TY - CONF A1 - Eberstein, Markus A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Rabe, Torsten A1 - Schiller, Wolfgang Arno A1 - Thiel, A. A1 - Deubener, J. T1 - Kinetic Modeling of LTCC-Shrinkage T2 - 3rd International Conference and Exhibition on Ceramic Interconnect and Ceramic Microsystems Technologies (CICMT 2007) CY - Denver, CO, USA DA - 2007-04-23 KW - LTCC KW - Glass matrix composites KW - Inclusions KW - Sintering kinetics KW - Modeling PY - 2007 SP - 1 EP - 8 PB - American Ceramic Soc. CY - Denver AN - OPUS4-14948 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Reinsch, Stefan A1 - Müller, Ralf A1 - Eberstein, Markus A1 - Deubener, J. A1 - Thiel, A. A1 - Schiller, Wolfgang Arno ED - J.G. Heinrich, ED - C.G. Aneziris, T1 - Effect of dispersed Al2O3 particles on sintering of glass matrix composites T2 - 10th International Conference of the European Ceramic Society CY - Berlin DA - 2007-06-17 KW - LTCC KW - Glass matrix composites KW - Inclusions KW - Sintering kinetics KW - Modelling PY - 2007 SN - 3-87264-022-4 SP - 290 EP - 295 PB - Göller CY - Baden-Baden AN - OPUS4-17445 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Ralf A1 - Reinsch, Stefan A1 - Eberstein, Markus A1 - Deubener, J. A1 - Thiel, A. A1 - Schiller, Wolfgang Arno T1 - Effects of dispersed Al2O3 particles on sintering of LTCC N2 - The sintering of Low Temperature Co-fired Ceramics prepared from alumoborosilicate glass- and Al2O3 powders of similar small particle size was studied by dilatometry, heating microscopy, microstructure analysis, glass- and effective viscosity measurements. The steric effect of Al3O3 inclusions was studied using a gnon-reactiveh model composite. With increasing Al3O3 volume fraction (Φ ≤ 0.45), sintering decelerates and its final stage shifts to higher temperature. The attainable shrinkage is reduced as Al2O3 particle clusters bearing residual pores become more frequent. The kinetics of sintering could be described formally superposing the weighed contributions of differentially sized and randomly composed glass-crystal particle clusters and assuming a sintering rate controlled by the effective matrix viscosity, which increases with Φ and with progressive wetting of Al2O3 particles during densification. The "reactive" model composite shows significant dissolution of Al2O3 into the glass, which has two opposed effects on sintering: reducing Φ and increasing glass viscosity. For the present case (Φ = 0.25), the latter effect dominates and sintering is retarded by Al2O3 dissolution. Crystallization of wollastonite starts after full densification. Dissolution of Al2O3 was found to promote the subsequent growth of anorthite. KW - LTCC KW - Glass matrix composites KW - Al2O3-inclusions KW - Sintering kinetics PY - 2005 SN - 1022-6680 SN - 1662-8985 VL - 39-40 SP - 375 EP - 380 PB - Trans Tech Publ. CY - Zurich AN - OPUS4-18441 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -