studies we focused on the UHMW-PE material GUR 4120 which was y irradiated at RT and compared to the untreated material. T2 - Jahrestagung Kerntechnik 2011 CY - Berlin, Germany DA - 17.05.2011 PY - 2011 SP - 1 EP - 5 AN - OPUS4-24620 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - von der Ehe, Kerstin A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Böhning, Martin A1 - Goering, Harald T1 - Radiation induced structural changes of (U)HMW polyethylene with regard to its application for radiation shielding N2 - The special properties of high molecular weight polyethylene (HMW-PE) and ultra high molecular weight polyethylene (UHMW-PE) result basically from their extreme chain lengths and their high degree of crystallinity. As high-performance polymers, they are used for a variety of applications. UHMW-PE in particular is often utilized for endoprothesis (due to its excellent slip and wear properties) and due to its high hydrogen content as a neutron moderator in casks for storage and transport of radioactive materials. To prepare the material for instance for its use as a total joint replacement, it is exposed to radiation for several reasons, such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better chemical stability. To be applicable for long term radiation shielding purposes for instance over a period of 40 years, PE has to withstand any type of degradation affecting safety relevant aspects. The scope of our investigation comprises an estimation of the radiation impact on the molecular and supra molecular structure of two types of PE and to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermo Gravimetric Analysis (TGA). Additionally FT-IR spectroscopy as well as density and gas sorption measurements were carried out. Due to the poor solubility of HMW-PE and UHMW-PE, some classical analytical techniques are not applicable. But TA-methods represent a feasible approach to detect structural and morphological features of these materials as well as changes caused by external influences, such as thermal treatment and/or irradiation. With the combination of the applied TA-techniques it is possible to distinguish between crosslinking and degradation. T2 - PATRAM 2010 - 16th International symposium on the packaging and transport of radioactive materials CY - London, UK DA - 2010-10-03 PY - 2010 SP - 1 EP - 8 (T25/Paper 173) AN - OPUS4-24621 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Schulz, Sebastian A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Characterization of the low temperature behaviour of rubber sealing materials N2 - Rubbers are often used for seal applications due to their special material properties and easy use. In many applications the material is exposed to low temperatures during Operation. Therefore it is important to know the material behavior at low temperatures to determine the temperature ränge that allows a Safe Operation of the seal, e.g. in storage and transport Containers for radioactive materials. The seal function of an elastomer is limited in temperature by the rubber-glass transition during which the material properties change from rubber-like to stiff and glass-like. For a given application this correlation is not trivial and therefore needs an in-depth investigation under consideration of the physical properties and the application conditions. In this work different analytical methods are used to characterize the material behavior at low temperature in the ränge of the glass-rubber-transition and are compared with the quality of Operation of a component which is here defined by the detected leakage rate. T2 - Technomer 2011 - 22. Fachtagung über Verarbeitung und Anwendung von Polymeren CY - Chemnitz, Deutschland DA - 10.11.2011 PY - 2011 SN - 978-3-939382-10-2 IS - Kap. 3.7 SP - 1 EP - 4 AN - OPUS4-24971 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stark, Wolfgang A1 - Jaunich, Matthias A1 - Bohmeyer, W. A1 - Lange, K. T1 - Investigation of the crosslinking behaviour of ehtylene vinyl acetate (EVA) for solar cell encapsulation by rheology and ultrasound N2 - EVA is a widely used material for the encapsulation of photovoltaic modules. It melts at elevated temperatures, and seals the module before it is crosslinked at temperatures above 130 °C by a peroxide-initiated crosslinking reaction. EVA has good optical properties necessary for application in solar modules. For process optimization and quality management, a method for the quick and reliable characterization of EVA crosslinking behaviour is of great value. Here, the practicability of ultrasound for online crosslinking monitoring is demonstrated. A sound velocity increase of about 8 m/s during the crosslinking reaction is found. The ultrasound results are compared with rheometer measurements performed with a curemeter typically used for the investigation of rubber crosslinking. KW - Ethylene vinyl acetate KW - EVA KW - Crosslinking KW - Ultrasound KW - Rheology KW - Curemeter KW - DSC PY - 2012 U6 - https://doi.org/10.1016/j.polymertesting.2012.07.004 SN - 0142-9418 VL - 31 IS - 7 SP - 904 EP - 908 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-26291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Investigating Low Temperature Properties of Rubber Seals T2 - Waste Management Symposia 2013 CY - Phoenix, AZ, USA DA - 2013-02-24 PY - 2013 AN - OPUS4-27795 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Goering, Harald T1 - Können UF-Formmassen überhärten? Die Aussage des Kochversuchs! T2 - 1. Wildauer Duromer-Tagung CY - Wildau, Germany DA - 2008-03-11 PY - 2008 AN - OPUS4-16730 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang T1 - Aktueller Stand der Online-Kontrolle der Elastomer Vulkanisation und Ausblick auf zukünftige Arbeiten T2 - Jahrestagung DKG-Bezirksgruppe Ost CY - Merseburg, Germany DA - 2008-11-06 PY - 2008 AN - OPUS4-18271 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang T1 - Überwachung des Vulkanisationsverlaufs mit Ultraschall T2 - Jahrestagung der Deutschen Kautschuk-Gesellschaft (DKG), Bezirksgruppe Ost CY - Bad Lauchstädt, Germany DA - 2007-11-08 PY - 2007 AN - OPUS4-16088 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Goering, Harald T1 - Härtung von Harnstoffformmassen: Die Aussagekraft des Kochversuchs! T2 - 10th International AVK Conference on Reinforced Plastics CY - Stuttgart, Germany DA - 2007-11-05 PY - 2007 AN - OPUS4-16089 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Stark, Wolfgang A1 - Wolff, Dietmar T1 - Properties of elastomeric seals at low temperature T2 - International Rubber Conference CY - Nuremberg, Germany DA - 2009-06-29 PY - 2009 AN - OPUS4-18052 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -