TY - CONF A1 - Daus, Lars-Hendrik A1 - Korzen, Manfred A1 - Schartel, Bernhard T1 - High-throughput fire tests and weathering-induced degradation behaviour of intumescent coatings N2 - In this work, the weathering-induced degradation of intumescent coatings was investigated by a systematic and comprehensive approach. A mechanism is revealed that is proposed to be responsible for the loss of function of intumescent coatings induced by weathering. First, the thermal decomposition of artificially weathered intumescent coatings was examined. To get a better understanding of the weathering and ageing phenomena, the degradation behaviour of the single ingredients during the weathering process was investigated, as well as their chemical and physical interactions. For the systematic approach, the materials that are essential for intumescence (ammonium polyphosphate, pentaerythritol, titanium dioxide, melamine and the binder) are treated with moisture, elevated temperature and UV radiation. Thermogravimetry (TG) and IR spectroscopy were used to compare the initial samples with their different grades of weathering. We demonstrate that ammonium polyphosphate, melamine and the binder are mainly responsible for the ageing process. Further, it was demonstrated that TG and IR spectroscopy are suitable measuring methods to detect the effects of weathering on intumescent coatings. Finally, a small-scale fire test procedure is introduced. Based on the reduction of the sample size, up to 50 samples can be tested in a single fire test. The results of this fire test have the same quality as the results from standard intermediate fire tests corresponding to DIN 4102-8. T2 - 3rd European Symposium on Fire Safety Science CY - Nancy, France DA - 12.09.1018 KW - Weathering KW - Intumescent coatings KW - High-Throughput Fire Tests PY - 2018 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-472023 UR - http://iopscience.iop.org/article/10.1088/1742-6596/1107/3/032014/pdf VL - 1107 SP - 032014 PB - IOP Publishing CY - Bristol AN - OPUS4-47202 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Daus, Lars-Hendrik A1 - Schartel, Bernhard A1 - Wachtendorf, Volker A1 - Mangelsdorf, R. A1 - Korzen, Manfred T1 - A chain is no stronger than its weakest link: Weathering resistance of water-based intumescent coatings for steel applications N2 - A systematic approach was used to investigate the weathering-induced degradation of a common water–based intumescent coating. In this study, the coatings are intended for humid indoor applications on steel substrates. The coating contains ammonium polyphosphate, pentaerythritol, melamine, and polyvinyl acetate. By replacing each ingredient with a less water-soluble substance, the most vulnerable substances, polyvinyl acetate and pentaerythritol, were identified. Furthermore, the weathering resistance of the system was improved by exchanging the ingredients. The coatings were stressed by artificial weathering tests and evaluated by fire tests. Thermogravimetry and Fourier-transform infrared spectroscopy were used to study the thermal decomposition. This study lays the foundation for the development of a new generation of water-based intumescent coatings. KW - Intumescence KW - Fire resistance KW - Fire protective coatings KW - Weathering KW - Thermogravimetric analyses PY - 2021 U6 - https://doi.org/10.1177/0734904120961064 SN - 0734-9041 SN - 1530-8049 VL - 39 IS - 1 SP - 72 EP - 102 PB - SAGE AN - OPUS4-52015 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -