TY - JOUR A1 - Höhm, S. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Laser-induced periodic surface structures on titanium upon single- and two-color femtosecond double-pulse irradiation N2 - Single- and two-color double-fs-pulse experiments were performed on titanium to study the dynamics of the formation of laser-induced periodic surface structures (LIPSS). A Mach-Zehnder inter-ferometer generated polarization controlled (parallel or cross-polarized) double-pulse sequences in two configurations – either at 800 nm only, or at 400 and 800 nm wavelengths. The inter-pulse delays of the individual 50-fs pulses ranged up to some tens of picoseconds. Multiple of these single- or two-color double-fs-pulse sequences were collinearly focused by a spherical mirror to the sample surface. In both experimental configurations, the peak fluence of each individual pulse was kept below its respective ablation threshold and only the joint action of both pulses lead to the formation of LIPSS. Their resulting characteristics were analyzed by scanning electron microscopy and the periods were quantified by Fourier analyses. The LIPSS periods along with the orientation allow a clear identification of the pulse which dominates the energy coupling to the material. A plasmonic model successfully explains the delay-dependence of the LIPSS on titanium and confirms the importance of the ultrafast energy deposition stage for LIPSS formation. PY - 2015 DO - https://doi.org/10.1364/OE.23.025959 SN - 1094-4087 VL - 23 IS - 20 SP - 25959 EP - 25971 PB - Optical Society of America CY - Washington, DC AN - OPUS4-34354 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Farag, Zeinab Ramadan A1 - Friedrich, Jörg Florian A1 - Krüger, Simone A1 - Hidde, Gundula A1 - Moustapha, M. E. T1 - Adhesion promotion of thick polyphosphate-poly(allylamine) films onto polyolefin substrates by plasma polymers N2 - The adhesion of thick poly(allylamine)-polyphosphate layers (1 µm) deposited by the wet-chemical layer-by-layer technique (LbL) onto polyethylene or polystyrene (each 100 µm) was very low. To promote the adhesion of these LbL layers the polyolefin substrates were oxidized at the surface by short exposure to the oxygen plasma (2 or 5 s) and subsequently coated with an interlayer of plasma-deposited poly(allylamine) or poly(allyl alcohol) (100 nm). The plasma polymer interlayers have improved strongly the adhesion between polyolefin substrates and polyphosphate coatings. Such phosphate coatings are interesting for life sciences (nucleotide formation) but also for fire retardancy in combination with N-rich compounds such as melamine. The intention was to prefer chemical and hydrogen bonds for adhesion promoting because of their high binding energy. Therefore, the introduced oxygen-containing groups at the polyolefin surface could interact with the OH or NH2 groups of the adhesion-promoting plasma polymer interlayer. These groups were also able to interact strongly with the poly(allylamine)-polyphosphate topcoating. The coated polyolefins were investigated using Fourier Transform Infrared Spectroscopy in Attenuated Total Reflectance mode (FTIR-ATR), X-ray Photoelectron Spectroscopy (XPS), Thermo-Gravimetric Analyses (TGA) and Atomic Force Spectroscopy (AFM) and 90° peel test. KW - Plasma-polymerized poly(allylamine) KW - Adhesion KW - Layer-by-layer deposition KW - Plasma polymerization PY - 2016 UR - http://www.tandfonline.com/doi/abs/10.1080/01694243.2015.1095626 DO - https://doi.org/10.1080/01694243.2015.1095626 SN - 1648-4142 VL - 30 IS - 3 SP - 231 EP - 246 PB - Taylor & Francis AN - OPUS4-35885 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Höhm, S. A1 - Koter, Robert A1 - Hartelt, Manfred A1 - Spaltmann, Dirk A1 - Pentzien, Simone A1 - Rosenfeld, A. A1 - Krüger, Jörg T1 - Tribological performance of sub-100-nm femtosecond laser-induced periodic surface structures on titanium N2 - Sub-100-nm laser-induced periodic surface structures (LIPSS) were processed on bulk titanium (Ti) surfaces by femtosecond laser pulse irradiation in air (30 fs pulse duration, 790 nm wavelength). The laser peak fluence, the spatial spot overlap, and the number of overscans were optimized in a sample-scanning geometry in order to obtain large surface areas (5 mm × 5 mm) covered homogeneously by the LIPSS. The laser-processed regions were characterized by optical microscopy (OM), white light interference microscopy (WLIM) and scanning electron microscopy (SEM). The friction coefficient of the nanostructured surfaces was tested during 1000 cycles under reciprocal sliding conditions (1 Hz, 1.0 N normal load) against a 10-mm diameter ball of hardened 100Cr6 steel, both in paraffin oil and in engine oil used as lubricants. Subsequently, the corresponding wear tracks were qualified by OM, SEM, and energy dispersive X-ray analyses (EDX). The results of the tribological tests are discussed and compared to that obtained for near wavelength-sized fs-LIPSS, processed under somewhat different irradiation conditions. Some constraints for a beneficial effect of LIPSS on the tribological performance are provided. KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures, LIPSS KW - Friction KW - Wear KW - Nanostructures KW - Surface functionalization PY - 2016 UR - http://www.sciencedirect.com/science/article/pii/S0169433215026987 DO - https://doi.org/10.1016/j.apsusc.2015.11.019 SN - 0169-4332 SN - 1873-5584 VL - 374 SP - 190 EP - 196 PB - Elsevier B.V. CY - Amsterdam, Netherlands AN - OPUS4-35937 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Höhm, S. A1 - Herzlieb, M. A1 - Rosenfeld, A. A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Dynamics of the formation of laser-induced periodic surface structures (LIPSS) upon femtosecond two-color double-pulse irradiation of metals, semiconductors, and dielectrics N2 - In order to address the dynamics and physical mechanisms of LIPSS formation for three different classes of materials (metals, semiconductors, and dielectrics), two-color double-fs-pulse experiments were performed on Titanium, Silicon and Fused Silica. For that purpose a Mach–Zehnder interferometer generated polarization controlled (parallel or cross-polarized) double-pulse sequences at 400 nm and 800 nm wavelength, with inter-pulse delays up to a few picoseconds. Multiple of these two-color double-pulse sequences were collinearly focused by a spherical mirror to the sample surfaces. The fluence of each individual pulse (400 nm and 800 nm) was always kept below its respective ablation threshold and only the joint action of both pulses lead to the formation of LIPSS. Their resulting characteristics (periods, areas) were analyzed by scanning electron microscopy. The periods along with the LIPSS orientation allow a clear identification of the pulse which dominates the energy coupling to the material. For strong absorbing materials (Silicon, Titanium), a wavelength-dependent plasmonic mechanism can explain the delay-dependence of the LIPSS. In contrast, for dielectrics (Fused Silica) the first pulse always dominates the energy deposition and LIPSS orientation, supporting a non-plasmonic formation scenario. For all materials, these two-color experiments confirm the importance of the ultrafast energy deposition stage for LIPSS formation. KW - Femtosecond laser ablation KW - Double-pulse experiments KW - Laser-induced periodic surface structures (LIPSS) KW - Mach-Zehnder interferometer KW - Ultrafast optical techniques PY - 2016 UR - http://www.sciencedirect.com/science/article/pii/S0169433215031347 DO - https://doi.org/10.1016/j.apsusc.2015.12.129 SN - 0169-4332 SN - 1873-5584 VL - 374 SP - 331 EP - 338 PB - Elsevier CY - Amsterdam, Netherlands AN - OPUS4-35938 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Krüger, Jörg T1 - Nanosecond laser damage of optical multimode fibers N2 - For pulse laser materials processing often optical step index and gradient index multimode fibers with core diameters ranging from 100 to 600 μm are used. The design of a high power fiber transmission system must take into account limitations resulting from both surface and volume damage effects. Especially, breakdown at the fiber end faces and self-focusing in the fiber volume critically influence the fiber performance. At least operation charts are desirable to select the appropriate fiber type for given laser parameters. In industry-relevant studies the influence of fiber core diameter and end face preparation on laser-induced (surface) damage thresholds (LIDT) was investigated for frequently used all-silica fiber types (manufacturer LEONI). Experiments on preform material (initial fiber material) and compact specimens (models of the cladding and coating material) accompanied the tests performed in accordance with the relevant LIDT standards ISO 11254-1 and ISO 11254-2 for 1-on-1 and S-on-1 illumination conditions, respectively. The relation beam diameter vs. LIDT was investigated for fused silica fibers and preforms. Additionally, the laser-induced (bulk) damage threshold of fused silica preform material F300 (manufacturer Heraeus) in dependence on external mechanical stress simulating fiber bending was measured. All experiments were performed with 10-ns laser pulses at 1064 and 532 nm wavelength with a Gaussian beam profile. T2 - Pacific Rim Laser Damage Conference CY - Yokohama, Japan DA - 18.05.2016 KW - Laser induced damage KW - Optical multimode fiber KW - Nd:YAG laser KW - Nanosecond Pulses PY - 2016 AN - OPUS4-36258 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Krüger, Jörg T1 - Herausforderungen der Femtosekunden-Technologie an den Laserschutz N2 - Die Verleihung des Deutschen Zukunftspreises an ein Team zum Thema "Ultrakurzpulslaser für die industrielle Massenfertigung - Produzieren mit Lichtblitzen" im Jahr 2013 belegt die industrielle Relevanz des Ultrakurzpulslasereinsatzes in der Materialbearbeitung. Zunehmend werden weitere Anwendungen z.B. in der Mess- und Medizintechnik erschlossen. Femtosekunden-Laserpulse weisen prinzipbedingt ein breites Spektrum auf und besitzen bereits bei moderaten Pulsenergien extreme Pulsspitzenleistungen, womit über „konventionelle“ Laserquellen hinausgehende Herausforderungen an den Laserschutz entstehen. Die in entsprechenden Laserschutzbrillen verwendeten Laserschutzfilter müssen eine große spektrale Absorptionsbandbreite aufweisen und dürfen nicht aufschalten, d.h. keine induzierte Transmission zeigen. Im Vortrag soll dargestellt werden, dass Laserschutzfilter auf Glasbasis, die über ein breites Absorptionsspektrum verfügen, einen ausreichenden Schutz gegenüber fs-Laserstrahlung bieten, wohingegen Laserschutzfilter auf Polymerbasis eine induzierte spektrale Transmission bei steigender Energiedichte aufweisen können, was zu einem drastischen Verlust der Schutzfunktion führt. T2 - Symposium Strahlenschutz – Neue Technologien im Laserschutz CY - BIZBw, Mannheim, Germany DA - 17.11.2015 KW - Laserschutz KW - Schutzbrille KW - Ultrakurzpulslaser KW - Glasfilter KW - Polymerfilter PY - 2015 AN - OPUS4-36259 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Krüger, Jörg T1 - Ultrakurze Laserpulse für technische und biomedizinische Applikationen T2 - Workshop "Brillante Diodenlaser für neue Anwendungen in der Lasermaterialbearbeitung" CY - Berlin, Germany DA - 2014-03-18 PY - 2014 AN - OPUS4-30579 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lone, S. A. A1 - Muck, M. A1 - Fosodeder, P. A1 - Mardare, C.C. A1 - Florian, Camilo A1 - Weth, A. A1 - Krüger, Jörg A1 - Steinwender, C. A1 - Baumgartner, W. A1 - Bonse, Jörn A1 - Heitz, J. A1 - Hassel, A.W. T1 - Impact of Femtosecond Laser Treatment Accompanied with Anodization of Titanium Alloy on Fibroblast Cell Growth N2 - Herein, Ti6Al4V alloy is surface modified by femtosecond laser ablation. The microstructure image obtained by secondary electron microscopy reveals a combination of micrometer spikes or cones superimposed by nanoripples (laser‐induced periodic surface structures). To make the surface hydrophilic, anodization is performed resulting in further smoothness of microstructure and a final thickness of 35 ± 4 nm is estimated for oxide produced after anodization at 10 V (scan rate = 0.1 V s−1) versus standard hydrogen electrode. The obtained electrochemically active surface area (ECSA) is approximately 8 times larger compared with flat mirror polished Ti6Al4V surface. Combined chemical analysis by Pourbaix diagram and X‐ray photoelectron spectroscopy (XPS) analyses reveal that titanium and aluminum are passivating into TiO2 and Al2O3, but the dissolution of aluminum in the form of solvated ion is inevitable. Finally, cell seeding experiments on anodized and laser‐treated titanium alloy samples show that the growth of murine fibroblast cells is significantly suppressed due to unique surface texture of the laser‐treated and anodized titanium alloy sample. KW - Anodization KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures, LIPSS KW - Ti6Al4V alloys KW - X-ray photoelectron spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-510263 DO - https://doi.org/https://doi.org/10.1002/pssa.201900838 SN - 1862-6300 SN - 1862-6319 VL - 217 IS - 13 SP - 1900838-1 EP - 1900838-9 PB - WILEY-VCH Verlag CY - Weinheim, Germany AN - OPUS4-51026 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stolzenberg, U. A1 - Schmitt Rahner, M. A1 - Pullner, B. A1 - Legall, Herbert A1 - Bonse, Jörn A1 - Kluge, M. A1 - Ortner, A. A1 - Hoppe, B. A1 - Krüger, Jörg T1 - X-ray emission hazards from ultrashort pulsed laser material processing in an industrial setting N2 - Interactions between ultrashort laser pulses with intensities larger than 10^13 W/cm^2 and solids during material processing can lead to the emission of X-rays with photon energies above 5 keV, causing radiation hazards to operators. A framework for inspecting X-ray emission hazards during laser material processing has yet to be developed. One requirement for conducting radiation protection inspections is using a reference scenario, i.e., laser settings and process parameters that will lead to an almost constant and high level of X-ray emissions. To study the feasibility of setting up a reference scenario in practice, ambient dose rates and photon energies were measured using traceable measurement equipment in an industrial setting at SCHOTT AG. Ultrashort pulsed (USP) lasers with a maximum average power of 220 W provided the opportunity to measure X-ray emissions at laser peak intensities of up to 3.3 × 10^15 W/cm^2 at pulse durations of ~1 ps. The results indicate that increasing the laser peak intensity is insufficient to generate high dose rates. The investigations were affected by various constraints which prevented measuring high ambient dose rates. In this work, a list of issues which may be encountered when performing measurements at USP-laser machines in industrial settings is identified. KW - X-ray emission hazards KW - Ultrashort pulsed laser KW - Radiation protection KW - Industrial applications KW - Protection housing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-538632 DO - https://doi.org/10.3390/ma14237163 SN - 1996-1944 VL - 14 SP - 1 EP - 17 PB - MDPI CY - Basel AN - OPUS4-53863 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Legall, Herbert A1 - Bonse, Jörn A1 - Krüger, Jörg T1 - Emission of X-rays during ultrashort pulse laser processing N2 - Ultrashort pulse laser materials processing can be accompanied by the production of X-rays. Small doses per laser pulse can accumulate to significant dose rates at high laser pulse repetition rates which may exceed the permitted X-ray limits for human exposure. Consequently, a proper radiation shielding must be considered in laser machining. A brief overview of the current state of the art in the field of undesired generation of X-ray radiation during ultrashort pulse laser material processing in air is presented. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - Ultra-short pulse laser processing KW - Laser-induced X-ray emission KW - Radiation protection PY - 2021 SP - 1 EP - 5 AN - OPUS4-53866 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -