TY - GEN A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Eberstein, Markus A1 - Deubener, J. A1 - Thiel, A. A1 - Schiller, Wolfgang Arno ED - J.G. Heinrich, ED - C.G. Aneziris, T1 - Effect of dispersed Al2O3 particles on sintering of glass matrix composites T2 - 10th International Conference of the European Ceramic Society CY - Berlin DA - 2007-06-17 KW - LTCC KW - Glass matrix composites KW - Inclusions KW - Sintering kinetics KW - Modelling PY - 2007 SN - 3-87264-022-4 SP - 290 EP - 295 PB - Göller CY - Baden-Baden AN - OPUS4-17445 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Eberstein, Markus A1 - Deubener, J. A1 - Thiel, A. A1 - Schiller, Wolfgang Arno T1 - Effects of dispersed Al2O3 particles on sintering of LTCC N2 - The sintering of Low Temperature Co-fired Ceramics prepared from alumoborosilicate glass- and Al2O3 powders of similar small particle size was studied by dilatometry, heating microscopy, microstructure analysis, glass- and effective viscosity measurements. The steric effect of Al3O3 inclusions was studied using a gnon-reactiveh model composite. With increasing Al3O3 volume fraction (Φ ≤ 0.45), sintering decelerates and its final stage shifts to higher temperature. The attainable shrinkage is reduced as Al2O3 particle clusters bearing residual pores become more frequent. The kinetics of sintering could be described formally superposing the weighed contributions of differentially sized and randomly composed glass-crystal particle clusters and assuming a sintering rate controlled by the effective matrix viscosity, which increases with Φ and with progressive wetting of Al2O3 particles during densification. The "reactive" model composite shows significant dissolution of Al2O3 into the glass, which has two opposed effects on sintering: reducing Φ and increasing glass viscosity. For the present case (Φ = 0.25), the latter effect dominates and sintering is retarded by Al2O3 dissolution. Crystallization of wollastonite starts after full densification. Dissolution of Al2O3 was found to promote the subsequent growth of anorthite. KW - LTCC KW - Glass matrix composites KW - Al2O3-inclusions KW - Sintering kinetics PY - 2005 SN - 1022-6680 SN - 1662-8985 VL - 39-40 SP - 375 EP - 380 PB - Trans Tech Publ. CY - Zurich AN - OPUS4-18441 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zietka, S. A1 - Deubener, J. A1 - Behrens, H. A1 - Müller, Ralf T1 - Glass transition and viscosity of hydrated silica glasses N2 - The viscosity of silica glasses with different water contents was measured by penetration of sapphire microspheres in the range from 1012-1014·7 Pas at ambient pressure. Commercial silica glasses were used together with hydrous silica glasses, which were prepared by melting glass powder plus water in an internally heated pressure vessel at 2-3 kbar and 1350-1450°C. The temperature dependence of the viscosity of silica glasses with total water contents Cw of 5·4×10-4, 7·0×10-4, 1·00×10-2, and 1·55×10-2(Cw in mass fractions) can be described by Arrhenius equations. From the results, the linear dependence of the T12 isokom (K) with the logarithm of the water content was determined as T12=192-409 logCw. The analysis of the compositional dependence of the T12 isokom in the H2O-Na2O-SiO2 system reveals a temperature depression of up to 200 K for mixed water- and sodium-bearing glasses compared to H2O-SiO2 and Na2O-SiO2 glasses with same molar silica content. From these findings we conclude that protons may contribute significantly to the mixed alkali effect in glasses. KW - Wassergehalt KW - Silicatgläser KW - Viskosität PY - 2007 SN - 1753-3562 SN - 0017-1050 SN - 0031-9090 SN - 1750-6697 VL - 48 IS - 6 SP - 380 EP - 387 PB - Society of Glass Technology CY - Sheffield AN - OPUS4-18396 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Eberstein, Markus A1 - Reinsch, Stefan A1 - Schiller, Wolfgang Arno A1 - Deubener, J. A1 - Thiel, A. T1 - Effect of rigid inclusions on sintering of low temperature co-fired ceramics KW - Sintering KW - Glass Matrix Composites KW - Rigid Inclusion KW - Effective Viscosity KW - Kinetic Modelling KW - LTCC PY - 2007 SN - 1753-3562 SN - 0017-1050 SN - 0031-9090 SN - 1750-6697 VL - 48 IS - 4 SP - 259 EP - 266 PB - Society of Glass Technology CY - Sheffield AN - OPUS4-16211 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, J. A1 - Kiechle, H. A1 - Ewert, Uwe A1 - Rädel, Christoph A1 - Redmer, Bernhard T1 - Mobile Computer Tomography for In-Service Inspection in Nuclear Power Plants T2 - 9th European Conference on NDT CY - Berlin, Germany DA - 2006-09-25 KW - Röntgen KW - Digitale Detektoren KW - Tomographie KW - TomoCAR KW - Schweißnähte KW - Analyse KW - Bewertung PY - 2006 SN - 3-931381-86-2 SP - 1(?) EP - 6(?) PB - European Federation for Non-Destructive Testing CY - Berlin AN - OPUS4-14376 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Reinsch, Stefan A1 - Meng, S. A1 - Eberstein, Markus A1 - Thiel, A. A1 - Müller, Ralf A1 - Deubener, J. T1 - Partial Solution of Dispersed alpha-Al2O3-Particles in Alumoborosilicate Glass T2 - 81. Glastechnische Tagung CY - Aachen, Deutschland DA - 2007-06-04 KW - Glasmatrixkomposite KW - Lösung KW - Sintern PY - 2007 SN - 978-3-921089-52-1 IS - CD-ROM SP - 1 EP - 5 PB - Deutsche Glastechnische Gesellschaft CY - Offenbach AN - OPUS4-16108 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, J. A1 - Behrens, H. A1 - Müller, Ralf A1 - Zietka, S. A1 - Reinsch, Stefan T1 - Kinetic fragility of hydrous soda-lime-silica glasses N2 - The effect of hydration on the kinetic fragility of soda-lime-silica glasses was investigated by viscometry in the glass transition range. Water-bearing glasses were prepared from industrial float glass (FG) and a ternary model glass (NCS = 16Na2O 10CaO 74SiO2 in mol%) by bubbling steam through the melt at 1480 °C and up to 7 bar. Additionally, a sodium borosilicate glass (NBS = 16Na2O 10B2O3 74SiO2 in mol%) was hydrated under equal conditions. As detected by infrared spectroscopy water dissolves in the glasses exclusively as OH-groups. The hydration resulted in a total water content CW up to ~ 0.2 wt% for FG, NCS and NBS glasses. Kinetic fragility, expressed by the steepness index m, was determined from the temperature dependence of η at the glass transition. Viscosity data from previous studies on hydrous float glasses (CW > 1 wt%) were surveyed together with literature data on the (H2O)–Na2O–CaO–SiO2, (H2O)–Na2O–SiO2 and (H2O)–SiO2 systems to expand the range of water concentration and bulk composition. We could demonstrate that m decreases for all glasses although water is dissolved as OH and should depolymerize the network. An empirical equation of the general type m = a - b logCW where a, b are fitting parameters, enables m to be predicted, for each glass series as function of the water content CW. The enlarged data base shows that the parameter B of the Arrhenius viscosity-temperature relation decreases much stronger than the isokom temperature at the glass transition. KW - Soda-lime-silica KW - Fragility KW - Viscosity KW - Water in glass PY - 2008 DO - https://doi.org/10.1016/j.jnoncrysol.2008.04.021 SN - 0022-3093 VL - 354 IS - 42-44 SP - 4713 EP - 4718 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-18187 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Bernd R. A1 - Lange, Axel A1 - Harwardt, Michael A1 - Hentschel, Manfred P. A1 - Illerhaus, Bernhard A1 - Goebbels, Jürgen A1 - Bamberg, J. A1 - Heutling, F. T1 - Refraction computed tomography - Application to metal matrix composites N2 - Erstmals wurden MMCs mit Hilfe der Interface-Kontrast verstärkenden Röntgen-Refraktions-Technik in Kombination mit der 3D-CT-Technik untersucht. Die Methode der Röntgen-Refraktions-Topography sowie der Röntgen-Refraktions-Tomography wurden in den letzten Jahren speziell für die zerstörungsfreie Charakterisierung von Leichtbau-Hochleistungs-Werkstoffen wie Verbund-Werkstoffen und Keramiken entwickelt. Die Technik basiert auf der Refraktion von Röntgenlicht an Grenzflächen zwischen Bereichen unterschiedlicher Elektronendichte wie z.B. Faser- und Matrix-Werkstoff. Auf Grund der kurzen Röntgen-Wellenlänge hat der Brechungsindex einen Wert dicht bei eins, sodass der Streuwinkel nur wenige Bogenminuten beträgt. Der Vorteil der kurzen Wellenlänge besteht jedoch darin, dass Poren und Risse detektiert werden können, deren Größe im Nanometerbereich liegen. Damit kann die Refraktions-Technik zum besseren Verständnis von Mikro- und Submikro-Strukturen in der Materialwissenschaft eingesetzt werden. Mit der hier vorgestellten Refraktions-CT wurden Ermüdungsmechanismen an MMCs, bestehend aus SiC-Faser verstärktem Titan (Ti6242) untersucht. Die Messungen wurden am Röntgen-Messplatz der BAM (BAMline) am Synchrotron-Speicherring-BESSY in Berlin Adlershof durchgeführt. KW - X-ray refraction KW - Computed tomography PY - 2004 DO - https://doi.org/10.3139/120.100592 SN - 0025-5300 VL - 46 IS - 6 SP - 314 EP - 319 PB - Carl Hanser Verlag CY - München AN - OPUS4-5870 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Müller, Christina A1 - Pavlovic, Mato A1 - Takahashi, Kazunori A1 - Ewert, Uwe A1 - Rosenthal, Martina A1 - Brekow, Gerhard A1 - Böhm, R. A1 - Ronneteg, U. A1 - Pitkänen, J. T1 - POD Evaluation of NDE Techniques for Canister-Components for Risk Assessment of Nuclear Waste Encapsulation T2 - 6th International Conference on NDE in Relation to Structural Integrity for Nuclear and Pressurised Components CY - Budapest, Hungary DA - 2007-10-08 KW - Zerstörungsfreie Prüfung KW - Zuverlässigkeit KW - POD PY - 2008 SN - 978-92-79-08897-1 DO - https://doi.org/10.2790/1274 SN - 1018-5593 SP - 168 EP - 179 AN - OPUS4-18589 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Müller, Christina A1 - Bertovic, Marija A1 - Gaal, Mate A1 - Heidt, Heinrich A1 - Pavlovic, Mato A1 - Rosenthal, Martina A1 - Takahashi, K. A1 - Pitkänen, J. A1 - Ronneteg, U. T1 - Progress in evaluating the reliability of NDE systems - Paradigm shift N2 - The paper will give an overview of new methodology for evaluating the reliability of NDE systems accurately, reliably and efficiently in accordance with the specific requirements of industrial application. After a review of the substantive issues from the previous workshops, the go forward guidance from these interactions is considered. At the beginning of the reliability analysis, the actual safety demands have to be defined in order to fit the investigation to the level of risk when the component would fail. Next, all the essential influencing parameters need to be documented and transferred to an appropriate design of experiments (DOE) to determine the reliability in terms of a qualitative assessment for lower risk or in terms of a quantitative probability of detection (POD) or ROC (Receiver Operating Characteristics) curves for higher safety demands. A new paradigm is offered to consider the POD or reliability of the system as a function of the configuration of input variables and use it for optimisation rather than for a final judgement. An advantage for the end user is also to sample all single PODs to an integral 'Volume POD' of a part. Among the influencing parameters, the human factor is the most important one. A systematic psychological approach shall help to find out where the bottlenecks are but most importantly to provide best possible working conditions for the human inspectors. T2 - 4th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2009-06-24 KW - Zuverlässigkeit von ZfP-Systemen KW - Multiparameter POD PY - 2009 UR - http://www.ndt.net/article/reliability2009/Inhalt/we1a2.pdf SN - 978-3-940283-17-7 IS - DGZfP-BB 116 SP - 1 EP - 13 AN - OPUS4-20616 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Takahashi, K. A1 - Pavlovic, Mato A1 - Ronneteg, U. A1 - Pitkänen, J. A1 - Müller, Christina T1 - Probability of detection from C-scan data for reliability analysis of ultrasonic non-destructive testing T2 - 4th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2009-06-24 KW - POD KW - UT KW - Reliability KW - C-scan PY - 2009 SN - 978-3-940283-17-7 IS - DGZfP-BB 116 SP - 1 EP - 7 AN - OPUS4-20617 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Pavlovic, Mato A1 - Takahashi, K. A1 - Ronneteg, U. A1 - Pitkänen, J. A1 - Müller, Christina T1 - Multi-parameter influence on the response of the flaw to the phased array ultrasonic NDT system. The volume POD. T2 - 4th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2009-06-24 KW - POD KW - Reliability KW - Multi-parameter signal response PY - 2009 SN - 978-3-940283-17-7 IS - DGZfP-BB 116 SP - 1 EP - 6 AN - OPUS4-20618 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Meszaros, Robert A1 - Peplinski, Burkhard A1 - Reinsch, Stefan A1 - Eberstein, Markus A1 - Schiller, Wolfgang Arno A1 - Deubener, J. T1 - Dissolution of alumina, sintering, and crystallization in glass ceramic composites for LTCC KW - LTCC KW - Sintering KW - Crystallization KW - Alumina dissolution KW - Rietveld analysis PY - 2009 DO - https://doi.org/10.1111/j.1551-2916.2009.03089.x SN - 0002-7820 SN - 1551-2916 VL - 92 IS - 8 SP - 1703 EP - 1708 PB - Blackwell Publishing CY - Malden AN - OPUS4-20676 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pitkänen, J. A1 - Salonen, T. A1 - Bertovic, Marija A1 - Müller, Christina A1 - Pavlovic, Mato T1 - NDT reliability in risk minimization during manufacturing and welding of spent nuclear fuel disposal components - a realistic tool for reliable inspections T2 - 4th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2009-06-24 KW - NDT reliability KW - Spent nuclear fuel KW - EB-weld PY - 2009 UR - http://www.ndt.net/article/reliability2009/Inhalt/fr1a2.pdf IS - Fr.1.A.2 SP - 1 EP - 21 AN - OPUS4-26082 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Behrens, H. T1 - Internal friction of hydrated soda-lime-silicate glasses N2 - The internal friction of hydrated soda-lime-silica glasses with total water content (CW ) up to 1.9 wt. % was studied by dynamic mechanical analysis (DMA) using temperature-frequency sweeps from 723 K to 273 K and from 1 s-1 to 50 s-1. Total water content and concentrations of H2O molecules (CH2O ) and OH groups (COH) in the DMA specimens were determined by infrared spectroscopy. For low water contents (CW ≈ COH < 0.25 wt. %) two discrete internal friction peaks below the glass transition (α relaxation) were assigned to the low-temperature motion of alkali ions (γ relaxation) and cooperative movements of dissimilar mobile species under participation of OH at higher temperature (βOH relaxation). For large water contents (CW > 1 wt. %), where significant amounts of molecular water are evident (CH2O > 0.15 wt. %), however, internal friction spectra change unexpectedly: the βOH peak heights saturate and a low temperature shoulder appears on the β-relaxation peak. This emerging relaxation mode (βH2O relaxation) was assigned to the motions of H2O molecules. βH2O relaxation was found to be faster than βOH but slower than γ relaxation. Activation energy of the different relaxation modes increased in the order γ < βH2O < βOH < α. KW - Internal friction KW - Glass KW - Water content PY - 2013 DO - https://doi.org/10.1063/1.4828740 SN - 0021-9606 SN - 1089-7690 VL - 139 SP - 174506-1 EP - 174506-6 PB - American Institute of Physics CY - Melville, NY AN - OPUS4-29698 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tielemann, Christopher A1 - Reinsch, Stefan A1 - Maaß, Robert A1 - Deubener, J. A1 - Müller, Ralf T1 - Internal nucleation tendency and crystal surface energy obtained from bond energies and crystal lattice data N2 - We present an easy-to-apply method to predict structural trends in the internal nucleation tendency of oxide glasses. The approach is based on calculated crystal fracture surface energies derived from easily accessible diatomic bond energy and crystal lattice data. The applicability of the method is demonstrated on literature nucleation data for isochemically crystallizing oxide glasses. KW - Glass KW - Nucleation tendency KW - Fracture surface energy KW - Crystal lattice KW - Bond energy PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-548814 DO - https://doi.org/10.1016/j.nocx.2022.100093 SN - 2590-1591 VL - 14 SP - 1 EP - 5 PB - Elsevier B.V. AN - OPUS4-54881 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sieber, M. J. A1 - Wilke, M. A1 - Appelt, O. A1 - Oelze, Marcus A1 - Koch-Müller, M. T1 - Melting relations of Ca–Mg carbonates and trace element signature of carbonate melts up to 9 GPa – A proxy for melting of carbonated mantle lithologies N2 - The most profound consequences of the presence of Ca–Mg carbonates (CaCO3–MgCO3) in the Earth’s upper mantle may be to lower the melting temperatures of the mantle and control the melt composition. Low-degree partial melting of a carbonate-bearing mantle produces CO2-rich, silica-poor melts compositionally imposed by the melting relations of carbonates. Thus, understanding the melting relations in the CaCO3–MgCO3 system facilitates the interpretation of natural carbonate-bearing silicate systems. We report the melting relations of the CaCO3–MgCO3 system and the partition coefficient of trace elements between carbonates and carbonate melt from experiments at high pressure (6 and 9 GPa) and temperature (1300–1800 ◦C) using a rocking multi-anvil press. In the absence of water, Ca–Mg carbonates are stable along geothermal gradients typical of subducting slabs. Ca–Mg carbonates (∼ Mg0.1–0.9Ca0.9–0.1CO3) partially melt beneath mid-ocean ridges and in plume settings. Ca–Mg carbonates melt incongruently, forming periclase crystals and carbonate melt between 4 and 9 GPa. Furthermore, we show that the rare earth element (REE) signature of Group-I kimberlites, namely strong REE fractionation and depletion of heavy REE relative to the primitive mantle, is resembled by carbonate melt in equilibrium with Ca-bearing magnesite and periclase at 6 and 9 GPa. This suggests that the dolomite–magnesite join of the CaCO3–MgCO3 system might be useful to approximate the REE signature of carbonate-rich melts parental to kimberlites. KW - High pressure experiments KW - Laser Ablation PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-561197 DO - https://doi.org/10.5194/ejm-34-411-2022 SN - 0935-1221 VL - 34 IS - 5 SP - 411 EP - 424 PB - Copernicus Publications CY - Göttingen AN - OPUS4-56119 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cant, D. J. H. A1 - Müller, Anja A1 - Clifford, C. A. A1 - Unger, Wolfgang A1 - Shard, A. G. T1 - Summary of ISO/TC 201 Technical Report 23173—Surface chemical analysis—Electron spectroscopies—Measurement of the thickness and composition of nanoparticle coatings N2 - ISO Technical Report 23173 describes methods by which electron spectroscopies, including X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES) and synchrotron techniques, can be employed to calculate the Coating thicknesses and compositions of nanoparticles. The document has been developed to review and outline the current state-of-the-art for such measurements. Such analyses of core–shell nanoparticles are common within the literature, however the methods employed are varied; the relative advantages and disadvantages of These methods, and the optimal usage of each may not be clear to the general analyst. ISO Technical Report 23173 aims to clarify the methods that are available, describe them in clear terms, exhibit examples of their use, and highlight potential issues users may face. The information provided should allow analysts of electron spectroscopy data to make clear choices regarding the appropriate analysis of electron spectroscopy data from coated nanoparticle systems and provide a basis for understanding and comparing results from different methods and systems. KW - Electron spectroscopy KW - Core-shell KW - Nanoparticles KW - ISO 23173 KW - XPS KW - Thickness KW - Composition PY - 2021 DO - https://doi.org/10.1002/sia.6987 SN - 0142-2421 VL - 53 IS - 10 SP - 893 EP - 899 PB - John Wiley & Sons Ltd AN - OPUS4-52976 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kupsch, Andreas A1 - Laquai, René A1 - Müller, Bernd R. A1 - Paciornik, S. A1 - Horvath, J. A1 - Tushtev, K. A1 - Rezwan, K. A1 - Bruno, Giovanni T1 - Evolution of Damage in All-Oxide Ceramic Matrix Composite After Cyclic Loading N2 - While structural ceramics usually display a brittle mechanical behavior, their composites may show nonlinearities, mostly due to microcracking. Herein, the stiffness evolution of a sandwich-like laminate of an Al2O3 15%vol. ZrO2 matrix reinforced with Nextel 610 fibers is studied as a function of number of cycles N in tension. The stiffness of the composite degrades with increasing N, indicating microcracking. However, synchrotron X-ray refraction radiography shows that the internal specific surface of such cracks varies differently. A modeling strategy is developed for the calculation of the equivalent stiffness of mixtures (first the matrix and then the sandwich), based on the Voigt and Reuß schemes. The Bruno–Kachanov model is then used to estimate the initial microcrack density in the matrix (due to the thermal expansion mismatch) and the amount of microcracking increase upon cyclic loading. The stiffness in the composite degrades dramatically already after 20 000 cycles but then remains nearly constant. The combination of mechanical testing, quantitative imaging analysis, and modeling provides insights into the damage mechanisms acting: microcrack propagation is more active than microcrack initiation upon cyclic loading, but the second also occurs. This scenario is similar but not equal to previous results on porous and microcracked ceramics. KW - Ceramic matrix composites KW - Homogenization schemes KW - Microcracking KW - Nonlinear behavior KW - Synchrotron X-ray refraction radiography PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-534541 DO - https://doi.org/10.1002/adem.202100763 SN - 1527-2648 SN - 1438-1656 VL - 24 IS - 6 SP - 2100763 -1 EP - 2100763 -13 PB - VCH GmbH CY - Weinheim AN - OPUS4-53454 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wipfler, B. A1 - Bradler, S. A1 - Büsse, S. A1 - Hammel, J. A1 - Müller, Bernd R. A1 - Pass, G. T1 - Evolutionary morphology of the antennal heart in stick and leaf insects (Phasmatodea) and webspinners (Embioptera) (Insecta: Eukinolabia) N2 - The morphology of the antennal hearts in the head of Phasmatodea and Embioptera was investigated with particular reference to phylogenetically relevant key taxa. The antennal circulatory organs of all examined species have the same basic construction: they consist of antennal vessels that are connected to ampullae located in the head near the antenna base. The ampullae are pulsatile due to associated muscles, but the points of attachment differ between the species studied. All examined Phasmatodea species have a Musculus (M.) interampullaris which extends between the two ampullae plus a M. ampulloaorticus that runs from the ampullae to the anterior end of the aorta; upon contraction, all these muscles dilate the lumina of both ampullae at the same time. In Embioptera, only the australembiid Metoligotoma has an M. interampullaris. All other studied webspinners instead have a M. ampullofrontalis which extends between the ampullae and the frontal region of the head capsule; these species do not have M. ampulloaorticus. Outgroup comparison indicates that an antennal heart with a M. interampullaris is the plesiomorphic character state among Embioptera and the likely ground pattern of the taxon Eukinolabia. Antennal hearts with a M. ampullofrontalis represent a derived condition that occurs among insects only in some embiopterans. These findings help to further clarify the controversially discussed internal phylogeny of webspinners by supporting the view that Australembiidae are the sister group of the remaining Embioptera. KW - Phylogeny KW - Polyneoptera KW - Metoligotoma PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-527795 DO - https://doi.org/10.1007/s00435-021-00526-4 SN - 1432-234X VL - 140 IS - 3 SP - 331 EP - 340 PB - Springer AN - OPUS4-52779 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Rouxel, T. A1 - Behrens, H. A1 - Deubener, J. A1 - Müller, Ralf T1 - Vacuum crack growth in alkali silicate glasses N2 - Crack growth velocity in alkali silicate glasses was measured in vacuum across 10 orders of magnitude with double cantilever beam technique. Measured and literature crack growth data were compared with calculated intrinsic fracture toughness data obtained from Young´s moduli and the theoretical fracture surface energy estimated from chemical bond energies. Data analysis reveals significant deviations from this intrinsic brittle fracture behavior. These deviations do not follow simple compositional trends. Two opposing processes may explain this finding: a decrease in the apparent fracture surface energy due to stress-induced chemical changes at the crack tip and its increase due to energy dissipation during fracture. KW - Silicate glass KW - Brittle fracture KW - Crack growth KW - Calculated intrinsic fracture toughness PY - 2021 DO - https://doi.org/10.1016/j.jnoncrysol.2021.121094 SN - 0022-3093 VL - 572 SP - 1 EP - 8 PB - Elsevier CY - Amsterdam AN - OPUS4-53144 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tschöke, K. A1 - Müller, I. A1 - Memmolo, V. A1 - Moix-Bonet, M. A1 - Moll, J. A1 - Lugovtsova, Yevgeniya A1 - Golub, M. A1 - Sridaran Venkat, R. A1 - Schubert, L. T1 - Feasibility of Model-Assisted Probability of Detection Principles for Structural Health Monitoring Systems based on Guided Waves for Fibre-Reinforced Composites N2 - In many industrial sectors, Structural Health Monitoring (SHM) is considered as an addition to Non-Destructive Testing (NDT) that can reduce maintenance effort during lifetime of a technical facility, structural component or vehicle. A large number of SHM methods is based on ultrasonic waves, whose properties change depending on structural health. However, the wide application of SHM systems is limited due to the lack of suitable methods to assess their reliability. The evaluation of the system performance usually refers to the determination of the Probability of Detection (POD) of a test procedure. Up to now, only few limited methods exist to evaluate the POD of SHM systems, which prevent them from being standardised and widely accepted in industry. The biggest hurdle concerning the POD calculation is the large amount of samples needed. A POD analysis requires data from numerous identical structures with integrated SHM systems. Each structure is then damaged at different locations and with various degrees of severity. All of this is connected to high costs. Therefore, one possible way to tackle this problem is to perform computer-aided investigations. In this work, the POD assessment procedure established in NDT according to the Berens model is adapted to guided wave-based SHM systems. The approach implemented here is based on solely computer-aided investigations. After efficient modelling of wave propagation phenomena across an automotive component made of a carbon fibre-reinforced composite, the POD curves are extracted. Finally, the novel concept of a POD map is introduced to look into the effect of damage position on system reliability. KW - Reliability KW - Acoustics KW - Monitoring KW - Automotive engineering KW - Elastodynamic Finite Inegration Technique PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-528218 DO - https://doi.org/10.1109/TUFFC.2021.3084898 VL - 68 IS - 10 SP - 3156 EP - 3173 AN - OPUS4-52821 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heuser, Lina A1 - Nofz, Marianne A1 - Müller, Ralf A1 - Deubener, J. T1 - Silver dissolution and precipitation in an Na2O–ZnO–B2O3 metallization paste glass N2 - Thermally stimulated interactions between silver and glass, that is, silver dissolution as Ag+ and precipitation as Ag0 were studied in two glass series of molar target composition xAg2O–(19 − x)Na2O–28ZnO–53B2O3 with x = 0, 0.1, 0.5, 5 and (19Na2O–28ZnO–53B2O3)+yAg2O with y = 0.01, 0.05. These act as model for low-melting borate glasses being part of metallization pastes. The occurrence of metallic silver precipitates in melt-quenched glass ingots demonstrated that silver dissolved only in traces (< 0.01 mol%) in the glasses. The dissolved silver was detected by means of Raman spectroscopy and energy-dispersive X-ray spectroscopy. Increasing x in the batch could not lead to a significant increase of the silver ion fraction in the glass as possible in binary silver borate glasses. In situ observation of heated AgNO3 mixed with the base glass frit in a hot stage microscope showed that Ag0 precipitation occurs already at the solid state. At higher temperatures, small droplets of liquid silver were found to move freely within the melt, whereas coalescence caused a stepwise increase of their size. These results contribute to the understanding of formation of silver precipitates in metallization pastes described in the literature. KW - Silver metallization paste KW - Batch reactions KW - Borate KW - Glass forming melts KW - Glass manufacturing KW - Raman spectroscopy PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559433 DO - https://doi.org/10.1111/ijag.16613 SN - 2041-1286 SP - 1 EP - 11 PB - Wiley Online Library AN - OPUS4-55943 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brüngel, R. A1 - Rückert, J. A1 - Müller, P. A1 - Babick, F. A1 - Friedrich, C. M. A1 - Ghanem, A. A1 - Hodoroaba, Vasile-Dan A1 - Mech, A. A1 - Weigel, S. A1 - Wohlleben, W. A1 - Rauscher, H. T1 - NanoDefiner Framework and e-Tool Revisited According to the European Commission’s Nanomaterial Definition 2022/C 229/01 N2 - The new recommended definition of a nanomaterial, 2022/C 229/01, adopted by the European Commission in 2022, will have a considerable impact on European Union legislation addressing chemicals, and therefore tools to implement this new definition are urgently needed. The updated NanoDefiner framework and its e-tool implementation presented here are such instruments, which help stakeholders to find out in a straightforward way whether a material is a nanomaterial or not. They are two major outcomes of the NanoDefine project, which is explicitly referred to in the new definition. This work revisits the framework and e-tool, and elaborates necessary adjustments to make these outcomes applicable for the updated recommendation. A broad set of case studies on representative materials confirms the validity of these adjustments. To further foster the sustainability and applicability of the framework and e-tool, measures for the FAIRification of expert knowledge within the e-tool’s knowledge base are elaborated as well. The updated framework and e-tool are now ready to be used in line with the updated recommendation. The presented approach may serve as an example for reviewing existing guidance and tools developed for the previous definition 2011/696/EU, particularly those adopting NanoDefine project outcomes. KW - Nanomaterial definition KW - Nanomaterial categorisation KW - Nanomaterial regulation KW - Nanomaterial legislation KW - Decision support KW - FAIRification PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-571618 DO - https://doi.org/10.3390/nano13060990 SN - 2079-4991 VL - 13 IS - 6 - Special Issue "Identification and Quantification of Nanomaterials" SP - 1 EP - 16 PB - MDPI CY - Basel, CH AN - OPUS4-57161 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Zoёga, Andreas A1 - Kurz, J. H. A1 - Oelschlägel, T. A1 - Rohrschneider, A. A1 - Müller, Christina A1 - Pavlovic, Mato A1 - Hintze, H. A1 - Kanzler, D. T1 - Investigations to introduce the probability of detection method for ultrasonic inspection of hollow axles at Deutsche Bahn N2 - Currently at Deutsche Bahn (DB) ultrasonic inspections in maintenance procedures for wheelset axles with a bore hole are, to the greatest possible extent, carried out using automated ultrasonic inspection system. Although the acceptance levels are in accordance with DIN 27201 part 7, the testing results have shown in recent years that in the case of true indications, the effective defect sizes were far below the level of acceptance. Due to this experience it can be assumed that the automated ultrasonic inspection systems are testing substantially more sensitively than required. This increased sensitivity leads to an increase in false indications, generally resulting in the unnecessary demounting of wheelsets. In Research cooperation between Federal Institute for Materials Research and Testing (BAM) and DB the effective flaw detection sensitivity of existing automated ultrasonic inspection system will be determined and the true/false indication ratio optimised. Through systematic investigations with the Probability of Detection method on the existing automated ultrasonic inspection system the results could be directly applied to the optimisation of existing ultrasonic inspections of wheelset axles with a bore hole in maintenance procedures and the level of reliability can be considerably increased. T2 - 19th World Conference on Non-Destructive Testing CY - München, Germany DA - 13.06.2016 KW - NDT KW - Reliability KW - POD KW - Railway KW - Axles KW - UT PY - 2016 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-375813 UR - http://www.ndt.net/article/wcndt2016/papers/we2g4.pdf SP - id 19515, 1 EP - 8 AN - OPUS4-37581 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ried, Peter A1 - Gaber, Martin A1 - Müller, Ralf A1 - Deubener, J. T1 - Hydrogen permeability of a barium-aluminoborosilicate glass - A methodical approach N2 - The H2 effusion from H2 saturated glass powders, H2 permeation through the wall of blown glass bulbs, and H2 permeation through the wall of glass capillaries were applied to evaluate the permeability of hydrogen gas in a barium-aluminoborosilicate (BABS) glass. To validate these methods, two commercial glasses (vitreous silica and borosilicate) were used as a reference. Permeation values obtained from the different experiments agreed within a factor of 3 or less. The H2 permeability of BABS glass at temperatures close to ambient was found to be at least 3 orders of magnitude below that of borosilicate and silica glasses. The powder method, which requires minimal sample preparation efforts, turned out to provide easy access to the measurement of H2 permeability of glasses down to P = 3.9 × 10- 21 mol s- 1 Pa- 1 m- 1. KW - Hydrogen gas KW - Permeability KW - Solubility KW - Diffusivity KW - Aluminoborosilicate glass PY - 2014 DO - https://doi.org/10.1016/j.jnoncrysol.2014.04.006 SN - 0022-3093 VL - 394-395 SP - 43 EP - 49 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-30720 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kanzler, Daniel A1 - Müller, Christina A1 - Pitkänen, J. T1 - Evaluation of radiographic testing performance with an advanced POD approach N2 - POD is the most often used approach for the evaluation of the reliability of non-destructive testing methods in critical areas. But especially for those cases the requirements for a sufficient amount of data, adequate type of defects and the statistical requirements are high. The claim for checking these requirements is not new, but never the less often ignored. Especially the large amount of data for critical real defects seems too often to be not really solvable. In this presentation we show an approach to use real defect data with knowledge from former testing results with the same equipment, in a useful adequate way. Furthermore we introduce a method to evaluate the real defect description parameters for the radiographic testing. This approach was used for a joint project with the company POSIVA, which is building a final depository for spent nuclear fuel in Finland. Radiographic testing is one of the NDT-methods they use to test the electron beam weld of the copper canister. The copper canister will be used in the deposit as a corrosion barrier within the deposit concept. Through the high sophisticated manufacturing methods of the canister there are almost no material defects, which could be used for reliability evaluation. In this context the idea of Bayesian Updating of the POD with real defect data with former results from artificial defect data was born to get a useful evaluation. T2 - 5th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 07.10.2013 PY - 2013 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-312641 SN - 978-3-940283-53-5 IS - DGZfP-BB 144 SP - Lecture 4, 1 EP - 7 PB - Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP) CY - Berlin AN - OPUS4-31264 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Christina A1 - Bertovic, Marija A1 - Holstein, R. A1 - Kanzler, Daniel A1 - Pitkänen, J. A1 - Ronneteg, U. A1 - Heckel, Thomas T1 - A plenary view on the vigour of our NDE reliability models N2 - Using the Modular Reliability Model the three different main influencing elements, i.e. intrinsic capability (IC), application parameters (AP) and the human factors (HF), are, in the first instance, investigated separately. The intrinsic capability stands for the pure physical-technological process of the signal detection caused by the waves or the rays from a material defect in the presence of noise (driven by the material and the devices). This intrinsic capability is the upper bound of the possible reliability. Already when measuring this intrinsic capability for thick walled components the original one-parameter POD must be extended to a multiparameter POD, where, in addition to the defect size, a number of additional physical parameters, such as the grain size distribution (or attenuation), defect depth, and angle or surface roughness, must be considered. For real life cycle assessments it is necessary to evaluate the signal response from real defects. The industrial application factors, e.g. coupling conditions, limited accessibility, heat and environmental vibrations, diminish the reliability. The amount of reduction can be determined quantitatively, if the underlying conditions are controlled. In case they are not controlled it is necessary to count for a fluctuation in the reliability in the field anyway. The third group of important influencing factors are the human factors, which do not only cover the individual performance capability of the inspectors but also the design of the working place,the procedure, the teamwork quality, interaction with systems, the organization, and finally, the relationship between the companies involved in the inspection process and to which extend the responsible parties are aware of it. When comparing an “ideal inspection” with a “real inspection” it is worth while to look how the existing practices, rules and standards support reliable testing and where the “delta” is. In the context of vigor, with respect to the industrial end user, it needs to be shown how the level of reliability of NDE, influenced by the different factors, has an impact on acceptance or rejection of safety critical parts. T2 - 5th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 07.10.2013 PY - 2013 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-312658 SN - 978-3-940283-53-5 IS - DGZfP-BB 144 SP - Lecture 2, 1 EP - 18 PB - Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP) CY - Berlin AN - OPUS4-31265 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pitkänen, J. A1 - Bertovic, Marija A1 - Brackrock, Daniel A1 - Brekow, Gerhard A1 - Ewert, Uwe A1 - Kanzler, Daniel A1 - Müller, Christina T1 - Reliable evaluation of the acceptability of the weld for final disposal based on the canister copper weld inspection using different NDT methods T2 - 5th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2013-10-07 PY - 2013 SN - 978-3-940283-53-5 IS - DGZfP-BB 144 SP - Lecture 37, 1 EP - 13 CY - Berlin AN - OPUS4-31267 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bertovic, Marija A1 - Calmon, P. A1 - Carter, L. A1 - Fischer, J. A1 - Forsyth, D. A1 - Holstein, R. A1 - McGrath, B. A1 - Müller, Christina A1 - Pavlovic, Mato A1 - Ronneteg, U. A1 - Rummel, W. A1 - Schubert, F. A1 - Selby, G. T1 - Summary of the "open space technology discussions" on reliability of NDE N2 - Since the beginnings of the European American Workshops (EAW) in 1997, the aim was to gather the experts in NDE reliability and discuss burning topics with the aim of identifying crucial problems and suggesting ways to move forward. This was usually achieved during the so-called break-out sessions, in which predetermined topics were discussed. During the 5th EAW, held in Berlin in 2013, this approach was replaced by an Open Space Technology (OST) approach. The benefit of this approach is seen in the freedom of topic choices, i. e., the topics are not predetermined but rather arise at that moment in that space and by the participants’ choice. The following topics arose: new reliability methods (Bayesian, MAPOD, …), structural health monitoring, definition of requirements of NDE by customer versus provider, what value of POD is good enough?, human factors, manual versus automated inspection, and basic concepts of reliability of NDE. The participants were encouraged to walk from one session to another and openly express their opinions. These were in the end summarized by a chosen group of moderators and presented in this paper. N2 - Seit den Anfängen der europäischen amerikanischen Workshops (EAW) im Jahr 1997 war es das Ziel, Experten auf dem Gebiet der ZfP-Zuverlässigkeit zusammenzuführen und aktuelle Themen zu diskutieren, um wichtige Probleme zu identifizieren und Wege für deren Lösung vorzuschlagen. Dies wurde in der Regel während der sogenannten „Break-out Sessions“ erreicht, in denen vorgegebene Themen diskutiert wurden. Während des 5. EAW, der in Berlin im Jahr 2013 stattfand, wurde dieser Ansatz durch einen Open Space Technology (OST) Ansatz ersetzt. Open Space ist eine Methode der Gruppenmoderation, die sehr gut geeignet ist, um neue Ideen zu entwickeln und selbstständiges Arbeiten zu fördern, d. h. die Themen werden nicht vorgegeben, sondern ergeben sich in diesem Moment in diesem Raum und durch die Wahl der Teilnehmer. Die folgenden Themen wurden herausgearbeitet: neue Zuverlässigkeitsmethoden (Bayes, MAPOD, ...…), Structural Health Monitoring, Definition von Anforderungen der Kunden gegenüber den ZfP-Anbietern, Welcher Wert der POD ist gut genug?, der Einfluss menschlicher Faktoren, manuelle gegenüber automatisierte Prüfung, sowie Grundkonzepte der ZfP-Zuverlässigkeit. Die Teilnehmer wurden aufgefordert, von einer Sitzung zur anderen zu wechseln und offen ihre Meinung zu äußern. Diese Meinungen wurden am Ende von einer ausgewählten Gruppe von Moderatoren zusammengefasst und werden in diesem Beitrag vorgestellt. KW - NDE reliability KW - POD KW - Bayesian approach KW - Structural health monitoring KW - Human factors KW - Open space technology PY - 2014 UR - http://www.hanser-elibrary.com/doi/pdf/10.3139/120.110604 DO - https://doi.org/10.3139/120.110604 SN - 0025-5300 VL - 56 IS - 7-8 SP - 602 EP - 606 PB - Hanser CY - München AN - OPUS4-31269 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bertovic, Marija A1 - Müller, Christina A1 - Fahlbruch, B. A1 - Ronneteg, U. A1 - Pitkänen, J. T1 - Holistic risk assessment and risk prevention approach to the mechanized NDT and the inspection procedure T2 - 5th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2013-10-07 PY - 2013 SN - 978-3-940283-53-5 IS - DGZfP-BB 144 SP - Lecture 20, 1 EP - 10 CY - Berlin AN - OPUS4-31270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bertovic, Marija A1 - Calmon, P. A1 - Carter, L. A1 - Fisher, J. A1 - Forsyth, D. A1 - Holstein, R. A1 - McGrath, B. A1 - Müller, Christina A1 - Pavlovic, Mato A1 - Ronneteg, U. A1 - Rummel, W. A1 - Schubert, F. A1 - Selby, G. T1 - Summary of the open space technology discussions T2 - 5th European-American workshop on reliability of NDE CY - Berlin, Germany DA - 2013-10-07 PY - 2013 SN - 978-3-940283-53-5 IS - DGZfP-BB 144 SP - 1 EP - 7(?) CY - Berlin AN - OPUS4-31271 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pitkänen, J. A1 - Bertovic, Marija A1 - Brackrock, Daniel A1 - Brekow, Gerhard A1 - Ewert, Uwe A1 - Kanzler, Daniel A1 - Müller, Christina T1 - Reliable evaluation of acceptability of weld for final disposal based on the canister copper weld inspection using different NDT methods N2 - The inspection of the sealing weld is an important phase for the evaluation of the acceptability of final disposal canister, but the weld is only a part of the 3D shielding of copper shell. The main tasks for reliable NDT evaluation requires an extensive evaluation of the parameters – which contains typical inspection related items like repeatability, S/N ratio, POD, setting up the equipment for inspection, and all practices for inspections. The other parameters are material parameters, their variation must be taken into account in the evaluation of NDT reliability. Further parameters include human factors, i. e. human inspectors and their interaction with technical systems; their effects were studied on an example of the evaluation of eddy current data. Final parameters are related to evaluation of detected defects, which means sizing and base for acceptance and this can be done in different ways. Some examples are given and results are compared with different methods for instance between radiographic testing and ultrasonic testing by raw data analysis and PA-SAFT results. Also, preliminary curves for the evaluation of metallographic results of 55 defects will be shown by EB weld measurements. Some practical items concerning copper inspections will be also discussed related to acceptability. N2 - Die Prüfung der Verschlussschweißnaht ist eine wichtige Phase in der Akzeptanzbewertung der Endlagerungskanister, obwohl die Verschlussschweißnaht nur ein Teil der dreidimensionalen Bedeckung der Kupfereinhüllung ist. Die Hauptaufgabe für die sichere zerstörungsfreie Prüfung (ZfP) erfordert eine umfangreiche Bewertung der Prüfparameter, die die typischen Prüfeinzelheiten, wie z. B. Wiederholbarkeit, Signal-Rausch-Verhältnis, POD, Einstellung der Geräte und alle Prüfvorgehen enthalten. Weitere Parameter sind die Schwankungen von Materialeigenschaften, die berücksichtigt werden müssen. Andere Parameter sind menschliche Faktoren, wie z. B. die Prüfer, und deren Interaktion mit den technischen Systemen, beispielsweise bei der Bewertung der Wirbelstromdaten. Weitere Einflussgrößen auf die Prüfung entstehen bei der Bewertung gefundener Fehler, bei der Größenbestimmung von Fehlern und basierend auf der strukturellen Integrität bei der Akzeptanz von definierten Fehlergrößen/Fehlerarten an verschiedenen Positionen in der Schweißnaht. Der Artikel zeigt einige Beispiele und den Vergleich zwischen verschiedenen ZfP-Methoden, z. B. der radiographische Prüfung, der Ultraschallprüfung mit Bewertung von Rohdaten und der Ultraschallprüfung mit Bewertung mittels PA-SAFT. Auch die vorläufigen Kurven für die metallographische Bewertung von 55 Fehlern der Elektronenstrahlschweißung sind gezeigt. Darüber hinaus wird auch eine praktische Vorgehensweise bei der Definition der Akzeptanzkriterien für die Kupferschweißnahtsprüfung diskutiert. KW - NDT reliability KW - Radiography KW - Ultrasonic testing KW - Eddy current testing KW - Visual testing PY - 2014 UR - http://www.hanser-elibrary.com/doi/pdf/10.3139/120.110609 DO - https://doi.org/10.3139/120.110609 SN - 0025-5300 VL - 56 IS - 9 SP - 748 EP - 757 PB - Hanser CY - München AN - OPUS4-31524 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Eberstein, Markus A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Deubener, J. A1 - Schiller, Wolfgang Arno T1 - Sintering of glass matrix composites with small rigid inclusions KW - Glass ceramics KW - Inclusions KW - Sintering KW - Mixing KW - Powders KW - Solid-state reaction PY - 2009 DO - https://doi.org/10.1016/j.jeurceramsoc.2009.02.007 SN - 0955-2219 SN - 1873-619X VL - 29 IS - 12 SP - 2469 EP - 2479 PB - Elsevier CY - Oxford AN - OPUS4-19570 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Müller, Bernd R. A1 - Lange, Axel A1 - Harwardt, Marco A1 - Hentschel, Manfred P. A1 - Illerhaus, Bernhard A1 - Goebbels, Jürgen A1 - Bamberg, J. A1 - Heutling, F. ED - Danny Van Hemelrijck, ED - Igor Solodov, ED - Anastasopoulos, Athanasios ED - Gerhard Busse, T1 - Synchrotron-Refraction-Computed-Tomography for NDT and characterisation of lightweight composite materials T2 - 4th International Conference of Emerging Technologies in Non-Destructive Testing (ETNDT 4) CY - Stuttgart, Germany DA - 2007-04-02 KW - Refraction KW - Computed Tomography KW - NDE KW - Ti-MMC PY - 2008 SN - 978-0-415-46476-5 SP - 217 EP - 221 PB - Taylor & Francis CY - London, UK AN - OPUS4-18680 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pavlovic, Mato A1 - Boehm, Rainer A1 - Müller, Christina A1 - Pitkänen, J. A1 - Ronneteg, U. T1 - Investigation of the influence of the material attenuation on the POD of the flaws T2 - 8th International conference on NDE in relation to structural integrity for nuclear and pressurised components CY - Berlin, Germany DA - 2010-09-29 KW - POD KW - NDT KW - Attenuation KW - Ultrasonic KW - Reliability PY - 2010 SN - 978-3-940283-30-6 IS - DGZfP-BB 125 (Th.2.B.2) SP - 1 EP - 9 CY - Berlin AN - OPUS4-23922 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Christina A1 - Bertovic, Marija A1 - Pavlovic, Mato A1 - Kanzler, Daniel A1 - Rosenthal, Martina A1 - Pitkänen, J. A1 - Ronneteg, U. T1 - Progress in evaluating the reliability of NDE systems - paradigm shift N2 - The paper will give an overview of new methodology for evaluating the reliability of NDE systems accurately, reliably and efficiently in accordance with the specific requirements of industrial application. After a review of the substantive issues from the previous workshops, the go forward guidance from these interactions is considered. At the beginning of the reliability analysis, the actual safety demands have to be defined in order to fit the investigation to the level of risk when the component would fail. Next, all the essential influencing parameters need to be documented and transferred to an appropriate design of experiments (DOE) to determine the reliability in terms of a qualitative assessment for lower risk or in terms of a quantitative probability of detection (POD) or ROC (Receiver Operating Characteristics) curves for higher safety demands. A new paradigm is offered to consider the POD or reliability of the system as a function of the configuration of input variables and use it for optimisation rather than for a final judgement. An advantage for the end user is also to sample all single PODs to an integral 'Volume POD' of a part. Among the influencing parameters, the human factor is the most important one. A systematic psychological approach shall help to find out where the bottlenecks are but most importantly to provide best possible working conditions for the human inspectors. T2 - 8th International conference on NDE in relation to structural integrity for nuclear and pressurised components CY - Berlin, Germany DA - 2010-09-29 KW - Reliability KW - POD KW - ROC KW - Safety PY - 2010 SN - 978-3-940283-30-6 IS - DGZfP-BB 125 (Th.3.A.4) SP - 1 EP - 10 CY - Berlin AN - OPUS4-23923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kanzler, Daniel A1 - Milsch, Steffen A1 - Pavlovic, Mato A1 - Müller, Christina A1 - Pitkänen, J. T1 - Concept of total reliability of NDT methods for inspection of the EB weld of the copper canister used for a long-term storage of spent nuclear fuel T2 - 8th International conference on NDE in relation to structural integrity for nuclear and pressurised components CY - Berlin, Germany DA - 2010-09-29 KW - POD KW - Ultrasonic testing KW - Radiographic testing KW - Eddy current testing PY - 2010 SN - 978-3-940283-30-6 IS - DGZfP-BB 125 (Th.3.A.5) SP - 1 EP - 6 CY - Berlin AN - OPUS4-23924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bertovic, Marija A1 - Müller, Christina A1 - Fahlbruch, B. A1 - Pitkänen, J. A1 - Ronneteg, U. T1 - Human factors approach to the reliability of NDT in nuclear waste management in Sweden and Finland N2 - Nuclear power industry has the responsibility to manage and dispose of all radioactive waste from its plants. Finnish Posiva and Swedish SKB are leading in the world in the development of disposal of spent nuclear fuel. Their method consists of encapsulating spent nuclear fuel in copper canisters and depositing them in the bedrock at a depth of about 500 meters for the next 100 000 years, leaving the radioactivity to decrease naturally through the decay of the radioisotopes in it. The copper canisters, consisting of a copper tube, a lid and a bottom (which make the outer shell) and an insert made of a cast iron, need to be inspected for their structural integrity to ensure no critical defects are present in the materials and welds that could lead to a leakage of the waste into the environment. Data acquired by 4 different non-destructive testing (NDT) methods (i.e. UT, ET, RT and VT with a remote camera) are evaluated by skilled human operators and therefore could be subject to human error. Human Factors approach lies in identifying potential errors made by the human, their causes and ways of preventing them. A customized Failure Modes and Effects Analysis (FMEA) was conducted to anticipate possible human failures during the data evaluation. The results led to designing several experiments (e.g. diffusion of responsibility within the 4-eye principle, over trust in automated systems) which are being experimentally tested in ongoing projects. The results are expected to lead to the optimization of the procedures followed by the NDT operators and consequently to the improvement of the overall NDT reliability. T2 - 8th International conference on NDE in relation to structural integrity for nuclear and pressurised components CY - Berlin, Germany DA - 2010-09-29 KW - Human factors KW - Reliability KW - NDT KW - Nuclear waste PY - 2010 UR - http://www.ndt.net/article/jrc-nde2010/papers/32.pdf SN - 978-3-940283-30-6 IS - DGZfP-BB 125 (Th.3.A.2) SP - 1 EP - 10 CY - Berlin AN - OPUS4-23925 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Behrens, H. A1 - Deubener, J. T1 - Impact of structure and relaxation on fatigue and micromechanical properties of oxide glasses: the role of volatiles and bonding state N2 - As subcritical crack growth (SCCG) can reduce tensile strength of glasses by many orders of magnitude, the potential for improvement of fatigue behaviour is most intriguing in developing ultra-strong glasses. An essential bottleneck is the basic understanding of the numerous interplaying pressure-, temperature- and water-affected relaxation phenomena at the crack tip and related toughening strategies. Therefore, the present project aims to advance the basic understanding of structural relaxation effects and local properties caused by increased water concentration and tensile stresses at the crack tip as they are a key for structural toughening designs to develop SCCG-free glasses and glass surfaces. Our first studies give clear evidence that glass structure and dynamics is strongly modified upon hydration of glasses. These changes are highly related to the nature of network formers but are affected as well by the counter ions (network modifier). Results of the 1st project part suggest that structural relaxation below glass transition temperature, i.e. overlapping of short-range (beta) and long-range (alpha) interactions can contribute to SCCG in water-free environments and that structurally dissolved water in the glasses can have decisive impact on this effect. In the 2nd project stage specific glasses compositions will be investigated to gain an improved understanding on the relation of sub-Tg relaxation and inert SCCG as well as to shed light to the related effects of dissolved water and its speciation. These glasses cover a broader range of different glass topologies and binding partners, whereby the coupling of alpha and beta relaxations is varied systematically by alkali-, alkaline earth ions and water species concentrations. Preparation of hydrous glasses (up to 8 wt% water) will be performed by high pressure syntheses. Structure will be resolved by NMR, Raman and IR spectroscopy while structural relaxation is accessed in the temperature and frequency domain using dynamic mechanical spectroscopy and ultrasonic damping. We will focus on measurements of inert SCCG (region III) conducting experiments in vacuum and dry gas atmospheres using indentation techniques and stressing of glass specimens in DCB geometry. Experimental data on SCCG will be provided to SPP groups, which deals with fatigue in metallic glasses and vice versa we will test theoretical predictions of ab-initio simulations of partner within SPP 1594 in order to quantify the effect of water on the crack tip. In summa topological factors controlling the subcritical crack growth with respect to water will be identified from which structural toughening designs for highly fatigue resistant-glasses can be derived. N2 - Subkritisches Risswachstum (SCCG) kann die Zugfestigkeit von Glas um viele Größenordnungen erniedrigen. Deshalb birgt die Verbesserung des Ermüdungsverhaltens ein hohes Potential für das topologische Design hochfester Gläser. Ein diesbezüglicher Engpass ist das Verständnis der zahlreichen interagierenden druck-, temperatur- und wasserbeeinflussten Relaxationsphänomene an der Rissspitze und hieraus abgeleitete Verstärkungsstrategien. Ziel des Projekts ist es daher, das grundlegende Verständnis der Effekte, die infolge erhöhter Wasserkonzentrationen und Zugspannungen an der Rissspitze entstehen, zu vertiefen, da sie als ein Schlüssel für künftige strukturelle Designprinzipien zur Entwicklung schadenstoleranter Gläser und Glasoberflächen gelten. Unsere ersten Studien zeigen, dass die Struktur und Dynamik von Gläsern nach einer Hydration stark verändert sind. Diese Modifikationen sind mit der Art der Netzwerkbildner stark verknüpft, aber auch von ihren Gegenionen (Netzwerkwandler) abhängig. Die Ergebnisse des ersten Projektabschnitts legen nahe, dass strukturelle Relaxation unterhalb der Glasübergangstemperatur, d. h. ein Überlappen von kurz-reichweitigen (beta) und lang-reichweitigen (alpha) Wechselwirkungen, zum subkritisches Risswachstum in wasserfreien Umgebungen beitragen kann und, dass strukturell gelöstes Wasser in Gläsern sich entscheidend auf diese Effekt auswirken kann. Im zweiten Projektabschnitt werden daher spezielle Glaszusammensetzungen untersucht, die zu einem besseren Verständnis der Verbindung zwischen sub-Tg Relaxation und SCCG führen aber auch den Einfluss von gelöstem Wasser und dessen Speziation näher beleuchten. Diese Gläser weisen eine großen Breite an verschiedenen Topologien und Bindungspartnern auf, wobei die Kopplung von alpha und beta Relaxation durch Veränderungen in den Gehalten von Alkali-, Erdalkalionen und der Wasserspezies systematisch variiert wird. Die Präparation hydratisierter Gläser (bis zu 8 Ma.%) erfolgt mittels Hochdrucksynthesen. Die Glasstruktur wird durch NMR, Raman und IR Spektroskopie aufgeklärt während die Strukturrelaxation anhand dynamische mechanische Spektroskopie und Ultraschalldämpfung im Temperatur- und Frequenzraum erfasst wird. Im Fokus werden Messungen des inerten subkritischen Risswachstums (Region III) stehen, die Indenter-Experimente im Vakuum und trockenen Gasatmosphären sowie Verspannen von Glasproben in DCB Geometrie beinhalten. Experimentelle SCCG Daten werden Gruppen im Schwerpunktprogramm zur Verfügung stellen, die sich mit Ermüdung in metallischen Gläsern beschäftigen und im Gegenzug werden wir theoretische Vorhersagen aus ab initio Simulationen der Partner im SPP 1594 testen, um den Einfluss von Wasser auf die mechanischen Eigenschaften an der Rissspitze und deren Einfluss auf SCCG zu quantifizieren. In summa werden topologische Faktoren bezüglich Wasser, die SCCG kontrollieren, identifiziert, um daraus Designprinzipien für hoch ermüdungsresistente Gläser abzuleiten. T2 - Kolloquium des DFG-PP 1594 CY - Jena, Germany DA - 17.9.2015 KW - Glass KW - Fatigue PY - 2015 AN - OPUS4-38334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Ralf A1 - Behrens, H. A1 - Deubener, J. A1 - Reinsch, Stefan A1 - Bauer, Ute A1 - Rößler, C. T1 - Impact of structure and relaxation on fatigue and micro-mechanical properties of oxide glasses: the role of volatiles and bonding state N2 - As subcritical crack growth (SCCG) can reduce tensile strength of glasses by many orders of magni-tude, the potential for improvement of fatigue behaviour is most intriguing in developing ultra-strong glasses. An essential bottleneck is the basic understanding of the numerous interplaying pressure-, temperature- and water-affected relaxation phenomena at the crack tip and related toughening strat-egies. Therefore, the present project aims to advance the basic understanding of structural relaxa-tion effects and local properties caused by increased water concentration and tensile stresses at the crack tip as they are a key for structural toughening designs to develop SCCG-free glasses and glass surfaces. Our first studies give clear evidence that glass structure and dynamics is strongly modified upon hy-dration of glasses. These changes are highly related to the nature of network formers but are affect-ed as well by the counter ions (network modifier). Results of the 1st project part suggest that struc-tural relaxation below glass transition temperature, i.e. overlapping of short-range (beta) and long-range (alpha) interactions can contribute to SCCG in water-free environments and that structurally dissolved water in the glasses can have decisive impact on this effect. In the 2nd project stage specific glasses compositions will be investigated to gain an improved un-derstanding on the relation of sub-Tg relaxation and inert SCCG as well as to shed light to the relat-ed effects of dissolved water and its speciation. These glasses cover a broader range of different glass topologies and binding partners, whereby the coupling of alpha and beta relaxations is varied systematically by alkali-, alkaline earth ions and water species concentrations. Preparation of hy-drous glasses (up to 8 wt% water) will be performed by high pressure syntheses. Structure will be resolved by NMR, Raman and IR spectroscopy while structural relaxation is accessed in the temper-ature and frequency domain using dynamic mechanical spectroscopy and ultrasonic damping. We will focus on measurements of inert SCCG (region III) conducting experiments in vacuum and dry gas atmospheres using indentation techniques and stressing of glass specimens in DCB geometry. Experimental data on SCCG will be provided to SPP groups, which deals with fatigue in metallic glasses and vice versa we will test theoretical predictions of ab-initio simulations of partner within SPP 1594 in order to quantify the effect of water on the crack tip. In summa topological factors con-trolling the subcritical crack growth with respect to water will be identified from which structural toughening designs for highly fatigue resistant-glasses can be derived. T2 - Kolloquium des DFG-PP 1593 Ultrastrong Glasses CY - Jena, Germany DA - 17.9.2015 KW - Glass KW - Fatigue PY - 2015 AN - OPUS4-38335 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Quercetti, Thomas A1 - Müller, Karsten A1 - Musolff, Andre A1 - Nakagami, M. A1 - Komatsuki, S. A1 - Tamaki, H. A1 - Kishimoto, J. A1 - Fujisawa, K. A1 - Nishio, T. ED - Quercetti, Thomas T1 - Experimental testing of RAM packages within Japanese German projects N2 - In context with Japanese disposal and transport container safety assessment the German Federal Institute for Materials Research and Testing (Bundesanstalt für Materialforschung und -prüfung) per-formed extensive drop test series with prototypes of RAM packages in recent years. The paper presents two cooperative projects focused on project management, testing performance and experimental results. In the first project, a full-scale prototype of a package for transport and storage of spent fuel elements with a total mass of 127,000 kg and its reduced-scale model which was similar to the prototype in both geometry and design were drop tested in 9 m and 1 m puncture tests at various drop orientations under regulatory conditions. In context with a corresponding research project the test data was used in combination with numerical methods to investigate the phenomenon of internal cask- content collisions during drop tests. Here, technological gaps between basket or radioactive content and cask body or primary lid can be a reason for significant high dynamic loadings of cask components and its internals due to additional impact interactions in the cask cavity caused by inner relative movement between content and cask. Further investigations were carried out in the field of similarity mechanics comparing experimental drop test data of the full-scale prototype and reduced-scale model in regard to the transferability of package impact response from reduced-scale models to full-scale packages. In the second project, drop tests with a waste container for intermediate depth disposal were per-formed being contracted by Kobe Steel, Ltd. and a consortium of Japanese electric power plant com-panies. The drop test program comprised three single 8-m drop tests in a specimen’s corner edge orientation. For drop tests according to legal regulations for interim storage or final disposal it is often necessary to use a target which represents the real ground of the storage facility. In such cases the container hits directly onto a well-defined concrete slab on top of the IAEA target. Here, the directly impact target for the drop tests were concrete slabs manufactured in Japan and connected by mortar to the impact pad of the unyielding IAEA target. KW - Drop testing KW - Package PY - 2016 SP - Paper 1043, 1 EP - 13 CY - Kobe, Japan AN - OPUS4-37557 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Kanzler, Daniel A1 - Müller, Christina A1 - Pitkänen, J. T1 - Probability of defect detection of Posiva's electron beam weld N2 - The report 'Probability of Defect Detection of Posiva's electron beam weld' describes POD curves of four NDT methods radiographic testing, ultrasonic testing, eddy current testing and visual testing. POD-curves are based on the artificial defects in reference blocks. The results are devoted to the demonstration of suitability of the methods for EB weld testing. Report describes methodology and procedure applied by BAM. Report creates a link from the assessment of the reliability and inspection performance to the risk assessment process of the canister final disposal project. Report ensures the confirmation of the basic quality of the NDT methods and their capability to describe the quality of the EB-weld. The probability of detection curves are determined based on the MIL-1823 standard and it's reliability guidelines. The MIL-1823 standard was developed for the determination of integrity of gas turbine engines for the US military. In the POD-process there are determined as a key parameter for the defect detectability the a90/95 magnitudes, i.e. the size measure a of the defect, for which the lower 95 % confidence band crosses the 90 % POD level. By this way can be confirmed that defects with a size of a90/95 will be detected with 90 % probability. In case the experiment will be repeated 5 % might fall outside this confidence limit. KW - Probability of detection curves KW - POD-curves KW - NDT-methods KW - EB-welding KW - Ultrasonic inspection KW - Radiographic inspection KW - Eddy current inspection KW - Visual inspection PY - 2013 UR - http://www.posiva.fi/en/databank/working_reports/probability_of_defect_detection_of_posiva_s_electron_beam_weld.1874.xhtml?xm_col_report_year=2013&xm_col_language=3&xm_col_type=5&cd_order=col_report_number&cd_offset=0#.VJAIY3uj_mc UR - http://www.posiva.fi/files/3527/WR_2013-70.pdf SP - 1 EP - 86 AN - OPUS4-32512 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nellesen, J. A1 - Laquai, René A1 - Müller, Bernd R. A1 - Kupsch, Andreas A1 - Hentschel, M. P. A1 - Anar, N. B. A1 - Soppa, E. A1 - Tillmann, W. A1 - Bruno, Giovanni T1 - In situ analysis of damage evolution in an Al/Al2O3 MMC under tensile load by synchrotron X-ray refraction imaging N2 - The in situ analysis of the damage evolution in a metal Matrix composite (MMC) using synchrotron X-ray refraction radiography (SXRR) is presented. The investigated material is an Al alloy (6061)/10 vol% Al2O3 MMC after T6 heat treatment. In an interrupted tensile test the gauge section of dog bone-shaped specimens is imaged in different states of tensile loading. On the basis of the SXRR images, the relative change of the specific surface (proportional to the amount of damage) in the course of tensile loading was analyzed. It could be shown that the damage can be detected by SXRR already at a stage of tensile loading, in which no Observation of damage is possible with radiographic absorption-based imaging methods. Moreover, the quantitative analysis of the SXRR images reveals that the amount of damage increases homogeneously by an average of 25% with respect to the Initial state. To corroborate the experimental findings, the damage distribution was imaged in 3D after the final tensile loading by synchrotron X-ray refraction computed tomography (SXRCT) and absorption-based synchrotron X-ray computed tomography (SXCT). It could be evidenced that defects and damages cause pronounced indications in the SXRCT images. KW - Composite materials KW - Defects KW - Micro analysis PY - 2018 DO - https://doi.org/10.1007/s10853-017-1957-x SN - 0022-2461 SN - 1573-4803 VL - 53 IS - 8 SP - 6021 EP - 6032 PB - Springer US AN - OPUS4-44241 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Behrens, H. A1 - Bauer, U. A1 - Reinsch, Stefan A1 - Kiefer, P. A1 - Müller, Ralf A1 - Deubener, J. T1 - Structural relaxation mechanisms in hydrous sodium borosilicate glasses N2 - Borosilicate glasses (16Na2O–10B2O3–74SiO2, NBS) with water contents up to 22 mol% H2O were prepared to study the effect of water on structural relaxation using DTA, viscometry and internal friction measurements. The results show that the glass transition temperature Tg of DTA and the isokom temperature T12, of viscometry are in excellent agreement, confirming the equivalence of enthalpy and viscous relaxation for NBS glass. Combining Tg data with water speciation data demonstrates that OH groups are mainly responsible for the decrease of Tg with increasing hydration, while molecular water plays only a minor role. Internal friction spectra at 7.125 Hz confirm the decisive influence of water on mechanical relaxation. The temperature range of α-relaxation (glass transition) strongly decreases while two β-relaxation peaks (sub-Tg) progressively appear with increasing water content. A high temperature β-relaxation peak, attributed to the presence of OH groups, shifts from 670 to 450 K as total water content increases from 0.01 to 5 wt%. A low temperature β-relaxation peak, attributed to molecular water, appears at 380 K and 330 K in glasses containing 3 and 5 wt% H2O, respectively. These findings suggest that relaxation mechanism of different hydrous species at low temperature may contribute to fatigue of stressed glasses. KW - Borosilicate glass KW - Water KW - Relaxation KW - Internal friction KW - Glass transition PY - 2018 DO - https://doi.org/10.1016/j.jnoncrysol.2018.05.025 VL - 497 SP - 30 EP - 39 PB - Elsevier B.V. AN - OPUS4-45608 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Maiwald, M. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Automated Analysis of Slow Crack Growth in Hydrous Soda-Lime Silicate Glasses N2 - To explore the impact of ambient and structural water on static fatigue, the initiation and growth of 3279 Vickers induced median radial cracks were automatically recorded and analyzed. We find that humidity is more efficient in initiating cracks and promoting their growth than water, which is dissolved in the glass structure. In particular for slow crack growth (< 3x10-6 m s-1), tests in dry nitrogen showed a considerable decrease in the crack growth exponent with increasing water content of the glasses. On the other hand, if tests were performed in humid air, the crack growth exponent was independent of the water content of the hydrous glasses, while stress intensity decreased slightly. These observations indicate that water promotes the processes at the crack-tip regardless of its origin. However, ambient water is more efficient. KW - Indentation fracture toughness KW - Slow crack growth KW - Automated analysis KW - Hydrous glass KW - Vickers indentation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513085 DO - https://doi.org/10.3389/fmats.2020.00268 VL - 7 SP - 268 AN - OPUS4-51308 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Herzel, Hannes A1 - Dombinov, V. A1 - Vogel, Christian A1 - Willbold, S. A1 - Levandowski, G. V. A1 - Meiller, M. A1 - Müller, F. A1 - Zang, J. W. A1 - da Fonseca-Zang, W. A. A1 - Jablonowski, N. D. A1 - Schrey, S. D. A1 - Adam, Christian T1 - Soybean Fertilized by P-Phases from Bagasse-Based Materials: P-Extraction Procedures, Diffusive Gradients in Thin Films (DGT), and X-ray Diffraction Analysis (XRD) N2 - The Brazilian sugarcane industry produced around 173 million tons (Mt) of bagasse in 2018. Bagasse is a by-product of juice extraction for ethanol and sugar production and is combusted in order to generate power, producing up to 10 Mt of ash per year. This ash contains various concentrations of plant nutrients, which allow the ash to be used as a crop fertilizer. However, the concentration and extractability of phosphorus (P), an essential plant nutrient, are low in bagasse ash. To increase the P content, we co-gasified and co-combusted bagasse with P-rich chicken manure. The resulting ash was thermochemically post-treated with alkali additives (Na2SO4 and K2SO4) to increase the availability of P to plants. We aimed to: (i) investigate the effect of thermochemical post-treatment of co-gasification residue and co-combustion ash on P availability to soybeans, (ii) explore the potential of chemical extraction methods (citric acid, neutral ammonium citrate, formic acid, and Mehlich-I) and diffusive gradients in thin films (DGT) to predict the availability of P to soybeans, and (iii) identify the responsible P-phases using X-ray diffraction . We evaluated P availability to soybeans growing in Brazilian Oxisol soil in two independent greenhouse pot experiments. The positive effect of thermochemical treatment on P availability from gasification residue was confirmed through the observation of increased P uptake and biomass in soybean plants. These findings were confirmed by chemical extraction methods and DGT. The gasification residue contained whitlockite as its main P-bearing phase. Thermochemical post-treatment converted whitlockite into highly soluble CaNaPO4. In contrast, co-combustion ash already contained highly soluble Ca(Na,K)PO4 as its main P-bearing phase, making thermochemical post-treatment unnecessary for increasing P availability. In conclusion, increased extractability and availability of P for soybeans were closely connected to the formation of calcium alkali phosphate. Our findings indicate that this combined methodology allows for the prediction of P-fertilization effects of ash. KW - Sugar cane bagasse KW - Chicken manure ash KW - Thermochemical treatment KW - Nutrient KW - Plant availability PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509735 DO - https://doi.org/10.3390/agronomy10060895 VL - 10 SP - 895 EP - 6 PB - MDPI AN - OPUS4-50973 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Balzer, R. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Kiefer, P. A1 - Deubener, J. A1 - Fechtelkord, M. T1 - Water in Alkali Aluminosilicate Glasses N2 - To understand the influence of water and alkalis on aluminosilicate glasses, three polymerized glasses with varying ratios of Na/K were synthesized [(22. 5-x)Na2O-xK2O-22.5 Al2O3-55 SiO2 with x = 0, 7.5, and 11.25]. Subsequently, these glasses were hydrated (up to 8 wt% H2O) in an internally heated gas pressure vessel. The density of hydrous glasses linearly decreased with water content above 1 wt%, consistent with the partial molar volume of H2O of 12 cm3/mol. Near-infrared spectroscopy revealed that hydroxyl groups are the dominant species at water content of <4 wt%, and molecular water becomes dominating at water content of >5 wt%. The fraction of OH is particularly high in the pure Na-bearing glass compared to the mixed alkali glasses. 27Al magic angle spinning-NMR spectroscopy shows that aluminum is exclusively fourfold coordinated with some variations in the local geometry. It appears that the local structure around Al becomes more ordered with increasing K/Na ratio. The incorporation of H2O reinforces this effect. The differential thermal analysis of hydrous glasses shows a significant mass loss in the range of glass transition already during the first upscan, implying the high mobility of water in the glasses. This observation can be explained by the open structure of the aluminosilicate network and by the low dissociation enthalpy of H2O in the glasses (≈ 8 kJ/mol). The effect of the dissolved H2O on the glass transition temperature is less pronounced than for other aluminosilicate glasses, probably because of the large fraction of Al in the glasses. KW - NMR spectroscopy KW - Alkali aluminosilicate glasses KW - Water speciation KW - Glass transition KW - Infrared spectroscopy PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509497 DO - https://doi.org/10.3389/fmats.2020.00085 VL - 7 SP - 85 AN - OPUS4-50949 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Waurischk, Tina A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Kiefer, P. A1 - Deubener, J. A1 - Balzer, R. A1 - Behrens, H. T1 - Crack Growth in Hydrous Soda-Lime Silicate Glass N2 - Stable crack growth was measured for nominal dry and water-bearing (6 wt%) soda-lime silicate glasses in double cantilever beam geometry and combined with DMA studies on the effects of dissolved water on internal friction and glass transition, respectively. In vacuum, a decreased slope of logarithmic crack growth velocity versus stress intensity factor is evident for the hydrous glass in line with an increase of b-relaxation intensity indicating more energy Dissipation during fracture. Further, inert crack growth in hydrous glass is found to be divided into sections of different slope, which indicates different water related crack propagation mechanism. In ambient air, a largely extended region II is observed for the hydrous glass, which indicates that crack growth is more sensitive to ambient water. KW - Internal friction KW - Soda-lime silicate glass KW - Water content KW - Stable crack growth KW - DCB geometry KW - Stress intensity factor PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506829 DO - https://doi.org/10.3389/fmats.2020.00066 VL - 7 SP - Articel 66 AN - OPUS4-50682 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Laquai, René A1 - Müller, Bernd R. A1 - Schneider, J. A1 - Kupsch, Andreas A1 - Bruno, Giovanni T1 - Using SXRR to Probe the Nature of Discontinuities in SLM Additive Manufactured Inconel 718 Specimens N2 - The utilization of additive manufacturing (AM) to fabricate robust structural components relies on understanding the nature of internal anomalies or discontinuities, which can compromise the structural integrity. While some discontinuities in AM microstructures stem from similar mechanisms as observed in more traditional processes such as casting, others are unique to the AM process. Discontinuities in AM are challenging to detect, due to their submicron size and orientation dependency. Toward the goal of improving structural integrity, minimizing discontinuities in an AM build requires an understanding of the mechanisms of formation to mitigate their occurrence. This study utilizes various techniques to evaluate the shape, size, nature and distribution of discontinuities in AM Inconel 718, in a non-hot isostatic pressed (HIPed) as-built, non-HIPed and direct age, and HIPed with two step age samples. Non-destructive synchrotron radiation refraction and transmission radiography (SXRR) provides additional information beyond that obtained with destructive optical microscopy. SXRR was able to distinguish between voids, cracks and lack of melt in, due to its sensitivity to the orientation of the discontinuity. KW - Additive manufacturing KW - X-ray refraction radiography KW - INCONEL 718 KW - Selective laser melting PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509836 DO - https://doi.org/10.1007/s11661-020-05847-5 SN - 1543-1940 VL - 51 IS - 8 SP - 4146 EP - 4157 PB - Springer AN - OPUS4-50983 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyerhofer, F. A1 - Dissinger, F. A1 - Weigert, Florian A1 - Jungclaus, J. A1 - Müller-Caspary, K. A1 - Waldvogel, S. R. A1 - Resch-Genger, Ute A1 - Voss, T. T1 - Citric Acid Based Carbon Dots with Amine Type Stabilizers: pHSpecific N2 - We report the synthesis and spectroscopic characteristics of two different sets of carbon dots (CDs) formed by hydrothermal reaction between citric acid and polyethylenimine (PEI) or 2,3-diaminopyridine (DAP). Although the formation of amide-based species and the presence of citrazinic acid type derivates assumed to be responsible for a blue emission is confirmed for both CDs by elemental analysis, infrared spectroscopy, and mass spectrometry, a higher abundance of sp2-hybridized nitrogen is observed for DAP-based CDs, which causes a red-shift of the n-π* absorption band relative to the one of PEI-based CDs. These CD Systems possess high photoluminescence quantum yields (QY) of ∼40% and ∼48% at neutral pH, demonstrating a possible tuning of the optical properties by the amine precursor. pH-Dependent spectroscopic studies revealed a drop in QY to < 9% (pH ∼ 1) and < 21% (pH ∼ 12) for both types of CDs under acidic and basic conditions. In contrast, significant differences in the pHdependency of the n-π* transitions are found for both CD types which are ascribed to different (de)protonation sequences of the CD-specific fluorophores and functional groups using Zeta potential analysis. KW - Fluorescence KW - Particle KW - Nano KW - Surface group analysis KW - Carbon dot KW - C-dot KW - Fluorescent probe KW - Quantum yield KW - Synthesis KW - IR KW - MS KW - Polymer KW - Ligand PY - 2020 DO - https://doi.org/10.1021/acs.jpcc.9b11732 VL - 124 IS - 16 SP - 8894 EP - 8904 PB - American Chemical Society AN - OPUS4-50813 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cant, D. J. H. A1 - Minelli, C. A1 - Sparnacci, K. A1 - Müller, Anja A1 - Kalbe, H. A1 - Stoger-Pollach, M. A1 - Unger, Wolfgang A1 - Werner, W. S. M. A1 - Shard, A. G. T1 - Surface-Energy Control and Characterization of Nanoparticle Coatings N2 - Accurate and reproducible measurement of the structure and properties of high-value nanoparticles is extremely important for their commercialization. A significant proportion of engineered nanoparticle systems consist of some form of nominally core-shell structure, whether by design or unintentionally. Often, these do not form an ideal core-shell structure, with typical deviations including polydispersity of the core or shell, uneven or incomplete shells, noncentral cores, and others. Such systems may be created with or without intent, and in either case an understanding of the conditions for formation of such particles is desirable. Precise determination of the structure, composition, size, and shell thickness of such particles can prove challenging without the use of a suitable range of characterization techniques. Here, the authors present two such polymer core-shell nanoparticle systems, consisting of polytetrafluoroethylene cores coated with a range of thicknesses of either polymethylmethacrylate or polystyrene. By consideration of surface energy, it is shown that these particles are expected to possess distinctly differing coating structures, with the polystyrene coating being incomplete. A comprehensive characterization of these systems is demonstrated, using a selection of complementary techniques including scanning electron microscopy, scanning transmission electron microscopy, thermogravimetric analysis, dynamic light scattering, differential centrifugal sedimentation, and X-ray photoelectron spectroscopy. By combining the results provided by these techniques, it is possible to achieve superior characterization and understanding of the particle structure than could be obtained by considering results separately. KW - Nanoparticles KW - Core-shell KW - XPS KW - Size KW - Thickness KW - Damage PY - 2020 DO - https://doi.org/10.1021/acs.jpcc.0c02161 VL - 124 IS - 20 SP - 11200 EP - 11211 PB - ACS CY - Washington DC AN - OPUS4-50899 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Rössler, C. A1 - Bauer, Ute A1 - Müller, Ralf A1 - Deubener, J. A1 - Behrens, H. T1 - Water, the other network modifier in borate glasses N2 - In the present study we have investigated whether the effect of water on properties of borate glasses resembles that of alkali oxide. Soda-lime-borate glasses with nominal compositions of x Na2O, 10 CaO, (90-x) B2O3 (x = 5, 15 and 25 mol%) were doped with up to 8 wt.% H2O by processing glass powder + distilled water in platinum capsules in an internally heated gas pressure vessel at 1523 K and 500 MPa. The water content of hydrous glasses was determined by Karl-Fischer titration and near-infrared spectroscopy. The glass transition temperature T-g. was derived from DTA and micropenetration experiments for which the effect of water loss at the surface of the hydrous glasses was studied. Heating glass samples at 10 K min(-1) in the DTA resulted in T-g values which are close to T-12 isokom temperatures confirming the equivalence of enthalpy relaxation and viscous relaxation for borate glasses. For all three glass series it is shown that T-g strongly decreases whereas the liquid fragility strongly increases upon the addition of water. These findings reveal that H2O primarily causes breaking of B-O-B bonds rather than supporting 4-fold coordinated boron as it is well-known for alkali oxides in this concentration range. (C) 2015 Elsevier B.V. All rights reserved. KW - Wasserhaltige Gläser KW - Viskosität KW - Boratgläser KW - Thermische Analyse KW - Viscosity KW - Borate glasses KW - Thermal analysis KW - Water-bearing glasses PY - 2016 DO - https://doi.org/10.1016/j.jnoncrysol.2015.10.010 SN - 0022-3093 VL - 432 SP - 208 EP - 217 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-35123 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Baer, D. R. A1 - Cant, D. J. H. A1 - Castner, D. G. A1 - Ceccone, G. A1 - Engelhard, M. H. A1 - Karakoti, A. S. A1 - Müller, Anja ED - Hodoroaba, Vasile-Dan ED - Unger, Wolfgang ED - Shard, A. G. T1 - Preparation of nanoparticles for surface analysis N2 - A variety of methods used to prepare nano-objects for surface analysis are described along with information about when they might be best applied. Intrinsic properties of NPs which complicate their characterization and need to be considered when planning for surface or other analyses of NPs are identified, including challenges associated with reproducible synthesis and functionalization of the particles as well as their dynamic nature. The relevant information about the sample preparation processes, along with analysis details and data that need to be added to the collection of material provenance information is identified. Examples of protocols that have been successfully used for preparation of nano-objects for surface analysis are included in an annex. KW - Sample preparation KW - Nanoparticles KW - Surface chemistry KW - XPS KW - Dynamic behavior KW - Nano-object KW - Surface analysis PY - 2020 SN - 978-0-12-814182-3 DO - https://doi.org/10.1016/B978-0-12-814182-3.00018-3 SP - 295 EP - 347 PB - Elsevier CY - Amsterdam AN - OPUS4-50186 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, I. A1 - Moll, J. A1 - Kexel, C. A1 - Schubert, L. A1 - Tschöke, K. A1 - Prager, Jens A1 - Lugovtsova, Yevgeniya A1 - Bach, M. A1 - Vogt, T. T1 - SHM using Guided Waves – Recent Activities and Advances in Germany N2 - Issues that prevent Structural Health Monitoring (SHM) based on Guided Waves (GW) from being a part of today’s monitoring solutions in industry are not all obvious to the scientific community. To uncover and overcome these issues, scientists working on SHM and GW problems joined in an expert committee under the patronage of the German Society for Non-Destructive Testing. An initiated online survey among more than 700 experts and users reveals the hurdles hindering the practical application of GWbased SHM. Firstly, methods for proof of reliability of SHM approaches are missing. Secondly, detailed understanding of phenomenological described wave-damage interactions is needed. Additionally, there are significant unsolved implementation issues and unsolved problems of signal processing including handling of environmental influences. To enable substantial proof of reliability without unaffordable experimental effort also efficient simulation tools including realistic damage interaction are needed, enabling the joint use of experimental and simulated data to predict the capabilities of the Monitoring system. Considering these issues, the committee focusses on simulation, signal processing, as well as probability of detection and standardization. In the presented work, recent activities of the expert committee starting with survey results are summarized. An open access data basis of life-like measurements is presented to allow testing and comparison of signal processing and simulation algorithms. Finally, a strategy for efficient proof of reliability increasing the acceptance of SHM in industry and for successful Integration of SHM into real-world engineering structures is proposed. T2 - The 12th International Workshop on Structural Health Monitoring (IWSHM) CY - Stanford, California, USA DA - 10.09.2019 KW - Structural Health Monitoring KW - Ultrasonic Guided Waves KW - Non-Destructive Testing KW - Survey KW - Probability of Detection KW - Reliability PY - 2019 SP - 1 EP - 10 AN - OPUS4-49232 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kunz, C. A1 - Bonse, Jörn A1 - Spaltmann, Dirk A1 - Neumann, C. A1 - Turchanin, A. A1 - Bartolomé, J. F. A1 - Müller, F. A. A1 - Gräf, S. T1 - Tribological performance of metal-reinforced ceramic composites selectively structured with femtosecond laser-induced periodic surface structures N2 - The impact of femtosecond (fs) laser-induced periodic surface structures (LIPSS) on tribological properties was investigated for metal-reinforced ceramic composites (Al2O3-ZrO2-Nb). For this purpose, the metallic niobium (Nb) phase was selectively structured with LIPSS in an air environment with different values of the fs-laser peak fluence by near-infrared fs-laser radiation (λ = 1025 nm, τ = 300 fs, frep = 1 kHz), taking advantage of the different light absorption behavior of ceramic and metal. The tribological performance was evaluated by reciprocating sliding tests in a ball-on-disc configuration using Ringer's solution as lubricant. The surfaces were characterized before and after laser irradiation by optical microscopy, scanning electron microscopy, atomic force microscopy, X-ray photoelectron spectroscopy, energy dispersive X-ray spectroscopy and by measuring the contact angle with Ringer's solution. The LIPSS formation resulted in an increased wetting of the surface with the lubricant. Moreover, the selectively structured composite surfaces revealed a coefficient of friction significantly reduced by a factor of ~3 when compared to the non-irradiated surface. Furthermore, the formation of a laser-induced oxidation layer was detected with NbO as the most prominent oxidation state. Selectively structured composites with outstanding mechanical properties and enhanced tribological performance are of particular interest for biomedical applications. KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Ceramic matrix composites KW - Tribology PY - 2020 DO - https://doi.org/10.1016/j.apsusc.2019.143917 SN - 0169-4332 SN - 1873-5584 VL - 499 IS - 1 SP - 143917 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-49255 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Laquai, René A1 - Müller, Bernd R. A1 - Kasperovich, G. A1 - Requena, G. A1 - Haubrich, J. A1 - Bruno, Giovanni T1 - Classification of defect types in SLM Ti-6Al-V4 by X-ray refraction topography N2 - Porosity in additively manufactured materials, such as laser powder bed fusion Ti-Al6-V4, can play an important role in their mechanical performance. Not only the total porosity but also the shape/morphology of the individual pores need to be considered. Therefore, it is necessary to determine the distributions of different defect types (especially fusing defects and keyhole pores) and their dependence on process parameters. We show that synchrotron X-ray refraction radiography allows analysis of large samples (up to several millimeters) without compromising the detectability of submicrometer defects. Correspondingly, a classification tool is introduced that is able to quantitatively distinguish defects such as keyhole pores and binding defects with a confidence level of 94 %, even when the shape cannot be discerned because of limited spatial resolution. KW - Additive manufacturing KW - Selective laser melting KW - X-ray refraction KW - Microscopy KW - Porosity KW - X-ray computed tomography KW - BAMline KW - Synchrotron Radiation PY - 2020 DO - https://doi.org/10.1520/MPC20190080 SN - 2379-1365 VL - 9 IS - 1 SP - 82 EP - 93 PB - ASTM International CY - West Conshohocken, PA AN - OPUS4-50470 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Welter, T. A1 - Marzok, Ulrich A1 - Deubener, J. A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Hydrogen diffusivity in sodium aluminosilicate glasses N2 - Hydrogen gas diffusivity of fourteen glasses of the Na2O-Al2O3-SiO2 system are studied along the joins quartzalbite-jadeite-nepheline (Qz-Ab-Jd-Np, fully polymerized) and albite-sodium disilicate (Ab-Ds, depolymerized). Density measurements show that ionic porosity decreases from 54.4% (Qz) to 51.5% (Np) and from 52.4% (Ab) to 50.2% (Ds). Hydrogen diffusivity D follows similar trends but at another scale. D at 523 K decreases from 4×10−12 to 3×10−14m2 s−1 (Qz-Np) and from 4×10−13 to 3×10−15m2 s−1 (Ab-Ds). Charge compensating Na+ acting as a filling agent in fully polymerized network structures leads to up to one order of Magnitude higher diffusivities as depolymerized glass structures of the same SiO2 content where Na+ takes the role of a modifier ion. Temperature dependence of the diffusivity indicates that both the activation energy involved with the moving H2 molecule as well as the accessible volume in the structure contribute to this compositional trend. KW - Aluminosilicate glasses KW - Hydrogen diffusivity KW - Ionic porosity PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.119502 VL - 521 SP - 119502 PB - Elsevier B.V. AN - OPUS4-50392 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Deubener, J. A1 - Müller, Ralf A1 - Behrens, H. T1 - Statistical analysis of propagation rates of indentation-induced radial cracks N2 - Due to the stochastic nature of crack nucleation by Vickers indentation, a statistical analysis of propagation rates of 185 radial cracks was performed. Crack growth was observed directly using a video camera with high Image acquisition rate. It is found that propagation rates are controlled by the environmental reactions at the crack-tip shortly after their initiation (< 1 s). Calibration of the stress intensity KI showed that the residual stress factor χ and the exponent n of the equation KI==χPc−n (with P==load and c==crack length) are broadly distributed among the 185 analyzed cracks, ranging from 10−16 to 104 and from 0.1 to 5, respectively. For the most frequent crack, the equation KI==0.052Pc−1.47 holds. The results show that correlations of indentation-induced crack length to stress intensity necessitate the use of statistical significant data that are calibrated by the environmental reactions at the crack-tip. KW - Stress intensity factor KW - Vickers indentation KW - Subcritical crack growth KW - Soda-lime-silica glass PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.119739 VL - 527 SP - 119739 PB - Elsevier B.V. AN - OPUS4-50393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Balzer, R. A1 - Behrens, H. A1 - Schuth, S. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Fechtelkord, M. A1 - Deubener, J. T1 - The influence of H2O and SiO2 on the structure of silicoborate glasses N2 - To understand the impact of dissolved water on structure and properties, four boron-rich glasses of molar compositions 15-x Na2O x CaO 15 SiO2 70 B2O3 (with x=0, 7.5, 10) and 10 Na2O 15 SiO2 75 B2O3 were prepared and subsequently hydrated (up to 8 wt% H2O). Density measurements show a non-linear trend upon hydration implying large structural changes in particular at water contents<2 wt%. Near-infrared spectroscopy shows hydroxyl groups are the dominant species in all glasses upon the entire range of water content. Molecular H2O is detectable only at total water contents>2 wt%. 11B MAS NMR spectra show that the abundance of BO4 species is mainly controlled by ratio of (Na2O+CaO)/B2O3 while incorporation of water plays a minor role. Compared to borate glasses, the efficiency of formation of BO4 tetrahedra is favored by crosslinking of the network by SiO4-units. The glass transition temperatures, determined by differential thermal analysis, decreases continuously with water content due to breakage of B-O-B bonds by hydrolysis. However, compared to Silicates and aluminosilicates, the effect of dissolved water is less pronounced which can be explained by weaker B-O-B bonds in comparison to Si-O-Si bonds. KW - High pressure KW - Water speciation KW - Silicoborate glasses KW - Infrared spectroscopy KW - NMR spectroscopy PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.05.030 VL - 519 SP - 38 EP - 51 PB - Elsevier B.V. AN - OPUS4-48748 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kiefer, P. A1 - Balzer, R. A1 - Deubener, J. A1 - Behrens, H. A1 - Waurischk, Tina A1 - Reinsch, Stefan A1 - Müller, Ralf T1 - Density, elastic constants and indentation hardness of hydrous soda-lime silica glasses N2 - The effect of structural water on density, elastic constants and microhardness of water-bearing soda-lime-silica glasses of up to 21.5 mol% total water is studied. It is found that the Poisson ratio and the water content are positively correlated, while density and the elastic moduli decrease with increasing water content. Vickers hardness decreases by approximately 27% from the dry to the most hydrous glass. For water fractions <3 mol%, the dependencies are non-linear reflecting the non-linear change in the concentrations of OH and H2O molecules dissolved, whereas for water fractions >3 mol% linear dependencies are found. To distinguish the effect of structural water and environmental water, indentations were performed in toluene, nitrogen gas and air. Timedependent softening was evident for testing dry glasses in humid atmospheres as well as for tests of hydrous glasses in dry atmospheres. This indicates that the response times of dissolved water species are effectively equal in both scenarios. KW - Elastic constants KW - Soda-lime-silica KW - Glass KW - Water content KW - Microhardness PY - 2019 DO - https://doi.org/10.1016/j.jnoncrysol.2019.119480 SN - 0022-3093 SN - 1873-4812 VL - 521 SP - 119480 PB - Elsevier B.V. AN - OPUS4-48758 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Welter, T. A1 - Müller, Ralf A1 - Deubener, J. A1 - Marzok, Ulrich A1 - Reinsch, Stefan T1 - Hydrogen Permeation Through Glass N2 - Physical storage of gaseous hydrogen under high-pressure in glassy micro-containers such as spheres and capillaries is a promising concept for enhancing safety and the volumetric capacity of mobile hydrogen storage systems. As very low permeation through the container wall is required for storage of compressed hydrogen, development of glasses of minimal hydrogen permeability is needed. For this purpose, one has to understand better the dependence of hydrogen permeability on glass structure. The paper points out that minimizing the accessible free volume is as one strategy to minimize hydrogen permeability. Based on previously measured and comprehensive literature data, it is shown that permeation is independently controlled by ionic porosity and network modifier content. Thus, ionic porosity in modified and fully polymerized networks can be decreased equally to the lowest hydrogen permeability among the glasses under study. Applying this concept, a drop of up to 30,000 with respect to the permeation of hydrogen molecules through silica glass is attainable. KW - Ionic porosity KW - hydrogen storage KW - Glass KW - Permeability KW - Solubility KW - Diffusivity PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513927 DO - https://doi.org/10.3389/fmats.2019.00342 VL - 6 SP - Article 342 AN - OPUS4-51392 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Waurischk, Tina A1 - Behrens, H. A1 - Deubener, J. T1 - Crack growth in borate and silicate glasses: Stress-corrosion susceptibility and hydrolytic resistance N2 - A double cantilever beam technique in air equipped with ultrasound modulation was used to measure the crack velocity v in borate and silicate glasses. In all glasses v and the stress intensity KI followed the empirical correlation v ~ KIn. Indicated by its smallest KI at v = 1 μm s − 1, KI* = 0.27 MPa m0.5, the silicoborate glass containing 70 mol% B2O3 was found most susceptible to stress-corrosion enhanced crack growth. Contrarily, the sodium calcium magnesium silicate glass appeared least susceptible with KI* = 0.57 MPa m0.5. No clear correlation is evident between KI*, reflecting the stress-corrosion susceptibility, and the hydrolytic resistance for all glasses under study, but values of n obtained from the present study and taken from previous literature for 35 glasses tend to decrease with increasing network modifier ion fraction. Energy dissipation during stress-corrosion enhanced crack propagation is assumed to cause this trend. KW - DCB KW - Alkali and alkaline earth silicate and borate glass KW - Crack growth in air KW - Stress-corrosion KW - Stress intensity PY - 2021 DO - https://doi.org/10.1016/j.jnoncrysol.2020.120414 VL - 551 SP - 120414 PB - Elsevier B.V. AN - OPUS4-51393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, U. A1 - McMahon, Dino Peter A1 - Rolff, J. T1 - Exposure of the wild bee Osmia bicornis to the honey bee pathogen Nosema ceranae N2 - Wild bees are important pollinators for agricultural crops and solitary species such as Osmia bicornis are particularly suitable for pollination management. Wild bees share floral resources with managed honey bees and may be exposed to emerging infectious diseases. Although studies have explored the prevalence of pathogens in solitary wild bee species, data regarding the impact of pathogens on solitary bee health are lacking. We carried out experiments examining whether the solitary bee species O. bicornis is susceptible to infection with the emerging pathogen The results obtained indicate that N. ceranae may be able to infect O. bicornis but its impact on host fitness is negligible: survival rates did not differ between Control and inoculated bees, although male survival was marginally lower after infection. To explore the possible field-relevance of our findings, we collected wild bees near an infected and a non-infected hive and showed that N. ceranae was shared between managed and wild bees, although only the in presence of infected honey bees. The findings of the present study show that O. bicornis is susceptible to pathogen spillover and could act as a potential reservoir host for N. ceranae in pollinator networks. Additional studies on this species incorporating sublethal effects, multiple infections and other interacting stressors are warranted. KW - Wild bees KW - Nosema ceranae KW - Osmia bicornis KW - Pathogen spillover KW - Survival rates PY - 2019 DO - https://doi.org/10.1111/afe.12338 SN - 1461-9555 SN - 1461-9563 VL - 21 IS - 4 SP - 363 EP - 371 PB - Wiley AN - OPUS4-49648 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bramke, K. A1 - Müller, U. A1 - McMahon, Dino Peter A1 - Rolff, J. T1 - Exposure of Larvae of the Solitary Bee Osmia bicornis to the Honey Bee Pathogen Nosema ceranae Aects Life History N2 - Wild bees are important pollinators of wild plants and agricultural crops and they are threatened by several environmental stressors including emerging pathogens. Honey bees have been suggested as a potential source of pathogen spillover. One prevalent pathogen that has recently emerged as a honey bee disease is the microsporidian Nosema ceranae. While the impacts of N. ceranae in honey bees are well documented, virtually nothing is known about its effects in solitary wild bees. The solitary mason bee Osmia bicornis is a common pollinator in orchards and amenable to Commercial management. Here, we experimentally exposed larvae of O. bicornis to food contaminated with N. ceranae and document spore presence during larval development. We measured mortality, growth parameters, and timing of pupation in a semi-field experiment. Hatched individuals were assessed for physiological state including fat body mass, wing muscle mass, and body size. We recorded higher mortality in the viable-spore-exposed group but could only detect a low number of Spores among the individuals of this treatment. Viable-spore-treated individuals with higher head capsule width had a delayed pupation start. No impact on the physiological status could be detected in hatched imagines. Although we did not find overt evidence of O. bicornis infection, our findings indicate that exposure of larvae to viable N. ceranae spores could affect bee development. KW - Bee diseases KW - Wild bees KW - Nosema ceranae KW - Osmia bicornis KW - Pathogen transmission KW - Solitary bees KW - Bee health PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-496497 DO - https://doi.org/10.3390/insects10110380 VL - 10 IS - 11 SP - 380 PB - MDPI AN - OPUS4-49649 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liens, A. A1 - Reveron, H. A1 - Douillard, T. A1 - Blanchard, N. A1 - Lughi, V. A1 - Sergo, V. A1 - Laquai, René A1 - Müller, Bernd R. A1 - Bruno, Giovanni A1 - Schomer, S. A1 - Fürderer, T. A1 - Adolfsson, E. A1 - Courtois, N. A1 - Swain, M. A1 - Chevalier, J. T1 - Phase transformation induces plasticity with negligible damage in ceria-stabilized zirconia-based ceramics N2 - Ceramics and their composites are in general brittle materials because they are predominantly made up of ionic and covalent bonds that avoid dislocation motion at room temperature. However, a remarkable ductile behavior has been observed on newly developed 11 mol.% ceria-stabilized zirconia (11Ce-TZP) composite containing fine alumina (8 vol.% Al2O3) and elongated strontium hexa-aluminate (8 vol.% SrAl12O19) grains. The as-synthesized composite also has shown full resistance to Low Temperature Degradation (LTD), relatively high strength and exceptionally high Weibull modulus, allowing its use in a broader range of biomedical applications. In this study, to deepen the understanding of plastic deformation in Ce-TZP based composites that could soon be used for manufacturing dental implants, different mechanical tests were applied on the material, followed by complete microstructural characterization. Distinct from pure Ce-TZP material or other zirconia-based ceramics developed in the past, the material here studied can be permanently strained without affecting the Young modulus, indicating that the ductile response of tested samples cannot be associated to damage occurrence. This ductility is related to the stress-induced tetragonal to monoclinic (t-m) zirconia phase transformation, analogue to Transformation-Induced Plasticity (TRIP) steels, where retained austenite is transformed to martensite. The aim of this study is to corroborate if the observed plasticity can be associated exclusively to the zirconia t-m phase transformation, or also to microcraking induced by the transformation. The t-m transformed-zones produced after bending and biaxial tests were examined by X-ray refraction and SEM/TEM coupled with Raman. The results revealed that the observed elastic-plastic behavior occurs without extensive microcracking, confirming a purely elastic-plastic behavior driven by the phase transformation (absence of damage). KW - Zirconia KW - Ceria KW - Ceramic matrix composite KW - Plasticity KW - Phase transformation KW - X-Ray Refraction PY - 2020 UR - http://www.sciencedirect.com/science/article/pii/S1359645419307177 DO - https://doi.org/10.1016/j.actamat.2019.10.046 SN - 1359-6454 VL - 183 SP - 261 EP - 273 PB - Elsevier Ltd. AN - OPUS4-49740 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Laquai, René A1 - Müller, Bernd R. A1 - Kasperovich, G. A1 - Haubrich, J. A1 - Requena, G. A1 - Bruno, Giovanni T1 - X-ray refraction distinguishes unprocessed powder from empty pores in selective laser melting Ti-6Al-4V N2 - For the first time, X-ray refraction techniques are proven for the identification of void formation in Ti-6Al-4V parts produced by selective laser melting. The topology and volume fraction of pores are measured in samples produced with different laser energy density. Unique X-ray refraction methods identify different kinds of defects, characteristic to the regions below and above the Optimum laser energy density, namely unprocessed powder (unmolten powder particles, balling effect, and Fusion defects) from empty keyhole pores. Furthermore, it is possible to detect small inhomogeneities (voids or cracks) with sizes below the spatial resolution of optical microscopy and X-ray computed tomography. KW - Additive manufacturing KW - X-ray refraction KW - Microscopy KW - X-ray computed tomography KW - Porosity PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-434041 DO - https://doi.org/10.1080/21663831.2017.1409288 SN - 2166-3831 VL - 6 IS - 2 SP - 130 EP - 135 PB - Taylor & Francis Group CY - London, UK AN - OPUS4-43404 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Buckle, T. A1 - van der Wal, S. A1 - van Malderen, S. A1 - Müller, Larissa A1 - Kuil, J. A1 - van Unen, V. A1 - Peters, R. A1 - van Bemmel, M. A1 - McDonnell, L. A1 - Velders, A. A1 - Koning, F. A1 - Vanhaeke, F. A1 - van Leeuwen, F. T1 - Hybrid imaging labels: providing the link between mass spectrometry-based molecular pathology and theranostics N2 - Development of theranostic concepts that include inductively coupled plasma mass spectrometry (ICP-MS) and laser ablation ICP-MS (LA-ICP-MS) imaging can be hindered by the lack of a direct comparison to more standardly used methods for in vitro and in vivo evaluation; e.g. fluorescence or nuclear medicine. In this study a bimodal (or rather, hybrid) tracer that contains both a fluorescent dye and a chelate was used to evaluate the existence of a direct link between mass spectrometry (MS) and in vitro and in vivo molecular imaging findings using fluorescence and radioisotopes. At the same time, the hybrid label was used to determine whether the use of a single isotope label would allow for MS-based diagnostics. KW - Imaging KW - Laser Ablation ICP-MS KW - Diagnostics PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-396813 DO - https://doi.org/10.7150/thno.17484 VL - 7 IS - 3 SP - 624 EP - 633 PB - IvySpring AN - OPUS4-39681 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Bernd R. A1 - Kupsch, Andreas A1 - Laquai, René A1 - Nellesen, J. A1 - Tillmann, W. A1 - Kasperovich, G. A1 - Bruno, Giovanni T1 - Microstructure characterisation of advanced materials via 2D and 3D X-ray refraction techniques N2 - 3D imaging techniques have an enormous potential to understand the microstructure, its evolution, and its link to mechanical, thermal, and transport properties. In this conference paper we report the use of a powerful, yet not so wide-spread, set of X-ray techniques based on refraction effects. X-ray refraction allows determining internal specific surface (surface per unit volume) in a non-destructive fashion, position and orientation sensitive, and with a nanometric detectability. We demonstrate showcases of ceramics and composite materials, where microstructural parameters could be achieved in a way unrivalled even by high-resolution techniques such as electron microscopy or computed tomography. We present in situ analysis of the damage evolution in an Al/Al2O3 metal matrix composite during tensile load and the identification of void formation (different kinds of defects, particularly unsintered powder hidden in pores, and small inhomogeneity’s like cracks) in Ti64 parts produced by selective laser melting using synchrotron X-ray refraction radiography and tomography. T2 - THERMEC 2018: 10TH international conference on processing and manufacturing of advanced materials CY - Paris, France DA - 08.07.2018 KW - Additive manufacturing (AM) KW - Creep KW - Damage evolution KW - Synchrotron X-ray refraction radiography KW - Metal matrix composites PY - 2018 UR - https://www.scientific.net/MSF.941.2401 SN - 978-3-0357-1208-7 DO - https://doi.org/10.4028/www.scientific.net/MSF.941.2401 SN - 1662-9752 SN - 0255-5476 VL - 941 SP - 2401 EP - 2406 PB - Trans Tech Publications CY - Switzerland AN - OPUS4-47148 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meyer, Klas A1 - Paul, Andrea A1 - Ruiken, J.-P. A1 - Westad, Frank A1 - Illner, M. A1 - Müller, D. A1 - Esche, E. A1 - Repke, J.-U. A1 - Maiwald, Michael T1 - Online Spectroscopy in Microemulsions – A Process Analytical Approach for a Hydroformylation Mini-plant N2 - Within the Collaborative Research Center InPROMPT a novel process concept for the hydroformylation of long-chained olefins is studied in a mini-plant, using a rhodium complex as catalyst in the presence of syngas. Recently, the hydroformylation in micro¬emulsions, which allows for the efficient recycling of the expensive rhodium catalyst, was found to be feasible. However, the high sensitivity of this multi-phase system with regard to changes in temperature and composition demands a continuous observation of the reaction to achieve a reliable and economic plant operation. For that purpose, we tested the potential of both online NMR and Raman spectroscopy for process control. The lab-scale experiments were supported by off-line GC-analysis as a reference method. A fiber optic coupled probe of a process Raman spectrometer was directly integrated into the reactor. 25 mixtures with varying concentrations of olefin (1-dodecene), product (n-tridecanal), water, n-dodecane, and technical surfactant (Marlipal 24/70) were prepared according to a D-optimal design. Online NMR spectroscopy was implemented by using a flow probe equipped with 1/16” PFA tubing serving as a flow cell. This was hyphenated to the reactor within a thermostated bypass to maintain process conditions in the transfer lines. Partial least squares regression (PLSR) models were established based on the initial spectra after activation of the reaction with syngas for the prediction of unknown concentrations of 1-dodecene and n-tridecanal over the course of the reaction in the lab-scale system. The obtained Raman spectra do not only contain information on the chemical composition but are further affected by the emulsion properties of the mixtures, which depend on the phase state and the type of micelles. Based on the spectral signature of both Raman and NMR spectra, it could be deduced that especially in reaction mixtures with high 1-dodecene content the formation of isomers as a competitive reaction was dominating. Similar trends were also observed during some of the process runs in the mini-plant. The multivariate calibration allowed for the estimation of reactants and products of the hydroformylation reaction in both laboratory setup and mini-plant. T2 - 4th European Conference on Process Analytics and Control Technology (EuroPACT 2017) CY - Potsdam, Germany DA - 10.05.2017 KW - Microemulsions KW - Process Analytical Technology KW - Reaction Monitoring KW - Online NMR Spectroscopy KW - Online Raman Spectroscopy PY - 2017 SP - 64 EP - 64 CY - Frankfurt a. M. AN - OPUS4-40228 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reveron, H. A1 - Serrano-Munoz, Itziar A1 - Kupsch, Andreas A1 - Müller, B.R. A1 - Chevalier, J. A1 - Bruno, Giovanni T1 - Transformation-induced plasticity in zirconia during tensile loading: A combined microscopy and synchrotron X-ray refraction study N2 - The stress-induced tetragonal to monoclinic (t-m) zirconia phase transformation can provide a certain degree of plasticity to Ceria-stabilized (Ce-TZP) zirconia-based composites. Characterizing and monitoring this phase transition on a millimeter-size range, within the bulk and in-situ remains a challenge. In this work, the mechanical behavior of Ce-TZP based composite was studied in tension, combining microscopy and synchrotron Xray refraction techniques. In contrast with microscopy methods, which only provide surface information, X-ray refraction radiography (SXRR) allowed the visualization of all the transformation bands, over the entire length and thickness of tested specimens, opening up new avenues for in-situ stress-induced t-m transformation studies. KW - Zirconia KW - Ceria KW - Composite KW - Phase transformation KW - Plasticity KW - Synchrotron X-ray refraction PY - 2024 DO - https://doi.org/10.1016/j.matlet.2024.136445 SN - 0167-577X SN - 1873-4979 VL - 366 SP - 1 EP - 4 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-59977 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klingbeil, Patrick A1 - Vogl, Jochen A1 - Pritzkow, Wolfgang A1 - Riebe, Gundel A1 - Müller, J. T1 - Comparative studies on the certification of reference materials by ICPMS and TIMS using isotope dilution procedures N2 - A comparison of different isotope dilution mass spectrometric (IDMS) procedures using inductively coupled plasma mass spectrometry (ICPMS) and thermal ionization mass spectrometry (TIMS) was carried out to examine the degree of equivalence between the used procedures in terms of requirements for reference material certification. The comparison was based on the measurement results and their uncertainties. The sample used in this study is a pure zinc metal to be certified by the Bureau Communie de Référence (BCR) for amount contents of different trace elements. This study focuses on cadmium and thallium. The TIMS values contributed to the certified values. To guarantee identical conditions as far as possible for the procedures under investigation, the samples were split into subsamples after spiking and digestion took place. Thus, every IDMS procedure started with an identical set of samples. In total, four different IDMS procedures and one external calibration procedure using internal standardization as an example of routine analysis were applied. The IDMS procedures divide in a group with and a group without trace/matrix separation. Multicollector TIMS (TI-MC-MS) and multicollector ICPMS (ICP-MC-MS) were used in combination with trace/matrix separation, whereas quadrupole ICPMS (ICP-QMS) and ICP-MC-MS were also applied to nonseparated samples. All IDMS results agree well within their combined uncertainties, while some results from the external calibration procedure do not. IDMS results obtained by ICPMS without separation are comparable to those obtained by TI-MC-MS with separation regarding precision and accuracy. The smallest uncertainties were achieved using ICP-MC-MS in combination with trace/matrix separation. KW - ICP-MS KW - TIMS KW - IDMS KW - multi-collector KW - uncertainty budget KW - Certification KW - reference material PY - 2001 DO - https://doi.org/10.1021/ac001278c SN - 0003-2700 SN - 1520-6882 VL - 73 IS - 8 SP - 1881 EP - 1888 PB - American Chemical Society CY - Washington, DC AN - OPUS4-909 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Deubener, J. A1 - Behrens, H. A1 - Müller, Ralf T1 - An overview on the effect of dissolved water on the viscosity of soda lime silicate melts N2 - In this review article, the impact of dissolved water on the viscous properties of soda lime silicate melts is addressed against the background of the upcoming switch from natural gas to hydrogen combustion. This change will lead to an increase in the total water content of the glasses by up to 0.4 mol%. In order to better define possible influences of water speciation, water-rich glasses were synthesised under increasing pressure up to the kbar range. It is shown that a distinction must be made between the influence of dissolved OH-groups and H2Omolecules in order to accurately reflect the dependence of isokom temperatures on water content. In addition, an increase of one order of magnitude in the tolerance to higher deformation rates was observed for the range of expected increased water contents during isothermal deformation processes, which is based on the timetemperature superposition principle, i.e. congruent flow curves were determined under isokomal conditions. KW - Water in glass KW - Viscosity KW - Soda lime silicate glass KW - Shear thinning KW - Nydrogen melting PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587276 DO - https://doi.org/10.1016/j.nocx.2023.100195 VL - 19 SP - 1 EP - 10 PB - Elsevier B.V. AN - OPUS4-58727 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dombinov, V. A1 - Herzel, Hannes A1 - Meiller, M. A1 - Müller, F. A1 - Willbold, S. A1 - Zang, J. W. A1 - da Fonseca-Zang, W. A. A1 - Adam, Christian A1 - Klose, H. A1 - Poorter, H. A1 - Jablonowski, N. D. A1 - Schrey, S. D. T1 - Sugarcane bagasse ash as fertilizer for soybeans: Effects of added residues on ash composition, mineralogy, phosphorus extractability and plant availability N2 - Sugarcane bagasse is commonly combusted to generate energy. Unfortunately, recycling strategies rarely consider the resulting ash as a potential fertilizer. To evaluate this recycling strategy for a sustainable circular economy, we characterized bagasse ash as a fertilizer and measured the effects of co-gasification and co-combustion of bagasse with either chicken manure or sewage sludge: on the phosphorus (P) mass fraction, P-extractability, and mineral P phases. Furthermore, we investigated the ashes as fertilizer for soybeans under greenhouse conditions. All methods in combination are reliable indicators helping to assess and predict P availability from ashes to soybeans. The fertilizer efficiency of pure bagasse ash increased with the ash amount supplied to the substrate. Nevertheless, it was not as effective as fertilization with triple-superphosphate and K2SO4, which we attributed to lower P availability. Co-gasification and co-combustion increased the P mass fraction in all bagasse-based ashes, but its extractability and availability to soybeans increased only when co-processed with chicken manure, because it enabled the formation of readily available Ca-alkali phosphates. Therefore, we recommend co-combusting biomass with alkali-rich residues to increase the availability of P from the ash to plants. KW - Combustion and gasification KW - Phosphate extractability and availability KW - X-ray diffraction (XRD) PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-567632 DO - https://doi.org/10.3389/fpls.2022.1041924 SN - 1664-462X VL - 13 SP - 1 EP - 13 PB - Frontiers Media CY - Lausanne AN - OPUS4-56763 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reinsch, Stefan A1 - Welter, T. A1 - Müller, Ralf A1 - Deubener, J. T1 - Hydrogen Permeability of Tectosilicate Glasses for Tank Barrier Liners N2 - The permeation of hydrogen gas was studied in meta-aluminous (tectosilicate) glass powders of Li2O×Al2O3×SiO2 (LAS), Na2O×Al2O3×SiO2 (NAS) and MgO×Al2O3×SiO2 (MAS) systems by pressure loading and vacuum extraction in the temperatures range 210–310 °C. With this method, both the solubility S and the diffusivity D were determined, while the permeability was given by the product SD. For all glasses, S was found to decrease with temperature, while D increased. Since the activation energy of diffusion of H2 molecules exceeded that of dissolution, permeation increased slightly with temperature. When extrapolated to standard conditions (25 °C), the permeability of tectosilicate glasses was found to be only 10-22–10-24 mol H2 (m s Pa)-1, which is 8–10 magnitudes lower than most polymers. Thin glass liners of these compositions are expected to be the most effective barrier for tanks of pressurised hydrogen. KW - Hydrogen permeation KW - Aluminosilicate glasses KW - Hydrogen storage tank KW - Glass liner PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587284 DO - https://doi.org/10.52825/glass-europe.v1i.425 VL - 1 SP - 1 EP - 11 AN - OPUS4-58728 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dal Molin, E. S. A1 - Henning, L. M. A1 - Müller, J. T. A1 - Smales, Glen Jacob A1 - Pauw, Brian Richard A1 - Bekheet, M. F. A1 - Gurlo, A. A1 - Simon, U. T1 - Robocasting of ordered mesoporous silica‐based monoliths: Rheological, textural, and mechanical characterization N2 - Hierarchically porous, high‐surface‐area silica materials are excellent candidates for multiple applications like catalysis and environmental remediation. Shaping these materials with additive manufacturing (AM) techniques, like robocasting, could enable their use with the benefit of on‐demand, customized shaping and maximizing performance. Herein, ordered mesoporous silica COK‐12 slurries were robocasted into monoliths, containing different ratios of uncalcined COK‐12 and sodium bentonite (0–25 wt.%). The rheology of the mixed slurries is characterized by lower flow indexes (0.69 vs. 0.32) and higher yield stresses (96 vs. 259 Pa) compared to pure COK‐12 ones. Monoliths were printed in woodpile structures and calcined at 600°C. Micro‐CT measurements showed a linear shrinkage of 25% after calcination. Mechanical characterization showed increased uniaxial strength (0.20 ± 0.07 to 1.0 ± 0.3 MPa) with increasing binder/solids ratio from 13 to 25%. The amorphous, mesoporous structure of COK‐12 was retained. The structures exhibited open porosities of 52 ± 4% and showed higher specific mesopore volumes, and increased average mesopore size (6 vs. 8 nm) compared to COK‐12. Small‐angle x‐ray scattering analysis revealed an increased lattice parameter (10.3 vs. 11.0 nm) and reduced wall thickness (3.1 nm vs. 4.1 nm) of the COK‐12 in the monoliths. These properties indicate suitability for their application as porous supports and adsorbents. KW - Industrial and Manufacturing Engineering KW - Additive manufacturing KW - OMS KW - Porous materials KW - Robocasting KW - X-ray scattering KW - MOUSE PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-582503 DO - https://doi.org/10.1002/nano.202300109 VL - 4 IS - 11-12 SP - 615 EP - 631 PB - Wiley-VCH GmbH AN - OPUS4-58250 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, W. A1 - Schweins, R. A1 - Nöcker, B. A1 - Kohlbrecher, J. A1 - Smales, Glen Jacob A1 - Huber, K. T1 - Comparative study of the co-assembly behaviour of 3-chloro-4-hydroxy-phenylazo dyes with DTAB N2 - The co-assembly of three one-fold negatively charged 3-chloro-4-hydroxy-phenylazo dyes (Yellow, Blue and Red) with the cationic surfactant dodecyltrimethylammoniumbromide (DTAB) was studied to probe dye–DTAB binding stoichiometry and assembly morphology. For each dye, phase separation was observed above a given dye : DTAB ratio with the ratio depending on the dye. While Yellow and DTAB showed liquid/liquid phase separation above Yellow : DTAB = 1 : 1.67, crystalline dye–DTAB complexes were observed for Blue–DTAB and Red–DTAB above Blue : DTAB = 1 : 2.56 and Red : DTAB = 1 : 2.94 respecively. In homogeneous solution, UV/vis spectroscopic investigations suggest stochiometries of Yellow : DTAB = 1 : 2, Blue : DTAB = 1 : 3 and Red : DTAB = 1 : 4. It was concluded, that Yellow exhibits the highest dye : DTAB binding stoichiometry in both, dye–surfactant complexes in the 2-phase region and in solution, whereas the lowest dye : DTAB binding stoichiometry was observed for Red–DTAB in both cases. The observed stoichiometries are inversely correlated to the impact dye addition has on the morphology of DTAB micelles. Generally, addition of dye to DTAB micelles leads to a reduction in spontaneous curvature of these micelles and to the formation of triaxial ellipsoidal or cylindrical micelles from oblate ellipsoidal DTAB micelles. At a DTAB concentration of 30 mM and a dye concentration of 5 mM, this effect was most pronounced for Red and least pronounced for Yellow, whilst Blue showed an intermediate effect. KW - Dye KW - DTAB KW - SAXS KW - Small-angle X-ray scattering KW - X-ray scattering KW - Data analysis KW - Micelle PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576978 DO - https://doi.org/10.1039/D3SM00501A SN - 1744-683X VL - 19 IS - 24 SP - 4588 EP - 4598 PB - Royal Society of Chemistry AN - OPUS4-57697 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Horn, Wolfgang A1 - Müller, B. A1 - Jann, Oliver A1 - Kasche, J. A1 - Däumling, C. A1 - Kalus, Sabine A1 - Brödner, Doris T1 - Emission and odour measurement of construction products evaluated using a german construction product evaluation scheme T2 - Indoor Air 2005 CY - Beijing, PR China DA - 2005-09-04 KW - AgBB-Scheme KW - Construction product KW - VOC emission KW - Odour KW - Chamber test PY - 2005 SN - 7-89494-830-6 IS - 2 SP - 2129 EP - 2133 PB - Tsinghua University Press CY - Beijing AN - OPUS4-10913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Kasche, J. A1 - Dahms, A. A1 - Horn, Wolfgang A1 - Jann, Oliver A1 - Müller, D. T1 - Sensory evaluation of building products - Results of a German round robin test T2 - VDI-Tagung CY - Bad Kissingen, Deutschland DA - 2007-11-13 KW - Bauprodukte KW - Emissionen KW - Geruch KW - AbBB-Schema KW - Kammermessungen KW - Blauer Engel PY - 2007 SN - 978-3-18-091995-9 SN - 0083-5560 IS - 1995 SP - 193 EP - 202 PB - VDI-Verl. CY - Düsseldorf AN - OPUS4-16322 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schartel, Bernhard A1 - Perret, Birgit A1 - Dittrich, Bettina A1 - Ciesielski, M. A1 - Krämer, J. A1 - Müller, P. A1 - Altstädt, V. A1 - Zang, L. A1 - Döring, M. T1 - Flame retardancy of polymers: the role of specific reactions in the condensed phase N2 - Condensed-phase mechanisms play a major role in fire-retardant polymers. Generations of development have followed the concept of charring to improve fire properties. Whereas the principal reactions are believed to be known, the specific description for multicomponent systems is lacking, as is the picture across different systems. A two-step approach is proposed in general, and also presented in greater detail. The second step covers the specific reactions controlling charring, whereas the actual reactants are provided in the preceding step. This model consistently incorporates the variety of structure–property relationships reported. A comprehensive case study is presented on seven phosphorus flame retardants in two epoxy resins to breathe life into the two-step approach. KW - Charring KW - Epoxy KW - Flame retardancy KW - Pyrolysis KW - Thermogravimetric analysis (TGA) PY - 2016 DO - https://doi.org/10.1002/mame.201500250 SN - 1438-7492 SN - 1439-2054 VL - 301 IS - 1 SP - 9 EP - 35 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-35273 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bennet, Francesca A1 - Müller, Anja A1 - Radnik, Jörg A1 - Hachenberger, Y. A1 - Jungnickel, H. A1 - Laue, P. A1 - Luch, A. A1 - Tentschert, J. T1 - Preparation of Nanoparticles for ToF-SIMS and XPS Analysis N2 - Nanoparticles have gained increasing attention in recent years due to their potential and application in different fields including medicine, cosmetics, chemistry, and their potential to enable advanced materials. To effectively understand and regulate the physico-chemical properties and potential adverse effects of nanoparticles, validated measurement procedures for the various properties of nanoparticles need to be developed. While procedures for measuring nanoparticle size and size Distribution are already established, standardized methods for analysis of their surface chemistry are not yet in place, although the influence of the surface chemistry on nanoparticle properties is undisputed. In particular, storage and preparation of nanoparticles for surface analysis strongly influences the analytical results from various methods, and in order to obtain consistent results, sample preparation must be both optimized and standardized. In this contribution, we present, in detail, some standard procedures for preparing nanoparticles for surface analytics. In principle, nanoparticles can be deposited on a suitable substrate from suspension or as a powder. Silicon (Si) Wafers are commonly used as substrate, however, their cleaning is critical to the process. For sample preparation from suspension, we will discuss drop-casting and spin-coating, where not only the cleanliness of the substrate and purity of the suspension but also its concentration play important roles for the success of the preparation methodology. For nanoparticles with sensitive ligand shells or coatings, deposition as powders is more suitable, although this method requires particular care in fixing the sample. KW - Titania nanoparticles KW - X-ray photoelectron spectroscopy KW - Secondary ion mass spectrometry KW - Surface chemisttry PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-520103 UR - https://www.jove.com/video/61758 DO - https://doi.org/10.3791/61758 VL - 163 SP - e61758 AN - OPUS4-52010 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Safarov, J. A1 - Tuma, Dirk A1 - Müller, K. T1 - Thermophysical properties of the paramagnetic ionic liquid 1-butyl-3-methylimidazolium tetrachloroferrate over an extended range of temperature and pressure N2 - The paramagnetic ionic liquid 1-butyl-3-methylimidazolium tetrachloroferrate [BMIM][FeCl4] was subject to multiple high-precision thermophysical property measurements under both ambient and high pressure. Density rho(p0,T) / kg m-3 and speed of sound u(p0,T) / m s-1 data at ambient pressure were recorded at temperatures T = (278.15 to 343.16) K using a DSA 5000 M combined vibrating tube densimeter and speed of sound analyser with a standard uncertainty of delta rho(p0,T) = ±0.001 kg m-3 and delta u(p0,T) = ±0.1 m s-1, respectively. High-pressure volumetric (p,rho,T) data were measured on an Anton Paar DMA HPM vibrating tube densimeter at T = (273.16 to 413.15) K and at pressures up to p = 140 MPa with an estimated experimental relative combined average percentage deviation (APD) of delta rho(p,T) / rho(p,T) = ±(0.01 to 0.08) %. The specific isobaric heat capacity cp(p0,T) / J kg-1 K-1, a caloric property, was determined at T = (273.15 to 413.15) K with an uncertainty delta cp / cp = ±0.5 % using a Perkin Elmer Pyris 1 DSC differential scanning calorimeter. To gain knowledge of transport properties, the dynamic viscosity eta(p0,T) / mPa s at ambient pressure was recorded at T = (275.03 to 413.18) K by an Anton Paar SVM 3000 Stabinger viscometer and additionally an Anton Paar rheometer MCR 302 device with uncertainties of delta eta / eta = ±0.35 % and delta eta / eta = ±1 %, respectively. The obtained data were first correlated by empirical polynomial equations of state and further processed by the application of classic thermodynamic potentials to determine isothermal compressibility kappa T(p,T) / MPa-1, isobaric thermal expansivity alpha p(p,T) / K-1, thermal pressure coefficient gamma(p,T) / MPa K-1, internal pressure pint(p,T) / MPa, specific heat capacity at constant pressure cp(p,T) / J kg-1 K-1 and at constant volume cv(p,T) / J kg-1 K-1, the difference of isobaric and isochoric heat capacity (cp–cv)(p,T) / J kg-1 K-1, speed of sound u(p,T) / m s-1 and ultimately isentropic exponent kappa s(p,T). This work extends knowledge about the thermophysical properties of [BMIM][FeCl4] particularly to high temperatures and pressures. KW - Ionic liquid KW - Volumetric properties KW - Transport properties KW - Caloric properties PY - 2022 DO - https://doi.org/10.1016/j.molliq.2021.117939 SN - 0167-7322 VL - 346 SP - 1 EP - 16 PB - Elsevier CY - Amsterdam AN - OPUS4-54228 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brücher, M. A1 - von Bohlen, A. A1 - Jacob, P. A1 - Franzke, J. A1 - Radtke, Martin A1 - Reinholz, Uwe A1 - Müller, Bernd R. A1 - Scharf, Oliver A1 - Hergenröder, R. T1 - The charge of solid-liquid interfaces measured by X-ray standing waves and streaming current N2 - Measurements of ion distributions at a charged solid–liquid interface using X-ray standing waves (XSW) are presented. High energy synchrotron radiation (17.48 keV) is used to produce an XSW pattern inside a thin water film on a silicon wafer. The liquid phase is an aqueous solution containing Br and Rb ions. The surface charge is adjusted by titration. Measurements are performed over a pH range from 2.2–9, using the native Si oxide layer and functional (amine) groups as surface charge. The Debye length, indicating the extension of the diffuse layer, could be measured with values varying between 1–4 nm. For functionalized wafers, the pH dependent change from attraction to repulsion of an ion species could be detected, indicating the isoelectric point. In combination with the measurement of the streaming current, the surface charge of the sample could be quantified. KW - Interfacial charge KW - Solid/liquid interfaces KW - Surface analysis KW - Surface functionalization KW - X-ray spectrometry KW - X-ray KW - Standing waves KW - XSW KW - Streaming current KW - Synchrotron radiation PY - 2010 DO - https://doi.org/10.1002/cphc.201000166 SN - 1439-4235 SN - 1439-7641 VL - 11 IS - 10 SP - 2118 EP - 2123 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-22057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Renate A1 - Rudolphi, Reinald A1 - Kasper, F.-J. A1 - Wagner, Armin T1 - The Thermal Transmittance of Windows PY - 1983 SN - 0306-9931 VL - 11 IS - 5 SP - 292 EP - 297 PB - Centre Scientifique et Technique du Bâtiment CY - Paris AN - OPUS4-1242 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Maul, Ronald A1 - Müller, C. A1 - Rieß, Stephanie A1 - Koch, Matthias A1 - Methner, F.-J. A1 - Nehls, Irene T1 - Germination induces the glucosylation of the Fusarium mycotoxin deoxynivalenol in various grains N2 - In food, the mycotoxin deoxynivalenol (DON) often occurs in conjunction with its 3-β-D-glucopyranoside (D3G). The transformation of DON to D3G through glucosylation is catalysed by plant enzymes, however, the exact circumstances are not well understood. In order to investigate the role of enzymatic glucosylation in germinating grains, DON treated kernels were steeped and germinated under laboratory conditions. Furthermore, the effect of malting on the DON content of the contaminated barley was investigated. In all cases, DON and its derivatives were quantified by HPLC-MS/MS before, during and after the experiments. Amongst the six tested cereals; wheat, rye, barley, spelt, and millet transformed DON to D3G during germination whilst the oats were inactive. For wheat, barley, and spelt the initial DON content was reduced by 50%, with the loss being almost entirely accounted for by D3G formation. As D3G might be cleaved during digestion, the elevated D3G concentration may obscure the toxicologically relevant DON content in processed food and beer. The germination process has a major influence on the 'masking' of DON, leading to high quantities of D3G that may be missed in common mycotoxin analyses. KW - Mycotoxins KW - Masked mycotoxins KW - Deoxynivalenol (DON) KW - DON-3-glucoside KW - Acetyl-DON KW - Germination KW - Malting PY - 2012 DO - https://doi.org/10.1016/j.foodchem.2011.08.077 SN - 0308-8146 VL - 131 IS - 1 SP - 274 EP - 279 PB - Elsevier CY - Amsterdam [u.a.] ; Jena AN - OPUS4-25732 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ast, S. A1 - Fischer, Tobias A1 - Müller, H. A1 - Mickler, W. A1 - Schwichtenberg, M. A1 - Rurack, Knut A1 - Holdt, H.-J. T1 - Integration of the 1,2,3-triazole 'click' motif as a potent signalling element in metal ion responsive fluorescent probes N2 - In a systematic approach we synthesized a new series of fluorescent probes incorporating donor–acceptor (D-A) substituted 1,2,3-triazoles as conjugative π-linkers between the alkali metal ion receptor N-phenylaza-[18]crown-6 and different fluorophoric groups with different electron-acceptor properties (4-naphthalimide, meso-phenyl-BODIPY and 9-anthracene) and investigated their performance in organic and aqueous environments (physiological conditions). In the charge-transfer (CT) type probes 1, 2 and 7, the fluorescence is almost completely quenched by intramolecular CT (ICT) processes involving charge-separated states. In the presence of Na+ and K+ ICT is interrupted, which resulted in a lighting-up of the fluorescence in acetonitrile. Among the investigated fluoroionophores, compound 7, which contains a 9-anthracenyl moiety as the electron-accepting fluorophore, is the only probe which retains light-up features in water and works as a highly K+/Na+-selective probe under simulated physiological conditions. Virtually decoupled BODIPY-based 6 and photoinduced electron transfer (PET) type probes 3–5, where the 10-substituted anthracen-9-yl fluorophores are connected to the 1,2,3-triazole through a methylene spacer, show strong ion-induced fluorescence enhancement in acetonitrile, but not under physiological conditions. Electrochemical studies and theoretical calculations were used to assess and support the underlying mechanisms for the new ICT and PET 1,2,3-triazole fluoroionophores. KW - Charge transfer KW - Click chemistry KW - Electron transfer KW - Fluorescent probes KW - Metal ions PY - 2013 DO - https://doi.org/10.1002/chem.201201575 SN - 0947-6539 SN - 1521-3765 VL - 19 IS - 9 SP - 2990 EP - 3005 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-27742 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Güttler, B. A1 - Schiel, D. A1 - Danzebrink, H. A1 - Unger, Wolfgang A1 - Gross, Thomas A1 - Lippitz, Andreas A1 - Müller, J.-P. T1 - Physical and Chemical Characterization of Thermal and Native Siliconoxide layers on Silicon T2 - Symposium "Reference Materials for Technologies in the New Millenium" CY - Berlin, BAM, Germany DA - 2000-05-22 PY - 2000 SP - 1(?) EP - 7(?) AN - OPUS4-6924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wirth, Cynthia A1 - Müller, Ralf A1 - Günster, Jens A1 - Mühler, T. A1 - Görke, R. A1 - Heinrich, J.G. T1 - Submicrometer silica spheres generated by laser fuming N2 - The production of agglomerate-free SiO2 particles exhibiting a monomodal distribution of particle sizes of around 300 nm by means of direct laser fuming of micrometric SiO2 powders has been successfully demonstrated. With a 12 kW cw CO2 laser system, a production rate of up to 1 kilogram powder per hour was achieved. Almost ideal spherical amorphous SiO2 particles in a broad particle size distribution between 10 nm and several 100 nm (d50 ≈ 300 nm) were synthesized. Several observations suggest weak agglomeration forces between the particles. A temperature reduction of 200 °C for sintering powder compacts was observed. KW - Laser KW - SiO2 KW - Nanopowder PY - 2013 DO - https://doi.org/10.4416/JCST2012-00033 SN - 2190-9385 N1 - Geburtsname von Wirth, Cynthia: Gomes, C. M. - Birth name of Wirth, Cynthia: Gomes, C. M. VL - 4 IS - 1 SP - 11 EP - 18 PB - Göller CY - Baden-Baden AN - OPUS4-31423 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Gardei, André A1 - Garcia, O. A1 - Riedl, Martin A1 - Vanhellemond, I. A1 - Suput, J.S. A1 - Santarelli, M.-L. A1 - Rodríguez-Maribona, I. A1 - Müller, Urs ED - Jadwiga W. Lukaszewicz, ED - Piotr Niemcewicz, T1 - Performance and durability of a new antigraffiti system for cultural heritage - the EC project GRAFFITAGE T2 - 11th International Congress on Deterioration and Conservation of Stone CY - Torun, Poland DA - 2008-09-15 KW - Cultural heritage KW - Antigraffiti system KW - Sandstone KW - Limestone KW - Brick KW - Monument KW - Cleaning KW - Historische Baustoffe PY - 2008 SN - 978-83-231-2237-1 VL - II SP - 889 EP - 897 PB - Nicolaus Copernicus University Press CY - Torun, Poland AN - OPUS4-18844 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Debatin, F. A1 - Thomas, A. A1 - Kelling, A. A1 - Hedin, N. A1 - Bacsik, Z. A1 - Senkovska, I. A1 - Kaskel, S. A1 - Junginger, M. A1 - Müller, H. A1 - Schilde, U. A1 - Jäger, Christian A1 - Friedrich, A. A1 - Holdt, H.-J. T1 - In situ synthesis of an imidazolate-4-amide-5-imidate ligand and formation of a microporous zinc-organic framework with H2-and CO2-storage ability KW - Metal-organic framework KW - Synthesis KW - XRD KW - FTIR KW - NMR KW - Gas sorption KW - Microporous materials KW - N,O ligands KW - Solvothermal synthesis PY - 2010 DO - https://doi.org/10.1002/anie.200906188 SN - 1433-7851 SN - 1521-3773 SN - 0570-0833 VL - 49 IS - 7 SP - 1258 EP - 1262 PB - Wiley-VCH CY - Weinheim AN - OPUS4-21132 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stephan, H. A1 - Walther, M. A1 - Fähnemann, S. A1 - Ceroni, P. A1 - Molloy, J.K. A1 - Bergamini, G. A1 - Heisig, F. A1 - Müller, C.E. A1 - Kraus, Werner A1 - Comba, P. T1 - Bispidines for dual imaging N2 - The efficient transformation of the hexadentate bispidinol 1 into carbamate derivatives yields functional bispidines enabling convenient functionalization for targeted imaging. The BODIPY-substituted bispidine 3 combines a coordination site for metal ions, such as radioactive 64CuII, with a fluorescent unit. Product 3 was thoroughly characterized by standard analytical methods, single crystal X-ray diffraction, radiolabeling, and photophysical analysis. The luminescence of ligand 3 was found to be strongly dependent on metal ion coordination: CuII quenches the BODIPY fluorescence, whereas NiII and ZnII ions do not affect it. It follows that, in imaging applications with the positron emitter 64CuII, residues of its origin from enriched 64Ni and the decay products 64NiII and 64ZnII, efficiently restore the fluorescence of the ligand. This allows for monitoring of the emitted radiation as well as the fluorescence signal. The stability of the 64CuII–3 complex is investigated by transmetalation experiments with ZnII and NiII, using fluorescence and radioactivity detection, and the results confirm the high stability of 64CuII–3. In addition, metal complexes of ligand 3 with the lanthanide ions TbIII, EuIII, and NdIII are shown to exhibit emission of the BODIPY ligand and the lanthanide ion, thus enabling dual emission detection. KW - Bispidines KW - Chelates KW - Imaging agents KW - Lanthanides KW - Radiolabeling KW - Nuclear medical application KW - Radioactive labelling KW - SPECT PY - 2014 DO - https://doi.org/10.1002/chem.201404086 SN - 0947-6539 SN - 1521-3765 VL - 20 IS - 51 SP - 17011 EP - 17018 PB - Wiley-VCH Verl. CY - Weinheim AN - OPUS4-32320 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mühler, T. A1 - Helsch, G. A1 - Heinrich, J.G. A1 - Yao, Dongxu A1 - Gräf, S. A1 - Müller, F.A. A1 - Günster, Jens T1 - Strategies for the selective volume sintering of ceramics N2 - The present study is dealing with the basic physics for a novel way to generate a free-formed ceramic body, not like common layer by layer, but directly by Selective Volume Sintering (SVS) in a compact block of ceramic powder. To penetrate with laser light into the volume of a ceramic powder compact it is necessary to investigate the light scattering properties of ceramic powders. Compared with polymers and metals, ceramic materials are unique as they offer a wide optical window of transparency. The optical window typically ranges from below 0.3 up to 5 µm wave length. In the present study thin layers of quartz glass (SiO2) particles have been prepared. As a function of layer thickness and the particle size, transmission and reflection spectra in a wave length range between 0.5 and 2.5 µm have been recorded. Depending on the respective particle size and by choosing a proper relation between particle size and wave length of the incident laser radiation, it is found that light can penetrate a powder compact up to a depth of a few millimeters. With an adjustment of the light absorption properties of the compact the initiation of sintering in the volume of the compact is possible. KW - Additive Manufacturing PY - 2014 DO - https://doi.org/10.1557/jmr.2014.174 SN - 0884-2914 VL - 29 IS - 17 SP - 2095 EP - 2099 PB - Materials Research Society CY - Warrendale, Pa. AN - OPUS4-32544 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Herrmann, Ralf A1 - Hille, Falk A1 - Said, Samir A1 - Sterthaus, Jens A1 - Müller, Karsten A1 - Quercetti, Thomas A1 - Wille, Frank A1 - Paffenholz, J.-A. A1 - Baeßler, Matthias ED - Papadrakakis, M. ED - Fragiadakis, M. ED - Papadimitriou, C. T1 - Implementing a Structural Health Monitoring system using digital models of the BAM large drop test facility in Horstwalde N2 - At the Bundesanstalt für Materialforschung und -prüfung (BAM) full scale specimens for nuclear transport and storage containers (casks) are tested for their structural integrity in a series of drop tests on the Test Site Technical Safety in Horstwalde, 50 km south of Berlin. These drop tests cause a major stress not only on the casks, but also on the steel tower structure of the test facility, itself. The load pattern makes the structure very interesting for detailed investigation. The focus of the monitoring lies on the bolted joints of the flange connections that are a typical connection for cylindrical elements if welding is technical or economical unfavorable. The definition of the monitoring takes was done by investigating the existing documents and inspection results accompanied by building an initial digital representation of the structure, consisting of two finite element (FE) models and a geometrical 3D point cloud representation. As a first step the structures behavior during static and dynamic loading was analyzed using measurement data and an updated numerical FE Model. The idea behind is to use models for a digital planning and operation/evaluation of the structural health monitoring. A static FE simulation and a dynamic FE simulation are generated, to investigate how the structure behaves under the load conditions. T2 - XI International Conference on Structural Dynamics (EuroDyn 2020) CY - Online meeting DA - 23.11.2020 KW - Structural Health Monitoring KW - Drop Tests KW - System Identification KW - Digital Models KW - BIM PY - 2020 UR - https://generalconferencefiles.s3-eu-west-1.amazonaws.com/eurodyn_2020_ebook_procedings_vol1.pdf SN - 978-618-85072-0-3 VL - 1 SP - 1293 EP - 1304 PB - Institute of Structural Analysis and Antiseismic Research CY - Athen AN - OPUS4-51592 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wolff, M. A1 - Wonneberger, R. A1 - Freiberg, K.E. A1 - Hertwig, Andreas A1 - Bonse, Jörn A1 - Giebeler, L. A1 - Koitzsch, A. A1 - Kunz, C. A1 - Weber, H. A1 - Hufenbach, J.K. A1 - Müller, F.A. A1 - Gräf, S. T1 - Formation of laser-induced periodic surface structures on Zr-based bulk metallic glasses with different chemical composition N2 - Bulk metallic glasses (BMG) are amorphous metal alloys known for their unique physical and mechanical properties. In the present study, the formation of femtosecond (fs) laser-induced periodic surface structures (LIPSS) on the Zr-based BMGs Zr46Cu46Al8, Zr61Cu25Al12Ti2, Zr52.5Cu17.9Al10Ni14.6Ti5 (Vit105) and Zr57Cu15.4Al10Ni12.6Nb5 (Vit106) was investigated as a function of their different chemical composition. For this purpose, LIPSS were generated on the sample surfaces in an air environment by fs-laser irradiation (λ = 1025 nm, τ = 300 fs, frep = 100 kHz). The surface topography was characterized by scanning electron microscopy and atomic force microscopy. Moreover, the impact of LIPSS formation on the structure and chemical surface composition was analyzed before and after fs-laser irradiation by X-ray diffraction and X-ray photoelectron spectroscopy as well as by transmission electron microscopy in combination with energy dispersive X-ray spectroscopy. Despite the different chemical composition of the investigated BMGs, the fs-laser irradiation resulted in almost similar properties of the generated LIPSS patterns. In the case of Zr61Cu25Al12Ti2, Vit105 and Vit106, the surface analysis revealed the preservation of the amorphous state of the materials during fs-laser irradiation. The study demonstrated the presence of a native oxide layer on all pristine BMGs. In addition, fs-laser irradiation results in the formation of laser-induced oxide layers of larger thickness consisting of an amorphous ZrAlCu-oxide. The precise laser-structuring of BMG surfaces on the nanoscale provides a versatile alternative to thermoplastic forming of BMG surfaces and is of particular interest for the engineering of functional material surfaces. KW - Bulk metallic glasses KW - Femtosecond laser KW - Laser-induced periodic surface structures (LIPSS) KW - Chemical analysis KW - Oxidation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-581799 DO - https://doi.org/10.1016/j.surfin.2023.103305 SN - 2468-0230 VL - 42 SP - 1 EP - 11 PB - Elsevier B.V. AN - OPUS4-58179 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meyer, Klas A1 - Ruiken, J.-P. A1 - Illner, M. A1 - Paul, Andrea A1 - Müller, D. A1 - Esche, E. A1 - Wozny, G. A1 - Maiwald, Michael T1 - Process spectroscopy in microemulsions - setup and multi-spectral approach for reaction monitoring of a homogeneous hydroformylation process N2 - Reaction monitoring in disperse systems, such as emulsions, is of significant technical importance in various disciplines like biotechnological engineering, chemical industry, food science, and a growing number other technical fields. These systems pose several challenges when it comes to process analytics, such as heterogeneity of mixtures, changes in optical behavior, and low optical activity. Concerning this, online nuclear magnetic resonance (NMR) spectroscopy is a powerful technique for process monitoring in complex reaction mixtures due to its unique direct comparison abilities, while at the same time being non-invasive and independent of optical properties of the sample. In this study the applicability of online-spectroscopic methods on the homogeneously catalyzed hydroformylation system of 1-dodecene to tridecanal is investigated, which is operated in a mini-plant scale at Technische Universität Berlin. The design of a laboratory setup for process-like calibration experiments is presented, including a 500 MHz online NMR spectrometer, a benchtop NMR device with 43 MHz proton frequency as well as two Raman probes and a flow cell assembly for an ultraviolet and visible light (UV/VIS) spectrometer. Results of high-resolution online NMR spectroscopy are shown and technical as well as process-specific problems observed during the measurements are discussed. KW - Online-spectroscopy KW - Quantitative NMR spectroscopy KW - Process analytical technology KW - Microemulsions PY - 2017 DO - https://doi.org/10.1088/1361-6501/aa54f3 SN - 0957-0233 SN - 1361-6501 VL - 28 IS - 3 SP - 035501-1 EP - 035501-11 PB - IOP Publishing Ltd. AN - OPUS4-39091 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Paul, Andrea A1 - Ruiken, J.-P. A1 - Meyer, Klas A1 - Westad, Frank A1 - Illner, M. A1 - Müller, D. A1 - Wozny, G. A1 - Maiwald, Michael T1 - Online spectroscopy in microemulsions – A process analytical approach for hydroformylation miniplant II - Calibration and prediction by Raman spectra N2 - The Collaborative Research Center InPROMPT aims to establish a novel process concept for the hydroformylation of long-chained olefins, using a rhodium complex as catalyst in the presence of syngas. Recently, the hydroformylation in micro-emulsions, which allows for the efficient recycling of the expensive rhodium catalyst, was found to be feasible. However, the temperature and concentration sensitive multi-phase system demands a continuous observation of the reaction to achieve an operational and economically feasible plant operation. For that purpose, we tested the potential of both NMR and Raman spectroscopy for process control assistance. The lab-scale experiments were supported by sampling for off-line GC-analysis as reference analytics. The results of the NMR experiments will be part of another contribution. T2 - 11. Kolloquium Arbeitskreis Prozessanalytik CY - Wien, Austria DA - 30.11.2015 KW - Prozessanalytik KW - Process analytical technology KW - Prozess-Spektroskopie KW - Emulsions KW - Hydroformylation KW - Reaction monitoring KW - Raman spectroscopy PY - 2015 SP - 66 EP - 67 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-38846 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meyer, Klas A1 - Ruiken, J.-P. A1 - Illner, M. A1 - Müller, D. A1 - Esche, E. A1 - Paul, Andrea A1 - Wozny, G. A1 - Maiwald, Michael T1 - Online spectroscopy in microemulsions – A process analytical approach for hydroformylation miniplant I – Experimental setup and NMR reaction monitoring N2 - Hydroformylation represents an important homogeneous catalyzed process, which is widely used within chemical industry. Usually applied with simple alkenes like Propene and Butene aldehydes obtained from alkenes >C6 are relevant intermediates in production of plasticizers, surfactants and polymers. Today the active catalyst species is often based on valuable Rhodium complexes in aqueous solution. This implies the problem of limited water solubility of the reactands, which is acceptable for short chain lengths, but states a problem in case of higher alkenes. Along with that efficient separation and recycling of the catalyst becomes more complicated. There are different approaches tackling this problem, e.g., by using of salt formation in the BASF process or downstream distillation within the Shell process T2 - 11. Kolloquium Arbeitskreis Prozessanalytik CY - Wien, Austria DA - 30.11.2015 KW - Prozessanalytik KW - Process analytical technology KW - Emuslions KW - Hydroformylation KW - Online NMR spectroscopy KW - Reaction monitoring PY - 2015 SP - 51 EP - 51 PB - Bundesanstalt für Materialforschung und -prüfung (BAM) CY - Berlin AN - OPUS4-38845 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bauer, L.J. A1 - Wieder, Frank A1 - Truong, V. A1 - Förste, F. A1 - Wagener, Y. A1 - Jonas, A. A1 - Praetz, S: A1 - Schlesiger, C. A1 - Kupsch, Andreas A1 - Müller, B.R. A1 - Kanngießer, B. A1 - Zaslansky, P. A1 - Mantouvalou, I. T1 - Absorption Correction for 3D Elemental Distributions of Dental Composite Materials Using Laboratory Confocal Micro-X-ray Fluorescence Spectroscopy N2 - Confocal micro-X-ray fluorescence (micro-XRF) spectroscopy facilitates three-dimensional (3D) elemental imaging of heterogeneous samples in the micrometer range. Laboratory setups using X-ray tube excitation render the method accessible for diverse research fields but interpretation of results and quantification remain challenging. The attenuation of X-rays in composites depends on the photon energy as well as on the composition and density of the material. For confocal micro-XRF, attenuation severely impacts elemental distribution information, as the signal from deeper layers is distorted by superficial layers. Absorption correction and quantification of fluorescence measurements in heterogeneous composite samples have so far not been reported. Here, an absorption correction approach for confocal micro-XRF combining density information from microcomputed tomography (micro-CT) data with laboratory X-ray absorption spectroscopy (XAS) and synchrotron transmission measurements is presented. The energy dependency of the probing volume is considered during the correction. The methodology is demonstrated on a model composite sample consisting of a bovine tooth with a clinically used restoration material. KW - Micro X-ray fluorescence spectroscopy KW - Dental composite materials KW - Computed tomography KW - Absorption correction PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601630 DO - https://doi.org/10.1021/acs.analchem.4c00116 SN - 0003-2700 SN - 1520-6882 VL - 96 IS - 21 SP - 8441 EP - 8449 PB - American Chemical Society Publications CY - Washington, DC AN - OPUS4-60163 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Stephan, Ina A1 - Askew, P. A1 - Gorbushina, Anna A1 - Grinda, Manfred A1 - Hertel, Horst A1 - Krumbein, W.E. A1 - Müller, R.-J. A1 - Pantke, Michael A1 - Plarre, Rüdiger A1 - Schmitt, G. A1 - Schwibbert, Karin ED - Czichos, Horst ED - Saito, T. ED - Smith, L. T1 - Biogenic impact on materials N2 - Materials as constituents of products or components of technical systems rarely exist in isolation and many must cope with exposure in the natural world. This chapter describes methods that simulate how a material is influenced through contact with living systems such as microorganisms and arthropods. Both unwanted and desirable interactions are considered. This biogenic impact on materials is intimately associated with the environment to which the material is exposed (Materials-Environment Interaction, Chap. 15). Factors such as moisture, temperature and availability of food sources all have a significant influence on biological systems. Corrosion (Chap. 12) and wear (Chap. 13) can also be induced or enhanced in the presence of microorganisms. Section 14.1 introduces the categories between desired (biodegradation) and undesired (biodeterioration) biological effects on materials. It also introduces the role of biocides for the protection of materials. Section 14.2 describes the testing of wood as a building material especially against microorganisms and insects. Section 14.3 characterizes the test methodologies for two other groups of organic materials, namely polymers (Sect. 14.3.1) and paper and textiles (Sect. 14.3.2). Section 14.4 deals with the susceptibility of inorganic materials such as metals (Sect. 14.4.1), concrete (Sect. 14.4.2) and ceramics (Sect. 14.4.3) to biogenic impact. Section 14.5 treats the testing methodology concerned with the performance of coatings and coating materials. In many of these tests specific strains of organisms are employed. It is vital that these strains retain their ability to utilize/attack the substrate from which they were isolated, even when kept for many years in the laboratory. Section 14.6 therefore considers the importance of maintaining robust and representative test organisms that are as capable of utilizing a substrate as their counterparts in nature such that realistic predictions of performance can be made. KW - Materialschutz KW - Biologie KW - Organismus KW - Standard KW - Prüfung PY - 2011 SN - 978-3-642-16640-2 SP - 769 EP - 844 PB - Springer CY - Berlin, Heidelberg AN - OPUS4-24210 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wolf, S. E. A1 - Müller, L. A1 - Barrea, R. A1 - Kampf, C.J. A1 - Leiterer, Jork A1 - Panne, Ulrich A1 - Hoffmann, T. A1 - Emmerling, Franziska A1 - Tremel, W. T1 - Carbonate-coordinated metal complexes precede the formation of liquid amorphous mineral emulsions of divalent metal carbonates N2 - During the mineralisation of metal carbonates MCO3 (M = Ca, Sr, Ba, Mn, Cd, Pb) liquid-like amorphous intermediates emerge. These intermediates that form via a liquid/liquid phase separation behave like a classical emulsion and are stabilized electrostatically. The occurrence of these intermediates is attributed to the formation of highly hydrated networks whose stability is mainly based on weak interactions and the variability of the metal-containing pre-critical clusters. Their existence and compositional freedom are evidenced by electrospray ionization mass spectrometry (ESI-MS). Liquid intermediates in non-classical crystallisation pathways seem to be more common than assumed. PY - 2011 DO - https://doi.org/10.1039/c0nr00761g SN - 2040-3364 SN - 2040-3372 IS - 3 SP - 1158 EP - 1165 PB - RSC Publ. CY - Cambridge AN - OPUS4-23355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -