TY - CONF A1 - Hüsken, Götz A1 - Brouwers, H.J.H. T1 - The influence of the fines on the early-age behavior of zero-slump concrete T2 - 18. Ibausil - Internationale Baustofftagung CY - Weimar, Germany DA - 2012-09-12 KW - Zero-slump concrete KW - Green-strength KW - Compaction behavior KW - Intensive compaction test PY - 2012 SN - 978-3-00-034075-8 VL - 2 IS - 3.07 SP - 2-0001 - 2-0008 AN - OPUS4-26541 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Quercia, G. A1 - Spiesz, P. A1 - Hüsken, Götz A1 - Brouwers, H.J.H. T1 - Chloride intrusion and freeze-thaw resistance of self-compacting concrete with two different nano-SiO2 T2 - 18. Ibausil - Internationale Baustofftagung CY - Weimar, Germany DA - 2012-09-12 KW - Nano-SiO2 KW - Concrete KW - Self compacting KW - Durability KW - Chloride and freeze-thaw KW - Nano-silica PY - 2012 SN - 978-3-00-034075-8 VL - 2 IS - 3.07 SP - 2-0123 - 2-0136 AN - OPUS4-26542 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hüsken, Götz A1 - Brouwers, J. T1 - The Influence of the Fines on the Early-Age Behavior of Zero-Slump Concrete T2 - IBAUSIL CY - Weimar, Germany DA - 2012-09-12 PY - 2012 AN - OPUS4-26514 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hüsken, Götz A1 - Brouwers, H.J.H. T1 - On the early-age behavior of zero-slump concrete N2 - This paper presents experimental investigations and analyses on the early-age-behavior of zero-slump concrete, such as compaction behavior and green-strength. First, the influence of the granulometric properties of the fines is discussed in detail. For this purpose, the early-age behavior of two different fines (quartz flour and fly ash) is investigated by means of the intensive compaction test (IC-test). The tests on the influence of the fines focus on effects caused by differences in the particle shape and the use of a plasticizing admixture. The conducted tests on the compaction behavior of the fines and their corresponding green-strength are extended to continuously graded granular mixes. Here, the influence of optimized particle packing on the early-age behavior is presented and a comparison on the basis of the aforementioned quartz flour and fly ash is made. In this consideration, experimental investigations on the early-age behavior of a zero-slump concrete mix and possible effects on the hardened concrete properties are included. KW - Zero-slump concrete (A) KW - Green-strength (C) KW - Compaction behavior (A) KW - Intensive compaction test (C) PY - 2012 U6 - https://doi.org/10.1016/j.cemconres.2011.11.007 SN - 0008-8846 SN - 1873-3948 VL - 42 IS - 3 SP - 501 EP - 510 PB - Pergamon Press CY - New York, NY AN - OPUS4-26078 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Quercia, G. A1 - Hüsken, Götz A1 - Brouwers, H.J.H. T1 - Water demand of amorphous nano silica and its impact on the workability of cement paste N2 - This paper addresses the characterization of six different amorphous silica samples with respect to their application in cement paste. Different mixes are compared and analyzed using the mini spread-flow test. Also the granular properties, different void fraction states of packing and distribution moduli q are analyzed and compared using a mix design tool. A deformation coefficient is derived from the spread-flow test, which correlates with the value of specific surface area computed from the particle size distribution, and intrinsic density of the samples. Finally, the thickness of a constant water layer of 25 nm around the particles is computed at the onset of flowing. The granular analysis demonstrated that it is possible to decrease the water demand of the cement paste when nanoparticles are added and the resulting grading follows the modified Andreasen and Andersen curve (q = 0.5), and the concentration of nano silica is less than 5% bwoc. KW - Nano silica (D) KW - Particle size distribution (B) KW - Surface area (B) KW - Water demand (A) KW - Workability (A) PY - 2012 U6 - https://doi.org/10.1016/j.cemconres.2011.10.008 SN - 0008-8846 SN - 1873-3948 VL - 42 IS - 2 SP - 344 EP - 357 PB - Pergamon Press CY - New York, NY AN - OPUS4-26079 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Weise, Frank A1 - Hüsken, Götz T1 - Ringversuch zum statischen Spaltzugversuch nach AL Sp-Beton N2 - Für die rechnerische Dimensionierung der Betondecken im Oberbau von Verkehrsflächen für den Neubau sowie die Erneuerung nach RDO-Beton 09 ist die statische Spaltzugfestigkeit an der unteren und oberen Bohrkernscheibe entsprechend der Vorgaben der AL Sp-Beton zu bestimmen. Aufgrund der unzureichenden Kenntnis der Präzision dieses Prüfverfahrens wurden, basierend auf dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen, mit einem breit aufgestellten Ringversuch die statistischen Kennwerte an Labor- und Bestandsbetonen unter Vergleich- und Wiederholbedingungen ermittelt. Zur möglichst guten statistischen Absicherung nahmen an dem Ringversuch dreizehn erfahrene Prüfstellen teil, die vorab einem Audit unterzogen wurden. Zur Abdeckung des vielschichtigen Einsatzes des Prüfverfahrens erfolgte der Ringversuch an acht Prüflosen, die sowohl die Erst-/ Eignungsprüfung und Übereinstimmungskontrolle bei Neubaumaßnahmen, als auch die Restsubstanzbewertung von Betonfahrbahnplatten berücksichtigen. Zur Bewertung des Materialeinflusses wurde zusätzlich ein Prüflos mit Labormörtel untersucht. Die Probenvorbereitung erfolgte zentral an der BAM. Zur Sicherstellung einheitlicher Prüfbedingungen bei den Prüfstellen wurde zusätzlich eine detaillierte Standardarbeitsanweisung erarbeitet, die partiell bereits Eingang in das Normenwerk gefunden hat. Bei der Plausibilitätsprüfung aller prüflosspezifischen Einzelwerte der Spaltzug- und Druckfestigkeit wurden vereinzelt sowohl Ausführungsfehler als auch Übertragungs- und Tippfehler festgestellt. Der sich anschließende Lilliefors-Test zeigt, dass die ermittelten Einzelwerte bis auf wenige Aus-nahmen normalverteilt sind und damit die Voraussetzungen für die statistische Auswertung gegeben sind. Mittels grafischer Darstellung der Mandel’s h- und k-Werte wurden die Auffälligkeiten hinsichtlich der Mittelwerte und Varianzen prüflosspezifisch für die einzelnen Prüfstellen visualisiert und anschließend einige von ihnen mittels Grubbs- und Cochran-Test als Ausreißer identifiziert. Nach Ausreißerelimination wurde mit dem klassischen Verfahren bei der Spaltzugfestigkeit der geringste Variationskoeffizient unter Vergleich- und Wiederholbedingungen bei der Erst-/Eignungsprüfung mit 6,2 und 6,4 Prozent ermittelt. Bei einer Verminderung des Materialeinflusses durch die Verwendung eines Labormörtels verbessern sich die statistischen Kennwerte auf 4,5 und 5,3 Prozent. Mit 8,2 und 9,5 Prozent beziehungsweise 8,6 und 9,5 Prozent werden bei der Restsubstanzbewertung von Wasch- und Unterbetonen die höchsten Werte bestimmt. Das robuste Auswerteverfahren (ohne Eliminierung der Ausreißer) nach dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen erwies sich in der Form als ungeeignet und bedurfte einer Überarbeitung. Bezüglich der vergleichend mit klassischen und robusten Verfahren gewonnenen Kennwerte ist festzustellen, dass bei sehr homogenen Messergebnissen eines Prüfloses beide Verfahren nahezu die gleichen statistischen Kennwerte liefern. Bei der Eliminierung von Ausreißern sind die Ergebnisse des robusten Verfahrens in der Regel etwas größer als die des klassischen Verfahrens. Die begleitenden vertiefenden Untersuchungen bei der Spaltzugprüfung mit innovativen Prüftechniken lieferten wertvolle Erkenntnisse zur Bewertung der Prüfeinflüsse. N2 - The computational design of concrete pavements according to the requirements of the RDO-Beton 09 requires the splitting tensile strength to be determined according to specifications of the AL Sp-Beton. However, detailed information on the precision of the described test procedure is missing. Therefore, a round robin test was set up in order to determine the statistical parameters of the prescribed splitting tensile strength test on laboratory concrete and cores extracted from concrete pavements in terms of repeatability and reproducibility. 13 testing institutes have been involved in the round robin test to guarantee a representative coverage of the sector. The selected testing institutes have been audited prior the round robin test in order to ensure their capabilities. The round robin test was divided into 8 testing lots for covering the broad field of possible applications. Thereby, the testing lots cover both the initial testing of concrete and quality control of new construction. The latter case implies also the assessment of existing concrete pavements. Additionally, a cementitious mortar was designed in order to consider the influence of the material, such as maximum grain size, on the test procedure. The samples were prepared at BAM to guarantee a uniform sample preparation. Furthermore, a standard operating procedure was prepared to assure constant test conditions at the testing institutes. This standard operating procedure is already partly considered by the corresponding standard. A revision of the data reported by the testing institutes revealed that execution errors, transcription errors as well as typing errors occurred. However, a Lilliefors-Test was conducted to verify the Gaussian distribution of the reported test data and to allow the further statistical analysis. Only view data sets do not follow a Gaussian distribution, has no remarkable influence on the obtained statistical data. By means of the graphical illustration of Mandel’s h- and k-values, abnormalities of the arithmetic mean and variance are depicted. These apparent abnormalities can be identified as outliers using the Grubbs and Cochran test. After eliminating the identified outliers, the corresponding statistical parameters have been determined using the classical method for data analysis. The lowest coefficient of variation that was determined for the splitting tensile strength by using the classical method for assessment of the repeatability and reproducibility of the test procedure amounts to 6.2 and 6.4%, respectively, for the initial testing of concrete. Reducing the material influence by using a cementitious mortar, the corresponding statistical parameters were reduced to 4.5 and 5.3%. On the contrary, the highest statistical values were obtained for the assessment of existing concrete pavements. Here, values of 8.2 and 9.5% were obtained for the exposed aggregate concrete and 8.6 and 9.5% for the subconcrete, respectively. The robust method for data analysis (without elimination of outliers) according to the draft version of the technical bulletin of the FGSV turned out to be inappropriate and required, therefore, a revision. Comparing the statistical parameters obtained by the classical and robust method used for data analysis it can be stated that both methods result in nearly identical values for homogeneous data sets without outliers. Considering outliers in the existing data sets, the statistical parameters obtained by the robust method are slightly higher than the values obtained by the classical method with elimination of outliers. The additional investigations on the splitting tensile strength using innovative test procedures provided valuable findings for the assessment of test results. KW - Verfahrenspräzision KW - Betonfahrbahndecke KW - Prüfverfahren AL Sp-Beton KW - Spaltzugfestigkeit KW - Ringversuch PY - 2022 SN - 978-3-95606-688-7 SN - 0943-9323 VL - Straßenbau Heft S 178 SP - 1 EP - 90 PB - Fachverlag NW in der Carl Ed. Schünemann KG CY - Bremen AN - OPUS4-54957 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weise, Frank A1 - Müller, U. A1 - Hüsken, Götz A1 - Gardei, Andre T1 - Begutachtung Berliner Tuffsteinfassaden - Turmruine der Kaiser-Wilhelm-Gedächtniskirche und Charlottenburger Tor N2 - Am Ende des 19. und zu Beginn des 20. Jahrhunderts wurden auch in Berlin vermehrt Bauwerke mit einer Fassadenverblendung aus Eifeler Tuffsteinen errichtet. Die Eifeler Tuffsteine zeichnen sich aufgrund ihrer hohen Porosität einerseits durch eine gute Verarbeitbarkeit aus. Andererseits sind sie nur schwach gebunden und besitzen deshalb eine geringe Verwitterungsbeständigkeit. T2 - Workshop Kulturguterhaltung - Vom Dampfkessel zu Nanomaterialien CY - Berlin, Germany DA - 17.11.2021 KW - Fassade KW - Tuffstein KW - Schalenbildung PY - 2021 SN - 2567-1251 VL - 3 SP - 107 EP - 123 PB - Druckerei G. Bohm CY - Berlin AN - OPUS4-54461 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mundra, Shishir A1 - Hüsken, Götz A1 - Kühne, Hans-Carsten ED - Sena-Cruz, J. ED - Correia, L. ED - Azenha, M. T1 - Electrochemical realkalisation of carbonated "Dalle de Verre" windows N2 - Concrete-glass windows or commonly referred to as “Dalle de Verre” windows are prevalent in historical monuments across Europe. “Dalle de Verre” windows were made by placing cut stained glasses, of various shapes and sizes, into a steel reinforced concrete frame. In addition to the steel reinforcement, a few steel wires run across the concrete elements to hold the glass windows into place. Much of these structures have been damaged due to carbonation of the thin concrete covers and consequent corrosion of the steel reinforcement; and exhibit several cracks due to the expansive nature of corrosion products formed at the steel–concrete interface. This study focussed on understanding the efficacy of electrochemical realkalisation in reinstating the passive state of the steel reinforcement embedded in such concrete glass windows. Simulant “Dalle de Verre” windows (representative of windows at Kaiser-Wilhelm Gedächtniskirche) were produced using different cements with a water/cement ratio of 0.6 and carbonated under accelerated conditions. Post carbonation, the concrete glass windows were electrochemically realkalised using a sacrificial anode. The influence of highly alkaline conditions due to electrochemical realkalisation on the glass-concrete interface has also been investigated. This study shows that the passive state of the steel reinforcement in “Dalle de Verre” windows, particularly at the Kaiser-Wilhelm Gedächtniskirche (memorial church) in Berlin, can be reinstated using the electrochemical realkalisation method. T2 - 3rd RILEM Spring Convention and Conference (RSCC 2020) CY - Online meeting DA - 10.03.2020 KW - Electrochemical realkalisation KW - Carbonation KW - Concrete-glass windows KW - Passivation KW - Dalle-de-verre PY - 2021 SN - 978-3-030-76465-4 U6 - https://doi.org/10.1007/978-3-030-76465-4_15 SN - 2211-0844 VL - RILEM bookseries 34 SP - 163 EP - 171 PB - Springer CY - Cham AN - OPUS4-54299 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Strangfeld, Christoph A1 - Schönsee, Eric A1 - Jeyifous, Olubunni Anthony A1 - Mezhov, Alexander A1 - Hüsken, Götz T1 - Introduction of a monitoring system for Bingham fluids in additive manufacturing with concrete N2 - Freeform additive manufacturing of concrete structures is a rising technology in civil engineering with several fascinating advantages. Nonetheless, to ensure reliability and structural integrity, standards and quality control are required in the future to bring this technology into the market. As the concrete is manufactured continuously, continuous quality control of the printing process is also required, i.e. comprehensive process monitoring. At BAM, a test rig will be installed, enabling the printing of concrete structures with a maximum size of 2 m x 1 m x 1 m (l x w x h). Here, process monitoring is the focus of the test rig. In this study, we show the results of the first pump tests, including the measurement of several parameters such as temperature and pressure along the supply system, i.e. from the concrete pump to the printer head. T2 - NDT-CE 2022 CY - Zurich, Switzerland DA - 16.08.2022 KW - Additive manufacturing of concrete KW - Process monitoring KW - Non-destructive testing KW - Bingham fluid PY - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-556367 SP - 1 EP - 12 AN - OPUS4-55636 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kühne, Hans-Carsten A1 - Hüsken, Götz A1 - Mundra, Shishir A1 - Sander, C. A1 - Obermann, S. T1 - Die Betondickglasfenster des Glockenturms am Eiermannbau der Kaiser-Wilhelm-Gedächtniskirche N2 - Die Kaiser-Wilhelm-Gedächtniskirche (KWG) gilt als eine der wichtigsten Sehenswürdigkeiten Berlins in der City West und als ein herausragendes Beispiel für die „Dalle de Verre“ Verglasungen in sakralen Gebäuden. Der vorliegende Beitrag widmet sich der Fassade und den Glasfenstern des neuen Glockenturms, wobei die beschriebenen Szenarien aufgrund der annähernd gleichen Bauweise der restlichen neuen Baukörper in weiten Teilen starke Analogien aufweisen und insofern übertragbar sind. T2 - Workshop Kulturguterhaltung - Vom Dampfkessel zu Nanomaterialien CY - Berlin, Germany DA - 17.11.2021 KW - Kaiser-Wilhelm-Gedächtniskirche KW - Betondickglasfenster KW - Instandsetzung KW - Elektrochemische Realkalisierung PY - 2021 VL - 3 SP - 125 EP - 140 PB - Druckerei G. Bohm CY - Berlin AN - OPUS4-57092 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -