TY - JOUR A1 - Ringleb, F. A1 - Eylers, K. A1 - Teubner, T. A1 - Schramm, H.-P. A1 - Symietz, Christian A1 - Bonse, Jörn A1 - Andree, Stefan A1 - Heidmann, B. A1 - Schmid, M. A1 - Krüger, Jörg A1 - Boeck, T. T1 - Growth and shape of indium islands on molybdenum at micro-roughened spots created by femtosecond laser pulses N2 - Indium islands on molybdenum coated glass can be grown in ordered arrays by surface structuring using a femtosecond laser. The effect of varying the molybdenum coated glass substrate temperature and the indium deposition rate on island areal density, volume and geometry is investigated and evaluated in a physical vapor deposition (PVD) process. The joined impact of growth conditions and spacing of the femtosecond laser structured spots on the arrangement and morphology of indium islands is demonstrated. The results yield a deeper understanding of the island growth and its precise adjustment to industrial requirements, which is indispensable for a technological application of such structures at a high throughput, for instance as precursors for the preparation of Cu(In,Ga)Se2 micro concentrator solar cells. KW - Indium islands KW - Femtosecond laser patterning KW - Diffusion KW - CIGSe micro solar cells PY - 2017 UR - http://www.sciencedirect.com/science/article/pii/S0169433216325764 DO - https://doi.org/10.1016/j.apsusc.2016.11.135 SN - 0169-4332 SN - 1873-5584 VL - 418 SP - 548 EP - 553 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-40551 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gappenach, C. A1 - Krauß, H.-J. A1 - Krüger, Jörg A1 - Offenhäuser, F. A1 - Pintaske, S. T1 - Auswahl Laserschutzprodukte - eine Handreichung N2 - Wer mit Laserstrahlung zu tun hat, sollte vor allem auf den Schutz seiner Augen achten, denn die Netzhaut ist eines der empfindlichsten Gewebe des menschlichen Körpers. Auch die Hornhaut des Auges kann durch Laserstrahlung gefährdet sein. Sie hat eine Dicke von nur etwa 0,5 mm. Der Schutz der Augen vor Laserstrahlung ist durch verschiedene Maßnahmen möglich. KW - Laserschutz KW - Schutzbrille KW - Justierbrille KW - Abschirmung KW - EN 207 KW - EN 208 KW - EN 12254 PY - 2015 SN - 1432-9778 VL - 3 SP - 40 EP - 45 PB - AT-Fachverl. CY - Fellbach AN - OPUS4-33431 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gappenach, C. A1 - Krüger, Jörg A1 - Offenhäuser, F. A1 - Pintaske, S. A1 - Krauß, H.-J. T1 - Selecting laser eye protectors - a helping hand N2 - The European laser safety standards EN 207, EN 208, and EN 12254 each contain an annex B, which serves as a guidance for the selection of products. These annexes are informative only and are therefore not binding. As there are a variety of hazard scenarios, it is not recommended to change these annexes to a normative status, through which they would become mandatory. Instead, it is recommended to allow users to apply their own skills and know-how in selecting appropriate products, justifying where and why they deviate from the guidance in the standards. This paper explains the background on which the guidance for selection in the annexes of the standards is based and shows physically meaningful leeway. KW - European standard KW - Laser safety KW - Personal protective equipment PY - 2015 DO - https://doi.org/10.1515/aot-2015-0043 SN - 2192-8576 SN - 2192-8584 VL - 4 IS - 5-6 SP - 389 EP - 395 PB - De Gruyter CY - Berlin; Boston, Mass. AN - OPUS4-35072 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Reuther, F. A1 - Krüger, Ralph-Peter A1 - Schulz, Günter A1 - Baehr, G. A1 - Westerwelle, U. A1 - Gruetzner, G. ED - Houlihan, F. M. T1 - Tailored novolak resins for advanced photoresists by a two-step procedure - new insight into the molecular structure by coupling GPC and MALDI-TOF-MS T2 - 17th Annual SPIE Conference on Advances in Resist Technology and Processing CY - Santa Clara, CA, USA DA - 2000-02-28 KW - Novolak KW - Structure KW - Synthesis KW - Gel permeation KW - Chromatography KW - MALDI-TOF-MS PY - 2000 SN - 0-8194-3617-8 SN - 1605-7422 N1 - Serientitel: SPIE proceedings series – Series title: SPIE proceedings series IS - 3999 SP - 464 EP - 471 PB - SPIE CY - Bellingham AN - OPUS4-2171 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Kautek, Wolfgang A1 - Hertwig, Andreas A1 - Martin, Sven A1 - Krüger, Jörg A1 - Lenzner, Matthias A1 - Spielmann, C. A1 - Lenner, M. A1 - Bunte, J. A1 - Puester, T. A1 - Burmester, T. A1 - Fiedler, A. A1 - Heberer, E. A1 - Brose, M. A1 - Stingl, A. A1 - Kiehl, P. A1 - Hönigsmann, H. A1 - Trautinger, F. A1 - Grabner, G. T1 - Safety in Femtosecond Laser Technology - Recent Results of a European Research Project (406) T2 - International Laser Safety Conference 2003 ; ILSC 2003 CY - Jacksonville, FL, USA DA - 2003-03-10 PY - 2003 SN - 0-912035-38-2 SP - 1(?) EP - 10(?) PB - Laser Institute of America CY - Orlando, Fla. AN - OPUS4-2259 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, C. A1 - Krausz, F. ED - Dubowski, J. T1 - Structuring of dielectric and metallic materials with ultrashort laser pulses between 20 fs and 3 ps N2 - Laser-micromachining of barium aluminum borosilicate glass, fused silica and stainless steel has been extended down to a pulse duration of 20 fs generated by a Ti:sapphire laser system at a wavelength of 0.8 micrometer. A systematic study shows that, below 100 fs, an enhanced precision and a substantial decrease of the ablation threshold fluence in comparison to pulse laser processing with pulses in the picosecond and nanosecond range could be achieved. The physical mechanism and the technical relevance of this novel microtechnology is discussed. T2 - Conference CY - San José, CA, USA DA - 1997-02-10 KW - Ablation KW - Laser processing KW - Micromachining KW - Structuring KW - Femtosecond pulse laser KW - Glass KW - Silica KW - Steel PY - 1997 SN - 0-8194-2402-1 DO - https://doi.org/10.1117/12.273740 SN - 1605-7422 N1 - Serientitel: SPIE proceedings series – Series title: SPIE proceedings series IS - 2991 SP - 40 EP - 47 PB - SPIE CY - Bellingham, Wash. AN - OPUS4-11893 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, C. A1 - Krausz, F. A1 - Krüger, Jörg A1 - Kautek, Wolfgang T1 - Nanometer precision material ablation and optical breakdown with sub-10 fs pulses T2 - 11th International Conference on Ultrafast Phenomena CY - Garmisch-Partenkirchen, Germany DA - 1998-07-12 PY - 1998 SN - 3-540-65430-5 SN - 0172-6218 N1 - Serientitel: Springer Series in chemical physics – Series title: Springer Series in chemical physics IS - 63 SP - 313 EP - 315 PB - Springer CY - Heidelberg AN - OPUS4-12042 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, C. A1 - Krausz, F. A1 - Krüger, Jörg A1 - Kautek, Wolfgang T1 - Optical Damage of Dielectrics down to 5 fs T2 - 17th Conference on Lasers and Electro-Optics (CLEO) CY - Baltimore, MD, USA DA - 1997-05-18 PY - 1997 SN - 1-557-52498-X IS - 11 SP - 218 EP - 219 PB - Optical Society of America CY - Washington, DC AN - OPUS4-12043 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kautek, Wolfgang A1 - Krüger, Jörg A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, Ch. A1 - Krausz, F. T1 - Laser ablation of dielectrics with pulse durations between 20 fs and 3 ps PY - 1996 SN - 0003-6951 SN - 1077-3118 VL - 69 IS - 21 SP - 3146 EP - 3148 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-11496 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lenzner, Matthias A1 - Krüger, Jörg A1 - Sartania, S. A1 - Cheng, Z. A1 - Spielmann, Ch. A1 - Mourou, G. A1 - Kautek, Wolfgang A1 - Krausz, F. T1 - Femtosecond Optical Breakdown in Dielectrics N2 - We report measurements of the optical breakdown threshold and ablation depth in dielectrics with different band gaps for laser pulse durations ranging from 5 ps to 5 fs at a carrier wavelength of 780 nm. For tau <100 fs, the dominant channel for free electron generation is found to be either impact or multiphoton ionization (MPI) depending on the size of the band gap. The observed MPI rates are substantially lower than those predicted by the Keldysh theory. We demonstrate that sub-10-fs laser pulses open up the way to reversible nonperturbative nonlinear optics (at intensities greater than 1014 W/cm2 slightly below damage threshold) and to nanometer-precision laser ablation (slightly above threshold) in dielectric materials. PY - 1998 SN - 0031-9007 SN - 1079-7114 VL - 80 IS - 18 SP - 4076 EP - 4079 PB - American Physical Society CY - Ridge, NY AN - OPUS4-11518 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Rücker, Werner A1 - Krüger, F. A1 - Savidis, S. A1 - Auersch, Lutz ED - Aubram, D. T1 - Ein umfassendes Prognoseprogramm für Erschütterungen T2 - 2. Hans Lorenz Symposium CY - Berlin, Deutschland DA - 2006-10-12 PY - 2006 SN - 3-7983-2024-1 N1 - Serientitel: Veröffentlichungen des Grundbauinstitutes der technischen Universität Berlin – Series title: Veröffentlichungen des Grundbauinstitutes der technischen Universität Berlin IS - 40 SP - 159 EP - 170 PB - TU Berlin CY - Berlin AN - OPUS4-13736 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Oberlies, F. A1 - Krüger, D. T1 - Verfahren zur Untersuchung von asbesthaltigen Erzeugnissen PY - 1942 SN - 0372-7076 IS - II. Folge/Heft 4 SP - 24 EP - 31 PB - Springer CY - Berlin AN - OPUS4-28416 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Sartania, S. A1 - Spielmann, C. A1 - Krausz, F. T1 - Laser micromachining of barium aluminium borosilicate glass with pulse durations between 20 fs and 3 ps N2 - Laser-micromachining of high-tech glass has been extended down to a pulse duration of 20 fs generated by a Ti sapphire laser system at a wavelength of 780 nm. A systematic electronmicroscopic study shows that, below 100 fs, an extreme precision and a substantial decrease of the ablation threshold fluence with respect to pulse laser processing with pulses in the picosecond and nanosecond range could be achieved. The technical relevance of this novel microtechnology is discussed. The morphology of the ablated areas is not determined by thermal processes, i.e. the heat affected zone. It is controlled by non-linear optical coupling effects. Multi-photon absorption becomes highly efficient below laser pulse durations of 100 fs so that light penetration is minimized and ablation cavities become smooth. At longer pulse durations, a higher light penetration due to a lower number of non-linearly absorbed photons allows mechanical relaxation processes in the glass material leading to roughening. KW - Laser micromachining KW - Subpicosecond laser ablation KW - Barium aluminium borosilicate glass PY - 1998 DO - https://doi.org/10.1016/S0169-4332(97)00763-0 SN - 0169-4332 SN - 1873-5584 IS - 127-129 SP - 892 EP - 898 PB - North-Holland CY - Amsterdam AN - OPUS4-887 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Krausz, F. T1 - Precision laser ablation of dielectrics in the 10-fs regime N2 - Zusammenfassung Laser pulses in the 10-fs domain provide a quality of micromachining of fused silica and borosilicate glass that is unobtainable with longer pulses in the range of several 100 femtoseconds up to picoseconds. The shortening of the pulses reduces the statistical behavior of the material removal and the ablation process thus attains a more deterministic and reproducible character. The improved reproducibility of ablation is accompanied by significantly smoother morphology. This offers the potential for lateral and vertical machining precision of the order of 100 nm and 10 nm, respectively. KW - Laser ablation PY - 1999 DO - https://doi.org/10.1007/s003390050906 SN - 0947-8396 VL - 68 IS - 3 SP - 369 EP - 371 PB - Springer CY - Berlin AN - OPUS4-825 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Krausz, F. T1 - Incubation of laser ablation in fused silica with 5-fs pulses N2 - Zusammenfassung The threshold fluences for laser-induced damage of fused silica with single 5-fs pulses from a Ti:sapphire laser system were determined by extrapolating the ablated volume to zero. These thresholds are about 4 times as high as the values previously obtained from multi-shot experiments. This result is interpreted in terms of an irreversible modification of the original material below the single-shot threshold (incubation). KW - Laser PY - 1999 DO - https://doi.org/10.1007/s003390051034 SN - 0947-8396 VL - 69 IS - 4 SP - 465 EP - 466 PB - Springer CY - Berlin AN - OPUS4-799 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Jörg A1 - Kautek, Wolfgang A1 - Lenzner, M. A1 - Krausz, F. T1 - Photoablation with sub-10 fs laser pulses N2 - Ablation experiments in several glasses with single and multishot irradiation by laser pulses in the 10-fs pulse duration domain are presented; physical and technological implications are discussed. We demonstrate that these short pulses offer the potential for lateral and vertical machining precision of the order of 100 nm. KW - Ablation KW - Laser pulses KW - Femtosecond pulses PY - 2000 DO - https://doi.org/10.1016/S0169-4332(99)00432-8 SN - 0169-4332 SN - 1873-5584 VL - 154-155 SP - 11 EP - 16 PB - North-Holland CY - Amsterdam AN - OPUS4-800 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Lucka, R. A1 - Elshani, B. A1 - Kilic, M. S. A1 - Klimke, S. A1 - Krüger, C. A1 - Menzel, Michael A1 - Stößer, R. A1 - Titiš, J. A1 - Boča, R. A1 - Renz, F. T1 - ESR and Mössbauer spectroscopy of iron(III) spin crossover complexes based on pentadentate Schiff base ligands with pseudohalide coligands N2 - Two iron(III) spin crossover complexes [Fe(5Cl-L)(NCS)] (1) and [Fe(5Cl-L)(NCSe)] (2) were synthesized with the pentadentate Schiff base ligand 5Cl-L and thiocyanato and selenocyanato as coligands. 5Cl-L, as an asymmetric {N3O2} donor Schiff base, was synthesized by a condensation reaction of 5-chlorosalicyladehyde using the asymmetric N-(2-aminoethyl)-1,3-propanediamine. The complexes exhibited a spin crossover at 280 (1) and 293 K (2), respectively, and were subjected to electron spin resonance (ESR) and Mössbauer spectroscopy at 77, 295 and 325 K. Ab initio CASSCF calculations followed by the NEVPT2 method were applied for predicting the g-tensor components as well as Mössbauer parameters. KW - Spin crossover KW - Iron(III) complexes KW - Mössbauer spectroscopy KW - ESR spectroscopy KW - Ab initio calculations PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-634061 DO - https://doi.org/10.3390/magnetochemistry11050043 SN - 2312-7481 VL - 11 IS - 5 SP - 1 EP - 9 PB - MDPI CY - Basel AN - OPUS4-63406 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Werrel, Martin A1 - Deubel, Jan A1 - Krüger, Simone A1 - Hofmann-Böllinghaus, Anja A1 - Antonatus, E. A1 - Krause, U. A1 - Duerler, F. T1 - Use and benefit of a controlled-atmosphere cone calorimeter N2 - A controlled-atmosphere cone calorimeter that is built by modifying the Standard apparatus with the addition of a controlled-atmosphere chamber offers a time- and cost-saving approach for reaction-to-fire testing in vitiation- and ventilation-controlled atmospheres. Due to the design of the added enclosure no mechanical changes on cone calorimeter’s Standard ductwork are required. This offers some advantages but also important limitations. The design has an open connection between the outlet of the added enclosure and the cone calorimeter’s exhaust hood. Therefore, sufficient ambient air from the laboratory surroundings is drawn into the System to introduce effects which have the potential to affect test results significantly. A procedure which is is suitable to consider physical effects of the ambient air on the calculation of the heat release rate is presented as well as initial results of an application towards toxic potency assessment. Signs for Chemical effects of the ambient air such as post reactions are shown but subject of an ongoing work. T2 - Fire and materials 2013 - 13th International conference and exhibition CY - San Francisco, CA, USA DA - 28.01.2013 KW - Controlled-atmosphere cone calorimeter KW - Heat release rate KW - Oxygen consumption KW - Smoke toxicity PY - 2013 SP - 273 EP - 286 PB - Interscience Communications CY - London, UK AN - OPUS4-27707 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Oliver A1 - Fiedler, F. A1 - Adam, Christian A1 - Vogel, Christian A1 - Senz, R. T1 - Determination of chromium (VI) in primary and secondary fertilizer and their respective precursors N2 - Hexavalent chromium species (Cr(VI)) are often carcinogenic, of high acute toxicity, highly mobile, and thus pose a severe risk to health and environment. Fertilizers usually contain significant amounts of chromium. Therefore, a reliable analysis of chromium and the fraction of Cr(VI) are crucial for safe use of fertilizers. This problem is expected to increase in the future, since more and more recycled fertilizers emerge due to increasing fertilizer demand and respective supply risks. However, existing analytical methods have been developed for conventional fertilizers and have to be tested whether they are suitable for the new materials. Thus, we performed a wet-chemical extraction for Cr(VI) on several matrices as well as respective quality control experiments including spiking with Cr(III) and Cr(VI)compounds. We found the Cr(VI) amounts to be below 2 mg/kg except for a thermally post-treated sewage sludge ash (SSA) that showed 12.3 mg/kg. The presence of organic matter e.g. in sludge or precipitated struvite caused a reduction of spiked Cr(VI) and thus no satisfying recovery for Quality control. Cr(VI) reduction was also observed for SSA, presumably due to the presence of Fe(II) compounds. Even though the tested procedure can be hampered in some recycled fertilizer matrices, it might be adapted to be applicable also for these complex samples. KW - Chromium speciation KW - Recycling fertilizers KW - Matrix dependencies PY - 2017 DO - https://doi.org/10.1016/j.chemosphere.2017.05.011 SN - 0045-6535 VL - 182 SP - 48 EP - 53 PB - Elsevier CY - Amsterdam AN - OPUS4-40101 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Maresca, A. A1 - Krüger, O. A1 - Herzel, Hannes A1 - Adam, Christian A1 - Kalbe, Ute A1 - Astrup, T. F. T1 - Influence of wood ash pre-treatment on leaching behaviour, liming and fertilising potential N2 - In Denmark, increasing amounts of woody biomass are being used for the production of renewable energy, resulting in more wood ashes being generated. While these materials have been mainly landfilled, wood ashes may also be utilised for fertilizing and liming purposes on top of soils. Pre-treatments involving hardening or granulation may be carried out prior to soil application. In this study, two Danish wood ash samples were hardened and/or granulated. Lab-hardening induced rapid changes in the shape of the acid neutralisation capacity curve of the ashes. Up-flow column tests, assuming local equilibrium conditions, were employed to investigate the leaching from pre-treated ashes. Granules and loose ashes demonstrated similar leaching behaviours, indicating that similar geochemical processes were governing their leaching. In comparison with untreated fresh ashes, the hardened ashes demonstrated reduced leaching of Ca, Ba, Pb and Zn with concentration levels generally below or close to the analytical limits of quantification; to the contrary, the leaching of As, P, Sb, Si, V and Mg was enhanced in the hardened ashes. The release of alkalinity was reduced by hardening. In general, all granules were barely breakable by finger-pinching and they could withstand one month of continuous leaching, preserving their overall shape. The solubility of phosphorous in neutral ammonium citrate indicated that about 30–51% of the total P content in the ash samples was released, suggesting that the ashes could be potentially valuable as P-fertiliser if applied onto soil. KW - Wood ash KW - Phoshpor availability KW - Leaching KW - Forest soils PY - 2019 DO - https://doi.org/10.1016/j.wasman.2018.11.003 SN - 0956-053X VL - 83 SP - 113 EP - 122 PB - Elsevier AN - OPUS4-46583 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -