TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Stark, Wolfgang T1 - Low temperature properties of rubber seals - Results of component tests - N2 - Rubbers are widely used as sealing material in various applications. In many fieldsthefunction of seal materials at lowtemperatures is required. Therefore the understanding of faiiure mechanisms that lead to leakage at low temperatures is of high importance. Therefore the lower Operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the Standard tests a faster and more efficient technique was developed and applied. In addition the breakdown temperature of the sealing function of O-ring seals at lowtemperatures is measured in a component test Setup in dependence of the material and the degree of compression. KW - Seal KW - O-ring KW - Low temperature KW - Component test KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Bauteilversuche KW - Druckverformungsrest PY - 2013 SN - 0948-3276 SN - 0022-9520 VL - 66 IS - 7-8 SP - 26 EP - 30 PB - Hüthig CY - Heidelberg AN - OPUS4-28894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Ageing of HNBR, EPDM and FKM O-rings N2 - HNBR, EPDM and FKM O-rings were aged uncompressed and compressed at 75 °C, 100 °C, 125 °C and 150 °C for up to 1 year. HNBR exhibited the strongest ageing effects with high increases of hardness and glass transition temperature. Furthermore, heterogeneous ageing caused by diffusion-limited oxidation effects had a significant influence for HNBR at ageing temperatures of 125 °C and 150 °C. EPDM showed similar property changes as HNBR, but less pronounced. FKM displayed only minor ageing effects. O-rings aged in compression exhibited considerable compression set (CS). CS data was used for a time-temperature shift and resulting master curve construction. Leakage rate measurements showed that O-rings can remain leak tight under static conditions even if material properties have already deteriorated strongly. N2 - HNBR-, EPDM- und FKM-O-Ringe wurden unverpresst und verpresst für bis zu 1 Jahr bei 75 °C, 100 °C, 125 °C und 150 °C gealtert. HNBR wies mit hohen Anstiegen von Härte und Glasübergangstemperatur die stärksten Alterungseffekte auf. Weiterhin hatte heterogene Alterung aufgrund von diffusionsbegrenzten Oxidationseffekten einen wesentlichen Einfluss auf HNBR bei Alterungstemperaturen von 125 °C und 150 °C. EPDM zeigte ähnliche Eigenschaftsänderungen wie HNBR, allerdings schwächer ausgeprägt. FKM wies nur geringfügige Alterungseffekte auf. O-Ringe, die verpresst gealtert wurden, hatten eine starke bleibende Verformung (DVR). Die gemessenen DVRWerte wurden für eine Zeit-Temperatur-Verschiebung und die Konstruktion einer Masterkurve genutzt. Leckageratenmessungen zeigten, dass O-Ringe unter statischen Bedingungen dicht bleiben können, auch wenn die Materialeigenschaften schon stark degradiert sind. KW - Aging KW - Degradation KW - Leakage KW - Compression KW - Seal PY - 2016 SN - 0022-9520 SN - 0948-3276 VL - 69 IS - 4 SP - 36 EP - 42 PB - Hüthig CY - Heidelberg, Germany AN - OPUS4-36336 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Influence of Ageing on Sealability of HNBR, EPDM and FKM O-rings N2 - At BAM, which is the federal institute for materials research and testing in Germany, it is one of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes assessment of elastomeric seals applied in the containers. Besides examining the low-temperature behaviour and irradiation effects of elastomeric seals, it is our goal to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Therefore, we started an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) which are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) up to 1 year. In order to assess sealability, O-rings are aged in compression by 25 % (corresponding to the compression during service) between plates as well as in flanges that allow leakage rate measurements. For comparison, uncompressed O-rings are aged as well. Further methods characterising seal performance are compression stress relaxation (CSR) reflecting the loss of sealing force of a compressed seal over time, and compression set (CS) which represents the recovery behaviour of a seal after release from compression. Additionally, hardness is measured for information about the change of mechanical properties. The experimental results indicate that while hardness, CSR and CS show considerable degradation effects, the leakage rate stays constant or even decreases until shrinkage and the loss of resilience of the aged seal leads to the formation of a leakage path. This indicates that static leakage rate, which is the only available direct seal performance criterion, has only limited sensitivity for the degradation of the seal material. T2 - International Sealing Conference CY - Stuttgart, Germany DA - 12.10.2016 KW - Rubber KW - Seal KW - Degradation PY - 2016 SN - 978-3-8163-0674-9 VL - 2016 SP - 551 EP - 563 PB - VDMA AN - OPUS4-38014 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Aging of elastomeric seals for storage casks N2 - Elastomeric seals are used in many containers, including casks for radioactive waste. However, like all polymers, elastomers are prone to aging, which leads to a loss of sealing force and the ability for recovery which can ultimately result in leakage. Therefore it is important to be able to define an end-of-lifetime criterion and to judge the lifetime of elastomeric seals. For this reason, we started an aging program on three kinds of rubbers (HNBR, EPDM, FKM), monitoring the change of properties at four different aging temperatures over extended periods up to five years. The measured data is used for lifetime prediction by applying a suitable model. T2 - WM2015 Conference CY - Phoenix, Arizona, USA DA - 15.03.2015 KW - Aging KW - Elastomer KW - Seal KW - Leakage KW - Compression PY - 2015 SN - 978-0-9828171-4-8 SP - 15080, 1 EP - 12 AN - OPUS4-33253 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Low temperature properties of rubber seals - influence of gamma irradiation N2 - Rubbers are widely used as sealing material in various applications. In many fields, the function of seal materials at low temperatures is required. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. KW - Compression set KW - Irradiation KW - O-ring KW - Seal PY - 2014 SN - 978-3981407624 SP - 1 EP - 7 AN - OPUS4-32326 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, Maha A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Overview of ongoing long-term ageing investigations on elastomer seals N2 - At the Bundesanstalt für Materialforschung und -prüfung (BAM) in Division 3.4 Safety of Storage Containers, one of our tasks is to evaluate the safety of containers designed for disposal of low and intermediate radioactive waste. As such containers might be transported before and stored until disposal, safe enclosure of the radioactive inventory is important for this time span. Elastomer O-rings are widely used as barrier seals in these containers. Thus, as for many other applications, an understanding of the practical effects of ageing degradation on elastomer seals during long-term exposure is mandatory for predicting the lifetime of such components. According to a long-term test programme on three kinds of rubbers (EPDM and FKM (relevant for application), HNBR (for comparison)), over several years we have studied the degradation and the change of mechanical properties (e.g. hardness, strain at break) at four different ageing temperatures (75 °C, 100 °C, 125 °C and 150 °C) as well as the change of sealing properties. Continuous and intermittent compression stress relaxation (CSR) measurements were performed in order to investigate the respective contribution of crosslinking and chain scission to the observed degradation effects. Thus, the degradation kinetics and mechanisms could be resolved more clearly. For assessing the seal performance, compression set (CS) and leakage rate measurements were conducted. The experimental results showed that the O-rings remained leak-tight under purely static conditions even when CSR, CS and mechanical properties already indicated far advanced degradation. For this reason, a modified leakage test involving a small and rapid partial decompression of the seal was developed that enabled determining an end-of-lifetime criterion for O-rings with a safety margin for thermal shrinkage and vibrations. KW - Seal KW - O-Ring KW - Ageing KW - Component tests PY - 2020 SN - 1863-7116 VL - 15 IS - 3 SP - 146 EP - 151 PB - Gupta CY - Ratingen AN - OPUS4-51161 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Influence of gamma irradiation on low temperature properties of rubber seal materials N2 - In many fields the function of seal materials is required at low temperatures. Therefore the understanding of failure mechanisms at low temperatures is of high importance. In some applications elastomeric seals are used in environments with increased irradiation backgrounds, as e.g. in containers for radioactive waste. This paper reports on the influence of gamma irradiation on the low temperature properties of different fluorocarbon rubber (FKM) materials. The samples were irradiated with gamma doses of up to 600 kGy and the induced changes of material properties were tested by methods sensitive to the rubber-glass transition, like DSC and DMA. Additionally, compression set measurements were performed to give information about recovery behaviour at low temperatures. KW - Seal KW - O-ring KW - Low temperature KW - Gamma irradiation KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Gamma-Bestrahlung KW - Druckverformungsrest PY - 2015 SN - 0948-3276 SN - 0022-9520 VL - 68 IS - 6 SP - 85 EP - 89 PB - Hüthig CY - Heidelberg AN - OPUS4-33552 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Alterung von Elastomerdichtungen für Lagerbehälter N2 - Unsere Aufgabe im Fachbereich 3.4 der Bundesanstalt für Materialforschung und prüfung (BAM) ist die sicherheitstechnische Begutachtung von Transport- und Lagerbehältern für radioaktiven Abfall, die für langfristige Zwischenlagerung ausgelegt sind. Ein Arbeitsschwerpunkt ist die Bewertung der Lebensdauer von Metall- und Elastomerdichtungen in den Behältern im Hinblick auf die Anforderungen für langfristige Behältersicherheit (min. 40 Jahre in Deutschland). Um die Eigenschaftsänderungen der Elastomerdichtungen während einer beschleunigten Alterung über lange Zeiträume (bis zu fünf Jahre) untersuchen zu können, wurde ein Alterungsprogramm an ausgewählten Elastomeren (HNBR, EPDM, FKM) begonnen. Im Gegensatz zu Normalterungsverfahren altern wir keine Normteile, sondern O-Ringe im unverpressten sowie verpressten Zustand. Diese Vorgehensweise ermöglicht die Bewertung des Einflusses der Verpressung auf die Alterung sowie die Untersuchung des Bauteilversagens mittels Leckageratenmessungen unter anwendungsnahen Bedingungen. Weitere Charakterisierungsmethoden sind Härtemessung, dynamisch-mechanische Analyse (DMA), Thermogravimetrie (TGA), Druckspannungsrelaxation, Druckverformungsrest (DVR), Dichtebestimmung und Zugversuch. Das Ziel ist, die Leckagerate mit anderen Eigenschaften bzw. Methoden zu korrelieren, um so ein aussagekräftiges und leichter zu bestimmendes Lebensdauerkriterium für elastomere O-Ringe abzuleiten. Während der Alterung können in Abhängigkeit von Material sowie Alterungsdauer und –temperatur Inhomogenitäten aufgrund von diffusionsbegrenzter Oxidation auftreten, durch die sich unterschiedliche Eigenschaften an der Oberfläche und im Volumen der Dichtung ergeben, was zu falschen Lebensdauerabschätzungen führen kann. Mittels Mikrohärtemessung über den Querschnitt werden diese Effekte charakterisiert und bei der Extrapolation mittels Zeit-Temperatur-Verschiebung und Arrheniusgraph berücksichtigt. Bisher liegen Daten von bis zu einem Jahr bei vier verschiedenen Temperaturen (75 °C, 100 °C, 125 °C und 150 °C) gealterten Proben vor. Nach 100 Tagen bei 150 °C weisen HNBR und EPDM schon einen DVR von über 80 % auf, aber noch keinen signifikanten Anstieg der Leckagerate. Diese sinkt zunächst während der Alterung, da die Permeabilität aufgrund von Vernetzungsreaktionen sinkt. Bei HNBR ist dies aufgrund der dominanteren Vernetzungsreaktionen während der Alterung noch stärker ausgeprägt als bei EPDM. T2 - Technomer 2015 - 24. Fachtagung über Verarbeitung und Anwendung von Polymeren CY - Chemnitz, Germany DA - 12.11.2015 KW - Aging KW - Elastomer KW - Seal KW - Leakage KW - Compression PY - 2015 SN - 978-3-939382-12-6 SP - 43 CY - Chemnitz AN - OPUS4-35050 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Ageing of elastomeric seals for storage containers N2 - At BAM Federal Institute for Materials Research and Testing in Germany, it is our responsibility to audit the safety of casks designed for transport and/or storage of radioactive material. With regard to the requirements on long-term safety of the containers, it is necessary to evaluate the service lifetime of the elastomeric seals used in the containers. With ageing, the elastomers will gradually lose their elasticity and their ability for recovery, which might result in a leakage above the allowed level or in a release of radioactivity during an incident. It is important to know the rate of degradation and which property can be used as an practical and easily measurable end-of-lifetime criterion. For this reason, we devised ageing experiments on different kinds of elastomers, namely FKM, EPDM and HNBR. The former two are actually used in containers for radioactive wastes – either as auxiliary seal in casks containing high activity waste, or as main seal in casks for medium or low activity waste. The latter is an often used seal material that is tested for comparative reasons. In our ageing program, these three materials are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) in order to extrapolate the data to service temperature using a suitable model. They are examined at logarithmic time intervals of several days up to 5 years. The samples are aged in their undeformed O-ring state as well as compressed between flanges with a deformation corresponding to the actual compression during service. Thus we can compare the ageing between relaxed and stressed sample. Additionally, we are ageing samples in flanges that allow leakage rate measurements. Other measurements include monitoring of the recovery force of the seal and the compression set. Furthermore, the samples are examined by thermal and dynamic-mechanical analysis for detecting changes in the glass transition temperature due to crosslinking or chain scission in the material. Besides, hardness is measured as a practical macroscopic indicator. Until now, we have analyzed samples aged up to 100 days. At the highest ageing temperature of 150 °C, the compressed EPDM has already reached a compression set of 95 %, while HNBR and FKM have reached 80 % and 30 %, respectively. Furthermore, HNBR has reached a Shore D hardness of 85, which is an immense increase after the initial value of 80 Shore A. However, when looking at the cross-section of the sample, it was obvious that only a layer of about 1 mm thickness has become so hard, while the inner part remained rubbery. This shows that there has been intense crosslinking mostly near the surface of the HNBR which forms a kind of oxygen diffusion barrier, inhibiting the thermooxidation of the inner part of sample which can retain elastic properties. In EPDM, the oxygen permeability is much greater, which leads to a more homogeneous degradation across the whole sample and thus resulted in a higher compression set. The low compression set of FKM shows the outstanding high-temperature properties of this material. T2 - Annual Meeting on Nuclear Technology 2015 CY - Berlin, Germany DA - 2015-05-05 KW - Elastomer KW - Rubber KW - Aging KW - Lifetime KW - Seal KW - Cask KW - Compression PY - 2015 SN - 978-3-926956-98-9 SP - 1 EP - 10(?) PB - INFORUM-Verl. u. Verwaltungsges. AN - OPUS4-33782 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Ageing of elastomeric seals for storage containers N2 - At BAM Federal Institute for Materials Research and Testing in Germany, it is our responsibility to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes the investigation of elastomeric seals applied in the containers. Besides examining the low-temperature behavior of elastomeric seals, it is our goal to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Furthermore, we deem it necessary to exceed the requirements given in the ageing standard DIN 53508 and take into account diffusion-limited oxidation (DLO) effects and non-Arrhenius behavior when making lifetime predictions. Therefore, we started an ageing programme with selected rubbers (HNBR, FKM and EPDM) which are oven-aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) in order to extrapolate the data to service temperature using different models and check which one is appropriate. Samples are examined at different times up to 5 years. In order to be able to compare between compressed and relaxed rubber, they are aged in two conditions: the undeformed O-ring state as well as compressed between plates with a compression of 25 % corresponding to the actual compression during service. Additionally, we are ageing samples in flanges that allow leakage rate measurements which is the central performance criterion. Analysis methods include hardness as a quick indicator, compression set and compression stress relaxation as measures reflecting the actual properties of a compressed seal. Additionally, we are applying classical polymer analysis methods like dynamic mechanic analysis and thermogravimetric analysis which show changes in the polymeric structure due to chain scission and crosslinking. Furthermore, we are testing the leakage rate of the O-rings in order to correlate the changes in physical properties to the actual performance of the seal. First results of samples aged up to 100 days show a strong increase in hardness for HNBR, a moderate increase for EPDM and hardly a change for FKM. A similar result is seen in the compression set of samples aged 100 d at 100 °C in compression as HNBR has reached 60 %, EPDM 25 % and FKM 15 % compression set. However, after ageing at 150 °C, EPDM shows a worse performance with 95 % compression set compared to HNBR with only 80 %. This is probably due to DLO effects in HNBR that appear because of the fast ageing and low oxygen permeability in HNBR. This leads to a deficit of oxygen in the center of the sample which is thus protected from ageing and can retain elastic properties. The full paper shall discuss the changes in material properties observed to date and the impact on the performance of elastomeric seals. T2 - IRC 2015 - International rubber conference CY - Nürnberg, Germany DA - 29.06.2015 KW - Elastomer KW - Rubber KW - Aging KW - Lifetime KW - Seal KW - Cask KW - Compression PY - 2015 SP - 1 EP - 10 AN - OPUS4-34939 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar ED - Van Breugel, K. ED - Koenders, E.A.B. T1 - Approach for the investigation of long-term behaviour of elastomeric seals for transport and storage packages N2 - Elastomers are widely used as main sealing materials for Containers for low and intermediate Ievel radioactive waste and as additional component to metal seals in spent fuel and high active waste Containers. According to appropriate guidelines and regulations safe enclosure of the radioactive Container contents has to be guaranteed for long storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of seal behaviour in general is of high importance and ageing of elastomeric seals has to be considered with regard to possible dynamic events taking possibly place during transport after storage. T2 - 1st Ageing of materials & structures 2014 conference CY - Delft, The Netherlands DA - 26.05.2014 KW - O-Ring KW - Seal KW - Ageing KW - Elastomer KW - Compression set PY - 2014 SN - 978-94-6186-313-3 SP - 87 EP - 93 AN - OPUS4-30820 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Grelle, Tobias A1 - Goral, Milan A1 - Wolff, Dietmar ED - Gehde, M. ED - Wagenknecht, U. ED - Bloß, P. T1 - Further investigations on the low temperature performance of rubber seals N2 - For many sealing applications low temperature performance is required. The overall understanding of the relevant influences on low temperature performance of rubber seals are summarized and the currently running investigations described. The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the performance during/after fast partial relief of seals at low temperatures. T2 - Technomer 2017 CY - Chemnitz, Germany DA - 09.11.2017 KW - Seal KW - Low temperature KW - Rubber KW - Recovery PY - 2017 SN - 978-3-939382-13-3 VL - 2017 SP - 40 EP - 40 AN - OPUS4-42845 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Subramani Bhagavatheswaran, E. A1 - Wießner, S. A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Aging study and electrical resistance based stress-monitoring of rubber seals N2 - Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste. In addition, they are also used in waste fuel storage and transportation casks as auxiliary seals. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with respect to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period. A fundamental understanding of the structure property relationship and their changes during aging can help to evaluate the long-term sealing performance. In the present study, specific materials are investigated to study the structure-property and seal performance-correlation. Fluoro-elastomer (FKM), silicone rubber (VMQ) and ethylene propylene diene rubber (EPDM) were chosen as base rubbers. Comparable mechanical properties for these seals, especially in terms of a comparable compression behavior were achieved by careful control of base rubber formulation, i.e., by opting for the right filler and its concentration, amount of crosslinking chemicals, and with the assistance of process oils. Moreover, with the same rubber, similar mechanical properties were achieved by varying the filler concentration and crosslinking degree, which shall enable to correlate the particular influence on the structure property dependency of the seals in detail. The materials are investigated under pristine and aged conditions to evaluate the influence of aging, e.g. on the stress relaxation or recovery behavior. These values appear to be suitable parameters to judge the expected sealing performance. Due to the electrically conducting nature of some fillers used to reinforce rubbers (such as carbon blacks, carbon nanotubes (CNTs), Graphene, etc.) it is possible to obtain current information about mechanical and visco-elastic properties by monitoring the electrical conductivity or resistivity. A simple relation that relates electrical resistance with mechanical stress was derived and the stress values were theoretically predicted from the electrical resistance values, which showed good correlation with experimental results. T2 - 192nd Technical meeting of the ACS Rubber Division CY - Cleveland, OH, USA DA - 09.10.2017 KW - Seal KW - Rubber KW - Degradation KW - Structure-property relationship KW - Ageing PY - 2017 VL - 2017 SP - 1 EP - 25 AN - OPUS4-42849 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Jaunich, Matthias A1 - Kömmling, Anja A1 - Wolff, Dietmar ED - Grellmann, W. ED - Langer, B. T1 - Investigations of elastomeric seals – Low temperature performance and aging behavior N2 - Due to their simple and reliable application, elastomers are used for many tasks. Many fields of application like transport, aviation and process technology, entail low temperatures where proper functionality of the employed seals has to be ensured. Therefore, understanding the low temperature behavior of elastomeric seals is important for safe seal operation to restrict the temperature application range. For all areas of application, the question of seal lifetime is also important for replacement or maintenance intervals. The lifetime is especially important in applications that allow no seal replacement. Since the seal can determine the lifetime of storage in such cases, reliable lifetime estimation is necessary for these applications, and requires an extensive knowledge of the specific aging behavior. KW - Seal KW - Rubber KW - Ageing KW - Replacement PY - 2017 SN - 978-3-319-41877-3 SN - 978-3-319-41879-7 U6 - https://doi.org/10.1007/978-3-319-41879-7_30 SN - 0933-033X SN - 2196-2812 VL - 247 SP - 431 EP - 443 PB - Springer Verlag AN - OPUS4-41167 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Hagenow, Peter A1 - Kasparek, Eva Maria A1 - Kömmling, Anja A1 - Noack, Volker A1 - Völzke, Holger A1 - Wolff, Dietmar T1 - Requirements for the use of elastomer seals in casks for final disposal of low and intermediate level waste N2 - Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period. In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits. Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to: - ensure full functionality until final container disposal, - maintain its function in case of a thermal or mechanical accident, - ensure encapsulation also at -20 °C. This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated. This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results. T2 - 13th Internationales Symposium "Konditionierung radioaktiver Betriebs- und Stillegungsabfälle CY - Dresden, Germany DA - 22.03.2017 KW - Disposal KW - Konrad repository KW - Seal PY - 2017 SP - 595 EP - 601 AN - OPUS4-39870 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -