TY - JOUR A1 - Serrano-Munoz, Itziar A1 - Evans, Alexander A1 - Mishurova, Tatiana A1 - Sprengel, Maximilian A1 - Pirling, T. A1 - Kromm, Arne A1 - Bruno, Giovanni T1 - The importance of subsurface residual stress in laser powder bed fusion IN718 N2 - The residual stress (RS) in laser powder bed fusion (LPBF) IN718 alloy samples produced using a 67°-rotation scan strategy is investigated via laboratory X-ray diffraction (XRD) and neutron diffraction (ND). The location dependence of the strain-free (d₀) lattice spacing in ND is evaluated using a grid array of coupons extracted from the far-edge of the investigated specimen. No compositional spatial variation is observed in the grid array. The calculated RS fields show considerable non-uniformity, significant stress gradients in the region from 0.6 to 2 mm below the surface, as well as subsurface maxima that cannot be accounted for via XRD. It is concluded that failure to determine such maxima would hamper a quantitative determination of RS fields by means of the stress balance method. KW - Laser powder bed fusion KW - Neutron and X-ray diffraction KW - Residual stress analysis KW - Strain-free lattice references KW - Stress balance PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532707 DO - https://doi.org/10.1002/adem.202100895 SN - 1615-7508 SN - 1527-2648 VL - 24 IS - 6 SP - 1 EP - 7 PB - Wiley-VCH CY - Weinheim AN - OPUS4-53270 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reveron, H. A1 - Serrano-Munoz, Itziar A1 - Kupsch, Andreas A1 - Müller, Bernd R. A1 - Chevalier, J. A1 - Bruno, Giovanni T1 - Transformation-induced plasticity in zirconia during tensile loading: A combined microscopy and synchrotron X-ray refraction study N2 - The stress-induced tetragonal to monoclinic (t-m) zirconia phase transformation can provide a certain degree of plasticity to Ceria-stabilized (Ce-TZP) zirconia-based composites. Characterizing and monitoring this phase transition on a millimeter-size range, within the bulk and in-situ remains a challenge. In this work, the mechanical behavior of Ce-TZP based composite was studied in tension, combining microscopy and synchrotron Xray refraction techniques. In contrast with microscopy methods, which only provide surface information, X-ray refraction radiography (SXRR) allowed the visualization of all the transformation bands, over the entire length and thickness of tested specimens, opening up new avenues for in-situ stress-induced t-m transformation studies. KW - Zirconia KW - Ceria KW - Composite KW - Phase transformation KW - Plasticity KW - Synchrotron X-ray refraction PY - 2024 DO - https://doi.org/10.1016/j.matlet.2024.136445 SN - 0167-577X SN - 1873-4979 VL - 366 SP - 1 EP - 4 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-59977 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rieder, Philipp A1 - Petrich, Lukas A1 - Serrano-Munoz, Itziar A1 - Fernández, Ricardo A1 - Bruno, Giovanni A1 - Schmidt, Volker T1 - Statistical Comparison of Substructures in Pure Aluminum Before and After Creep Deformation, Based on EBSD Image Data N2 - Electron backscatter diffraction (EBSD) images of extruded pure aluminum were statistically analyzed to investigate creep-induced subgrain structures after applying two different levels of creep stress, corresponding to the power law (PL) and power-law breakdown (PLB) regimes. Kernel average misorientation analysis of EBSD measurements revealed 2D morphologies, which were subdivided by a multi-step segmentation procedure into subgranular arrangements. Various descriptors were employed to characterize the “subgrains” quantitatively, including their size, shape, spatial arrangement, and crystallographic orientation. In particular, the analysis of the orientations of subgrains was conducted by neglecting rotations around the loading axis. This approach facilitated the individual investigation of the {001} and {111} subgrain families with respect to the loading axis for two investigated stress levels plus a reference specimen. For the PL regime, the statistical analysis of subgrain descriptors computed from segmented image data revealed a similar degree of strain accumulation for {111} and {001} subgrains. In contrast, for the PLB regime, the analyzed descriptors indicate that {111} subgrains tend to accumulate significantly more strain than {001} ones. These observations suggest that the mechanisms leading to PLB may be associated with strain localization dependent on intergranular stress, hindering the recovery process within {111} grains. KW - Crystallographic descriptor KW - Dislocation-climb-controlled creep KW - Electron backscatter diffraction (EBSD) KW - Geometric descriptor KW - Ernel average misorientation (KAM) KW - pure aluminum KW - Qquantification and segmentation KW - Statistical image analysis KW - subgrain PY - 2023 DO - https://doi.org/10.1093/micmic/ozad121 SN - 1431-9276 SP - 1 EP - 12 PB - Oxford University Press AN - OPUS4-58730 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bruno, Giovanni A1 - Mishurova, Tatiana A1 - Serrano-Munoz, Itziar A1 - Ulbricht, Alexander A1 - Fritsch, Tobias A1 - Sprengel, Maximilian A1 - Evans, Alexander A1 - Kromm, Arne A1 - Madia, Mauro ED - Bruno, Giovanni T1 - A Critical Discussion on the Diffraction-Based Experimental Determination of Residual Stress in AM Parts N2 - As opposed to reviewing results on experimental determination of residual stress by diffraction, this paper discusses the open issues when dealing with residual stress determination in additive manufactured parts, in particular those manufactured with laser powder bed fusion techniques. Three points are addressed in detail: (a) the proper determination of the strain-free reference d0, (b) the problem of the determination of the principal axes, and (c) the use of the correct diffraction elastic constants. It is shown that all methods to determine the strain-free reference d0 suffer from caveats, and care must be taken in evaluating the most suitable for the problem being tackled. In addition, it is shown that, in some systems, the principal axes do correspond to the geometrical axes of the specimen, but this needs to be systematically checked, especially in the case of uni- or bidirectional hatching strategies. Finally, the need to experimentally determine the proper diffraction elastic constants is underlined, especially in the case of strongly textured specimens, which again depends on the deposition strategy. T2 - ASTM ICAM 2020 – ASTM International Conference on Additive Manufacturing CY - Online meeting DA - 16.11.2020 KW - Additive Manufacturing KW - Diffraction KW - Residual Stress PY - 2020 DO - https://doi.org/10.1520/STP163120190148 VL - STP1631 SP - 122 EP - 138 PB - ASTM International CY - USA AN - OPUS4-51347 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Serrano-Munoz, Itziar T1 - Influence of the scanning strategy on the residual stress state in IN718 additive manufactured parts N2 - Laser Powder Bed Fusion (L-PBF) is an additive manufacturing technique enabling the design of complex geometries that are unrivalled by conventional production technologies. Nevertheless, L-PBF process is known to induce a high amount of residual stresses (RS) due to the high temperature gradients present during powder melting by laser. High tensile residual stresses are to be found the edges whereas the bulk material shows balancing compressive RS. Literature shows that the RS is highly sensitive to the process parameters. In particular, this study presents the characterization of the RS state in two L-PBF parts produced with a rastering scan vector that undergoes 90° or 67° rotation between subsequent layers. T2 - MLZ User Meeting 2020 CY - Online meeting DA - 08.12.2020 KW - Laser Powder Bed Fusion KW - IN718 KW - EBSD analysis KW - Residual stress state PY - 2020 AN - OPUS4-51821 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Mishurova, Tatiana A1 - Fritsch, Tobias A1 - Serrano-Munoz, Itziar A1 - Evans, Alexander A1 - Sprengel, Maximilian A1 - Klaus, M. A1 - Genzel, C. A1 - Schneider, J. A1 - Bruno, Giovanni T1 - On the influence of heat treatment on microstructure and mechanical behavior of laser powder bed fused Inconel 718 N2 - A range of heat treatments have been developed for wrought Inconel 718 to obtain desired properties. For additively manufactured Inconel 718, the recently developed standard ASTM F3301 provides guidance for heat treatment of powder bed fusion specimens. Although this standard is based on standards developed for wrought Inconel 718, it does not include direct aging. Since direct aging reduces the number of processing steps, it can result in a post processing cost reduction if the desired properties are obtained. In this study, we characterized the microstructure and tensile behavior of Inconel 718 specimens produced by a laser powder bed fusion process. The specimens were heat treated according to two different routines after stress relieving: a full heat Treatment versus a one-step direct aging process. Differences in the resulting texture and grain morphology were observed. The ex-situ stress-strain behavior was broadly similar. However, a slight increase in yield strength was observed for the direct aged specimen. In order to understand this behavior, investigations with in-situ synchrotron Energy dispersive X-ray diffraction tensile testing revealed differences in the load partitioning among different Crystal directions. Importantly, the elastic anisotropy expressed by the magnitude of the diffraction elastic constants showed a dependency on the microstructures. KW - Electron microscopy KW - X-ray analysis KW - Inconel 718 KW - Additive Manufacturing KW - Mechanical behavior KW - Diffraction elastic constants PY - 2021 DO - https://doi.org/10.1016/j.msea.2020.140555 VL - 805 SP - 40555 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-52142 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mishurova, Tatiana A1 - Artzt, K. A1 - Rehmer, Birgit A1 - Haubrich, J. A1 - Ávila Calderón, Luis A1 - Schoenstein, F. A1 - Serrano-Munoz, Itziar A1 - Requena, G. A1 - Bruno, Giovanni T1 - Separation of the impact of residual stress and microstructure on the fatigue performance of LPBF Ti-6Al-4V at elevated temperature N2 - Manufacturing defects, high residual stress (RS), and microstructures affect the structural integrity of laser powder bed fusion (LPBF) Ti-6Al-4V. In this study, the individual effect of these factors on fatigue performance at elevated temperature (300 °C) was evaluated. Material in as-built condition and subjected to post-processing, including two heat treatments and hot isostatic pressing, was investigated. It was found that in the absence of tensile RS, the fatigue life at elevated temperature is primary controlled by the defects; and densification has a much stronger effect than the considered heat treatments on the improvement of the mechanical performance. KW - Additive manufacturing KW - Ti-6Al-4V KW - Residual stress KW - Fatigue performance KW - Computed tomography PY - 2021 DO - https://doi.org/10.1016/j.ijfatigue.2021.106239 SN - 0142-1123 VL - 148 SP - 106239 PB - Elsevier Ltd. AN - OPUS4-52369 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ulbricht, Alexander A1 - Altenburg, Simon A1 - Sprengel, Maximilian A1 - Sommer, Konstantin A1 - Mohr, Gunther A1 - Fritsch, Tobias A1 - Mishurova, Tatiana A1 - Serrano-Munoz, Itziar A1 - Evans, Alexander A1 - Hofmann, M. A1 - Bruno, Giovanni T1 - Separation of the Formation Mechanisms of Residual Stresses in LPBF 316L N2 - Rapid cooling rates and steep temperature gradients are characteristic of additively manufactured parts and important factors for the residual stress formation. This study examined the influence of heat accumulation on the distribution of residual stress in two prisms produced by Laser Powder Bed Fusion (LPBF) of austenitic stainless steel 316L. The layers of the prisms were exposed using two different border fill scan strategies: one scanned from the centre to the perimeter and the other from the perimeter to the centre. The goal was to reveal the effect of different heat inputs on samples featuring the same solidification shrinkage. Residual stress was characterised in one plane perpendicular to the building direction at the mid height using Neutron and Lab X-ray diffraction. Thermography data obtained during the build process were analysed in order to correlate the cooling rates and apparent surface temperatures with the residual stress results. Optical microscopy and micro computed tomography were used to correlate defect populations with the residual stress distribution. The two scanning strategies led to residual stress distributions that were typical for additively manufactured components: compressive stresses in the bulk and tensile stresses at the surface. However, due to the different heat accumulation, the maximum residual stress levels differed. We concluded that solidification shrinkage plays a major role in determining the shape of the residual stress distribution, while the temperature gradient mechanism appears to determine the magnitude of peak residual stresses. KW - Additive Manufacturing KW - Laser Powder Bed Fusion KW - LPBF KW - AISI 316L KW - Online Process Monitoring KW - Thermography KW - Residual Stress KW - Neutron Diffraction KW - X-ray Diffraction KW - Computed Tomography PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-512903 DO - https://doi.org/10.3390/met10091234 VL - 10 IS - 9 PB - MDPI CY - Basel AN - OPUS4-51290 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mouiya, M. A1 - Martynyuk, M. A1 - Kupsch, Andreas A1 - Laquai, R. A1 - Müller, Bernd R. A1 - Doyen, N.T. A1 - Tamraoui, Y. A1 - Serrano-Munoz, Itziar A1 - Huger, M. A1 - Kachanov, M. A1 - Bruno, Giovanni T1 - The stress–strain behavior of refractory microcracked aluminum titanate: The effect of zigzag microcracks and its modeling N2 - The stress–strain behavior of ceramics, such as aluminum titanate, has certain features that are unusual for brittle materials—in particular, a substantial nonlinearity under uniaxial tension, and load–unload hysteresis caused by the sharp increase of the incremental stiffness at the beginning of unloading. These features are observed experimentally and are attributed to microcracking. Here we compare different degrees of stress–strain nonlinearity of aluminum titanate materials and quantitatively model them. We use advanced mechanical testing to observe the mechanical response at room and high temperature; electron microscopy, and X-ray refraction radiography to observe the microstructural changes. Experiments show that two types of microcracks can be distinguished: (i) microcracks induced by cooling from the sintering temperature (due to heterogeneity and anisotropy of thermal expansion), with typical sizes of the order of grain size, and (ii) much larger microcracks generated by the mechanical loading. The two microcrack types produce different effects on the stress–strain curves. Such microcracks and the features of the stress–strain behavior depend on the density of the cooling-induced microcracks and on the distribution of grain sizes. They are modeled analytically and numerically. KW - Hystersis KW - Nonlinear stress-strain curve KW - Refractory KW - Stiffness KW - X-ray refraction PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-580517 DO - https://doi.org/10.1111/jace.19325 SN - 1551-2916 VL - 106 SP - 6995 EP - 7008 PB - Wiley-Blackwell CY - Oxford [u.a.] AN - OPUS4-58051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, Bernd R. A1 - Kupsch, Andreas A1 - Serrano-Munoz, Itziar A1 - Laquai, René A1 - Bruno, Giovanni T1 - Anwendungen der Röntgenrefraktionstechnik zur zerstörungsfreien Charakterisierung von Keramiken und Verbundwerkstoffen N2 - Die Brechung von Röntgenstrahlen (Röntgenrefraktion) an Grenzflächen zwischen Materialien unterschiedlicher Dichte ist analog zur Ablenk-ung von sichtbarem Licht an z.B. Glasoberflächen. Es gibt jedoch zwei wesentliche Unterschiede: a) konvexe Grenzflächen verursachen Divergenz (d.h. der Brechungsindex n ist kleiner als 1), und b) die Ablenkungswinkel sind sehr klein, und reichen von einigen Bogensekunden bis zu einigen Bogenminuten (d.h. n ist nahe bei 1); Wie auch bei sichtbarem Licht ist die Ablenkungsrichtung der Röntgenstrahlen abhängig von der Orientierung der durchstrahlten Grenzfläche. Aufgrund dieser Eigenschaften eignen sich Röntgenrefraktionsmethoden hervorragend für: a) die Erkennung und Quantifizierung von Defekten wie Poren und Mikrorissen und b) die Bewertung von Porosität und Partikeleigenschaften wie Orientierung, Größe und räumliche Verteilung. Wir zeigen die Anwendung der Röntgenrefraktionsradiographie (2,5D Technik) und der -tomographie (3D Technik) für die Untersuchung verschiedener Probleme in der Werkstoffwissenschaft und -technologie: a) Sintern von SiC-Grünkörpern b) Porositätsanalyse in Dieselpartikelfiltersilikaten c) Faser-Matrix-Haftung in Metall- und Polymermatrixverbundwerkstoffen d) Mikrorissbildung in Glaskeramik. Wir zeigen, dass der Einsatz von Röntgenrefraktionsmethoden quantitative Ergebnisse liefert, die direkt als Parameter in Werkstoffmodellen verwendet werden können. T2 - DACH-Jahrestagung 2023 CY - Friedrichshafen, Germany DA - 15.05.2023 KW - Röntgen-Refraktion KW - Verbundwerkstoffe KW - Keramik PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576171 UR - https://jahrestagung.dgzfp.de/Portals/jt2023/BB180/Inhalt/p9.pdf UR - https://jahrestagung.dgzfp.de/Portals/jt2023/BB180/Inhalt/default.htm SN - 978-3-947971-29-9 SP - 1 EP - 16 PB - Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP) CY - Berlin AN - OPUS4-57617 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fernández, R. A1 - Bokuchava, G. A1 - Bruno, Giovanni A1 - Serrano-Munoz, Itziar A1 - González Doncel, G. T1 - On the dependence of creep-induced dislocation configurations on crystallographic orientation in pure Al and Al-Mg N2 - The peak broadening in neutron diffraction experiments on tensile specimens of pure Al (99.8%) and an Al-Mg alloy pre-deformed at different creep strains is analysed. These results are combined with the kernel angular misorientation of electron backscatter diffraction data from the creep-deformed microstructures. It is found that differently oriented grains possess different microstrains. These microstrains vary with creep strain in pure Al, but not in the Al-Mg alloy. It is proposed that this behaviour can explain the power-law breakdown in pure Al and the large creep strain observed in Al-Mg. The present findings further corroborate a description of the creep-induced dislocation structure as a fractal, predicated on previous work. KW - Creep KW - Aluminium alloys KW - Dislocations KW - Fractals KW - Diffraction peak width PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-575527 DO - https://doi.org/10.1107/S1600576723003771 SN - 0021-8898 VL - 56 IS - Pt 3 SP - 764 EP - 775 AN - OPUS4-57552 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nadammal, Naresh A1 - Mishurova, Tatiana A1 - Fritsch, Tobias A1 - Serrano-Munoz, Itziar A1 - Kromm, Arne A1 - Haberland, C. A1 - Portella, Pedro Dolabella A1 - Bruno, Giovanni T1 - Critical role of scan strategies on the development of microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing N2 - Laser based powder bed fusion additive manufacturing offers the flexibility to incorporate standard and userdefined scan strategies in a layer or in between the layers for the customized fabrication of metallic components. In the present study, four different scan strategies and their impact on the development of microstructure, texture, and residual stresses in laser powder bed fusion additive manufacturing of a nickel-based superalloy Inconel 718 was investigated. Light microscopy, scanning electron microscopy combined with electron backscatter diffraction, and neutron diffraction were used as the characterization tools. Strong textures with epitaxially grown columnar grains were observed along the build direction for the two individual scan strategies. Patterns depicting the respective scan strategies were visible in the build plane, which dictated the microstructure development in the other planes. An alternating strategy combining the individual strategies in the successive layers and a 67◦ rotational strategy weakened the texture by forming finer microstructural features. Von Mises equivalent stress plots revealed lower stress values and gradients, which translates as lower distortions for the alternating and rotational strategies. Overall results confirmed the scope for manipulating the microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing by effectively controlling the scan strategies. KW - Additive manufacturing KW - Laser powder bed fusion KW - Nickel-based superalloys KW - Scan strategies KW - Residual stresses KW - Microstructure and texture PY - 2021 DO - https://doi.org/10.1016/j.addma.2020.101792 VL - 38 SP - 1792 PB - Elsevier B.V. AN - OPUS4-51944 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Isaac, Augusta A1 - Serrano‐Munoz, Itziar A1 - Kostka, Aleksander A1 - Widjaja, Martinus Putra A1 - González‐Doncel, Gaspar A1 - Bruno, Giovanni A1 - Fernández, Ricardo T1 - Subgrain and Cavity Development during Creep of Al‐3.85%Mg N2 - It is classically considered that the creep mechanisms for type M (e.g., pure Al) and type A alloys (e.g., Al–Mg alloys) are different. In previous studies, it is predicated that fractal dislocation structures build up during creep can unify the creep behavior of pure Al and Al–Mg alloys. So far, good agreement between model and experimental data for pure Al is obtained. In this work, an Al‐3.85%Mg material crept at different strain levels (6%, 12%, 24%, and 35%) is analyzed by means of electron channelling contrast imaging. The formation of subgrains is observed at very large deformations (35%). Further examinations at 35% deformation, using electron backscatter diffraction, indicate that the subgrains and cavities tend to localize at regions where high intergranular stress mismatch is expected to occur. Laboratory X‐ray computed tomography is used to analyze the evolution of cavities between 12% and 24% stages, indicating that the fractal dimension of the cavities smaller than 100 μm varies with creep strain, as a reflection of the evolution of dislocation distribution. It is explained how the present data feed the model of the creep behavior of Al‐3.85%Mg. KW - Al–Mg alloys KW - Creep KW - Dislocations KW - Fractal KW - Intergranular residual stress KW - Subgrains PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-645905 DO - https://doi.org/10.1002/adem.202500263 SN - 1438-1656 SP - 1 EP - 10 PB - Wiley VHC-Verlag AN - OPUS4-64590 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pohl, P. A1 - Kümmel, F. A1 - Schunk, C. A1 - Serrano-Munoz, Itziar A1 - Markötter, Henning A1 - Göken, M. A1 - Höppel, H. W. T1 - About the Role of Interfaces on the Fatigue Crack Propagation in Laminated Metallic Composites N2 - The influence of gradients in hardness and elastic properties at interfaces of dissimilar materials in laminated metallic composites (LMCs) on fatigue crack propagation is investigated experimentally for three different LMC systems: Al/Al-LMCs with dissimilar yield stress and Al/Steel-LMCs as well as Al/Ti/Steel-LMCs with dissimilar yield stress and Young’s modulus, respectively. The damage tolerant fatigue behavior in Al/Al-LMCs with an alternating layer structure is enhanced significantly compared to constituent monolithic materials. The prevalent toughening mechanisms at the interfaces are identified by microscopical methods and synchrotron X-ray computed tomography. For the soft/hard transition, crack deflection mechanisms at the vicinity of the interface are observed, whereas crack bifurcation mechanisms can be seen for the hard/soft transition. The crack propagation in Al/Steel-LMCs was studied conducting in-situ scanning electron microscope (SEM) experiments in the respective low cycle fatigue (LCF) and high cycle fatigue (HCF) regimes of the laminate. The enhanced resistance against crack propagation in the LCF regime is attributed to the prevalent stress redistribution, crack deflection, and crack bridging mechanisms. The fatigue properties of different Al/Ti/Steel-LMC systems show the potential of LMCs in terms of an appropriate selection of constituents in combination with an optimized architecture. The results are also discussed under the aspect of tailored lightweight applications subjected to cyclic loading. KW - Laminated metallic composites KW - Toughening mechanisms KW - Interfaces KW - Fatigue crack propagation KW - Fatigue crack growth PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-526531 DO - https://doi.org/10.3390/ma14102564 VL - 14 IS - 10 SP - 2564 PB - MDPI AN - OPUS4-52653 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -