TY - CONF A1 - Jaunich, Matthias A1 - Grelle, Tobias A1 - Goral, Milan A1 - Wolff, Dietmar ED - Gehde, M. ED - Wagenknecht, U. ED - Bloß, P. T1 - Further investigations on the low temperature performance of rubber seals N2 - For many sealing applications low temperature performance is required. The overall understanding of the relevant influences on low temperature performance of rubber seals are summarized and the currently running investigations described. The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the performance during/after fast partial relief of seals at low temperatures. T2 - Technomer 2017 CY - Chemnitz, Germany DA - 09.11.2017 KW - Seal KW - Low temperature KW - Rubber KW - Recovery PY - 2017 SN - 978-3-939382-13-3 VL - 2017 SP - 40 EP - 40 AN - OPUS4-42845 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Hagenow, Peter A1 - Kasparek, Eva Maria A1 - Kömmling, Anja A1 - Noack, Volker A1 - Völzke, Holger A1 - Wolff, Dietmar T1 - Requirements for the use of elastomer seals in casks for final disposal of low and intermediate level waste N2 - Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period. In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits. Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to: - ensure full functionality until final container disposal, - maintain its function in case of a thermal or mechanical accident, - ensure encapsulation also at -20 °C. This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated. This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results. T2 - 13th Internationales Symposium "Konditionierung radioaktiver Betriebs- und Stillegungsabfälle CY - Dresden, Germany DA - 22.03.2017 KW - Disposal KW - Konrad repository KW - Seal PY - 2017 SP - 595 EP - 601 AN - OPUS4-39870 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Jaunich, Matthias A1 - Kömmling, Anja A1 - Wolff, Dietmar ED - Grellmann, W. ED - Langer, B. T1 - Investigations of elastomeric seals – Low temperature performance and aging behavior N2 - Due to their simple and reliable application, elastomers are used for many tasks. Many fields of application like transport, aviation and process technology, entail low temperatures where proper functionality of the employed seals has to be ensured. Therefore, understanding the low temperature behavior of elastomeric seals is important for safe seal operation to restrict the temperature application range. For all areas of application, the question of seal lifetime is also important for replacement or maintenance intervals. The lifetime is especially important in applications that allow no seal replacement. Since the seal can determine the lifetime of storage in such cases, reliable lifetime estimation is necessary for these applications, and requires an extensive knowledge of the specific aging behavior. KW - Seal KW - Rubber KW - Ageing KW - Replacement PY - 2017 SN - 978-3-319-41877-3 SN - 978-3-319-41879-7 U6 - https://doi.org/10.1007/978-3-319-41879-7_30 SN - 0933-033X SN - 2196-2812 VL - 247 SP - 431 EP - 443 PB - Springer Verlag AN - OPUS4-41167 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Low temperature properties of rubber seals - influence of gamma irradiation N2 - Rubbers are widely used as sealing material in various applications. In many fields, the function of seal materials at low temperatures is required. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. KW - Compression set KW - Irradiation KW - O-ring KW - Seal PY - 2014 SN - 978-3981407624 SP - 1 EP - 7 AN - OPUS4-32326 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Influence of gamma irradiation on low temperature properties of rubber seal materials N2 - In many fields the function of seal materials is required at low temperatures. Therefore the understanding of failure mechanisms at low temperatures is of high importance. In some applications elastomeric seals are used in environments with increased irradiation backgrounds, as e.g. in containers for radioactive waste. This paper reports on the influence of gamma irradiation on the low temperature properties of different fluorocarbon rubber (FKM) materials. The samples were irradiated with gamma doses of up to 600 kGy and the induced changes of material properties were tested by methods sensitive to the rubber-glass transition, like DSC and DMA. Additionally, compression set measurements were performed to give information about recovery behaviour at low temperatures. KW - Seal KW - O-ring KW - Low temperature KW - Gamma irradiation KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Gamma-Bestrahlung KW - Druckverformungsrest PY - 2015 SN - 0948-3276 SN - 0022-9520 VL - 68 IS - 6 SP - 85 EP - 89 PB - Hüthig CY - Heidelberg AN - OPUS4-33552 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Wolff, Dietmar ED - Van Breugel, K. ED - Koenders, E.A.B. T1 - Approach for the investigation of long-term behaviour of elastomeric seals for transport and storage packages N2 - Elastomers are widely used as main sealing materials for Containers for low and intermediate Ievel radioactive waste and as additional component to metal seals in spent fuel and high active waste Containers. According to appropriate guidelines and regulations safe enclosure of the radioactive Container contents has to be guaranteed for long storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of seal behaviour in general is of high importance and ageing of elastomeric seals has to be considered with regard to possible dynamic events taking possibly place during transport after storage. T2 - 1st Ageing of materials & structures 2014 conference CY - Delft, The Netherlands DA - 26.05.2014 KW - O-Ring KW - Seal KW - Ageing KW - Elastomer KW - Compression set PY - 2014 SN - 978-94-6186-313-3 SP - 87 EP - 93 AN - OPUS4-30820 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Stark, Wolfgang T1 - Low temperature properties of rubber seals - Results of component tests - N2 - Rubbers are widely used as sealing material in various applications. In many fieldsthefunction of seal materials at lowtemperatures is required. Therefore the understanding of faiiure mechanisms that lead to leakage at low temperatures is of high importance. Therefore the lower Operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the Standard tests a faster and more efficient technique was developed and applied. In addition the breakdown temperature of the sealing function of O-ring seals at lowtemperatures is measured in a component test Setup in dependence of the material and the degree of compression. KW - Seal KW - O-ring KW - Low temperature KW - Component test KW - Compression set KW - Dichtungen KW - O-Ringe KW - Tiefe Temperatur KW - Bauteilversuche KW - Druckverformungsrest PY - 2013 SN - 0948-3276 SN - 0022-9520 VL - 66 IS - 7-8 SP - 26 EP - 30 PB - Hüthig CY - Heidelberg AN - OPUS4-28894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Ageing of HNBR, EPDM and FKM O-rings N2 - HNBR, EPDM and FKM O-rings were aged uncompressed and compressed at 75 °C, 100 °C, 125 °C and 150 °C for up to 1 year. HNBR exhibited the strongest ageing effects with high increases of hardness and glass transition temperature. Furthermore, heterogeneous ageing caused by diffusion-limited oxidation effects had a significant influence for HNBR at ageing temperatures of 125 °C and 150 °C. EPDM showed similar property changes as HNBR, but less pronounced. FKM displayed only minor ageing effects. O-rings aged in compression exhibited considerable compression set (CS). CS data was used for a time-temperature shift and resulting master curve construction. Leakage rate measurements showed that O-rings can remain leak tight under static conditions even if material properties have already deteriorated strongly. N2 - HNBR-, EPDM- und FKM-O-Ringe wurden unverpresst und verpresst für bis zu 1 Jahr bei 75 °C, 100 °C, 125 °C und 150 °C gealtert. HNBR wies mit hohen Anstiegen von Härte und Glasübergangstemperatur die stärksten Alterungseffekte auf. Weiterhin hatte heterogene Alterung aufgrund von diffusionsbegrenzten Oxidationseffekten einen wesentlichen Einfluss auf HNBR bei Alterungstemperaturen von 125 °C und 150 °C. EPDM zeigte ähnliche Eigenschaftsänderungen wie HNBR, allerdings schwächer ausgeprägt. FKM wies nur geringfügige Alterungseffekte auf. O-Ringe, die verpresst gealtert wurden, hatten eine starke bleibende Verformung (DVR). Die gemessenen DVRWerte wurden für eine Zeit-Temperatur-Verschiebung und die Konstruktion einer Masterkurve genutzt. Leckageratenmessungen zeigten, dass O-Ringe unter statischen Bedingungen dicht bleiben können, auch wenn die Materialeigenschaften schon stark degradiert sind. KW - Aging KW - Degradation KW - Leakage KW - Compression KW - Seal PY - 2016 SN - 0022-9520 SN - 0948-3276 VL - 69 IS - 4 SP - 36 EP - 42 PB - Hüthig CY - Heidelberg, Germany AN - OPUS4-36336 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Influence of Ageing on Sealability of HNBR, EPDM and FKM O-rings N2 - At BAM, which is the federal institute for materials research and testing in Germany, it is one of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes assessment of elastomeric seals applied in the containers. Besides examining the low-temperature behaviour and irradiation effects of elastomeric seals, it is our goal to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Therefore, we started an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) which are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) up to 1 year. In order to assess sealability, O-rings are aged in compression by 25 % (corresponding to the compression during service) between plates as well as in flanges that allow leakage rate measurements. For comparison, uncompressed O-rings are aged as well. Further methods characterising seal performance are compression stress relaxation (CSR) reflecting the loss of sealing force of a compressed seal over time, and compression set (CS) which represents the recovery behaviour of a seal after release from compression. Additionally, hardness is measured for information about the change of mechanical properties. The experimental results indicate that while hardness, CSR and CS show considerable degradation effects, the leakage rate stays constant or even decreases until shrinkage and the loss of resilience of the aged seal leads to the formation of a leakage path. This indicates that static leakage rate, which is the only available direct seal performance criterion, has only limited sensitivity for the degradation of the seal material. T2 - International Sealing Conference CY - Stuttgart, Germany DA - 12.10.2016 KW - Rubber KW - Seal KW - Degradation PY - 2016 SN - 978-3-8163-0674-9 VL - 2016 SP - 551 EP - 563 PB - VDMA AN - OPUS4-38014 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kömmling, Anja A1 - Jaunich, Matthias A1 - Wolff, Dietmar T1 - Aging of elastomeric seals for storage casks N2 - Elastomeric seals are used in many containers, including casks for radioactive waste. However, like all polymers, elastomers are prone to aging, which leads to a loss of sealing force and the ability for recovery which can ultimately result in leakage. Therefore it is important to be able to define an end-of-lifetime criterion and to judge the lifetime of elastomeric seals. For this reason, we started an aging program on three kinds of rubbers (HNBR, EPDM, FKM), monitoring the change of properties at four different aging temperatures over extended periods up to five years. The measured data is used for lifetime prediction by applying a suitable model. T2 - WM2015 Conference CY - Phoenix, Arizona, USA DA - 15.03.2015 KW - Aging KW - Elastomer KW - Seal KW - Leakage KW - Compression PY - 2015 SN - 978-0-9828171-4-8 SP - 15080, 1 EP - 12 AN - OPUS4-33253 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -