TY - JOUR A1 - Laquai, René A1 - Müller, Bernd R. A1 - Kasperovich, G. A1 - Requena, G. A1 - Haubrich, J. A1 - Bruno, Giovanni T1 - Classification of defect types in SLM Ti-6Al-V4 by X-ray refraction topography N2 - Porosity in additively manufactured materials, such as laser powder bed fusion Ti-Al6-V4, can play an important role in their mechanical performance. Not only the total porosity but also the shape/morphology of the individual pores need to be considered. Therefore, it is necessary to determine the distributions of different defect types (especially fusing defects and keyhole pores) and their dependence on process parameters. We show that synchrotron X-ray refraction radiography allows analysis of large samples (up to several millimeters) without compromising the detectability of submicrometer defects. Correspondingly, a classification tool is introduced that is able to quantitatively distinguish defects such as keyhole pores and binding defects with a confidence level of 94 %, even when the shape cannot be discerned because of limited spatial resolution. KW - Additive manufacturing KW - Selective laser melting KW - X-ray refraction KW - Microscopy KW - Porosity KW - X-ray computed tomography KW - BAMline KW - Synchrotron Radiation PY - 2020 DO - https://doi.org/10.1520/MPC20190080 SN - 2379-1365 VL - 9 IS - 1 SP - 82 EP - 93 PB - ASTM International CY - West Conshohocken, PA AN - OPUS4-50470 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Laquai, René A1 - Müller, Bernd R. A1 - Kasperovich, G. A1 - Haubrich, J. A1 - Requena, G. A1 - Bruno, Giovanni T1 - X-ray refraction distinguishes unprocessed powder from empty pores in selective laser melting Ti-6Al-4V N2 - For the first time, X-ray refraction techniques are proven for the identification of void formation in Ti-6Al-4V parts produced by selective laser melting. The topology and volume fraction of pores are measured in samples produced with different laser energy density. Unique X-ray refraction methods identify different kinds of defects, characteristic to the regions below and above the Optimum laser energy density, namely unprocessed powder (unmolten powder particles, balling effect, and Fusion defects) from empty keyhole pores. Furthermore, it is possible to detect small inhomogeneities (voids or cracks) with sizes below the spatial resolution of optical microscopy and X-ray computed tomography. KW - Additive manufacturing KW - X-ray refraction KW - Microscopy KW - X-ray computed tomography KW - Porosity PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-434041 DO - https://doi.org/10.1080/21663831.2017.1409288 SN - 2166-3831 VL - 6 IS - 2 SP - 130 EP - 135 PB - Taylor & Francis Group CY - London, UK AN - OPUS4-43404 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - de Moraes, Flavia A1 - Müller, Wolfgang A1 - Frischat, G.H. A1 - Müller, Ralf T1 - Corrosion and crystallization at the inner surfaces of glass bricks N2 - Glass bricks are important transparent building materials. They are produced by joining two halves of glass pressings at 600–700 °C. During this production process alkali oxides evaporate and are redeposited at the cooler inner front surfaces of the bricks. This surface layer reacts with H2O and CO2 from the residual brick atmosphere, leading to the formation of an alkali-rich silicate-hydrate layer of ≥50 nm thickness, which could be evidenced leading to a reduced nano-hardness of similar thickness, and from which NaHCO3 crystals can finally grow. Climate chamber experiments (repeated cooling between at -8 and -14 °C and reheating to 0 to 15 °C) resulted in reversible NaHCO3 crystallization and redissolution, presumably influenced by water evaporation or condensation and driven by the NaHCO3 supersaturation of the silicate-hydrate layer. Depending on the time–temperature schedule, different crystal morphologies became visible in this closed system, e.g. isolated spherical crystals, crystals arranged in chains and in double-chains, respectively, which can limit already the transmittance of the glass bricks. When a crack occurs or the brick is opened, the hygroscopic NaHCO3 crystals take up more H2O from the ambient, react irreversibly with the glass surface, finally leading to a total loss of transmittance. KW - Chemical properties KW - Chemical durability KW - Corrosion KW - Crystallization KW - Crystal growth KW - Nucleation KW - Glasses KW - Mass spectroscopy KW - Mechanical properties KW - Hardness KW - Indentation KW - Microindentation KW - Microscopy KW - Optical microscopy KW - Scanning electron microscopy KW - Optical properties KW - Optical spectroscopy KW - Oxide glasses KW - Alkali silicates KW - Soda-lime-silica KW - Surfaces and interfaces PY - 2008 DO - https://doi.org/10.1016/j.jnoncrysol.2007.07.086 SN - 0022-3093 VL - 354 IS - 2-9 SP - 284 EP - 289 PB - North-Holland Publ. Co. CY - Amsterdam AN - OPUS4-16433 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -