TY - JOUR A1 - Schork, B. A1 - Zerbst, Uwe A1 - Kiyak, Yusuf A1 - Kaffenberger, M. A1 - Madia, Mauro A1 - Oechsner, M. T1 - Effect of the parameters of weld toe geometry on the FAT class as obtained by means of fracture mechanics-based simulations N2 - The fracture mechanics-based IBESS approach is applied to the determination of FAT classes of butt welds with crack Initiation along the weld toe. The aim is an investigation of the effect of the geometrical parameters toe radius, flank angle, reinforcement and secondary notches such as roughness or undercuts. The influence of these parameters is discussed both individually and in combination; however, excluding statistical distributions of them and the material data. The results, when compared with conventional FAT classes for butt welds, are encouraging with respect to a potential contribution of IBESS to the discussion of more advanced quality criteria for welds. To that purpose, demands for further research are proposed. KW - Fracture mechanics KW - Weld toe geometry KW - Fatigue crack initiation KW - FAT class approach PY - 2020 U6 - https://doi.org/10.1007/s40194-020-00874-7 IS - 64 SP - 925 EP - 936 PB - Springer AN - OPUS4-53079 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zerbst, Uwe A1 - Madia, Mauro A1 - Schork, B. A1 - Kaffenberger, M. A1 - Oechsner, M. A1 - Kucharzcyk, P. A1 - Hensel, J. A1 - Bernhard, J. A1 - Tchuindjang, D. T1 - The effect of the local and global weld geometry as well as material defects on crack initiation and fatigue strength N2 - The paper provides an application of the IBESS approach to the investigation of the influence of various parameters of the global and local weld geometry as well as material defects on the fatigue strength of weldments. For this purpose, the global weld parameters, such as the weld toe radius, the flank angle, the excess weld metal, local secondary notches (in the present study as a measure of surface imperfections) and inclusions sizes have been determined as statistical distributions for different joint types and geometries and two steels of different strengths. The results are in line with literature data and reveal the potential of the theoretical approach to predict the correct trends. The combination with an advanced weld quality system has been demonstrated to be possible. KW - Weldments KW - Fatigue strength KW - Fracture mechanics KW - Weld geometry KW - Inclusions KW - Multiple crack initiation PY - 2018 U6 - https://doi.org/10.1016/j.engfracmech.2017.07.001 SN - 0013-7944 SN - 1873-7315 VL - 198 SP - 103 EP - 122 PB - Elsevier AN - OPUS4-46858 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -